Preparation method of supporting layer of scroll type display device

The supporting layer with a specific hollow pattern is formed through UV picosecond laser cutting, which solves the problem of poor folding traces and deformation recovery of the curled screen support layer in long-term use, and achieves better stability and service life.

CN118968885APending Publication Date: 2024-11-15XIAMEN JINGJIA PHOTOELECTRIC TECH
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411038212.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-31
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The support layer of the curled screen is prone to produce folding marks and poor recovery during long-term expansion and curling use, resulting in deformation or damage to the screen, limiting the stability and life of the product.

Method used

The composite layer is cut by ultraviolet picosecond laser to form a specific first hollow pattern and a second hollow pattern. Combined with the material and protective layer of the flexible film, a support layer with a cross-shaped pattern is designed, and the metal fixture and blowing is blown. The device removes cutting waste, ensuring the accuracy of the hollow pattern and no abnormal appearance.

Benefits of technology

The support layer is achieved uniform tension during the expansion and curling process, which reduces folding marks, improves stability and stretch uniformity, extends service life, and controls the thermal effect within ±0.005mm, ensuring the performance and appearance qualification.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004971687210000061
    Figure BDA0004971687210000061
  • Figure HDA0004971687230000011
    Figure HDA0004971687230000011
  • Figure HDA0004971687230000012
    Figure HDA0004971687230000012
Patent Text Reader

Abstract

The invention discloses a preparation method of a supporting layer of a scroll type display device. The preparation method comprises the following steps: laminating protective layers on two surfaces of a flexible film for forming the supporting layer to form a composite layer; the composite layer is cut through purple picosecond laser, first hollow-out patterns and second hollow-out patterns are formed, the first hollow-out patterns are arranged at intervals in an array mode, and the second hollow-out patterns are cross-shaped patterns arranged in the array intervals of the first hollow-out patterns; the composite layer is placed on a metal jig when being cut, the metal jig is provided with a groove, bosses are evenly distributed on the groove in a laser-path-free area and used for bearing the composite layer, an air blowing device is arranged above the metal jig, and cut waste materials are separated from the composite layer and fall into the groove through the air blowing device. Through the combination of the structure and the technology, the supporting layer can keep uniform tension in the unfolding and curling process, the large-amplitude stretching function is achieved, no crease or fracture exists after repeated bending and unfolding, the appearance is not abnormal, and the production yield is high.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of flexible displays, and in particular relates to a method for preparing a support layer of a scroll-type display device. Background Art

[0002] Rollable screens are a new type of display technology that can be unfolded and rolled up to provide a zooming experience. They can freely change size, making the display more flexible and portable, and providing users with a better visual experience. Rollable phones and other applications of rollable screens are examples.

[0003] In addition to flexible deformation, a rollable screen also requires a certain level of support and resilience to ensure a pleasant user experience and tactile quality during use. Therefore, a support layer is necessary. During long-term unfolding and curling, the support layer is prone to folding marks and poor deformation recovery due to the stress. Furthermore, prolonged stretching can easily lead to delamination, which can cause screen deformation or even breakage, limiting the product's stability and lifespan. Summary of the Invention

[0004] In view of the deficiencies in the prior art, the present invention provides a method for preparing a support layer of a scroll-type display device.

[0005] In order to achieve the above objectives, the technical solution of the present invention is:

[0006] A method for preparing a support layer of a scroll-type display device, comprising:

[0007] Laminating protective layers on both sides of a flexible film used to form a support layer to form a composite layer;

[0008] The composite layer is cut using an ultraviolet picosecond laser to form a first hollow pattern and a second hollow pattern. The first hollow pattern is arranged in an array and spaced apart, and the second hollow pattern is a cross pattern arranged in the array intervals of the first hollow pattern. The cutting speed of the ultraviolet picosecond laser is 1300-1700 mm / s, the frequency is 1900-2200 kHz, and the cutting depth is to the thickness of the composite layer.

[0009] The composite layer is placed on a metal jig during cutting. The metal jig is provided with grooves. The grooves have evenly distributed bosses in the area without the laser path for receiving the composite layer. An air blowing device is provided above the metal jig to separate the cut waste from the composite layer and drop it into the grooves.

