Lamination winding structure process of lithium ion battery

Through the laminated winding structure process, the problems of insufficient energy storage and low production efficiency of lithium-ion batteries are solved, and higher capacity density and energy density are achieved, reducing dummy welding, extending battery life, and improving production efficiency.

CN118983531AInactive Publication Date: 2024-11-19SUZHOU MINGXIANG NEW ENERGY TECH CO LTD

Patent Information

Application Number
CN202411070421.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-06
Publication Date
2024-11-19
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The winding process of lithium-ion batteries has less energy storage, great application limitations, and low production efficiency of lamination process.

Method used

Using the laminated winding structure process, the laminated welding and tablet slitting of the electrode group are performed first, and the electrode group is formed by cross-stacking by Z-shaped lamination machines, and the SEI film is formed on the negative electrode surface to improve the stability of the battery, using heat The press makes the electrode group tightly bonded to prevent the diaphragm from deforming and forming a laminated winding battery.

Benefits of technology

It improves the capacity density and energy density of lithium-ion batteries, reduces the phenomenon of dummy welding, extends the battery life, and improves production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118983531A_ABST
    Figure CN118983531A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of lithium ion battery manufacturing, and provides a lamination winding structure process of a lithium ion battery. The preparation method comprises the following steps: preparing positive and negative electrode slurry, uniformly coating a current collector with the positive and negative electrode slurry, drying to form positive and negative electrode plates, and drying; cutting polyethylene into a diaphragm with the pore diameter of 0.01-0.1 mu m, laminating the dried positive and negative pole pieces according to the sequence of the positive pole piece, the diaphragm, the negative pole piece and the diaphragm to form a pole group, then tabletting, cutting the pole group into strip-shaped pole groups with different sizes after tabletting, winding, putting a battery unit into a battery shell, and injecting electrolyte into the battery shell; and finally, sealing and forming, and activating positive and negative electrode materials in the battery in a charging and discharging manner after the battery is assembled.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of lithium ion battery manufacturing, in particular to a laminate winding structure process of a lithium ion battery. Background Art

[0002] Lithium-ion batteries can be classified into soft-pack, square and cylindrical batteries according to packaging methods and appearance. From the perspective of internal molding process, soft-pack and square batteries can adopt winding or lamination process, while cylindrical batteries have curvature everywhere and can only adopt winding process. Although the winding process has been developed for a relatively longer time, the process is mature, the cost is low and the yield rate is high, but with the promotion and development of new energy vehicles, the lamination process has become a rising star with its advantages such as high volume utilization, stable structure, low internal resistance and long cycle life.

[0003] The winding process is to wind and extrude the previously processed positive electrode sheets, separators, and negative electrode sheets in sequence through a fixed winding needle. The specific process is to stack the raw materials in the order of negative electrode, separator, positive electrode, and separator, and directly roll them into a cylindrical or elliptical shape through the winding method, and then place them in a square or cylindrical metal shell. However, its process characteristics make it only suitable for preparing lithium batteries with regular shapes, which can store less electrical energy and have limited applications.

[0004] The stacking process is a manufacturing process in which the positive and negative electrodes are cut into small pieces and stacked with isolation membranes to form small battery cells, and then the small battery cells are stacked and connected in parallel to form a large battery cell. The positive and negative electrode sheets and isolation membranes are stacked alternately through a sheet feeding mechanism to form a stacked core. Regular or irregular-shaped lithium batteries can be prepared, and the capacity density is higher than that of the winding process. However, in the production process of stacked batteries, the stacking operation time is long and the production efficiency is low. Summary of the invention

[0005] The present invention provides a stacked winding structure process for lithium-ion batteries, which solves the problems of low energy storage and application limitations of wound batteries, as well as the problem of low production efficiency of stacked batteries; improves the applicability and productivity of lithium-ion batteries. The specific process is as follows:

[0006] S1: Preparation of positive electrode slurry, the raw materials are composed of active material, conductive agent and binder; the conductive agent and binder are baked, and the conductive agent, binder and active material are placed in a stirring tank and mixed and stirred evenly to obtain positive electrode slurry, and the slurry is passed through a 100 mesh sieve when it is transferred out;

