Circuit wiring manufacturing method and printed circuit board

By using the through holes of the mask plate in the production of printed circuit boards, and combining electroplating and screen printing processes, the problem of insufficient circuit wiring accuracy in the prior art is solved, and higher accuracy and Reliable circuit wiring improves the performance of the printed circuit board.

CN118946022APending Publication Date: 2024-11-12SUZHOU GUOXIAN INNOVATION TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411206819.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-30
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

When making printed circuit boards and integrated circuit carrier boards, the production accuracy of circuit traces is limited, resulting in performance improvement. Especially in the production of high-density interconnection boards, line width and line distance are difficult. Accurate control makes it easy to cause the side wall inclination angle not close to 90 degrees, resulting in circuit breakage and reliability problems.

Method used

The patterned trace layer is prepared using the through holes of the mask plate, and the seed layer between the patterned trace layer and the substrate is patterned. The cross-sectional shape of the trace layer is controlled by using different opening widths and shapes of the through holes. Combining electroplating and screen printing processes, improve the accuracy and reliability of circuit wiring.

Benefits of technology

It realizes higher precision circuit wiring production, reduces the risk of wiring circuit breakers, improves the performance and reliability of printed circuit boards, and has a more efficient process flow, reducing the waste of photoresist materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118946022A_ABST
    Figure CN118946022A_ABST
Patent Text Reader

Abstract

The invention discloses a circuit wiring manufacturing method and a printed circuit board. The circuit wiring manufacturing method comprises the following steps: preparing a seed layer on one side of a substrate; arranging a mask plate on one side, far away from the substrate, of the seed layer, wherein the mask plate comprises a first surface, a second surface and a through hole, preparing a patterned wiring layer on one side, far away from the substrate, of the seed layer through the mask plate, and limiting the line spacing or line width of the patterned wiring layer through the through holes; and performing patterning processing on a part of the seed layer exposed between the patterned wiring layers to form a patterned seed layer, thereby obtaining the circuit wiring. According to the circuit wiring manufacturing method and the printed circuit board provided by the embodiment of the invention, the graphical wiring layers are prepared by using the through holes of the mask, and the circuit wiring is obtained by performing graphical processing on the part, exposed between the graphical wiring layers, of the seed layer prepared between the graphical wiring layers and the substrate in advance. The circuit wiring with higher precision can be manufactured, and the use performance of the printed circuit board is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of chip packaging technology, and in particular to a circuit routing manufacturing method and a printed circuit board. Background Art

[0002] Semi-Additive Process (SAP) is a common process for manufacturing integrated circuit substrates (IC) and printed circuit boards (PCB) for packaging and testing of integrated circuits. However, the current PCB boards or IC substrates have limited circuit routing accuracy and their performance needs to be improved. Summary of the invention

[0003] The embodiments of the present application provide a circuit routing manufacturing method and a printed circuit board, which can improve the manufacturing accuracy of the circuit routing on the printed circuit board, thereby improving the performance of the printed circuit board.

[0004] In a first aspect, a circuit routing manufacturing method is provided according to an embodiment of the present application, comprising:

[0005] preparing a seed layer on one side of the substrate;

[0006] A mask is arranged on a side of the seed layer away from the substrate, wherein the mask comprises a first surface and a second surface arranged opposite to each other and at least one through hole penetrating the first surface and the second surface;

[0007] A patterned wiring layer is prepared on a side of the seed layer away from the substrate by using a mask, and a line pitch or line width of the patterned wiring layer is limited by using through holes;

[0008] The exposed portion of the seed layer between the patterned wiring layers is patterned to form a patterned seed layer to obtain a circuit wiring. The circuit wiring includes a patterned seed layer and a patterned wiring layer stacked in sequence in a direction away from the substrate.

[0009] According to one aspect of an embodiment of the present application, in the step of setting a mask on the side of the seed layer away from the substrate, the width of the first opening of the through hole located on the first surface is greater than the width of the second opening of the through hole located on the second surface.

[0010] According to one aspect of the embodiment of the present application, the opening width of the cross section of the through hole gradually decreases along the direction from the first surface to the second surface.

[0011] According to one aspect of the embodiments of the present application, the mask is a glass mask.

[0012] According to one aspect of an embodiment of the present application, in the step of setting a mask on the side of the seed layer away from the substrate, the first surface of the mask is located on the side of the seed layer away from the substrate, and the first opening is located on the side of the second opening close to the seed layer.

[0013] According to one aspect of an embodiment of the present application, the step of preparing a patterned wiring layer on a side of the seed layer away from the substrate through a mask further includes:

[0014] Preparing a routing layer in the through hole;

[0015] Remove the mask to obtain the patterned routing layer.

[0016] According to one aspect of an embodiment of the present application, the step of preparing the routing layer further includes:

[0017] The routing layer includes metal material, and the routing layer is prepared in the through hole by using an electroplating process.

[0018] According to one aspect of an embodiment of the present application, the routing layer includes at least one material of copper, aluminum, and tin.

[0019] According to one aspect of the embodiment of the present application, the step of removing the mask further includes:

[0020] The mask is removed along the mask thickness direction.

[0021] According to one aspect of an embodiment of the present application, in the step of setting a mask on the side of the seed layer away from the substrate, the second surface of the mask is located on the side of the seed layer away from the substrate, and the second opening is located on the side of the first opening close to the seed layer.

[0022] According to one aspect of an embodiment of the present application, the step of preparing a patterned wiring layer on a side of the seed layer away from the substrate through a mask further includes:

[0023] preparing an insulating layer on a side of the mask away from the seed layer;

[0024] removing the mask to obtain a patterned insulating layer;

[0025] preparing a wiring layer between the patterned insulating layers;

[0026] The patterned insulating layer is removed to obtain a patterned wiring layer.

[0027] According to one aspect of an embodiment of the present application, the step of preparing the insulating layer also includes: the insulating layer is an insulating material, and the insulating layer is prepared by a screen printing process.

[0028] According to one aspect of an embodiment of the present application, the step of preparing a routing layer further includes: the routing layer includes a metal material, and the routing layer is prepared by an electroplating process.

[0029] According to one aspect of an embodiment of the present application, the routing layer includes at least one material of copper, aluminum, and tin.

[0030] According to one aspect of an embodiment of the present application, the step of patterning the portion of the seed layer exposed between the patterned wiring layers further includes: etching the seed layer using a wet etching process.

[0031] According to one aspect of an embodiment of the present application, the step of preparing a seed layer on one side of the substrate also includes: the seed layer is prepared using at least one of copper, nickel, chromium, gold and silver.

