Fluidized bed reactor for post-treatment of powdered carbon
By combining plasma technology in a fluidized bed reactor, the carbon nanoparticles are post-treated, and the efficiency and uniformity of powdered carbon treatment in the prior art are solved, thereby achieving efficient carbon nanoparticle treatment.
Patent Information
- Application Number
- CN202380031465.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-05-09
- Filing Date
- 2023-05-05
- Publication Date
- 2024-11-15
AI Technical Summary
The prior art cannot effectively post-treat powdered carbon on industrial scale, especially in fluidized bed architectures, where conventional semiconductor plasma instruments cannot adopt plasma fluidized bed technology, and it is difficult to provide uniformity in vacuum chambers or vacuum drum systems. and efficient handling.
A system including a fluidized bed reactor, a gas feed source, an intake valve, a gas-solid separator and an energy source was designed, and carbon nanoparticles were post-treated in the fluidized bed using plasma technology and subjected to electromagnetic excitation. The excitation and processing of carbon nanoparticles is achieved by microwave-coupling plasma torches, enhancing the energy transfer rate and processing efficiency.
Achieve uniform treatment of carbon nanoparticles, improve the flux efficiency of the fluidized bed reactor, and can efficiently perform carbon powder post-treatment on industrial scale, provide tunable gas temperature and residence time, ensuring the treatment Uniformity and efficiency.
Smart Images

Figure CN118973697A_ABST
Abstract
Description
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS
[0002] This patent application claims priority to U.S. Patent Application No. 17 / 739,397, filed on May 9, 2022, entitled "FLUIDIZED BED REACTORS FOR POS T-PROCESSING POWDERED CARBON", which has been assigned to the assignee of this application. The disclosures of all prior applications are considered part of and incorporated by reference into this patent application. Technical Field
[0003] The present disclosure relates generally to processing carbon particles, and more particularly to post-processing carbon powder in a fluidized bed. Background Art
[0004] Reactors are typically included to hold various raw materials, such as carbon (also known as "carbonaceous") particles, which may undergo further processing (known as "post-processing") before being shipped to customers. Through post-processing, the raw materials can be energetically excited by microwave radiation to produce final products, such as carbon-on-carbon growth and / or metal-decorated carbon nanoparticles. For example, the final product can be used in electric vehicle (EV) battery components. Various types of chemical treatment methods can be used to post-process carbon particles, such as plasma-based post-processing methods. These methods provide a way to obtain desired chemicals at energy levels that are not available through conventional thermal processes or liquid-based processes. In addition, the energy transfer between plasma materials and raw material gases is faster than the convection heating used in thermal processes. Therefore, plasma-based post-processing methods can complement fluidized bed architectures, which also provide rapid energy transfer and thus tend to improve the flux efficiency of reactors during batch post-processing of carbon particles. Therefore, what is needed is to further improve the post-processing of carbon powders in fluidized beds. Summary of the invention
[0005] This Summary is provided to introduce a selection of concepts in a simplified form that are further described below in the Detailed Description. This Summary is not intended to identify key features or essential features of the claimed subject matter, nor is it intended to limit the scope of the claimed subject matter.
[0006] An innovative aspect of the subject matter described in the present disclosure may be implemented as a system for post-processing carbon materials in a fluidized bed (e.g., a plasma fluidized bed). In some aspects, the system may include a fluidized bed reactor having an interior including a fluidized bed region. The fluidized bed reactor may be formed as an elongated tube having a top section, a bottom section positioned relative to the top section, a length extending from the top section toward the bottom section, and an outlet extending from the bottom section. In addition, the fluidized bed reactor may have a gas feed source coupled to the fluidized bed reactor. In this way, the gas feed source may output a gas phase mixture to the interior of the fluidized bed reactor. In some cases, an inlet valve may be coupled to a gas feed source and fluidly connected. In this way, the inlet valve may be opened and / or closed and the flow rate of the gas phase mixture entering the interior of the fluidized bed reactor may be adjusted accordingly. In one embodiment, a gas-solid separator may be positioned in the fluidized bed reactor upstream of the inlet valve. The gas-solid separator may be used, for example, to separate solids from gases in a mixture processed in the interior of the fluidized bed reactor. The outlet of the fluidized bed reactor may output a gas phase mixture or one or more of other gases associated with the operation of the fluidized bed reactor. For example, the gas phase mixture may have a pressure between 1 mTorr and 760 Torr.
[0007] In some other aspects, the fluidized bed reactor may be formed as an elongated cylindrical tube, the elongated cylindrical tube comprising a main section having a first cross-sectional diameter and a tapered section connected to the main section, the tapered section having at least a second cross-sectional diameter that may be different from the first cross-sectional diameter. For example, in some aspects, the tapered section may limit carbon nanoparticles preloaded into the fluidized bed region prior to operation of the fluidized bed reactor. In addition, the tapered section may include a contraction region that may increase the fluid velocity associated with the insertion of a gas phase mixture that may include one or more of a pure gas or a mixture of two or more gases. The gas phase mixture may prevent at least some carbon nanoparticles from escaping from the fluidized bed reactor. In addition, in some aspects, the fluidized bed reactor may have a cross-sectional area formed as one of a rectangle, a square, a bell, a circle, or an ellipse.
[0008] In some embodiments, the carbon nanoparticles in powder form can be loaded into the fluidized bed region before the operation of the fluidized bed reactor. The carbon nanoparticles may include one or more non-hollow carbon spheres (NHCS) particles. In this way, the carbon nanoparticles can be fluidized above the gas-solid separator based on the gas phase mixture flowing into the fluidized bed region. In addition, the carbon nanoparticles can be electromagnetically excited, and the electromagnetic excitation is caused by an energy source. In some cases, the pressure control assembly is connected to the fluidized bed reactor and can control one or more of the pressure or gas velocity associated with the fluidization of the carbon nanoparticles in the fluidized bed region.
[0009] In addition, the system may include an energy source that can operate in a pulsed mode or a continuous mode. The energy source may be or may include an inductively coupled plasma source, a capacitively coupled plasma source, a microwave coupled plasma torch, a microwave coupled surface wave source, a DC coupled plasma source, a DC coupled arc source, or a pulsed DC plasma source. In some cases, the microwave coupled plasma torch may operate at a pressure between 1 mTorr and 760 Torr. In addition, the microwave coupled plasma torch may be positioned along one or more sides of the fluidized bed reactor or positioned adjacent to a gas feed source. The microwave coupled plasma torch may disperse a large amount of additional plasma phase mixture into the interior of the fluidized bed reactor. In this way, a large amount of additional plasma phase mixture may energetically excite one or more of a gas phase mixture, a plasma phase mixture, or carbon nanoparticles. The interior of the fluidized bed reactor may retain one or more of a gas phase mixture or a plasma phase mixture. In addition, the inductively coupled plasma source may be formed as a coil surrounding the fluidized bed reactor.
[0010] In some aspects, the energy source may be positioned at one or more positions relative to the inlet valve and / or may be positioned away from the fluidized bed reactor. In some other aspects, the energy source may be positioned at one or more positions of the energy source including one of the following: downstream of the inlet valve, upstream of the fluidized bed region, adjacent to the fluidized bed region, or downstream of the fluidized bed region. In one embodiment, the energy source may be coupled to the fluidized bed reactor. In this way, the energy source electromagnetically excites the gas phase mixture and produces a plasma phase mixture. In some aspects, the plasma phase mixture may be formed in a plasma region that is positioned adjacent to or within the interior of the fluidized bed reactor. The plasma region may be characterized by one or more of a gas temperature, an electron temperature and velocity, or a fluid flow rate.
[0011] In some cases, a vacuum pump may be coupled to a fluidized bed reactor and thereby control the formation of a fluidized bed region. For example, a vacuum pump and / or an energy source may control the energy properties of a plasma phase mixture in a fluidized bed reactor. In some aspects, an energy source may produce a plasma phase mixture as one or more of a thermal equilibrium plasma phase mixture or a non-thermal equilibrium plasma phase mixture. In addition, a control knob may be coupled to a fluidized bed reactor. In this way, a control knob may set a thermal equilibrium setting for a plasma phase mixture. For example, a thermal equilibrium setting may produce a thermal equilibrium plasma phase mixture or a non-thermal equilibrium plasma phase mixture. In addition, a thermal equilibrium setting may control energy properties associated with one or more of a plasma phase mixture or a gas phase mixture. For example, in some cases, energy properties may include an energy transfer rate between a plasma phase mixture and a gas phase mixture. In some other cases, energy properties may include a plasma-material interaction based on the interaction between a plasma phase mixture and carbon nanoparticles.
[0012] In some cases, the energy management device can be located remote from the fluidized bed reactor. The energy management device can include a matching network that controls energy excitation of the gas phase mixture via an energy source. In some aspects, a side port can be formed in the fluidized bed reactor to supply additional gas phase mixture to the fluidized bed reactor. In some cases, the fluidized bed region can be associated with a fluidized bed architecture that can control residence time associated with operation of the matching network.
[0013] Details of one or more embodiments of the subject matter described in the present disclosure are set forth in the accompanying drawings and the following description. Other features, aspects, and advantages will become apparent from the specification, drawings, and claims. Note that the relative sizes of the following figures may not be drawn to scale. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] The drawings described below are for illustration purposes only. The drawings are not intended to limit the scope of the present disclosure.
[0015] Figure 1 An exemplary system for post-processing carbon nanoparticles in a fluidized bed reactor is shown, according to some embodiments.
[0016] Figure 2A According to some embodiments Figure 1 An exemplary configuration of a fluidized bed reactor is depicted.
[0017] Figure 2B According to some embodiments Figure 1 Another exemplary configuration of a fluidized bed reactor is depicted.
[0018] Figure 3According to some embodiments Figure 1 Another exemplary configuration of a fluidized bed reactor is depicted.
[0019] Figure 4 According to some embodiments Figure 1 Another exemplary configuration of a fluidized bed reactor is depicted.
[0020] Figure 5 According to some embodiments Figure 1 Another exemplary configuration of a fluidized bed reactor is depicted.