[0010] Optionally, the wavelength of the ultraviolet picosecond laser is 355 nm, the power of the laser generator is 30 W, the output power is 5%, and the number of cutting times is 20 to 30 times.

[0011] Optionally, the material of the film used for the support layer is PET, PU or CPI, and the thickness is 0.05 to 0.09 mm.

[0012] Optionally, the flexible film used to form the support layer is respectively adhered to a first protective layer and a second protective layer on both sides, the thickness of the first protective layer is 0.04 to 0.06 mm, and the thickness of the second protective layer is 0.06 to 0.08 mm. During cutting, the laser light is incident from the first protective layer.

[0013] Optionally, a PSA layer with a thickness of 0.01 to 0.03 mm is provided between the first protective layer and the flexible film.

[0014] Optionally, adjacent rows in the array of the first hollow patterns are staggered, and the center of the cross pattern is located between two adjacent first hollow patterns in the row, and extends to the four spacing areas between the two adjacent first hollow patterns and the upper and lower rows of first hollow patterns to form a cross shape.

[0015] Optionally, the cross-shaped patterns are arranged in alternate rows in the array of the first hollow patterns, and the bosses are correspondingly located between two adjacent first hollow patterns in the alternate rows.

[0016] Optionally, the minimum width of the cross-shaped pattern is ≤0.2 mm.

[0017] Optionally, the characteristic size of the first hollow pattern is 2 to 3 mm.

[0018] Optionally, the air outlet direction of the blowing device is perpendicular to the surface of the composite layer, and the air pressure is 0.2-0.3 MPa.

[0019] The characteristic size mentioned here refers to the diameter of the circumscribed circle of the first hollow pattern. For a diamond pattern, it is the length of the diagonal line; for an elliptical pattern, it is the length of the major axis.

[0020] The beneficial effects of the present invention are:

[0021] (1) By combining the first hollow pattern and the second hollow pattern, the flexible support layer can maintain uniform tension during the unfolding and curling process, thereby reducing the generation of folding marks and achieving a large-scale stretching function, providing better support for the scroll-type display device, having strong stability, stretching uniformity and recovery, avoiding screen deformation, cracking, etc., and improving service life;

[0022] (2) The size after cutting meets the precision requirements of the structural design, with no burrs, damage or carbonization on the edges, and no abnormal appearance; repeated bending and unfolding without creases or breaks, good performance, and thermal effect can be controlled within ±0.005mm;

[0023] (3) Under the premise of ensuring the performance and appearance are qualified, waste can be eliminated efficiently and the defective rate can be reduced. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 is a schematic diagram of the cross-sectional structure of the composite layer of an embodiment;

[0025] Figure 2 A schematic diagram of laser cutting of a composite layer of an embodiment;

[0026] Figure 3a is a schematic structural diagram of the support layer of Example 1, Figure 3b This is a partially enlarged schematic diagram of the support layer of Example 1. Figure 3c Schematic diagram of the first hollow pattern and the second hollow pattern of the support layer of Example 1;

[0027] Figure 4 This is a photo of the appearance of the support layer of Example 1;

[0028] Figure 5a to Figure 5g These are the appearance photos of the support layers of Comparative Examples 1 to 7 respectively;

[0029] Figure 6a is a schematic structural diagram of the support layer of Example 2, Figure 6b This is a partially enlarged schematic diagram of the support layer of Example 2. Figure 6c Schematic diagram of the first hollow pattern and the second hollow pattern of the support layer of Example 2. DETAILED DESCRIPTION

[0030] The present invention is further explained below with reference to the accompanying drawings and specific embodiments. The drawings are provided for illustrative purposes only to facilitate understanding of the present invention, and their specific proportions may be adjusted according to design requirements. Those skilled in the art will understand that the vertical relationships between components and the definitions of front and back in the figures described herein refer to the relative positions of components. Therefore, they can be flipped to present the same components, and all such representations are within the scope of this specification.

