Minimum port interdigital sensor array based on screen printing and preparation method thereof

Through screen printing technology, the interfin sensor array is constructed on a flexible substrate, which solves the problems of many output ports and poor flexibility performance of the sensor array, and realizes high sensitivity and stability pressure detection, which is suitable for human skin surface applications.

CN118945987AActive Publication Date: 2024-11-12OCEAN UNIV OF CHINA +2

Patent Information

Application Number
CN202410999484.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-24
Publication Date
2024-11-12
Estimated Expiration
2044-07-24

AI Technical Summary

Technical Problem

The existing interfinger sensor arrays have shortcomings in sensor integration and comprehensive information detection, and have poor flexibility and conformal adhesion performance when applied to human skin surfaces. This is mainly due to the single-sided construction of interfinger sensors, resulting in complex conductor crossing. There are many output ports.

Method used

The smallest port interdigital sensor array is prepared by screen printing technology, and the interdigital electrode layer, insulating layer, wire layer and sensitive layer are formed by laser etching and screen printing on a flexible substrate, combining the spacer layer and the second Insulating layer realizes electrical shielding and structural reinforcement of wire crossing.

Benefits of technology

It effectively reduces the number of sensor output ports, improves flexibility and mechanical performance, improves the sensitivity and stability of the sensor, realizes high-sensitivity pressure detection, and shows excellent abilities in haptic sensing and physiological information detection.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118945987A_ABST
    Figure CN118945987A_ABST
Patent Text Reader

Abstract

The invention discloses a minimum port interdigital sensor array based on screen printing and a preparation method thereof, and belongs to the field of flexible wearable electronics and micro-nano sensing devices. The preparation method of the interdigital sensor array comprises the following steps: S1, preparing an interdigital electrode layer; s2, coating a first insulating layer; s3, coating an electrode layer wire; s4, coating a second insulating layer; s5, coating a spacing layer; s6, preparing a sensitive layer; s7, packaging the sensor array; and aligning and bonding the electrode layer, the first insulating layer, the electrode layer wire, the second insulating layer and the spacer layer thin film prepared in the step S5 with the sensitive layer prepared in the step S6, and packaging to obtain the minimum port interdigital sensor array based on screen printing. The number of output ports of the interdigital sensor array can be reduced as much as possible, excellent flexibility is kept, the overall mechanical property is improved, and high sensitivity and high stability are achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of flexible wearable electronics and micro-nano sensor devices, and in particular relates to a minimum port interdigital sensor array based on screen printing and a preparation method thereof. Background Art

[0002] As a new cross-disciplinary subject, flexible sensors are booming in the fields of electronic skin, human-computer interaction and medical diagnosis. As one of the classic choices of flexible sensors, "interdigital electrode" type sensors have been widely discussed by scholars. However, the scope of discussion is mostly limited to single sensors and multi-channel small sensor arrays, or large-area arrays based on FPCB. The former has serious deficiencies in sensor integration and comprehensive information detection, while the latter has mechanical disadvantages in sensor flexibility, conformal attachment and human skin surface application. The reason is that as a typical representative of single-sided construction of positive and negative electrodes, the construction of multi-channel sensor arrays faces the current situation of numerous leads and dense I / O ports. The minimum port output is designed to achieve the crossover of rows and columns of the sensor array, and the sensor is selected by rows and columns, which can effectively reduce the number of output ports in the interdigital sensor. At this stage, most solutions rely on FPCB via manufacturing to avoid wire crossing at the expense of flexibility. Obviously, this is not a good choice. Summary of the invention

[0003] Based on the above technical problems, the present invention proposes a minimum port interdigital sensor array based on screen printing and a preparation method thereof.

[0004] The technical solution adopted by the present invention is:

[0005] One of the purposes of the present invention is to provide a method for preparing a minimum port interdigital sensor array based on screen printing, comprising the following steps:

[0006] S1, preparing an interdigitated electrode layer;

[0007] Selecting a flexible substrate, and performing laser etching on the flexible substrate to obtain a flexible substrate with a shading structure;

[0008] Screen printing a conductive ink on a flexible substrate with a textured structure to obtain an interdigitated electrode layer;

[0009] S2, coating a first insulating layer;

[0010] Screen printing insulating ink on the lead overlapped position on the interdigital electrode layer to form a first insulating layer, thereby obtaining an electrode layer-first insulating layer film;

[0011] S3, coating electrode layer wire;

[0012] Screen printing a conductive ink on the electrode layer-first insulating layer film obtained in S2 to form an electrode layer wire interconnecting the electrodes, thereby obtaining an electrode layer-first insulating layer-electrode layer wire film;

[0013] S4, applying a second insulating layer;

[0014] Screen-printing insulating ink on the electrode layer-first insulating layer-electrode layer wire film obtained in S3 to form a second insulating layer to prevent crosstalk, thereby obtaining an electrode layer-first insulating layer-electrode layer wire-second insulating layer film;

[0015] S5, coating a spacer layer;

[0016] Screen-printing the spacer layer ink on the electrode layer-first insulating layer-electrode layer wire-second insulating layer film obtained in S4 to form a spacer layer, thereby obtaining an electrode layer-first insulating layer-electrode layer wire-second insulating layer-spacer layer film;

[0017] S6, preparing a sensitive layer;

[0018] Select a flexible substrate, screen-print the sensitive layer ink on the flexible substrate, and then perform laser etching to obtain a sensitive layer;

[0019] S7, sensor array packaging;

[0020] The electrode layer-first insulating layer-electrode layer wire-second insulating layer-spacer layer film prepared in S5 is aligned and bonded with the sensitive layer prepared in S6, and then packaged to obtain a minimum port interdigital sensor array based on screen printing.