[0021] Figure 6 According to some embodiments Figure 1 An exemplary recirculating bed configuration for at least a section of a fluidized bed reactor is depicted.
[0022] Figure 7 According to some embodiments Figure 1 An exemplary reactor for producing carbon particles or post-processing carbon nanoparticles is depicted.
[0023] Figure 8 According to some embodiments Figure 1 Another exemplary reactor for producing carbon particles or post-processing carbon nanoparticles is depicted.
[0024] Fig. 9 According to some embodiments, Figure 1 Exemplary few-layer graphene (FLG) nanosheets produced by the depicted system.
[0025] Fig.10 A micrograph of a graphene material produced by sulfuric acid (H2SO4) exfoliation from graphite is shown, according to some embodiments.
[0026] Fig.11 Micrographs showing wavy and / or wrinkled graphene based on microwave energy, according to some embodiments.
[0027] Fig.12 Shown is a photomicrograph of exemplary carbon particles according to some embodiments.
[0028] Fig.13A A diagram showing exemplary carbon particles according to some embodiments.
[0029] Fig. 13B shows a representation according to some embodiments Figure 5 An exemplary step function for an exemplary carbon particle of A.
[0030] Fig.14Shown is a graph depicting an exemplary distribution of pore volume versus pore width for exemplary carbon particles according to some embodiments.
[0031] Fig.15A Shown are photomicrographs of exemplary carbon particles, aggregates, and / or agglomerates according to some embodiments.
[0032] Fig. 15B Shown are photomicrographs of exemplary carbon particles, aggregates, and / or agglomerates according to some embodiments.
[0033] Fig.16 Shown is a graph depicting the cumulative pore volume versus pore width of micropores and mesopores dispersed throughout an exemplary carbon particle according to some embodiments.
[0034] Fig.17 Exemplary configurations of exemplary carbon particles according to some embodiments are shown.
[0035] Fig.18 A diagram depicting an exemplary battery according to some embodiments is shown.
[0036] Throughout the various drawings, like reference numbers and names refer to like elements. DETAILED DESCRIPTION
[0037] The following description relates to some exemplary embodiments for the purpose of describing the innovative aspects of the present disclosure. However, one of ordinary skill in the art will readily recognize that the teachings herein can be applied in a variety of different ways. The described embodiments can be implemented in any type of fluidized bed reactor and can be used to post-process carbon particles. Therefore, the disclosed embodiments are not limited to the examples provided herein, but rather encompass all embodiments contemplated by the appended claims. In addition, well-known elements of the present disclosure will not be described in detail or will be omitted to avoid obscuring the relevant details of the present disclosure.
[0038] Plasma-based processing of gaseous and / or solid materials has become a preferred solution for chemical manufacturing. In such a setting, an energy source (e.g., an inductively coupled plasma, "ICP") can be used to energetically excite a reaction chamber containing one or more raw materials (e.g., hydrocarbon gases, such as methane (CH4)) or semi-finished materials (e.g., carbon particles) intended for post-processing. In order to process raw materials such as gases, the energy source can electromagnetically excite the hydrocarbon gas and thereby crack it, promoting the self-ignition of the gas to form a plasma (e.g., including one or more plasma-based substances). Typically, the plasma may not exist in a thermal equilibrium state within the reaction chamber and may thus constantly change physical parameters. This constant change within the plasma creates an energy environment that is favorable, for example, for further dissociation of cracked hydrocarbons into methyl radicals (CH3·), which can combine and recombine in cooler regions of the reaction chamber to self-nucleate and produce desired output products, such as carbon materials in powder form (e.g., referred to herein as "carbon particles"). In addition, for post-processing operations, the plasma can promote various plasma-material interactions (e.g., ion bombardment) that may be suitable for certain post-processing methods (e.g., carbon growth on carbon). Typically, the reaction chamber containing methyl radicals can be operated at relatively high power coupling efficiency and low ion energy. In this way, the output carbon material may include few-layer graphene (FLG), graphitized materials, carbon nano onions (CNO), etc. In some cases, the carbon material can be further post-processed into a layered material in the reaction chamber. The layered material can then be incorporated into various consumer products such as carbon-based automobile bumpers, battery electrodes, and harmful gas sensors.
[0039] It is noteworthy that certain plasma-based post-processing methods (e.g., including those used in the semiconductor industry) can provide several desirable performance-related features compared to conventional hot gas-phase and / or liquid-phase post-processing methods. These features may include the ability to obtain certain chemicals (e.g., raw materials and / or semi-finished products) at lower energy levels that are not conveniently available in conventional thermal and / or liquid-based methods. In addition, the observed energy transfer rate between the plasma species and the gas contained in the reaction chamber is faster than convective heating (e.g., as used in thermal processes). In this way, plasma-based post-processing methods often complement reactors including reaction vessels with fluidized bed architectures, thereby facilitating efficient batch processing. Plasma-based post-processing methods can result in high-energy ion bombardment, which can improve the flux efficiency of certain processing methods (e.g., reactive ion etching). High-energy ion bombardment is not available in conventional (e.g., thermal) processing methods.
[0040] Aspects of the present disclosure recognize that conventional semiconductor plasma instruments cannot use plasma fluidized bed technology to post-process powdered substrates. In addition, such instruments may not be able to post-process powdered substrates at industrial (e.g., 10 kg / hour or higher) levels. According to various aspects of the subject matter disclosed herein, a system for post-processing carbon powder is provided. In some cases, the system may include a fluidized bed reactor having an interior including a fluidized bed region. The system may include a gas feed source, an inlet valve, a gas-solid separator, and an energy source may be coupled to the fluidized bed reactor. Carbon nanoparticles in powder form may be loaded into the fluidized bed region prior to operation of the fluidized bed reactor. The energy management device may be positioned away from the fluidized bed reactor. The gas feed source may output a gas phase mixture into the interior of the fluidized bed reactor. In this way, the energy source may electromagnetically excite the gas phase mixture and produce a plasma phase mixture, which is formed in a plasma region, which is positioned adjacent to or within the interior of the fluidized bed reactor. The energy source may be positioned at one or more positions relative to the inlet valve.
[0041] Aspects of the subject matter disclosed herein may include using the system to perform one or more plasma-based carbon powder post-processing methods, including heteroatom doping, carbon-on-carbon growth, plasma activation, metal decoration, plasma-based etching, carbide formation and / or growth, carbon phase changes (e.g., sp 2 Hybridized to sp 3 Hybridization) or carbon-on-carbon grafting. Typically, these processes are performed in static vacuum chambers or vacuum drum systems, making industrial scale-up difficult or perhaps impossible. In addition, vacuum chambers or vacuum drum systems may not provide uniformity of post-processing treatments, resulting in irregular semi-finished material that is not suitable for customer use. Aspects of the subject matter disclosed herein may include using a fluidized bed architecture to uniformly treat (e.g., post-treat) carbon particles and / or powders, directly control residence time, energy transfer rate, and provide adjustable gas temperature treatments.
[0042] Figure 1An exemplary system 100 for post-processing carbon nanoparticles in a fluidized bed reactor according to some embodiments is shown. In some cases, the system may include: a fluidized bed reactor 110 having an interior 112 including a fluidized bed region 114; and an energy source 120, the energy source being coupled to a coil 122 positioned proximate to the fluidized bed reactor 110. The fluidized bed reactor 110 may be formed as an elongated tube 111 having a top section 180, a bottom section 190 positioned opposite the top section 180, a length extending from the top section 180 toward the bottom section 190, and an outlet 195 extending from the bottom section. In addition, the fluidized bed reactor 110 may be coupled to a gas feed source 130. In this manner, the gas feed source 130 may feed a gas phase mixture (e.g., including one or more hydrocarbon gases, such as methane (CH4), and not shown for simplicity) to the fluidized bed reactor 110. Figure 1 112 of the fluidized bed reactor 110. For example, in some cases, the gaseous mixture may include one or more of a pure gas or a mixture of two or more gases. In some cases, an inlet valve 134 may be coupled to and / or fluidically connected to the gas feed source 130. In this way, the inlet valve 134 may be opened and / or closed and accordingly adjust the flow rate of the gaseous mixture entering the interior 112 of the fluidized bed reactor 110. In one embodiment, a gas-solid separator 116 may be positioned within the fluidized bed reactor 110 upstream of the inlet valve 134. The gas-solid separator 116 may be used, for example, to separate solids from gases in a mixture being processed within the interior 112 of the fluidized bed reactor 110. The outlet of the fluidized bed reactor may output a gaseous mixture or other gases associated with the operation of the fluidized bed reactor (not shown for simplicity). Figure 1 ) and / or post-treated particles 160. For example, the gas phase mixture may have a pressure between 1 mTorr and 760 Torr. In operation, the carbon nanoparticles 118 may be suspended in a fluidized bed region 114 within the interior 112 of the fluidized bed reactor 110. In this way, at least some of the carbon nanoparticles 118 may be treated and / or post-treated by the gas and / or plasma species generated when the gas is energetically excited within the interior 112. The post-treatment operation may, for example, grow additional carbon on the exposed surfaces of the carbon nanoparticles 118, thereby providing carbon-on-carbon growth. Other post-treatment operations may also be supported by the fluidized bed reactor 110 and described elsewhere in this disclosure.
[0043] In some other aspects, the fluidized bed reactor 110 can be formed as an elongated tube 111 (eg, an elongated cylindrical tube) that can include a main section (not shown for simplicity) having a first cross-sectional diameter. Figure 1) and a conical section coupled to the main section. The conical section may have at least a second cross-sectional diameter that may be different from the first cross-sectional diameter. For example, in some aspects, the conical section may at least temporarily confine carbon nanoparticles 118 preloaded into the fluidized bed region 114 prior to operation of the fluidized bed reactor 110. In addition, the conical section may include a constriction region (not shown for simplicity). Figure 1 ), the constricted region can increase the fluid velocity associated with the insertion of the gas phase mixture. In this way, the gas phase mixture can prevent the carbon nanoparticles 118 from escaping from the fluidized bed reactor 110. In addition, in some aspects, the fluidized bed reactor 110 can have a cross-sectional area formed as one of a rectangle, a square, a bell, a circle, or an ellipse (not shown for simplicity). Figure 1 ).
