Semiconductor structure and preparation method thereof
By forming an oxide side wall and a passivation side wall on the gate side wall of the semiconductor structure, the bidirectional adjustment problem during electrical properties in the semiconductor structure is solved, reliability and electrical properties are improved, and dislocation damage is avoided.
Patent Information
- Application Number
- CN202411435854.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-15
- Publication Date
- 2024-11-15
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In semiconductor structures, when adjusting electrical properties through ion implantation, it is impossible to make bidirectional adjustments to NMOS and PMOS at the same time, and parameters such as the concentration of ion implantation need to be adjusted multiple times, resulting in dislocations and other damages within the semiconductor structure, affecting reliability and Electricity.
By forming an oxide side wall and a passivation side wall on the side wall of the gate structure, the oxide side wall absorbs boron elements and blocks the diffusion of hydrogen elements, adjusting the speed of PMOS and NMOS, avoiding the need to adjust the ion implantation parameters multiple times .
Bidirectional adjustment during electrical adjustment of semiconductor structure is achieved, reliability and electrical performance are improved, and dislocation damage is avoided.
Smart Images

Figure CN118969736A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductor technology, and in particular to a semiconductor structure and a method for preparing the same. Background Art
[0002] In the semiconductor industry, complementary metal-oxide-semiconductor (CMOS) consists of N-metal-oxide-semiconductor (NMOS) and P-metal-oxide-semiconductor (PMOS), which are used to design logic functions and have the advantages of high speed, low power consumption and high noise tolerance. CMOS needs to work under a certain range of source voltage and input voltage. The electrical fluctuations of NMOS and PMOS will have a huge impact on the working performance of CMOS. The N / P ratio (i.e., the electrical ratio of NMOS to PMOS) is usually used to measure the impact of CMOS on the electrical fluctuations of NMOS and PMOS. That is, the N / P ratio needs to be stable within a certain range so as not to affect the normal operation of the device. The adjustment of the electrical properties of semiconductor structures is mostly achieved by adjusting ion implantation, that is, by changing the energy / dose of ions during doping implantation to control the substrate doping dose, thereby achieving the effect of adjusting the electrical properties of the semiconductor.
[0003] However, when the electrical properties of the semiconductor structure are adjusted by ion implantation, it is impossible to perform bidirectional adjustments on NMOS and PMOS at the same time. In addition, during the ion implantation process, parameters such as the ion implantation concentration need to be adjusted multiple times, which may cause damage such as dislocations inside the semiconductor structure, affecting the reliability and electrical properties of the semiconductor structure. Summary of the invention
[0004] The purpose of the present application is to provide a semiconductor structure and a method for preparing the same, which solves the problem that when adjusting the electrical properties of the semiconductor structure, it is impossible to adjust both NMOS and PMOS at the same time, and during the ion implantation process, it is necessary to adjust the ion implantation concentration and other parameters multiple times, thereby causing damage such as dislocations inside the semiconductor structure, thereby improving the reliability and electrical properties of the semiconductor structure. To achieve the purpose of the present application, the present application provides the following technical solutions:
[0005] In a first aspect, the present application provides a method for preparing a semiconductor structure, comprising:
[0006] A semiconductor initial structure is provided, wherein the semiconductor initial structure comprises a substrate, and a deep well region, a well region of a first conductivity type, and an active region of a second conductivity type which are sequentially formed and stacked in the substrate; the substrate is doped with boron;
[0007] A gate structure is formed on a surface of the active region away from the deep well region; wherein a projection of the gate structure toward the well region falls into the well region;
[0008] An oxide sidewall and a passivation sidewall are sequentially formed on the sidewalls of the gate structure; wherein the projections of the oxide sidewall and the passivation sidewall toward the active area fall into the active area, the oxide sidewall is used to absorb the boron element, and the passivation sidewall is used to block the diffusion of hydrogen elements in the oxide sidewall.
[0009] The method for preparing the semiconductor structure of the present application includes first providing a semiconductor initial structure, wherein the semiconductor initial structure includes a substrate, and a deep well region, a well region of a first conductivity type, and an active region of a second conductivity type sequentially stacked on the substrate; the substrate is doped with boron; a gate structure is formed on the surface of the active region away from the deep well region; and an oxide sidewall and a passivation sidewall are sequentially formed on the sidewall of the gate structure. The boron element in the substrate and the boron element in the well region of the first conductivity type can be attracted to the oxide sidewall to reduce the boron element in the well region of the first conductivity type, thereby slowing down the PMOS and speeding up the NMOS. The passivation sidewall will block the diffusion of hydrogen elements in the oxide sidewall, thereby enhancing the attraction of the oxide sidewall to the boron element. The thicker the passivation side wall is, the stronger the ability to block the diffusion of hydrogen in the oxide side wall is, the stronger the ability of the oxide side wall to attract boron is, and the lower the concentration of boron in PMOS is. Therefore, the speed of PMOS and NMOS can be adjusted by adjusting the thickness of the passivation side wall, which solves the problem that when the electrical properties of the semiconductor structure are adjusted, it is impossible to adjust NMOS and PMOS in both directions at the same time. There is no need to adjust parameters such as the concentration of ion implantation multiple times, thereby avoiding the problem of damage such as dislocations inside the semiconductor structure, and improving the reliability and electrical properties of the semiconductor structure.
