Method for reducing surface glossiness of polymer ink
By using a low-band light source to irradiate polymer ink in an oxygen-free environment during inkjet printing, a low-gloss surface film layer is formed, which solves the reflection problem caused by excessive gloss of polymer ink and improves the printing Readability and visual effects avoid the risk of nozzle clogging.
Patent Information
- Application Number
- CN202411065606.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-05
- Publication Date
- 2024-11-19
AI Technical Summary
The glossiness of polymer inks is too high, leading to reflection problems, especially during inkjet printing, large-particle materials can easily clog the nozzle, affecting the visual experience of the printed material and the information transmission effect.
After printing polymer inks through an inkjet printer and precuring, it is irradiated with a low-band light source in an oxygen-free environment to form a low-gloss surface film layer to reduce the gloss of the ink. Specific steps include printing, precuring, low-band light source irradiation and complete curing, controlling the light source wavelength, energy and time to form a stable low-gloss surface film.
When the ink is not completely cured, a low-band light source is used to form a low-gloss surface film layer, which solves the reflection problem caused by excessive gloss of polymer ink, avoids the risk of large-particle materials blocking the nozzle, and improves the ability of printed materials Readability and visual effects.
Smart Images

Figure CN118977518A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of polymer ink, and in particular to a method for reducing the surface glossiness of polymer ink. Background Art
[0002] As an important choice in printing and coating applications, polymer inks use the properties of polymer compounds to achieve excellent printing quality and durability. This type of ink is favored for its compatibility with a variety of substrates and chemical stability, and is suitable for printing needs on a variety of surfaces from paper to plastic boards, glass and metal.
[0003] However, some polymer inks currently have a significant technical defect: the reflection problem caused by excessive gloss. In printed display or advertising materials, excessive gloss may cause reflected light, affecting the visual experience and information communication effect. Especially in applications such as outdoor signs, packaging and posters, reflections may make information difficult to read or the visual effect is poor, thus affecting the actual use value of the printed matter.
[0004] In the prior art, large particles are generally added to the polymer ink to reduce the glossiness of the polymer ink. However, when the printhead in a printer using the inkjet printing (IJP) technology prints the polymer material, the large particles are likely to clog the printhead and cause a malfunction. Therefore, the prior art has the problem of reflection caused by the excessive glossiness of the polymer ink. Summary of the invention
[0005] The main purpose of the present invention is to provide a method for reducing the surface glossiness of polymer ink, aiming to solve the problem of reflection caused by excessive glossiness of polymer ink.
[0006] To achieve the above object, the present invention provides a method for reducing the surface gloss of polymer ink, the method for reducing the surface gloss of polymer ink comprising:
[0007] The polymer ink is sprayed onto the product surface through the nozzle of the inkjet printer;
[0008] Pre-curing the polymer ink sprayed onto the surface of the product;
[0009] In an oxygen-free environment, a low-band light source is used to irradiate the pre-cured polymer ink;
[0010] The polymer ink is completely cured after being irradiated by a low-wavelength light source.
[0011] Furthermore, in an oxygen-free environment, the low-band light source is selected to irradiate the pre-cured polymer ink, including:
[0012] In an inert gas environment, a low-band light source is selected to irradiate the pre-cured polymer ink.
[0013] Furthermore, in an oxygen-free environment, the low-band light source is selected to irradiate the pre-cured polymer ink, including:
[0014] In an oxygen-free environment, a UV light source with a wavelength of 172 nm to 260 nm is selected to irradiate the pre-cured polymer ink.
[0015] Furthermore, the low-band light source irradiates the pre-cured polymer ink for a period of 0.2s to 0.5s.
[0016] Furthermore, in an oxygen-free environment, a low-band light source is selected to irradiate the pre-cured polymer ink:
[0017] The polymer ink irradiated with the low-band light source is placed in an oxygen-free environment for 10 to 20 minutes.
[0018] Furthermore, the pre-curing of the polymer ink sprayed onto the surface of the product includes:
[0019] The polymer ink sprayed onto the surface of the product is irradiated by a UV light source with a wavelength of 365nm to 395nm.
[0020] Furthermore, the energy output by the UV light source is 800mj to 1200mj.
[0021] Furthermore, the polymer ink sprayed onto the surface of the product is pre-cured to a degree of curing of 15% to 30% of full curing.
[0022] Furthermore, the polymer ink is sprayed onto the surface of the product by the nozzle of the inkjet printer to a thickness of 10 microns to 15 microns.