[0021] The second object of the present invention is to provide a minimum port interdigital sensor array based on screen printing prepared by the above method, the interdigital sensor array comprises a sensitive layer, a spacer layer, a second insulating layer, an electrode layer wire, a first insulating layer and an interdigital electrode layer stacked in sequence from top to bottom;

[0022] The interdigital electrode layer is an integrated structure formed by a first flexible substrate with a first shading structure and an interdigital electrode array screen-printed thereon; the first insulating layer covers the overlapping parts of the leads of the interdigital electrode array, the electrode layer wires are arranged above the first insulating layer, the overlapping parts of the leads of the interdigital electrode array are separated from the electrode layer wires by the first insulating layer, and the electrode layer wires are connected to the interdigital electrode array;

[0023] The second insulating layer covers the first flexible substrate, and an array through hole is provided at a position on the second insulating layer directly facing the interdigital electrode array;

[0024] The spacing layer comprises an outer frame, and spacing bars are arranged in an inner space formed by the outer frame, the spacing bars are located at the gaps facing the interdigital electrode array, and the spacing bars comprise a plurality of segments;

[0025] The sensitive layer comprises a second flexible substrate, on which a sensitive region array is arranged, the sensitive region array is located directly above the interdigital electrode array, and a second shading structure is etched on the sensitive region array.

[0026] The beneficial technical effects of the present invention are:

[0027] (1) The present invention can reduce the number of output ports of the interdigital sensor array as much as possible while maintaining excellent flexibility, and the overall mechanical properties are improved, with high sensitivity and high stability.

[0028] (2) The preparation method of the present invention applies screen-printed insulating ink to the intersection of the sensor wires, realizes a "break" connection at the intersection of the sensor's "row lead" and "column lead", shields the electrical connection while ensuring mechanical stability, and achieves the purpose of reducing the number of output ports. Combined with the layout of the second insulating layer, the spacing layer, etc., the sensitivity and stability of the sensor are further improved. In addition, the TPU laser engraved shading at the bottom of the interdigitated electrode layer and the microstructure of the sensitive layer are interlaced to form a stable "arch bridge" reinforcement structure. This overall reinforcement structure improves the conductivity, stability and mechanical properties of the composite system; compared with a single system, this improvement in mechanical properties, the conductive network of the dot-line structure has a higher perception sensitivity; under certain pressure conditions, the pressure perception range is improved, so that the sensor has high sensitivity and high stability. The life of the sensor of the present invention can reach 100,000 times.

[0029] (3) The interdigital sensor array prepared by the present invention is a flexible pressure sensor that can achieve ultra-high sensitivity detection of pressure, and has the characteristics of full flexibility and greatly reduced number of output ports. The sensitive layer is made of carbon nanotubes after screen printing and then laser engraving, which increases the working range of the sensor while maintaining ultra-high sensitivity. At the same time, the transparent flexible substrate TPU laser engraving background at the bottom of the electrode layer can further improve the sensitivity, working range and other parameters of the sensor. The minimum port output is intended to achieve the row and column crossing of the sensor array. Sensor selection through rows and columns can effectively reduce the number of I / O points. The sensor array produced by screen printing of insulating ink shows good electrical shielding at the intersection of the wires, ensuring the accuracy of the sensor during the measurement process. The prepared sensor and its array show excellent capabilities in tactile sensing and physiological information detection. This provides a reliable method for the organic integration of printed electronics, interdigital sensor arrays and minimum ports.

[0030] (4) The present invention successfully reduces the number of output ports from 17 to 8 to achieve electrical insulation and three-dimensional interconnection of wire intersections. The unique printing strategy provides a new idea for the production and manufacturing of matrix-structured interdigitated sensor arrays. The sensor array is fully screen-printed, demonstrating its outstanding flexibility. At the same time, the present invention further improves the mechanical-electrical performance of the sensor by laser engraving the sensitive layer and electrode layer substrate. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] Figure 1 It is a flow chart of the method for preparing the minimum port interdigital sensor array based on screen printing of the present invention;

[0032] Figure 2 This is a schematic diagram of the structural principle of the minimum port interdigital sensor array based on screen printing prepared by the present invention;

[0033] Figure 3 It is a schematic diagram of the structural principle of coating a first insulating layer on the interdigital electrode array in the present invention;

[0034] Figure 4 It is a schematic diagram of the structural principle of the second insulating layer in the present invention;

[0035] Figure 5 Schematic diagram of the structural principle of the spacer layer in the present invention;

[0036] Figure 6 It is a planar schematic diagram of the electrode layer-first insulating layer-electrode layer wire film in the present invention;

[0037] Figure 7 is a schematic plan view of the sensitive layer in the present invention;

[0038] Figure 8 Schematic diagram of the stretching and bending of the interdigital sensor array prepared by the present invention; a shows the stretching state, b shows the bending state, c shows the twisting state, and d shows the protruding state;

[0039] Fig. 9 This is a test data diagram of the interdigital sensor array produced by the present invention.