[0031] The method for preparing the support layer of the scroll-type display device of the embodiment includes compounding multiple layers of materials and laser cutting the compound layer through an ultraviolet picosecond laser to form a hollow pattern, and removing the cutting waste to obtain a support layer with a specific hollow pattern for use in the scroll-type display device.

[0032] refer to Figure 1, the flexible film forming the support layer is selected from materials that are flexible, wear-resistant, high-temperature resistant, corrosion-resistant, and have good elasticity and recovery properties to ensure that the support layer will not be deformed or damaged during the unfolding and curling process. The flexible film is preferably PET, PU or CPI, with a thickness of 0.05 to 0.09 mm. Among them, PET (polyethylene terephthalate) film has excellent transparency, impact resistance and UV resistance; PU (polyurethane) film has excellent flexibility, elasticity and wear resistance; CPI (colorless and transparent polyimide) film has excellent high-temperature resistance, chemical corrosion resistance and wear resistance, and has excellent electrical and optical properties. The two sides of the flexible film 1' are respectively adhered to the first protective layer 2 and the second protective layer 3 to form a composite layer. The protective layer provides protection for the surface of the flexible film 1' during the manufacturing process to avoid pollution or damage that affects the performance. The thickness of the first protective layer 2 is 0.04-0.06 mm, and the thickness of the second protective layer 3 is 0.07-0.08 mm. The first protective layer is, for example, a PET protective film, and the second protective layer is, for example, a textured protective film. A PSA (pressure-sensitive adhesive) layer 4 with a thickness of 0.01-0.03 mm is located between the first protective layer 2 and the flexible film 1'.

[0033] refer to Figure 2 , place the composite layer on the metal jig 5, and use an ultraviolet picosecond laser to cut the composite layer to form a first hollow pattern and a second hollow pattern, wherein the first hollow pattern is arranged in an array and spaced apart, and the second hollow pattern is a cross pattern arranged in the array interval of the first hollow pattern. Specifically, the adjacent rows in the array of the first hollow pattern are staggered, and the center of the cross pattern is located between the two adjacent first hollow patterns in the row, and extends to the four spacing areas between the two adjacent first hollow patterns and the upper and lower rows of the first hollow patterns to form a cross shape. The cross pattern is arranged in alternate rows in the array of the first hollow pattern. The design of the first hollow pattern can remain flat when unfolded, and can automatically curl when curled; the cross hollow design can increase the flexibility, elasticity and stability of the structure, so that the support layer can maintain uniform tension during the unfolding and curling process to reduce the generation of folding marks.

[0034] During cutting, one side of the second protective layer 3 is placed on the metal jig 5, and the laser is incident from the side of the first protective layer 2. The wavelength of the ultraviolet picosecond laser used is 355nm, the power of the laser generator is 30W, the output power is 5%, the cutting speed is 1300-1700mm / s, the frequency is 1900-2200khz, and the number of cuts is controlled until the composite material is completely cut off. The characteristic size of the first hollow pattern is 2-3mm, and the minimum width of the second hollow pattern is ≤0.2mm. Other cutting technologies, such as die-cutting and carbon dioxide infrared light cutting, cannot achieve the above-mentioned precision standards. The cutting gap is too large and the appearance does not meet the design requirements. By using ultraviolet picosecond laser through parameter control, the cutting gap requirement of less than 0.15mm line width can be achieved, and the thermal effect range can be controlled within ±0.005mm, achieving the appearance requirements of fine patterns.

[0035] The metal jig 5 is provided with a groove 51, and the bosses 52 for receiving the composite layer are evenly distributed in the groove 51. The distribution of the bosses 52 is designed according to the structure of the support layer and is distributed in the area without the laser path to ensure the flatness of the material during cutting. For example, the bosses can be distributed between two adjacent first hollow patterns in the above-mentioned interval rows. The metal jig 5 is an air suction and waste discharge jig, and a blowing device 6 is provided on the top. During cutting, the blowing device 6 is used to separate the cut waste from the composite layer and fall into the groove. The cut material is removed from the jig and the waste in the jig is cleaned to ensure that the waste is removed in time and does not cause secondary pollution to the product. Specifically, the wind direction of the blowing device 6 is perpendicular to the surface of the composite layer, and the air pressure is 0.25Mp. After the flexible film is cut, a support layer 1 with a hollow pattern is formed.