[0044] In some embodiments, the carbon nanoparticles 118 can be prepared in powder form and can be loaded into the fluidized bed region before the operation of the fluidized bed reactor. In some cases, the carbon nanoparticles 118 may include one or more non-hollow carbon spheres (NHCS) particles, as described elsewhere in this disclosure. In this way, the carbon nanoparticles 118 can be fluidized above the gas-solid separator 116 based on the gas phase mixture flowing into the fluidized bed region 114. In addition, the carbon nanoparticles 118 can be electromagnetically excited, such as the energy source 120 and / or the coil 122. In addition, in some cases, the pressure control assembly 150 can be connected to the fluidized bed reactor 110, so that the pressure or gas velocity associated with the fluidization of the carbon nanoparticles 118 in the fluidized bed region 114 can be controlled. In some other cases, the system 100 can be configured to be connected to the plasma feed source 140 through a plasma feed line 142, and the plasma feed source may contain one or more plasma-based substances (e.g., methyl radicals CH3·), and the plasma feed line is controlled by a plasma pressure controller 144. In this manner, additional amounts of energizing species (eg, plasma-based species stored in a plasma feed source) may be added to the gas flowing into the fluidized bed region 114 to provide additional tunability of the system 100 .
[0045] In addition, with respect to the process tunability of the system 100, the system may include an energy source 120 that can operate in a pulsed mode or a continuous mode. For example, the energy source 120 can be or can include an inductively coupled plasma source, a capacitively coupled plasma source, a microwave coupled plasma torch, a microwave coupled surface wave source, a DC coupled plasma source, a DC coupled arc source, or a pulsed DC plasma source. In some cases, the energy source 120 can be configured as a microwave coupled plasma torch that can operate at a pressure between 1 mTorr and 760 Torr. In addition, the microwave coupled plasma torch can be positioned along one or more sides of the fluidized bed reactor (e.g., next to the coil 122) or adjacent to a gas feed source. The microwave coupled plasma torch can be configured to provide a large amount of additional, for example, a plasma phase mixture (not shown for simplicity). Figure 1 10 (shown in FIG. 10 ) is dispersed into the interior of the fluidized bed reactor 110. In this way, a large additional amount of the plasma phase mixture can energetically excite one or more of the gas phase mixture, the plasma phase mixture, or the carbon nanoparticles 118, for example, as may be associated with post-processing. In some cases, the interior of the fluidized bed reactor 110 may retain one or more of the gas phase mixture or the plasma phase mixture. Furthermore, in some embodiments, the inductively coupled plasma source may be formed as a coil 122 surrounding the fluidized bed reactor.
[0046] In some aspects, the energy source 120 may be positioned at one or more locations relative to the intake valve 134 (not shown for simplicity). Figure 1 14) and / or may be located remote from the fluidized bed reactor 110. In some other aspects, the energy source 120 may be located at one or more locations including one of the following: downstream of the inlet valve 134, upstream of the fluidized bed region 114, adjacent to the fluidized bed region 114, or downstream of the fluidized bed region 114. In one embodiment, the energy source 120 may be coupled to the fluidized bed reactor 110. In this way, the energy source may electromagnetically excite the gas phase mixture and produce a plasma phase mixture. In some aspects, the plasma phase mixture may be formed in a plasma region (not shown in FIG. 14 for simplicity). Figure 1 ), the plasma region is located adjacent to or within the interior 112 of the fluidized bed reactor 110. The plasma region may be characterized by one or more of gas temperature, electron temperature and velocity, or fluid flow rate.
[0047] In some cases, vacuum pump 198 may be coupled to fluidized bed reactor 110 and thereby control the formation of fluidized bed region 114. Vacuum pump 198 may be coupled to fluidized bed reactor 110 and thereby control the formation of fluidized bed region 114. Figure 1 1 is shown coupled to a plasma feed source 140, but other layouts and / or configurations are possible. Figure 1In the exemplary configuration shown, the vacuum pump 198 can regulate the flow of an additional amount of plasma-based material contained within the plasma feed source 140 and flowing into the top section 180 of the fluidized bed reactor 110 via the plasma feed line 142. In one or more alternative configurations, the vacuum pump 198 can be coupled to the energy source 120, the gas feed source 130, and / or the pressure control assembly 150 to cooperate with the inlet valve 134 and / or the gas feed line 132 to regulate the flow of plasma and / or gaseous material into the interior of the fluidized bed reactor 110. For example, in one embodiment, the vacuum pump 198 and / or the energy source 120 can control the energy properties of the plasma phase mixture within the fluidized bed reactor 110. In some aspects, the energy source 120 can generate the plasma phase mixture as one or more of a thermal equilibrium plasma phase mixture or a non-thermal equilibrium plasma phase mixture. In addition, the control knob 199 can be coupled to the fluidized bed reactor 110. In this way, the control knob 199 can set the thermal equilibrium setting of the plasma phase mixture. For example, the thermal equilibrium setting can produce a thermal equilibrium plasma phase mixture or a non-thermal equilibrium plasma phase mixture. In addition, the thermal equilibrium setting can control the energy properties associated with one or more of the plasma phase mixture or the gas phase mixture. For example, in some cases, the energy properties may include the energy transfer rate between the plasma phase mixture and the gas phase mixture. In some other cases, the energy properties may include plasma-material interactions based on the interaction between the plasma phase mixture and the carbon nanoparticles 118.
[0048] In some cases, the energy management device 170 may be located remote from the fluidized bed reactor 110. The energy management device 170 may include a power source 172 and a matching network 174. The power source 172 may provide power to the energy source 120. The matching network 174 may use the energy source 120 to energetically excite the gas phase mixture. In addition, the side port (for simplicity in FIG. 1 ) may be configured to provide a power source 172 and a matching network 174. Figure 1 In some cases, the fluidized bed region may be associated with a fluidized bed architecture, which may thereby control the residence time associated with the operation of the power source and the matching network. In general, a fluidized bed architecture may mean a physical phenomenon that occurs when a solid particulate material (typically present in a holding container) is placed under specific conditions so that it behaves like a fluid. A fluidized bed (e.g., fluidized bed region 114) may be achieved by pumping a pressurized fluid into the particles (e.g., carbon nanoparticles). The resulting medium may have the properties and characteristics of an ordinary fluid, such as the ability to flow freely under gravity, or the ability to be pumped using fluid technology.
[0049] In this way, the fluidized bed reactor 110 can modify the particle morphology of one or more carbon nanoparticles, modify the crystal structure of one or more carbon nanoparticles, and chemically change one or more exposed surfaces of at least one carbon nanoparticle. In addition, the fluidized bed reactor 110 can deposit one or more materials on one or more exposed surfaces of at least one carbon nanoparticle. In addition, in some aspects, the fluidized bed reactor 110 can be associated with the performance of one of post-processing by reactive ion etching, heteroatom doping of at least some of the carbon nanoparticles, and / or carbon-on-carbon growth on at least some of the carbon nanoparticles. In some other aspects, the fluidized bed reactor 110 can be associated with the performance of one of plasma activation of at least some of the carbon nanoparticles, metal decoration of at least some of the carbon nanoparticles, and plasma-based etching of at least some of the carbon nanoparticles. In addition, the fluidized bed reactor 110 can be associated with the formation and growth of carbides on at least some of the carbon nanoparticles, the removal of at least some of the carbon nanoparticles from sp 2 Relative to sp 3 The fluidized bed reactor 110 is associated with performing one of a carbon phase change of the phase or a carbon-on-carbon grafting of at least some of the carbon nanoparticles. In this way, the fluidized bed reactor 110 can homogenize at least some of the carbon nanoparticles in powder form.
[0050] Figure 2A According to some embodiments Figure 1 An exemplary configuration 200A of a fluidized bed reactor 110 is depicted. Exemplary configuration 200A may be referred to as an "adjacent plasma". In some cases, a plasma feed gas 210 may be supplied to a plasma applicator 220 positioned adjacent to a fluidized bed reactor section 240, which may be a Figure 1 1. An example of a fluidized bed reactor 110 is depicted. In this manner, the plasma applicator can inject the plasma volume 230A into the fluidized bed region 260 positioned above the gas-solid separator 216 and thereby generate a gas chemical zone 250 extending longitudinally along the fluidized bed reactor section 240. The fluidizing gas 270 can flow into the fluidized bed reactor section 240 and contact one or more of the plasma volume 230A, the gas chemical zone 250, and / or the fluidized bed region 260. For example, at least some of the fluidizing gas 270 can at least partially cause the fluidized bed reactor section 240 to flow into the fluidized bed reactor section 240. Figure 1 The carbon nanoparticles 118 (not shown for simplicity) Figure 2A 2 (shown in FIG. 2 ), and allowing the plasma volume 230A to contact the carbon nanoparticles 118 suspended within the fluidized bed region 260. In this way, by tuning the layout and / or orientation of the plasma volume 230 as it enters the fluidized bed region 260, the carbon nanoparticles 118 can be post-processed in one or more specific listed methods (e.g., carbon-on-carbon growth, etc.).
[0051] Figure 2B According to some embodiments Figure 1 Another exemplary configuration 200B of the fluidized bed reactor 110 is depicted. Exemplary configuration 200A may be referred to as a "remote plasma". Configuration 200B may be Figure 2A 200A, except for the positioning of the plasma volume 230B. Instead of entering the fluidized bed region 260, the plasma volume 230 can be positioned adjacent to the fluidized bed reactor section 240 to post-process the material suspended within the fluidized bed region 260 accordingly.