[0023] Furthermore, the polymer ink sprayed onto the surface of the product is pre-cured for 5 to 10 minutes.
[0024] The beneficial effect of the technical solution of the present invention is that: when the ink has not yet solidified, a low-band light source is selected to irradiate the surface of the polymer ink in an oxygen-free environment, so that a low-gloss surface film layer is produced on the surface of the polymer ink, thereby reducing the glossiness of the polymer ink surface and solving the reflection problem caused by the excessive glossiness of the polymer ink. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 A schematic diagram of steps provided for an embodiment of a method for reducing the surface glossiness of a polymer ink according to the present invention;
[0026] Figure 2 A detailed schematic diagram of step S21 and step S31 provided for an embodiment of a method for reducing the surface glossiness of a polymer ink of the present invention;
[0027] Figure 3 A detailed schematic diagram of step S32 is provided for an embodiment of a method for reducing the surface glossiness of polymer ink of the present invention.
[0028] The realization of the purpose, functional features and advantages of the present invention will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION
[0029] The scheme in the embodiment of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiment of the present invention. Obviously, the described embodiment is only a part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0030] It should be noted that all directional indications in the embodiments of the present invention (such as up, down, left, right, front, back, etc.) are only used to explain the relative position relationship, movement status, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.
[0031] It should also be noted that when an element is referred to as being "fixed on" or "disposed on" another element, it may be directly on the other element or there may be an intermediate element at the same time. When an element is referred to as being "connected to" another element, it may be directly connected to the other element or there may be an intermediate element at the same time.
[0032] In addition, the descriptions of "first", "second", etc. in the present invention are only used for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In addition, the technical solutions between the various embodiments can be combined with each other, but they must be based on the ability of ordinary technicians in the field to implement them. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such a combination of technical solutions does not exist and is not within the scope of protection required by the present invention.
[0033] like Figure 1 As shown, the present invention provides a method for reducing the surface glossiness of polymer ink, and the method for reducing the surface glossiness of polymer ink comprises the following steps (S1, S2, S3 and S4):
[0034] Step S1: Print the polymer ink onto the surface of the product through the nozzle of the inkjet printer. Specifically, the inkjet printer adopts the inkjet printing (IJP) technology. The inkjet printing technology is an advanced printing technology that recreates digital graphics by spraying tiny ink droplets onto the surface of the material. The inkjet printing technology does not require plate making or mold making, nor does it require contact with the material to complete the surface coating. The nozzle of the inkjet printer using the inkjet printing technology has micron-level nozzle holes, and the nozzle holes of the inkjet printer nozzle are arranged in rows to control the polymer ink injection position and form ink dots. In a specific embodiment, the polymer ink is a nanomaterial ink.
[0035] As an implementation method, step S1 includes: controlling the movement of the inkjet printer's nozzle according to the position information of the preset printing area, and printing the polymer ink to the preset printing area on the surface of the product. Specifically, the product to be printed is fixed on a preset jig. After the jig is moved to the printing station, the position of the jig and the position of the nozzle are pre-set. After obtaining the position information of the product on the jig, the position information of the product can be determined, thereby obtaining the position information of the preset printing area on the surface of the product. Furthermore, the position information of the preset printing area is obtained and the movement of the nozzle is controlled by the printer controller.
[0036] In other embodiments, a visual positioning component is preset in the printer, and the visual positioning component includes a camera and an image processing unit. The visual positioning component is used to obtain the position information of the preset printing area on the surface of the product. For example, in the product to be printed after laser engraving, such as key cap characters, the controller printer determines the position information of the preset printing area of the product according to the image information of the laser engraving mark fed back by the visual positioning component, and controls the nozzle of the inkjet printer to print the preset printing area according to the position information of the preset printing area.
[0037] In some embodiments, the printer controller may optionally:
[0038] First, the programmable logic controller (PLC), which is a computer specially used for industrial automation control, has the characteristics of high reliability, strong anti-interference ability, and flexible programming. It is widely used in automation control in industrial production, including mechanical control, process control, and motion control. It is simple to program, easy to maintain, and highly reliable, and is suitable for a variety of industrial environments.
[0039] Second, industrial PC (IPC), industrial PC has strong computing power and flexible interface configuration, and can handle complex control and data processing tasks. It is suitable for scenarios that require high computing power and complex control logic, such as real-time data acquisition, complex motion control, and advanced human-machine interface (HMI) applications. It has strong computing power and good scalability, and can run complex control algorithms and software.
