Integral machining method for crane
By using the methods of marking drilling, welding and CNC boring and milling machines in the crane tower processing process, combining efficient tools and special clamping tooling, the problems of poor accuracy and low craftsmanship in the existing technology are solved, and the problem of poor accuracy and low craftsmanship in the existing technology is realized. The efficient and precise overall tower body is equipped with a guaranteed production tasks under high output conditions.
Patent Information
- Application Number
- CN202411255483.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-09
- Publication Date
- 2024-11-22
AI Technical Summary
The existing crane tower processing process has problems of poor accuracy and low craftsmanship, especially under high output conditions, it is difficult to ensure the smooth completion of production tasks, and the meshing rate between the pinion and the large ring is insufficient after the rotating mechanism is assembled.
A method of adding a crane is adopted, including marking and drilling the main holes on the bottom plate of the tower, welding and closing the tower, and using a CNC boring and milling machine to finish the ring groove surface and motor holes, using medium and high-speed disc milling cutters and alloys Efficient tools such as drilling and spiral tapping are combined with special clamping tools for overall clamping, optimizing cutting angle and cooling methods, and improving processing efficiency and accuracy.
It significantly improves the machining accuracy and efficiency of the screw holes on the ring groove surface, shortens the processing time, ensures that the tower body is closed and welded in one pass, saves processing time and improves assembly accuracy and efficiency.
Smart Images

Figure CN118989879A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of ship deck machinery, and in particular relates to a method for integrally machining a crane. Background Art
[0002] It is understood that in the 1990s, due to the lack of CNC boring and milling machines in China, the tower bodies of Mag cranes were first rough-turned on vertical lathes to turn the ring grooves, then the screw holes on the ring grooves were marked and drilled, and then the motor holes were bored and scraped on the floor boring machines. After the tower body was closed, the ring grooves were fine-milled using the factory-made equipment. Due to the simplicity of the homemade equipment and poor geometric accuracy, the accuracy of the processed ring grooves often exceeded the tolerance. The reverse side of the motor hole could not be fine-machined after welding, and the parallelism with the ring groove surface exceeded the tolerance. Among them, the parallelism error of one tower body was the largest (1mm difference within the range of φ435), resulting in only 30% meshing rate between the pinion and the large gear ring after the rotating mechanism was assembled.
[0003] Entering the 21st century, with the increase in the number of domestic CNC boring and milling machines, the crane tower body machining has always used the following process flow: first use the vertical lathe to rough-process the ring groove, then mark and drill the screw holes on the ring groove surface, then weld and close the tower body, and finally use the CNC boring and milling machine to fine-process the ring groove surface, motor hole and reverse side. In this way, since the processing of the ring groove surface, motor hole and reverse side is a one-time clamping process, the meshing rate of the small gear and the large gear ring can be guaranteed after the rotating mechanism is assembled. However, since the screw holes on the ring groove are manually marked and the drilling machine operator manually calibrates and drills the screw holes, the chord length of the two holes and the chord length of the ten holes often exceed the tolerance. 20% of the tower body bottom plates need to be tested with the large gear ring provided by Mag to determine whether they can be reused. Some individual screw holes also need to be bored and inserted for repair (the error of the chord length of the two holes is more than 2.5mm). Therefore, there is room for improvement in the processing accuracy and work efficiency of this process.
[0004] In recent years, with the doubling of crane orders, annual output has increased from 300 units to 600 units. The original processing flow can no longer ensure the smooth completion of production tasks. The improvement of machining technology is imminent, and an overall tower body machining plan is imperative. Summary of the invention
[0005] The purpose of the present invention is to provide a In order to achieve the above objectives, the present invention provides a crane integral machining method, comprising the following steps: Step 1: Mark and drill the secondary holes on the bottom plate of the tower; Step 2: Weld the tower body together, and complete the welding of the tower body bottom plate, arm bracket, tower body middle part, and tower body head; Step 3: Use CNC milling machine to finish the ring groove surface, process the screw holes on the ring groove surface, and process the motor hole.
