Thermally activated delayed fluorescence red light material capable of being processed by solution as well as preparation method and application of thermally activated delayed fluorescence red light material

By using a solution-processed thermally activated delayed fluorescent material in red light OLED, the red light emission efficiency is improved by using phenanthropyrazine structure and methyl benzoate, and the problem of low crossing efficiency between the reverse system of the red light material is solved, and the problem of low crossing efficiency between the reverse system is achieved. High external quantum efficiency and excellent luminous performance, suitable for flat panel display and solid state lighting.

CN118955487AActive Publication Date: 2024-11-15GUANGDONG UNIV OF TECH

Patent Information

Application Number
CN202411029790.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-30
Publication Date
2024-11-15
Estimated Expiration
2044-07-30

AI Technical Summary

Technical Problem

The inter-coordinate crossover efficiency of red light materials in existing fluorescent OLEDs is low, resulting in low external quantum efficiency and difficult to match the performance of blue/green TADF devices, limiting the development of red light OLED devices.

Method used

Using solution-processed thermally activated delayed fluorescent red light materials, two thermally activated delayed fluorescent materials are synthesized through electrophilic phenanthizine structural units, which have a small △Est, exhibit good TADF characteristics, and are benzoic acid Methyl ester increases the solubility of molecules and improves the red light emission efficiency.

Benefits of technology

It achieves high external quantum efficiency of red light OLED devices, up to 17%, excellent luminous performance, and has a wide range of application prospects in flat panel display and solid state lighting fields.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118955487A_ABST
    Figure CN118955487A_ABST
Patent Text Reader

Abstract

The invention discloses a solution-processable TADF (thermally activated delayed fluorescence) red-light-emitting material as well as a preparation method and application thereof, and belongs to the technical field of organic light-emitting diodes, and two TADF red-light-emitting materials are synthesized by taking a phenanthropyrazine receptor as a first receptor and a methyl benzoate group as a second receptor and connecting phenoxazine. Corresponding organic electroluminescent devices are provided according to the two red light TADF materials; the obtained red light TADF material has relatively small Est, is beneficial to improving anti-intersystem crossing and shows good TADF characteristics, and the phenanthropyrazine structural unit has certain rigidity and can well inhibit non-radiative transition; in addition, the second acceptor is introduced and the connection site of the second acceptor is changed, so that the light color can be changed; and on the other hand, molecular solubility is increased, device preparation for solution processing is easy, energy level regulation on a receptor based on an excited state is realized, device efficiency of red light in solution processing is finally improved, and the material has a wide application prospect and is expected to be widely applied to the fields of panel display, solid-state illumination and the like.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of organic electroluminescent materials, and more specifically, to a solution-processable thermally activated delayed fluorescent red light material and a preparation method and application thereof. Background Art

[0002] Organic light-emitting diodes (OLEDs) are also called organic electroluminescent diodes. Organic electroluminescence refers to a luminescence phenomenon in which organic small molecules, metal-organic complex molecules or polymer molecular luminescent materials directly convert electrical energy into light energy under the action of a forward bias electric field. OLEDs can not only emit light autonomously, do not require a backlight source and save energy, but also have the characteristics of fast response speed, low driving voltage, high luminous efficiency, high resolution, wide viewing angle and high contrast. OLEDs use cheap glass, metal or even flexible plastic as substrates, and have the advantages of low cost, simple production process and large-scale production. They have become a new generation of full-color display and lighting technology, and have broad application prospects in mobile phones, computers, televisions, digital cameras, GPS, bendable and foldable electronic products and lighting fields, and have received widespread attention from academia and industry.

[0003] The ratio of singlet excitons to triplet excitons generated in OLEDs is 1:3. In conventional fluorescent OLEDs, only singlet excitons can be used for photon generation, resulting in an internal quantum efficiency (IQE) of only 25% in theory. Phosphorescent OLEDs can utilize both singlet and triplet excitons by introducing phosphorescent materials containing heavy metals, and can theoretically achieve an IQE of 100%, but the rarity of heavy metals is undesirable for the further application of phosphorescent OLEDs. In the past few years, an emerging technology based on the thermally activated delayed fluorescence (TADF) mechanism has attracted great interest from academia and industry due to its potential to fully utilize excitons on metal-free emitters, and is considered to be the next generation of OLEDs. In TADF emitters, a small energy difference (△Est) between the lowest excited singlet state (S1) and triplet state (T1) is the basic requirement for achieving reverse intersystem crossing (RISC) from triplet excitons to singlet excitons. Therefore, an effective separation between the highest occupied molecular orbital (HOMO) and the lowest unoccupied molecular orbital (LUMO) is crucial. Connecting the electron donor (D) unit to the electron acceptor (A) unit through a highly twisted bridge to break their conjugation can effectively reduce ΔEst, but the weakened DA connection will also reduce the oscillation intensity (f) and reduce the radiation attenuation. Among the three primary colors, blue and green light have a larger energy gap Eg, which makes blue-green light have a smaller non-radiative transition relative to red light, so that the efficiency of solution-processable devices is much higher than that of red light materials. Therefore, in view of the above problems, improving the anti-intersystem crossing efficiency of red light materials is a key way to obtain high device efficiency.

[0004] Patent application content

[0005] In order to overcome one of the problems existing in the above-mentioned prior art, the primary purpose of the present application is to provide a solution-processable thermally activated delayed fluorescent red light material. The solution-processable thermally activated delayed fluorescent red light material can be used in the preparation of solution-processed red light OLED devices to meet the development requirements matching the performance of blue / green TADF devices, thereby hopefully obtaining a higher external quantum efficiency.

