Heat conduction pad production process
By adding compensation technology and multiple vulcanization treatments in the thermal pad production process, the problems of insufficient edge thickness and low raw material utilization in the thermal pad production are solved, and more efficient resource utilization and performance improvement are achieved.
Patent Information
- Application Number
- CN202410768799.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-14
- Publication Date
- 2024-11-22
AI Technical Summary
In the existing thermal pad production process, there are problems such as severe spillage on both sides, poor thickness of edge materials and low raw material utilization rate, resulting in waste of resources and poor performance.
The additional compensation process is adopted, and the treatment agent is brushed on the surface of the thermal pad after peeling off the release film and re-coated the raw material, combined with multiple vulcanization treatments and traction slicing processes to ensure the improvement of edge thickness and raw material utilization.
It effectively avoids edge spills, improves raw material utilization, and ensures efficient production and performance improvement of thermal pads.
Smart Images

Figure CN118991102A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of thermal conductive pads for technical electronic products, and in particular to a production process of thermal conductive pads. Background Art
[0002] Thermal pad is a high-performance gap-filling thermal conductive material, mainly used for the transfer interface between electronic equipment and heat sink or product housing. It has good viscosity, flexibility, compression performance and excellent thermal conductivity, and can completely remove the air between the electronic components and the heat sink during use, so that the two are in full contact, thereby significantly increasing the heat dissipation effect.
[0003] At present, the conventional thermal pad coating and molding process includes calendering (thickness molding), vulcanization line (oven), process correction, pulling and slicing / winding.
[0004] In conventional production processes, there is serious overflow on both sides, the thickness of the edge material does not meet the standard, and a lot of raw materials are wasted. Although the use of baffles has improved it, the raw material utilization rate is only about 80%. Summary of the invention
[0005] The purpose of the present invention is to provide a thermal pad production process to solve the problems raised in the above-mentioned prior art.
[0006] To achieve the above-mentioned invention object, the technical solution adopted by the present invention is: 1. A thermal pad production process, characterized in that the production process comprises the following steps:
[0007] S1. Select a substrate, combine the release film with the raw materials on the substrate, and press it into the required thickness through a calendering process;
[0008] S2, vulcanizing the calendered thermal pad;
[0009] S3, peeling off the release film, and then entering the compensation process, brushing the treatment agent on the surface of the thermal pad, applying the raw material on the surface of the thermal pad, and laminating the release film;
[0010] S4, vulcanizing the calendered thermal pad again, and then pulling and slicing or rolling it.
[0011] Preferably, the release film is provided with one layer on the upper and lower sides of the substrate, and then pressed out to the required thickness of the thermal pad by the roller of the calendering platform.
[0012] Preferably, the thermally conductive pad is vulcanized in a first oven to form the thermally conductive pad.
[0013] Preferably, the thermal pad is corrected by a correction device to prevent material deviation.
[0014] Preferably, after the thermally conductive pad passes through the pulling roller of the first traction device, the upper release film is peeled off through the first laminating and peeling device.
[0015] Preferably, the thermal pad thickness compensation process steps are: first, a treatment agent is brushed on the surface of the thermal pad from which the upper release film has been peeled off by a double-station coater to increase the bonding effect, and then the raw material is squeezed onto the surface-treated thermal pad, and the raw material is scraped again by the double-station coater, and then the release film is attached.
[0016] Preferably, the coated thermal pad is vulcanized in a second oven to reshape the thermal pad.
[0017] Preferably, the thermal pad is pulled by a second traction device, pulled and peeled by a second lamination and peeling device, and then sliced by a slicer or rolled up by a rolling device.
[0018] Preferably, the length of the first oven vulcanization line is 13.5 m, and the length of the second oven vulcanization line is 2.5 m.