[0006] The process flow of the present invention is: first mark and drill the minor holes on the bottom plate, then weld and close the tower body, and finally use a CNC boring and milling machine to fine-process the annular groove surface, the screw holes on the annular groove surface, and the motor holes. The present invention uses a CNC boring and milling machine to process the tower body bottom plate, the arm bracket, the middle part of the tower body, and the tower body head after all welding is completed; instead of machining the annular grooves and screw holes on the tower body bottom plate and the arm bracket holes, and then welding them with the middle part of the tower body and the head into a whole.
[0007] The present invention further adopts the following technical solution: Preferably, in step 3, the specific processing method is as follows: a. When machining the annular groove surface, the annular groove surface should be machined first and then drilling and tapping are performed. The face milling cutter is subjected to a relatively uniform force during operation. The cutting angle of the face milling cutter blade is 45°. Because the cutting force is slightly lighter and the cutting depth is greater, the work efficiency is higher; b. When machining the reverse side of the motor hole, use a medium-high speed disc milling cutter to scrape the reverse side, which increases the efficiency by 80-90%; c. When processing the screw holes around the motor hole, a medium-high speed alloy drill is used, and it is a composite drill. Two holes are drilled at a time, and then the threads are tapped directly. The drill bit cooling method during processing is internal cooling, which is more fully cooled and has better effects. The work efficiency is increased by 40%, which reduces the labor intensity of the operator; d. When processing the screw holes on the ring groove surface, use a spiral tap to process directly on the CNC boring and milling machine. The chip removal direction is improved, reducing the extrusion of the chips on the processed threads. The thread finish has a qualitative leap, and the processing accuracy and work efficiency are greatly improved.
[0008] Preferably, the tower body is clamped as a whole between steps 2 and 3, and the method of clamping the tower body as a whole includes: A. When working on the tower, the cab frame is facing downwards, and the operator drills into the tower. Use the Z-direction side plate of the cab frame to support the left and right points of the tower. Insert the left and right ends of the pressure plate into the holes of the left and right arm brackets respectively to press the two points with the grooved pressure plate. B. The outside of the tower body is pressed tightly by two sets of arm bracket holes, and the bottom plate is supported by bolts at different heights to offset the Z-direction cutting force.
[0009] Furthermore, the tower body is clamped as a whole by a special clamping tool, and the special clamping tool includes a pressure plate and a tool base. The pressure plate can be inserted into the hole of the arm bracket, and the tool base is installed on a workbench. Six screw holes are provided on the tool base along the height direction, and bolts are set in conjunction with the screw holes.
[0010] Furthermore, a groove is provided on the lower surface of the pressing plate along its length direction, and the groove is matched with the top of the support rod to support the pressing plate.
[0011] Furthermore, the pressing plate has an arc surface matching the hole of the arm support.
[0012] The present invention adjusts the process of drilling and tapping the screw holes on the annular groove surface by a radial drill with low efficiency and poor precision to a CNC boring and milling machine with high efficiency and good precision, thereby shortening the processing time, improving the processing precision of the screw holes on the annular groove surface, and further improving the assembly precision and efficiency, ensuring that the tower body closing welding ship inspection passes in one time. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] The present invention will be further described below in conjunction with the accompanying drawings.
[0014] Figure 1 It is a schematic diagram of the processing of the ring groove surface of the present invention.
[0015] In the figure: 1. Tower body plate, 2. Bottom plate, 3. Ring groove surface, 4. Weld. DETAILED DESCRIPTION Embodiment 1
[0016] A method for integrally machining a crane comprises the following steps: Step 1: Mark and drill the secondary holes on the tower base.
[0017] Step 2: Weld the tower body together, and complete the welding of the tower base plate, arm bracket, middle part of the tower body, and tower head.