[0006] Another object of the present application is to provide a method for preparing the above-mentioned solution-processable thermally activated delayed fluorescent red light material.

[0007] Another object of the present application is to provide an application of the above-mentioned solution-processable thermally activated delayed fluorescent red light material in an organic light-emitting device.

[0008] The above-mentioned purpose of this application is achieved through the following technical solutions:

[0009] A solution-processable heat-activated delayed fluorescent red light material, wherein the structural formula of the solution-processable heat-activated delayed fluorescent red light material has the following molecular structure:

[0010]

[0011] Wherein, R1 and R2 are H or 2-(methoxycarbonyl)phenyl; when R1 is H, R2 is 2-(methoxycarbonyl)phenyl; when R2 is H, R1 is 2-(methoxycarbonyl)phenyl, wherein the molecular structure of the 2-(methoxycarbonyl)phenyl is as follows:

[0012]

[0013] Preferably, the molecular structure of the solution-processable thermally activated delayed fluorescent red light material is as follows:

[0015]

[0016] The present application also provides a method for preparing the above-mentioned solution-processable thermally activated delayed fluorescent red light material, comprising the following steps:

[0017] S1. Preparation of Intermediate A

[0018] 3,6-dibromo-9,10-phenanthrenequinone, phenoxazine, tri(dibenzylideneacetone)dipalladium, cesium carbonate and tri-tert-butylphosphine tetrafluoroborate are added to anhydrous toluene in a molar ratio of 1:(2.3-3):(0.04-0.1):(2.25-3):(0.1-0.2) under nitrogen protection to obtain a mixed solution A with a concentration of 0.03-0.05 mmol / ml of 3,6-dibromo-9,10-phenanthrenequinone, and the mixture is heated to 100-120° C. and stirred for reaction. After 3,6-dibromo-9,10-phenanthrenequinone is completely reacted, palladium salt and cesium carbonate precipitated during the reaction are filtered and distilled to obtain a crude product A; the crude product A is purified by a chromatographic column, and then the remaining phenoxazine and by-products are removed by an eluent, and the intermediate A is obtained after recrystallization, suction filtration and high-temperature sublimation;

[0019] S2. Preparation of intermediate product B1 or B2

[0020] The intermediate A and 4-bromobenzene-1,2-diamine or 3-bromobenzene-1,2-diamine are added to glacial acetic acid in a molar ratio of 1:(1.2-2) under nitrogen protection to obtain a mixed solution B with a concentration of 0.03-0.05 mmol / ml of the intermediate A, and the solution is heated to 100-130° C. and stirred for reaction. After the intermediate A is completely reacted, the solution is cooled to room temperature, poured into the prepared deionized water, filtered, and then recrystallized from ethanol to obtain an intermediate product B1 or B2;

[0021] S3. Preparation of target product m-DBPP or o-DBPP

[0022] The intermediate product B1 or B2, (2-(methoxycarbonyl)phenyl)boric acid, tetrakistriphenylphosphine palladium and 2M potassium carbonate are added to 1,4-dioxane in a molar ratio of 1:(1.5-2):(0.04-0.1):(2-4.5) under nitrogen protection to obtain a mixed solution C with a concentration of 0.03-0.05 mmol / ml of the intermediate product B1, and the mixture is heated to 100-105° C. and stirred for reaction. After the intermediate product is completely reacted, the mixture is cooled to room temperature, extracted with ethyl acetate EA and saturated brine for 1-2 times, and the organic phase is dried on a rotary evaporator, separated and purified by column using a mixed eluent of petroleum ether and dichloromethane, and further recrystallized to obtain the target product m-DBPP or o-DBPP.

[0023] Preferably, the eluents in step S1 are petroleum ether and dichloromethane, and the volume ratio of the eluents is 1:1.

[0024] Preferably, the eluents in step S3 are petroleum ether and dichloromethane, and the volume ratio between the two is 2:1.

[0025] The present application also provides an organic electroluminescent device, which includes a light-emitting layer formed by mixing a host material and the above-mentioned solution-processable thermally activated delayed fluorescent red light material.

[0026] Preferably, the mass proportion of the organic thermally activated delayed fluorescent material in the light-emitting layer is 0.4-20%.

[0027] More preferably, the organic electroluminescent device further comprises a substrate, an anode electrode, a hole transport layer, a light-emitting layer, an electron transport layer and a cathode electrode arranged in sequence from bottom to top, and the thickness of the light-emitting layer is 20 to 40 nm.

[0028] More preferably, the anode electrode is ITO; the hole transport layer is PEDOT:PSS; the electron transport layer is TmPyPB; and the cathode electrode is LiF / Al.

[0029] More preferably, the main material is TCTA, and the substrate and anode electrodes are both ITO conductive glass.

[0030] Compared with the prior art, the beneficial effects of this application are:

[0031] 1. The solution-processable heat-activated delayed fluorescent red light material proposed in this application uses an electrophilic phenanthropyrazine structural unit as the receptor core to synthesize two heat-activated delayed fluorescent materials with a small ΔEst and good TADF properties. The pyrazine phenanthrophenanthrene structural unit has a certain rigidity, which can well inhibit non-radiative transitions and improve red light emission efficiency. In addition, the introduction of methyl benzoate greatly increases the solubility of the molecule, which provides favorable conditions for preparing devices in solution processing.