[0032] According to one aspect of an embodiment of the present application, before the step of setting a mask on a side of the seed layer away from the substrate, the step further includes:

[0033] Through holes are prepared on the substrate to obtain a mask.

[0034] According to one aspect of an embodiment of the present application, the step of preparing a through hole on a substrate further includes: inducing denaturation of a partial area of ​​the substrate using a laser induced process; and etching the substrate using a wet etching process to form a through hole.

[0035] According to one aspect of an embodiment of the present application, in the step of preparing a through hole on a substrate, a first opening width and a second opening width of a cross section of the through hole do not exceed 5 μm.

[0036] In a second aspect, according to an embodiment of the present application, a printed circuit board is provided, comprising a circuit trace manufactured by the circuit trace manufacturing method provided by any one of the embodiments of the first aspect.

[0037] In the third aspect, according to an embodiment of the present application, a printed circuit board is also provided, comprising: a substrate; a circuit routing, arranged on one side of the substrate; the circuit routing comprises a patterned seed layer and a patterned routing layer stacked in sequence in a direction away from the substrate, the cross-sectional shape of the circuit routing along its own thickness direction comprises a first cross-sectional shape formed in sequence in the patterned seed layer and a second cross-sectional shape formed in the patterned routing layer, the width of the second cross-sectional shape on a side close to the first cross-sectional shape is greater than the width of the second cross-sectional shape on a side away from the first cross-sectional shape, and the width of the first cross-sectional shape is greater than or equal to the width of the second cross-sectional shape.

[0038] According to one aspect of the embodiment of the present application, the width of the second cross section decreases in a direction away from the substrate.

[0039] According to one aspect of the embodiment of the present application, the width of the second cross section is W, where W≠0.

[0040] According to one aspect of an embodiment of the present application, the patterned routing layer includes a metal material.

[0041] According to one aspect of an embodiment of the present application, the patterned routing layer includes at least one material of copper, aluminum, and tin.

[0042] According to one aspect of the embodiments of the present application, the line width or line spacing of the patterned routing layer does not exceed 5 μm.

[0043] According to one aspect of an embodiment of the present application, the seed layer is prepared from a material including at least one of copper, nickel, chromium, gold and silver.

[0044] According to one aspect of the embodiment of the present application, the width of the first cross section gradually increases in a direction away from the second cross section.

[0045] According to one aspect of the embodiment of the present application, the side inclination angle of the first cross section is less than or equal to the side inclination angle of the second cross section.

[0046] The circuit routing production method and printed circuit board provided in the embodiments of the present application use the through holes of a mask plate to prepare a patterned routing layer, and pattern the portion of a seed layer pre-prepared between the patterned routing layer and the substrate exposed between the patterned routing layer to obtain circuit routing, which can produce higher-precision circuit routing while improving the performance of the printed circuit board. BRIEF DESCRIPTION OF THE DRAWINGS

[0047] The features, advantages and technical effects of exemplary embodiments of the present application will be described below with reference to the accompanying drawings.

[0048] Figure 1 It is a flow chart of a circuit routing manufacturing method provided in an embodiment of the present application;

[0049] Figure 2a to Figure 2c It is a schematic diagram of the process steps of a circuit routing manufacturing method provided in an embodiment of the present application;

[0050] Figure 3 It is a schematic diagram of the process steps of another circuit routing manufacturing method provided in an embodiment of the present application;

[0051] Figure 4 It is a flow chart of another circuit routing manufacturing method provided in an embodiment of the present application;

[0052] Figure 5a to Figure 5c It is a schematic diagram of the process steps of another circuit routing manufacturing method provided in an embodiment of the present application;

[0053] Figure 6 It is a schematic diagram of the process steps of another circuit routing manufacturing method provided in an embodiment of the present application;

[0054] Figure 7 It is a flow chart of another circuit routing manufacturing method provided in an embodiment of the present application;

[0055] Figures 8a to 8dIt is a schematic diagram of the process steps of another circuit routing manufacturing method provided in an embodiment of the present application;

[0056] Fig. 9 It is a schematic diagram of a stacked structure of a printed circuit board provided in an embodiment of the present application;

[0057] Fig.10 It is a schematic diagram of the stacking structure of another printed circuit board provided in an embodiment of the present application.

[0058] in:

[0059] 10-substrate;

[0060] 20-seed layer; 20'-patterned seed layer;

[0061] 30-mask; 31-first surface; 32-second surface;

[0062] 34-through hole; 341-first opening; 342-second opening;

[0063] 40-wiring layer; 40'-graphical wiring layer;

[0064] 50-circuit routing; 51-first cross section; 52-second cross section;

[0065] 60-insulating layer; 60'-patterned insulating layer;

[0066] 100-Printed Circuit Board.

[0067] In the drawings, the same reference numerals are used for the same components. The drawings are not drawn to scale. DETAILED DESCRIPTION

[0068] The features and exemplary embodiments of various aspects of the present application will be described in detail below. In the detailed description below, many specific details are proposed to provide a comprehensive understanding of the present application. However, it is obvious to those skilled in the art that the present application can be implemented without the need for some of these specific details. The following description of the embodiments is only to provide a better understanding of the present application by illustrating examples of the present application. In the accompanying drawings and the following description, at least some of the known structures and technologies are not shown to avoid unnecessary ambiguity in the understanding of the key points of the content of the present application; and, for clarity, the size of some structures may be exaggerated. In addition, the features, structures or characteristics described below may be combined in one or more embodiments in any suitable manner.

[0069] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply that there is any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variant thereof are intended to cover non-exclusive inclusion, so that the process, method, article or equipment including a series of elements not only includes those elements, but also includes other elements not clearly listed, or also includes elements inherent to such process, method, article or equipment. In the absence of more restrictions, the elements limited by the sentence "comprise..." do not exclude the existence of other identical elements in the process, method, article or equipment including the elements.

[0070] The directional words appearing in the following description are all directions shown in the figure, and do not limit the specific structure of the printed circuit board of this application. In the description of this application, it should also be noted that, unless otherwise clearly specified and limited, the terms "set" and "connect" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be directly connected or indirectly connected. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to the specific circumstances.

[0071] In the related art, the SAP process for manufacturing IC carriers and PCBs forms a circuit pattern on the surface of a substrate. The SAP process is also used in the manufacturing process of high-density interconnects (HDI).