[0007] S2: Preparation of negative electrode slurry, the raw materials are composed of active material, conductive agent, binder and dispersant; the conductive agent, binder and dispersant are baked, and the conductive agent, binder, active material and dispersant are placed in a stirring tank and mixed and stirred evenly to obtain negative electrode slurry, and the slurry is passed through a 100 mesh sieve when it is transferred out;

[0008] S3: coating and drying, the positive electrode and negative electrode slurries are evenly coated on the current collector to form positive and negative electrode sheets, and the coated electrode sheets are placed in a 40°C constant temperature box for drying for one hour for drying;

[0009] The material of the positive electrode current collector is aluminum foil, and the material of the negative electrode current collector is copper foil;

[0010] S4: Lamination winding, first use a diaphragm slitting machine to cut polyethylene into a diaphragm with a pore size of 0.01-0.1μm, then use a Z-shaped laminating machine to cross-stack the dried positive and negative electrodes in the order of positive electrode, diaphragm, negative electrode, and diaphragm to form an electrode group, and then laser welding is performed at the four corners of the electrode group; the welded electrode group is pressed by a hot press to make the electrode groups more tightly bonded to prevent the diaphragm from deforming. After pressing, the electrode group is cut into strip electrode groups of 57mm×65mm or 66mm×70mm or 44mm×50mm; the slit laminated electrode group is wound into a cylindrical shape by a winding machine to form the basic structural unit of the laminated winding battery;

[0011] S5: Put the battery cell into the battery shell and inject electrolyte into the battery shell;

[0012] S6: Sealing and formation, sealing the battery. After the battery is assembled, the positive and negative electrode materials inside the battery are activated by charging and discharging. At the same time, the fluoroethylene carbonate in the electrolyte forms a good SEI film on the surface of the negative electrode.

[0013] Preferably, the active substance in the positive electrode material is lithium iron phosphate (LiFePO4), the conductive agent is 1-2 parts of conductive carbon black (SP), and the binder is PVDF.

[0014] The positive electrode slurry may be composed of the following components: 45-46 parts of LiFePO4, 1-2 parts of SP, and 1-2 parts of PVDF glue.

[0015] Preferably, the active substance in the negative electrode material is graphite, the conductive agent is graphene, the binder is PVDF, and the dispersant is sodium carbonate.

[0016] The negative electrode slurry may be composed of the following components: 45-46 parts of graphite, 1-2 parts of graphene, 1-2 parts of PVDF glue, and 1 part of sodium carbonate.

[0017] The preparation process of PVDF glue is as follows: a certain amount of solvent N-methylpyrrolidone is first injected into an ordinary stirring tank, PVDF powder is added thereto at a solid content of 5% to 10%, and PVDF glue is obtained after stirring for 4 to 6 hours.

[0018] Preferably, the electrolyte formula is: 7 parts of ethylene carbonate (EC), 7 parts of dimethyl carbonate (DMC), 1 part of polycarbonate (PC), 3-4 parts of fluoroethylene carbonate (FEC), and 13-15 parts of water.

[0019] Compared with the prior art, the present invention has the following beneficial effects:

[0020] 1. The present invention provides a lithium-ion battery stacking and winding structure process, which first performs stacking welding on the battery electrode group and then performs sheet pressing and slitting. It is easier to weld a large-area electrode group than a small electrode group, and is less likely to have problems of cold welding or false welding, thereby improving production efficiency.

[0021] 2. The stacking and winding structure process of a lithium-ion battery provided by the present invention has a higher capacity density and energy density than simple stacking or winding lithium-ion batteries, so that the battery can store and provide more electrical energy, effectively prevent the battery from having cold solder joints due to high-frequency charging and discharging, and reduce battery damage.

[0022] 3. The present invention provides a lithium-ion battery stacking winding structure process, in which FEC is added to the lithium-ion battery electrolyte, which can form a SEI film on the negative electrode surface, has stability, better protects the battery, and prolongs the battery life. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 This is a process flow chart of the lithium-ion battery stack winding structure of the present invention;

[0024] Figure 2 It is a schematic diagram of the internal structure of the lithium-ion battery unit of the present invention. DETAILED DESCRIPTION

[0025] The following embodiments of the present invention are described in further detail in conjunction with the accompanying drawings and examples. The following examples are used to illustrate the present invention, but are not intended to limit the scope of the present invention.