[0040] In the figure: 1-second flexible substrate, 2-sensitive layer, 3-spacer layer, 4-second insulating layer, 5-electrode layer wire, 6-first insulating layer, 7-interdigitated electrode layer, 8-first flexible substrate;

[0041] 101 - second shading structure, 201 - sensitive area array, 301 - outer frame, 302 - spacer bar, 3021 - segment body, 401 - array through hole, 701 - interdigital electrode array, 702 - gap, 801 - first shading structure. DETAILED DESCRIPTION

[0042] The present invention relies on a planar printing process to produce a sensor array with crossed rows and columns. By sequentially coating a first insulating layer, a second insulating layer, etc., the crossing of wires is effectively avoided during the printing process, and the minimum port output of the sensor plane distribution is achieved; and a vertical groove microstructure is laser engraved on the interdigital electrode layer and the sensitive layer. When the sensitive layer is bonded and aligned with the interdigital electrode layer, the vertical groove microstructure of the sensitive layer and the interdigital electrode layer forms a stable "arch bridge" reinforcement structure, which can further enhance the stability, sensitivity and other performances of the sensor array.

[0043] The present invention will be further described below in conjunction with the accompanying drawings and specific implementations.

[0044] like Figure 1 As shown, a method for preparing a minimum port interdigital sensor array based on screen printing comprises the following steps:

[0045] S1, preparing an interdigitated electrode layer;

[0046] A flexible substrate is selected, and laser etching is performed on one side of the flexible substrate to obtain a flexible substrate with a shading structure (or a vertical groove microstructure). Then, a conductive ink is screen-printed on the flexible substrate with the shading structure (printed on the side with the shading structure etched) to form an interdigitated electrode array. The interdigitated electrode array and the flexible substrate are an integrated structure, namely, an interdigitated electrode layer.

[0047] Specifically, the flexible substrate uses a polyurethane hot melt adhesive film (TPU), which is first placed in a plasma cleaning machine for cleaning, and then placed on the platform below the UV laser machine for vacuum adsorption, and then laser etching is performed. After the etching is completed, the polyurethane hot melt adhesive film is placed in a plasma cleaning machine to clean the etching residues, thereby obtaining a flexible substrate with a shading structure.

[0048] The conductive ink is prepared by stirring slow-drying water and conductive silver paste and mixing them evenly. The conductive ink is screen-printed on one side of the flexible substrate with a shading structure etched thereon to form an interdigital electrode array, which is then heated and cured to obtain an interdigital electrode layer, such as Figure 2 shown.

[0049] S2, coating a first insulating layer;

[0050] The insulating ink is screen-printed on the overlapped part of the lead wires on the interdigitated electrode layer to form a first insulating layer, such as Figure 3 As shown, an electrode layer-first insulating layer thin film is obtained.

[0051] Specifically, the interdigitated electrode layer is placed on a screen printing table, the first insulating layer screen is aligned and placed above the interdigitated electrode layer, the drying type insulating ink is inverted on the first insulating layer screen, and the scraper is tilted to print on the overlapping parts of the interdigitated electrode leads; then it is placed on a heating table for heating and curing to obtain an electrode layer-first insulating layer film.

[0052] S3, coating electrode layer wire;

[0053] Conductive ink is screen-printed on the electrode layer-first insulating layer film obtained in S2 to form electrode layer wires for interconnecting electrodes, thereby obtaining an electrode layer-first insulating layer-electrode layer wire film, such as Figure 6 shown.

[0054] Specifically, the conductive ink is prepared by stirring slow-drying water and conductive silver paste and mixing them evenly. The cured electrode layer-first insulating layer film is placed on a screen printing table, the electrode layer wire screen is aligned and placed above the first insulating layer, the conductive ink is inverted on the electrode layer wire screen, and the scraper is tilted to print at the overlap of the interdigitated electrode leads. Then it is placed on a heating table for heating, and after curing, an electrode layer-first insulating layer-electrode layer wire film is obtained.

[0055] The first insulating layer covers the overlapping parts of the leads of the interdigital electrode array. The electrode layer wires are arranged above the first insulating layer. The overlapping parts of the leads of the interdigital electrode array are separated from the electrode layer wires by the first insulating layer. The electrode layer wires are connected to the interdigital electrode array.

[0056] S4, applying a second insulating layer;

[0057] The insulating ink is screen-printed on the electrode layer-first insulating layer-electrode layer wire film obtained in S3 to form a second insulating layer to prevent crosstalk, thereby obtaining an electrode layer-first insulating layer-electrode layer wire-second insulating layer film.

[0058] Specifically, the electrode layer-first insulating layer-electrode layer wire film obtained after curing is placed on a screen printing table, the second insulating layer screen is aligned and placed above the film, the drying type insulating ink is inverted on the second insulating layer screen, and the scraper is tilted for printing. Then, it is placed on a heating table for heating and curing to obtain an electrode layer-first insulating layer-electrode layer wire-second insulating layer film.