[0010] In one embodiment, the step of forming the well region of the first conductivity type comprises:
[0011] forming an initial well region on a surface of the deep well region away from the substrate;
[0012] Boron ions are implanted into the initial well region to form a well region of the first conductivity type.
[0013] In one embodiment, after sequentially forming an oxide sidewall spacer and a passivation sidewall spacer on the sidewall of the gate structure, the method further comprises:
[0014] The resulting structure is placed in a thermal oxidation atmosphere to activate the well region of the first conductivity type.
[0015] In one embodiment, in the thermal oxidation atmosphere, oxygen ions in the oxide sidewalls form covalent bonds with boron ions in the well region of the first conductivity type and boron ions in the substrate.
[0016] In one embodiment, the passivation spacer includes a silicon nitride spacer, and the thickness of the passivation spacer is positively correlated with the barrier capability of blocking the diffusion of hydrogen elements in the oxide spacer.
[0017] In a second aspect, the present application further provides a semiconductor structure, comprising:
[0018] A semiconductor initial structure, wherein the semiconductor initial structure comprises a substrate, and a deep well region, a well region of a first conductivity type, and an active region of a second conductivity type sequentially stacked on the substrate; the substrate is doped with boron;
[0019] A gate structure is located on a surface of the active region away from the deep well region; wherein a projection of the gate structure toward the well region falls into the well region;
[0020] The oxide sidewalls and the passivation sidewalls are sequentially located on the sidewalls of the gate structure; wherein the projections of the oxide sidewalls and the passivation sidewalls toward the active area fall into the active area, the oxide sidewalls are used to absorb the boron element, and the passivation sidewalls are used to block the diffusion of hydrogen elements in the oxide sidewalls.
[0021] The semiconductor structure of the present application includes a semiconductor initial structure, a gate structure, an oxide sidewall and a passivation sidewall, wherein the semiconductor initial structure includes a substrate, and a deep well region, a well region of a first conductivity type and an active region of a second conductivity type sequentially stacked on the substrate, and the substrate is doped with boron. The boron element in the substrate and the boron element in the well region of the first conductivity type can both be attracted to the oxide sidewall to reduce the boron element in the well region of the first conductivity type, thereby slowing down PMOS and speeding up NMOS. The passivation sidewall will block the diffusion of hydrogen elements in the oxide sidewall, thereby enhancing the attraction of the oxide sidewall to the boron element. The thicker the passivation side wall is, the stronger the ability to block the diffusion of hydrogen in the oxide side wall is, the stronger the ability of the oxide side wall to attract boron is, and the lower the concentration of boron in PMOS is. Therefore, the speed of PMOS and NMOS can be adjusted by adjusting the thickness of the passivation side wall, which solves the problem that when the electrical properties of the semiconductor structure are adjusted, it is impossible to adjust NMOS and PMOS in both directions at the same time. There is no need to adjust parameters such as the concentration of ion implantation multiple times, thereby avoiding the problem of damage such as dislocations inside the semiconductor structure, and improving the reliability and electrical properties of the semiconductor structure.
[0022] In one embodiment, the well region of the first conductivity type is doped with boron.
[0023] In one embodiment, oxygen ions in the oxide spacer form covalent bonds with boron ions in the well region of the first conductivity type and boron ions in the substrate.
[0024] In one embodiment, the passivation spacer includes a silicon nitride spacer, and the thickness of the passivation spacer is positively correlated with the barrier capability of the oxide spacer against diffusion of hydrogen.
[0025] In one embodiment, the semiconductor structure further includes: a plurality of shallow trench isolation structures, each of the shallow trench isolation structures penetrates the semiconductor initial structure, and an upper surface of the shallow trench isolation structure is higher than an upper surface of the semiconductor initial structure.