[0026] The present invention provides a stacking winding structure process for a lithium-ion battery. The following five embodiments only change the ratios of the raw material components of the positive electrode slurry, the negative electrode slurry and the electrolyte.

[0027] Embodiment 1

[0028] S1: Bake SP and PVDF powders, prepare positive electrode slurry according to 45 parts of LiFePO4, 1 part of SP, and 1 part of PVDF glue, and pass the slurry through a 100-mesh sieve when it is transferred out;

[0029] S2: baking graphene, PVDF powder and sodium carbonate powder, preparing negative electrode slurry according to 45 parts of graphite, 1 part of graphene, 1 part of PVDF glue and 1 part of sodium carbonate, and transferring the slurry to pass through a 100-mesh sieve;

[0030] S3: evenly coating the positive electrode and negative electrode slurries on the current collector, and then drying them to form positive and negative electrode sheets, and drying the coated electrode sheets;

[0031] S4: Use a diaphragm slitting machine to cut polyethylene into diaphragms with a pore size of 0.01-0.1μm, then use a Z-shaped stacking machine to cross-stack the dried positive and negative electrodes in the order of positive electrode, diaphragm, negative electrode, and diaphragm to form an electrode group, and then laser weld the four corners of the electrode group; use a hot press to press the welded electrode group to make the electrode groups more tightly bonded to prevent the diaphragm from deforming. After pressing, cut the electrode group into strip electrode groups of 57mm×65mm or 66mm×70mm or 44mm×50mm; use a winding machine to wind the slit laminated electrode group into a cylindrical shape to form the basic structural unit of the laminated wound battery;

[0032] S5: Place the battery cell into a battery case, prepare an electrolyte solution by 7 parts of EC, 7 parts of DMC, 1 part of PC, 3 parts of FEC, and 13 parts of water, and inject the electrolyte solution into the battery case;

[0033] S6: After sealing the battery and completing the assembly of the battery, the positive and negative electrode materials inside the battery are activated by charging and discharging. At the same time, the fluoroethylene carbonate in the electrolyte forms a good SEI film on the surface of the negative electrode.

[0034] Embodiment 2

[0035] S1: Bake SP and PVDF powders, prepare positive electrode slurry according to 46 parts of LiFePO4, 1 part of SP, and 1 part of PVDF glue, and pass the slurry through a 100-mesh sieve when it is transferred out;

[0036] S2: baking graphene, PVDF powder and sodium carbonate powder, preparing negative electrode slurry according to 46 parts of graphite, 1 part of graphene, 1 part of PVDF glue and 1 part of sodium carbonate, and passing the slurry through a 100-mesh sieve when transferring;

[0037] S3: evenly coating the positive electrode and negative electrode slurries on the current collector, and then drying them to form positive and negative electrode sheets, and drying the coated electrode sheets;

[0038] S4: Use a diaphragm slitting machine to cut polyethylene into diaphragms with a pore size of 0.01-0.1μm, then use a Z-shaped stacking machine to cross-stack the dried positive and negative electrodes in the order of positive electrode, diaphragm, negative electrode, and diaphragm to form an electrode group, and then laser weld the four corners of the electrode group; use a hot press to press the welded electrode group to make the electrode groups more tightly bonded to prevent the diaphragm from deforming. After pressing, cut the electrode group into strip electrode groups of 57mm×65mm or 66mm×70mm or 44mm×50mm; use a winding machine to wind the slit laminated electrode group into a cylindrical shape to form the basic structural unit of the laminated wound battery;

[0039] S5: Place the battery cell into a battery case, prepare an electrolyte solution by 7 parts of EC, 7 parts of DMC, 1 part of PC, 3 parts of FEC, and 14 parts of water, and inject the electrolyte solution into the battery case;

[0040] S6: After sealing the battery and completing the assembly of the battery, the positive and negative electrode materials inside the battery are activated by charging and discharging. At the same time, the fluoroethylene carbonate in the electrolyte forms a good SEI film on the surface of the negative electrode.