[0036] Example 1

[0037] like Figure 3a to Figure 3c As shown, the first hollow pattern of the support layer 1A is a diamond pattern 11, preferably a square. The extension direction of one diagonal of each diamond pattern 11 in the array is consistent with the row direction (X direction in the figure), and the extension direction of the other diagonal is consistent with the Y direction. The X direction and the Y direction are perpendicular to each other; the upper and lower rows are staggered, that is, in the Y direction, the diamond patterns 11 are aligned in alternate rows. The center 121 of the cross pattern 12 is located between two adjacent diamond patterns 11a and 11b in the row, and extends to the four spacing areas between the two adjacent diamond patterns 11a and 11b and the upper and lower row diamond patterns 11c and 11d to form arms 122, thereby achieving a uniform stress dispersion effect. Thus, grid lines 13 of the same width are formed by the spacing areas of the diamond patterns 11. The use of a grid structure can improve flatness when unfolded, and can automatically curl when curled, and can be stretched and contracted in multiple directions, with good flexibility and elasticity. The center 121 of the cross pattern 12 is located at the intersection 13a of the grid lines 13. Combined Figure 3b and Figure 3c, the arm length L2 of the cross pattern 12 is not less than the side length L1 of the diamond pattern 11, and is less than the distance between the center points of adjacent intersections. Therefore, the cross pattern 12 can be considered to be arranged in rows and columns of diamond patterns 11, aligned in the Y direction, with the arms 122 of four adjacent cross patterns 12 converging at the intersection 13b in the alternate row, but not connected to each other. Compared to an overall membrane structure without a hollow pattern design, the combination of diamond and cross patterns can increase the stretching amplitude by more than 10%, and the flatness error is controlled within ±0.10mm, effectively reducing the occurrence of screen creases.

[0038] In the row direction, Figure 3c As shown, the length of the diagonal line L3 of the diamond pattern 11 is 2.5 to 3 mm, and the spacing L4 between adjacent diamond patterns 11 is 40% to 60% of the length of the diagonal line L3 of the diamond pattern. For example, the length of the diagonal line L3 is 2.7 mm, and the spacing L4 is 1.3 mm. This provides a suitable hollowing degree to provide better bending ability and stretchability, avoiding excessive deformation after stretching, resulting in poor recovery, and insufficient hollowing area, resulting in delamination and breakage due to the inability to release tension during bending. The arm width D1 of the cross pattern is 10% to 30% of the width D2 of the grid line. For example, the arm width D1 is 0.15 mm and the grid line width D2 is 0.85 mm. This can provide a more reasonable stress-bearing structure while meeting the processing accuracy requirements. The four corners of the diamond pattern 11 are rounded structures 111, and the corners of the cross pattern 12 are all rounded structures 123, which can effectively avoid stress concentration and make the stress more uniform.

[0039] The support layer 1A is made of a 0.075mm thick CPI flexible film, the first protective layer is 0.05mm thick, the second protective layer is 0.075mm thick, and the PSA layer is 0.025mm thick. The composite layer is placed on the metal fixture 4, with the bosses 42 corresponding to the intersections 13b. The cutting speed of the ultraviolet picosecond laser is 1500mm / s, the frequency is 2000kHz, the number of cuts is 25, and the air pressure of the air blowing device during cutting is 0.25Mp. Figure 4 As shown, the size after cutting meets the above structural design requirements, the edges have no burrs, damage or carbonization, and the appearance is normal; repeated bending and unfolding have no creases or breaks, and the performance is good.

[0040] Comparative Examples 1 to 7

[0041] Comparative Examples 1 to 7 have the same structural design as Example 1, except that the laser parameters are set differently during the preparation process. The parameters and cutting effects of the products are shown in the following table, and the corresponding physical photos are shown in the following table. Figure 5a to Figure 5g shown.