[0019] The beneficial effects of the present invention are mainly embodied in:
[0020] The production process of the thermal pad has added a compensation process. After peeling off the release film, the treatment agent is brushed on the surface of the thermal pad, and the raw material is applied to the surface of the thermal pad again, and then vulcanized again. The second coating and scraping compensates for the thickness of both sides of the thermal pad and improves the utilization rate of raw materials. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is a flowchart of the production process of the present invention;
[0022] Figure 2 It is the prior art production process diagram of the present invention;
[0023] Figure 3 It is the production process diagram of the present invention;
[0024] Figure 4 A schematic cross-sectional view of a thermal pad of the prior art of the present invention;
[0025] Figure 5 is a schematic cross-sectional view of a thermal conductive pad of the present invention;
[0026] Figure 6 It is a schematic diagram of a calender of the present invention;
[0027] Figure 7 is a schematic diagram of a first oven of the present invention;
[0028] Figure 8 It is a schematic diagram of the process correction equipment of the present invention;
[0029] Fig. 9 It is a schematic diagram of the compensation process of the present invention;
[0030] Fig.10 It is a schematic diagram of the second traction, second lamination and peeling and slicer equipment of the present invention;
[0031] Fig.11 It is a schematic diagram of the winding device of the present invention;
[0032] Among them, 1. calender; 2. first oven; 3. process correction equipment; 4. first traction equipment; 5. first lamination and peeling equipment; 6. double-station coating machine; 7. second oven; 8. second traction equipment; 9. second lamination and peeling equipment; 10. slicer; 11. thermal pad. DETAILED DESCRIPTION
[0033] In order to make the objectives, technical solutions and advantages of the present application clearer, the technical solutions in the embodiments of the present application will be described in more detail below in conjunction with the drawings in the preferred embodiments of the present application.
[0034] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, or it can be an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0035] In the description of the present application, it should be understood that the terms "upper", "lower", "front", "back", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating orientations or positional relationships, are orientations or positional relationships based on the drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0036] In addition, the terms "comprises," "comprising," and "having," and any variations thereof, are intended to cover a non-exclusive inclusion, for example, a process, method, system, product, or display comprising a series of steps or elements is not necessarily limited to those steps or elements explicitly listed, but may include other steps or elements not explicitly listed or inherent to such process, method, product, or display.
[0037] Embodiment 1
[0038] See also Figure 1-Figure 4 , a thermal pad production process.
[0039] The thermal pad 11 produced by this process is mainly used in high-performance computers to solve the heat dissipation problem. In the field of high-performance computers, since core components such as processors and graphics cards generate a lot of heat during operation, if the heat is not dissipated in time, it will cause the performance of the equipment to decline or even be damaged. The thermal pad 11 is used to fill the space between the core components such as the processor and graphics card in the high-performance computer and the heat sink. The high thermal conductivity of the thermal pad 11 can quickly transfer the heat generated by the core components to the heat sink, and dissipate the heat into the air through the heat sink, thereby achieving an efficient heat dissipation effect.
[0040] In addition, the thermal pad 11 can also be used in the fields of communication hardware, household appliances, such as communication equipment, set-top boxes, household appliances and mobile devices. In these applications, the thermal pad 11 can also effectively improve the heat dissipation performance of the equipment and ensure the stability and reliability of the equipment.
[0041] In this embodiment, the production process comprises the following steps:
[0042] S1. Select a substrate, combine the release film with the raw materials on the substrate, and press it into the required thickness through a calendering process;
[0043] S2, vulcanizing the rolled thermal pad 11;
[0044] S3, peeling off the release film, and then entering the compensation process, brushing the treatment agent on the surface of the thermal pad 11, and applying the raw material on the surface of the thermal pad 11, and laminating the release film;
[0045] S4, vulcanizing the rolled thermal pad 11 again, and then pulling and slicing or rolling it up.
[0046] Compared with traditional processes, the thermal conductive pads produced by this process have added compensation measures to ensure the edge thickness after coating compensation, avoid edge overflow, and improve the raw material utilization rate of the product.
[0047] Next, the above process flow is further explained as a more specific implementation of this embodiment. The release film is provided with a layer on the upper and lower sides of the substrate, and then the release film is pressed by a calender 1, and the required thickness of the thermal pad 11 is pressed by the roller of the calendering platform.
[0048] The raw materials can be silicone, silicone grease, silver paste, etc. These materials can effectively conduct heat and quickly transfer the heat of the electronic equipment to the radiator, thereby reducing the temperature of the device.
[0049] During the setting, a group of calendering rollers are respectively arranged on the left and right sides of the calendering platform of the calendering machine 1, and a group of calendering rollers are arranged at intervals up and down, and the release film with the raw material passes through the calendering rollers to achieve pressing.
[0050] The required thickness of the thermal pad 11 can be determined according to the thermal conductivity. For example, if a product with a thermal conductivity of 2.3 W / mK is to be produced, the required thickness of the thermal pad is 10 mm.
[0051] As a more specific implementation of this embodiment, the thermal pad 11 is vulcanized in the first oven 2, so that the thermal pad 11 is formed after vulcanization.
[0052] As a more specific implementation of this embodiment, the thermal pad 11 is corrected by a process correction device 3 to prevent material deviation.
[0053] The process correction device 3 may use the SG9200 coil correction machine of the Synmec brand.
[0054] As a more specific implementation of this embodiment, after the thermal pad 11 passes through the pulling roller of the first traction device 4, it passes through the first laminating and peeling device 5 to peel off the upper release film.