[0041] Embodiment 3

[0042] S1: Bake SP and PVDF powders, prepare positive electrode slurry according to 45 parts of LiFePO4, 2 parts of SP, and 2 parts of PVDF glue, and pass the slurry through a 100-mesh sieve when it is transferred out;

[0043] S2: baking graphene, PVDF powder and sodium carbonate powder, preparing negative electrode slurry according to 45 parts of graphite, 2 parts of graphene, 2 parts of PVDF glue and 1 part of sodium carbonate, and passing the slurry through a 100-mesh sieve when transferring;

[0044] S3: evenly coating the positive electrode and negative electrode slurries on the current collector, and then drying them to form positive and negative electrode sheets, and drying the coated electrode sheets;

[0045] S4: Use a diaphragm slitting machine to cut polyethylene into diaphragms with a pore size of 0.01-0.1μm, then use a Z-shaped stacking machine to cross-stack the dried positive and negative electrodes in the order of positive electrode, diaphragm, negative electrode, and diaphragm to form an electrode group, and then laser weld the four corners of the electrode group; use a hot press to press the welded electrode group to make the electrode groups more tightly bonded to prevent the diaphragm from deforming. After pressing, cut the electrode group into strip electrode groups of 57mm×65mm or 66mm×70mm or 44mm×50mm; use a winding machine to wind the slit laminated electrode group into a cylindrical shape to form the basic structural unit of the laminated wound battery;

[0046] S5: Place the battery cell into a battery case, prepare an electrolyte solution by 7 parts of EC, 7 parts of DMC, 1 part of PC, 3 parts of FEC, and 15 parts of water, and inject the electrolyte solution into the battery case;

[0047] S6: After sealing the battery and completing the assembly of the battery, the positive and negative electrode materials inside the battery are activated by charging and discharging. At the same time, the fluoroethylene carbonate in the electrolyte forms a good SEI film on the surface of the negative electrode.

[0048] Embodiment 4

[0049] S1: Bake SP and PVDF powders, prepare positive electrode slurry according to 46 parts of LiFePO4, 2 parts of SP, and 2 parts of PVDF glue, and pass the slurry through a 100-mesh sieve when it is transferred out;

[0050] S2: baking graphene, PVDF powder and sodium carbonate powder, preparing negative electrode slurry according to 46 parts of graphite, 2 parts of graphene, 2 parts of PVDF glue and 1 part of sodium carbonate, and passing the slurry through a 100-mesh sieve when transferring;

[0051] S3: evenly coating the positive electrode and negative electrode slurries on the current collector, and then drying them to form positive and negative electrode sheets, and drying the coated electrode sheets;

[0052] S4: Use a diaphragm slitting machine to cut polyethylene into diaphragms with a pore size of 0.01-0.1μm, then use a Z-shaped stacking machine to cross-stack the dried positive and negative electrodes in the order of positive electrode, diaphragm, negative electrode, and diaphragm to form an electrode group, and then laser weld the four corners of the electrode group; use a hot press to press the welded electrode group to make the electrode groups more tightly bonded to prevent the diaphragm from deforming. After pressing, cut the electrode group into strip electrode groups of 57mm×65mm or 66mm×70mm or 44mm×50mm; use a winding machine to wind the slit laminated electrode group into a cylindrical shape to form the basic structural unit of the laminated wound battery;

[0053] S5: Place the battery cell into a battery case, prepare an electrolyte solution by 7 parts of EC, 7 parts of DMC, 1 part of PC, 4 parts of FEC, and 14 parts of water, and inject the electrolyte solution into the battery case;

[0054] S6: After sealing the battery and completing the assembly of the battery, the positive and negative electrode materials inside the battery are activated by charging and discharging. At the same time, the fluoroethylene carbonate in the electrolyte forms a good SEI film on the surface of the negative electrode.