[0072] Among them, the manufacturing step of forming the circuit pattern uses a windowed photoresist as a shielding pattern, and the material is deposited on the surface of the seed layer exposed by the window of the photoresist to form a metal layer constituting the routing.

[0073] The main production process of window photoresist used in SAP process is to adopt laser direct etching process (Laser Direct Imaging, LDI), that is, a laser beam controlled by a computing device is directly exposed on the photoresist material coated on the surface of the substrate, without using a traditional mask. A window can be formed on the surface of the photoresist by laser etching, and the window pattern is the pattern of the required routing loop.

[0074] However, due to the limitations of photoresist materials and LDI manufacturing process, the routing line width or line spacing manufacturing accuracy of the windowed photoresist made by the LDI process needs to be improved. In addition, due to the difference in light intensity of the laser light source irradiating the photoresist on the side close to the laser light source and the side far from the laser light source, when the LDI process is used to etch the photoresist to form a window pattern, the inclination angle of the side wall of the photoresist window is difficult to control to close to 90°, that is, the angle between the side wall of the photoresist window and the surface of the photoresist close to the seed layer is always less than 90°.

[0075] In the SAP process using windowed photoresist as a mask, the line width of the routing or the line spacing between routings has limited manufacturing accuracy, and the cross-sectional shape of the routing is an inverted trapezoidal shape that is narrower on the side close to the seed layer and wider on the side away from the seed layer. When the exposed portion of the seed layer between the routings is subsequently etched, side etching problems are likely to occur on the side of the routing close to the seed layer, resulting in the risk of routing breakage and reliability issues.

[0076] Based on the consideration and technical needs for solving the above-mentioned problems, the present application proposes a circuit routing manufacturing method and a printed circuit board.

[0077] In order to better understand this application, Figure 1 and Figure 2a to Figure 2c The circuit routing manufacturing method of the embodiment of the present application is described in detail.

[0078] See also Figure 1 In a first aspect, an embodiment of the present application provides a circuit routing manufacturing method, the circuit routing manufacturing method comprising:

[0079] Step S100, see Figure 2a , preparing a seed layer 20 on one side of the substrate 10;

[0080] Step S200, see Figure 2b , a mask 30 is disposed on a side of the seed layer 20 away from the substrate 10, the mask 30 includes a first surface 31 and a second surface 32 that are oppositely disposed and at least one through hole 34 that penetrates the first surface 31 and the second surface 32;

[0081] Step S300, preparing a patterned wiring layer 40' on the side of the seed layer 20 away from the substrate by using a mask plate 30, and using the through hole 34 to limit the line pitch or line width of the patterned wiring layer 40';

[0082] Step 300, see Figure 2c The exposed portion of the seed layer 20 between the patterned wiring layer 40' is patterned to form a patterned seed layer 20', thereby obtaining a circuit wiring 50, which includes a patterned seed layer 20' and a patterned wiring layer 40' stacked in sequence in a direction away from the substrate 10.

[0083] The method for manufacturing the circuit trace 50 provided in the embodiment of the present application uses the through hole 34 of the mask plate 30 to prepare the patterned trace layer 40', and the seed layer 20 pre-prepared between the patterned trace layer 40' and the substrate 10 is patterned to obtain the circuit trace 50. While manufacturing a higher-precision circuit trace 50, the performance of the printed circuit board 100 can be improved.

[0084] See also Figure 2a The substrate 10 is mainly made of inorganic materials, usually composed of one or more materials selected from glass, ceramics, synthetic polymer resins and reinforcing materials, and plays an insulating role.

[0085] The main function of the substrate 10 is to provide mechanical support and electrical connection carrier for electronic components, and at the same time, as an insulating medium, ensure the stability and safety of the circuit. In addition, the material of the substrate 10 also affects the electrical characteristics, mechanical strength and thermal stability of the circuit board.

[0086] The seed layer 20 is a material layer used in the thin film growth process, and its main functions include improving the interface characteristics between the thin film and the substrate and serving as a conductive layer in the electroplating process. The material selection of the seed layer 20 depends on the properties of the target thin film material and the desired application.

[0087] For example, during the physical vapor deposition (PVD) process of the patterned wiring layer 40', the seed layer 20 can prevent the metal material from diffusing into the substrate 10, while improving the conductivity of the circuit wiring 50. In addition, during the electroplating process preparation of the patterned wiring layer 40', the seed layer 20 improves the microtexture and surface morphology of the film by controlling the grain orientation and adjusting the interface structure. During the electroplating process, the seed layer 20 acts as a thin metal film and provides the necessary conductivity to promote metal deposition.

[0088] Therefore, a thin metal film is usually prepared on one side of the substrate 10 by electroplating as a seed layer 20, which is beneficial to improve the adhesion efficiency of metal deposition during the subsequent electroplating of metal material routing. The seed layer 20 is usually prepared on one side of the substrate 10 by electroplating on the entire surface of the substrate 10. After the patterned routing layer 40' is prepared, the portion of the seed layer 20 exposed between the patterned routing layers 40' needs to be removed by an additional preparation process to form the final circuit routing 50.

[0089] The mask 30 with the through holes 34 is also used as a substrate in three-dimensional packaging, that is, as a substrate for high-density chip packaging in the through glass via technology (TGV) or through silicon via technology (TSV).

[0090] The glass substrate used in TGV technology or the silicon substrate used in TSV technology has good electrical, thermal and mechanical properties, which makes it have unique advantages in the fields of radio frequency chips, high-end sensors, high-density system integration, etc. Using the glass substrate or silicon substrate as a mask 30 for the production process of high-density routing of IC carriers, PCB boards, HDI boards, etc. also has a unique effect.

[0091] See also Figure 2b The through holes 34 formed on the mask 30 are usually tiny through holes 34 that penetrate vertically.

[0092] The mask 30 can be recycled and reused in the entire process of manufacturing the circuit wiring 50. In the related art, a pattern defining the patterned wiring layer 40' is formed by using a photoresist through a laser direct writing exposure process. Before each patterned wiring layer 40' is manufactured, the photoresist coated on the substrate 10 needs to be exposed and developed through a light shield to obtain the required photoresist pattern of the patterned wiring layer 40'; after the patterned wiring layer 40' is manufactured, the photoresist will be cleaned and removed. Each time the patterned wiring layer 40' is manufactured, the photoresist needs to be re-manufactured, which reduces the work efficiency and causes waste of photoresist materials.

[0093] By using the mask 30 , the shape of the through hole 34 can be changed by adjusting the formation process of the through hole 34 , so that the cross-sectional shape of the patterned wiring layer 40 ′ after formation can be controlled with higher precision.