[0052] Figure 3 According to some embodiments Figure 1 Another exemplary configuration 300 of a fluidized bed reactor 110 is depicted. Exemplary configuration 300 may be referred to as a "direct plasma". Configuration 300 may include a fluidized bed reactor section 340, which may be Figure 1 1. The fluidized bed reactor 110 of FIG. 1 is an example of a fluidized bed reactor 110 of FIG. 1. The fluidized bed reactor section 340 may be flanked by plasma applicators 350 on multiple sides of the fluidized bed reactor section 340. In this way, the plasma applicators 350 may energize the fluidizing gas and plasma feed 370 fed into the fluidized bed region 260 of the fluidized bed reactor section 240 and generate a plasma zone 330 and / or a gas chemical zone 375, such as Figure 3 Additionally, at least some of the fluidizing gas and plasma feed 370 can escape via a gas outlet 372 positioned opposite the inlet for the fluidizing gas and plasma feed 370 .
[0053] Figure 4 According to some embodiments Figure 1 Another exemplary configuration 400 of the fluidized bed reactor 110 is depicted. The configuration 400 may be Figure 3 4. The configuration 400 is an example of a configuration 300 of the embodiment of the present invention, except that the plasma zone 430 can be generated below the semi-molten region 410. In this manner, the exemplary configuration 400 can be referred to as a "remote plasma below the semi-molten region". In some cases, the semi-molten region 410 can be suitable for forming one or more compositions (including ceramic compositions) that can be melted, quenched and / or granulated, as well as mixing substances provided by the fluidizing gas and the plasma feed 470. In this manner, the configuration 400 can produce a fluidized bed region 460 suitable for quenching the carbon nanoparticles 118 ( Figure 4 Gas chemical zone 475 for post-processing (not shown).
[0054] Figure 5 According to some embodiments Figure 1Another exemplary configuration 500 of the fluidized bed reactor 110 is depicted. The configuration 500 may be Figure 4 5. The configuration 500 is an example of a configuration 400, except that the plasma zone 530 can be generated above the gas-solid region 510. In addition, the configuration 500 can include a plasma applicator 550 flanking the fluidized bed reactor section 540 to generate the plasma zone 530 above the fluidized bed region 560 and a gas chemical zone 575 extending away from the plasma zone 530 toward the gas outlet 572.
[0055] Figure 6 According to some embodiments Figure 1 An exemplary recirculating bed configuration 600 of a fluidized bed reactor 110 is depicted. In some cases, the configuration 600 may be Figure 1 600 can include a recirculation section 610 that can extend outwardly from the main section 605. In this way, carbon nanoparticles can be suspended within the configuration 600 and travel in the fluidization direction 660 into the recirculation section 610. There, the carbon nanoparticles can be energetically excited by the plasma applicator 650 to return to the main section and float above the gas-solid separator 616 to be optionally recycled to the recirculation section 610.
[0056] Figure 7 An exemplary reactor 700 according to some embodiments is shown. In some cases, the reactor 700 may be Figure 1 700 is an example of a fluidized bed reactor 110. In addition, or in an alternative, the reactor 700 may be implemented as a plasma torch. The reactor 700 may include a microwave energy source 710, an input gas inlet 715, a reaction vessel 720, an electric potential source 730, and a metal substrate 740. The reaction vessel 720 may include a reaction chamber 722, a downstream region 724, and a collector 726. The reaction chamber 722 has a length L along a direction 702 parallel to the reaction chamber 722. The input gas inlet 715 is connected between the reaction vessel 720 and a process material source (not shown for simplicity) and can be used to flow or otherwise provide a material 705 (e.g., one or more gases, liquids, particles, etc.) into the reaction chamber 722. For example, in some cases, the material 705 may include various structured carbons, such as (but not limited to) CNTs, fullerenes, etc.
[0057] The microwave energy source 710 may generate microwave energy 712, which may excite the material 705 to generate a plasma from which carbon-based free radicals may be separated or extracted. In some cases, the microwave energy source 710 may generate pulsed microwave energy, for example, as described in co-owned U.S. Patent Nos. 9,767,992 and 10,314,512. In other cases, the microwave energy source 710 may generate continuous microwave energy. The microwave energy source 710 may include a control circuit system that may adjust various characteristics of the microwave energy 712 based on one or more control signals (CTRL). For example, the CTRL signal may determine one or more of a pulse duration, a pulse frequency, a duty cycle, an instantaneous power level, or an average power level of the microwave energy 712. In this manner, the reactor 700 can configure the size, number of graphene layers, and concentration of few-layer graphene (FLG) nanosheets to be formed, for example, in the substrate 750 by adjusting the pulse duration, pulse frequency, duty cycle, instantaneous power level, and / or average power level of the microwave energy 712 generated to produce the non-thermal equilibrium plasma in the reaction chamber 722. The ability to control the energy applied to the non-thermal equilibrium plasma allows targeted reactions to occur and promotes the distribution of FLG nanosheets and other particles throughout the substrate 750.
[0058] In some embodiments, a mixture of hydrocarbon gas and silane may be flowed into the reaction chamber 722 via the input gas inlet 715 at a suitable flow rate. The hydrocarbon gas may be any suitable carbon-containing gas, such as, but not limited to, methane gas. The silane may be any suitable silane gas or a liquid precursor containing silane. In some aspects, the silane may be flowed into the reaction chamber 722 at a flow rate between about 1 standard liter per minute (slm) and 10 slm per minute. In some aspects, an additive may be provided to the reaction chamber 722, for example, while the mixture is flowing into the reaction chamber 722. In some cases, the additive may include an alkali metal (e.g., lithium, sodium, potassium, calcium, fluorine, or bromine), a transition metal (e.g., copper or iron), or any combination thereof. In other cases, the additive may include lithium, nickel, manganese, copper, trimethylaluminum (TMA), trimethylgallium (TMG), sulfur, or any combination thereof. The additive may be flowed into the reactor at a flow rate between about 1% and 75% of the flow rate of the hydrocarbon gas.
[0059] The microwave energy 712 generated by the microwave energy source 710 can be directed to the portion of the reaction chamber 722 containing the mixture of hydrocarbon gas and silane. The microwave energy 712, which can have a power level between about 300 watts (W) and 25 kilowatts (kW), can excite the mixture of hydrocarbon gas and silane to produce a non-thermal equilibrium plasma. In some aspects, the microwave energy source 710 can be a klystron or a traveling wave tube amplifier (TWTA). The non-thermal equilibrium plasma can include carbon-based radicals (e.g., methyl radicals), positively charged particles, ionized inert gas particles, or any combination thereof. In various embodiments, the carbon-based radicals, positively charged particles, and / or ionized inert gas particles 760 output from the reaction chamber 722 via the collector 726 can be directed toward the surface-air interface of the substrate 750 via bombardment and / or implantation. The substrate 750 may be bombarded with carbon-based radicals, positively charged particles, and / or ionized noble gas particles to form, strengthen, and / or reinforce one or more portions of the substrate 750. Portions of the substrate 750 formed, strengthened, or reinforced according to the techniques disclosed herein may have increased compressive strength, increased tensile strength, and increased fracture toughness, and thus be more resilient to cracking and surface defects than conventional substrates (e.g., glass materials).
[0060] More specifically, the surface-air interface of the substrate 750 may be bombarded with carbon-based radicals and ionized inert gas particles separated from the non-thermal equilibrium plasma in the reaction chamber 722. The ionized inert gas particles may penetrate the surface-air interface of the substrate 750 and form microcracks, microvoids, and / or surface defects in a portion of the substrate 750 located below the surface-air interface. In some aspects, the microcracks, microvoids, and / or surface defects formed by the ion bombardment of the substrate 750 may define an interphase region of the substrate 750. The carbon-based radicals that penetrate the surface-air interface of the substrate 750 may be implanted in the interphase region.
[0061] In some embodiments, an external electric field can be applied to the reaction chamber 722 to accelerate positively charged particles through the reaction chamber 722 toward the substrate 750 in the direction 704, thereby increasing the speed and energy at which the positively charged particles can impact the surface-air interface of the substrate 750. For example, the potential source 730 can generate a negative electric field or potential that can accelerate positively charged particles in the direction 704 toward the substrate 750 located on the metal substrate 740. In some aspects, the negative potential generated by the potential source 730 can be configured to extract or separate positively charged gas particles from the non-thermal equilibrium plasma based on the electrical polarity. In this way, the negative electric field or potential can allow positively charged particles, as well as ionized noble gas particles and carbon-based radicals, to penetrate deeper into the interphase region of the substrate 750.
[0062] In various embodiments, the reactor 700 can be cylindrical with a diameter of up to 1 inch. In some embodiments, the reactor 700 can be configured as a Gaussian reactor, while in other embodiments, the reactor 700 can be configured as a non-Gaussian reactor (e.g., where plasmas produced in non-Gaussian reactors generally exhibit better energy dissipation and distribution than plasmas produced in Gaussian reactors).
[0063] Figure 8 Another exemplary reactor 800 is shown, which may be Figure 7 The reactor 700 and / or Figure 1 The reactor 800 may be similar in some aspects to the fluidized bed reactor 110 of FIG. Figure 7 The reactor 700 of FIG. 1 and may differ from the reactor 700 of FIG. Figure 7 Reactor 700. For example, reactor 800 may include microwave energy source 710, input gas inlet 715, reaction chamber 820, potential source 830, metal substrate 740, and collector 726. One aspect in which reactor 800 differs from reactor 700 is that, rather than having potential source 730 that generates an electric field within one or more portions of reaction chamber 820, reactor 800 includes a plurality of electrodes 828 positioned on opposite sides of one or more portions of reaction chamber 820. Electrodes 828 may be configured to generate an internal electric field (e.g., based on a current and / or voltage provided by a power supply) that can accelerate a plurality of positively charged particles. In addition, or in the alternative, reactor 800 may also include an additional potential source (not shown for simplicity) positioned such that a negative potential appears across reaction chamber 822 in direction 804 and induces a current 832 along the interior-facing wall of reaction chamber 822. The current 832 induced within the reaction chamber 822 can generate a magnetic field that can attract and accelerate at least positively charged gas particles through the reaction chamber 822 and out of the collector 726 toward the substrate 750 .
