Method for shielding cathode roller by using memory polymer material

By using shape memory polymer materials and polyurethane modified acrylate adhesives, the problems of complex operations and waste of resources during the cathode roller shielding process are solved, and efficient and low-cost copper foil production and shielding effect are achieved.

CN118979293APending Publication Date: 2024-11-19NANJING LONGDIAN HUAXIN NEW ENERGY MATERIALS IND TECH RES INST CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202411052630.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-01
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

In the prior art, the cathode roller shielding process is complex and uncontrollable, especially when using liquid or solid epoxy resins, it requires regulation and metering control, resulting in high production costs and waste of resources.

Method used

The shape memory polymer material is used as the shielding material. After preparation and molding, it is stored at a specific temperature and then restored to the original shape by thermal, light and chemical action when needed. The edge sealing is used with polyurethane modified acrylic adhesive. deal with.

Benefits of technology

The preparation of copper foils with different widths is achieved without the need to replace the cathode rollers, which reduces production costs, improves construction efficiency, reduces resource waste, and extends the use cycle of the shielding layer through edge sealing treatment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118979293A_ABST
    Figure CN118979293A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of electrolytic copper foil, in particular to a method for shielding a cathode roller by using a memory polymer material, which comprises the following steps of: 1, selecting a shape memory polymer material as a shielding material; 2, preparing the shape memory high polymer material into a required shape or size; 3, at the specific temperature, the shielding material is stored and packaged into a shape convenient to transport; step 4, covering the shielding material to an area needing to be subjected to cathode shielding; and step 5, restoring the shape of the shielding material to the shape during preparation and molding through thermal, optical and chemical actions and the like. The selected edge sealing material is a polyurethane modified acrylate adhesive and can be simply and conveniently obtained from the market, and the edge sealing treatment is relatively simple, easy to operate and easy to peel off and does not damage the cathode roller.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of electrolytic copper foil, in particular to a method for realizing cathode roller shielding by using memory polymer material. Background Art

[0002] Electrolytic copper foil is an important electronic material. It is a copper-clad product formed by depositing pure copper metal on a substrate by electrolysis. Electrolytic copper foil is a metal foil with very high electrical conductivity, thermal conductivity and strength. It is an important material for the manufacture of copper clad laminates (CCLs), printed circuit boards (PCBs), and lithium-ion batteries. In today's rapidly developing electronic information industry, electrolytic copper foil is called the "neural network" for signal and power transmission and communication of electronic products. A pure copper block is placed at the negative electrode, and a substrate (usually a polyimide film) is placed at the positive electrode, and then they are immersed in an electrolyte solution. By applying voltage to the electrodes, copper ions are reduced to metallic copper at the positive electrode, and then deposited on the substrate to form a layer of copper foil. The thickness of the electrolytic copper foil is generally between 5-70um, and the density is 8.9g / cm 3 , high surface flatness, good finish, the chemical properties of electrolytic copper foil are stable, not easy to oxidize, and can maintain good surface and conductive properties for a long time. At the same time, it has high thermal stability, can withstand high temperature heating, and is not easy to react chemically, is not affected by solvents and acidic environments, and is easy to process. Electrolytic copper foil can be processed in a variety of ways, including stamping, chemical etching, copper coating and other treatments. Due to its excellent mechanical properties and thermal stability, electrolytic copper foil is suitable for complex processing technology and can meet the needs of different fields. The manufacturing process of electrolytic copper foil mainly includes four major processes: copper dissolution, raw foil, post-processing and slitting. Among them, raw foil is the core process, involving steps such as electrolyte preparation and copper ion electrodeposition on the surface of the cathode roller to form raw foil. Post-processing is to carry out surface treatment processes such as pickling and organic anti-oxidation on the raw foil to meet customer requirements. Slitting is to cut, inspect and package according to customer requirements for the quality, width, weight and other requirements of copper foil. With the continuous development of the electronic information industry and the new energy field, the market demand for electrolytic copper foil will continue to grow. At the same time, with the continuous advancement of technology and continuous optimization of processes, the performance and quality of electrolytic copper foil will continue to improve to meet more demanding application scenarios;

[0003] In the art, special tapes, inks, common insulating coatings, etc. are selected to shield the cathode before electrodeposition of raw foil. The shielding material disclosed in the patent with announcement number CN 115094487U is an epoxy resin shielding layer. In specific implementation, liquid epoxy resin needs to be regulated, or when solid epoxy is selected, metering control and softening and casting processes are required. The operation of this process is slightly complicated and uncontrollable. In view of the above problems, a method for shielding the cathode roller using a memory polymer material is provided. Summary of the invention