[0032] 2. Application Organic electroluminescent devices containing solution-processable thermally activated delayed fluorescent red light materials can be used for red light emission, with an external quantum efficiency (EQE) of up to 17%, excellent luminescence performance, and broad application prospects. They are expected to be widely used in fields such as flat panel displays and solid-state lighting. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] Figure 1 This is the hydrogen spectrum of the compound m-DBPP prepared in Example 1 of the present application measured by a Bruker 400 MHz superconducting nuclear magnetic resonance instrument.

[0034] Figure 2 This is the hydrogen spectrum of the compound o-DBPP prepared in Example 2 of the present application measured by a Bruker 400 MHz superconducting nuclear magnetic resonance instrument.

[0035] Figure 3 This is the absorption-emission (Abs-FL) spectrum of the m-DBPP thermally activated delayed fluorescent material with a molecular structure obtained in Example 1 of the present application at room temperature.

[0036] Figure 4 This is the thermogravimetric analysis curve of the organic thermally activated delayed fluorescent materials m-DBPP and o-DBPP.

[0037] Figure 5 This is a graph showing the redox potential of the organic thermally activated delayed fluorescent material molecule m-DBPP according to Example 1 of the present application.

[0038] Figure 6 This is a photoluminescence decay curve of measuring transient lifetime of 5% m-DBPP, an organic thermally activated delayed fluorescent material molecule of Example 1 of the present application, doped in CBP.

[0039] Figure 7 This is a photoluminescence decay curve diagram of the long lifespan measured when 5% m-DBPP, an organic thermally activated delayed fluorescent material molecule of Example 1 of the present application, is doped in CBP.

[0040] Figure 8 This is an electroluminescence spectrum of an organic electroluminescent device of the thermally activated delayed fluorescent material m-DBPP obtained in Example 1 of the present application.

[0041] Fig. 9 This is a current density-voltage-luminescence intensity curve of an organic electroluminescent device of the thermally activated delayed fluorescent material m-DBPP obtained in Example 1 of the present application.

[0042] Fig.10 This is a graph of the external quantum efficiency (EQE) of an organic electroluminescent device of the thermally activated delayed fluorescent material m-DBPP obtained in Example 1 of the present application.

[0043] Fig.11 This is the absorption-emission (Abs-FL) spectrum of the thermally activated delayed fluorescent material molecule o-DBPP obtained in Example 2 of the present application.

[0044] Fig.12 This is a graph showing the redox potential of the thermally activated delayed fluorescent material molecule o-DBPP obtained in Example 2 of the present application.

[0045] Fig.13 This is a photoluminescence decay curve diagram of the transient lifetime measured by 5% o-DBPP, a thermally activated delayed fluorescent material molecule obtained in Example 2 of the present application, doped in CBP.

[0046] Fig.14 This is a photoluminescence decay curve diagram of the measured lifetime of 5% o-DBPP, an organic thermally activated delayed fluorescent material molecule obtained in Example 2 of the present application, doped in CBP.

[0047] Fig.15This is an electroluminescence spectrum of an organic electroluminescent device of the thermally activated delayed fluorescent material o-DBPP obtained in Example 2 of the present application.

[0048] Fig.16 This is the current density-voltage-luminescence intensity curve of the organic electroluminescent device of the thermally activated delayed fluorescent material o-DBPP obtained in Example 2 of the present application.

[0049] Fig.17 This is a graph of the external quantum efficiency (EQE) of an organic electroluminescent device of the thermally activated delayed fluorescent material o-DBPP obtained in Example 2 of the present application.

[0050] Fig.18 This is the fluorescence and phosphorescence spectra of the thermally activated delayed fluorescent material m-DBPP obtained in Example 1 of the present application at 77K.

[0051] Fig.19 This is the fluorescence and phosphorescence spectra of the thermally activated delayed fluorescent material o-DBPP obtained in Example 2 of the present application at 77K. DETAILED DESCRIPTION

[0052] The embodiments of the present application will be described in detail below in conjunction with the examples, but it will be appreciated by those skilled in the art that the following examples are only used to illustrate the present application and should not be considered as limiting the scope of the present application. In the examples, if specific conditions are not specified, they are carried out according to normal conditions or the conditions recommended by the manufacturer. If the manufacturer is not specified for the reagents or instruments used, they are all conventional products that can be purchased commercially.

[0053] It should be noted that:

[0054] In this application, unless otherwise specified, all the embodiments and preferred implementation methods mentioned herein can be combined with each other to form a new technical solution.

[0055] In the present application, unless otherwise specified, percentage (%) or part refers to the weight percentage or weight part relative to the composition.

[0056] In the present application, unless otherwise specified, the components or preferred components involved can be combined with each other to form a new technical solution.

[0057] In this application, unless otherwise specified, the numerical range "a-b" represents an abbreviation of any real number combination between a and b, where a and b are real numbers. For example, the numerical range "1-5" means that all real numbers between "1-5" are listed in this document, and "1-5" is just an abbreviation of these numerical combinations.

[0058] The "range" disclosed in the present application is in the form of a lower limit and an upper limit, which can be one or more lower limits, and one or more upper limits, respectively.

[0059] In the present application, unless otherwise specified, each reaction or operation step can be carried out sequentially or in accordance with the sequence. Preferably, the reaction method herein is carried out sequentially.

