Stable liquid crosslinker composition for heat curable inks

By using a combination of TACT crosslinking agent, hydroxy functional polymer and non-volatile diluent in ink, the problem of solubility and stability of TACT crosslinking agent in high-speed offset printing ink is solved, and formaldehyde-free, thermally curable and Stable ink for hard surface printing.

CN118974184APending Publication Date: 2024-11-15INX INTERNATIONAL INK CO
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202280094001.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2022-03-03
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The TACT crosslinking agent is difficult to dissolve in thermally curable inks, resulting in poor printing characteristics during high-speed offset printing, and may lead to solid precipitation due to the evaporation of butanol, interfering with the printing process.

Method used

Using an ink carrier composition containing a TACT crosslinker, a hydroxy functional polymer and a nonvolatile diluent, a liquid crosslinker composition containing no butanol is formed by mixing and evaporating at least 98% of butanol to form a butanol-free liquid crosslinker composition for preparation The ink can be heat-cured to ensure stability at room temperature without crosslinking or precipitation.

Benefits of technology

Formaldehyde-free, heat-curable, printable ink is achieved, suitable for image printing on hard surfaces such as metal surfaces, maintaining long-term stability and avoiding solid precipitation and component layering.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118974184A_ABST
    Figure CN118974184A_ABST
Patent Text Reader

Abstract

The present disclosure provides an ink vehicle composition comprising a crosslinker compound of formula (I), a hydroxyl-functional polymer, and a non-volatile diluent wherein the composition is substantially free of butanol. Also provided are thermoset heat-curable inks comprising the ink carrier composition, and methods of printing on a surface of a substrate by applying the thermoset heat-curable inks. The ink carrier compositions and thermoset heat curable inks herein may be stable at room temperature for about 6 to about 24 months. # imgabs0 #
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to stable compositions containing 1,3,5-triazine carbamate (TACT) crosslinkers for use in high-speed offset printing, such as heat-curable inks, and methods for making the same. Background Art

[0002] TACT compounds are trifunctional melamine-type crosslinkers containing reactive carbamate functional groups. TACT crosslinkers are solid materials that need to be dissolved in a solvent. TACT crosslinkers are insoluble in polyether glycol-type solvents, and commercial TACT crosslinkers are typically provided as 50-52% n-butanol solutions. However, due to the boiling point of butanol, butanol solutions of TACT do not provide adequate printing properties for high-speed offset printing of thermosetting (heat-curable) ink formulations. In addition, the solid crosslinker may precipitate from the ink during storage due to evaporation of butanol, thereby interfering with the printing process.

[0003] To date, the use of TACT crosslinkers in heat-curable, high-speed offset inks (e.g., inks for printing images on metal surfaces) remains a technical challenge. TACT itself is insoluble in typical ink diluents due to its solubility parameters. Therefore, there remains a need for stable TACT crosslinker compositions for use in heat-curable high-speed offset inks that are expected to have comparable or better printing properties than existing formulations that do not use TACT as a curing agent. Summary of the invention

[0004] In one aspect, an ink carrier composition is disclosed, comprising a crosslinker compound of formula (I),

[0005]

[0006] Where R 1 , R 2 and R 3 Each is independently C 1-10 an alkyl group; a hydroxy-functional polymer; and a nonvolatile diluent, wherein the composition is substantially free of butanol.

[0007] In another aspect, disclosed is a method of preparing an ink carrier composition, the method comprising:

[0008] mixing a crosslinker compound of formula (I), a hydroxyl functional polymer, and a non-volatile diluent to form a mixture,

[0009]

[0010] Where R 1 , R 2 and R 3 Each is independently C 1-10an alkyl group, and wherein the crosslinker compound is dissolved in butanol; and

[0011] At least 98% of the butanol is evaporated from the mixture to provide the disclosed ink vehicle composition.

[0012] In another aspect, disclosed are thermosetting heat-curable inks comprising (a) the disclosed ink carrier composition; and (b) a colorant.

[0013] In another aspect, a method of printing ink onto a substrate is disclosed, the method comprising: applying the disclosed thermosetting heat-curable ink onto a surface of the substrate; and heating the applied thermosetting heat-curable ink to thereby cure the applied thermosetting heat-curable ink. DETAILED DESCRIPTION

[0014] The present disclosure provides a liquid crosslinker composition containing a TACT crosslinker compound. The liquid crosslinker composition is particularly suitable for preparing curable compositions such as high-solids coating compositions, overprint varnishes, printable inks and other related applications. In addition, the TACT crosslinker process does not release or generate formaldehyde. For heat-curable inks, the TACT crosslinker can be mixed with a hydroxyl-functional polymer and a non-volatile diluent to form a heat-curable composition, which can be used as an ink carrier composition for preparing printable inks. The crosslinker composition and ink described herein can remain stable for a long time at room temperature without crosslinking, solid precipitation or component delamination. Therefore, the present disclosure provides a formaldehyde-free, heat-curable, printable ink that can be used to print images on hard surfaces (e.g., metal surfaces of containers).

