Manufacturing process of screw rotor
By forming screw wires with forging molds and combining machining and Teflon spraying, the problems of waste of materials and insufficient mechanical properties in the rotor manufacturing process of traditional screw compressors are solved, achieving time and cost savings and strength improvements.
Patent Information
- Application Number
- CN202410859849.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-28
- Publication Date
- 2024-11-15
AI Technical Summary
In the traditional screw compressor rotor manufacturing process, the forging process leads to waste of materials and increased processing time, while the casting process has problems of insufficient mechanical properties and multiple heat treatments, resulting in excessive manufacturing cost and time consumption.
The rod material is heated and extruded and forged to form a screw line, followed by cooling and annealing and machining, and finally Teflon spraying is carried out, combining forging and casting processes to reduce processing steps and time and enhance materials. strength.
The design mechanical properties of screw rotor blanks are achieved, which shortens processing time and cost, and avoids material waste and heat treatment requirements in traditional processes.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of compressor manufacturing technology, and more specifically to a manufacturing process for a screw rotor. Background Art
[0002] The screw compressor is composed of a pair of parallel, intermeshing female and male screws, and is the most widely used type of rotary compressor. The screw rotor is the core component of the screw compressor. The traditional manufacturing methods include forging and casting. The former is to heat the metal material and then use the forging process to make the rotor round bar. After the initial round bar size is formed, it is processed into a finished product using CNC equipment such as a lathe, screw milling, and screw grinding. Although this forging process can achieve the stress, toughness, and hardness of the material, the disadvantage is that the initial forging is all cylindrical bars, which increases a lot of processing time in the process of screw milling profiles, and the waste under the chips cannot be reused, which not only increases the processing cost, but also wastes a lot of metal materials. The latter is to use a mold to make the rotor profile, and then use the corresponding liquid material for casting, and then CNC processing after cooling. Although this method can cast a preliminary screw profile and reduce processing allowances, because there is not enough pressure on the cavity during the casting process, large sand holes and insufficient mechanical properties may appear. Therefore, multiple heat treatments are required during the later processing to solve these defects, which greatly increases the manufacturing cost and processing time. Summary of the invention
[0003] The technical problem to be solved by the present invention is to provide a manufacturing process for a screw rotor, wherein the screw rotor blank obtained by the manufacturing process not only conforms to the concept of design mechanics, but also saves the time for roughening the rotor profile.
[0004] The technical solution of the present invention is to provide a manufacturing process of a screw rotor having the following steps: S1. Prepare the bar blank and heat it to 650-800℃; S2, placing the heated bar into a forging die, and after extrusion and forging of the die, forming a preliminary screw profile to produce a screw rotor blank; S3, performing cooling annealing treatment on the screw rotor blank; S4, machining the cooled screw rotor blank to produce a screw rotor of predetermined specifications; S5. Perform Teflon spraying treatment on the surface of the screw rotor.
[0005] After adopting the above structure, the manufacturing process of the screw rotor of the present invention has the following advantages compared with the prior art: Compared with forging bars, the manufacturing process of the screw rotor of the present invention reduces multiple casting and processing processes, greatly shortens the time cycle of the finished rotor, and reduces capital investment; compared with the method of casting the screw rotor, forging can enhance the stress and strength of the rotor shaft and the screw, and does not require repeated heat treatment like the casting mold without pressure extrusion. The manufacturing process of the screw rotor of the present invention combines the two processes of forging and casting, and the obtained screw rotor blank not only meets the concept of design mechanics, but also saves the time of roughening the rotor profile, killing two birds with one stone.
[0006] As an improvement, in step S5, Teflon spraying specifically includes the following steps: S501, pre-treating the surface of the screw rotor, including high-temperature baking to remove grease and roughening the surface; S502, spraying primer on the screw rotor; S503, spraying on the surface of the screw rotor to form a dispersion coating; S504, spraying on the surface of the screw rotor to form a powder coating; S505, sintering the screw rotor to form a strong coating.
[0007] As an improvement, in step S502, the screw rotor is fixed, and Teflon primer is sprayed on the surface of the screw rotor, and then dried and sintered to form a solid coating.
[0008] As an improvement, in step S503, the coating material is evenly distributed in the solvent to form a dispersion, which is atomized by high-pressure air and sprayed onto the surface of the screw rotor; then dried and sintered to melt the coating material and form a network structure with the bonding agent.