[0060] Unless otherwise specified, the professional and scientific terms used in this article have the same meanings as those familiar to those skilled in the art. In addition, any method or material similar or equivalent to the content described herein can also be applied to this application. The present application provides a solution-processable heat-activated delayed fluorescent red light material, the structural formula of which has the following molecular structure:

[0061]

[0062] Wherein, R1 and R2 are H or 2-(methoxycarbonyl)phenyl; when R1 is H, R2 is 2-(methoxycarbonyl)phenyl; when R2 is H, R1 is 2-(methoxycarbonyl)phenyl, wherein the molecular structure of the 2-(methoxycarbonyl)phenyl is as follows:

[0063]

[0064] In some preferred embodiments, the molecular structure of the solution-processable thermally activated delayed fluorescent red light material is as follows:

[0065]

[0066] The present application also provides a method for preparing the above-mentioned solution-processable thermally activated delayed fluorescent red light material. The method comprises the following steps:

[0067] S1. Preparation of Intermediate A

[0068] 3,6-dibromo-9,10-phenanthrenequinone, phenoxazine, tri(dibenzylideneacetone)dipalladium, cesium carbonate and tri-tert-butylphosphine tetrafluoroborate are added to anhydrous toluene in a molar ratio of 1:(2.3-3):(0.04-0.1):(2.25-3):(0.1-0.2) under nitrogen protection to obtain a mixed solution A with a concentration of 0.03-0.05 mmol / ml of 3,6-dibromo-9,10-phenanthrenequinone, and the mixture is heated to 100-120° C. and stirred for reaction. After 3,6-dibromo-9,10-phenanthrenequinone is completely reacted, palladium salt and cesium carbonate precipitated during the reaction are filtered and distilled to obtain a crude product A; the crude product A is purified by a chromatographic column, and then the remaining phenoxazine and by-products are removed by an eluent, and the intermediate A is obtained after recrystallization, suction filtration and high-temperature sublimation;

[0069] S2. Preparation of intermediate product B1 or B2

[0070] The intermediate A and 4-bromobenzene-1,2-diamine or 3-bromobenzene-1,2-diamine are added to glacial acetic acid in a molar ratio of 1:(1.2-2) under nitrogen protection to obtain a mixed solution B with a concentration of 0.03-0.05 mmol / ml of the intermediate A, and the solution is heated to 100-130° C. and stirred for reaction. After the intermediate A is completely reacted, the solution is cooled to room temperature, poured into the prepared deionized water, filtered, and then recrystallized from ethanol to obtain an intermediate product B1 or B2;

[0071] S3. Preparation of target product m-DBPP or o-DBPP

[0072] The intermediate product B1 or B2, (2-(methoxycarbonyl)phenyl)boric acid, tetrakistriphenylphosphine palladium and 2M potassium carbonate are added to 1,4-dioxane in a molar ratio of 1:(1.5-2):(0.04-0.1):(2-4.5) under nitrogen protection to obtain a mixed solution C with a concentration of 0.03-0.05 mmol / ml of the intermediate product B1, and the mixture is heated to 100-105° C. and stirred for reaction. After the intermediate product is completely reacted, the mixture is cooled to room temperature, extracted with ethyl acetate EA and saturated brine for 1-2 times, and the organic phase is dried on a rotary evaporator, separated and purified by column using a mixed eluent of petroleum ether and dichloromethane, and further recrystallized to obtain the target product m-DBPP or o-DBPP.

[0073] In the preparation method described in the present application, the eluents in step S1 are petroleum ether and dichloromethane, and the volume ratio of the eluents is 1:1.

[0074] In the preparation method described in the present application, the eluents in step S3 are petroleum ether and dichloromethane, and the volume ratio of the eluents is 2:1.

[0075] The present application also provides an organic electroluminescent device, which includes a light-emitting layer formed by mixing a host material and the above-mentioned solution-processable thermally activated delayed fluorescent red light material.

[0076] In some preferred embodiments of the present application, the mass proportion of the organic thermally activated delayed fluorescent material in the light-emitting layer is 0.4-20%.

[0077] In some more preferred embodiments of the present application, the organic electroluminescent device further comprises a substrate, an anode electrode, a hole transport layer, a light-emitting layer, an electron transport layer and a cathode electrode arranged in sequence from bottom to top, and the thickness of the light-emitting layer is 20 to 40 nm.

[0078] In some more preferred embodiments of the present application, the anode electrode is ITO; the hole transport layer is PEDOT:PSS; the electron transport layer is TmPyPB; and the cathode electrode is LiF / Al.

[0079] In some more preferred embodiments of the present application, the main material is TCTA, and the substrate and anode electrodes are both ITO conductive glass.

[0080] The preparation method of the solution-processable thermally activated delayed fluorescent red light material compounds o-DBPP and m-DBPP will be described in detail below.

[0081] Example 1

[0082] This embodiment provides a solution-processable thermally activated delayed fluorescent red light material, the molecular structure of which is m-DBPP as shown below:

[0083]

[0084] The main synthetic route is as follows:

[0085]

[0086] The preparation method of the solution-processable thermally activated delayed fluorescent red light material m-DBPP specifically comprises the following steps:

[0087] S11. Preparation of Intermediate A

[0088] 3,6-dibromo-9,10-phenanthrenequinone (0.726 g, 2 mmol), phenoxazine (1.1 g, 5.6 mmol), tris(dibenzylideneacetone)dipalladium (0.0915 g, 0.1 mmol), cesium carbonate (2.6 g, 8 mmol) and tri-tert-butylphosphine tetrafluoroborate (0.087 g, 0.3 mmol) were added to a 100 mL two-necked round-bottom flask with a magnetic rod in sequence, and nitrogen was replaced three times. Under nitrogen protection, 30 mL of anhydrous toluene was drawn with a 50 mL syringe and added to the round-bottom flask, and the reaction was stirred at an oil bath temperature of 110 ° C for 24 h; thin layer chromatography (TCL) spot plate detection was used, and after 3,6-dibromo-9,10-phenanthrenequinone was completely reacted, it was cooled to room temperature, saturated brine and dichloromethane (DCM) were added for extraction, and the organic phase was separated, and the aqueous phase was extracted twice with DCM. The organic phase was dried over anhydrous magnesium sulfate and filtered. The solvent was removed from the obtained filtrate under reduced pressure. The product was purified by silica gel column using petroleum ether and dichloromethane (PE / DCM=1:1) as eluent to obtain a black solid (1.5 g 2.6 mmol) with a yield of 73%.