[0040] As an implementation mode, when the product is a special-shaped product, the printer controller obtains the surface data information of the surface contour of the preset printing area, and controls the nozzle to move along the preset printing path according to the surface data information of the surface contour. Specifically, special-shaped products may be those products with irregular shapes and without common standard geometric shapes. These products may have complex and unique shapes, for example, with special curves, asymmetric structures, complex three-dimensional shapes, or be composed of a plurality of parts of different shapes. The printer controller may obtain the surface data information of the surface contour of the printing area through a sensor, a scanner or other measuring device. The surface data information of the surface contour may include data such as the height, curvature, and flatness of the printing area to plan the preset printing path.
[0041] Furthermore, controlling the nozzle to move along a preset printing path according to the surface data information of the surface profile includes the following steps: controlling the nozzle to maintain a constant distance from the surface to be sprayed of the preset special-shaped product according to the surface data information of the surface profile; and controlling the nozzle to move at a uniform speed along the preset printing path. Specifically, the surface to be sprayed of the special-shaped product is the surface where the preset printing area is located. Controlling the nozzle to maintain a constant distance from the surface to be sprayed of the special-shaped product can ensure that the polymer ink is evenly distributed on the entire surface, avoiding the problem of uneven polymer ink amount or leakage due to inconsistent distance. In addition, since the nozzle moves at a uniform speed along the preset printing path, the rate at which the polymer ink flows out is also consistent, avoiding the problem of polymer ink density difference or leakage due to uneven speed.
[0042] As an embodiment, controlling the nozzle to maintain a constant distance from the surface to be sprayed of the preset special-shaped product according to the surface data information of the surface profile includes the following steps: determining the preset distance between the nozzle and the surface to be sprayed of the special-shaped product according to the surface data information of the surface profile; obtaining multiple surface profile coordinates corresponding to the surface profile, each profile coordinate including coordinate information corresponding to different positions of the special-shaped product; based on a preset conversion rule, according to the preset distance, converting the multiple surface profile coordinates into corresponding trajectory paths. Wherein, the conversion rule can be a formula for converting the obtained multiple contour coordinates from points to lines. Further, since the glass surface to be printed is fixed on a preset fixture, after the fixture is moved to the printing station, the coordinates of the fixture can be obtained in advance, and the multiple surface contour coordinates corresponding to the surface profile can be determined by the coordinates of the fixture. In other embodiments, after the surface to be sprayed of the special-shaped product is determined to be scanned, a series of multiple surface contour coordinates can be obtained. After determining the multiple surface contour coordinates, based on the preset conversion rule, the multiple surface contour coordinate points are smoothly connected to form a continuous trajectory path, and then the formed continuous trajectory path is adjusted according to the preset distance.
[0043] Furthermore, when the printing area contains surface data information of the surface contour of straight lines and curves, the distance between the straight line and the nozzle and the distance between the curve and the nozzle are calculated, and the speed of the nozzle movement is determined according to the distance between the straight line and the nozzle and the distance between the curve and the nozzle, so as to control the nozzle to move at a uniform speed along the preset printing path. Specifically, when the nozzle prints ink on the surface of the product, the nozzle is parallel to the surface of the product, that is, the surface contour of the straight line contained in the printing area of the product surface is equal to the distance from the nozzle. However, the surface contour of the curve contained in the printing area of the product surface is not equal to the distance from the nozzle. Since the surface contour containing the curve is longer than the surface contour containing the curve, the nozzle needs to move a longer path when printing the contour of the surface containing the curve. Therefore, the nozzle needs to move faster when printing the contour of the surface containing the curve to control the nozzle to move at a uniform speed along the preset printing path.
[0044] Step S2: Pre-curing the polymer ink sprayed onto the surface of the product. Specifically, the polymer ink sprayed onto the surface of the product is a thermosetting ink. The thermosetting ink can be quickly cured after heating after spraying, so that the ink on the glass surface can quickly reach a state that can be subsequently operated and processed. Thermosetting ink is suitable for high-speed printing and application on production lines, which improves production efficiency. As an embodiment, the pre-curing of the polymer ink sprayed onto the surface of the product is thermal curing. Thermal curing is a processing technology widely used in the chemical industry and materials science fields. It is mainly used to cure (harden) materials or compounds so that the materials or compounds form a stable structure or chemical connection at high temperatures. In this embodiment, the degree of curing of the polymer ink sprayed onto the surface of the product is 15% to 30% of the full curing. At this degree of curing, the polymer ink remains in a semi-dry state and is not easy to flow, so that the position and shape of the polymer ink do not change.