[0094] In the related art, the tilt angle of the photoresist cannot be close to 90°, and the cross-sectional shape of the patterned wiring layer 40 ′ can only be an inverted trapezoidal shape, which is prone to side etching and circuit breaking in the subsequent preparation process step of removing part of the seed layer 20 .

[0095] By using the mask 30, the width of the through hole 34 or the distance between the through holes 34 can be smaller, so that the line spacing between the patterned wiring layers 40' or the line width of the patterned wiring layers 40' can be controlled more finely and with higher precision. In the related art, photoresist is used as the shielding pattern, and the cross-sectional width of the window of the photoresist is large, so the line spacing or line width precision between the patterned wiring layers 40' is limited.

[0096] A patterned wiring layer 40 ′ is formed on the side of the seed layer 20 away from the substrate 10 through a mask 30 . The pattern on the mask 30 can be set to a wiring-shaped pattern or a negative wiring-shaped pattern.

[0097] The negative pattern here should be understood as the pattern prepared by the mask 30, and the pattern of the wiring shape is the part that passes through or is recessed in the pattern prepared by the mask 30. In the subsequent process, the patterned wiring layer 40' is further prepared by the pattern prepared by the mask 30, and the aperture of the through hole 34 of the mask 30 actually determines the distance between the wirings of the patterned wiring layer 40'.

[0098] Therefore, in some optional embodiments, the line width of the wiring of the patterned wiring layer 40 ′ is defined by the aperture of the through hole.

[0099] In some other optional embodiments, the line spacing between the routing lines of the patterned routing layer is defined by the aperture of the through hole.

[0100] See also Figure 2c After the patterned wiring layer 40' is formed on the seed layer 20 through the through hole 34 of the glass mask 30, since the seed layer 20 is formed by electroplating on the entire surface during preparation, the exposed portion of the seed layer 20 between the patterned wiring layers 40' will still form multiple electrical connections for the entire circuit wiring 50, causing the circuit wiring 50 to be short-circuited and unable to be used normally. The seed layer 20 is patterned to obtain the patterned seed layer 20' from the exposed portion of the seed layer 20 between the patterned wiring layers 40'.

[0101] The patterned seed layer 20 ′ and the patterned wiring layer 40 ′ are stacked to form the final circuit wiring 50 .

[0102] In some embodiments, step S200 further includes:

[0103] See also Figure 3 The through hole 34 includes a first opening 341 located on the first surface 31 and a second opening 342 located on the second surface 32 , and a width of the first opening 341 is greater than a width of the second opening 342 .

[0104] In these embodiments, by setting the first opening 341 of the through hole 34 on the first surface 31 and the second opening 342 of the second surface 32 to different sizes, the width of the cross-sectional area of ​​the patterned wiring layer 40' formed by the mask plate 30 on the side close to the first surface 31 and the width of the cross-sectional area of ​​the wiring on the side close to the second surface 32 can be controlled respectively, thereby producing a circuit wiring 50 with higher precision.

[0105] Optionally, in the process of preparing the through hole 34 of the mask 30, the size and position of the first opening 341 may be preliminarily defined on the first surface 31, and the size and position of the second opening 342 may be defined on the second surface 32, and finally the first opening 341 and the second opening 342 may be connected to form the through hole 34. Optionally, the process of preparing the through hole 34 in the embodiment of the present application is not limited thereto, and the above description does not constitute a limitation on the process of preparing the through hole 34 in the embodiment of the present application.

[0106] In some optional embodiments, step S200 further includes:

[0107] See also Figure 3 The opening width of the cross section of the through hole 34 gradually decreases along the direction from the first surface 31 to the second surface 32 .

[0108] In these optional embodiments, the cross-section of the through hole 34 is a trapezoid, which can control the cross-section of the patterned wiring layer 40 ′ formed by the mask 30 to also be a trapezoid, thereby manufacturing a circuit wiring 50 with higher precision.

[0109] Optionally, after the first opening 341 and the second opening 342 are connected to form the through hole 34, the inner wall of the through hole 34 needs to be polished or cleaned to ensure that the opening width gradually decreases from the first surface 31 to the second surface 32, so that the cross-section of the through hole 34 is a trapezoid. Optionally, the process for preparing the through hole 34 in the embodiment of the present application is not limited thereto, and the above description does not constitute a limitation on the process for preparing the through hole 34 in the embodiment of the present application.

[0110] In some optional embodiments, step S200 further includes:

[0111] The mask 30 is a glass mask.

[0112] In these optional embodiments, the mask 30 is configured as a glass mask, which is less susceptible to wear and tear during continuous process steps, thereby saving costs.

[0113] In some embodiments, step S200 further includes:

[0114] See also Figure 3 The first surface 31 of the mask 30 is located on the side of the seed layer 20 away from the substrate 10 , and the first opening 341 is located on the side of the second opening 342 close to the seed layer 20 .

[0115] In these embodiments, the first surface 31 is arranged in contact with the seed layer 20, that is, in a direction perpendicular to the substrate, the cross-section of the through hole 34 is a right trapezoid, and the patterned routing layer 40' can be directly prepared in the through hole 34 to form a routing with a wider cross-sectional width close to one side of the seed layer 20, thereby preventing the patterned routing layer 40' side from being cut into a short circuit in the subsequent process steps of patterning part of the seed layer 20.

[0116] See also Figure 4 In some optional embodiments, step S200 further includes:

[0117] Step S210, see Figure 5a , preparing a wiring layer 40 in the through hole 34;

[0118] Step S220, see Figure 5b , remove the mask 30 to obtain a patterned wiring layer 40'.

[0119] In these optional embodiments, after the patterned wiring layer 40' is directly grown from the portion of the seed layer 20 defined by the through hole 34 to form the wiring layer, the mask 30 is removed to obtain the patterned wiring layer 40'. The position and shape of the patterned wiring layer 40' are defined by the through hole 34, and the width of the patterned wiring layer 40' close to the first surface 31 is greater than the width close to the second surface 32, so as to prevent the patterned wiring layer 40' from being cut into the side to cause a circuit break during the process step of patterning the portion of the seed layer 20.

[0120] The preparation of the routing layer 40 in the through hole 34 should be understood as follows: the seed layer 20 defines a portion of the seed layer 20 exposed by the through hole 34 through the through hole 34, and the routing layer 40 grows on these portions of the seed layer 20, so the routing layer 40 is gradually formed in a direction from the side of the seed layer 20 away from the substrate 10 to the direction away from the substrate 10.