[0089] The chemical reaction equation in this preparation method is as follows:

[0090]

[0091] The obtained intermediate was subjected to 400 MHz 1 HMNR spectrum test detection, get 1 HMNR (400Mhz, CDCl3) δ8.46 (d, J=8.3Hz, 1H), 7.95 (d, J=1.9Hz, 1H), 6.74 (qd, J=7.9, 1.8Hz, 4H), 6.65 (ddd, J=8.0, 6.8, 2.1Hz, 2H), 6.12 (dd, J=7.9, 1.3Hz, 2H), indicating that intermediate A was obtained.

[0092] S12. Preparation of intermediate product B1

[0093] Add intermediate A (1.14 g, 2 mmol) and 4-bromobenzene-1,2-diamine (0.372 g, 2 mmol) to a 100 mL two-necked round-bottom flask with a magnetic magnet, replace nitrogen three times, and use a 20 mL syringe to extract 50 mL of glacial acetic acid and add it to the round-bottom flask under nitrogen protection. Stir the reaction at an oil bath temperature of 120 ° C for 12 hours, and use thin layer chromatography (TCL) spot plate detection. After the intermediate A is completely reacted, take out the reaction immediately, and pour the product after the reaction into 200 ml of deionized water. Filter, wash the obtained solid with water, and wash it again with anhydrous ethanol to obtain a reddish brown solid B1, dry it, and use it directly in the next step without column chromatography.

[0094] The chemical reaction equation in this preparation method is as follows:

[0095]

[0096] S13. Preparation of target product m-DBPP

[0097] To a 100mL two-necked round-bottom flask with a magnet, B1 (1.44g, 2mmol), (2-(methoxycarbonyl)phenyl)boric acid (0.54g, 3mmol), tetrakistriphenylphosphine palladium (0.12g, 0.1mmol), and 2MK2CO35ml were added in sequence, and nitrogen was replaced three times. Under nitrogen protection, 50mL 1,4-dioxane was extracted with a 50mL syringe and added to the round-bottom flask, and the reaction was stirred at an oil bath temperature of 100°C for 12h; thin layer chromatography (TCL) spot plate detection was used, and after B1 was completely reacted, the room temperature was cooled, extracted with EA and saturated brine, the organic phase was spin-dried, and the eluent of petroleum ether and dichloromethane (PE / DCM=2:1) ​​was used to purify by chromatographic column to obtain the red target product m-DBPP (2.1g 2.7mmol) with a yield of 71%.

[0098] The chemical reaction equation in this preparation method is as follows:

[0099]

[0100] Example 2

[0101] This embodiment provides a solution-processable thermally activated delayed fluorescent red light material, the molecular structure of which is o-DBPP as shown below:

[0102]

[0103] The main synthetic route is as follows:

[0104]

[0105] The preparation method of the solution-processable thermally activated delayed fluorescent red light material m-DBPP specifically comprises the following steps:

[0106] S21. Preparation of Intermediate A

[0107] The synthesis route and synthesis method steps of step S21 here are exactly the same as those of step S11 in Example 1. For specific operations, please refer to the method and steps of step S11 in Example 1.

[0108] S22. Preparation of intermediate product B2

[0109] Add intermediate A (1.14 g, 2 mmol) and 3-bromobenzene-1,2-diamine (0.372 g, 2 mmol) to a 100 mL two-necked round-bottom flask with a magnet, replace nitrogen three times, and under nitrogen protection, use a 20 mL syringe to extract 50 mL of glacial acetic acid and add it to the round-bottom flask. Stir the reaction for 12 hours at an oil bath temperature of 120 ° C. Use thin layer chromatography (TCL) spot plate detection. After the intermediate A is completely reacted, take out the reaction immediately and pour the product after the reaction into 200 ml of deionized water. Filter, wash the obtained solid with water, and wash it again with anhydrous ethanol to obtain a reddish brown solid B2, dry it, and use it directly in the next step without column chromatography. The chemical reaction equation in this preparation method is as follows:

[0110]

[0111] S23. Preparation of target product o-DBPP

[0112] To a 100mL two-necked round-bottom flask with a magnet, B2 (1.44g, 2mmol), (2-(methoxycarbonyl)phenyl)boric acid (0.54g, 3mmol), tetrakistriphenylphosphine palladium (0.12g, 0.1mmol), and 2MK2CO35ml were added in sequence, and nitrogen was replaced three times. Under nitrogen protection, 50mL 1,4-dioxane was extracted with a 50mL syringe and added to the round-bottom flask, and the reaction was stirred at an oil bath temperature of 100°C for 12h; thin layer chromatography (TCL) spot plate detection was used, and after B2 was completely reacted, the room temperature was cooled, extracted with EA and saturated brine, the organic phase was spin-dried, and an eluent of petroleum ether and dichloromethane (PE / DCM=2:1) ​​was used to purify by a chromatographic column to obtain the red target product o-DBPP (1.9g 2.7mmol) with a yield of 70%.

