Double-sided packaging structure of hybrid memory chip and preparation method thereof

By stacking multi-layer chips in the double-sided packaging structure of the memory chip and making RDL layers, the interconnection between chips is achieved, which solves the problem that traditional packaging methods cannot meet the needs of high performance, high density and miniaturization, and improves the reliability of the chips and I/O density and reduce manufacturing costs.

CN118983292APending Publication Date: 2024-11-19JIANGSU SILICON INTEGRITY SEMICON TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410972312.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-19
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

Traditional memory chip packaging methods cannot meet the needs of modern electronic products for high performance, high density and miniaturization, and the complex manufacturing process leads to high manufacturing costs and reliability impacts.

Method used

Using a double-sided packaging structure of hybrid memory chips, multi-layer chips are stacked on both sides of the substrate, and RDL layers are made on the surface of the plastic seal to realize the interconnection between the chips. The substrate and RDL layers are interconnected by conductive columns to form an integral interconnection. structure.

Benefits of technology

It achieves the stability and reliability of the chip and improves I/O density, meets the high performance, high density and miniaturization needs of modern electronic products, while reducing manufacturing costs and expanding the scope of application of packaging structures.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118983292A_ABST
    Figure CN118983292A_ABST
Patent Text Reader

Abstract

According to the technical scheme, the double-face packaging structure of the hybrid storage chip comprises a substrate, first chips are welded to the front face and the back face of the substrate, second chips are welded to the surfaces of the first chips, a plurality of metal protruding blocks are arranged on the surfaces of the second chips, the first chips are electrically connected with the substrate through welding wires, and the metal protruding blocks are electrically connected with the substrate through welding wires. Plastic packaging bodies covering the first chip, the second chip and the bonding wires are arranged on the front face and the back face of the substrate, conductive columns used for leading out circuits of the substrate to the surfaces of the plastic packaging bodies are arranged on the plastic packaging bodies, RDL layers used for connecting metal protruding blocks on the surfaces of the second chip and the conductive columns are arranged on the surfaces of the plastic packaging bodies, and solder balls are arranged on the surface of one RDL layer. The multiple layers of chips are stacked on the front face and the back face of the substrate, the RDL layer is manufactured on the surface of the plastic package body, interconnection between the metal protruding blocks on the second chip and the RDL layer and interconnection between the first chip and the substrate are achieved, the substrate and the RDL layer are interconnected through the conductive columns, and overall interconnection between the multiple chips on the front face and the back face is achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of memory chips, in particular to a double-sided packaging structure of a hybrid memory chip and a preparation method thereof. Background Art

[0002] Memory chips are the specific application of the concept of embedded system chips in the storage industry. Therefore, whether it is a system chip or a memory chip, it is achieved by embedding software in a single chip to achieve multi-function and high performance, as well as support for multiple protocols, multiple hardware and different applications.

[0003] In the field of semiconductor integrated circuit manufacturing, memory chip packaging technology is an important link. The traditional memory chip packaging method is mainly a positive stacking plus a wire bonding structure. This structure is simple and easy, but due to its relatively single structure type, it can no longer meet the needs of modern electronic products for high performance, high density, and miniaturization. In addition, existing packaging technology often requires complex manufacturing processes, which not only increases manufacturing costs, but may also affect product reliability. Summary of the invention

[0004] In view of the deficiencies in the prior art, an object of the present invention is to provide a double-sided packaging structure of a hybrid memory chip and a preparation method thereof.

[0005] In order to achieve the above object, the technical solution of the present invention is as follows:

[0006] A double-sided packaging structure of a hybrid memory chip comprises a substrate, wherein metal circuits are arranged on the surface and inside of the substrate, and vertical metal columns are arranged inside the substrate 1 for conducting the front and back sides of the substrate, chip 1 is welded on both the front and back sides of the substrate, chip 2 is welded on the surface of chip 1, a plurality of metal bumps are arranged on the surface of chip 2, chip 1 is electrically connected to the substrate via welding wires, plastic packaging bodies covering chip 1, chip 2 and welding wires are arranged on both the front and back sides of the substrate, conductive columns for leading the substrate circuits to the surface of the plastic packaging body are arranged on the plastic packaging body, an RDL layer for interconnecting the metal bumps on the surface of chip 2 and the conductive columns is arranged on the surface of the plastic packaging body, and a solder ball is arranged on the surface of one of the RDL layers.

[0007] Preferably, the thickness of the substrate is set to 200-400um.

[0008] Preferably, the chip 1 and the chip 2 are in a stepped shape.

