Method for controlling uniformity of stainless steel clad steel bars
By employing precise heating, a specialized die system, and grinding processes, combined with controlled rolling and cooling and roller conveyor technology, the problems of uneven thickness and scratches in the stainless steel coating of composite steel bars have been solved, achieving uniformity and no leaks in the stainless steel coating and improving the finished quality of composite steel bars.
Patent Information
- Application Number
- CN202411160192.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-11-15
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of metallurgy, and in particular to a method for controlling uniformity of stainless steel coated steel bars. Background Art
[0002] Corrosion-resistant, high-strength hot-rolled carbon steel-stainless steel composite rebar, the outer layer is stainless steel with excellent corrosion resistance (304, 316L, etc.); the inner layer is high-strength carbon steel (HRB400, HRB500), which has both the corrosion resistance of stainless steel and the high mechanical properties of carbon steel. It can greatly increase the service life and reduce maintenance and use costs when used in the construction of bridges, highways, coastal roads, coastal defense islands.
[0003] In the prior art, the production of composite steel bars is still in the test and development stage. The composite cold rolling process is used to make the carbon steel and stainless steel achieve metallurgical bonding performance. Before the composite cold rolling of the rebar, the oxide layer and oil stains on the surface of the steel bar need to be cleaned and pre-treated. When the steel bar is polished after the existing cleaning pre-treatment, it is only polished in the transmission direction of the steel bar, resulting in poor steel bar grinding effect, stainless steel leakage points at the root of the transverse rib, and a failure rate of more than 50%, resulting in huge losses.
[0004] Stainless steel is a composite steel billet with a soft texture and thin composite layer (the billet is 8mm, and the thinnest part of the steel is required to be 0.18mm). It is necessary to design a precise and appropriate hole system, pressing procedure, and temperature system. Otherwise, the billet will easily delaminate, and the finished product will have uneven thickness. Since stainless steel is soft, it is easy to scratch, resulting in leaks. It is necessary to formulate scratch prevention requirements for the entire process from billet to steel delivery. Summary of the invention
[0005] Aiming at the problems in the prior art that stainless steel is soft in texture and has a thin composite layer, and is very prone to delamination of steel billets, uneven thickness, scratches, and leaks, the present invention provides a method for controlling the uniformity of stainless steel coated steel bars, which ensures that the stainless steel coated steel bars are uniform and have no leaks, and the difference between the thinnest and thickest stainless steel coatings is ≤0.5mm.
[0006] A method for controlling uniformity of stainless steel coated steel bars comprises the steps of heating, rough rolling, finish rolling, controlled rolling and controlled cooling, and grinding a round steel billet in sequence, including: (1) The furnace gas temperature in the heating and soaking section is controlled at 1150-1200℃; (2) The round billet matches the rough rolling pass; (3) Rolling guides are used throughout the rough rolling process; (4) A bypass roller table with rollers is used in the controlled rolling and controlled cooling area; (5) Grinding includes grinding of cooling bed and rear roller.
[0007] Furthermore, the round steel billet is composed of two layers, an inner layer and an outer layer, wherein the outer layer is a stainless steel cladding and the core is a threaded steel 400Mpa grade steel rod.
[0008] Furthermore, the rough rolling pass of the rough rolling process adopts an elliptical-circular hole system.
[0009] Furthermore, the rough rolling line includes 20 rolling mills.
[0010] Furthermore, the rough rolling hole filling degree is 90%-95%.
[0011] Furthermore, the reduction of the first 6 roughing mills is ≤40mm.
[0012] Furthermore, the rough rolling 6# material type is selected to be 71mm×71mm.
[0013] Furthermore, the finishing rolling includes grinding holes on the K1 finished roll.
[0014] The beneficial effects of the present invention are: The present invention provides a method for controlling the uniformity of stainless steel coated steel bars, which adopts a process route of "precise heating system + special elliptical hole system + small reduction process procedure + grinding K1 chamfer", adopts a bypass roller with rollers in the controlled rolling and cooling area, and grinds the cooling bed and the rear area rollers to achieve the uniformity of the stainless steel coated steel bars, so that the final rolled stainless steel coating is uniform and has no leaks, and the difference between the thinnest and thickest stainless steel coatings is ≤0.5mm. DETAILED DESCRIPTION
[0015] In order to enable those skilled in the art to better understand the technical solutions in the present invention, the technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.