[0055] Embodiment 5

[0056] S1: Bake SP and PVDF powders, prepare positive electrode slurry according to 46 parts of LiFePO4, 1 part of SP, and 2 parts of PVDF glue, and pass the slurry through a 100-mesh sieve when it is transferred out;

[0057] S2: baking graphene, PVDF powder and sodium carbonate powder, preparing negative electrode slurry according to 46 parts of graphite, 1 part of graphene, 2 parts of PVDF glue and 1 part of sodium carbonate, and passing the slurry through a 100-mesh sieve when transferring;

[0058] S3: evenly coating the positive electrode and negative electrode slurries on the current collector, and then drying them to form positive and negative electrode sheets, and drying the coated electrode sheets;

[0059] S4: Use a diaphragm slitting machine to cut polyethylene into diaphragms with a pore size of 0.01-0.1μm, then use a Z-shaped stacking machine to cross-stack the dried positive and negative electrodes in the order of positive electrode, diaphragm, negative electrode, and diaphragm to form an electrode group, and then laser weld the four corners of the electrode group; use a hot press to press the welded electrode group to make the electrode groups more tightly bonded to prevent the diaphragm from deforming. After pressing, cut the electrode group into strip electrode groups of 57mm×65mm or 66mm×70mm or 44mm×50mm; use a winding machine to wind the slit laminated electrode group into a cylindrical shape to form the basic structural unit of the laminated wound battery;

[0060] S5: Place the battery cell into a battery case, prepare an electrolyte solution by 7 parts of EC, 7 parts of DMC, 1 part of PC, 4 parts of FEC, and 15 parts of water, and inject the electrolyte solution into the battery case;

[0061] S6: After sealing the battery and completing the assembly of the battery, the positive and negative electrode materials inside the battery are activated by charging and discharging. At the same time, the fluoroethylene carbonate in the electrolyte forms a good SEI film on the surface of the negative electrode.

[0062] Experimental analysis

[0063] A laminated lithium-ion battery, a wound lithium-ion battery, and laminated wound lithium-ion batteries prepared in five embodiments were selected and numbered A1, A2, A3, A4, A5, A6, and A7. The battery capacity, average voltage, and mass of the seven batteries were measured respectively. According to the capacity density = battery capacity × battery average voltage / battery mass, the capacity density of the seven batteries was obtained. The volume of the seven lithium-ion batteries used in the test was π×9 2 ×65=16532.1mm 3 According to energy density = battery capacity × average battery voltage / battery volume, the energy densities of seven batteries were obtained; then A1, A2, A3, A4, A5, A6, and A7 were used on seven identical new laptops, and the standby time of the seven laptops was recorded without the assistance of external power supply.

[0064] Table 1 Comparison of performance indicators of lithium-ion batteries

[0065]

[0066] It can be seen from Table 1 that the capacity density and energy density of A3, A4, A5, A6, and A7 are significantly higher than those of A1 and A2. Therefore, compared with the laminated lithium-ion battery and the wound lithium-ion battery, the laminated wound lithium-ion battery prepared in the embodiment of the present invention has higher capacity density and energy density; compared with using A1 and A2 as the power supply battery for the laptop computer, when A3, A4, A5, A6, and A7 are used as the power supply battery for the laptop computer, the standby time of the laptop computer is longer, but when A3, A4, A5, A6, and A7 are used as the power supply battery for the laptop computer, the standby time of the laptop computer also varies.

[0067] For the five batteries prepared in the embodiments of the present invention, different raw material ratios of positive and negative electrode slurries and electrolytes are the reason for the differences in the standby time of laptop computers. When the raw material ratio of the positive electrode slurry is 45 parts of LiFePO4, 1 part of SP, and 1 part of PVDF glue, the raw material ratio of the negative electrode slurry is 45 parts of graphite, 1 part of graphene, 1 part of PVDF glue, and 1 part of sodium carbonate, and the raw material ratio of the electrolyte is 7 parts of EC, 7 parts of DMC, 1 part of PC, 3 parts of FEC, and 13 parts of water; or when the raw material ratio of the positive electrode slurry is 46 parts of LiFePO4, 1 part of SP, and 2 parts of PVDF glue, the raw material ratio of the negative electrode slurry is 46 parts of graphite, 1 part of graphene, 2 parts of PVDF glue, and 1 part of sodium carbonate, and the raw material ratio of the electrolyte is 7 parts of EC, 7 parts of DMC, 1 part of PC, 4 parts of FEC, and 15 parts of water, the laptop computer has the longest standby time without the assistance of an external power supply.

[0068] In summary, a large capacity density can store more electrical energy. The more electrical energy stored, the less times the battery is charged and discharged. This can effectively prevent the battery from overheating due to high-frequency charging and discharging, which can cause aging of the internal electrode group welding points, reduce the occurrence of cold solder joints, and extend the battery life. A large energy density can provide more electrical energy, which can enhance the performance of laptop computers as described in the above experiment. Therefore, the laminated wound lithium-ion battery prepared by the present invention is more practical.