[0042]

[0043] Regarding waste removal, in other comparative examples, a blow hole needle is used to remove small hole waste. This method removes waste that will fly everywhere, polluting the surrounding environment and causing secondary pollution to the product. Adhesive tape is used to remove waste. This method easily deforms the product, and the tape will indirectly contaminate the product. The material to be cut is placed horizontally on an acrylic plate with suction holes evenly distributed on the acrylic plate to fix the material. This method causes the material to appear yellowish overall, with waste bulging in some areas. In addition, smoke and dust cannot be discharged in time during laser cutting, and smoke and dust will adhere to the cut edge, causing yellowing and severe thermal effects. In the embodiment of the present invention, a hollow suction platform metal fixture is used to efficiently remove waste and reduce the defective rate while ensuring qualified performance and appearance.

[0044] Example 2

[0045] refer to Figure 6a to Figure 6c The first hollow pattern of the support layer 1B is an array of elliptical patterns 14 arranged in an alternating pattern of first and second rows a and b. The major axis of the elliptical patterns 14 in the first row a is aligned with the row direction (X direction in the figure), while the minor axis of the elliptical patterns 14 in the second row b is aligned with the row direction (X direction in the figure). The upper and lower rows are staggered so that the elliptical patterns 14 in the alternate rows are aligned in the Y direction, which is perpendicular to the X direction. The center 151 of the cross pattern 15 is located between two adjacent elliptical patterns 14a and 14b in the first row a. The cross pattern 15 extends into the four spacing areas between the two adjacent elliptical patterns 14a and 14b and the upper and lower rows of elliptical patterns 14c and 14d to form extensions 152. This achieves a uniform stress dispersion effect. The structure composed of an elliptical grid can remain flat when unfolded and can automatically curl when curled. The elliptical shape is characterized by its ability to expand and contract in one direction, providing good flexibility and elasticity. The center points of the elliptical patterns 14 in the second row b and the midpoints of the intervals between adjacent elliptical patterns 14 in the first row a are aligned in the Y direction. Furthermore, the distance between the farthest ends of adjacent elliptical patterns 14a and 14b in the first row a is equal to the distance between the farthest ends of elliptical patterns 14c and 14d in the upper and lower second rows b, thereby achieving a regular and uniform arrangement and providing a uniform force-bearing structure. The minor axis length L2 of the elliptical patterns 14 is 50% to 65% of the major axis length L1, for example, if the major axis length L1 is 2.4 mm and the minor axis length L2 is 1.4 mm. In the first row a, the distance L3 between adjacent elliptical patterns 14 is 60% to 70% of the major axis length L1, for example, 1.6 mm. This provides an appropriate degree of hollowing for good bending and stretchability, avoiding excessive deformation after stretching, resulting in poor recovery, and insufficient hollowing, resulting in tension release during bending, leading to delamination and breakage.

[0046] The cross-shaped pattern 15 is located between adjacent elliptical patterns 14a and 14b in the first row a. The line segment facing the adjacent elliptical pattern 14 is a first arc segment 153 parallel to the elliptical pattern 14. The distance L4 between the first arc segment 153 and the elliptical pattern 14 is 15% to 25% of the distance L3 between the adjacent elliptical patterns, for example, 0.35 mm. An extension 152 is formed between the two first arc segments 153. The ends of the extension 152 are enclosed by a second arc segment 154, making the width of the ends of the extension 152 greater than the width of the middle, with the minimum width in the middle being 0.16 mm. The extensions 152 of the four adjacent cross-shaped patterns 15 converge between the two adjacent elliptical patterns in the second row b and are not connected to each other. The cross-shaped pattern 15 is formed by the smooth transition of arc segments, which effectively avoids stress concentration and ensures more uniform stress distribution. Compared with the overall membrane structure without hollow pattern design, the combination of the above-mentioned elliptical pattern and cross pattern can increase the stretching amplitude by more than 10%, and the flatness error is controlled within ±0.10mm, effectively reducing the occurrence of screen creases.