[0026] In summary, the present application provides a semiconductor structure and a method for preparing the same. By sequentially forming an oxide sidewall and a passivation sidewall on the sidewall of the gate structure, the unexpected effect is that the boron element in the substrate and the boron element in the well region of the first conductivity type can be attracted to the oxide sidewall to reduce the boron element in the well region of the first conductivity type, thereby slowing down the PMOS and speeding up the NMOS. The passivation sidewall blocks the diffusion of hydrogen elements in the oxide sidewall, thereby enhancing the attraction of the oxide sidewall to the boron element. The thicker the passivation sidewall, the stronger the blocking ability to the diffusion of hydrogen elements in the oxide sidewall, the stronger the attraction of the oxide sidewall to the boron element, and the lower the concentration of the boron element in the PMOS. Therefore, the speed of the PMOS and NMOS can be adjusted by adjusting the thickness of the passivation sidewall, which solves the problem that when the semiconductor structure is electrically adjusted, the NMOS and PMOS cannot be adjusted bidirectionally at the same time, and there is no need to adjust the parameters such as the concentration of ion implantation multiple times, thereby avoiding the problem of damage such as dislocation inside the semiconductor structure, and improving the reliability and electrical properties of the semiconductor structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] In order to more clearly illustrate the technical solutions in the embodiments of the present disclosure or the conventional technology, the drawings required for use in the embodiments or the conventional technology descriptions will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present disclosure, and for ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0028] FIG1 is a schematic diagram of a cross-sectional structure of an ion implantation process for adjusting the electrical properties of a semiconductor in the prior art;
[0029] FIG2 is a schematic diagram of a cross-sectional structure of dislocation damage inside a semiconductor structure caused by an ion implantation process in the prior art;
[0030] FIG3 is a flow chart of a method for preparing a semiconductor structure provided in one embodiment;
[0031] 4 is a schematic cross-sectional view of a structure obtained from steps S11 to S13 in a method for preparing a semiconductor structure provided in an embodiment;
[0032] FIG5 is a flow chart of steps S111 to S112 in a method for preparing a semiconductor structure provided in an embodiment;
[0033] FIG6 is a schematic cross-sectional view of the principle of adjusting the electrical properties of a semiconductor in a method for preparing a semiconductor structure provided in an embodiment;
[0034] FIG7 is a schematic diagram of a covalent bond formed in a method for preparing a semiconductor structure provided in an embodiment;
[0035] FIG8 is a linear relationship diagram of the N / P ratio of the passivation sidewall thickness and the threshold voltage in a method for preparing a semiconductor structure provided in an embodiment;
[0036] FIG9 is a linear relationship diagram of the thickness of a passivation sidewall and the N / P ratio of a saturation current in a method for preparing a semiconductor structure provided in an embodiment;
[0037] FIG. 10 is a flow chart of steps S121 to S122 in a method for preparing a semiconductor structure provided in one embodiment.
[0038] Description of Reference Numerals
[0039] 10. Semiconductor initial structure; 101. Substrate; 102. Deep well region; 103. Well region; 104. Active region; 20. Gate structure; 201. Gate oxide layer; 202. Gate conductive layer; 30. Oxide sidewall; 40. Passivation sidewall; 50. Shallow trench isolation structure. DETAILED DESCRIPTION
[0040] In order to facilitate understanding of the present application, the present application will be described more fully below with reference to the relevant drawings. The preferred embodiments of the present application are given in the drawings. However, the present application can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present application more thorough and comprehensive.
[0041] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used herein in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application.
[0042] It should be understood that when an element or layer is referred to as being "on, adjacent to, connected to or coupled to other elements or layers, it may be directly on, adjacent to, connected to or coupled to other elements or layers, or there may be intervening elements or layers. On the contrary, when an element is referred to as being "directly on, directly adjacent to, directly connected to or directly coupled to other elements or layers, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc. may be used to describe various elements, components, regions, layers, doping types and / or parts, these elements, components, regions, layers, doping types and / or parts should not be limited by these terms. These terms are merely used to distinguish one element, component, region, layer, doping type or part from another element, component, region, layer, doping type or part. Therefore, without departing from the teachings of the present invention, the first element, component, region, layer, doping type or portion discussed below may be represented as a second element, component, region, layer or portion; for example, the first doping type may be referred to as the second doping type, and similarly, the second doping type may be referred to as the first doping type; the first doping type and the second doping type are different doping types, for example, the first doping type may be P-type and the second doping type may be N-type, or the first doping type may be N-type and the second doping type may be P-type.
[0043] Spatially relative terms such as "under," "beneath," "below," "under," "above," "above," and the like may be used herein to describe the relationship of an element or feature shown in the figures to other elements or features. It should be understood that, in addition to the orientations shown in the figures, spatially relative terms also include different orientations of the device in use and operation. For example, if the device in the accompanying drawings is flipped, an element or feature described as "under other elements" or "under it" or "under it" will be oriented as being "above" the other elements or features. Thus, the exemplary terms "under" and "under" may include both upper and lower orientations. In addition, the device may also include additional orientations (e.g., rotated 90 degrees or other orientations), and the spatial descriptors used herein are interpreted accordingly.
[0044] When used herein, the singular forms "a", "an", and "said / the" may also include plural forms, unless the context clearly indicates otherwise. It should also be understood that when the terms "consisting of" and / or "comprising" are used in this specification, the presence of the features, integers, steps, operations, elements and / or parts can be determined, but the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or groups is not excluded. At the same time, when used herein, the term "and / or" includes any and all combinations of the relevant listed items.
[0045] In the semiconductor industry, complementary metal oxide semiconductors are composed of NMOS and PMOS, which are used to design logic functions and have the advantages of high speed, low power consumption and high noise tolerance. CMOS needs to work under a certain range of source voltage and input voltage. The electrical fluctuations of NMOS and PMOS will have a huge impact on the working performance of CMOS. The N / P ratio is usually used to measure the impact of CMOS on the electrical fluctuations of NMOS and PMOS, that is, the N / P ratio needs to be stable within a certain range so as not to affect the normal operation of the device. The adjustment of the electrical properties of the semiconductor structure is mostly achieved by ion implantation as shown in Figure 1, that is, by changing the energy / dose of the ions during doping implantation to control the substrate doping dose, thereby achieving the effect of adjusting the electrical properties of the semiconductor.
[0046] However, when the electrical properties of the semiconductor structure are adjusted by ion implantation, it is impossible to perform bidirectional adjustments on NMOS and PMOS at the same time, and during the ion implantation process, parameters such as the ion implantation concentration need to be adjusted multiple times, which may cause dislocation damage inside the semiconductor structure as shown in FIG. 2 , affecting the reliability and electrical properties of the semiconductor structure.