[0069] The embodiments of the present invention are provided for the purpose of illustration and description. Although the embodiments of the present invention have been shown and described above, it can be understood that the above embodiments are exemplary and cannot be understood as limitations of the present invention. Ordinary technicians in this field can change, modify, replace and modify the above embodiments within the scope of the present invention.

Claims

1. A process for winding a laminated structure of a lithium-ion battery, characterized in that: The specific process of the structural process is as follows: S1: Preparation of positive electrode slurry, baking the conductive agent and the binder, placing the conductive agent, the binder and the active material in a stirring tank and stirring them evenly, and passing the slurry through a 100-mesh sieve when it is transferred out; S2: Preparation of negative electrode slurry: baking the conductive agent, binder, and dispersant. The conductive agent, binder, active material, and dispersant are placed in a stirring tank and stirred evenly. When the slurry is transferred out, it is sieved through a 100-mesh sieve; S3: coating and drying, coating the positive electrode and negative electrode slurries evenly on the current collector, and then drying to form positive and negative electrode sheets, and drying the coated electrode sheets; S4: Lamination winding, first use a diaphragm slitting machine to cut polyethylene into a diaphragm with a pore size of 0.01-0.1μm, then use a Z-shaped laminating machine to cross-stack the dried positive and negative electrode sheets in the order of positive electrode sheet, diaphragm, negative electrode sheet, and diaphragm to form an electrode group, and then perform laser welding; use a hot press to press the welded electrode group, and then cut the electrode group into strip electrode groups of different sizes; use a winding machine to wind the slit laminated electrode group into a cylindrical shape to form the basic structural unit of the laminated winding battery; S5: Put the battery cell into the battery shell and inject electrolyte into the battery shell; S6: Sealing and formation, sealing the battery and activating the positive and negative electrode materials inside through charging and discharging.

2. The process for winding a lithium-ion battery laminate as claimed in claim 1, characterized in that: In S1, the active material is lithium iron phosphate, the conductive agent is conductive carbon black, and the binder is PVDF glue.

3. The process for winding a lithium-ion battery laminate as claimed in claim 1, characterized in that: In S2, the active material is graphite, the conductive agent is graphene, the binder is PVDF glue, and the dispersant is sodium carbonate.

4. The process for winding a lithium-ion battery laminate as claimed in claim 2, characterized in that: The preparation method of the PVDF glue solution is as follows: a certain amount of solvent N-methylpyrrolidone is first injected into a common stirring tank, a binder PVDF powder is added into the solvent at a solid content of 5% to 10%, and the PVDF glue solution is obtained after stirring for 4 to 6 hours.

5. The process for winding a lithium-ion battery laminate as claimed in claim 2, characterized in that: In S1, the formula of the positive electrode slurry is: 45-46 parts of lithium iron phosphate, 1-2 parts of conductive carbon black, and 1-2 parts of PVDF glue.

6. The process for winding a lithium-ion battery laminate as claimed in claim 3, characterized in that: In S2, the formula of the negative electrode slurry is: 45-46 parts of graphite, 1-2 parts of graphene, 1-2 parts of PVDF glue, and 1 part of sodium carbonate.

7. The process for winding a lithium-ion battery laminate as claimed in claim 1, characterized in that: In S6, the electrolyte is composed of the following raw materials: 7 parts of ethylene carbonate, 7 parts of dimethyl carbonate, 1 part of polycarbonate, 3-4 parts of fluoroethylene carbonate, and 13-15 parts of water.

Citation Information

Patent Citations

  • A preparation method of a split laminated wound flexible lithium ion battery cell

    CN109004260A

  • Rapid lamination method and lamination tool of battery cell pole group and battery cell pole group

    CN111430774A

  • Battery cell, preparation method thereof and battery pack

    CN114843619A

  • Negative pole piece, preparation method thereof and lithium ion battery

    CN117253978A

  • Method for stacking cells inside secondary battery and cell stack manufactured using same

    WO2014042424A1

Cited By

  • Preparation method of laminated pole group and laminated battery and electrochemical device

    CN121862892A