[0113] The chemical reaction equation in this preparation method is as follows:

[0114]

[0115] Characterization and performance testing

[0116] The compounds prepared in Examples 1 and 2 were characterized and tested for performance. Figures 1 to 11 shown.

[0117] Figure 1 The compound m-DBPP prepared in Example 1 of the present application was tested for hydrogen spectrum by a Bruker 400MHz superconducting nuclear magnetic resonance instrument, and the solvent was deuterated chloroform. The intermediate obtained was tested by a Bruker 500MHz instrument 1 HMNR spectrum test detection, get 1H NMR(500MHz,Chloroform-d)δ9.71(t,J=8.5Hz,2H),8.49(d,J=2.1Hz,2H),8.44–8.37(m,2H),8.04(dd,J=7.8 ,1.3Hz,1H),7.88(dd,J=8.7,1.9Hz,1H),7.78(ddd,J=8.4,6.4,1.9Hz,2H),7.68(td,J=7.4,1.4Hz,1H),7.60( dd, J = 7.8, 1.4 Hz, 1H), 7.56 (td, J = 7.6, 1.3 Hz, 1H), 6.72 (dt, J = 8.0, 1.7 Hz, 4H), 6.65 (s, 4H), 6.61–6.54 (m, 4H), 6.04 (dd, J = 8.3, 3.6 Hz, 4H), 3.69 (s, 3H), the integral value of the nuclear magnetic resonance hydrogen spectrum is basically consistent with the theoretical value of the target luminescent molecule, and it can be determined that the solution-processable thermally activated delayed fluorescent red light material m-DBPP is obtained. Moreover, the peaks in the above hydrogen spectrum can correspond one-to-one with the hydrogen atoms of the m-DBPP molecule, and the number is reasonable, indicating that the synthesis of m-DBPP is obtained, and the structure is single and the purity is high.

[0118] Figure 2 The compound o-DBPP prepared in Example 2 of the present application was tested for hydrogen spectrum by a Bruker 400MHz superconducting nuclear magnetic resonance instrument, and the solvent was deuterated chloroform. The intermediate obtained was tested by a Bruker 500MHz instrument 1 HMNR spectrum test detection, get 1H NMR(500MHz,Chloroform-d)δ9.72(d,J=8.5Hz,1H),9.22(d,J=8.5Hz,1H),8.48–8.40(m,3H),8.18–8.12(m,1H),8.02(dd,J=8. 5,7.0Hz,1H),7.96(dd,J=7.0,1.4Hz,1H),7.77(dd,J=8.5,1.9Hz,1H),7.72(td,J=7.5,1.5Hz,1H),7.66(dd,J=8.5,1.9Hz,1H) ,7.61(td,J=8.5,8.0,1.3Hz,2H),6.71(td,J=7.9,1.5Hz,4H),6.68–6.60(m,4H),6.55(dtd,J=15.5,7.7,1.6Hz,4H),6.03(dd,J=8.0,1.4Hz,2H),5.96(dd,J=8.0,1.4Hz,2H),3.23(s,3H), the integral value of the nuclear magnetic resonance hydrogen spectrum is basically consistent with the theoretical value of the target luminescent molecule, and it can be determined that the solution-processable thermally activated delayed fluorescent red light material o-DBPP is obtained. And the peaks in the above hydrogen spectrum can correspond one-to-one with the hydrogen atoms of the o-DBPP molecule, and the number is reasonable, indicating that o-DBPP is synthesized, and the structure is single and the purity is high.

[0119] Figure 3 The normalized absorption spectrum of the ultraviolet absorption and emission spectra of the compound m-DBPP in toluene solvent measured by Shimadzu UV-2700 ultraviolet visible spectrophotometer is shown in the figure. The organic thermally activated delayed fluorescent material with a molecular structure of m-DBPP obtained in Example 1 was prepared with toluene at a concentration of 10-5 mol / L, and the absorption and emission (Abs-FL) spectrum was measured at room temperature, as shown in the figure. Figure 3 As shown, it can be seen that the absorption peak of the organic thermally activated delayed fluorescent material with the molecular structure of m-DBPP is at 459nm, indicating that it has a good TADF charge transfer state, and the emission peak is at 620nm, indicating that it can achieve red light emission.

[0120] Figure 4 Thermogravimetric analysis curves of organic thermally activated delayed fluorescent materials m-DBPP and o-DBPP. Figure 4 It can be seen that the thermal decomposition temperatures of the molecular structures of m-DBPP and o-DBPP are 445°C and 458°C, indicating that both have good thermal stability.

[0121] The present application also applies the solution-processable phenanthropyrazine receptor organic thermally activated delayed fluorescent material m-DBPP prepared in Example 1 to an organic electroluminescent device. Specifically, the OLED structure includes a glass substrate, an ITO anode electrode, a 40nm thick PEDOT:PSS hole transport layer, a 40nm thick TCTA:m-DBPP light-emitting layer, a 40nm thick TmPyPB electron transport layer, and a LiF / Al cathode electrode arranged in sequence from bottom to top; wherein the TCTA:m-DBPP light-emitting layer is a mixed film formed by mixing the main material TCTA and the organic thermally activated delayed fluorescent material with a molecular structure of m-DBPP.

[0122] like Figure 5 As shown, by testing the redox potential curve of the organic thermally activated delayed fluorescent material with a molecular structure of m-DBPP, it can be seen that its oxidation potential is -5.21eV and its reduction potential is -3.11eV, which can well match the energy level of the main material TCTA.