[0059] like Figure 4 As shown, the second insulating layer covers the flexible substrate, and an array through hole is provided on the second insulating layer at a position directly opposite to the interdigital electrode array. That is, the electrode layer-first insulating layer-electrode layer wire film can be covered by the second insulating layer, and the interdigital electrode array is exposed through the array through hole.

[0060] S5, coating a spacer layer;

[0061] The spacer layer ink is screen-printed on the electrode layer-first insulating layer-electrode layer wire-second insulating layer film obtained in S4 to form a spacer layer, thereby obtaining an electrode layer-first insulating layer-electrode layer wire-second insulating layer-spacer layer film.

[0062] Specifically, thermoplastic polyurethane elastomer is mixed with N,N-dimethylformamide, and magnetic stirring is performed to obtain a spacer layer ink. The electrode layer-first insulating layer-electrode layer wire-second insulating layer film obtained after curing is placed on a screen printing table, the spacer layer screen is aligned and placed above the film, the spacer layer ink is inverted on the spacer layer screen, and the scraper is tilted for printing to obtain an electrode layer-first insulating layer-electrode layer wire-second insulating layer-spacer layer film.

[0063] like Figure 5 As shown, the spacing layer includes an outer frame, and spacing bars are arranged in the inner space formed by the outer frame. The spacing bars are located at the gap facing the interdigital electrode array, and the spacing bars include a plurality of segments. The purpose of the spacing layer is to allow a gap to exist between the interdigital electrode layer and the sensitive layer. When the sensor is subjected to pressure, the sensitive layer and the interdigital electrodes contact each other. When the pressure is removed, the gap between the sensitive layer and the interdigital electrode layer needs to be restored to its original state by the spacing layer for the next pressure measurement. In addition, the sensitive layer and the lower layers such as the interdigital electrode layer and the insulating layer need to be bonded together by the spacing layer.

[0064] S6, preparing a sensitive layer;

[0065] A flexible substrate is selected, and the sensitive layer ink is screen-printed on the flexible substrate, and then laser etching is performed to obtain the sensitive layer.

[0066] Specifically, thermoplastic polyurethane elastomer and N,N-dimethylformamide are mixed, magnetically stirred, and carbon nanotube powder is added in the stirring state to obtain sensitive layer ink.

[0067] The flexible substrate adopts a polyurethane hot melt adhesive film, which is placed in a plasma cleaning machine for cleaning and then placed on a heating table for preheating. The polyurethane hot melt adhesive film is then fixed on a screen printing table, a sensitive layer screen is fixed on top of the film, and the sensitive layer ink is inverted on the sensitive layer screen. A scraper is used for tilted printing, and after printing is completed, the film is placed on a heating table for heating and curing.

[0068] Then the polyurethane hot melt adhesive film is placed on the platform below the UV laser machine, vacuum adsorbed, and laser etching is performed on one side of the polyurethane hot melt adhesive film printed with sensitive layer ink, and the upper shading (or vertical grooves) is also etched. After the etching is completed, it is placed in a plasma cleaning machine to clean the etching residues and obtain the sensitive layer.

[0069] like Figure 2As shown, the sensitive layer is a sensitive area array arranged on one side of the flexible substrate, the sensitive area array is arranged corresponding to the interdigital electrode array, and the sensitive area array is located directly above the interdigital electrode array. Figure 2 This is mainly for the convenience of showing the arrangement of the sensitive area array. In actual packaging, the sensitive layer needs to be turned upside down and then combined with the interdigital electrode layer.

[0070] S7, sensor array packaging;

[0071] The electrode layer-first insulating layer-electrode layer wire-second insulating layer-spacer layer film prepared by S5 are aligned and bonded with the sensitive layer prepared by S6, placed in a vacuum heating box, evacuated, heated to 100-110°C, and heated at this temperature for 50-60 minutes, and then cooled to achieve flexible packaging, thereby obtaining a minimum port interdigital sensor array based on screen printing.

[0072] The present invention also provides a minimum port interdigital sensor array based on screen printing prepared by the above method, such as Figure 2-7 As shown, the interdigital sensor array includes a second flexible substrate 1, a sensitive layer 2, a spacer layer 3, a second insulating layer 4, an electrode layer wire 5, a first insulating layer 6, an interdigital electrode layer 7 and a first flexible substrate 8 which are stacked in sequence from top to bottom. The interdigital electrode layer 7 is an integrated structure formed by a first flexible substrate 8 with a first shading structure 801 and an interdigital electrode array 701 screen-printed on the first shading structure. The first insulating layer 6 covers the overlapping part of the leads of the interdigital electrode array 701, and the first insulating layer 6 is a plurality of isolated sheet structures. The electrode layer wire 5 is arranged above the first insulating layer 6, and the overlapping part of the leads of the interdigital electrode array is separated from the electrode layer wire 5 by the first insulating layer 6, and the electrode layer wire 5 is connected to the interdigital electrode array 701. The second insulating layer 4 covers the first flexible substrate 8, and an array through hole 401 is arranged at a position on the second insulating layer 4 directly opposite to the interdigital electrode array. The spacer layer 3 includes an outer frame 301, and spacer bars 302 are arranged in the inner space surrounded by the outer frame 301. The spacer bars are located at the gap 702 facing the interdigital electrode array, and the spacer bars 302 include a plurality of segments 3021. The sensitive layer 2 is formed on the second flexible substrate 1, and a sensitive area array 201 is arranged on the second flexible substrate 1. The sensitive area array 201 is located directly above the interdigital electrode array 701. A second shading structure 101 is etched on the sensitive area array 201.