[0015] 1. Definition

[0016] As used herein, the terms "comprises," "including," "having," "may," "containing," and variations thereof are intended as open transitional phrases, terms, or words that do not exclude the possibility of additional actions or structures. The singular forms "a," "an," and "the" include plural referents unless the context indicates otherwise. The present disclosure also contemplates other embodiments that "comprise," "consist of," and "consist essentially of" the embodiments or elements set forth herein, whether explicitly stated or not.

[0017] The modifier "about" used in conjunction with a quantity includes the stated value and has the meaning dictated by the context (e.g., it includes at least the degree of error associated with the measurement of a particular quantity). The modifier "about" should also be considered to disclose a range defined by the absolute values ​​of the two endpoints. For example, the expression "about 2 to about 4" also discloses a range of "2 to 4". The term "about" can refer to plus or minus 10% of the number shown. For example, "about 10%" can mean a range of 9% to 11%, and "about 1" can mean 0.9-1.1. Other meanings of "about" may be apparent from the context, such as rounding, so, for example, "about 1" can also mean from 0.5 to 1.4.

[0018] For numerical ranges described herein, each intervening number with equal precision therebetween is expressly contemplated. For example, for a range of 6-9, in addition to 6 and 9, the numbers 7 and 8 are also contemplated, and for a range of 6.0-7.0, the numbers 6.0, 6.1, 6.2, 6.3, 6.4, 6.5, 6.6, 6.7, 6.8, 6.9, and 7.0 are expressly contemplated.

[0019] As used herein, the term "alkyl" refers to a straight or branched saturated hydrocarbon chain containing 1 to 20 carbon atoms. 1-6 “Alkyl” refers to a straight or branched chain hydrocarbon containing from 1 to 6 carbon atoms. Representative examples of alkyl include, but are not limited to, methyl, ethyl, n-propyl, isopropyl, n-butyl, sec-butyl, isobutyl, tert-butyl, n-pentyl, isopentyl, neopentyl, n-hexyl, 3-methylhexyl, 2,2-dimethylpentyl, 2,3-dimethylpentyl, n-heptyl, n-octyl, n-nonyl, and n-decyl.

[0020] In some cases, the number of carbon atoms in an alkyl group is indicated by the prefix "C x-y ” or “C x -C y -" where x is the minimum number of carbon atoms in the substituent and y is the maximum number of carbon atoms. Thus, for example, "C 1-4 "Alkyl" or "C1-C4 alkyl" refers to an alkyl substituent containing 1 to 4 carbon atoms.

[0021] The term "butanol" means n-butanol having the formula CH3(CH2)3OH.

[0022] The term "cure" or "curing" means a process that causes hardening of a hydroxy-functional polymer and / or crosslinking of a hydroxy-functional polymer with other hydroxy-functional polymers, within the same polymer, or a combination thereof. In addition, the non-volatile diluent may also interact with the crosslinker, depending on whether the non-volatile diluent has functional groups that are capable of reacting with the crosslinker compound. Curing may be initiated by heating.

[0023] The term "substantially free" means that the component is not present in the composition or is present in the composition in an amount of 2% or less by weight of the composition, including 1% or less, 0.5% or less, 0.01% or less, 0.005% or less, or 0.001% or less by weight.

[0024] The terms "hydroxy" or "hydroxyl" are used interchangeably herein and refer to an -OH group.

[0025] Unless expressly stated otherwise, the term "molecular weight" means number average molecular weight.Molecular weight can be measured by standard techniques known in the art, such as gel permeation chromatography, size exclusion chromatography, and / or rheological analysis.

[0026] When referring to components of an ink carrier composition and / or ink, the terms "non-volatile" and "volatile" refer to the percentage of a component (e.g., a non-volatile diluent) that is released from the ink carrier composition and / or ink under specified baking conditions as described in ASTM D2369-20. For example, "volatile" refers to a component that substantially evaporates (e.g., greater than 90%, greater than 95%, greater than 99%, or about 100%) from the ink carrier composition and / or ink when heated at 110±5°C for 60 minutes. "Non-volatile" refers to a component that does not substantially evaporate (e.g., less than 10%, less than 5%, less than 1%, or about 0%) from the ink carrier composition and / or ink when heated at 110±5°C for 60 minutes.

[0027] The term "oligomer" refers to a material having a molecular weight of about 1,000 g / mol to 3,000 g / mol.