[0018] Step 3, the tower body is clamped as a whole. The method of clamping the tower body as a whole combines the characteristics and requirements of the overall processing of the tower body. For example, the Z-direction cutting force of the process of drilling the bottom hole of the screw is very large, which has a great impact on the tower body. Some special clamping tools are designed. The new clamping method does not clamp by on-site welding process. The special clamping tool includes a pressure plate and a tool base. The lower surface of the pressure plate is provided with a groove along its length direction. The top of the support rod is provided with the groove to support the pressure plate. There are two groups of arm brackets, which are welded on both sides of the bottom plate of the tower body. The arm bracket is provided with a hole. When in use, the pressure plate can be inserted into the hole of the arm bracket. Since the hole of the arm bracket has been processed, the pressure plate should have an arc so as not to damage the processed surface of the hole of the arm bracket. The tool base is installed on the workbench. Six screw holes are provided on the tool base along the height direction, and bolts are provided in conjunction with the screw holes.
[0019] The methods for clamping the tower as a whole include: A. When the workbench of the CNC boring and milling machine is on the tower body, the cab frame is facing downward, and the operator drills into the tower body, and uses the Z-direction plate of the cab frame to support the left and right points of the tower body, and then uses the grooved pressure plate to press the two points, that is, insert the left and right ends of the pressure plate into the left and right sets of arm bracket holes respectively; B. The outside of the tower body is pressed tightly by two sets of arm bracket holes, and six screw holes are provided on the tooling base to ensure that the bottom plate of the tower body is supported by bolts at different heights to offset the Z-direction cutting force.
[0020] Step 4: Use a CNC milling machine to fine-process the annular groove surface 3, the screw holes on the annular groove surface 3, and the motor holes. The specific processing method is as follows: a. When machining the annular groove surface 3, the original method was to drill and tap first, and then machine the surface. The face milling cutter would hit the cutter when passing through the screw hole, which had a certain impact force on the cutter, so there were certain requirements for the toughness of the cutter. Now the annular groove surface 3 is machined first and then drill and tap. The face milling cutter is subjected to a more uniform force during operation, so the cutting angle of the face milling cutter blade is changed from the original 90° to 45°, because the latter has a slightly lighter cutting force, a greater cutting depth, and higher work efficiency. b. When processing the reverse side of the motor hole, the domestic medium-low speed disc milling cutter was used for reverse scraping, but now the imported medium-high speed disc milling cutter is used for reverse scraping, which improves the efficiency by 80-90%; c. When processing screw holes around the motor hole, we used to use domestic medium- and low-speed twist drills with two drill bits, and then drilled twice, and then tapped by hand. After investigation, it was found that more than 95% of MacGregor GLB cranes have M20 screw holes and φ26.5 countersunk holes, with the number of each unit ranging from 50 to 150, which is batch processing. Now we use imported medium- and high-speed alloy drills, and it is a composite drill. Two holes are drilled at a time, and then the threads are tapped directly. The drill bit cooling method during processing has changed from the original external cooling to internal cooling, which is more sufficient and has better effects. The work efficiency is increased by 40%, and the labor intensity of operators is reduced; d. When processing the screw holes on the ring groove surface 3, ordinary taps were originally used for processing on the radial drill, but now imported spiral taps are used for direct processing on the CNC boring and milling machine. The chip removal direction is improved, reducing the extrusion of chips on the processed threads, the thread finish has a qualitative leap, and the processing accuracy and work efficiency are greatly improved.
[0021] This embodiment selects tools and blades suitable for integral machining.