[0073] Furthermore, when preparing the interdigitated electrode layer 7, a first shading structure 801 is etched on one side of the first flexible substrate 1, and the interdigitated electrode array 701 is screen-printed on the first shading structure 801. The extension direction of the first shading structure 801 is perpendicular to the direction of the interdigitated electrodes in the interdigitated electrode array 701. When preparing the sensitive layer 2, a sensitive area array 201 is screen-printed on one side of the second flexible substrate 1, and then a second shading structure 101 is etched on the sensitive area array 201. The extension direction of the second shading structure 101 is the same as that of the first shading structure 801. Figure 2 It can also be seen that the extension direction of the shading structure is also perpendicular to the extension direction of the electrode layer wire 5. When the sensor array is packaged, the second flexible substrate 1 is inverted on the first flexible substrate 8, and the sensitive area array 201 and the interdigital electrode array 701 are arranged facing each other.

[0074] The present invention prepares an integrated structure including a sensitive layer, a substrate shading and a forked electrode and a transparent flexible substrate TPU, and obtains a flexible forked sensor array by bonding and aligning. The back-end circuit reads the sensor pressure data, and the host computer displays the pressure data. The flexible pressure sensor of the present invention realizes ultra-high sensitivity detection of pressure, and has the characteristics of full flexibility and greatly reducing the number of output ports. The sensitive layer is made of carbon nanotubes after screen printing and laser engraving, which increases the working range of the sensor while maintaining ultra-high sensitivity. At the same time, the transparent flexible substrate TPU laser engraving shading at the bottom of the electrode layer can further improve the sensitivity, working range and other parameters of the sensor. The minimum port output is intended to achieve the row and column crossing of the sensor array, and the sensor selection through the row and column can effectively reduce the number of I / O points. The sensor array made by screen printing of insulating ink shows good electrical shielding at the intersection of the wires, which ensures the accuracy of the sensor during the measurement process. The prepared sensor and its array show excellent capabilities in tactile sensing and physiological information detection. The present invention provides a reliable method for the organic integration of printed electronics, forked sensor arrays and minimum ports.

[0075] The present invention will be further described below in conjunction with specific embodiments.

[0076] Embodiment 1:

[0077] A screen-printed minimum port interdigital sensor array includes: a sensitive layer, a spacer layer, a second insulating layer, an electrode layer wire, a first insulating layer, and an interdigital electrode layer, which are stacked in sequence from top to bottom. The substrate pattern and the interdigital electrode array form an integrated structure on a transparent flexible substrate, the first insulating layer is located above the interdigital electrode array, the electrode layer wire is located above the overlap of the interdigital electrode array and the first insulating layer, and the electrode layer-first insulating layer-electrode layer wire film is connected to the sensitive layer through the second insulating layer and the spacer layer.

[0078] The method for preparing the interdigital sensor array comprises the following steps:

[0079] S1, preparing the integrated structure of substrate shading and interdigital electrode array (interdigital electrode layer):

[0080] Take a culture dish, add 0.05 ml of slow-drying water and 2 g of conductive silver paste, stir for 5 minutes, mix evenly, and prepare conductive ink.

[0081] Take a 10×20cm 2 The polyurethane hot melt adhesive film with a size and thickness of 100μm is placed in a plasma cleaning machine for 2-3 minutes, and then placed on the platform below the UV laser machine, vacuum adsorbed, input the pre-designed vertical grain structure contour, and cut and etched by laser for 9-11 cycles by adjusting the power of the UV light to 3-5W, the laser frequency to 60KHz, and the laser pulse width to 10us. After all the contour cutting is completed, the polyurethane hot melt adhesive film is placed in a plasma cleaning machine for 2-3 minutes to clean the etching residues, and then the pre-designed flexible substrate shading structure is obtained.

[0082] The polyurethane hot melt adhesive film with laser etched shading was placed on a heating table and preheated at 70°C for 2-3 minutes. Then, the polyurethane hot melt adhesive film with laser etched shading was fixed to the screen printing table with tape, and the interdigital electrode screen was fixed on the top of the film. The prepared conductive ink was placed upside down on the screen and printed with a scraper at a 45° angle; the screen printing thickness was controlled to be 5-15um; and then the printed polyurethane hot melt adhesive film was placed on a heating table at 70°C for heating and curing for 5-10 minutes to obtain a cured base shading and an integrated structure of the interdigital electrode array (interdigital electrode layer).

[0083] S2, preparing the first insulating layer:

[0084] Place the cured polyurethane hot melt adhesive film electrode layer on the screen printing table, align the first insulating layer screen plate height and place it above the electrode layer film, invert the drying type insulating ink JC JY302 on the first insulating layer screen plate, and print the cross-finger electrode lead overlap at a 45-degree angle with a scraper. Then place the printed cross-finger electrode layer-first insulating layer film on a 70°C heating table and heat it for 5-10 minutes to obtain the cured electrode layer-first insulating layer film.