[0121] In some optional embodiments, step S200 further includes:

[0122] The wiring layer 40 includes a metal material and is prepared in the through hole 34 by using an electroplating process.

[0123] In these optional embodiments, the routing layer 40 of the metal material can be deposited layer by layer on the portion of the seed layer 20 defined in the through hole 34 by using an electroplating process, and after removing the mask 30 , a patterned routing layer 40 ′ is finally formed.

[0124] The electroplating process is a surface treatment technology that is mainly based on the electrolysis process. The metal ions are reduced from the electrolyte solution by electric current and deposited on the surface of the workpiece as the cathode to form a metal film.

[0125] The main principle of applying the electroplating process to prepare the wiring layer 40 of the metal material in the through hole 34 is to form a metal layer on the seed layer 20 on the substrate 10 using the principle of electrolytic deposition. This process involves using the seed layer 20 as a cathode and the wiring layer 40 of the metal material as an anode, both of which are immersed in an electroplating solution containing metal ions as the material of the wiring layer 40. By applying an electric current, the metal of the anode dissolves into ions and enters the electroplating solution, and then is reduced and deposited into a metal layer on the surface of the seed layer 20 as the cathode, forming the wiring layer 40.

[0126] Therefore, the routing layer 40 is prepared and formed in the through hole 34 , and is directly deposited on the portion of the seed layer 20 exposed by the through hole 34 and is deposited layer by layer to form the routing layer 40 .

[0127] In some optional embodiments, step S200 further includes:

[0128] The wiring layer 40 includes at least one material of copper, aluminum, and tin.

[0129] In some optional embodiments, step S220 further includes:

[0130] See also Figure 5c , remove the glass mask 30 along the thickness direction of the mask 30.

[0131] In these optional embodiments, by removing the mask 30 along the thickness direction of the mask 30 , the shape of the routing layer 40 formed in the through hole 34 is not affected.

[0132] In the step of removing the mask 30, since the first surface 31 of the mask 30 is arranged in contact with the seed layer 20, the cross-section of the through hole 34 is a regular trapezoid. Therefore, in the step of removing the mask 30 along the thickness direction of the mask 30, the inner wall of the through hole 34 of the mask 30 and the wiring layer 40 formed in the through hole 34 do not interfere with each other, and removing the glass mask 30 does not affect the shape of the wiring layer 40.

[0133] In some embodiments, step 200 further includes:

[0134] See also Figure 6 The second surface 32 of the mask 30 is located on the side of the seed layer 20 away from the substrate 10 , and the second opening 342 is located on the side of the first opening 341 close to the seed layer 20 .

[0135] In these embodiments, the second surface 32 is arranged to fit the seed layer 20, that is, the shape of the through hole 34 is an inverted trapezoid in the cross-sectional direction from the substrate 10 in the downward direction, and the patterned routing layer 40' can be prepared on the side of the mask 30 away from the substrate 10 and prepared between the insulating layers whose cross-sectional shape is an inverted trapezoid limited by the through hole 34 of the mask 30, so that a routing with a wider cross-sectional width close to the side of the seed layer 20 can be obtained, thereby preventing the patterned routing layer 40' side from being engraved to cause a short circuit in the subsequent process steps of patterning the seed layer 20.

[0136] See also Figure 7 In some optional embodiments, step S200 further includes:

[0137] Step S230, see Figure 8a , preparing an insulating layer 60 on a side of the mask 30 away from the seed layer 20;

[0138] Step S240, see Figure 8b , removing the mask 30 to obtain a patterned insulating layer 60';

[0139] Step S250, see Figure 8c , preparing a wiring layer 40 between the patterned insulating layers 60';

[0140] Step S260, see Figure 8d , remove the patterned insulating layer 60' to obtain the patterned wiring layer 40'.

[0141] In these optional embodiments, an insulating layer 60 is prepared on the side of the mask 30 facing away from the substrate 10 through the through hole 34 of the mask 30 , and a wiring layer 40 of a desired shape is prepared using the insulating layer 60 .

[0142] The wiring layer 40 is indirectly prepared using the insulating layer 60. In the entire process of manufacturing the circuit wiring 50, the mask 30 can be recycled and reused. At the same time, the preparation of the insulating layer 60 does not require process steps such as coating, exposure, and development. The use of the mask 30 can simplify the process.

[0143] The patterned insulating layer 60' is formed by the shape of the through hole 34. The cross-sectional shape of the patterned insulating layer 60' is narrower on the side close to the substrate 10, and the cross-sectional shape defined between the patterned insulating layers 60' is wider on the side close to the seed layer 20. The routing layer 40 is made between the patterned insulating layers 60', so that a routing with a wider cross-sectional width close to the seed layer 20 can be obtained, thereby preventing the patterned routing layer 40' side from being engraved into a circuit break in the subsequent process steps of patterning part of the seed layer 20.

[0144] In some optional embodiments, step S230 further includes:

[0145] The insulating layer 60 is made of insulating material and is prepared by a screen printing process.

[0146] In these optional embodiments, an insulating layer 60 is prepared on the side of the mask 30 facing away from the substrate 10, and the insulating material for preparing the insulating layer 60 is coated on the side of the glass mask 30 facing away from the substrate 10 through a screen printing process. The insulating material is limited to form a specific shape by the through holes 34 in the mask 30, and the required patterned insulating layer 60' is obtained after removing the mask 30. The process is simple and the cost is low.

[0147] The screen printing process uses the mesh structure that constitutes the pattern part of the screen to allow the slurry to pass through, while the mesh of the non-pattern part is impermeable to the slurry. During the printing process, the slurry is squeezed through the mesh of the screen onto the substrate to form the desired shape pattern.

[0148] The advantage of screen printing technology is that it can easily achieve high-precision printing. Screen printing has good coverage and ink layer thickness, and can provide high-precision pattern shapes. It also has wide adaptability, is suitable for substrates of different shapes and sizes, has flexible and diverse operations, is easy to make plates and has low costs. Screen printing technology is widely used in the printing process of resists, solder resists, etc. due to its high precision and cost-effectiveness.

[0149] The screen printing process is used to prepare the insulating layer using the mask 30 , which can form the required pattern of the graphic insulating layer 60 ′ with high precision and has low cost, and is suitable for rapid preparation of the insulating layer 60 .

[0150] In some optional embodiments, step S250 further includes:

[0151] The wiring layer 40 is made of metal material and is prepared by an electroplating process.