[0022] The tower body integral machining of the present invention has the following advantages: 1. Give full play to the effectiveness of CNC equipment The following table shows the cutting parameters of the two machining processes for machining the ring groove surface 3 Tower body processing process Spindle speed n(r / min) Cutting speed v(mm / min) Feed amount (mm) Original processing flow 300 400 2-3 Overall machining of the tower 600 700 4-6 (1) The maximum spindle speed of the CNC boring and milling machine is 800r / min. When machining the ring groove surface 3 of the tower body, the spindle only used 300r / min. Since there is no screw hole in the integral machining of the tower body, a new blade is selected when machining the ring groove surface 3, and the spindle speed reaches 600r / min. Take the φ250 cutter head as an example: The original cutting speed is V1=π×d×n1 / 60 / 1000=3.14×250×300 / 60 / 1000=3.925m / s The current cutting speed is V2=π×d×n2 / 60 / 1000=3.14×250×600 / 60 / 1000=7.85m / s As the cutting line speed of the blade increases, the iron chips cut off are finer and more uniform than before, and the roughness of the ring groove surface 3 is greatly improved.
[0023] (2) The change of cutting speed directly affects the processing efficiency. Take the processing of φ2700 middle diameter ring groove as an example: The original milling time for one circle is t1=π×D / v1=3.14×2700 / 400=21.195min The time for milling one circle is t2=π×D / v2=3.14×2700 / 700=12.111min The milling time for one circle was shortened by about 9 minutes.
[0024] (3) The amount of feed determines the number of cuts for rough milling the ring groove surface 3. In the overall machining process, only one rough milling and one fine milling cut are required to process the ring groove surface 3; however, due to the small amount of feed, the original processing flow sometimes requires one more rough milling cut.
[0025] (II) Shorten the processing cycle of the tower body in the machining workshop and the multi-process flow of the workpiece The time statistics of each process using the original machining process are as follows: It takes 30 minutes to mark the ring groove surface 3 processing line; it takes about 1 hour to rough turn the ring groove surface 3; it takes about 30 minutes to transfer between machining processes; it takes 2 hours and 30 minutes to mark the screw holes on the ring groove surface 3 and other processing lines; it takes 9 hours to drill and tap the screw holes on the ring groove surface 3 and other holes; it takes 2 hours to weld the steel structure on the tower body; it takes 2 hours to prepare for the process rigging and clamping on the CNC boring and milling machine, 50 minutes to fine-machine the ring groove surface 3 and the reference surface, 1 hour and 40 minutes to machine the two motor holes, 3 hours to drill the screw bottom holes around the motor holes and tap the guide holes; it takes 3 hours for the fitter to manually tap the screw holes around the motor holes, and 1 hour to remove the process rigging and finish.
[0026] The original machining process took about 25 hours to machine one tower body.
[0027] The time statistics of each machining process of the present invention are as follows: It takes 1 hour to mark the ordinary holes on the bottom plate surface; it takes 3 hours to drill and tap the ordinary holes on the bottom plate surface; it takes 1 hour to rotate the steel structure and weld the upper part of the tower body; it takes 1 hour and 20 minutes to prepare for clamping on the CNC boring and milling machine, 30 minutes to process the ring groove surface 3 and the reference surface, 5 hours to drill and tap the screw holes on the ring groove surface 3, 1 hour to process the two motor holes, and 2 hours and 20 hours to drill and tap the screw holes around the motor holes; it takes 30 minutes for fitter finishing.
[0028] The total machining time for a tower body is about 15 hours.
[0029] Compared with the original machining process, the machining process of the present invention can save 10 hours of time for machining a tower body.
[0030] (III) Improve the machining accuracy of the screw holes on the ring groove surface and improve the assembly accuracy and efficiency (1) During integral machining, the bottom hole of the ring groove screw is first milled flat with a milling cutter, and the screw hole is tapped with a spiral tap to ensure the effective depth of the threaded hole and the screw-in length of the high-strength bolt; (2) CNC machining ensures the position accuracy of the screw holes of the large gear ring, and one-time clamping ensures the verticality of the screw holes and the ring groove surface 3, thereby ensuring that the large gear ring is assembled successfully in one go; (3) After the screw holes are processed, there is no need for welding, the screw holes are not deformed, and there is no need to rewind the thread during assembly, which improves assembly efficiency.