[0085] S3, preparation of electrode layer wires:

[0086] The solidified interdigitated electrode layer-first insulating layer film is placed on a screen printing table, the electrode layer wire screen is highly aligned and placed above the first insulating layer, the conductive ink is inverted on the electrode layer wire screen, and the scraper is tilted 45 degrees to print on the overlapping parts of the interdigitated electrode leads; then the printed interdigitated electrode layer-first insulating layer-electrode layer wire film is placed on a 70°C heating table and heated for 5-10 minutes to obtain a solidified electrode layer-first insulating layer-electrode layer wire film, thereby forming electrode interconnection.

[0087] S4, preparing a second insulating layer:

[0088] Place the solidified interdigitated electrode layer-first insulating layer-electrode layer wire film on the screen printing table, align the second insulating layer screen plate with the height above the film, invert the drying type insulating ink JC JY302 on the second insulating layer screen plate, and print with a squeegee at a 45-degree tilt. Then place the printed interdigitated electrode layer-first insulating layer-electrode layer wire-second insulating layer film on a 70°C heating table and heat for 5-10 minutes to obtain a solidified electrode layer-first insulating layer-electrode layer wire-second insulating layer film to prevent crosstalk between different layers.

[0089] S5, preparation of spacer layer:

[0090] Take a 20 ml glass bottle, add 3 g of thermoplastic polyurethane elastomer, then add 5 ml of N, N-dimethylformamide, put in magnetic beads, and stir thoroughly for 120 minutes at 100°C with a magnetic stirrer to obtain a spacer layer ink.

[0091] The cured electrode layer - first insulating layer - electrode layer wire - second insulating layer film is placed on the screen printing table, the spacer layer screen is highly aligned and placed above the film, the spacer layer ink is inverted on the spacer layer screen, and the scraper is tilted 45 degrees to print to obtain the electrode layer - first insulating layer - electrode layer wire - second insulating layer - spacer layer film.

[0092] S6, preparing the sensitive layer:

[0093] Take a 20ml glass bottle, add 2g of thermoplastic polyurethane elastomer, then add 5ml of N,N-dimethylformamide, put in magnetic beads, and stir them thoroughly at 100℃ for 60min using a magnetic stirrer. Add 0.5g of carbon nanotube powder while stirring, and continue stirring at 100℃ for 120min to obtain the sensitive layer ink.

[0094] Take a 10×20cm 2The polyurethane hot melt adhesive film with a size and thickness of 100μm is placed in a plasma cleaning machine for 2-3 minutes, and then placed on a heating table for preheating at 70℃ for 2-3 minutes. Then the polyurethane hot melt adhesive film is fixed to the screen printing table with tape, the sensitive layer screen is fixed on the top of the film, and the prepared sensitive layer ink is placed upside down on the screen, and printed with a scraper at a 45° angle. Then the printed sensitive layer film is placed on a 70℃ heating table for heating and curing for 5-10 minutes to obtain a cured sensitive layer.

[0095] Place the sensitive layer film on the platform below the UV laser machine, vacuum adsorb, input the pre-designed vertical grain structure contour, adjust the UV power to 3-5W, the laser frequency to 60KHz, and the laser pulse width to 10us for 20-25 cycles of cutting and laser etching. After all contour cutting is completed, place the polyurethane hot melt adhesive film in a plasma cleaning machine for 2-3 minutes to clean the etching residues, and then obtain the pre-designed sensitive layer film.

[0096] S7, sensor package:

[0097] The electrode layer - first insulating layer - electrode layer wire - second insulating layer - spacer layer film prepared by S5 are highly aligned and bonded with the sensitive layer film prepared by S6, placed in a vacuum heating box, evacuated, heated to 100°C for 60 minutes, and cooled to achieve flexible packaging, thus completing the preparation of the minimum port fork finger sensor array based on screen printing.

[0098] The interdigital sensor array prepared in this embodiment achieves shielding between the crossed electrodes by screen-printing insulating ink to avoid wire crossing, and is combined with the interdigital sensor to realize the rapid preparation of a flexible pressure sensor array. Due to the introduction of insulating ink at the intersection of the wires and the rationally designed structural configuration, the output ports of the sensor are greatly reduced from 17 to 8 to achieve electrical insulation and three-dimensional interconnection of the wire intersections. The electrode layer and the bottom TPU laser engraved shading and the sensitive layer microstructure are intertwined to form a stable "arch bridge" reinforcement structure. This overall reinforcement structure has a certain effect on the conductivity, stability and mechanical properties of the composite system. Compared with a single system, this improvement in mechanical properties and the conductive network of the point-line structure have higher perception sensitivity. Within a certain pressure range, the pressure perception range is improved, so that the sensor has high sensitivity and high stability.

[0099] Figure 8 The schematic diagram of the stretching and bending of the flexible interdigital pressure sensor array is shown, proving that the prepared sensor array has ultra-high flexibility. The present invention further structures the structure by laser engraving the surface of the electrode and the sensitive layer of the sensor, so that the sensitivity and stability are further improved. Fig. 9This is a test data diagram of the interdigital sensor array made by the present invention. The sensitivity of the sensor in the range of 0-15kPa is as high as 17433.3kPa -1 The sensitivity of the sensor in the range of 15-50kPa is up to 7644.5kPa -1 .