[0028] The term "polymer" refers to a macromolecule having a molecular structure comprising a large number of smaller units bonded together. The smaller units are usually derived from monomers or oligomers. The term is used interchangeably with resin herein.

[0029] The term "room temperature" means a temperature of about 20°C to about 25°C.

[0030] 2. Ink carrier composition

[0031] In one aspect, the present disclosure provides an ink carrier composition comprising

[0032] A crosslinker compound of formula (I),

[0033]

[0034] Where R 1 , R 2 and R 3 Each is independently C 1-10alkyl;

[0035] Hydroxy-functional polymers; and

[0036] Non-volatile diluent,

[0037] wherein the composition is substantially free of butanol.

[0038] In some embodiments, R 1 , R 2 and R 3 Each is independently C 1-4 In some embodiments, R 1 , R 2 and R 3 Each is independently n-butyl (—CH2CH2CH2CH3) or methyl (—CH3). TACT-type crosslinker compounds are commercially available and are typically provided in n-butanol as a solvent. n-Butanol and any other volatile co-solvents can be replaced with non-volatile diluents by appropriate solvent exchange.

[0039] The crosslinker compound may also be referred to herein as a 1,3,5-triazine carbamate (TACT) crosslinker. TACT crosslinkers can be used to crosslink polymers containing hydroxyl, epoxy, thiol, amino, and / or carboxyl functional groups. For example, TACT crosslinkers can react with hydroxyl groups of hydroxyl functional polymers at >125°C to form carbamate bonds. The TACT-based crosslinking process does not generate or release formaldehyde. Therefore, the disclosed ink carrier composition can be formaldehyde-free. In some embodiments, the ink carrier composition is free of or substantially free of formaldehyde.

[0040] The crosslinker compound can be used as the sole crosslinker in the ink carrier composition, or it can be used in combination with other crosslinkers, such as amino resins or isocyanates. Other crosslinkers can be used to obtain a balance of properties. In some embodiments, the ink carrier composition does not contain any other crosslinkers other than the crosslinker compound.

[0041] The ink carrier composition may include from about 10 wt % to about 90 wt % of the crosslinker compound, such as from about 20 wt % to about 80 wt %, or from about 25 wt % to about 70 wt %.

[0042] Hydroxy-functional polymers as described herein are polymers containing multiple hydroxyls. For example, hydroxy-functional polymers can contain at least two, preferably more than two hydroxyls. The hydroxyl group can be suspended from the main chain of the polymer, or can be at the end of the polymer, or both. The hydroxy-functional polymer can be modified by one or more fatty acids. Suitable hydroxy-functional polymers include, for example, polyacrylic acid, polyester, polyurethane and alkyd materials. Suitable hydroxy-functional polyacrylic acid polymers can be obtained, for example, by copolymerization of acrylate or methacrylate with hydroxy-functional acrylate or methacrylate (such as hydroxyethyl acrylate or hydroxyethyl methacrylate). Suitable hydroxy-functional polyesters can be obtained, for example, by reacting polycarboxylic acids with excess polyols (polyhydric alcohol). In some embodiments, the hydroxy-functional polymer is a hydroxy-functional polyester, a hydroxy-functional polyacrylic acid, a hydroxy-functional polyurethane or a combination thereof. In some embodiments, the hydroxy-functional polymer is a hydroxy-functional polyester or a hydroxy-functional polyacrylic acid.

[0043] The hydroxy-functional polymer may have a molecular weight and a hydroxyl value that make it suitable for use in ink formulations such as thermosetting, heat-curable inks. For example, the hydroxy-functional polymer may have a weight average molecular weight (Mw) of about 1000 g / mol to about 6000 g / mol and a number average molecular weight (Mn) of about 500 g / mol to about 3000 g / mol. In addition, the hydroxy-functional polymer may have a hydroxyl value of about 30 to about 300 mg KOH / g polymer. The hydroxy-functional polymer may also have an acid value of about 10 to about 100 mg KOH / g polymer.

[0044] Examples of hydroxy-functional polymers include 540 acrylic polymer (SC Johnson & Sons, Racine, WI), 500 acrylic resin (SC Johnson & Sons, Racine, WI), AT-400 acrylic resin (Rohm & Haas, Philadelphia, PA), 1531 polyester resin (Cytec Industries, West Patterson, NJ), CARGILL 3000 and 5776 polyester resins (Cargill, Minneapolis, MN), Polyester resin (Union Carbide, Danbury, CT), XM-2302 and XM-2306 resins (King Industries, Norwalk, CT), 11-1369 resin (Cook Composites and Polymers, Port Washington, WI), AC-1024 acrylic emulsion resin (Rohm & Haas, Philadelphia, PA), 4005 water-reducible acrylic resin (Cytec Industries, West Patterson, NJ), 3494 solid hydroxyl-terminated polyester resin (UCB CHEMICALS USA, Smyrna, GA), 101 polyester resin (Ruco Polymer, Hicksville, NY), SCX-800-A and SCX800-B hydroxy-functional solid acrylic resins (SC Johnson & Sons, Racine, WI), AN 745 hydroxy-functional polyester resin, a product of Hoechst, etc.