[0009] Preferably, the diameter of the metal bumps on the second surface of the chip is set to 40-100 um, and the spacing between the metal bumps on the second surface of the chip is set to 80-200 um.

[0010] Preferably, the diameter of the conductive column is set to 100-200 um, and the conductive column is set to a metal copper column or a conductive glue column.

[0011] Preferably, the line width of the RDL layer is set to 2-20 um, the line spacing of the RDL layer is set to 2-20 um, and the lines of the RDL layer are arranged in 2-6 layers.

[0012] Preferably, the diameter of the solder ball is set to 120-300um.

[0013] The present invention also provides a method for preparing the above hybrid memory chip double-sided packaging structure, comprising the following steps:

[0014] S1, prepare the substrate, solder chip 1 to the substrate with DAF or silver glue on both sides of the substrate, and solder chip 2 with metal bumps on the surface of chip 1 to chip 1 with DAF or silver glue on the surface of chip 1;

[0015] S2, bonding wires between the front and back surfaces of the substrate and the chip 1 to form bonding wires, so that the chip 1 and the substrate are electrically connected;

[0016] S3, using epoxy resin to perform plastic sealing on both sides of the substrate to form a plastic sealing body covering chip 1, chip 2 and bonding wires;

[0017] S4, laser drilling is performed on the plastic packaging bodies on both sides of the substrate, the laser holes are connected to the internal circuits of the substrate, and conductive materials are filled in the laser holes to form conductive columns;

[0018] S5, grinding and thinning the plastic package body to expose the metal bumps of the chip 2;

[0019] S6, making an RDL layer on the surface of the plastic package body to interconnect the metal bumps of the second chip with the conductive pillars, and planting a solder ball on the surface of one of the RDL layers.

[0020] Preferably, metal copper is filled in the laser hole through an electroplating process to form a conductive column, and the conductive column is a metal copper column.

[0021] Preferably, a conductive glue is injected into the laser hole through a filling process to form a conductive column, and the conductive column is a conductive glue column.

[0022] Compared with the prior art, the present invention has the following beneficial effects:

[0023] 1. The present invention stacks multiple layers of chips on both the front and back sides of the substrate, and manufactures an RDL layer on the surface of the plastic package body, thereby realizing the interconnection between the metal bumps on the second chip and the RDL layer, the interconnection between the first chip and the substrate, and then the substrate and the RDL layer are interconnected through conductive pillars, and finally realizing the overall interconnection structure between the multiple chips on the front and back sides, thereby stabilizing the chip reliability and improving the I / O density of the memory chip. This structure not only meets the requirements of modern electronic products for high performance, high density, and miniaturization, but also has higher integration and smaller volume than the traditional positive stacking and wire bonding structure;

[0024] 2. The packaging process of the present invention mainly includes the steps of chip stacking, plastic sealing, wafer thinning, RDL layer preparation and solder ball planting, etc. These steps are relatively simple and easy to perform, which greatly reduces the manufacturing cost;

[0025] 3. The memory chip packaging structure of the present invention can be applied not only to memory chips, but also to other types of semiconductor integrated circuits, and has a large scope of application and thus has broad application prospects. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] The disclosure of the present invention is described with reference to the accompanying drawings. It should be understood that the drawings are only for illustrative purposes and are not intended to limit the scope of protection of the present invention. In the drawings, the same reference numerals are used to refer to the same components. Among them:

[0027] Figure 1 is a schematic structural diagram of a substrate of the present invention;

[0028] Figure 2 It is a schematic diagram of the structure of chip 1 and chip 2 of the present invention;

[0029] Figure 3 It is a structural schematic diagram of the welding wire of the present invention;

[0030] Figure 4 It is a structural schematic diagram of the plastic package body of the present invention;

[0031] Figure 5 It is a schematic structural diagram of the conductive column of the present invention;

[0032] Figure 6 It is a structural schematic diagram of the RDL layer of the present invention;

[0033] Figure 7 It is a schematic diagram of the overall structure of the present invention.

[0034] Notes in the figure: 1. Substrate; 2. Chip 1; 3. Chip 2; 4. Bonding wire;

[0035] 5. Plastic package; 6. Conductive column; 7. RDL layer; 8. Solder ball. DETAILED DESCRIPTION

[0036] It is easy to understand that according to the technical solution of the present invention, without changing the essential spirit of the present invention, a person skilled in the art can propose a variety of interchangeable structural modes and implementation modes. Therefore, the following specific implementation modes and drawings are only exemplary descriptions of the technical solution of the present invention, and should not be regarded as the whole of the present invention or as a limitation or restriction to the technical solution of the present invention.