[0047] The present application provides a method for preparing a semiconductor structure. Please refer to FIG. 3 and FIG. 4 . The method for preparing a semiconductor structure may include:
[0048] S11: Providing a semiconductor initial structure, wherein the semiconductor initial structure includes a substrate, and a deep well region, a well region of a first conductivity type, and an active region of a second conductivity type which are sequentially stacked in the substrate; the substrate is doped with boron.
[0049] As an example, the substrate 101 may include but is not limited to at least one of a silicon substrate, a gallium nitride (GaN) substrate, a silicon carbide (SiC) substrate, a sapphire substrate, a silicon on insulator (SOI) substrate, a silicon on diamond (SOD) substrate, and a strained layer silicon substrate deposited on a germanium silicon wafer. Specifically, in the present embodiment, the substrate 101 is a silicon substrate, and the silicon substrate is doped with boron.
[0050] For example, an ion implantation process may be used but is not limited to implanting ions into the substrate 101 to form the deep well region 102 .
[0051] Exemplarily, an ion implantation process may be used but is not limited to form a well region 103 of the first conductivity type on a surface of the deep well region 102 away from the substrate 101. The first conductivity type may include a P-type conductivity type or an N-type conductivity type. Specifically, in this embodiment, the well region 103 of the first conductivity type is a P-type well region.
[0052] Exemplarily, an ion implantation process may be used but is not limited to form an active region 104 of the second conductivity type in the well region 103 of the first conductivity type. Specifically, in this embodiment, the active region 104 of the second conductivity type is an N-type active region.
[0053] S12: forming a gate structure on a surface of the active region away from the deep well region; wherein a projection of the gate structure toward the well region falls into the well region.
[0054] As an example, the gate structure 20 is formed on a surface of the active region 104 away from the deep well region 102 ; wherein a projection of the gate structure 20 toward the well region 103 falls into the well region 103 .
[0055] S13: forming oxide sidewalls and passivation sidewalls on the sidewalls of the gate structure in sequence; wherein the projections of the oxide sidewalls and the passivation sidewalls toward the active area fall into the active area, the oxide sidewalls are used to absorb boron elements, and the passivation sidewalls are used to block the diffusion of hydrogen elements in the oxide sidewalls.
[0056] As an example, the oxide spacer 30 may be formed on the sidewall of the gate structure 20 by a thermal oxidation process but not limited thereto; the passivation spacer 40 may be formed by a physical vapor deposition process (PVD), a chemical vapor deposition process (CVD) or an atomic layer deposition process (ALD) but not limited thereto; wherein the projections of the oxide spacer 30 and the passivation spacer 40 toward the active area 104 fall into the active area 104. Specifically, in the present embodiment, the oxide spacer 30 contains hydrogen ions, and the passivation spacer 40 is a silicon nitride spacer.
[0057] The method for preparing the semiconductor structure of the present application first provides a semiconductor initial structure 10, wherein the semiconductor initial structure 10 includes a substrate 101, and a deep well region 102, a well region 103 of a first conductivity type, and an active region 104 of a second conductivity type sequentially stacked on the substrate 101; the substrate 101 is doped with boron; secondly, a gate structure 20 is formed on the surface of the active region 104 away from the deep well region 102; finally, an oxide spacer 30 and a passivation spacer 40 are sequentially formed on the sidewalls of the gate structure 20. The boron element in the substrate 101 and the boron element in the well region 103 of the first conductivity type can be attracted to the oxide spacer 30 to reduce the boron element in the well region 103 of the first conductivity type, thereby slowing down the PMOS and speeding up the NMOS. The passivation spacer 40 blocks the diffusion of hydrogen elements in the oxide spacer 30, thereby enhancing the attraction of the oxide spacer 30 to the boron element. The thicker the passivation sidewall 40 is, the stronger the ability to block the diffusion of hydrogen in the oxide sidewall 30 is, and thus the oxide sidewall 30 has a stronger ability to attract boron, and the concentration of boron in the PMOS is lower. Therefore, the speed of PMOS and NMOS can be adjusted by adjusting the thickness of the passivation sidewall 40, which solves the problem that when the electrical properties of the semiconductor structure are adjusted, it is impossible to adjust NMOS and PMOS in both directions at the same time, and there is no need to adjust the parameters such as the concentration of ion implantation multiple times, thereby avoiding the problem of damage such as dislocations inside the semiconductor structure, thereby improving the reliability and electrical properties of the semiconductor structure.
[0058] In some embodiments, referring to FIG. 4 and FIG. 5 , the step of forming the well region 103 of the first conductivity type may include:
[0059] S111: forming an initial well region on a surface of the deep well region away from the substrate.
[0060] As an example, an initial well region (not shown) may be formed on a surface of the deep well region 102 away from the substrate 101 by using, but not limited to, an ion implantation process.
[0061] S112: implanting boron ions into the initial well region to form a well region of the first conductivity type.
[0062] As an example, boron ions may be implanted into the initial well region using, but not limited to, an ion implantation process to form the well region 103 of the first conductivity type.