[0045] In some embodiments, the hydroxyl functional polymer is a hydroxyl functional polyester (also known as a polyester polyol). Suitable polyester polyols include, for example, tridecyl ester polymers prepared from 1,3-phthalic acid, 1,3-dihydro-1,3-dioxo-5-isobenzofurancarboxylic acid, and 2,2-dimethyl-1,3-propanediol.

[0046] In some embodiments, the hydroxyl-functional polymer is a hydroxyl-functional polyacrylic acid. Exemplary hydroxyl-functional polyacrylic acids are 500, which has the following properties.

[0047]

[0048]

[0049] The ink carrier composition may include from about 20 wt % to about 80 wt % of the hydroxy-functional polymer, such as from about 30 wt % to about 70 wt %, or from about 40 wt % to about 60 wt %.

[0050] The non-volatile diluent is an oligomer and is non-volatile, as defined in D2369-20 and herein. Because the non-volatile diluent is an oligomer, it has a lower molecular weight compared to the hydroxyl functional polymer. The non-volatile diluent can be a hydrocarbon, a glycol, an alkylated polyglycol, a polyester, a fatty alcohol, or a combination thereof. The non-volatile diluent can allow high-speed offset printing with little or no evaporation. For example, the non-volatile diluent can have a boiling point of at least 145°C, such as at least 150°C, at least 160°C, or at least 170°C. In some embodiments, the non-volatile diluent has a boiling point of about 145°C to about 200°C, such as about 145°C to about 190°C or about 150°C to about 185°C. Therefore, the non-volatile diluent is not easily evaporated into a gas at room temperature or as high as a temperature for thermal ink curing.

[0051] As described above, the cross-linker compound can be provided in a solvent. In these embodiments, the non-volatile diluent can be exchanged with the solvent and can have a boiling point that is at least 30°C higher than the boiling point of the exchanged solvent, such as at least 40°C higher than the boiling point of the exchanged solvent, at least 50°C higher than the boiling point of the exchanged solvent, or at least 60°C higher than the boiling point of the exchanged solvent.

[0052] During the curing process, the non-volatile diluent may or may not participate in the cross-linking reaction. Whether the non-volatile diluent participates in the cross-linking reaction depends on whether the non-volatile diluent has a functional group that can react with the cross-linker compound. In some embodiments, the non-volatile diluent reacts with the cross-linker compound during curing. For example, the non-volatile diluent may have hydroxyl, epoxy, sulfhydryl, amino and / or carboxyl functional groups. In some embodiments, the non-volatile diluent has at least one hydroxyl functional group. In other embodiments, the non-volatile diluent does not react with the cross-linker compound during curing.

[0053] Suitable non-volatile diluents include commercially available polyalkanolamines (Eastman), glycols and polyglycols (BASF, Dow) and fatty alcohols (such as tridecanol). In some embodiments, the non-volatile diluent is a polyalkylene glycol. Polyalkylene glycol can be synthesized by the ring-opening reaction of alkylene oxides (such as ethylene oxide and propylene oxide) and alcohols (such as glycols). Polyalkylene glycol can be a type of monomer or can include two or more monomers. In addition, polyalkylene glycol can be alkylated. In some embodiments, polyalkylene glycol is polyethylene oxide, polypropylene oxide, butoxy-(polyethylene oxide-polypropylene oxide) mixture or a combination thereof. In some embodiments, the non-volatile diluent is polyalkylene glycol, butoxy-(polyethylene oxide-polypropylene oxide) mixture or a combination thereof.

[0054] The ink carrier composition may include from about 5 wt % to about 30 wt % of a nonvolatile diluent, such as from about 5 wt % to about 20 wt %, or from about 10 wt % to about 20 wt %.

[0055] In some embodiments, the ink carrier composition may include from about 10% to about 30% by weight of a crosslinker compound, from about 40% to about 80% by weight of a hydroxyl-functional polymer, and from about 5% to about 20% by weight of a non-volatile diluent. An exemplary composition is shown below.

[0056] weight% Hydroxy Functional Polymers 49.5% Non-volatile diluent 35% Crosslinker compounds 15.5% total 100%

[0057] In some embodiments, the composition comprises: a crosslinker compound of formula (I), wherein R 1 , R 2 and R 3each independently being methyl or n-butyl; a hydroxy-functional polyester as the hydroxy-functional polymer; and a polyalkylene glycol as the nonvolatile diluent.