[0047] The support layer 1B is constructed of a 0.075mm thick PET flexible film, with a first protective layer of 0.05mm, a second protective layer of 0.075mm, and a PSA layer of 0.025mm. This composite layer is then placed on a metal fixture 5, with bosses 42 corresponding one-to-one with the spacing between two adjacent elliptical patterns in row b of the second arrangement. The UV picosecond laser cuts at a speed of 1500mm / s, a frequency of 2000kHz, and 25 cuts. The air pressure of the air blowing device during cutting is 0.25MPa. The cut dimensions meet the aforementioned structural design requirements, with no burrs, damage, or carbonization on the edges, and no abnormalities in appearance. Repeated bending and unfolding produce no creases or breaks, demonstrating excellent performance. Testing has shown that the support layer 1B maintains good ductility and resilience after hundreds of thousands of bends.

[0048] The above embodiments are only used to further illustrate a method for preparing a supporting layer of a scroll-type display device of the present invention, but the present invention is not limited to the embodiments. Any simple modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention fall within the protection scope of the technical solution of the present invention.

Claims

1. A method for preparing a support layer of a scroll display device, characterized in that: include: Laminating protective layers on both sides of a flexible film used to form a support layer to form a composite layer; The composite layer is cut by ultraviolet picosecond laser to form a first hollow pattern and a second hollow pattern, wherein the first hollow pattern is arranged in an array and spaced apart, and the second hollow pattern is a cross pattern arranged in the array interval of the first hollow pattern; the cutting speed of the ultraviolet picosecond laser is 1300-1700 mm / s, the frequency is 1900-2200 khz, and the cutting depth is to the thickness of the composite layer; The composite layer is placed on a metal jig when being cut. The metal jig is provided with a groove. The groove has evenly distributed bosses in the area without the laser path for receiving the composite layer. An air blowing device is provided above the metal jig to separate the cut waste from the composite layer and let it fall into the groove.

2. The method for preparing a support layer of a scroll display device according to claim 1, characterized in that: The wavelength of the ultraviolet picosecond laser is 355nm, the power of the laser generator is 30W, the output power is 5%, and the number of cutting times is 20 to 30 times.

3. The method for preparing a support layer of a scroll display device according to claim 1, characterized in that: The material of the film used for the support layer is PET, PU or CPI, and the thickness is 0.05-0.09 mm.

4. The method for preparing a support layer of a scroll display device according to claim 1, characterized in that: The flexible film used to form the support layer has a first protective layer and a second protective layer on both sides, the first protective layer has a thickness of 0.04-0.06 mm, and the second protective layer has a thickness of 0.06-0.08 mm. During cutting, the laser light is incident from the first protective layer.

5. The method for preparing a support layer of a scroll display device according to claim 4, characterized in that: A PSA layer with a thickness of 0.01-0.03 mm is provided between the first protective layer and the flexible film.

6. The method for preparing a support layer of a scroll display device according to claim 1, characterized in that: Adjacent rows in the array of the first hollow patterns are staggered, the center of the cross pattern is located between two adjacent first hollow patterns in the row, and extends to four spacing areas between the two adjacent first hollow patterns and the upper and lower rows of first hollow patterns to form a cross.

7. The method for preparing a support layer of a scroll display device according to claim 6, characterized in that: The cross-shaped patterns are arranged in alternate rows in the array of the first hollow patterns, and the bosses are correspondingly located between two adjacent first hollow patterns in the alternate rows.

8. The method for preparing a support layer of a scroll display device according to claim 1, characterized in that: The minimum width of the cross-shaped pattern is ≤0.2 mm.

9. The method for preparing a support layer of a scroll display device according to claim 1, characterized in that: The characteristic size of the first hollow pattern is 2-3 mm.

10. The method for preparing a support layer of a scroll display device according to claim 1, characterized in that: The air outlet direction of the air blowing device is perpendicular to the surface of the composite layer, and the air pressure is 0.2-0.3 MPa.

Citation Information

Patent Citations

  • Supporting film, flexible mother board, flexible display panel and manufacturing method of flexible display panel

    CN115691327A

  • Supporting piece and display panel

    CN116110289A

  • A tool for sheet punches

    CN208051183U

  • Laser cutting jig

    CN210080966U

  • Waste discharge device for double-faced adhesive tape product

    CN212126976U