Method for correcting warping of board-level packaging
By cutting narrow slots on the bottom surface of the board-level packaging space to release residual stress, the problems of reduced packaging efficiency and mold damage caused by warpage correction in the prior art are solved, and an efficient and reliable warpage correction process is achieved.
Patent Information
- Application Number
- CN202411050426.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-01
- Publication Date
- 2024-11-15
AI Technical Summary
Existing technologies, when correcting board-level package warpage, can easily alter the chip's injection mold, increasing the probability of demolding damage, leading to reduced packaging efficiency and placing a burden on subsequent cleaning processes.
After board-level packaging is completed, a narrow groove is cut on the bottom surface of the space between adjacent packaging units by a laser beam through the glass carrier to release residual stress and correct warpage. This avoids changing the injection mold and the narrow groove structure avoids demolding damage and subsequent process impact.
It effectively corrects warpage, avoids changes in injection molds and demolding damage, improves packaging efficiency and reliability, ensures that subsequent processes are not affected, and prevents dust contamination by keeping the narrow grooves from being exposed to the outside.
Smart Images

Figure CN118969677A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of advanced chip packaging, and in particular to a method for correcting warpage of a board-level package. Background Art
[0002] At present, advanced packaging is the key development area of current chip technology. There are many technologies for advanced packaging, which are divided into wafer level and board level according to the size of the package. The wafer level size is represented by a 12-inch wafer with a diameter of 300mm; the board level has a variety of sizes, the most common ones are 300x300mm, 510x515mm, 600x600mm, 700x700mm, etc. Whether it is wafer-level or board-level packaging, serious warping will occur after temporary bonding and debonding. For board-level advanced packaging, as the board size increases, the degree of warping also increases in a square relationship. Therefore, how to effectively suppress warping is an important issue related to advanced packaging production efficiency and product quality.
[0003] The reason for the warpage of board-level packaging is the existence of residual stress in the packaging structure, which is caused by the inconsistency of thermal expansion coefficients between materials used, differences in chip size and shape, uneven shrinkage of plastic curing, and loads such as temperature and pressure during the packaging process. The principle of warpage correction is to eliminate or minimize residual stress.
[0004] However, the existing method for correcting warpage uses two types of grooves of different widths and depths to open on the upper surface of the packaging plastic to reduce residual stress and thus reduce the overall packaging warpage. This method changes the injection mold of the chip, and the demolding process also increases the probability of damage to the packaging unit, resulting in reduced packaging efficiency; at the same time, it brings a burden to the subsequent cleaning process. Summary of the invention
[0005] In view of the shortcomings of the prior art, the purpose of the present invention is to provide a method for correcting the warping of a board-level package, which has the advantages of being able to avoid changing the injection molding mold of the chip, avoiding demolding damage, and improving the packaging efficiency; at the same time, it does not have any adverse effects on subsequent processes such as cleaning.
[0006] The above-mentioned invention object of the present invention is achieved through the following technical solution: A method for correcting warpage of a board-level package, comprising the following steps:
[0007] S101, after completing the patch and injection molding process of the board-level package, measure the warpage of the board;
[0008] S102, using a laser beam to penetrate the glass carrier plate and cut a narrow groove on the bottom surface of the plastic sealing layer of the space between two adjacent packaging units until the warpage correction effect of the plate is no longer increased or the warpage correction goal is achieved;
[0009] S103. Perform unit division or debonding on the corrected board-level package and then perform unit division.
[0010] Preferably, for the method for correcting warpage of a board-level package provided by the present invention, in S101, after the chip mounting and injection molding processes of the board-level package are completed, measure the warpage degree of the board, including:
[0011] S1011. Arrange a plurality of the packaging units in a matrix on the glass carrier plate, leave the spacing space between every two adjacent packaging units, and provide a chip bonding area at the edge of each packaging unit. Paste a chip unit in each chip bonding area, wherein the chip unit includes a plurality of chips, and the plurality of chips are sequentially pasted on the chip bonding area;
[0012] S1012. Connect the chip unit to the redistribution layer on the glass carrier plate so that the chips in the chip unit are connected;
[0013] S1013. After injection molding to complete the encapsulation of the encapsulation layer, measure the warpage degree of the board.
[0014] Preferably, for the method for correcting warpage of a board-level package provided by the present invention, the narrow groove is a cross-shaped narrow groove, a middle-shaped narrow groove or a well-shaped narrow groove.