[0004] The purpose of the present invention is to provide a method for shielding a cathode roller using a memory polymer material to solve the problems raised in the above background technology. To achieve the above purpose, the present invention provides the following technical solution: A method for shielding a cathode roller using a memory polymer material comprises the following steps:

[0005] Step 1, selecting a shape memory polymer material as a masking material;

[0006] Step 2, preparing the shape memory polymer material into a desired shape or size;

[0007] Step 3, at a specific temperature, packing the shielding material into a shape that is convenient for transportation;

[0008] Step 4, covering the area where cathode shielding is required with the shielding material;

[0009] Step 5, restoring the morphology of the masking material to the shape when it was prepared and formed through heat, light, chemical action, etc.;

[0010] Step 6, selecting an appropriate adhesive as the edge sealing material and applying the adhesive evenly and neatly to the edge of the polymer memory material forming the shield with the help of a special tool;

[0011] Step seven, using a UV curing machine to cure and cross-link the adhesive to form a good edge sealing effect and deposit raw copper to destroy the shielding effect of the shielding material.

[0012] Preferably, the shape memory polymer material is a polyurethane shape memory polymer material.

[0013] Preferably, the shape memory polymer material recovers its shape in 5 minutes at a temperature of 60 degrees Celsius.

[0014] Preferably, the shape fixing temperature of the shape memory polymer material is 80 degrees Celsius.

[0015] Preferably, in step 2, the shape memory polymer material is prepared into a cylindrical shape with a diameter of 2700 mm.

[0016] Preferably, the specific temperature in step three is 80 degrees Celsius.

[0017] Preferably, the shape for easy storage and transportation is a ring with a diameter of 50 cm.

[0018] Preferably, the shielding area of ​​the cathode roller has a diameter of 2700 mm and a width of 300 mm.

[0019] Preferably, the thermal action temperature in step five is 60 degrees Celsius.

[0020] Preferably, the adhesive in step six is ​​a polyurethane modified acrylate adhesive.

[0021] Compared with the prior art, the present invention has the following beneficial effects:

[0022] The present invention can prepare copper foils of different widths by using special shielding materials to shield the cathode roller, and there is no need to replace the cathode roller, thereby greatly reducing the production cost. At the same time, since the shielding material of the present invention has the characteristics of shape memory effect, high restoring force and low density, it is convenient for construction and application, further reducing the production cost. The shielding material of the present invention can be unfolded and covered to the area where cathode shielding is required under the action of external force, and its morphology can be restored to the shape at the time of preparation and molding through heat, light, chemical action, etc., so that it is tightly attached to the cathode roller shielding area. This design makes the cathode shielding construction process more efficient and improves production efficiency. Reduce resource waste: The shielding material of the present invention can be prepared into the required shape or size according to demand, avoiding a large amount of waste of raw materials, energy and production costs due to mismatch of copper foil width, and realizing effective utilization of resources. In order to achieve a longer and more durable shielding effect, the edge sealing glue can be used to form an efficient edge sealing, so that the shielding layer has a good shielding effect for a longer period in the electroplating liquid environment, which can overcome the shortcomings of the existing technology, is easy to operate, and has good environmental friendliness. This solution uses a shape memory material with high resilience to shield the cathode roller. This shielding material has the characteristics of shape memory effect, high resilience and low density. During preparation, it can be formed into the required shape or size according to needs; for easy storage and transportation, it is stored and packaged into a shape that is convenient for transportation at a specific temperature; when it is used, it can be unfolded and covered to the area where the cathode shielding is required under the action of external force, and its morphology is restored to the shape when it was prepared through heat, light, chemical action, etc., so that it is tightly covered on the cathode roller shielding area. The selected edge sealing material is a polyurethane modified acrylic adhesive, which can be easily obtained from the market, and the edge sealing treatment is relatively simple, easy to operate, and easy to peel off without damaging the cathode roller. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 This is a flowchart of a method for realizing cathode roller shielding using memory polymer materials according to the present invention;

[0024] Figure 2 This is an implementation diagram of a method for realizing cathode roller shielding using memory polymer materials according to the present invention. DETAILED DESCRIPTION

[0025] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technical personnel in this field without creative work are within the scope of protection of the present invention.