[0123] like Figure 6 and Figure 7 As shown, the luminescence decay curve of the organic thermally activated delayed fluorescence material with a tested molecular structure of m-DBPP in the TCTA:m-DBPP luminescent layer shows that the transient lifetime of the thermally activated delayed fluorescence material with a molecular structure of m-DBPP is 76.1ns and the delayed lifetime is 5.8μs, indicating that it has significant TADF characteristics.

[0124] In Example 1 of the present application, a light-emitting layer of a thermally activated delayed fluorescent material is prepared, and the light-emitting performance of an organic electroluminescent device containing an organic thermally activated delayed fluorescent material m-DBPP based on a solution-processable phenanthropyrazine acceptor is tested, and the following is obtained: Figure 8 The electroluminescence spectrum shown in the figure shows that the EL emission peak is 640nm, which is significantly red-shifted compared to 620nm in toluene solution. This may be attributed to the strong intermolecular interaction between the host and the guest, resulting in strong charge transfer. Fig. 9 The current density-voltage-luminous intensity curves shown in FIG. 1 show that the changing trends of the current density-voltage-luminous intensity match each other, indicating that the selected device structure is feasible. Fig.10 The external quantum efficiency (EQE) diagram shown in the figure shows that when the device with organic thermally activated delayed fluorescent material is at the maximum EQE, 100 cd.m -2 and 1000cd.m -2 The device efficiency achieved high efficiencies close to 16.2%, 16.1% and 12.3%.

[0125] The organic thermally activated delayed fluorescent material with a molecular structure of o-DBPP obtained in Example 2 was prepared at a concentration of 10 -5 mol / L toluene, the absorption emission (Abs-FL) spectrum measured at room temperature, such as Fig.11 As shown, it can be seen that the absorption peak of the organic thermally activated delayed fluorescent material with a molecular structure of o-DBPP is at 463nm, indicating that it has a good TADF charge transfer state, and the emission peak is at 625nm, indicating that it can achieve red light emission.

[0126] The present application also applies the solution-processable phenanthropyrazine receptor organic thermally activated delayed fluorescent material o-DBPP prepared in Example 2 to an organic electroluminescent device. Specifically, the OLED structure includes a glass substrate, an ITO anode electrode, a 40nm thick PEDOT:PSS hole transport layer, a 40nm thick TCTA:o-DBPP luminescent layer, a 40nm thick TmPyPB electron transport layer, and a LiF / Al cathode electrode arranged in sequence from bottom to top; wherein the TCTA:o-DBPP luminescent layer is a mixed film formed by mixing the main material TCTA and the organic thermally activated delayed fluorescent material with a molecular structure of o-DBPP.

[0127] like Fig.12 As shown in the figure, the redox potential curve of the organic thermally activated delayed fluorescent material with a molecular structure of o-DBPP is tested. By testing the redox potential curve of the organic thermally activated delayed fluorescent material with a molecular structure of o-DBPP, it can be seen that its oxidation potential is -5.22eV and its reduction potential is -3.09eV, which can match the energy level of the main material TCTA well.

[0128] like Fig.13 and Fig.14 As shown in the figure, the luminescence decay curve of the organic thermally activated delayed fluorescence material with a molecular structure of o-DBPP in the TCTA:o-DBPP luminescent layer shows that the transient lifetime of the organic thermally activated delayed fluorescence material with a molecular structure of o-DBPP is 74.1ns and the delayed lifetime is 6.8μs, indicating that it has significant TADF characteristics.

[0129] In Example 2 of the present application, a light-emitting layer of an organic thermally activated delayed fluorescent material is prepared, and the light-emitting performance of an organic electroluminescent device containing an organic thermally activated delayed fluorescent material (o-DBPP) based on a solution-processable pyrazinophenanthrene acceptor is tested, and the following results are obtained: Fig.15 The electroluminescence spectrum shown in the figure shows that the EL emission peak is 644nm, which is significantly red-shifted compared to 625nm in toluene solution. This may be attributed to the strong intermolecular interaction between the host and the guest, resulting in strong charge transfer. Fig.16 The current density-voltage-luminous intensity curves shown in FIG. 1 show that the changing trends of the current density-voltage-luminous intensity match each other, indicating that the selected device structure is feasible. Fig.17 The external quantum efficiency (EQE) diagram shown in the figure shows that when the device with organic thermally activated delayed fluorescent material is at the maximum EQE, 100 cd.m -2 and 1000cd.m -2 The device efficiency achieved high efficiencies close to 14.4%, 14.2% and 11%.

[0130] The present application proposes a solution-processable thermally activated delayed fluorescent red light material, a preparation method and an application thereof, and synthesizes two thermally activated delayed fluorescent materials with a small ΔEst (from Fig.18 and Fig.19 It can be seen that the pyrazinophenanthrene structural unit has a certain rigidity, which can well inhibit non-radiative transitions and improve the red light emission efficiency. In addition, the introduction of methyl benzoate greatly increases the solubility of the molecule, which provides favorable conditions for the preparation of devices in solution processing, as shown in the following table:

[0131] Table 1

[0132]

[0133] The present application also applies the prepared solution-processable thermally activated delayed fluorescent red light material to organic electroluminescent devices for red light emission, with an external quantum efficiency (EQE) of up to 17%, excellent luminescence performance, and broad application prospects, and is expected to be widely used in fields such as flat panel displays and solid-state lighting.

[0134] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "illustrative embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials, or characteristics described in conjunction with the embodiments or examples are included in at least one embodiment or example of the present application. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials, or characteristics described may be combined in any one or more embodiments or examples in a suitable manner.

[0135] Although several embodiments of the present application have been shown and described, those skilled in the art will appreciate that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present application, and that the scope of the present application is defined by the claims and their equivalents.