[0064] In addition to the methane gas applied to reactor 700 and reactor 800 to generate carbon-based radicals, the carbon-containing precursor may include any known carbon particles or structures, such as those disclosed in ISO / TS 80004-13:2017 (en), entitled "Nanotechnologi es—Vocabulary—Part 13: Graphene and related two-dimensional (2D) materials."
[0065] In some aspects, the hydrocarbon gas flowing into the reactor 800 may be a short-chain hydrocarbon gas, while in other aspects, the hydrocarbon gas flowing into the reactor 800 may be a long-chain hydrocarbon gas. Specifically, the hydrocarbon gas may include methane (CH4) and / or butane (C4H 10 In various embodiments, the generation of suitable carbon-based radicals from a non-thermal equilibrium plasma may be based on one or more of the following:
[0066] The input carbon-containing gas flow rate is 100 standard cubic centimeters per minute (sccm) to 5 standard liters per minute (slm);
[0067] Lower flow rates generally provide enhanced fidelity and tunability, and thus may be advantageous in accelerating the carbon-based species through reaction chambers 722 and 810, which may result in lower additive doping rates;
[0068] Higher flow rates generally result in higher output but can reduce the fidelity and / or directionality of the FLG nanosheets;
[0069] • Silane and / or silane-containing liquid precursors, such as hexamethyldisiloxane (HMDSO) or hexamethyldisilazane (HMDSN), as well as pure silane may be flowed into reactors 700 and 800 to provide various suitable silicon source rates. In some embodiments, the silicon source rate may be one of 1 L / min to 10 L / min, 11 L / min to 20 L / min, 21 L / min to 30 L / min, 31 L / min to 40 L / min, 41 L / min to 50 L / min, 51 L / min to 60 L / min, 61 L / min to 70 L / min, 71 L / min to 80 L / min, 81 L / min to 90 L / min, 91 L / min to 100 L / min, 101 L / min to 200 L / min, or 201 L / min to 530 L / min, wherein higher flow rates may allow additional coating of the corresponding additive material on the accelerated ionized particles 716 and 816;
[0070] A gaseous substance containing lithium (Li), nickel (Ni), manganese (Mn), copper (Cu), trimethylaluminum (TMA), trimethylgallium (TMG), and sulfur (S) may be flowed into the reactors 700 and 800 to provide a silicon source rate of one of 1 to 10 liters / minute, 11 to 20 liters / minute, 21 to 30 liters / minute, 31 to 40 liters / minute, 41 to 50 liters / minute, 51 to 60 liters / minute, 61 to 70 liters / minute, 71 to 80 liters / minute, 81 to 90 liters / minute, 91 to 100 liters / minute, 101 to 200 liters / minute, or 201 to 530 liters / minute, wherein a higher flow rate may allow for a thicker coating of the additive on the FLG nanosheets;
[0071] The additive including silica may be flowed into the reactors 700 and 800 and / or dispersed in the form of particles at a rate of about 1% to 75% of the flow rate of the methane gas;
[0072] Additives may be configured to coat and / or decorate the accelerated ionized particles 760; and
[0073] • A preferred chemistry for substrate 750 may include between about 0.1% to 5% additives and between about 65% to 99% silicon dioxide, with the remainder attributed to carbon-containing materials (eg, FLG nanosheets).
[0074] Fig. 9 An exemplary FLG nanosheet 900 according to some embodiments is shown. The FLG nanosheet 900 may be made of Figure 1 The FLG nanosheets 900 may be produced and / or post-processed in the fluidized bed reactor 110 to produce, for example, the post-processed particles 160. For example, the FLG nanosheets 900 may be agglomerated with additional instances of the FLG nanosheets 900 to produce one or more of the post-processed particles 160. In some cases, the FLG nanosheets 900 may have a wrinkled or corrugated structure in which groups of carbon-carbon bonded atoms may bend or fold in response to an external force, pressure, or load.
[0075] for Fig. 9 In the example of FIG. 1 , the FLG nanosheet 900 is shown as including four graphene layers 901 to 904 stacked (e.g., vertically or substantially vertically) on top of each other. In other embodiments, the FLG nanosheet 900 may include other numbers of graphene layers. The number of graphene layers in the FLG nanosheet 900 may affect one or more properties of the FLG nanosheet 900. These properties may include (but are not limited to) the ability to absorb or dissipate energy, the ability to conduct electricity, and the ability to self-heal cracks formed in one or more materials.
[0076] Fig.10 1000 shows a micrograph of a graphene material 1005 produced by sulfuric acid (H2SO4) exfoliation from graphite, according to some embodiments. In some aspects, at least some of the graphene material 1005 coalesces with one or more additional instances of the graphene material 1005 and produces Figure 1 At least some of the depicted carbon nanoparticles 118 and / or post-treated particles 160. In some other aspects, the shape and / or morphology of at least some of the graphene materials 1005 is a flat nanosheet and / or resembles a flat nanosheet. In addition, at least some of the graphene materials 1005 may have a "wavy" or "wrinkled" morphology 1010, which may indicate that at least some of the flat nanosheets are adjacent at one or more defined angles (rather than straight, flat, or 180° angles), which may result in a relatively higher ratio of surface area per unit volume to volume than non-wavy or non-wrinkled graphene materials.
[0077] Fig.11 A micrograph 1100 of microwave-powered wavy and / or wrinkled graphene 1105 is shown, according to some embodiments. In some cases, at least some of the microwave-powered wavy and / or wrinkled graphene 1105 may coalesce with one or more additional instances of itself to produce Figure 1 At least some of the depicted carbon nanoparticles 118 and / or post-treated particles 160. In addition, at least some of the wavy and / or wrinkled graphene 1105 based on microwave energy may be Fig.10 In some aspects, at least some of the graphene nanosheets of the microwave energy-based wavy and / or wrinkled graphene 1105 can be abutted together to define various ridges and valleys 1115. In this way, at least some of the ridges and valleys 1115 can create regions of increased flexibility within the microwave energy-based wavy and / or wrinkled graphene 1105, which can be suitable for infiltration by, for example, a polymeric substance (e.g., PPgMA, etc.). In some aspects, sp 3 Hybrid polymer chains (e.g., polyethylene PE) can exhibit relative sp 2 -C chain conjugated polymers (eg, poly(p-phenylene)) have increased flexibility.
[0078] Fig.12 A micrograph of exemplary carbon particles 1205 is shown according to some embodiments. In some aspects, at least some of the carbon particles 1205 can each be Figure 1 An example of one or more of the carbon nanoparticles 118 and / or post-treated particles 160 depicted. In addition, at least some of the carbon particles 1205 may be Fig.10 Graphene material 1005 and / or Fig.11 The carbon particles 1205 may be separated from each other by a first plurality of pores 1210 formed between adjacent instances of the carbon particles 1205. Fig.12 As shown, each of the carbon particles 1205 can be a porous structure containing an additional plurality of pores (e.g., including a second plurality of pores 1220) created by overlapping secondary carbon particles 1215. In various embodiments, the average size of the first plurality of pores 1210 can be greater than the average size of the second plurality of pores 1220.
[0079] Fig.13A According to some embodiments Fig.12 Figure 1300A shows an example of a carbon particle (e.g., a three-region particle). In various embodiments, the three-region particle 1300A can be Figure 1 An example of one or more of the carbon nanoparticles 118 and / or post-treated particles 160 depicted. The three-region particle 1300A may include three discrete regions, such as, but not limited to, a first region 1301, a second region 1302, and a third region 1303. In some aspects, each of the regions 1301-1303 surrounds and / or encapsulates the previous region. For example, the first region 1301 may be surrounded or encapsulated by the second region 1302, and the second region 1302 may be surrounded or encapsulated by the third region 1303. The first region 1301 may correspond to an interior region of the three-region particle 1300A, the second region 1302 may correspond to an intermediate transition region of the three-region particle 1300A, and the third region 1303 may correspond to an exterior region of the three-region particle 1300A. In some aspects, the three-region particle 1300A may include a permeable shell 1305 that deforms in response to contact with one or more adjacent non-three-region particles and / or the three-region particle 1300A.
[0080] In some embodiments, the first region 1301 may have a relatively low density, a relatively low conductivity, and a relatively high porosity, the second region 1302 may have a medium density, a medium conductivity, and a medium porosity, and the third region 1303 may have a relatively high density, a relatively high conductivity, and a relatively low porosity. In some aspects, the first region 1301 may have a carbon material density between about 1.5 g / cc and 5.0 g / cc, the second region 1302 may have a carbon material density between about 0.5 g / cc and 3.0 g / cc, and the third region 1303 may have a carbon material density between about 0.0 g / cc and 1.5 g / cc. In other aspects, the first region 1301 may include pores having a width between about 0 nm and 40 nm, the second region 1302 may include pores having a width between about 0 nm and 35 nm, and the third region 1303 may include pores having a width between about 0 nm and 30 nm. In some other embodiments, the second region 1302 may not be defined for the three-region particle 500A. In one embodiment, the first region 1301 may have a major dimension D1 between approximately 0 nm and 100 nm, the second region 1302 may have a major dimension D2 between approximately 20 nm and 150 nm, and the third region 1303 may have a major dimension D3 of approximately 200 nm.
[0081] Aspects of the present disclosure recognize that the unique layout of the three-region particle 1300A and the relative sizes, porosities, and conductivity of the first region 1301, the second region 1302, and the third region 1303 can be selected and / or modified to achieve a desired balance between minimizing the polysulfide shuttling effect and maximizing the specific capacity of the host battery. Specifically, in some aspects, the size and volume of the pores can decrease from one region to another. In some embodiments, the three-region particle can be composed entirely of one region with a range of pore sizes and pore distributions (e.g., pore densities). For Fig. 13B In the example, pores 1311 associated with the first zone 1301 or the first porosity region have a relatively large width and can be defined as macropores, pores 1312 associated with the second zone 1302 or the second porosity region have a medium-sized width and can be defined as mesopores, and pores 1313 associated with the third zone 1303 or the third porosity region have a relatively small width and can be defined as micropores.