[0015] Preferably, for the method for correcting warpage of a board-level package provided by the present invention, in S102, use a laser beam to cut a narrow groove through the glass carrier plate to the bottom surface of the encapsulation layer in the spacing space between two adjacent packaging units until the warpage correction effect of the board no longer increases or reaches the warpage correction target, including:
[0016] S1021. Select one or several of the spacing spaces on the side of the encapsulation layer facing the glass carrier plate according to the measured warpage direction of the board and perform cutting in two directions, vertical and horizontal, to form a cross-shaped narrow groove;
[0017] S1022. Measure the warpage degree and add cutting grooves according to the change of the warpage degree to form one or more middle-shaped narrow grooves or well-shaped narrow grooves;
[0018] S1023. Repeat step S1022 until the warpage correction effect of the board no longer increases or reaches the warpage correction target.
[0019] Preferably, for the method for correcting warpage of a board-level package provided by the present invention, the thickness range of the plastic layer is 150 - 200 microns.
[0020] Preferably, for the method for correcting warpage of a board-level package provided by the present invention, the width range of the narrow groove is 10 - 20 microns.
[0021] Preferably, in the method for correcting warpage of board-level packaging provided by the present invention, the depth of the narrow groove is in the range of 25-50 microns.
[0022] Preferably, in the method for correcting warpage of a board-level package provided by the present invention, the depth of the narrow groove is greater than 1.2 times the width of the narrow groove.
[0023] Preferably, in the method for correcting warpage of board-level packaging provided by the present invention, the depth of the narrow groove is less than or equal to one half of the thickness of the plastic layer.
[0024] Preferably, in the method for correcting warpage of a board-level package provided by the present invention, the step S103 of dividing the corrected board-level package into units or debonding and then dividing the units comprises:
[0025] S1031, if the package carries a glass carrier, the corrected board-level package is divided into units;
[0026] S1032: If the package does not include a glass carrier, the plastic layer is debonded from the glass carrier and then the units are separated.
[0027] In summary, the beneficial technical effects of the present invention are as follows: the method for correcting the warpage of a board-level package provided in the present application comprises the following steps: after completing the patch and injection molding processes of the board-level package, measuring the warpage of the board; using a laser beam to penetrate a glass carrier and cut a narrow groove on the bottom surface of the plastic sealing layer of the spacing space left between two adjacent packaging units until the warpage correction effect of the board is no longer increased or the warpage correction goal is achieved; performing unit segmentation or debonding on the corrected board-level package and then performing unit segmentation; by cutting a narrow groove on the bottom surface of the plastic sealing layer of the spacing space to release the residual stress in the board-level package structure, compared with other methods for correcting warpage, it avoids changing the injection molding mold of the chip, avoids mold removal damage, does not damage the chip and its outer plastic, does not affect subsequent debonding, cleaning, slicing and other processes, and improves the reliability of picking up and conveying the board and the packaging efficiency; in addition, the narrow groove is sealed between the glass carrier and the top of the plastic layer and is not exposed to the outside space, thereby preventing the narrow groove from being contaminated by dust and having no effect on the subsequent cleaning process. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 It is a flow chart of a method for correcting warpage of a board-level package provided in an embodiment of the present invention.
[0029] Figure 2 It is a partial plan view of a board-level package (excluding the plastic layer) in the method for correcting warpage of a board-level package provided in an embodiment of the present invention.
[0030] Figure 3It is a cross-sectional view (including a plastic layer) of a board-level package in a method for correcting warpage of a board-level package provided in an embodiment of the present invention.
[0031] Figure 4a It is a cross-sectional view of a packaging unit with a glass carrier obtained after cutting in the method for correcting warpage of a board-level packaging provided by an embodiment of the present invention.
[0032] Figure 4b It is a cross-sectional view of a packaging unit without a glass carrier obtained after cutting in the method for correcting warpage of a board-level packaging provided by an embodiment of the present invention.
[0033] Figure 5 It is a structural schematic diagram of a cross-shaped narrow groove in a method for correcting warpage of a board-level package provided in an embodiment of the present invention.
[0034] Figure 6 It is a structural schematic diagram of a Chinese-shaped narrow groove in a method for correcting warpage of a board-level package provided in an embodiment of the present invention.
[0035] Figure 7 It is a structural schematic diagram of a tic-tac-toe-shaped narrow groove in a method for correcting warpage of a board-level package provided in an embodiment of the present invention.