[0063] In the embodiment of the present application, a P-type well region 103 is formed by injecting boron ions into the initial well region. The concentration of boron ions in the P-type well region 103 is proportional to the speed of PMOS and NMOS. Specifically, when the concentration of boron ions in the P-type well region 103 is higher, the PMOS is faster and the NMOS is slower; when the concentration of boron ions in the P-type well region 103 is lower, the PMOS is slower and the NMOS is faster.
[0064] In some embodiments, please continue to refer to FIG. 4 , after sequentially forming oxide spacers and passivation spacers on the sidewalls of the gate structure, a step of placing the resulting structure in a thermal oxidation atmosphere to activate the well region of the first conductivity type may also be included.
[0065] As an example, the obtained structure is placed in a thermal oxidation atmosphere to activate the ions implanted in the initial well region to activate the well region 103 of the first conductivity type. Specifically, the obtained structure may be annealed to perform thermal oxidation.
[0066] In the embodiment of the present application, the obtained structure is placed in a thermal oxidation atmosphere to activate the ions injected into the initial well region, thereby activating the well region 103 of the first conductivity type. When ions are injected into the initial well region, the high-energy injected ions collide with atoms on the semiconductor lattice, causing some lattice atoms to shift, thereby causing a large number of vacancies in the atoms. The vacancies cause the atoms in the injected region to be arranged in a disordered manner or become an amorphous region. Therefore, placing the semiconductor structure in a thermal oxidation atmosphere after ion implantation can also restore the structure of the crystal and eliminate defects.
[0067] In some embodiments, referring to FIG. 6 to FIG. 9 , in a thermal oxidation atmosphere, oxygen ions in the oxide spacer 30 form covalent bonds with boron ions in the well region 103 of the first conductivity type and boron ions in the substrate 101 .
[0068] As an example, as shown in FIG. 6 , in a thermal oxidation atmosphere, boron ions in the well region 103 and boron ions in the substrate 101 will be transferred to the oxide sidewalls 30 , and hydrogen ions in the oxide sidewalls 30 will also diffuse. The passivation sidewalls 40 can block the diffusion of hydrogen ions and increase the hydrogen ion concentration in the oxide sidewalls 30 . The oxygen ions and hydrogen ions in the oxide sidewall 30 can form a covalent bond HBO≡Si with the boron ions in the well region 103 of the first conductivity type and the boron ions in the substrate 101 as shown in FIG. 7 . The covalent bond HBO≡Si has strong stability. Therefore, the greater the hydrogen ion concentration in the oxide sidewall 30, the more boron ions in the well region 103 and the substrate 101 are attracted, thereby reducing the boron ion concentration in the well region 103 of the first conductivity type, thereby slowing down the PMOS and speeding up the NMOS. As shown in FIGS. 8 and 9 , there is a strong linear relationship between the thickness of the passivation sidewall 40 and the N / P ratio of the MOS. The thicker the passivation sidewall 40, the smaller the N / Pratio of the threshold voltage and the larger the N / P ratio of the saturation current. By adjusting the thickness of the passivation sidewall 40, the ability of the oxide sidewall 30 to attract the boron ion concentration in the well region 103 can be changed, and the speed of the PMOS and NMOS can be effectively adjusted. The method has strong adjustability and wide applicability and can be applied to more CMOS devices.
[0069] In the embodiment of the present application, in the thermal oxidation atmosphere, the oxide sidewall 30 attracts the boron ions in the well region 103 of the first conductivity type and the boron ions in the substrate 101, thereby reducing the boron ion concentration in the well region 103 of the first conductivity type, thereby slowing down the PMOS and speeding up the NMOS, and by adjusting the thickness of the passivation sidewall 40, the ability of the oxide sidewall 30 to attract the boron ion concentration in the well region 103 can be changed, and the speed of the PMOS and NMOS can be effectively adjusted. Therefore, in the embodiment of the present application, there is no need to adjust the relevant parameters of the ion implantation multiple times in the ion implantation process and perform multiple ion implantations. The electrical properties of the PMOS and NMOS can be effectively adjusted by the oxide sidewall 30 attracting the boron ions in the well region 103 of the first conductivity type and the boron ions in the substrate 101, and by adjusting the thickness of the passivation sidewall 40, thereby avoiding damage such as atomic dislocation caused by ion implantation.
[0070] In some embodiments, referring to FIG. 4 and FIG. 10 , forming the gate structure 20 on the surface of the active region 104 away from the deep well region 102 may include the following steps:
[0071] S121: forming a gate oxide layer on a surface of the active region away from the deep well region, wherein the gate oxide layer is flush with a surface of the passivation sidewall in a thickness direction of the substrate.
[0072] As an example, a thermal oxidation process may be used but is not limited to form the gate oxide layer 201 on the surface of the active region 104 away from the deep well region 102. Specifically, in this embodiment, the gate oxide layer is a silicon dioxide layer.
[0073] S122: forming a gate conductive layer on a surface of the gate oxide layer away from the active region to form a gate structure.
[0074] As an example, a physical vapor deposition process (PVD), a chemical vapor deposition process (CVD), or an atomic layer deposition process (ALD) may be used but is not limited to form a gate conductive layer 202 on a surface of the gate oxide layer 201 away from the active area 104. Specifically, in the present embodiment, the gate conductive layer 202 is a polysilicon layer.