[0026] See also Figure 1 to Figure 2 The present invention provides a technical solution: a method for realizing cathode roller shielding using memory polymer material, comprising the following steps:

[0027] Step 1, selecting a shape memory polymer material as a masking material;

[0028] Step 2, preparing the shape memory polymer material into a desired shape or size;

[0029] Step 3, at a specific temperature, the shielding material is packed into a shape that is convenient for transportation;

[0030] Step 4, covering the area requiring cathode shielding with a shielding material;

[0031] Step 5, the morphology of the masking material is restored to the shape when it was prepared and formed through heat, light, chemical action, etc.;

[0032] Step 6, selecting an appropriate adhesive as the edge-sealing material and applying the adhesive uniformly and neatly to the edge of the high-molecular memory material forming the shield with the aid of a special tool, wherein the adhesive is a polyurethane-modified acrylate adhesive, which is an advanced adhesive combining the advantages of polyurethane and acrylate, and has a wide range of application prospects and excellent performance. As the name implies, the polyurethane-modified acrylate adhesive is a new type of adhesive obtained by modifying polyurethane and acrylate, which combines the high strength, wear resistance, oil resistance, chemical corrosion resistance and other characteristics of polyurethane with the excellent film-forming property, weather resistance, water resistance and other characteristics of acrylate, forming an adhesive with superior comprehensive performance;

[0033] Step seven, use a UV curing machine to cure and cross-link the adhesive to form a good edge sealing effect and deposit raw copper to destroy the shielding effect of the shielding material. UV curing technology is a curing method based on photochemical reaction. Under the irradiation of UV light, the photoinitiator (or photosensitizer) in the curing material absorbs ultraviolet light to produce active free radicals or cations, which in turn trigger chemical reactions such as monomer polymerization, cross-linking and grafting, so that the adhesives, coatings and other materials that were originally in liquid state are transformed into solid in a very short time. This process is usually called "light curing" or "UV curing". The UV curing process usually only takes a few seconds to a few minutes, which greatly improves production efficiency. Compared with traditional thermal curing or natural curing methods, UV curing can significantly shorten the production cycle. UV curing process No solvent is needed in the process, which reduces the emission of volatile organic compounds (VOC) and meets environmental protection requirements. At the same time, UV light sources have high energy efficiency and relatively low energy consumption. UV-cured materials have excellent physical properties and chemical stability, such as high hardness, high wear resistance, and good weather resistance. In addition, UV-cured materials also have good optical properties and bonding strength. UV curing technology can be applied to a variety of materials, including glass, metal, plastic, etc., and can be closely integrated with automated production lines to achieve efficient and accurate curing operations. UV ultraviolet curing equipment usually includes light source systems, reflection systems, cooling systems, and transmission systems. The light source is the core component of UV curing equipment. Commonly used light sources include UV lamps (such as medium-pressure mercury lamps, high-pressure mercury lamps, etc.) and UV LED light source, UV LED light source has the advantages of high energy efficiency, long life, and environmental protection, and has gradually become the mainstream light source in the field of UV curing. UV light has a certain harmful effect on the human body, so protective glasses and gloves and other protective equipment need to be worn during operation. The selection of UV curing materials should be based on specific application scenarios and needs to ensure the curing effect and product quality. The effect of UV curing is affected by multiple factors such as light source intensity, irradiation time, material thickness, etc., so it is necessary to adjust the curing conditions according to actual conditions to obtain the best curing effect;

[0034] The present invention uses a special shielding material to shield the cathode roller, so that copper foils of different widths can be prepared without replacing the cathode roller, thereby greatly reducing the production cost. At the same time, since the shielding material of the present invention has the characteristics of shape memory effect, high restoring force and low density, it is convenient for construction and application, further reducing the production cost. The shielding material of the present invention can be unfolded and covered to the area requiring cathode shielding under the action of external force, and its morphology can be restored to the shape at the time of preparation and molding through heat, light, chemical action, etc., so that it is tightly covered on the cathode roller shielding area. This design makes the cathode shielding construction process more efficient, improves production efficiency, and reduces resource waste: the shielding material of the present invention can be prepared into the required shape or size according to demand, avoiding a large amount of raw materials, energy and production cost waste caused by mismatch of copper foil width, realizing effective utilization of resources, and achieving a longer and more durable shielding effect. , it can be treated with edge sealing glue to form efficient edge sealing, so that the shielding layer has a good shielding effect for a longer period in the electroplating solution environment, can overcome the shortcomings of the existing technology, and is easy to operate and environmentally friendly. This scheme uses a shape memory material with high resilience to shield the cathode roller. The shielding material has the characteristics of shape memory effect, high resilience and low density. During preparation, it can be formed into the required shape or size according to needs; for the convenience of storage and transportation, it is stored and packaged into a shape that is convenient for transportation at a specific temperature; when it is used, it can be unfolded and covered to the area where cathode shielding is required under the action of external force, and its morphology can be restored to the shape when it was prepared through heat, light, chemical action, etc., so that it is tightly covered on the cathode roller shielding area. The selected edge sealing material is a polyurethane modified acrylic adhesive, which can be easily obtained on the market, and the edge sealing treatment is relatively simple, easy to operate, and easy to peel off without damaging the cathode roller.