[0058] As described above, butanol is incompatible with heat-curable ink formulations. Therefore, since the disclosed ink carrier compositions can be used in heat-curable ink compositions, they can contain little or no butanol. For example, the ink carrier composition can contain 2 wt % or less butanol, such as 1 wt % or less, 0.5 wt % or less, 0.1 wt % or less, 0.05 wt % or less, 0.01 wt % or less, 0.005 wt % or less, or 0.001 wt % or less. In some embodiments, the ink carrier composition contains 0.1 wt % or less butanol. In some embodiments, the ink carrier composition is substantially free of butanol. In some embodiments, the ink carrier composition is free of butanol.

[0059] Additionally, the ink vehicle composition can be substantially free of other volatile solvents, including water and organic solvents known in the art such as hydrocarbon, alcohol, ketone, ether, ester, and amide solvents. In some embodiments, the composition is free of any volatile solvents.

[0060] The ink carrier composition may have properties that make it suitable for ink formulations. For example, the ink carrier composition may be a liquid. In addition, the ink carrier composition may have a viscosity of about 200 to about 500 poise, such as about 250 to about 350 poise. The ink carrier composition may also have a density of about 8 pounds per gallon to about 12 pounds per gallon, such as about 9, about 9.5, about 10, or about 11 pounds per gallon. In some embodiments, the composition may have a density of about 9.3 pounds per gallon.

[0061] The ink carrier composition can be in the form of a transparent liquid. The ink carrier composition can have a refractive index of 1.2 or greater, such as 1.3 or greater, 1.4 or greater, 1.5 or greater, or 1.6 or greater. In some embodiments, the composition has a refractive index of 1.496 or greater.

[0062] The combination of crosslinker compounds, hydroxyl-functional polymers, and non-volatile diluents can impart favorable stability to the ink carrier composition and its ink. For example, the ink carrier composition can be stable at room temperature for at least 6 months, including at least 12 months, at least 18 months, or at least 24 months. In some embodiments, the ink carrier composition is stable at room temperature for about 6 to about 24 months. As described herein, if no changes in the physical appearance or chemical properties of the ink carrier composition are observed over a period of time, the ink carrier composition is considered to be stable during that period of time. These changes include, for example, decomposition of components, reactions between different components, precipitation of solid materials, stratification of components, or changes in color. The stability of the ink carrier composition can be measured or evaluated by observing the time-dependent changes in the rheology of the composition under storage conditions from room temperature to hot box to freeze-thaw; see, for example, ASTM D1849, ASTM D2337. For example, stability can be shown by maintaining at 60°C or -20°C and returning to room temperature without changes in viscosity or rheology and without the formation of gel particles.

[0063] a. Method for preparing ink carrier composition

[0064] The ink carrier composition can be prepared by a process comprising mixing a crosslinker compound, a hydroxyl functional polymer, and a nonvolatile diluent dissolved in butanol to form a mixture, and evaporating at least 98% of the butanol from the mixture to provide the disclosed ink carrier composition.

[0065] The evaporation can be performed by heating the mixture under reduced pressure (e.g., 20 mmHg (torr) or less, 10 mmHg or less, or 5 mmHg or less). The evaporation can be performed at a temperature of about 55°C to about 75°C, such as about 60°C, about 65°C, or about 70°C. In some embodiments, the evaporation is performed by heating the mixture at about 60°C to about 75°C under a pressure of 20 mmHg or less.

[0066] The remaining amount of butanol in the ink carrier composition after the evaporation step can be 2% or less of the amount of butanol before evaporation, including 1.5% or less, 1.0% or less, 0.5% or less, 0.1% or less, 0.05% or less or 0.01% or less.

[0067] 3. Thermosetting heat curable ink

[0068] In another aspect, the present disclosure provides a thermosetting heat-curable ink comprising: (a) an ink carrier composition as described herein and (b) a colorant.