[0016] Example 1 A method for controlling uniformity of stainless steel coated steel bars comprises the steps of heating, rough rolling, finish rolling, controlled rolling and controlled cooling, and grinding a round steel billet in sequence, specifically comprising: The round steel billet section is 140mm×140mm. The round steel billet consists of two layers, the outer layer is stainless steel cladding, and the core is a 400Mpa grade threaded steel bar. The inner and outer layers are bonded together by vacuuming. The rough rolling hole adopts an elliptical-circular hole system. The round steel billet matches the rough rolling hole. The rough rolling line includes 20 rolling mills. The first 6 rough rolling mills have a reduction of ≤30mm and a hole filling degree of 90%-93% to prevent ears. The rough rolling 6# material type is 71mm×71mm; the furnace gas temperature in the heating and soaking section is controlled at 1150-1180℃; the whole line 2 All 0 rolling mills use elliptical holes; the whole line uses rolling guides, without steel rotation, steel inversion, and guide deviation, and the guide plug-in and surface are smooth without sharp protrusions; the controlled rolling and controlled cooling area uses a bypass roller with rollers to prevent scratch defects; the cooling bed and the rear area roller are all polished and repaired to ensure that there are no scratch defects and prevent the stainless steel coating from scratching and leaking; the finishing rolling includes grinding the holes of the K1 finished roller, grinding the sharp parts and engraved marks at the intersection of the transverse rib and the base circle into a smooth obtuse angle to prevent the transverse rib from being filled and leaking. Through the implementation of the above technical measures, the steel bars with uniform stainless steel coating and no leaks are finally rolled. It can be obtained that the rolled stainless steel coating is uniform and has no leaks, the thinnest part is 1.5mm, the thickest part is 1.8mm, and the surface coating thickness differs by 0.3mm.
[0017] Example 2 A method for controlling uniformity of stainless steel coated steel bars comprises the steps of heating, rough rolling, finish rolling, controlled rolling and controlled cooling, and grinding a round steel billet in sequence, specifically comprising: The round steel billet section is 150mm×150mm. The round steel billet consists of two layers, the outer layer is stainless steel cladding, and the core is a 400Mpa grade threaded steel bar. The inner and outer layers are bonded together by vacuuming. The rough rolling hole adopts an elliptical-circular hole system. The round steel billet matches the rough rolling hole. The rough rolling line includes 20 rolling mills. The first 6 rough rolling mills have a reduction of ≤35mm and a hole filling degree of 91%-94% to prevent ears. The rough rolling 6# material type is 71mm×71mm; the furnace gas temperature in the heating and soaking section is controlled at 1150-1190℃; 20 All rack rolling mills use elliptical round holes for rolled pieces; rolling guides are used throughout the line, with no steel rotation, steel inversion, or guide deviation, and the guide plug-ins and surfaces are smooth without sharp protrusions; bypass rollers with rollers are used in the controlled rolling and cooling areas to prevent scratch defects; the cooling bed and rear area rollers are all polished and repaired to ensure that there are no scratch defects and to prevent scratch leaks on the stainless steel coating; finishing rolling includes grinding the holes of the K1 finished rollers, and grinding the sharp parts and engraved marks at the intersection of the transverse ribs and the base circle into smooth obtuse angles to prevent the transverse ribs from being infilled, thereby causing leaks. Through the implementation of the above technical measures, steel bars with uniform stainless steel coating and no leaks are finally rolled.
[0018] It can be concluded that the rolled stainless steel coating is uniform and leak-free, with the thinnest part being 1.4 mm and the thickest part being 1.8 mm, and the surface coating thickness differing by 0.4 mm.