[0055] The first traction device 4 drives the pulling roller to rotate through a driving motor, thereby achieving progressive traction of the thermal pad 11 after deviation correction.
[0056] The first laminating and peeling device 5 can peel off the upper release film of the thermal pad 11 through a peeling scraper.
[0057] As a more specific implementation method of this embodiment, the thermal pad thickness compensation process steps are: first, the double-station coater 6 is used to brush the treatment agent on the surface of the thermal pad 11 from which the upper release film has been peeled off to increase the bonding effect, and then the raw material is squeezed onto the thermal pad 11 after the surface treatment, and the double-station coater 6 is used to scrape the raw material again, and then the release film is attached.
[0058] The double-station coating machine 6 is provided with a treatment agent scraper and a raw material scraper, through which the treatment agent scraper and the raw material scraper are respectively applied to the treatment agent and the raw material.
[0059] Among them, the treatment agent is usually a high-temperature glue that can maintain stable adhesion at high temperatures. In order to improve the performance and service life of the thermal pad, some other ingredients such as fillers and antioxidants may also be added.
[0060] As a more specific implementation of this embodiment, the coated thermal pad 11 is vulcanized in a second oven 7, so that the thermal pad 11 is vulcanized again and then formed.
[0061] As a more specific implementation of this embodiment, the thermal pad 11 is pulled by the second traction device 8, pulled and peeled by the second lamination and peeling device 9, and then sliced by the slicer 10 or rolled up by the winding device.
[0062] As a more specific implementation of this embodiment, the length of the vulcanization line of the first oven 2 is 13.5m, while the length of the vulcanization line of the second oven 7 is 2.5m. Because the thickness of the raw material scraped again is less than the thickness of the raw material scraped before, the latter vulcanization line can be shortened.
[0063] As a more specific implementation of this embodiment, the release film is any one of a polyester (PET) film, a polypropylene (PP) film or a polyimide (PI) film, which can be combined with or separated from the raw material.
[0064] As a more specific implementation of this embodiment, the raw material is any one of a silica gel material, a silicone grease material, and a silver paste material. These materials can effectively conduct heat and quickly transfer the heat of the electronic device to the radiator, thereby reducing the temperature of the device. The substrate is a flexible material, such as a polyimide film (Polyimide Film), a polyamide film (Polyamide Film), etc., which provides support and protection for the thermal conductive material and has certain insulation properties.
[0065] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. The patent protection scope of the present invention shall be based on the claims. All equivalent structural changes made using the contents of the description and drawings of the present invention should also be included in the protection scope of the present invention.
Claims
1. A thermal pad production process, characterized in that: The production process comprises the following steps: S1. Select a substrate, combine the release film with the raw materials on the substrate, and press it into the required thickness through a calendering process; S2, vulcanizing the calendered thermal pad; S3, peeling off the release film, and then entering the compensation process, brushing the treatment agent on the surface of the thermal pad, applying the raw material on the surface of the thermal pad, and laminating the release film; S4, vulcanizing the calendered thermal pad again, and then pulling and slicing or rolling it.
2. A thermal pad production process according to claim 1, characterized in that: The release film is provided with one layer on the upper and lower sides of the substrate, and then pressed out to the required thickness of the thermal pad by the roller of the calendering platform.
3. A thermal pad production process according to claim 1, characterized in that: The thermally conductive pad is vulcanized in a first oven to form the thermally conductive pad.
4. A thermal pad production process according to claim 1, characterized in that: The thermal pad is corrected by a correction device to prevent material deviation.
5. A thermal pad production process according to claim 1, characterized in that: After the thermal pad passes through the pulling roller of the first traction device, the upper release film is peeled off through the first laminating and peeling device.
6. A thermal pad production process according to claim 1, characterized in that: The thermal pad thickness compensation process steps are as follows: First, a double-station coating machine is used to brush the treatment agent on the surface of the thermal pad from which the upper release film has been peeled off to increase the bonding effect. Then the raw material is squeezed onto the thermal pad after the surface treatment, and the double-station coating machine is used to scrape the raw material again, and then the release film is attached.
7. A thermal pad production process according to claim 1, characterized in that: The coated thermal pad is vulcanized in a second oven to reshape the thermal pad.
8. A thermal pad production process according to claim 1, characterized in that: The thermal pad is pulled by a second pulling device, pulled and peeled by a second laminating and peeling device, and then sliced by a slicer or rolled up by a rolling device.
9. A thermal pad production process according to claim 1, characterized in that: The length of the first oven vulcanization line is 13.5 m, while the length of the second oven vulcanization line is 2.5 m.