[0152] In these optional embodiments, the routing layer 40 of metal material can be deposited layer by layer on the portion of the seed layer 20 defined between the patterned insulating layers 60' by electroplating process, and finally the patterned insulating layer 60' is removed to form the patterned routing layer 40'.

[0153] In some optional embodiments, step S250 further includes:

[0154] The wiring layer 40 includes at least one material of copper, aluminum, and tin.

[0155] Regarding step S240 , optionally, the mask 30 is removed along a thickness direction of the mask 30 .

[0156] The mask plate 30 is directly removed along the thickness direction of the mask plate 30 , and the process steps are simple.

[0157] Optionally, the through hole 34 connects at least one side surface of the mask 30 .

[0158] The through hole 34 not only penetrates and connects the first surface 31 and the second surface 32 of the mask 30, but also connects at least one side surface of the mask 30, so that when the mask 30 is removed, the through hole 34 on the mask 30 and the graphic shape of the patterned insulating layer 60' formed in the through hole 34 will not interfere with each other.

[0159] Optionally, the mask 30 is removed in a direction perpendicular to the side surface.

[0160] Removing the mask 30 in a direction perpendicular to the side surface can allow the patterned insulating layer 60' to escape from the opening on the side where the through hole 34 is connected to the side surface, and the mask 30 can be pulled out of the patterned insulating layer 60'. The through hole 34 of the mask 30 and the patterned insulating layer 60' will not interfere with each other to cause the cross-sectional shape of the patterned insulating layer 60' to be destroyed.

[0161] In the step of removing the mask 30, since the second surface 32 of the mask 30 is arranged in contact with the seed layer 20, the cross-sectional shape of the through hole 34 is an inverted trapezoid. Therefore, in the step of removing the mask 30 along the thickness direction of the mask 30, if the mask 30 is removed along the thickness direction of the mask 30, the inner wall of the through hole 34 of the mask 30 and the patterned insulating layer 60' formed in the through hole 34 may interfere with each other, causing the cross-sectional shape of part of the patterned insulating layer 60' to be destroyed.

[0162] Therefore, when the through hole 34 is connected to at least one side surface of the mask 30, by removing the patterned insulating layer 60' from the opening on the side where the through hole 34 is connected to the side surface, removing the mask 30 will not affect the cross-sectional shape of the patterned insulating layer 60', and will not affect the shape of the patterned routing layer 40' subsequently formed between the patterned insulating layers 60'.

[0163] Optionally, the glass mask 30 includes a first sub-mask and a second sub-mask, and the through hole 34 includes a first sub-through hole and a second sub-through hole, the first sub-through hole connects at least one first side surface of the first sub-mask, and the second sub-through hole connects at least one second side surface of the second sub-mask.

[0164] A through hole 34 is divided into a first sub-through hole and a second sub-through hole, and the glass mask 30 is divided into a first sub-mask and a second sub-mask. The situation where a through hole 34 needs to remove a glass mask 30 as a whole is divided into removing the first sub-mask and the second sub-mask separately. The first sub-through hole is connected to at least one first side surface, and the second sub-through hole is connected to at least one second side surface. This further facilitates the removal of the glass mask 30, and the through hole 34 on the glass mask 30 and the graphic shape of the patterned insulating layer 60' formed in the through hole 34 will not interfere with each other.

[0165] Optionally, the first sub-mask is removed along a direction perpendicular to the first side surface, and the second sub-mask is removed along a direction perpendicular to the second side surface.

[0166] By removing the first sub-mask and the second sub-mask along a direction perpendicular to the first side surface and a direction perpendicular to the second side surface respectively, the patterned insulating layer 60' can be removed from the opening on the side where the first sub-through hole is connected to the first side surface and the opening on the side where the second sub-through hole is connected to the second side surface respectively. The glass mask 30 can be split into the first sub-mask and the second sub-mask and pulled out of the patterned insulating layer 60'. The through hole 34 of the glass mask 30 and the patterned insulating layer 60' will not interfere with each other to cause the cross-sectional shape of the patterned insulating layer 60' to be destroyed.

[0167] In some embodiments, step S300 further includes:

[0168] The seed layer 20 is etched using a wet etching process.

[0169] In these embodiments, the seed layer 20 is etched by a wet etching process. Even if the patterned wiring layer 40' close to the seed layer 20 is slightly etched when etching the seed layer 20, the patterned wiring layer 40' has a higher reliability because its cross-sectional shape is wider on the side close to the seed layer 20, and the problem of the patterned wiring layer 40' being broken due to etching is not likely to occur.

[0170] The wet etching process is used to etch the seed layer 20 by using a specific chemical solution to react chemically with the seed layer 20 material, thereby removing the excess seed layer 20. The seed layer 20 is usually made of metal, such as copper or nickel, and the wet etching process uses a corresponding chemical solvent, such as an acid solution, to dissolve these metals.

[0171] The wet etching process can selectively etch specific materials without affecting other materials. While ensuring the integrity of other parts of the circuit board, it can handle complex patterns and shapes and is suitable for the production of fine circuits.

[0172] In some embodiments, step S300 further includes:

[0173] The seed layer is prepared from at least one of copper, nickel, chromium, gold and silver.

[0174] In some embodiments, before step S200, the method further includes:

[0175] A through hole 34 is prepared on the glass substrate to obtain a glass mask 30 .

[0176] In these embodiments, it is necessary to prepare through holes 34 on the glass substrate to form the glass mask 30 .

[0177] In some optional embodiments, the step of preparing a through hole on a glass substrate to obtain a glass mask further includes:

[0178] A laser-induced process is used to induce partial region denaturation of the glass substrate;

[0179] The glass substrate is etched by a wet etching process to form a through hole 34 .

[0180] In these optional embodiments, the TGV through-hole manufacturing technology is used to manufacture the through-holes 34 on the glass mask 30 to ensure accuracy and production efficiency.

[0181] The laser-induced wet etching method first uses a laser to generate a denatured layer on the surface of the glass substrate, and then uses a chemical solution to wet-etch the denatured area. Since the etching rate of the laser-denatured glass substrate in the chemical solution is different, a through hole 34 with a desired cross-sectional shape can be formed. The laser-induced wet etching method combines the high precision of the laser and the selectivity of wet etching, and is suitable for making a through hole 34 with a high aspect ratio.

[0182] The through holes 34 are formed on the glass substrate by physical or chemical methods, which are usually used, including but not limited to laser ablation, focused discharge, plasma etching, and electrochemical discharge machining.