[0045] In a specific embodiment, Figure 2 As shown, the pre-curing of the polymer ink printed on the surface of the product includes step S21: irradiating the polymer ink printed on the surface of the product with a UV light source with a wavelength of 365nm to 395nm. Specifically, the UV light source is a UVLED (ultraviolet light emitting diode), which has higher energy efficiency than traditional mercury lamps and consumes less electricity. In addition, the UVLED has a longer life, reducing the frequency of replacing the light source and maintenance costs. At the same time, the UVLED can be started and stopped instantly without preheating time, which helps to improve production efficiency. In addition, the UVLED can provide highly uniform ultraviolet light output, and can accurately control the light intensity and beam shape to adapt to different processing requirements and material properties. Furthermore, the light with a wavelength of 365nm to 395nm belongs to the UV-A band, and the light energy in the wavelength range of 365nm to 395nm is strong enough to effectively excite the polymer ink and enable the polymer ink to quickly start the curing reaction.
[0046] As an embodiment, the energy output by the UV light source is 800mj to 1200mj, the duration of the UV light source irradiating the polymer ink sprayed on the surface of the product is 0.1s to 0.2s, and the pre-curing duration of the polymer ink sprayed on the surface of the product is 5 minutes to 10 minutes. The degree of thermal curing of the polymer ink is controlled by controlling the energy output by the UV light source, the duration of irradiating the polymer ink, and the curing duration of the polymer ink, so that the degree of thermal curing of the polymer ink is 15% to 30% of complete curing. Exemplarily, the energy output by the UV light source is 1000mj, the duration of the UV light source irradiating the polymer ink is 0.15s, and the curing duration of the polymer ink is 7 minutes.
[0047] Step S3: In an oxygen-free environment, a low-band light source is selected to irradiate the pre-cured polymer ink. Specifically, in an oxygen-free environment, the presence of oxygen can be reduced. Since oxygen may interfere with the propagation of UV light or compete with the reactants in the polymer ink, removing or reducing oxygen can improve the efficiency and quality of UV curing. Furthermore, in an oxygen-free environment, after the pre-cured polymer ink is irradiated by a low-band light source, a low-gloss surface film layer will be formed on the surface of the polymer ink to reduce the glossiness of the polymer ink surface and solve the reflection problem caused by the high gloss of the polymer ink. It should be noted that the polymer ink in this embodiment is a UV nano-special polymer ink. After the pre-cured UV nano-special polymer ink is irradiated by a low-band light source in an oxygen-free environment, it can react with the light generated by the low-band light source, thereby forming a low-gloss surface film layer on the surface of the polymer ink.
[0048] As an embodiment, in an oxygen-free environment, selecting a low-band light source to irradiate the pre-cured polymer ink includes: selecting a low-band light source to irradiate the pre-cured polymer ink in an inert gas environment. Exemplary inert gases include nitrogen (N), helium (He), neon (Ne), argon (Ar), krypton (Kr), xenon (Xe) and radon (Rn). Preferably, the low-band light source is selected to irradiate the pre-cured polymer ink in a nitrogen environment.
[0049] As an implementation method, Figure 2 As shown, in an oxygen-free environment, selecting a low-band light source to irradiate the pre-cured polymer ink includes step S31: in an oxygen-free environment, selecting a UV light source with a wavelength of 172nm to 260nm to irradiate the pre-cured polymer ink. Specifically, the light with a wavelength of 172nm to 260nm belongs to the UV-C band, and the light in the UV-C band has stronger energy than the light in the UV-A band, so that the surface of the polymer ink forms a low-gloss surface film layer.
[0050] As an embodiment, the low-band light source irradiates the pre-cured polymer ink for 0.2s to 0.5s. The longer the low-band light source irradiates the pre-cured polymer ink, the lower the glossiness of the surface film formed on the surface of the polymer ink.
[0051] As an implementation method, Figure 3As shown, the method for reducing the surface glossiness of polymer ink of the present invention further includes step S32: placing the polymer ink irradiated by the low-band light source in an oxygen-free environment for 10 to 20 minutes. Exemplarily, the polymer ink irradiated by the low-band light source is placed in an oxygen-free environment for 15 minutes. Specifically, step S32 is located after step S3 and before step S4, and step S31 is used to make the surface film layer with low glossiness formed on the surface of the polymer ink more stable.