[0069] The colorant can be a pigment or a dye. The colorant can be a self-dispersing material, or it can be used in combination with a separate dispersant. In some embodiments, the colorant is a pigment. Generally, any pigment that is compatible with the other components of the ink and is thermally stable at the necessary curing temperature can be used. The pigment can be cyan, magenta, yellow, black, white, red, orange, purple, blue, green, brown, or a mixture thereof. Examples of pigments can be grouped by corresponding color indices:

[0070] Pigment Yellow 1, 3, 5, 12, 13, 14, 15, 17, 34, 35, 37, 41, 42, 43, 55, 74, 81, 83, 87, 93, 94, 95, 97, 108, 109, 110, 117, 119, 138, 139, 153, 154, 155, 157, 166, 167, 168, 174, 175, 180, 185, 193, 213, 214 and 215;

[0071] Pigment Red 3, 5, 19, 22, 23, 31, 38, 41, 43, 48:1, 48:2, 48:3, 48:4, 48:5, 49:1, 52, 52:1, 52:2, 53:1, 57:1, 57:2, 58:4, 63:1, 64:1, 81, 81:1, 81:2, 81:3, 81:4, 88, 95, 104, 108, 112, 122, 123, 136, 144, 146, 149, 166, 168, 169, 170, 175, 177, 178, 179, 184, 185, 208, 216, 226, 254, 257 and 279;

[0072] Pigment Blue 1, 15, 15:1, 15:2, 15:3, 15:4, 15:6, 16, 17:1, 22, 24, 24:1, 27, 28, 29, 36, 60, 61, 62, 63, and 75;

[0073] Pigment Black 7, 9, 10, 28 and 34;

[0074] Pigment White 6, 11, 12, 18, 21 and 22;

[0075] Pigment Orange 4, 5, 13, 16, 20, 34, 36 and 64;

[0076] Pigment Violet 1, 2, 3, 19, 23, 25, 27, 29, 30, 37 and 50;

[0077] Pigment Green 7, 8, 10, 17, 26 and 36; and

[0078] Pigment Brown 3, 5, 25 and 26.

[0079] The thermosetting heat curable ink may contain about 0.1 wt % to about 60 wt % of the ink carrier composition, such as about 30 wt % to about 60 wt %, or about 40 wt % to about 60 wt %. In addition, the thermosetting heat curable ink may contain about 0.1 wt % to about 50 wt % of the colorant, such as about 10 wt % to about 60 wt %, or about 20 wt % to about 60 wt %.

[0080] Thermosetting heat curable inks may also include lubricants, viscosity modifiers, viscosity modifiers, flow modifiers, surfactants, diluents or combinations thereof. Thermosetting heat curable inks may include about 0 wt % to about 5 wt % of viscosity modifiers. Suitable viscosity modifiers include, for example, talc, clay, silica or combinations thereof. Thermosetting heat curable inks may include about 0 wt % to about 5 wt % of surfactants. Suitable surfactants include, for example, alkoxylated surfactants. Thermosetting heat curable inks may include about 0 wt % to about 20 wt % of viscosity modifiers. Thermosetting heat curable inks may include about 0 wt % to about 5 wt % of flow modifiers. Suitable viscosity modifiers and flow modifiers are known in the art.

[0081] Thermosetting heat curable inks can be prepared by mixing an ink carrier composition as described herein, a colorant, and any other ingredients. Typically, the ink carrier composition is metered into a mixing tank. The colorant is then added and dispersed. Diluents and other ingredients may also be added to adjust the viscosity to a desired level.

[0082] Representative thermosetting heat curable inks prepared by the methods described herein can be used to print on any surface that can withstand the temperature required to cure the thermosetting heat curable ink. Exemplary surfaces include metal surfaces (such as aluminum surfaces). Exemplary thermosetting heat curable inks can exhibit the following physical properties:

[0083] · Viscosity, 1', 90°F (32.2°C) @ 1200rpm:

[0084] o 8.0-21.0±1(ink)

[0085] o 14.0-25.0±1(matrix);

[0086] · Grinding :

[0087] o<3NPIRI

[0088] o<7.5 μm; and

[0089] · Laray viscosity, 25°C:

[0090] o 50+ / -20 berths.

[0091] Thermosetting heat curable inks as described herein can be stable at room temperature for at least 6 months, including at least 12 months, at least 18 months, or at least 24 months. In some embodiments, thermosetting heat curable inks are stable at room temperature for about 6 to about 24 months. Thermosetting heat curable inks can be free of discoloration caused by heat or air oxidation, or discoloration caused by heat or air oxidation can be kept very low. Crosslinking reactions will not occur in the ink of the present invention until there is enough activation energy during the curing cycle (e.g., in a baking enamel oven). The ink of the present invention can avoid pigment sedimentation during storage or use.

[0092] 4.Printing

[0093] In another aspect, the present disclosure provides a method of printing ink onto a substrate, comprising applying a thermosetting heat-curable ink as described herein to a surface of the substrate, and heating the applied ink to cure the applied ink. Curing can generally be accomplished without the use of a catalyst. In addition, the cured film and / or ink can exhibit useful hardness, chemical resistance, exterior durability, and environmental etching resistance.

[0094] Heating can be performed at a temperature of at least 150°C, including at least 170°C, at least 190°C, or at least 210°C. In some embodiments, heating is performed at about 180°C to about 200°C, such as about 185°C, about 190°C, or about 195°C.