[0100] The present invention has been proven to be a simple method to reduce the number of electrical output ports of the interdigital electrodes of the flexible sensor array by screen-printing insulating ink at the cross-electrodes to achieve electrical shielding between the wires. It can be extended to the future for the manufacture of large-area flexible interdigital electrode sensor arrays, illuminating the research blind spot of printing fully flexible minimum-port interdigital sensors. The full screen printing process, the application of soft materials and the ultra-high sensor performance make the sensor show strong application potential in tactile perception and pulse detection.

[0101] Of course, the above description is only a preferred embodiment of the present invention, and does not limit the patent scope of the present invention. All equivalent structural changes made by using the contents of the present invention specification and drawings under the inventive concept of the present invention, or directly / indirectly used in other related technical fields are included in the patent protection scope of the present invention and should be protected by the present invention.

Claims

1. A method for preparing a minimum port interdigital sensor array based on screen printing, characterized in that The following steps are involved: S1, preparing an interdigitated electrode layer; Selecting a flexible substrate, and performing laser etching on the flexible substrate to obtain a flexible substrate with a shading structure; Screen printing a conductive ink on a flexible substrate with a textured structure to obtain an interdigitated electrode layer; S2, coating a first insulating layer; Screen printing insulating ink on the lead overlapped position on the interdigital electrode layer to form a first insulating layer, thereby obtaining an electrode layer-first insulating layer film; S3, coating electrode layer wire; Screen printing a conductive ink on the electrode layer-first insulating layer film obtained in S2 to form an electrode layer wire interconnecting the electrodes, thereby obtaining an electrode layer-first insulating layer-electrode layer wire film; S4, applying a second insulating layer; Screen-printing insulating ink on the electrode layer-first insulating layer-electrode layer wire film obtained in S3 to form a second insulating layer to prevent crosstalk, thereby obtaining an electrode layer-first insulating layer-electrode layer wire-second insulating layer film; S5, coating a spacer layer; Screen-printing the spacer layer ink on the electrode layer-first insulating layer-electrode layer wire-second insulating layer film obtained in S4 to form a spacer layer, thereby obtaining an electrode layer-first insulating layer-electrode layer wire-second insulating layer-spacer layer film; S6, preparing a sensitive layer; Select a flexible substrate, screen-print the sensitive layer ink on the flexible substrate, and then perform laser etching to obtain a sensitive layer; S7, sensor array packaging; The electrode layer-first insulating layer-electrode layer wire-second insulating layer-spacer layer film prepared in S5 is aligned and bonded with the sensitive layer prepared in S6, and then packaged to obtain a minimum port interdigital sensor array based on screen printing.

2. The method for preparing a minimum port interdigital sensor array based on screen printing according to claim 1, characterized in that: In step S1: The flexible substrate is made of a polyurethane hot melt adhesive film, which is first cleaned in a plasma cleaning machine, and then placed on a platform below an ultraviolet laser machine for vacuum adsorption, and then laser etching is performed; After the etching is completed, the polyurethane hot melt adhesive film is placed in a plasma cleaning machine to clean the etching residues, thereby obtaining a flexible substrate with a shading structure; The conductive ink is prepared by stirring slow-drying water and conductive silver paste and mixing them evenly; After the conductive ink is screen-printed on the flexible substrate, it is heated and cured to obtain an interdigitated electrode layer; Control the cleaning time of the plasma cleaning machine to 2-3 minutes; input the pre-designed vertical grain structure profile into the UV laser machine, adjust the UV light power to 3-5W, the laser frequency to 60KHz, the laser pulse width to 10us, and perform 9-11 cycles of cutting; control the heating and curing temperature to 70°C, and the heating and curing time to 5-10 minutes.

3. The method for preparing a minimum port interdigital sensor array based on screen printing according to claim 1, characterized in that: In step S2: place the interdigitated electrode layer on a screen printing table, align the first insulating layer screen and place it above the interdigitated electrode layer, invert the drying type insulating ink on the first insulating layer screen, and print it at an angle on the overlapping parts of the interdigitated electrode leads with a scraper; then place it on a 70°C heating table and heat it for 5-10 minutes, and after curing, obtain an electrode layer-first insulating layer film.

4. The method for preparing a minimum port interdigital sensor array based on screen printing according to claim 1, characterized in that: In step S3: the conductive ink is prepared by stirring slow-drying water and conductive silver paste and mixing them evenly; the cured electrode layer-first insulating layer film is placed on a screen printing table, the electrode layer wire screen is aligned and placed above the first insulating layer, the conductive ink is inverted on the electrode layer wire screen, and the scraper is tilted to print on the overlapping part of the interdigitated electrode leads; then it is placed on a 70°C heating table and heated for 5-10 minutes, and after curing, the electrode layer-first insulating layer-electrode layer wire film is obtained.

5. The method for preparing a minimum port interdigital sensor array based on screen printing according to claim 1, characterized in that: In step S4: the electrode layer-first insulating layer-electrode layer wire film obtained after curing is placed on the screen printing table, the second insulating layer screen is aligned and placed above the film, the drying type insulating ink is inverted on the second insulating layer screen, and the scraper is tilted for printing; then it is placed on a 70°C heating table and heated for 5-10 minutes, and the electrode layer-first insulating layer-electrode layer wire-second insulating layer film is obtained after curing.