[0036] In the figure, 1, board-level packaging; 10, glass carrier; 20, packaging unit; 21, chip; 22, spacing space; 30, plastic sealing layer; 40, narrow groove. DETAILED DESCRIPTION
[0037] The present invention is further described in detail below in conjunction with the accompanying drawings.
[0038] Reference Figures 1 to 4b , a method for correcting warpage of a board-level package 1 disclosed in the present invention, comprising the following steps:
[0039] S101, after completing the patch and injection molding processes of the board-level package 1, measuring the warpage of the board.
[0040] Among them, S101, after completing the patch and injection molding process of the board-level package 1, measuring the warpage of the board, including:
[0041] S1011. Arrange a plurality of packaging units 20 arranged in a matrix on a glass carrier 10, with a spacing space 22 being left between each two adjacent packaging units 20, and a chip 21 bonding area being provided at the edge of each packaging unit 20, and a chip 21 unit being pasted on each chip 21 bonding area, wherein the chip 21 unit includes a plurality of chips 21, and the plurality of chips 21 are sequentially pasted on the chip 21 bonding area.
[0042] It should be noted that the spacing space 22 is a space reserved for cutting the glass carrier 10 after the plastic packaging is completed. The position and width of the spacing space 22 are determined by the injection mold. Generally speaking, the narrower the spacing space 22, the higher the density of the packaging unit 20 on the glass carrier 10, which is more conducive to improving the yield.
[0043] S1012 , connecting the chip 21 unit to the rewiring layer on the glass carrier 10 , so that the chips 21 in the chip 21 unit are connected.
[0044] It should be noted that the chips 21 in each packaging unit 20 are connected to each other, but the packaging units 20 are not connected to each other.
[0045] by Figure 2 As shown in the example, the chip 21 unit includes a plurality of chips 21 of different sizes and shapes. To reduce the influence of the size and shape of the chip 21, each packaging unit 20 is arranged in a rotational manner.
[0046] S1013, after the plastic packaging layer 30 is packaged by injection molding, the warpage of the board is measured.
[0047] It should be noted that measuring the warpage of a board is well known to those skilled in the art, and the process of measuring the warpage of a board will not be described in detail herein.
[0048] S102, using a laser beam to penetrate the glass carrier 10 and cut a narrow groove 40 on the bottom surface of the plastic sealing layer 30 in the spacing space 22 left between two adjacent packaging units 20 until the warping correction effect of the board is no longer increased or the warping correction goal is achieved; by cutting the narrow groove 40 in the plastic sealing layer 30 in the spacing space 22, the residual stress in the board-level packaging 1 structure is released to achieve the purpose of correcting the warping.
[0049] Continue to refer to Figures 5 to 7 In this embodiment, the narrow groove 40 can be a cross-shaped narrow groove 40, a center-shaped narrow groove 40 or a well-shaped narrow groove 40.
[0050] It should be noted that the chips 21 in the board-level package 1 are arranged horizontally and vertically in a rectangular shape, so oblique grooves or circular grooves cannot be used to avoid damaging the integrity of the chip 21 packaging unit 20. However, in addition to the cross-shaped narrow grooves 40, the Chinese-shaped narrow grooves 40 or the well-shaped narrow grooves 40, any horizontal and vertical narrow grooves 40 with different numbers can be used, and the specific selection can be based on the packaging process and the observed warping degree.
[0051] Among them, S102, using a laser beam to penetrate the glass carrier 10 to cut a narrow groove 40 on the bottom surface of the plastic sealing layer 30 of the spacing space 22 left between two adjacent packaging units 20 until the warpage correction effect of the board is no longer increased or the warpage correction goal is achieved, includes:
[0052] S1021 , according to the measured warping direction of the board, one or more plastic sealing layers 30 of the spacing spaces 22 are selected and cut in both vertical and horizontal directions toward one side of the glass carrier board 10 to form a cross-shaped narrow groove 40 .
[0053] Specifically, for the initial grooving, a direction and position with a large warp is selected, and a laser beam emitted by a laser is used to penetrate the glass carrier 10 to first cut a cross-shaped narrow groove 40 on the side of the plastic sealing layer 30 facing the glass carrier 10 in the spacing space 22 where the warp is located.
[0054] S1022, measuring the warpage and adding grooves according to the change of the warpage to form one or more narrow grooves 40 in the shape of a Chinese character "Z" or a Chinese character "Ji".
[0055] S1023, looping step S1022 until the warpage correction effect of the board no longer increases or the warpage correction target is reached.