[0035] In this embodiment, the shape memory polymer material is a polyurethane shape memory polymer material. Polyurethane shape memory polymer material (abbreviated as polyurethane SMP) is a new type of functional polymer material with unique shape memory properties. Polyurethane SMP refers to an intelligent material that can be deformed to a temporary shape under certain conditions and restore to its original shape under external stimuli (such as temperature, current, magnetic field, ultraviolet light, etc.). It combines the properties of plastics and rubbers, and has the advantages of high elasticity, good biocompatibility and degradability. The preparation technology of polyurethane SMP includes a variety of methods, such as in-situ polymerization, blending, etc. By selecting appropriate raw materials and process conditions, polyurethane SMPs with different properties and uses can be prepared. For example, using boric acid as a chain extender can enhance the mechanical properties and shape memory properties of polyurethane SMP. With its biocompatibility and degradability, it can be used to make medical devices, implants, etc. In the manufacture of aircraft, rockets and other spacecraft, polyurethane SMP can be used to make deformable parts to improve the adaptability and safety of aircraft. In the fields of flexible screens and wearable devices, polyurethane SMP can be used to make bendable and foldable circuit boards and connectors. With its shape memory properties, intelligent regulation and precise control of robots can be achieved. With the continuous deepening of research on polyurethane SMP and the continuous advancement of technology, its application field will continue to expand. In the future, polyurethane SMP is expected to play an important role in more fields and make greater contributions to scientific and technological progress and social development.

[0036] In this embodiment, the shape memory polymer material takes 5 minutes to recover its shape at a temperature of 60 degrees Celsius.

[0037] In this embodiment, the shape fixing temperature of the shape memory polymer material is 80 degrees Celsius.

[0038] In this embodiment, the shape memory polymer material in step 2 is prepared into a cylindrical shape with a diameter of 2700 mm.

[0039] In this embodiment, the specific temperature in step three is 80 degrees Celsius.

[0040] In this embodiment, the shape that is convenient for storage and transportation is a cylinder with a diameter of 50 cm.

[0041] In this embodiment, the shielding area of ​​the cathode roller has a diameter of 2700 mm and a width of 300 mm.

[0042] In this embodiment, the heat action temperature in step five is 60 degrees Celsius.

[0043] In this embodiment, the adhesive in step six is ​​a polyurethane modified acrylate adhesive. The polyurethane modified acrylate adhesive is an advanced adhesive that combines the advantages of polyurethane and acrylate, and has broad application prospects and excellent performance. As the name suggests, the polyurethane modified acrylate adhesive is a new type of adhesive obtained by modifying polyurethane and acrylate. It combines the high strength, wear resistance, oil resistance, chemical corrosion resistance and other characteristics of polyurethane with the excellent film-forming property, weather resistance, water resistance and other characteristics of acrylate, forming an adhesive with excellent comprehensive performance. The polyurethane modified acrylate adhesive The raw materials of the adhesive mainly include polyurethane, acrylate monomer, initiator, emulsifier, solvent, etc. The specific formula will be adjusted according to different application needs and performance requirements. For example, in some formulas, the content of polyurethane may be between 10% and 35%, and the acrylate monomer is the main component, which may account for up to 100% or more. In addition, in order to adjust the viscosity and stability of the adhesive, an appropriate amount of solvent and other additives will be added. The preparation process of polyurethane modified acrylate adhesive is relatively complicated, but it can be roughly divided into the following steps. First, the raw materials of polyurethane (such as polyether polyol, isocyanate The step is the key to form a polyurethane skeleton. Acrylate monomers are added to the prepolymers, and the acrylate monomers and the polyurethane prepolymers are chemically reacted by free radical polymerization or graft copolymerization to form polyurethane-modified acrylate copolymers. In order to obtain water-based adhesives, the copolymers are usually emulsified. In this step, emulsifiers and an appropriate amount of water are added, and the copolymers are dispersed in water to form an emulsion by high-speed stirring or ultrasonic waves. Finally, the emulsions are filtered, the viscosity is adjusted, and other post-treatment operations are performed to obtain polyurethane-modified acrylate adhesives that meet the requirements. In the process of automobile manufacturing, polyurethane modified acrylate adhesives can be used in the bonding, sealing and painting of the car body to improve the overall performance and aesthetics of the car. In the field of architectural decoration, the adhesive can be used for the pasting and fixing of materials such as tiles, floors, and wallpapers, and has excellent bonding strength and durability. In the process of furniture manufacturing, polyurethane modified acrylate adhesives can be used for the bonding and assembly of materials such as wood and artificial boards to improve the stability and aesthetics of furniture. In the field of electronics and electrical appliances, the adhesive can be used in the bonding and packaging of electronic components, and has good insulation and high temperature resistance.