[0037] like Figure 1 As shown, as a double-sided packaging structure of a hybrid memory chip of the present invention, it includes a substrate 1, the thickness of the substrate 1 is set to 300um, the surface and the inside of the substrate 1 have metal circuits, and vertical metal columns are also provided for conducting the front and back sides of the substrate 1, such as Figure 7 As shown, chip 1 2 is welded on both sides of substrate 1, metal pads are arranged around chip 1 2, chip 2 3 is welded on the surface of chip 1 2, chip 1 2 and chip 2 3 are stepped, and chip 1 2 and chip 2 3 are stacked up and down, a plurality of metal bumps are arranged on the surface of chip 2 3, the diameter of the metal bumps on the surface of chip 2 3 is set to 70um, and the spacing between the metal bumps on the surface of chip 2 3 is set to 140um, the metal pads around chip 1 2 are electrically connected to substrate 1 through welding wires 4, plastic sealing bodies 5 are arranged on both sides of substrate 1, the plastic sealing bodies 5 cover chip 1 2, chip 2 3 and welding wires 4, and the plastic sealing bodies 5 are provided on the front and back sides of substrate 1. The body 5 is provided with a conductive column 6 for leading the circuit of the substrate 1 to the surface of the plastic package body 5. The conductive column 6 is connected with the internal circuit of the substrate 1. The diameter of the conductive column 6 is set to 150um, and the conductive column 6 is set to a metal copper column or a conductive glue column. The surface of the plastic package body 5 is provided with an RDL layer 7 for interconnecting the metal bumps on the surface of the chip 23 and the conductive column 6. The line width of the RDL layer 7 is set to 11um, the line spacing of the RDL layer 7 is set to 11um, and the circuit of the RDL layer 7 is set to 4 layers, and a solder ball 8 is provided on the surface of one of the RDL layers 7, which is connected to the external circuit board through the solder ball 8, and the diameter of the solder ball 8 is set to 210um;

[0038] By stacking multiple layers of chips on both the front and back sides of the substrate 1 and making an RDL layer 7 on the surface of the plastic package 5, the metal bumps on the chip 2 3 and the RDL layer 7 are interconnected, the chip 1 2 is interconnected with the substrate 1, and then the substrate 1 and the RDL layer 7 are interconnected through the conductive column 6, finally realizing the overall interconnection structure between the multiple chips on the front and back sides, thereby stabilizing the chip reliability while also improving the I / O density of the storage chip. This structure not only meets the requirements of modern electronic products for high performance, high density and miniaturization, but also has higher integration and smaller size than the traditional upright stacking and wire bonding structure.

[0039] In addition, based on a double-sided packaging structure of a hybrid memory chip, the present invention also provides a method for preparing the double-sided packaging structure of a hybrid memory chip, comprising the following steps:

[0040] S1. Prepare substrate 1, such as Figure 2 As shown, chip 1 2 is welded to substrate 1 with DAF or silver glue on both sides of substrate 1, and chip 2 3 with metal bumps on the surface of chip 1 2 is welded to chip 1 2 with DAF or silver glue on the surface of chip 1 2;

[0041] S2, such as Figure 3 As shown, wires are bonded between the front and back sides of the substrate 1 and the metal pads around the chip 1 2 to form bonding wires 4, so that the chip 1 2 and the substrate 1 are electrically connected;

[0042] S3, such as Figure 4 As shown, epoxy resin is used to perform plastic encapsulation on both sides of the substrate 1 to form a plastic encapsulation body 5 covering the chip 1 2, the chip 2 3 and the bonding wire 4;

[0043] S4, such as Figure 5 As shown, laser drilling is performed on the plastic package body 5 on both sides of the substrate 1, the laser hole is connected with the internal circuit of the substrate 1, and a conductive material is filled in the laser hole to form a conductive column 6;

[0044] S5, such as Figure 5 As shown, the plastic package body 5 is polished and thinned to expose the metal bumps of the chip 2 3;

[0045] S6, such as Figure 6 As shown, an RDL layer 7 is formed on the surface of the plastic package 5 to interconnect the metal bumps of the chip 2 3 with the conductive pillars 6, and as shown in FIG. Figure 7 As shown, a solder ball 8 is implanted on the surface of one of the RDL layers 7 .

[0046] The conductive material can be filled in the laser hole by an electroplating process to fill metal copper in the laser hole to form a conductive column 6, where the conductive column 6 is a metal copper column. The conductive column 6 can also be formed by injecting conductive glue into the laser hole through a filling process, where the conductive column 6 is a conductive glue column, so that the circuit of the substrate 1 is led out to the surface of the plastic package 5 through the conductive column 6.