[0183] The laser ablation method utilizes a high-energy laser beam to irradiate the glass substrate, and the thermal effect of the laser causes the glass substrate to melt or vaporize instantly in a local area, thereby forming a through hole 34. The laser ablation method can realize the production of the through hole 34 with high precision, but the laser energy needs to be controlled to avoid damaging the glass substrate.

[0184] The focused discharge method places a glass substrate between two electrodes, uses the high temperature generated by the discharge to partially melt the glass, and then generates high stress inside the glass through Joule heat, causing dielectric breakdown to form a through hole 34. The focused discharge method can quickly produce a through hole 34 with a small aperture and a high aspect ratio on the glass.

[0185] The plasma etching method uses plasma to physically or chemically etch the glass surface to remove material to form the through hole 34. Plasma is generated by the excitation of gas under a high electric field, has high activity, and can effectively remove material. The plasma etching method can realize a through hole 34 with smooth side walls and good verticality, but the etching rate is relatively slow.

[0186] The electrochemical discharge machining method combines the principles of electric spark machining and electrolytic machining, and generates electrochemical discharge by applying voltage between the glass substrate 70 and the tool electrode to remove the glass material. The electrochemical discharge machining method is simple to operate and has low cost, but it is currently mainly suitable for making through holes 34 with larger apertures and tapered shapes.

[0187] In some optional embodiments, the step of preparing a through hole on a glass substrate to obtain a glass mask further includes:

[0188] The width of the first opening 341 and the width of the second opening 342 of the cross section of the through hole 34 do not exceed 5 μm.

[0189] In these optional embodiments, by using a glass mask 30 , the width of the first opening 341 and the second opening 342 of the through hole 34 can be controlled to be no more than 5 μm, so that the line width or line spacing of the patterned wiring layer 40 ′ is no more than 5 μm, further improving the manufacturing accuracy of the circuit wiring 50 .

[0190] When the manufacturing method of placing the first surface 31 of the glass mask 30 on the seed layer 20 is adopted, the wiring layer 40 is directly formed in the through hole 34, and the line width of the patterned wiring layer 40' can be controlled within 5 μm.

[0191] When the second surface 32 of the glass mask 30 is bonded to the seed layer 20, the through hole 34 defines the patterned insulating layer 60' disposed between the patterned wiring layers 40', and the line spacing between the wirings of the patterned wiring layers 40' can be controlled within 5 μm.

[0192] In a second aspect, an embodiment of the present application further provides a printed circuit board 100, comprising a circuit trace 50 manufactured by any circuit trace manufacturing method provided in the embodiment of the first aspect.

[0193] The printed circuit board 100 provided in the embodiment of the present application includes the circuit trace 50 manufactured by the circuit trace manufacturing method of any of the above-mentioned first aspect embodiments. Therefore, the printed circuit board 100 provided in the second aspect embodiment of the present application has the beneficial effects of the circuit trace manufacturing method provided in the first aspect embodiment, which will not be repeated here.

[0194] See also Fig. 9In a third aspect, an embodiment of the present application further provides a printed circuit board 100 , comprising a substrate 10 and a circuit trace 50 .

[0195] The circuit routing 50 is arranged on one side of the substrate 10, and the circuit routing 50 includes a patterned seed layer 20' and a patterned routing layer 40' which are stacked in sequence in a direction away from the substrate 10. The cross-sectional shape of the circuit routing 50 along its own thickness direction includes a first section 51 formed in sequence in the patterned seed layer 20' and a second section 52 in the patterned routing layer 40'. The width of the second section 52 on the side close to the first section 51 is greater than the width of the second section 52 on the side away from the first section 51, and the width of the first section 51 is greater than or equal to the width of the second section 52.

[0196] The printed circuit board 100 provided in the embodiment of the present application controls the shape of the second cross section 52 to ensure that when etching to form the patterned seed layer 20', the patterned wiring layer 40' is not prone to the problem of short circuit caused by side etching; the width of the first cross section 51 can control the etching rate during etching and keep it greater than the width of the second cross section 52, and the patterned wiring layer 40' and the patterned seed layer 20' can also be etched synchronously, so that the width of the first cross section 51 is equal to the width of the second cross section 52, so that the process selection window is larger and the reliability is strong.

[0197] Optionally, in the process step of etching to form the patterned seed layer 20', the width of the first section 51 can be kept larger than the width of the second section 52 by controlling the etching rate, and the patterned routing layer 40' will not be etched when etching the patterned seed layer 20'.

[0198] Optionally, in the process step of etching to form the patterned seed layer 20', the patterned routing layer 40' where the second section 52 is located and the patterned seed layer 20' where the first section 51 is located can be simultaneously etched so that the overall width of the first section 51 remains the same as the maximum width of the second section 52.

[0199] In these optional embodiments, since the cross-sectional shape of the patterned routing layer 40' is a second section 52 whose width near the first section 51 is greater than the width away from the first section 51, even if the patterned routing layer 40' undergoes partial side engraving, it is not prone to problems such as routing breakage.

[0200] See also Fig. 9 In some embodiments, the width of the second cross section 52 decreases in a direction away from the substrate 10 .

[0201] In these embodiments, the width of the first cross section 51 changes evenly, further improving reliability.

[0202] See also Fig. 9In some optional embodiments, the width of the second cross section 52 is W, where W≠0.

[0203] In these optional embodiments, the cross-sectional shape of the first cross section 51 is a regular trapezoid, which further improves reliability.

[0204] In some optional embodiments, the patterned routing layer 40 ′ includes a metal material.

[0205] In some optional embodiments, the patterned wiring layer 40 ′ includes at least one material of copper, aluminum, and tin.

[0206] In some optional embodiments, the line width or line spacing of the patterned wiring layer 40 ′ does not exceed 5 μm.

[0207] In these optional embodiments, the manufacturing accuracy of the circuit trace 50 is further improved.

[0208] When the manufacturing method of placing the first surface 31 of the mask 30 in contact with the seed layer 20 is adopted, the wiring layer 40 is directly formed in the through hole 34 , and the line width of the patterned wiring layer 40 ′ can be controlled within 5 μm.

[0209] When the manufacturing method of placing the second surface 32 of the mask 30 on the seed layer 20 is adopted, the through hole 34 defines the insulating layer disposed between the patterned wiring layers 40 ′, and the line spacing between the wirings of the patterned wiring layers 40 ′ can be controlled within 5 μm.

[0210] In some embodiments, the seed layer 20 is made of a material including at least one of copper, nickel, chromium, gold, and silver.