[0056] Specifically, cut the grooves again, observe the degree of warping correction, and gradually increase the number of cutting vertical narrow grooves 40 or horizontal narrow grooves 40 to make the structure of the cross-shaped narrow grooves 40 evolve into the middle-shaped narrow grooves 40 and then into the well-shaped narrow grooves 40. Stop cutting the grooves when the warping correction is stable. That is to say, stop cutting the grooves when it is observed that the warping correction effect is no longer obvious.
[0057] Furthermore, in this embodiment, the thickness of the plastic layer is in the range of 150-200 microns.
[0058] The width of the narrow groove 40 cut on the plastic layer by the laser beam is in the range of 10-20 microns; the depth of the narrow groove 40 is in the range of 25-50 microns.
[0059] Further, in this embodiment, the depth of the narrow groove 40 is greater than 1.2 times the width of the narrow groove 40 .
[0060] Specifically, according to the principle of the blind hole method, as long as the depth of the narrow groove 40 is greater than 1.2 times the width of the narrow groove 40 , the residual stress can be effectively released to achieve the purpose of correcting the warpage.
[0061] It should be noted that a small spot laser beam is used so that the width of the narrow groove 40 is controlled within the range of several microns to twenty microns, and the depth of the narrow groove 40 is greater than 1.2 times the width of the narrow groove 40. The depth of the narrow groove 40 can be considered based on factors such as the size of the glass carrier 10, the size of the chip 21 in the packaging unit 20, and the layout of its redistribution layer (RDL).
[0062] The depth of the narrow groove 40 is less than or equal to half of the thickness of the plastic layer.
[0063] Specifically, the maximum depth of the narrow groove 40 does not exceed half of the thickness of the plastic layer, thereby ensuring the integrity of the board-level dimensions of the entire plastic layer and facilitating the picking up and transporting of the plastic layer after debonding; in addition, the narrow groove 40 is cut on the bonding surface between the glass carrier 10 and the plastic layer, and the narrow groove 40 is sealed between the glass carrier 10 and the top of the plastic layer and is not exposed to the external space, thereby preventing the narrow groove 40 from being contaminated by dust and causing cleaning pressure, and has no negative impact on the subsequent debonding, picking up, and transporting of the packaging process.
[0064] S103, performing unit division or debonding and then unit division on the corrected board-level package 1.
[0065] The respective packaging units 20 in the corrected board-level package 1 are cut off. After slicing, each packaging unit 20 is a circuit block with the same function and is used separately.
[0066] By setting the cut narrow groove 40 in the spacing space 22, the cut narrow groove 40 releases the residual stress, which only affects the packaging process, that is, by releasing the residual stress to reduce the warpage, the packaging process can proceed smoothly. After the last step of the slicing process of the packaging process is completed, each independent packaging unit 20 has no cut grooves or other damages to ensure the integrity and reliability of the packaging.
[0067] Wherein, S103, performing unit segmentation or debonding and then unit segmentation on the corrected board-level package 1, comprises:
[0068] S1031 , if the package carries a glass carrier 10 , the corrected board-level package 1 is divided into units.
[0069] S1032, if the package does not carry the glass carrier 10, the plastic layer is debonded from the glass carrier 10 and then the unit is separated.
[0070] Specifically, for the package without the glass carrier 10, after the step S102 is completed, the plastic layer is debonded from the glass carrier 10, and then annealed, cleaned, and then transferred to the slicing process, and the debonded plastic layer is cut and divided into independent packaging units 20 for use.
[0071] Specifically, the debonding may be performed by laser debonding.
[0072] In order not to affect the solidification state of the plastic, annealing is performed at a temperature below 100°C for a period of time. The annealing temperature and time can be adjusted according to the packaging materials and processes. By combining the thermal relaxation process with the stress release effect of the narrow groove 40, the residual stress is further reduced to reduce the degree of package warpage.
[0073] It should be noted that the debonding, annealing, cleaning and slicing processes are well known to those skilled in the art, and will not be described in detail herein.