[0019] Example 3 A method for controlling uniformity of stainless steel coated steel bars comprises the steps of heating, rough rolling, finish rolling, controlled rolling and controlled cooling, and grinding a round steel billet in sequence, specifically comprising: The round steel billet section is 160mm×160mm. The round steel billet consists of two layers, the outer layer is stainless steel cladding, and the core is a 400Mpa grade threaded steel bar. The inner and outer layers are bonded together by vacuuming. The rough rolling pass adopts an elliptical round pass system. The round steel billet matches the rough rolling pass. The rough rolling line includes 20 rolling mills. The first 6 rough rolling mills have a reduction of ≤40mm and a pass filling degree of 90%-95% to prevent ears. The rough rolling 6# material type is 71mm×71mm; the furnace gas temperature in the heating and soaking section is controlled at 1150-1200℃; the whole line 20 All rack rolling mills use elliptical round holes; the entire line uses rolling guides, without steel rotation, steel inversion, or guide deviation, and the guide plug-ins and surfaces are smooth without sharp protrusions; bypass rollers with rollers are used in the controlled rolling and controlled cooling areas to prevent scratch defects; the cooling bed and rear area rollers are all polished and repaired to ensure that there are no scratch defects and to prevent scratches and leaks on the stainless steel coating; finishing rolling includes grinding the holes of the K1 finished rollers, and grinding the sharp parts and engraved marks at the intersection of the transverse ribs and the base circle into smooth obtuse angles to prevent the transverse ribs from being infilled and thus leaking. Through the implementation of the above technical measures, steel bars with uniform stainless steel coating and no leaks are finally rolled.
[0020] It can be concluded that the rolled stainless steel coating is uniform and leak-free, with the thinnest part being 1.4 mm and the thickest part being 1.8 mm, and the surface coating thickness differing by 0.4 mm.
[0021] Although the present invention has been described in detail by way of preferred embodiments, the present invention is not limited thereto. Without departing from the spirit and essence of the present invention, a person of ordinary skill in the art may make various equivalent modifications or substitutions to the embodiments of the present invention, and such modifications or substitutions shall be within the scope of the present invention. Any person of ordinary skill in the art may easily conceive of changes or substitutions within the technical scope disclosed by the present invention, and such changes or substitutions shall be within the scope of protection of the present invention.
Claims
1. A method for controlling uniformity of stainless steel coated steel bars, comprising the steps of heating, rough rolling, finish rolling, controlled rolling and controlled cooling, and grinding a round steel billet in sequence, characterized in that: (1) The furnace gas temperature in the heating and soaking section is controlled at 1150-1200℃; (2) The round billet matches the rough rolling pass; (3) Rolling guides are used throughout the rough rolling process; (4) A bypass roller table with rollers is used in the controlled rolling and controlled cooling area; (5) Grinding includes grinding of cooling bed and rear roller.
2. A method for controlling uniformity of stainless steel coated steel bars according to claim 1, characterized in that: The round steel billet consists of two layers, the outer layer is stainless steel cladding and the core is threaded steel 400Mpa grade steel rod.
3. A method for controlling uniformity of stainless steel coated steel bars according to claim 1, characterized in that: The rough rolling hole profile of rough rolling adopts an elliptical-circular hole system.
4. A method for controlling uniformity of stainless steel coated steel bars according to claim 1, characterized in that: The rough rolling line includes 20 rolling mills.
5. A method for controlling uniformity of stainless steel coated steel bars as claimed in claim 3, characterized in that: The rough rolling hole filling degree is 90%-95%.
6. A method for controlling uniformity of stainless steel coated steel bars as claimed in claim 4, characterized in that: The reduction of the first 6 rough rolling mills is ≤40mm.
7. A method for controlling uniformity of stainless steel coated steel bars as claimed in claim 1, characterized in that: The rough rolling 6# material type selected is 71mm×71mm.
8. A method for controlling uniformity of stainless steel coated steel bars as claimed in claim 1, characterized in that: Finishing rolling includes grinding the holes of the K1 finished roll.
Citation Information
Patent Citations
Combined control rolling process for hot-rolled steel bar with rib
CN101367094A
Controlled rolling and controlled cooling system for bars
CN103551403A
Stainless steel composite steel bar and preparation method thereof
CN113877961A
Rolling method of MG500Wphi24 high-strength high-toughness small-pitch threaded rib anchor rod steel bar
CN115740032A
Roller way reconditioning device
CN200977612Y