[0047] The packaging process mainly includes the steps of chip stacking, plastic sealing, grinding and thinning, making RDL layer 7 and solder ball planting 8. These steps are relatively simple and easy, which greatly reduces the manufacturing cost. Moreover, the memory chip packaging structure of the present invention can be applied not only to memory chips, but also to other types of semiconductor integrated circuits, and has broad application prospects. In the future, as electronic products have higher and higher requirements on performance, density and size, the packaging structure of the present invention is expected to become a mainstream packaging method.

[0048] The technical scope of the present invention is not limited to the contents in the above description. Those skilled in the art can make various deformations and modifications to the above embodiments without departing from the technical idea of ​​the present invention, and these deformations and modifications should all fall within the protection scope of the present invention.

Claims

1. A double-sided packaging structure of a hybrid memory chip, Features: The invention comprises a substrate (1), wherein metal circuits are arranged on the surface and inside of the substrate (1), and vertical metal columns are arranged inside the substrate (1) for conducting the front and back sides of the substrate (1), a chip (2) is welded on both the front and back sides of the substrate (1), a chip (3) is welded on the surface of the chip (2), a plurality of metal bumps are arranged on the surface of the chip (3), the chip (2) and the substrate (1) are electrically connected via welding wires (4), a plastic package (5) covering the chip (2), the chip (3) and the welding wires (4) are arranged on both the front and back sides of the substrate (1), a conductive column (6) for leading the circuit of the substrate (1) to the surface of the plastic package (5) is arranged on the plastic package (5), an RDL layer (7) for interconnecting the metal bumps on the surface of the chip (3) and the conductive column (6) is arranged on the surface of the plastic package (5), and a solder ball (8) is arranged on the surface of one of the RDL layers (7).

2. The double-sided packaging structure of a hybrid memory chip according to claim 1, Features: The thickness of the substrate (1) is set to 200-400 um.

3. The double-sided packaging structure of a hybrid memory chip according to claim 1, Features: The chip one (2) and the chip two (3) are in a stepped shape.

4. The double-sided packaging structure of a hybrid memory chip according to claim 1, Features: The diameter of the metal bumps on the surface of the second (3) chip is set to 40-100 um, and the spacing between the metal bumps on the surface of the second (3) chip is set to 80-200 um.

5. The double-sided packaging structure of a hybrid memory chip according to claim 1, Features: The diameter of the conductive column (6) is set to 100-200 um, and the conductive column (6) is set to be a metal copper column or a conductive rubber column.

6. The double-sided packaging structure of a hybrid memory chip according to claim 1, Features: The line width of the RDL layer (7) is set to 2-20 um, the line spacing of the RDL layer (7) is set to 2-20 um, and the lines of the RDL layer (7) are arranged in 2-6 layers.

7. The double-sided packaging structure of a hybrid memory chip according to claim 1, Features: The diameter of the solder ball (8) is set to 120-300 um.

8. A method for preparing the double-sided packaging structure of the hybrid memory chip according to any one of claims 1 to 7, It is characterized in that The steps include: S1, preparing the substrate (1), soldering the chip 1 (2) to the substrate (1) on both sides of the substrate (1) using DAF or silver glue, and soldering the chip 2 (3) with metal bumps on the surface of the chip 1 (2) to the chip 1 (2) using DAF or silver glue; S2, bonding wires (4) between the front and back surfaces of the substrate (1) and the chip one (2), so as to complete electrical connection between the chip one (2) and the substrate (1); S3, using epoxy resin to perform plastic encapsulation on the front and back sides of the substrate (1) to form a plastic encapsulation body (5) covering the chip 1 (2), the chip 2 (3) and the bonding wire (4); S4, laser drilling is performed on the plastic package (5) on both sides of the substrate (1), wherein the laser holes are connected to the internal circuit of the substrate (1), and a conductive material is filled in the laser holes to form conductive columns (6); S5, grinding and thinning the plastic package body (5) to expose the metal bumps of the second chip (3); S6, making an RDL layer (7) on the surface of the plastic package (5) so that the metal bumps of the second chip (3) are interconnected with the conductive pillars (6), and a solder ball (8) is planted on the surface of one of the RDL layers (7).

9. The method for preparing a hybrid memory chip double-sided packaging structure according to claim 8, Features: Metal copper is filled in the laser hole through an electroplating process to form a conductive column (6), and the conductive column (6) is a metal copper column.

10. The method for preparing a hybrid memory chip double-sided packaging structure according to claim 8, Features: Conductive glue is injected into the laser hole through a filling process to form a conductive column (6), and the conductive column (6) is a conductive glue column.