[0075] In the embodiment of the present application, by forming a gate structure 20 on the surface of the active region 104 away from the deep well region 102, the current and conductivity of the device can be controlled by changing the voltage of the gate structure 20, and the gate structure 20 in the embodiment of the present application has a small capacitance and a fast response speed to signals.
[0076] In some embodiments, please continue to refer to FIG. 4 , the passivation spacer 40 includes a silicon nitride spacer, and the thickness of the passivation spacer 40 is positively correlated with the ability to block the diffusion of hydrogen elements in the oxide spacer 30 .
[0077] As an example, the passivation sidewall 40 is a silicon nitride sidewall. The thicker the passivation sidewall 40 is, the stronger the barrier to the diffusion of hydrogen in the oxide sidewall 30 is. Thus, the oxide sidewall 30 has a stronger attraction to the boron element, and the concentration of the boron element in the PMOS is lower. Therefore, the speed of the PMOS and NMOS can be adjusted by adjusting the thickness of the passivation sidewall 40.
[0078] An embodiment of the present application provides a semiconductor structure. Please continue to refer to FIG. 4 . The semiconductor structure may include: a semiconductor initial structure 10 , a gate structure 20 , an oxide spacer 30 and a passivation spacer 40 .
[0079] The semiconductor initial structure 10 includes a substrate 101, and a deep well region 102, a well region 103 of a first conductivity type, and an active region 104 of a second conductivity type sequentially stacked on the substrate 101; the substrate 101 is doped with boron.
[0080] As an example, the substrate 101 may include but is not limited to at least one of a silicon substrate, a gallium nitride (GaN) substrate, a silicon carbide (SiC) substrate, a sapphire substrate, a silicon on insulator (SOI) substrate, a silicon on diamond (SOD) substrate, and a strained layer silicon substrate deposited on a germanium silicon wafer. Specifically, in the present embodiment, the substrate 101 is a silicon substrate, and the silicon substrate is doped with boron.
[0081] Exemplarily, the first conductivity type may include a P-type conductivity type or an N-type conductivity type. Specifically, in this embodiment, the well region 103 of the first conductivity type is a P-type well region, and the active region 104 of the second conductivity type is an N-type active region.
[0082] The gate structure 20 is located on a surface of the active region 104 away from the deep well region 102 ; wherein a projection of the gate structure 20 toward the well region 103 falls into the well region 103 .
[0083] The oxide spacer 30 and the passivation spacer 40 are sequentially located on the sidewalls of the gate structure 20 ; wherein the projections of the oxide spacer 30 and the passivation spacer 40 toward the active area 104 fall into the active area 104 , the oxide spacer 30 is used to absorb boron elements, and the passivation spacer 40 is used to block the diffusion of hydrogen elements in the oxide spacer 30 .
[0084] As an example, the oxide spacer 30 contains hydrogen ions, and the passivation spacer 40 may include but is not limited to a silicon nitride spacer.
[0085] In the embodiment of the present application, the semiconductor initial structure 10 includes a substrate 101, and a deep well region 102, a well region 103 of the first conductivity type, and an active region 104 of the second conductivity type sequentially stacked on the substrate 101; the substrate 101 is doped with boron; then a gate structure 20 is arranged, which is located on the surface of the active region 104 away from the deep well region 102; wherein the projection of the gate structure 20 toward the well region 103 falls into the well region 103; and then an oxide sidewall 30 and a passivation sidewall 40 are arranged, which are sequentially located on the sidewalls of the gate structure 20; wherein the projection of the oxide sidewall 30 and the passivation sidewall 40 toward the active region 104 falls into the active region 104. The boron element in the substrate 101 and the boron element in the well region 103 of the first conductivity type can be attracted to the oxide sidewall 30 to reduce the boron element in the well region 103 of the first conductivity type, thereby making the PMOS slower and the NMOS faster. The passivation sidewall 40 blocks the diffusion of hydrogen in the oxide sidewall 30, thereby enhancing the attraction of the oxide sidewall 30 to the boron element. The thicker the passivation sidewall 40 is, the stronger the blocking ability of the diffusion of hydrogen in the oxide sidewall 30 is, and the stronger the attraction of the oxide sidewall 30 to the boron element is, and the lower the concentration of the boron element in the PMOS is. Therefore, the speed of the PMOS and NMOS can be adjusted by adjusting the thickness of the passivation sidewall 40, which solves the problem that when adjusting the electrical properties of the semiconductor structure, the NMOS and PMOS cannot be adjusted in both directions at the same time, and there is no need to adjust the parameters such as the concentration of ion implantation multiple times, thereby avoiding the problem of damage such as dislocation inside the semiconductor structure, and improving the reliability and electrical properties of the semiconductor structure.
[0086] In some embodiments, please continue to refer to FIG. 4 , the well region 103 of the first conductivity type is doped with boron.
[0087] As an example, the well region 103 of the first conductivity type is doped with boron. When the concentration of the doped boron is high, the speed of PMOS is fast and the speed of NMOS is slow; when the concentration of the doped boron is low, the speed of PMOS is slow and the speed of NMOS is fast. Therefore, the concentration of the doped boron in the well region 103 of the first conductivity type can be adjusted to adjust the speed of PMOS and NMOS in both directions.