[0031] The threaded holes processed by the drilling machine in the original process have uneven hole mouths, and there are inspection hole lines and four punch holes on the outer mouth to prevent deviation from scratching. The threads are uneven and the roughness is not high. The threaded holes processed by the CNC boring and milling machine in the process of the present invention have flat hole mouths, flat threads, high roughness, and the plug gauge inspection passes once.
[0032] (IV) Ensure that the tower body welding ship inspection passes once According to the original process, the screw holes on the annular groove surface are processed before the tower body is closed. Figure 1 As shown in the figure, the phenomenon of roof caving or even drilling through often occurs when drilling holes. When the tower body is closed, the intersection of the tower body plate 1 and the bottom plate 2 is often burned through. After plugging, the weld 4 still cannot pass during ultrasonic detection, which affects the ship inspection. The process flow of the present invention is to first process the annular groove surface screw hole and then close the tower body, which avoids the above situation. The annular groove surface screw hole adopts M36, the effective depth of the annular groove surface screw hole is 45m, the thickness of the bottom plate is 60m, and the thickness of the bottom of the screw hole from the top surface of the bottom plate is at least 5m.
[0033] In addition to the above embodiments, the present invention may also have other implementation modes. Any technical solution formed by equivalent replacement or equivalent transformation falls within the protection scope required by the present invention.
Claims
1. A method for integral machining of a crane. It is characterized in that The following steps are involved: Step 1: Mark and drill the secondary holes on the bottom plate of the tower; Step 2: Weld the tower body together, and complete the welding of the tower body bottom plate, arm bracket, tower body middle part, and tower body head; Step 3: Use CNC milling machine to finish the ring groove surface, process the screw holes on the ring groove surface, and process the motor hole.
2. According to the method for integrally machining a crane according to claim 1, It is characterized in that In step 3, the specific processing method is as follows: a. When machining the annular groove surface, the annular groove surface is machined first and then drilling and tapping are performed. The cutting angle of the face milling cutter blade is 45°; b. When machining the reverse side of the motor hole, use a medium-high speed disc milling cutter to scrape it back; c. When processing screw holes around the motor hole, use a medium-high speed alloy drill to drill two holes at a time, and then tap the threads directly. The drill bit cooling method during processing is internal cooling; d. When machining screw holes on the ring groove surface, use a spiral tap to machine directly on a CNC boring and milling machine.
3. According to the method for integrally machining a crane as claimed in claim 2, It is characterized in that The tower body is clamped as a whole between steps 2 and 3, and the method for clamping the tower body as a whole includes: A. When working on the tower, the cab frame is facing downwards, and the operator drills into the tower. Use the Z-direction side plate of the cab frame to support the left and right points of the tower. Insert the left and right ends of the pressure plate into the holes of the left and right arm brackets respectively to press the two points with the grooved pressure plate. B. The outside of the tower body is pressed tightly by two sets of arm bracket holes, and the bottom plate is supported by bolts at different heights to offset the Z-direction cutting force.
4. A crane integral machining method according to claim 3, It is characterized in that The tower body is clamped as a whole by a special clamping tool, which includes a pressure plate and a tool base. The pressure plate can be inserted into the hole of the arm bracket. The tool base is installed on a workbench. Six screw holes are provided on the tool base along the height direction, and bolts are set in conjunction with the screw holes.
5. A crane integral machining method according to claim 4, It is characterized in that The lower surface of the pressing plate is provided with a groove along its length direction, and the groove is matched with the top of the supporting rod to support the pressing plate.
6. A crane integral machining method according to claim 5, It is characterized in that The pressing plate has an arc surface matched with the hole of the arm support bracket.
Citation Information
Patent Citations
Machining method for multi-thin-wall-hole rotating body welding structural part
CN111299968A
Secondary opening piston and machining process thereof
CN112377512A
Modular tower horn frame welding frock
CN207548026U
Welding tool for single-limb structure of tower body of I-shaped main chord tower crane
CN218081080U
Boring and milling machine for off-highway dumper suspension