[0082] A group of three-region particles 1300A may be joined together to form an aggregate (not shown for simplicity), and a group of aggregates may be joined together to form an agglomerate (not shown for simplicity). In some embodiments, a plurality of mesopores may be dispersed throughout the aggregates formed by the respective group of three-region particles 1300A. In some aspects, the first porosity region 1311 may be at least partially encapsulated by the second porosity region 1312, such that the respective aggregates may include one or more mesopores and one or more macropores. In one embodiment, each mesopore may have a major dimension between 3.3 nanometers (nm) and 19.3 nm, and each macropore may have a major dimension between 0.1 μm and 1,000 μm. In some cases, the three-region particles 1300A may include carbon fragments that are entangled with each other and separated from each other by at least some of the mesopores.
[0083] In some embodiments, the three-region particle 1300A may include a surfactant or polymer that can act as a binder to join a group of carbon materials together, including one or more of styrene butadiene rubber, polyvinylidene fluoride, polyacrylic acid, carboxymethyl cellulose, polyvinyl pyrrolidone, and / or polyvinyl acetate. In other embodiments, the three-region particle 1300A may include a gel-phase electrolyte or a solid-phase electrolyte disposed within at least some of the pores.
[0084] In some embodiments, the three-region particle 1300A may have a 2 / g to 3,000m 2 The surface area of the exposed carbon surface is approximately in the range of 10 m / g and / or 2 / g to 3,000m 2 In one embodiment, the composition of matter including the plurality of three-region particles 1300A may have a conductivity in the approximate range of between 100 S / m and 20,000 S / m at a pressure of 12,000 pounds per square inch (psi) and a sulfur-to-carbon weight ratio of between about 1:5 and 10:1.
[0085] Fig. 13B shows a representation according to some embodiments Fig.13AAn exemplary step function for a three-zone particle. As discussed, pores distributed throughout the three-zone particle 1300A may have different sizes, volumes, or distributions. In some embodiments, the average pore volume may decrease based on the distance between the center of the three-zone particle 1300A and an adjacent zone, for example, such that pores associated with the first zone 1301 or first porosity region have a relatively large volume or pore size, pores associated with the second zone 1302 or second porosity region have a medium volume, and pores associated with the third zone 1303 or third porosity region have a relatively small volume. The interior region has a higher pore volume than the region near the periphery. Regions with higher pore volumes provide high sulfur loading, while outer regions of lower pore volume mitigate polysulfide migration during battery cycling. Figure 8 In the example of C, the average pore volume in the inner region is about 3 cc / g The average pore volume in the outermost region is about 0.5 cc / g , and the average pore volume in the middle region is 0.5 cc / g with 3 cc / g between.
[0086] Fig.14 A graph 1400 depicting an exemplary distribution of pore volume versus pore width for exemplary carbon particles according to some embodiments is shown. In some cases, the exemplary carbon particles may be Figure 1 One of the depicted carbon nanoparticles 118 and / or post-treated particles 160. As depicted in graph 1400, pores associated with relatively high pore volumes can have relatively low pore widths, for example, such that the pore width generally increases with decreasing pore volume. In some aspects, pores having a pore width of less than about 1.0 nm can be referred to as micropores, pores having a pore width between about 3 nm and 11 nm can be referred to as mesopores, and pores having a pore width greater than about 24 nm can be referred to as macropores.
[0087] Fig.15A According to some embodiments Fig.12 and / or Fig.13A Photomicrographs of exemplary carbon particles, aggregates and / or agglomerates depicted. In some aspects, Fig.15A The carbon particles depicted may be Figure 1An example of the carbon nanoparticles 118 and / or post-treated particles 160 depicted. In some embodiments, each of the carbon structures 1502 may have a substantially hollow core region surrounded by various overall carbon growths and / or stratifications. In some aspects, the overall carbon growths and / or stratifications may be examples of various carbon structures, growths and / or stratifications. In some cases, the carbon structure 1502 may include several concentric multilayer fullerenes and / or carbon structures of similar shape organized at different densities and / or concentration levels. For example, the actual final shape, size, and graphene configuration of each of the carbon structures 1502 may depend on various manufacturing processes. In some aspects, the carbon structure 1502 may exhibit poor water solubility. Therefore, in some embodiments, non-covalent functionalization may be used to change one or more dispersibility properties of the carbon structure 1502 without affecting the inherent properties of the basic carbon nanomaterial. In some aspects, the basic carbon nanomaterial may be a shaped sp 2 In some embodiments, each of the carbon structures 1502 may have a diameter between approximately 20 nm and 500 nm. In various embodiments, multiple groups of carbon structures 1502 may coalesce and / or join together to form aggregates 1504. Additionally, multiple groups of aggregates 1504 may coalesce and / or join together to form agglomerates 1506. In some aspects, one or more of the carbon structures 1502, aggregates 1504, and / or agglomerates 1506 may be used to form Figure 1 One or more of the carbon nanoparticles 118 and / or post-treated particles 160 are depicted.
[0088] Fig. 15B A micrograph 1550 of aggregates formed from carbon material according to some embodiments is shown. In some embodiments, aggregates 1560 may be Fig.15A In one embodiment, the outer carbon shell structure 1552 can be fused together with carbon provided by other carbon shell structures 1554 to form a carbon structure 1556. A group of carbon structures 1556 can coalesce and / or bond with each other to form an aggregate 1560. In some aspects, the core region 1558 of each of the carbon structures 1556 can be tunable, for example, because the core region 1558 can include interconnected graphene structures and / or carbon particles at various defined concentration levels, as described in reference to Figure 5 A and / or Figure 5 B. In some embodiments, some of the carbon structures 1556 may have a first interconnected carbon concentration of approximately between 0.1 g / cc and 2.3 g / cc at or near the outer carbon shell structure 1552. Each of the carbon structures 1556 may have pores to transmit lithium cations (Li ions) extending inward toward the core region 1558. + ).
[0089] In some embodiments, the pores in each of the carbon structures 1556 may have a width or size between about 0.0 nm and 0.5 nm, between about 0.0 nm and 0.1 nm, between about 0.0 nm and 6.0 nm, or between about 0.0 nm and 35 nm. Each carbon structure 1556 may also have a second concentration at or near the core region 1558 that is different from the first concentration. For example, the second concentration may include a number of relatively low-density carbon regions in a concentric configuration. In one embodiment, the second concentration may be between about 0.0 g / cc and 1.0 g / cc or between about 1.0 g / cc and 1.5 g / cc lower than the first concentration. In some aspects, the relationship between the first concentration and the second concentration can be used to confine sulfur or polysulfide within the respective electrodes and allow lithium cations (Li + ) are present in a first concentration and at least temporarily confined within and / or dispersed throughout a second concentration.
[0090] In some embodiments, at least some of the carbon structures 1556 may include CNO oxides organized as a monolithic and / or interconnected growth and produced in a thermal reactor. For example, the carbon structures 1556 may be decorated with cobalt nanoparticles according to the following exemplary recipe: Cobalt (II) acetate (C4H6CoO4), a cobalt salt of acetic acid (often present as a tetrahydrate Co(CH3CO2)2·4H2O, which may be abbreviated as Co(Oac)2·4H2O) may be flowed into a thermal reactor at a ratio of approximately 59.60 wt % corresponding to 40.40 wt % carbon (relating to carbon in the form of CNO), resulting in the functionalization of active sites on the CNO oxide with cobalt, correspondingly showing a 15,000x level of cobalt decorated CNO. In some embodiments, a suitable gas mixture for producing carbon #29 and / or cobalt decorated CNO may include the following steps:
[0091] Ar purge, 0.75 standard cubic feet per minute (scfm), for 30 minutes;
[0092] Ar purge, changed to 0.25scfm, continuous operation;
[0093] Temperature increase: 25°C to 300°C, 20 minutes; and
[0094] Temperature increase: 300°C to 500°C, 15 minutes.
[0095] refer to Fig.15A and 15BThe carbon material described may include or be otherwise formed of one or more examples of graphene, which may include a monolayer of carbon atoms, each atom being bonded to three neighbors in a honeycomb structure. A monolayer may be a discontinuous material that is limited in one dimension, such as within or at a surface of a condensed phase. For example, graphene may grow outward only in the x and y planes (and not in the z plane). In this way, graphene may be a two-dimensional (2D) material comprising one or more layers, wherein the atoms in each layer are strongly bonded (e.g., by multiple carbon-carbon bonds) to neighboring atoms in the same layer.
[0096] In some embodiments, the graphene nanosheets (e.g., the shaped structures included in each of the carbon structures 1556) may include multiple instances of graphene, such as a first graphene layer, a second graphene layer, and a third graphene layer, all stacked on top of each other in a vertical direction. Each of the graphene nanosheets, which may be referred to as GNPs, may have a thickness between 1 nm and 3 nm, and may have a lateral dimension in the range of approximately 100 nm to 100 μm. In some embodiments, the graphene nanosheets may be produced by roll-to-roll ("R2R") production, by multiple plasma torches configured in sequence. In some aspects, R2R production may include deposition on a continuous substrate that is processed as a rolled sheet, including transferring one or more 2D materials to a separate substrate. In some cases, the plasma torches used in the described R2R process may spray different concentration levels of carbon material to produce graphene nanosheets at a specific concentration level. Thus, the R2R process may provide a fine level of tunability to produce Figure 1 Depicted carbon nanoparticles 118 and / or post-treated particles 160 and / or other carbon particles as described elsewhere in this disclosure.
[0097] Fig.16 FIG. 1 shows a diagram depicting a plurality of Fig.12 1600 of cumulative pore volume versus pore width for micropores and mesopores in carbon particles 1205 depicted in micrograph 1200 of FIG. As used herein, "Carbon 1" refers to a structured carbon material that includes primarily micropores (e.g., a major dimension less than 5 nm), and "Carbon 2" refers to a structured carbon material that includes primarily mesopores (e.g., a major dimension between about 20 nm and 50 nm). In some embodiments, an electrode suitable for use in one of the batteries disclosed herein can be prepared to have the pore size and pore distribution depicted in graph 1600.