[0088] In this embodiment, the first conductivity type well region 103 is doped with boron, and the concentration of the boron doped in the first conductivity type well region 103 can be adjusted to adjust the speed of the PMOS and NMOS in both directions.
[0089] In some embodiments, referring to FIG. 6 to FIG. 9 , oxygen ions in the oxide spacer 30 form covalent bonds with boron ions in the well region 103 of the first conductivity type and boron ions in the substrate.
[0090] As an example, as shown in FIG. 6 , in a thermal oxidation atmosphere, boron ions in the well region 103 and boron ions in the substrate 101 will be transferred to the oxide sidewalls 30 , and hydrogen ions in the oxide sidewalls 30 will also diffuse. The passivation sidewalls 40 can block the diffusion of hydrogen ions and increase the hydrogen ion concentration in the oxide sidewalls 30 . The oxygen ions and hydrogen ions in the oxide sidewall 30 can form a covalent bond HBO≡Si with the boron ions in the well region 103 of the first conductivity type and the boron ions in the substrate 101 as shown in FIG. 7 . The covalent bond HBO≡Si has strong stability. Therefore, the greater the hydrogen ion concentration in the oxide sidewall 30, the more boron ions in the well region 103 and the substrate 101 are attracted, thereby reducing the boron ion concentration in the well region 103 of the first conductivity type, thereby slowing down the PMOS and speeding up the NMOS. As shown in FIGS. 8 and 9 , there is a strong linear relationship between the thickness of the passivation sidewall 40 and the N / P ratio of the MOS. The thicker the passivation sidewall 40, the smaller the N / Pratio of the threshold voltage and the larger the N / P ratio of the saturation current. By adjusting the thickness of the passivation sidewall 40, the ability of the oxide sidewall 30 to attract the boron ion concentration in the well region 103 can be changed, and the speed of the PMOS and NMOS can be effectively adjusted. The method has strong adjustability and wide applicability and can be applied to more CMOS devices.
[0091] In the embodiment of the present application, in the thermal oxidation atmosphere, the oxide sidewall attracts the boron ions in the well region 103 of the first conductivity type and the boron ions in the substrate, thereby reducing the boron ion concentration in the well region 103 of the first conductivity type, thereby slowing down the PMOS and speeding up the NMOS, and by adjusting the thickness of the passivation sidewall 40, the ability of the oxide sidewall 30 to attract the boron ion concentration in the well region 103 can be changed, and the speed of the PMOS and NMOS can be effectively adjusted. Therefore, in the embodiment of the present application, there is no need to adjust the relevant parameters of the ion implantation multiple times in the ion implantation process and perform multiple ion implantations. The electrical properties of the PMOS and NMOS can be effectively adjusted by the oxide sidewall 30 attracting the boron ions in the well region 103 of the first conductivity type and the boron ions in the substrate, and by adjusting the thickness of the passivation sidewall 40, thereby avoiding damage such as atomic dislocation caused by ion implantation.
[0092] In some embodiments, please continue to refer to Figure 4, the gate structure 20 may include: a gate oxide layer 201, located on the surface of the active area 104 away from the deep well area 102; the gate oxide layer 201 is flush with the surface of the passivation sidewall 40 in the thickness direction of the substrate 101; and a gate conductive layer 202, located on the surface of the gate oxide layer 201 away from the active area 104.
[0093] As an example, the gate oxide layer 201 may include but is not limited to a silicon dioxide layer, and the gate conductive layer 202 may include but is not limited to a polysilicon layer.
[0094] In the embodiment of the present application, the current and conductivity of the device can be controlled by changing the voltage of the gate structure 20, and the gate structure in the embodiment of the present application has a small capacitance and a fast response speed to the signal.
[0095] In some embodiments, please continue to refer to FIG. 4 , the semiconductor structure may further include: a plurality of shallow trench isolation structures 50 , the shallow trench isolation structures 50 penetrate the semiconductor initial structure 10 , and the upper surface of the shallow trench isolation structures 50 is higher than the upper surface of the semiconductor initial structure.
[0096] As an example, a silicon nitride mask may be used to form a groove after deposition, patterning, and etching of silicon, and the groove may be filled with deposited oxide to form a shallow trench isolation structure 50 for isolation from the substrate.
[0097] In the embodiment of the present application, a plurality of shallow trench isolation structures 50 are provided, each shallow trench isolation structure 50 penetrates the semiconductor initial structure 10, and the upper surface of the shallow trench isolation structure 50 is higher than the upper surface of the semiconductor initial structure, so as to achieve the effect of isolation from the substrate 101, and the shallow trench isolation structure 50 can also serve as an effective barrier layer to prevent leakage current from being generated in the sidewall structure of the device.
[0098] In some embodiments, please continue to refer to FIG. 4 , the passivation spacer 40 includes a silicon nitride spacer, and the thickness of the passivation spacer 40 is positively correlated with the ability to block the diffusion of hydrogen elements in the oxide spacer 30 .
[0099] As an example, the passivation sidewall 40 is a silicon nitride sidewall. The thicker the passivation sidewall 40 is, the stronger the barrier to the diffusion of hydrogen in the oxide sidewall 30 is. Thus, the oxide sidewall 30 has a stronger attraction to the boron element, and the concentration of the boron element in the PMOS is lower. Therefore, the speed of the PMOS and NMOS can be adjusted by adjusting the thickness of the passivation sidewall 40.