[0095] The substrate can be any substrate that can withstand the temperature required to cure the thermosetting heat curable ink. For example, the substrate can include a metal surface or be made of metal. Suitable substrates include containers for industrial or consumer products, such as beverage or food containers. In some embodiments, the substrate is a metal container, such as an aluminum can for holding beverages or food.

[0096] In some embodiments, the thermosetting heat curable ink of the present invention is used in a high-speed offset printing process to provide a printed image or decoration on a metal surface. Suitable processes include those performed under the applicable standards described by the National Printing Ink Research Institute (NPIRI). A typical high-speed offset printing process includes transferring ink from a single color (pigmented) ink hole to a lithographic printing plate having an ink-receiving image area. The process can be performed in a rotary system, and the thin metal plate can be wrapped around the cylinder. The ink image can be transferred from the printing plate to a "rubber blanket", an intermediate cylinder covered with a layer of rubber, which transfers the image to the substrate surface. For printing aluminum cans, printing can be performed at a high speed of about 1000 to about 2000 cans per minute (cpm).

[0097] 5. Examples

[0098] Example 1 - Preparation of ink carrier composition

[0099] The solid TACT crosslinking agent of formula (I) (wherein R 1 , R 2 and R 3 A mixture of about 50 wt% butanol (15.5 wt. parts), polyester polyol (49.5 wt. parts) and a polyalkylene glycol nonvolatile diluent (35 wt. parts) are mixed. At least 98% of the butanol is removed from the mixture by rotary evaporation at 65° C. under a reduced pressure of about 20 torr.

[0100] The resulting composition was stored at room temperature for up to 2 years without any observed precipitation.

[0101] Example 2 - Preparation of Thermosetting Heat-curable Ink

[0102] A thermosetting heat-curable ink was prepared according to the following formulation:

[0103] Element weight% Ink carrier composition (Example 1) 45.0 Non-volatile diluent 20.0 Additives (viscosity modifiers and flow modifiers) 3.0 Red Pigment 32.0 total 100.0

[0104] Example 3 - Printing on Aluminum Cans

[0105] The ink prepared in Example 2 was printed onto aluminum cans by a high-speed offset printing process, and the ink on the printed cans was cured in an oven at a temperature of 193°C (380°F).

[0106] For reasons of completeness, various aspects of the invention are set out in the following numbered clauses:

[0107] Item 1. An ink carrier composition comprising a crosslinker compound of formula (I),

[0108]

[0109] Where R 1 , R 2 and R 3 Each is independently C 1-10 an alkyl group; a hydroxy-functional polymer; and a nonvolatile diluent, wherein the composition is substantially free of butanol.

[0110] Item 2. The composition of Item 1, wherein R 1 , R 2 and R 3 Each is independently C 1-4 alkyl.

[0111] Clause 3. The composition of Clause 1 or Clause 2, wherein the amount of the crosslinker compound is from about 10% to about 90% by weight of the composition.

[0112] Clause 4. The composition of any of Clauses 1-3, wherein the hydroxyl-functional polymer is selected from the group consisting of hydroxyl-functional polyesters, hydroxyl-functional polyacrylic acids, hydroxyl-functional polyurethanes, and combinations thereof.

[0113] Clause 5. The composition of any of Clauses 1-4, wherein the amount of the hydroxyl-functional polymer is from about 20% to about 80% by weight of the composition.

[0114] Clause 6. The composition of any of Clauses 1-5, wherein the non-volatile diluent is selected from the group consisting of hydrocarbons, glycols, polyalkylene glycols, polyesters, and combinations thereof.

[0115] Clause 7. The composition of any of Clauses 1-6, wherein the amount of the non-volatile diluent is from about 5% to about 30% by weight of the composition.

[0116] Clause 8. The composition of any of Clauses 1-7, having a viscosity of about 200 to about 500 poise.

[0117] Clause 9. The composition of any of Clauses 1-8, wherein the composition is stable at room temperature for about 6 to about 24 months.

[0118] Clause 10. The composition of any one of clauses 1 to 9, wherein R 1 , R 2 and R 3 each independently is methyl or n-butyl; the hydroxy-functional polymer is a hydroxy-functional polyester; and the non-volatile diluent is a polyalkylene polyglycol.

[0119] Clause 11. A method of preparing an ink carrier composition, the method comprising:

[0120] mixing a crosslinker compound of formula (I), a hydroxyl functional polymer, and a non-volatile diluent to form a mixture,

[0121]

[0122] Where R 1 , R 2 and R 3 Each is independently C 1-10 an alkyl group, and wherein the crosslinker compound is dissolved in butanol; and

[0123] At least 98% of the butanol is evaporated from the mixture to provide a composition as described in any of clauses 1-10.