[0074] The method for correcting the warpage of a board-level package 1 provided in the present application comprises the following steps: measuring the warpage of the board after completing the patch and injection molding processes of the board-level package 1; using a laser beam to penetrate a glass carrier 10 and cut a narrow groove 40 on the bottom surface of a plastic sealing layer 30 of a spacing space 22 left between two adjacent packaging units 20 until the warpage correction effect of the board is no longer increased or the warpage correction target is achieved; performing unit division or debonding of the corrected board-level package 1 and then performing unit division; cutting a narrow groove 40 on the bottom surface of a plastic sealing layer 30 of a spacing space 22 and then performing unit division; Cutting a narrow groove 40 to release the residual stress in the structure of the board-level package 1, compared with other methods of correcting warpage, avoids changing the injection mold of the chip 21, avoids demolding damage, does not damage the chip and its outer plastic, does not affect the subsequent debonding, cleaning, slicing and other processes, and improves the reliability of board picking and transmission and the packaging efficiency; in addition, the narrow groove 40 is sealed between the glass carrier 10 and the top of the plastic layer and is not exposed to the outside space, thereby preventing the narrow groove 40 from being contaminated by dust and having no effect on the subsequent cleaning process.
[0075] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the statement "comprise a ..." do not exclude the presence of other identical elements in the process, method, article or device including the elements.
[0076] Finally, it should be noted that: Obviously, the above embodiments are only examples for clearly explaining the present invention, and are not intended to limit the implementation methods. For ordinary technicians in the relevant field, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived from this are still within the scope of protection of the present invention.
Claims
1. A method for correcting warpage of a board-level package, characterized in that: It includes the following steps: S101. After completing the chip mounting and injection molding processes of the board-level package, measure the warpage of the board. S102. Use a laser beam to cut narrow grooves through the bottom surface of the encapsulation layer in the gap space left between two adjacent packaging units through the glass carrier plate until the warpage correction effect of the board no longer increases or reaches the warpage correction target. S103. Perform unit division on the corrected board-level package or debond and then perform unit division.
2. The method for correcting warpage of board-level packaging according to claim 1, characterized in that: The S101. After completing the chip mounting and injection molding processes of the board-level package, measure the warpage of the board, including: S1011. Set a plurality of the packaging units arranged in a matrix on the glass carrier plate. There is the gap space left between every two adjacent packaging units. A chip bonding area is provided at the edge of each packaging unit. Chip units are pasted in each chip bonding area. Among them, the chip unit includes a plurality of chips, and the plurality of chips are sequentially pasted on the chip bonding area. S1012. Connect the chip unit to the redistribution layer on the glass carrier plate so that each chip in the chip unit is connected. S1013. After injection molding to complete the encapsulation layer packaging, measure the warpage of the board.
3. The method for correcting warpage of board-level packaging according to claim 1, characterized in that: The narrow groove is a cross-shaped narrow groove, a middle-shaped narrow groove or a grid-shaped narrow groove.
4. The method for correcting warpage of board-level packaging according to claim 3, characterized in that: The S102. Use a laser beam to cut narrow grooves through the bottom surface of the encapsulation layer in the gap space left between two adjacent packaging units through the glass carrier plate until the warpage correction effect of the board no longer increases or reaches the warpage correction target, including: S1021. Select one or several of the gap spaces, and cut in two directions, vertical and horizontal, on the side of the encapsulation layer facing the glass carrier plate to form a cross-shaped narrow groove according to the measured warpage direction of the board. S1022. Measure the warpage and add cutting grooves according to the change of the warpage to form one or more middle-shaped narrow grooves or grid-shaped narrow grooves. S1023. Repeat step S1022 until the warpage correction effect of the board no longer increases or reaches the warpage correction target.
5. The method for correcting warpage of board-level packaging according to claim 1, characterized in that: The thickness range of the plastic layer is 150 - 200 microns.
6. The method for correcting warpage of board-level packaging according to claim 5, characterized in that: The width range of the narrow groove is 10 - 20 microns.
7. The method for correcting warpage of board-level packaging according to claim 6, characterized in that: The depth range of the narrow groove is 25 - 50 microns.
8. The method for correcting warpage of board-level packaging according to claim 7, characterized in that: The depth of the narrow groove is greater than 1.2 times the width of the narrow groove.
9. The method for correcting warpage of board-level packaging according to claim 8, characterized in that: The depth of the narrow groove is less than or equal to half of the thickness of the plastic layer.
10. The method for correcting warpage of board-level packaging according to claim 1, characterized in that: The S103. Perform unit division on the corrected board-level package or debond and then perform unit division, including: S1031. If it is a package carrying a glass carrier plate, perform unit division on the corrected board-level package. S1032. If it is a package not carrying a glass carrier plate, debond the plastic layer from the glass carrier plate and then perform unit division.
Citation Information
Cited By
Method for improving warping of packaging substrate through laser drilling
CN121156541A