[0100] In summary, the present application provides a semiconductor structure and a method for preparing the same. By sequentially forming an oxide sidewall and a passivation sidewall on the sidewall of the gate structure, the unexpected effect is that the boron element in the substrate and the boron element in the well region of the first conductivity type can be attracted to the oxide sidewall to reduce the boron element in the well region of the first conductivity type, thereby slowing down the PMOS and speeding up the NMOS. The passivation sidewall blocks the diffusion of hydrogen elements in the oxide sidewall, thereby enhancing the attraction of the oxide sidewall to the boron element. The thicker the passivation sidewall, the stronger the blocking ability to the diffusion of hydrogen elements in the oxide sidewall, the stronger the attraction of the oxide sidewall to the boron element, and the lower the concentration of the boron element in the PMOS. Therefore, the speed of the PMOS and NMOS can be adjusted by adjusting the thickness of the passivation sidewall, which solves the problem that when the semiconductor structure is electrically adjusted, the NMOS and PMOS cannot be adjusted bidirectionally at the same time, and there is no need to adjust the parameters such as the concentration of ion implantation multiple times, thereby avoiding the problem of damage such as dislocation inside the semiconductor structure, and improving the reliability and electrical properties of the semiconductor structure.
[0101] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features of the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0102] The above-described embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be construed as limiting the scope of the patent application. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the patent application shall be subject to the attached claims.
Claims
1. A method for preparing a semiconductor structure, It is characterized in that include: A semiconductor initial structure is provided, wherein the semiconductor initial structure comprises a substrate, and a deep well region, a well region of a first conductivity type, and an active region of a second conductivity type which are sequentially formed and stacked in the substrate; the substrate is doped with boron; A gate structure is formed on a surface of the active region away from the deep well region; wherein a projection of the gate structure toward the well region falls into the well region; An oxide sidewall and a passivation sidewall are sequentially formed on the sidewalls of the gate structure; wherein the projections of the oxide sidewall and the passivation sidewall toward the active area fall into the active area, the oxide sidewall is used to absorb the boron element, and the passivation sidewall is used to block the diffusion of hydrogen elements in the oxide sidewall.
2. The method for preparing a semiconductor structure according to claim 1, It is characterized in that The step of forming the well region of the first conductivity type comprises: forming an initial well region on a surface of the deep well region away from the substrate; Boron ions are implanted into the initial well region to form a well region of the first conductivity type.
3. The method for preparing a semiconductor structure according to claim 2, It is characterized in that After the oxide sidewall and the passivation sidewall are sequentially formed on the sidewall of the gate structure, the method further includes: The resulting structure is placed in a thermal oxidation atmosphere to activate the well region of the first conductivity type.
4. The method for preparing a semiconductor structure according to claim 3, It is characterized in that In the thermal oxidation atmosphere, oxygen ions in the oxide sidewalls form covalent bonds with boron ions in the well region of the first conductivity type and boron ions in the substrate.
5. The method for preparing a semiconductor structure according to claim 1, It is characterized in that The passivation spacer includes a silicon nitride spacer, and the thickness of the passivation spacer is positively correlated with the blocking capability of blocking the diffusion of hydrogen elements in the oxide spacer.
6. A semiconductor structure, It is characterized in that include: A semiconductor initial structure, wherein the semiconductor initial structure comprises a substrate, and a deep well region, a well region of a first conductivity type, and an active region of a second conductivity type sequentially stacked on the substrate; the substrate is doped with boron; A gate structure is located on a surface of the active region away from the deep well region; wherein a projection of the gate structure toward the well region falls into the well region; The oxide sidewalls and the passivation sidewalls are sequentially located on the sidewalls of the gate structure; wherein the projections of the oxide sidewalls and the passivation sidewalls toward the active area fall into the active area, the oxide sidewalls are used to absorb the boron element, and the passivation sidewalls are used to block the diffusion of hydrogen elements in the oxide sidewalls.
7. The semiconductor structure according to claim 6, It is characterized in that The well region of the first conductivity type is doped with boron.
8. The semiconductor structure according to claim 7, It is characterized in that Oxygen ions in the oxide spacer form covalent bonds with boron ions in the well region of the first conductivity type and boron ions in the substrate.
9. The semiconductor structure according to claim 6, It is characterized in that The passivation sidewall spacer includes a silicon nitride sidewall spacer, and the thickness of the passivation sidewall spacer is negatively correlated with the diffusion of hydrogen elements in the oxide sidewall spacer.
10. The semiconductor structure according to claim 6, It is characterized in that The semiconductor structure further comprises: A plurality of shallow trench isolation structures are provided, each of the shallow trench isolation structures penetrates the semiconductor initial structure, and an upper surface of the shallow trench isolation structure is higher than an upper surface of the semiconductor initial structure.
Citation Information
Patent Citations
Thin-film transistor and manufacture thereof
JP1995153958A
Method for manufacturing semiconductor device
JP2001319972A
Novel gate sidewall spacer and method of manufacture therefor
US20070004156A1
Cited By
Semiconductor structure and preparation method thereof
CN116259650A
Semiconductor device and preparation method
CN119653824A