6. The method for preparing a minimum port interdigital sensor array based on screen printing according to claim 1, characterized in that: In step S5: a thermoplastic polyurethane elastomer is mixed with N,N-dimethylformamide, and magnetically stirred to obtain a spacer layer ink; the electrode layer-first insulating layer-electrode layer wire-second insulating layer film obtained after curing is placed on a screen printing table, the spacer layer screen is aligned and placed above the film, the spacer layer ink is inverted on the spacer layer screen, and the scraper is tilted for printing to obtain an electrode layer-first insulating layer-electrode layer wire-second insulating layer-spacer layer film.

7. The method for preparing a minimum port interdigital sensor array based on screen printing according to claim 1, characterized in that: In step S6: thermoplastic polyurethane elastomer and N,N-dimethylformamide are mixed, magnetically stirred, and carbon nanotube powder is added in the stirring state to obtain sensitive layer ink; The flexible substrate is made of a polyurethane hot melt adhesive film, which is cleaned in a plasma cleaning machine and then preheated on a heating table. The polyurethane hot melt adhesive film is then fixed on a screen printing table, a sensitive layer screen is fixed above the film, and the sensitive layer ink is inverted on the sensitive layer screen. A scraper is used for tilted printing, and after printing is completed, the film is placed on a heating table for heating and curing. Then place the polyurethane hot melt adhesive film on the platform below the UV laser machine, vacuum adsorb it, and perform laser etching; After the etching is completed, it is placed in a plasma cleaning machine to clean the etching residues to obtain a sensitive layer; Control the cleaning time of the plasma cleaning machine to 2-3 minutes; the preheating temperature of the heating table is 70°C, and the preheating time is 2-3 minutes; control the heating and curing temperature to 70°C, and the heating and curing time is 5-10 minutes; input the pre-designed vertical grain structure profile into the UV laser machine, adjust the UV light power to 3-5W, the laser frequency to 60KHz, the laser pulse width to 10us, and perform 20-25 cycles of cutting.

8. The method for preparing a minimum port interdigital sensor array based on screen printing according to claim 1, characterized in that: In step S7: align and bond the electrode layer-first insulating layer-electrode layer wire-second insulating layer-spacer layer film prepared in S5 with the sensitive layer prepared in S6, place them in a vacuum heating box, evacuate the box, heat to 100-110°C, and heat at this temperature for 50-60 minutes, then cool to achieve flexible packaging.

9. A screen-printed minimum port interdigital sensor array prepared by the method of any one of claims 1 to 8, characterized in that: The interdigital sensor array comprises a sensitive layer, a spacer layer, a second insulating layer, an electrode layer wire, a first insulating layer and an interdigital electrode layer which are stacked in sequence from top to bottom; The interdigital electrode layer is an integrated structure formed by a first flexible substrate with a first shading structure and an interdigital electrode array screen-printed thereon; the first insulating layer covers the overlapping parts of the leads of the interdigital electrode array, the electrode layer wires are arranged above the first insulating layer, the overlapping parts of the leads of the interdigital electrode array are separated from the electrode layer wires by the first insulating layer, and the electrode layer wires are connected to the interdigital electrode array; The second insulating layer covers the first flexible substrate, and an array through hole is provided at a position on the second insulating layer directly facing the interdigital electrode array; The spacing layer comprises an outer frame, and spacing bars are arranged in an inner space formed by the outer frame, the spacing bars are located at the gaps facing the interdigital electrode array, and the spacing bars comprise a plurality of segments; The sensitive layer comprises a second flexible substrate, on which a sensitive region array is arranged, the sensitive region array is located directly above the interdigital electrode array, and a second shading structure is etched on the sensitive region array.

10. The screen-printed minimum port interdigital sensor array according to claim 9, characterized in that: When preparing the interdigital electrode layer, a first shading structure is etched on one side of the first flexible substrate, and an interdigital electrode array is screen-printed on the first shading structure; and the extension direction of the first shading structure is perpendicular to the interdigital direction of the interdigital electrode array; When preparing the sensitive layer, a sensitive area array is screen-printed on one side of the second flexible substrate, and then a second shading structure is etched on the sensitive area array, wherein the extension direction of the second shading structure is the same as that of the first shading structure; When the sensor array is packaged, the second flexible substrate is inverted on top of the first flexible substrate, and the sensitive area array and the interdigital electrode array are arranged facing each other.

Citation Information

Patent Citations

  • Large area array separated pressure sensor, preparation method thereof, waterborne conductive slurry and preparation method thereof

    CN110108394A

  • Interdigital large-area flexible array sensor and preparation method thereof

    CN110333010A

  • Flexible pressure sensor for monitoring pulse waves and preparation method thereof

    CN115024698A

  • Composite structure for a pressure sensor and pressure sensor

    US20220299385A1

Cited By

  • Strain isolation type flexible temperature gradient sensor array and preparation method thereof

    CN122408988A

  • Strain-isolated flexible temperature gradient sensor array and method of manufacturing the same

    CN122408988B