[0044] The use method and advantages of the present invention: When in use, the working process is as follows:

[0045] The cathode roller is shielded by a special shielding material: first, a shape memory polymer material with high restoring force is selected as the shielding material. This material has the characteristics of shape memory effect, high restoring force and low density. Then, the material is formed into the required shape or size according to the needs, so as to adapt to the process of producing foils with different widths. At a specific temperature, the shielding material is stored and packaged into a shape that is convenient for transportation. When it is needed, it is quickly unfolded to cover the area where the cathode shielding is required. When the shielding material is covered on the shielding area of ​​the cathode roller, we can restore its morphology to the shape at the time of preparation and molding through heat, light, chemical action, etc., so that it is closely attached to the shielding area of ​​the cathode roller. The edge of the memory material after shielding can be treated with acid-resistant edge sealing glue to prevent liquid seepage, so that the shielded cathode roller can be used for a longer time. Based on the above, the width can be changed without changing the cathode roller to prepare copper foils of different widths; at the same time, the waste of raw materials, energy and production costs caused by the mismatch of the copper foil width is reduced, and production efficiency is improved.

[0046] The above shows and describes the basic principles, main features and advantages of the present invention. Technical personnel in this industry should understand that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only preferred examples of the present invention and are not used to limit the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention to be protected. The scope of protection of the present invention is defined by the attached claims and their equivalents.

Claims

1. A method for realizing cathode roller shielding using memory polymer material, characterized in that: The steps include: Step 1, selecting a shape memory polymer material as a masking material; Step 2, preparing the shape memory polymer material into a desired shape or size; Step 3, at a specific temperature, packing the shielding material into a shape that is convenient for transportation; Step 4, covering the area where cathode shielding is required with the shielding material; Step 5, restoring the morphology of the masking material to the shape when it was prepared and formed through heat, light, chemical action, etc.; Step 6, selecting an appropriate adhesive as the edge sealing material and applying the adhesive evenly and neatly to the edge of the polymer memory material forming the shield with the help of a special tool; Step seven, using a UV curing machine to cure and cross-link the adhesive to form a good edge sealing effect and deposit raw copper to destroy the shielding effect of the shielding material.

2. A method for realizing cathode roller shielding using memory polymer material according to claim 1, characterized in that: The shape memory polymer material is a polyurethane shape memory polymer material.

3. A method for realizing cathode roller shielding using memory polymer material according to claim 1, characterized in that: The shape memory polymer material can recover its shape in 5 minutes under the temperature condition of 60 degrees Celsius.

4. A method for realizing cathode roller shielding using memory polymer material according to claim 1, characterized in that: The shape-fixing temperature of the shape memory polymer material is 80 degrees Celsius.

5. The method for realizing cathode roller shielding using memory polymer material according to claim 1, characterized in that: In the step 2, the shape memory polymer material is prepared into a ring shape with a diameter of 2700 mm.

6. The method for realizing cathode roller shielding using memory polymer material according to claim 1, characterized in that: The specific temperature in step three is 80 degrees Celsius.

7. The method for realizing cathode roller shielding using memory polymer material according to claim 1, characterized in that: The shape that is convenient for storage and transportation is a circular ring with a diameter of 50 cm.

8. The method for realizing cathode roller shielding using memory polymer material according to claim 1, characterized in that: The shielding area of ​​the cathode roller has a diameter of 2700 mm and a width of 300 mm.

9. The method for realizing cathode roller shielding using memory polymer material according to claim 1, characterized in that: The heat action temperature in step 5 is 60 degrees Celsius.

10. The method for realizing cathode roller shielding using memory polymer material according to claim 1, characterized in that: The adhesive in step six is ​​a polyurethane modified acrylate adhesive.

Citation Information

Patent Citations

  • Novel shielding material for electrolytic copper foil and use method

    CN115094487A