[0211] See also Fig.10 In some optional embodiments, the width of the first cross section 51 gradually increases in a direction away from the second cross section 52;

[0212] In these optional embodiments, the first cross-section 51 can be set to a right trapezoid, and the shape of the first cross-section 51 can match the shape of the second cross-section 52, so that the overall cross-sectional shape of the circuit routing 50 formed by the first cross-section 51 and the second cross-section 52 can be set to a right trapezoid, making the circuit routing 50 more regular as a whole.

[0213] The wet etching process in the process flow can control the rate of wet etching the seed layer 20 to etch the first cross section 51 into a regular trapezoidal shape, further avoiding the problem of side etching and over etching of the second cross section 52 when the wet etching process etches to form the first cross section 51.

[0214] See also Fig.10In some optional embodiments, the side inclination angle of the first section 51 is less than or equal to the side inclination angle of the second section 52.

[0215] The wet etching process in the process flow can further control the rate of wet etching the seed layer 20, so that the side inclination angle of the first section 51 is smaller than the side inclination angle of the second section 52, so that the width of the first section 51 changes more gradually along the thickness direction, thereby further avoiding the problem of side etching and over-etching of the second section 52 when the wet etching process etches to form the first section 51.

[0216] Although the present application has been described with reference to preferred embodiments, various modifications may be made thereto and parts thereof may be replaced with equivalents without departing from the scope of the present application. In particular, the various technical features mentioned in the various embodiments may be combined in any manner as long as there are no structural conflicts. The present application is not limited to the specific embodiments disclosed herein, but includes all technical solutions falling within the scope of the claims.

Claims

1. A method for making a circuit routing, characterized in that: include: preparing a seed layer on one side of the substrate; A mask is arranged on a side of the seed layer away from the substrate, wherein the mask comprises a first surface and a second surface arranged opposite to each other and at least one through hole penetrating the first surface and the second surface; Using the mask to prepare a patterned wiring layer on the side of the seed layer away from the substrate, and using the through hole to limit the line spacing or line width of the patterned wiring layer; The exposed portion of the seed layer between the patterned wiring layers is patterned to form a patterned seed layer, thereby obtaining a circuit wiring. The circuit wiring includes the patterned seed layer and the patterned wiring layer which are sequentially stacked in a direction away from the substrate.

2. The circuit routing method according to claim 1, characterized in that: In the step of arranging a mask on the side of the seed layer away from the substrate, the width of the first opening of the through hole whose cross section is located on the first surface is greater than the width of the second opening of the through hole located on the second surface; Preferably, the opening width of the cross section of the through hole gradually decreases along the direction from the first surface to the second surface; Preferably, the mask is a glass mask.

3. The circuit routing method according to claim 2, characterized in that: In the step of arranging a mask on the side of the seed layer away from the substrate, the first surface of the mask is located on the side of the seed layer away from the substrate, and the first opening is located on the side of the second opening close to the seed layer; Preferably, the step of preparing a patterned wiring layer on a side of the seed layer away from the substrate through a mask further comprises: Preparing a routing layer in the through hole; Removing the mask to obtain the patterned wiring layer; Preferably, the step of preparing the routing layer further includes: The wiring layer includes a metal material, and the wiring layer is prepared in the through hole by an electroplating process; Preferably, the routing layer includes at least one material of copper, aluminum, and tin; Preferably, the step of removing the mask further comprises: The mask is removed along a thickness direction of the mask.

4. The circuit routing method according to claim 2, characterized in that: In the step of arranging a mask on the side of the seed layer away from the substrate, the second surface of the mask is located on the side of the seed layer away from the substrate, and the second opening is located on the side of the first opening close to the seed layer; Preferably, the step of preparing a patterned wiring layer on a side of the seed layer away from the substrate through a mask further comprises: preparing an insulating layer on a side of the mask away from the seed layer; removing the mask to obtain a patterned insulating layer; Preparing a wiring layer between the patterned insulating layers; Removing the patterned insulating layer to obtain the patterned wiring layer; Preferably, the step of preparing the insulating layer further comprises: The insulating layer is made of insulating material and is prepared by screen printing process; Preferably, the step of preparing the routing layer further includes: The wiring layer comprises a metal material and is prepared by an electroplating process; Preferably, the step of preparing the routing layer further includes: The routing layer includes at least one material of copper, aluminum, and tin.

5. The circuit routing manufacturing method according to claim 1, characterized in that: The step of patterning the portion of the seed layer exposed between the patterned wiring layers also includes: Etching the seed layer using a wet etching process; Preferably, the step of preparing a seed layer on one side of the substrate further includes: The seed layer is prepared from at least one of copper, nickel, chromium, gold and silver.

6. The circuit routing manufacturing method according to claim 2, characterized in that: Before the step of arranging a mask on the side of the seed layer away from the substrate, the method further comprises: Preparing through holes on a substrate to obtain the mask; Preferably, the step of preparing a through hole on the substrate further includes: Inducing denaturation of a partial region of the substrate by a laser induction process; Etching the substrate using a wet etching process to form the through hole; Preferably, in the step of preparing a through hole on the substrate, the first opening width and the second opening width of the cross section of the through hole are no more than 5 μm.

7. A printed circuit board, characterized in that: It comprises a circuit trace made by the circuit trace making method according to any one of claims 1 to 6.

8. A printed circuit board, characterized in that: include: substrate; A circuit trace is arranged on one side of the substrate; The circuit routing includes a patterned seed layer and a patterned routing layer stacked in sequence in a direction away from the substrate. The cross-sectional shape of the circuit routing along its own thickness direction includes a first cross-sectional shape of the patterned seed layer and a second cross-sectional shape of the patterned routing layer. The width of the second cross-sectional shape on a side close to the first cross-sectional shape is greater than the width of the second cross-sectional shape on a side away from the first cross-sectional shape. The width of the first cross-sectional shape is greater than or equal to the width of the second cross-sectional shape.

9. The printed circuit board according to claim 8, characterized in that: The second cross-sectional width decreases in a direction away from the substrate; Preferably, the second cross-sectional width is W, W≠0; Preferably, the patterned routing layer comprises a metal material; Preferably, the patterned wiring layer includes at least one material of copper, aluminum, and tin; Preferably, the line width or line spacing of the patterned wiring layer does not exceed 5 μm.

10. The printed circuit board according to claim 8, characterized in that: The seed layer is prepared from at least one of copper, nickel, chromium, gold and silver; Preferably, the width of the first cross section gradually increases in a direction away from the second cross section; Preferably, the side inclination angle of the first cross section is less than or equal to the side inclination angle of the second cross section.