[0052] In a specific embodiment, in a pure nitrogen environment, a low-band light source is selected to irradiate the pre-cured polymer ink, the low-band light source is a UVLED with a light emission wavelength of 172nm to 260nm, the energy output by the low-band light source is 1500mj to 2500mj, and the duration of the low-band light source irradiating the pre-cured polymer ink is 0.2s to 0.5s. The glossiness of the low-gloss surface film layer formed on the surface of the polymer ink is controlled by controlling the energy output by the low-band light source, the light emission wavelength of the low-band light source, and the duration of irradiating the pre-cured polymer ink. Exemplarily, the low-band light source is a UVLED with a light emission wavelength of 220nm, the energy output by the low-band light source is 2000mj, and the duration of the low-band light source irradiating the pre-cured polymer ink is 0.3s.
[0053] Furthermore, the thickness of the polymer ink sprayed onto the product surface by the nozzle of the inkjet printer is 10 microns to 15 microns. In a specific embodiment, the thickness of the polymer ink sprayed onto the product surface by the nozzle of the inkjet printer is 13 microns.
[0054] Step S4: Completely solidify the polymer ink after being irradiated by the low-band light source. As an embodiment, the polymer ink after being irradiated by the low-band light source is completely solidified by a UV light source. The UV light source may be a UVLED or other UV light sources. The emission wavelength may be 365nm to 395nm or other ranges of emission wavelengths.
[0055] The beneficial effect of the technical solution of the present invention is that: when the ink has not yet solidified, a low-band light source is selected to irradiate the surface of the polymer ink in an oxygen-free environment, so that a low-gloss surface film layer is produced on the surface of the polymer ink, thereby reducing the glossiness of the polymer ink surface and solving the reflection problem caused by the excessive glossiness of the polymer ink.
[0056] The above are only partial or preferred embodiments of the present invention. Neither the text nor the drawings can limit the scope of protection of the present invention. All equivalent structural changes made by using the contents of the present invention specification and drawings under the overall concept of the present invention, or direct / indirect application in other related technical fields are included in the scope of protection of the present invention.
Claims
1. A method for reducing the surface gloss of a polymer ink, characterized in that: include: Print polymer ink onto the product surface; Pre-curing the polymer ink sprayed onto the surface of the product; In an oxygen-free environment, a low-band light source is used to irradiate the pre-cured polymer ink; The polymer ink is completely cured after being irradiated by a low-wavelength light source.
2. The method for reducing the surface glossiness of polymer ink according to claim 1, characterized in that: The step of selecting a low-band light source to irradiate the pre-cured polymer ink in an oxygen-free environment comprises: In an inert gas environment, a low-band light source is selected to irradiate the pre-cured polymer ink.
3. The method for reducing the surface glossiness of polymer ink according to claim 1, characterized in that: The step of selecting a low-band light source to irradiate the pre-cured polymer ink in an oxygen-free environment comprises: In an oxygen-free environment, a UV light source with a wavelength of 172 nm to 260 nm is selected to irradiate the pre-cured polymer ink.
4. The method for reducing the surface glossiness of polymer ink according to claim 1, characterized in that: The low-band light source irradiates the pre-cured polymer ink for a period of 0.2s to 0.5s.
5. The method for reducing the surface glossiness of polymer ink according to claim 1, characterized in that: In an oxygen-free environment, a low-band light source is used to irradiate the pre-cured polymer ink: The polymer ink irradiated with the low-band light source is placed in an oxygen-free environment for 10 to 20 minutes.
6. The method for reducing the surface glossiness of polymer ink according to claim 1, characterized in that: The pre-curing of the polymer ink sprayed onto the surface of the product comprises: The polymer ink sprayed onto the surface of the product is irradiated by a UV light source with a wavelength of 365nm to 395nm.
7. The method for reducing the surface glossiness of polymer ink according to claim 6, characterized in that: The energy output by the UV light source is 800mj to 1200mj.
8. The method for reducing the surface glossiness of polymer ink according to claim 1, characterized in that: The degree of pre-curing of the polymer ink sprayed onto the product surface is 15% to 30% of the degree of full curing.
9. The method for reducing the surface glossiness of polymer ink according to claim 1, characterized in that: The step of printing the polymer ink onto the product surface comprises: The polymer ink is sprayed onto the surface of the product through the nozzle of the inkjet printer with a thickness of 10 to 15 microns.
10. The method for reducing the surface glossiness of polymer ink according to claim 1, characterized in that: The polymer ink sprayed onto the product surface is pre-cured for 5 to 10 minutes.