[0124] Clause 12. The method of Clause 11, wherein the evaporating comprises heating the mixture at a temperature of about 65°C at a pressure of 20 mmHg (Torr) or less.

[0125] Item 13. A thermosetting heat-curable ink comprising (a) the ink carrier composition of any of Items 1-10; and (b) a colorant.

[0126] Clause 14. The thermosetting heat-curable ink of Clause 13, wherein the ink is stable at room temperature for at least 6 months.

[0127] Clause 15. The thermosetting heat curable ink of Clause 13 or Clause 14, wherein the amount of the ink carrier composition is from about 30% to about 60% by weight of the ink.

[0128] Clause 16. The thermosetting heat-curable ink of any of Clauses 13-15, wherein the amount of the colorant is from about 10% to about 60% by weight of the ink.

[0129] Clause 17. The thermosetting heat curable ink of any of Clauses 13-16, further comprising a lubricant, a viscosity modifier, a tack modifier, a flow modifier, a surfactant, a diluent, or a combination thereof.

[0130] Item 18. A method of printing ink onto a substrate, the method comprising: applying the thermosetting heat-curable ink of any one of Items 13-17 onto a surface of the substrate; and heating the applied thermosetting heat-curable ink to thereby cure the applied thermosetting heat-curable ink.

[0131] Clause 19. The method of Clause 18, wherein the surface is a metal surface.

[0132] Clause 20. The method of Clause 18 or Clause 19, wherein the substrate is a container.

[0133] Various features, advantages and embodiments are set forth in the following claims.

Claims

1. An ink carrier composition comprising A crosslinker compound of formula (I), Where R 1 , R 2 and R 3 Each is independently C 1-10 alkyl; Hydroxy-functional polymers; and Non-volatile diluent, wherein the composition is substantially free of butanol.

2. The composition according to claim 1, wherein R 1 , R 2 and R 3 Each is independently C 1-4 alkyl.

3. The composition of claim 1, wherein the amount of the crosslinker compound is from about 10% to about 90% by weight of the composition.

4. The composition of claim 1, wherein the hydroxyl-functional polymer is selected from the group consisting of hydroxyl-functional polyesters, hydroxyl-functional polyacrylic acids, hydroxyl-functional polyurethanes, and combinations thereof.

5. The composition of claim 1, wherein the hydroxyl functional polymer is present in an amount of from about 20% to about 80% by weight of the composition.

6. The composition of claim 1, wherein the non-volatile diluent is selected from the group consisting of hydrocarbons, glycols, polyalkylene glycols, polyesters, and combinations thereof.

7. The composition of claim 1, wherein the amount of the non-volatile diluent is from about 5% to about 30% by weight of the composition.

8. The composition of claim 1 having a viscosity of about 200 to about 500 poise.

9. The composition of claim 1, wherein the composition is stable at room temperature for about 6 to about 24 months.

10. The composition according to claim 1, wherein R 1 , R 2 and R 3 are each independently methyl or n-butyl; The hydroxy-functional polymer is a hydroxy-functional polyester; and The non-volatile diluent is a polyalkylene polyglycol.

11. A method for preparing an ink carrier composition, the method include: mixing a crosslinker compound of formula (I), a hydroxyl functional polymer, and a non-volatile diluent to form a mixture, Where R 1 , R 2 and R 3 Each is independently C 1-10 an alkyl group, and wherein the crosslinker compound is dissolved in butanol; and At least 98% of the butanol is evaporated from the mixture to provide the composition of claim 1.

12. The method of claim 11, wherein the evaporating comprises heating the mixture at a temperature of about 65°C at a pressure of 20 mmHg (Torr) or less.

13. A thermosetting heat curable ink comprising (a) the ink carrier composition according to claim 1; and (b) Colorant.

14. The thermosetting heat curable ink of claim 13, wherein the ink is stable at room temperature for at least 6 months.

15. The thermosetting heat curable ink of claim 13, wherein the ink carrier composition is present in an amount of about 30% to about 60% by weight of the ink.

16. The thermosetting heat curable ink of claim 13, wherein the colorant is present in an amount of about 10% to about 60% by weight of the ink.

17. The thermosetting heat curable ink of claim 13, further comprising a lubricant, a viscosity modifier, a tack modifier, a flow modifier, a surfactant, a diluent, or a combination thereof.

18. A method for printing ink onto a substrate, the method include: applying the thermosetting heat-curable ink according to claim 13 onto a surface of a substrate; as well as The applied thermosetting heat curable ink is heated, thereby curing the applied thermosetting heat curable ink.

19. The method of claim 18, wherein the surface is a metal surface.