[0098] Fig.17 According to some embodiments Fig.12 An exemplary configuration 1700 of exemplary carbon particles is depicted. In some embodiments, configuration 1700 may be Figure 1An example of one or more of the carbon nanoparticles 118 and / or post-treated particles 160 depicted. Configuration 1700 may be suitable for use in producing, for example, a carbon-based battery cathode, such as a carbon scaffold for incorporation into a lithium-sulfur battery. In one embodiment, configuration 1700 includes a first porous carbon region 1710 and a second porous carbon region 1720 positioned adjacent to the first porous carbon region 1710. The first porous carbon region 1710 may be formed of a carbon material at a first concentration level, and the second porous carbon region 1720 may be formed of a carbon material at a second concentration level that is different from the first concentration level of the carbon material. For example, the second porous carbon region 1720 may have a lower concentration level of carbon material than the first porous carbon region 1710, such as Fig.17 In some aspects, additional porous carbon regions (not shown for simplicity) Fig. 9 ) may be coupled to at least a second porous carbon region 1720.
[0099] Specifically, these additional porous carbon regions can be configured in an order of decreasing carbon material concentration levels in an incremental manner in a direction away from the first porous carbon region 1710 to provide full tunability. That is, in one embodiment, the second porous carbon region 1720 can face the desired region and the first porous carbon region 1710 of the configuration 1700 can be positioned according to customer specifications. In this way, denser carbon regions, such as the first porous carbon region 1710, can contribute to relatively low levels of species between adjacent contact points of carbon materials, while sparser carbon regions, such as the second porous carbon region 1720, can contribute to relatively high levels of species infiltration. In some embodiments, additional carbon regions coupled to and positioned adjacent to the second porous carbon region 1720 can have a lower carbon material density than the second porous carbon region 1720. In this way, the lower density additional carbon regions can accommodate higher levels of lithium ion transport to, for example, allow tuning of various performance characteristics of a composite material including the configuration 1700.
[0100] In one embodiment, first porous carbon region 1710 may include first non-three-region particles 1711. The configuration of first non-three-region particles 1711 within the first porous carbon region is an exemplary configuration. Other positions, orientations, arrangements, etc. are possible for non-three-region particles. In some aspects, each non-three-region particle may be an example of one or more carbon materials disclosed elsewhere in this disclosure. First porous carbon region 1710 may also include first three-region particles 1712, such as Fig.17 1711, or positioned in any other position, orientation, or configuration. Each first three-region particle 1712 may be Fig.13AIn addition or alternatively, each first three-region particle 1712 may include first carbon fragments 1713 that are entangled with each other and separated from each other by mesopores 1714. Each three-region particle may have a first deformable periphery 1715 configured to coalesce with adjacent first non-three-region particles 1711 and / or first three-region particles 1712.
[0101] The first porous carbon region 1710 may also include first aggregates 1716, wherein each aggregate includes a plurality of first third-region particles 1712 bonded together. In one or more specific instances, each first aggregate may have a major dimension in a range between 10 nanometers (nm) and 10 micrometers (μm). Mesopores 914 may be dispersed throughout the first plurality of aggregates, wherein each mesopore has a major dimension between 3.3 nanometers (nm) and 19.3 nm. In addition, the first porous carbon region 910 may include first agglomerates 917, wherein each agglomerate includes a plurality of first aggregates 916 bonded to each other. In some aspects, each first agglomerate 917 may have a major dimension in an approximate range between 0.1 μm and 1,000 μm. Macropores 918 may be dispersed throughout the first aggregate 916, wherein each macropore may have a major dimension between 0.1 μm and 1,000 μm. In some embodiments, one or more of the carbon materials, allotropes, and / or structures discussed above may be Fig.15A and Fig. 15B One or more instances of those shown.
[0102] The second porous carbon may include second non-three-region particles 1721, which may be an example of first non-three-region particles 1711. The second porous carbon region 1720 may include second three-region particles 1722, which may each be an example of each of the first three-region particles 1712 and / or may be Fig.13A In addition or alternatively, each second third region particle 1322 may include second carbon fragments 1323 that are entangled with each other and separated from each other by mesopores 1714. Each second third region particle 1722 may have a second deformable periphery 1725 configured to coalesce with one or more adjacent second non-third region particles 1721 or second third region particles 1722.
[0103] In addition, the second porous carbon region 1720 may include second aggregates 1726, wherein each second aggregate 1726 may include a plurality of second third region particles 1722 bonded together. In one or more specific examples, each second aggregate 1726 may have a major dimension in a range between 10 nanometers (nm) and 10 micrometers (μm). Mesopores 1714 may be dispersed throughout the second aggregate 1726, each mesopore having a major dimension between 3.3 nanometers (nm) and 19.3 nm. In addition, the second porous carbon region 1720 may include second agglomerates 1727, each second agglomerate 1727 may include a plurality of second aggregates 1726 bonded to each other, wherein each agglomerate may have a major dimension in an approximate range between 0.1 μm and 1,000 μm. Macropores 918 may be dispersed throughout the second plurality of aggregates, wherein each macropore has a major dimension between 0.1 μm and 1,000 μm. In some embodiments, one or more of the carbon materials, allotropes, and / or structures discussed above may be Fig.17 A and Fig.17 B shows one or more instances of those shown.
[0104] In one embodiment, the first porous carbon region 1710 and / or the second porous carbon region 1720 may include a selectively permeable shell (not shown for simplicity). Fig. 9 ), which may form a separated liquid phase on the first porous carbon region 910 or the second porous carbon region 1720, respectively. An electrolyte, such as any of the electrolytes disclosed in the present disclosure, may be dispersed within the first porous carbon region and / or the second porous carbon region to facilitate lithium ion transport associated with the discharge-charge operation cycle of the lithium-sulfur battery.
[0105] In one or more specific examples, the first porous carbon region 1710 can have an electrical conductivity in the approximate range of 500 S / m to 20,000 S / m at a pressure of 12,000 pounds per square inch (psi). The second porous carbon region 920 can have an electrical conductivity in the approximate range of 0 S / m to 500 S / m at a pressure of 12,000 pounds per square inch (psi). The first agglomerates 1717 and / or the second agglomerates 1727 can include aggregates connected to each other by one or more polymer-based binders.
[0106] In some aspects, each first third region particle 1712 can have a first porosity region (not shown for simplicity) located around the center of the first third region particle 1712. Fig.17 Similarly, each second third region particle 1722 may have a first porosity region (not shown for simplicity) located around the center of the second third region particle 99. Fig.17The first porosity region may include first pores. The second porosity region (not shown for simplicity) Fig.17 ) may surround a first porosity region. A second porosity region may include second pores. In one embodiment, the first pores may define a first pore density, and the second pores may define a second pore density different from the first pore density.
[0107] In some aspects, the mesopores 1714 can be grouped into first mesopores and second mesopores (neither of which is shown in the figure for simplicity). Fig.17 ). In one or more specific examples, the first mesopores may have a first mesopore density, and the second mesopores may have a second mesopore density different from the first mesopore density. In addition, the macropores 1718 may be grouped into first macropores that may have a first pore density, and second macropores that may have a second pore density different from the first pore density (both are not shown in FIG. 1 for simplicity). Fig.17 ).
[0108] Fig.18 An exemplary battery 1800 according to some embodiments is shown. In one embodiment, battery 1800 may be implemented as a lithium-sulfur battery and may include an anode 1820 (e.g., an anode active material including lithium foil), a cathode 1810, and a solid electrolyte 1830. In some cases, solid electrolyte 1830 may replace one or more of the electrolyte solution compositions presented in Examples 1 to 20. In some aspects, cathode 1810 may be loaded with 3 milligrams (mg) / cubic centimeter (cm 3 ) of elemental sulfur. In other aspects, cathode 1810 can be loaded with 3 milligrams (mg) / cubic centimeter (cm3) of sulfur suitable for maximizing the discharge-charge cycle efficiency of battery 1800. 3 ) other concentrations of elemental sulfur. In some aspects, cathode 1810 can be porous and comprise a composition of matter including a plurality of pores 1812 (not shown for simplicity). Fig.18 The composition of matter may be an example of various carbonaceous materials and / or structures disclosed herein.
[0109] The solid electrolyte 1830 may be dispersed in the pores 1812 of at least the entire cathode 1810, and may also be in contact with the anode 1820. In some aspects, the solid electrolyte 1830 may be formed as a membrane, and thus provide ion conductivity associated with the separator. In one embodiment, the solid electrolyte 1830 may be formed of and / or include a polymer matrix 1831, which may be formed of glass fibers 1833 interconnected with each other. In some aspects, the polymer matrix 1831 may have ionic conductivity (e.g., conduct lithium cations (Li +)) and may include between 8 weight percent (wt%) and 12 weight percent of polyethylene oxide (PEO) 1832, between 13 weight percent and 17 weight percent of polyvinyl difluoride (PVDF) 1834, between 3 weight percent and 7 weight percent of a polyvinyl difluoride (PVDF) 1834 having repeating oxypropylene units in its backbone (not shown for simplicity). Fig.18 ), and between 5 wt % and 10 wt % of one or more lithium-containing salts, the one or more lithium-containing salts comprising lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) or lithium iodide (LiI) (not shown for simplicity) Fig.18 In some embodiments, at least some of the lithium-containing salts may dissociate into lithium cations (Li + ) and thus facilitate lithium ion transfer between the anode 1820 and the cathode 1810 during the operational discharge-charge cycle of the battery 1800.