Claims

1. A solution-processable thermally activated delayed fluorescent red light material, characterized in that: It has a molecular structure as shown in formula (1): Wherein, R1 and R2 are H or 2-(methoxycarbonyl)phenyl; when R1 is H, R2 is 2-(methoxycarbonyl)phenyl; when R2 is H, R1 is 2-(methoxycarbonyl)phenyl, wherein the molecular structure of the 2-(methoxycarbonyl)phenyl is as follows:

2. The solution-processable thermally activated delayed fluorescent red light material according to claim 1, characterized in that: The molecular structure of the solution-processable thermally activated delayed fluorescent red light material is as follows:

3. The method for preparing the solution-processable thermally activated delayed fluorescent red light material according to claim 2, characterized in that: The following steps are involved: S1. Preparation of Intermediate A 3,6-dibromo-9,10-phenanthrenequinone, phenoxazine, tri(dibenzylideneacetone)dipalladium, cesium carbonate and tri-tert-butylphosphine tetrafluoroborate are added to anhydrous toluene in a molar ratio of 1:(2.3-3):(0.04-0.1):(2.25-3):(0.1-0.2) under nitrogen protection to obtain a mixed solution A with a concentration of 0.03-0.05 mmol / ml of 3,6-dibromo-9,10-phenanthrenequinone, and the mixture is heated to 100-120° C. and stirred for reaction. After 3,6-dibromo-9,10-phenanthrenequinone is completely reacted, palladium salt and cesium carbonate precipitated during the reaction are filtered and distilled to obtain a crude product A; the crude product A is purified by a chromatographic column, and then the remaining phenoxazine and by-products are removed by an eluent, and the intermediate A is obtained after recrystallization, suction filtration and high-temperature sublimation; S2. Preparation of intermediate product B1 or B2 The intermediate A and 4-bromobenzene-1,2-diamine or 3-bromobenzene-1,2-diamine are added to glacial acetic acid in a molar ratio of 1:(1.2-2) under nitrogen protection to obtain a mixed solution B with a concentration of 0.03-0.05 mmol / ml of the intermediate A, and the solution is heated to 100-130° C. and stirred for reaction. After the intermediate A is completely reacted, the solution is cooled to room temperature, poured into the prepared deionized water, filtered, and then recrystallized from ethanol to obtain an intermediate product B1 or B2; S3. Preparation of target product m-DBPP or o-DBPP The intermediate product B1 or B2, (2-(methoxycarbonyl)phenyl)boric acid, tetrakistriphenylphosphine palladium and 2M potassium carbonate are added to 1,4-dioxane in a molar ratio of 1:(1.5-2):(0.04-0.1):(2-4.5) under nitrogen protection to obtain a mixed solution C with a concentration of 0.03-0.05 mmol / ml of the intermediate product B1, and the mixture is heated to 100-105° C. and stirred for reaction. After the intermediate product is completely reacted, the mixture is cooled to room temperature, extracted with ethyl acetate EA and saturated brine for 1-2 times, and the organic phase is dried on a rotary evaporator, separated and purified by column using a mixed eluent of petroleum ether and dichloromethane, and further recrystallized to obtain the target product m-DBPP or o-DBPP.

4. The method for preparing the solution-processable thermally activated delayed fluorescent red light material according to claim 3, characterized in that: The eluents in step S1 are petroleum ether and dichloromethane, and the volume ratio of the eluents is 1:

1.

5. The method for preparing the solution-processable thermally activated delayed fluorescent red light material according to claim 3, characterized in that: The eluents in step S3 are petroleum ether and dichloromethane, and the volume ratio of the eluents is 2:

1.

6. An organic electroluminescent device, characterized in that: The invention comprises a light-emitting layer which is formed by mixing a main material and the solution-processable thermally activated delayed fluorescent red light material as claimed in claim 1 or 2.

7. The organic electroluminescent device according to claim 6, characterized in that: The weight percentage of the organic thermally activated delayed fluorescent material in the light-emitting layer is 0.4-20%.

8. The organic electroluminescent device according to claim 7, characterized in that: The organic electroluminescent device further comprises a substrate, an anode electrode, a hole transport layer, a light emitting layer, an electron transport layer and a cathode electrode which are sequentially arranged from bottom to top, and the thickness of the light emitting layer is 20-40 nm.

9. The organic electroluminescent device according to claim 8, characterized in that: The anode electrode is ITO; the hole transport layer is PEDOT:PSS; the electron transport layer is TmPyPB; and the cathode electrode is LiF / Al.

10. The organic electroluminescent device according to claim 9, characterized in that: The main material is TCTA, and the substrate and anode electrodes are both ITO conductive glass.

Citation Information

Patent Citations

  • Organic thermally-induced delayed fluorescence material based on pyrazine receptor as well as preparation method and application of organic thermally-induced delayed fluorescence material

    CN112961148A

  • Application of thermally active delayed fluorescent material capable of being processed in solution in blue light devices and hybrid white light devices

    CN113078278A

  • Organic electroluminescent material based on benzene carbonyl dibenzophenazine and application of organic electroluminescent material in OLED (Organic Light Emitting Diode)

    CN114014841A

  • Red thermal activation delayed fluorescence material, organic electroluminescent device and preparation method of red thermal activation delayed fluorescence material

    CN114292264A

  • Compound, light-emitting material, delayed fluorescence material, and organic light-emitting element

    WO2022097626A1

Cited By

  • Red light-near infrared organic material based on triptycene bridging and preparation method and application thereof

    CN119954808A