[0009] As an improvement, in step S504, the coating material used is in the form of fine solid particles, which are sprayed on the surface of the screw rotor and then melted in a furnace to form a powder coating. DETAILED DESCRIPTION
[0010] In order to better understand the present application, various aspects of the present application will be described in more detail. It should be understood that these detailed descriptions are only descriptions of exemplary embodiments of the present application, and do not limit the scope of the present application in any way.
[0011] It should also be understood that the terms “comprises,” “has,” “includes,” and “including,” when used in this specification, indicate the presence of the described features, integers, steps, operations, elements, and / or parts, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, parts, and / or combinations thereof.
[0012] The present application discloses a manufacturing process of a screw rotor, comprising the following steps: S1. Prepare the bar blank and heat it to 650-800℃. At this time, the blank will be deformed by extrusion; the specific heating temperature depends on the actual situation of the bar.
[0013] S2. Place the heated bar into the forging die, and after the die is extruded and forged up and down, a preliminary screw profile is formed to produce a screw rotor blank.
[0014] S3, performing cooling annealing treatment on the screw rotor blank. In this specific embodiment, the cooling treatment is performed by oil cooling.
[0015] S4. The cooled screw rotor blank is machined to produce a screw rotor of predetermined specifications; the processing is carried out specifically through screw milling, screw grinding, CNC lathe, cylindrical grinding and other equipment.
[0016] S5, performing Teflon spraying treatment on the surface of the screw rotor, specifically comprising the following steps: S501, pre-treating the surface of the screw rotor, including high-temperature baking to remove grease and roughening the surface; S502, spraying the screw rotor with primer, that is, fixing the screw rotor, spraying Teflon primer on the surface of the screw rotor, and drying and sintering after spraying to form a solid coating.
[0017] S503, spraying a dispersion coating on the surface of the screw rotor, that is, evenly distributing the coating material in the solvent to form a dispersion, atomizing it with high-pressure air and spraying it on the surface of the screw rotor; then drying and sintering, so that the coating material melts and forms a network structure with the adhesive additive.
[0018] S504, spraying on the surface of the screw rotor to form a powder coating, that is, the coating material used is in the form of fine solid particles, spraying the coating material on the surface of the screw rotor, and then melting in a furnace to form a powder coating.
[0019] S505, sintering the screw rotor to form a strong coating.
[0020] The above description is only a preferred embodiment of the present application and is not intended to limit the present application. Any modifications, equivalent substitutions and improvements made within the principles and spirit of the present application are included in the protection scope of the present application.
Claims
1. A process for manufacturing a screw rotor, comprising the following steps: S1. Prepare the bar blank and heat it to 650-800℃; S2, placing the heated bar into a forging die, and after extrusion and forging of the die, forming a preliminary screw profile to produce a screw rotor blank; S3, performing cooling annealing treatment on the screw rotor blank; S4, machining the cooled screw rotor blank to produce a screw rotor of predetermined specifications; S5. Perform Teflon spraying treatment on the surface of the screw rotor.
2. The manufacturing process of the screw rotor according to claim 1, characterized in that: In step S5, Teflon spraying specifically includes the following steps: S501, pre-treating the surface of the screw rotor, including high-temperature baking to remove grease and roughening the surface; S502, spraying primer on the screw rotor; S503, spraying on the surface of the screw rotor to form a dispersion coating; S504, spraying on the surface of the screw rotor to form a powder coating; S505, sintering the screw rotor to form a strong coating.
3. The manufacturing process of the screw rotor according to claim 2, characterized in that: In step S502, the screw rotor is fixed, and Teflon primer is sprayed on the surface of the screw rotor, and then dried and sintered to form a solid coating.
4. The manufacturing process of the screw rotor according to claim 2, characterized in that: In step S503, the coating material is evenly distributed in the solvent to form a dispersion, which is atomized by high-pressure air and sprayed on the surface of the screw rotor; then dried and sintered to melt the coating material and form a network structure with the adhesive additive.
5. The manufacturing process of the screw rotor according to claim 2, characterized in that: In step S504, the coating material used is in the form of fine solid particles, which are sprayed on the surface of the screw rotor and then melted in a furnace to form a powder coating.
Citation Information
Patent Citations
Female rotor blank rolling method of screw compressor
CN104815931A
Screw pump rotor rotary die extrusion forming process
CN112518239A
Semi-solid closed precision swaging composite forming process for screw complex parts
CN115740311A
Preparation process of single-screw pump rotor
CN116163949A