[0110] In some cases, during the operational discharge-charge cycle of the battery 1800, the battery 1800 may generate undesirable lithium-containing polysulfide species (not shown for simplicity). Fig.18 ). In some cases, cathode 1810 can at least partially entrap and / or retain lithium-containing polysulfide species, thereby preventing blockage of lithium transport channels (e.g., as shown as charging cycle flow 1825) within solid electrolyte 1830. In some aspects, anode 1820 can be formed to provide lithium cations (Li + ) of the lithium layer. In this way, during the discharge-charge cycle of operation of the battery 1800, the lithium layer can provide lithium cations (Li + ). In other aspects, during the operating charge cycle of the battery 1800, the cavity 1822 can receive lithium deposits from the cathode 1810. That is, the lithium cations (Li + ) can travel along the charge cycle flow 1824 from the cathode 1810 to the cavity 1822, as can be associated with the electrons 1874 that may be encountered or associated with the battery charge and / or recharge cycle back toward the battery 1800. In this way, the cavity 1822 can be transformed into the anode 1820, which can be capable of again transferring lithium cations (Li + ) are provided to the corresponding electrochemically favorable positions of the lithium cations in the cathode 1810.
[0111] In one embodiment, the composition of matter used to form cathode 1810 may be formed and / or include one or more non-three-region particles, three-region particles, aggregates or agglomerates as disclosed herein. In some aspects, each three-region particle used in cathode 1810 may include carbon fragments entangled with each other. At least some carbon fragments may be separated from each other by mesopores. A deformable periphery may be defined when one or more adjacent non-three-region particles or three-region particles are agglomerated. Each aggregate may include a plurality of three-region particles bonded together and having a major dimension in a range between 10 nanometers (nm) and 10 micrometers (μm). Mesopores may be dispersed throughout the aggregate. Each mesopore may have a major dimension between 3.3 nanometers (nm) and 19.3 nm. Each agglomerate may be formed by a plurality of aggregates bonded to each other and having a major dimension in an approximate range between 0.1 μm and 1,000 μm. Macropores may be dispersed throughout the aggregate, wherein each macropore has a major dimension between 0.1 μm and 1,000 μm.
[0112] In some embodiments, when formed and / or deposited as a film on anode 1820 (not shown for simplicity), Fig.18 ), the ionic conductivity of the solid electrolyte 1830 can be based on the relative concentration levels of one or more lithium-containing salts doped into the polymer matrix 1831. In this way, at a temperature between 18 degrees Celsius (° C.) and 22° C., the ionic conductivity of the solid electrolyte 1830 can be between 0.97×10 -3 Siemens / meter (S / m) and 1.03×10 -3 In other embodiments, the membrane can be coated onto the anode 1820 such that the ionic conductivity of the membrane is between 3.97×10 -6 Siemens / meter (S / m) and 4.03×10 -6 In some aspects, higher amounts of one or more lithium-containing salts can be associated with an increase in the ionic conductivity of the polymer matrix 1831 .
[0113] In one embodiment, solid electrolyte 1830 has a thickness between 10 micrometers (μm) and 50 μm when formed into a film, and may have a uniform density throughout its thickness. For example, in some cases, solid electrolyte 1830 may have a density of 2 grams per cubic centimeter (g / cm 3 ) and 3g / cm 3 In some aspects, the membrane can be coated onto a sacrificial polymer (not shown for simplicity). Fig.18), the sacrificial polymer may be disposed on the anode 1820 facing the solid electrolyte 1830. In this way, the solid electrolyte 1830 may prevent electrons from traveling from the anode 1820 to the cathode 1810 through the solid electrolyte 1830. In addition, the contact point between the solid electrolyte 1830 and the anode 1820 may prevent the impedance of the battery 1800 from increasing.
[0114] In one embodiment, cathode 1810 has a thickness between 50 micrometers (μm) and 150 μm, and a density of 5 grams per cubic centimeter (g / cm 3 ) and 15g / cm 3 In some aspects, the solid electrolyte 2360 can be prepared without a liquid electrolyte, such as Examples 1 to 20 disclosed herein. Additionally or alternatively, the solid electrolyte 1830 can confine lithium-containing polysulfide species within the cathode 1810 and / or prevent the growth of lithium-containing dendrite structures from the anode 1820. In some aspects, during the operating discharge-charge cycle of the battery 1800, the anode 1820 can expand in volume by between 5% and 20% of its initial size. In some cases, during the operating discharge-charge cycle of the battery 1800, the solid electrolyte 1830 can provide interfacial stability between the anode 1820 and the solid electrolyte 1830, for example to reduce or limit the volume expansion of the anode 1820.
[0115] As used herein, phrases referring to "at least one of" or "one or more of" a list of items refer to any combination of those items, including single members. For example, "at least one of a, b, or c" is intended to cover the following possibilities: only a, only b, only c, a combination of a and b, a combination of a and c, a combination of b and c, and a combination of a, b, and c.
[0116] The various illustrative components, logic, logic blocks, modules, circuits, operations, and algorithmic processes described in conjunction with the embodiments disclosed herein may be implemented as electronic hardware, firmware, software, or a combination of hardware, firmware, or software, including the structures disclosed in this specification and their structural equivalents. The interchangeability of hardware, firmware, and software has been generally described with respect to functionality and is shown in the various illustrative components, blocks, modules, circuits, and processes described above. Whether such functionality is implemented in hardware, firmware, or software depends on the application and the design constraints imposed on the overall system.
[0117] Those skilled in the art may readily appreciate various modifications to the embodiments described in the present disclosure, and the general principles defined herein may be applied to other embodiments without departing from the spirit or scope of the present disclosure. Therefore, the claims are not intended to be limited to the embodiments shown herein, but should be given the broadest scope consistent with the present disclosure, the principles disclosed herein, and the novel features.
[0118] In addition, various features described in this specification in the context of separate embodiments may also be implemented in combination in a single embodiment. Conversely, various features described in the context of a single embodiment may also be implemented separately in multiple embodiments or in any suitable subcombination. Thus, although features may be described above as being combined with each other, and even initially claimed as such, one or more features from a claimed combination may be removed from the combination in some cases, and a claimed combination may be directed to a subcombination or a variation of a subcombination.
[0119] Similarly, although the operation is depicted in a specific order in the drawings, this should not be understood as requiring to perform these operations in the specific order shown or in a sequential order, or requiring to perform all the operations shown to reach the desired result. In addition, the drawings can schematically depict one or more exemplary processes in the form of a flow chart (flowchart / flow diagram). However, other operations that are not depicted can be incorporated into the exemplary process shown schematically. For example, one or more additional operations can be performed before, after, simultaneously or between any one of the operations shown. In some cases, multitasking and parallel processing can be advantageous. In addition, the separation of various system components in the above-mentioned embodiments should not be understood as requiring such separation in all embodiments, and it should be understood that the described program components and systems can be integrated together or packaged into multiple products in a single product.
Claims
1. A system comprising a fluidized bed reactor, comprising: a gas feed source configured to flow a gas phase mixture into the interior of the fluidized bed reactor; an air inlet valve coupled to and in fluid communication with the gas feed source, the air inlet valve being configured to regulate a flow rate of the gas phase mixture entering the interior of the fluidized bed reactor; a gas-solid separator positioned in the fluidized bed reactor upstream of the gas inlet valve; an energy source configured to generate a plasma phase mixture in response to electromagnetic excitation of the gas phase mixture, the plasma phase mixture being formed in a plasma region adjacent to or within the interior of the fluidized bed reactor; a pressure control assembly configured to adjust one or more of a pressure or a velocity of at least some of the plurality of carbon nanoparticles loaded within the interior of the fluidized bed reactor; as well as An energy management device is outside the fluidized bed reactor, and is configured to control energy excitation of the gas phase mixture via the energy source.
2. The system of claim 1, wherein the fluidized bed reactor is formed as an elongated tube, the elongated tube comprising an outlet configured to output the gas phase mixture and one or more gases generated in conjunction with generating the plasma phase mixture.
3. The system of claim 1, wherein the energy source comprises a microwave coupled plasma torch configured to operate in a pulsed mode or a continuous mode.
4. The system of claim 3, wherein the microwave coupled plasma torch is configured to operate at a pressure between 1 millitorr (mTorr) and 760 Torr.
5. The system of claim 4, wherein the cross-sectional area of the fluidized bed reactor is one of rectangular, square, bell-shaped, circular, or elliptical.
6. The system of claim 3, wherein the microwave coupled plasma torch is positioned along one or more sides of the fluidized bed reactor.
7. The system of claim 3, wherein the microwave coupled plasma torch is configured to disperse an additional amount of the plasma phase mixture into the interior of the fluidized bed reactor, the additional amount of the plasma phase mixture being configured to energetically excite one or more of the gas phase mixture, the plasma phase mixture, or the plurality of carbon nanoparticles.
8. The system of claim 1, wherein the gas phase mixture is configured to prevent the carbon nanoparticles from escaping from the fluidized bed reactor.
9. The system of claim 1, further comprising: A side port is formed in the fluidized bed reactor, and the side port is configured to supply additional gas phase mixture into the fluidized bed reactor.
10. The system of claim 1, wherein the energy source is external to the fluidized bed reactor.
11. The system of claim 1, wherein the fluidized bed reactor is configured to modify a crystal structure of at least some of the carbon nanoparticles.
12. The system of claim 1, wherein the fluidized bed reactor is configured to chemically alter one or more exposed surfaces of at least some of the carbon nanoparticles.
13. The system of claim 1, wherein the energy source is configured to generate the plasma phase mixture in a thermal equilibrium state or a non-thermal equilibrium state in response to a control signal.
14. The system of claim 13, wherein the thermal equilibrium state is configured to control a plurality of energetic properties associated with one or more of the plasma phase mixture or the gas phase mixture.
15. The system of claim 14, wherein the plurality of energy properties includes a rate of energy transfer between the plasma phase mixture and the gas phase mixture.
16. The system of claim 1, wherein the fluidized bed reactor is configured to homogenize at least some of the plurality of carbon nanoparticles.
17. The system of claim 1, wherein the plurality of carbon nanoparticles comprises one or more non-hollow carbon sphere (NHCS) particles.
18. The system of claim 1, wherein the energy management device further comprises a matching network coupled to the energy source, the fluidized bed reactor being configured to control a residence time associated with the matching network.
19. The system of claim 18, wherein the plurality of carbon nanoparticles are carried in a powder that is pre-loaded into the interior of the fluidized bed reactor.