Indication integrated deoxidizer packaging material and manufacturing method thereof

By combining the protective film made of environmentally friendly materials such as modified starch and other environmentally friendly materials with the paper substrate, the integrated deoxidant packaging material formed is solved, and the problems of powder leakage and non-degradability are achieved, achieving the dual effects of leakage prevention and degradability.

CN118992323AActive Publication Date: 2024-11-22NANJING JIEYUAN PACKING CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202411232382.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-11-22
Estimated Expiration
2044-09-04

AI Technical Summary

Technical Problem

Existing indicator integrated deoxidant packaging materials are prone to powder leakage and the raw materials are not degradable.

Method used

Use protective film made of modified starch, xylitol, polyvinyl alcohol, borax powder and modified epoxy soybean oil, combined with the paper matrix, and bonded to form a packaging bag through environmentally friendly glue to avoid hole punching and use environmentally friendly materials. Ensure that the material is degradable.

Benefits of technology

Effectively prevent powder leakage and improve the degradability of packaging materials, enhancing environmental protection performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118992323A_ABST
    Figure CN118992323A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of deoxidizing agents, particularly relates to an indication integrated deoxidizing agent packaging material and a manufacturing method, and provides the following scheme aiming at the problems that an existing deoxidizing agent packaging material is prone to powder leakage and does not have degradability: the deoxidizing agent packaging material comprises a packaging bag and an indication bag bonded on the surface of the packaging bag, the packaging bag is made of a base body and a protective film, the indicating bag is made of a protective film, and the indicating bag is filled with an indicator; the protective film is prepared from the following raw materials in parts by mass: 80 to 90 parts of modified starch, 0.50 to 1.00 parts of xylitol, 0.50 to 1.00 parts of polyvinyl alcohol, 1 to 5 parts of borax powder, 0.10 to 0.50 part of sodium trimetaphosphate and 7 to 15 parts of modified epoxidized soybean oil, so that internal powder leakage is not easy to cause, and meanwhile, the protective film has the advantages that the protective film is easy to clean, and the service life of the protective film is prolonged. The protective film is prepared from modified starch, xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil, is made of environment-friendly materials and can be naturally degraded.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of deoxidizers, and in particular to an indicator-integrated deoxidizer packaging material and a manufacturing method thereof. Background Art

[0002] The Chinese patent document with application number 201710584471.5 discloses an indicator-integrated deoxidizer packaging material and a manufacturing method, which solves the problem that the oxygen content in the existing food bags using deoxidizers cannot be intuitively indicated. The indicator-integrated deoxidizer packaging material includes a packaging paper body, and the packaging paper body includes an inner film, a PET layer and an outer film. The inner film is compounded on the bottom surface of the PET layer by an adhesive, and the outer film is compounded on the top surface of the PET layer by an adhesive. The outer film has an indicator pattern for detecting and indicating the oxygen content. The indicator pattern set on the outer film of the deoxidizer packaging material can detect the oxygen content in the food bag containing the deoxidizer and display it by color, which is convenient for users to identify and improve the safety of eating.

[0003] However, there are also some problems with the indicating integrated deoxidizer packaging material and the manufacturing method. For example, a plurality of pinholes are provided on the surface of the indicating integrated deoxidizer packaging material for ventilation, but its structure is also prone to leakage of powder in the indicating integrated deoxidizer packaging material, and the raw materials of the indicating integrated deoxidizer packaging material are mostly chemical materials and are not degradable. Summary of the invention

[0004] Based on the problems that the background technology is prone to powder leakage and is not degradable, the present invention proposes an indicator-integrated deoxidizer packaging material and a manufacturing method.

[0005] The present invention provides an indicator-integrated deoxidizer packaging material, which comprises a packaging bag and an indicator bag bonded to the surface of the packaging bag, wherein the packaging bag is made of a substrate and a protective film, the indicator bag is made of the protective film, and the indicator bag is filled with an indicator; The raw material composition and content of the protective film include 80 to 90 parts of modified starch, 0.50 to 1.00 parts of xylitol, 0.50 to 1.00 parts of polyvinyl alcohol, 1 to 5 parts of borax powder, 0.10 to 0.50 parts of sodium trimetaphosphate and 7 to 15 parts of modified epoxidized soybean oil by mass. The modified starch includes corn starch, cassava starch and potato starch. The packaging bag is made of a base and a protective film. The paper material of the base itself has strong air permeability. At the same time, the material properties of the protective film allow a large number of gaps to exist inside it, so there is no need to punch holes, and it is not easy to cause internal powder leakage. At the same time, the protective film is made of modified starch, xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil. It uses environmentally friendly materials and can be naturally degraded.

[0006] Preferably, the substrate is mainly made of log pulp, and the packaging bag is bonded to the indicator bag with environmentally friendly glue, which can enhance environmental performance.

[0007] Preferably, the weight ratio of corn starch, tapioca starch and potato starch in the modified starch is: 1-2: (1-2): 1-2, and the corn starch, tapioca starch and potato starch are all sieved through a 100-mesh sieve to enhance the compatibility of the modified starch.

[0008] Preferably, the preparation method of the modified starch comprises: obtaining corn starch, cassava starch and potato starch, adding deionized water in an amount of 10 times the total amount thereof, mixing evenly to obtain a starch mixture, adding hydrochloric acid to adjust the pH value of the starch mixture, stirring and emulsifying, adding 1% acrylic acid, 2% nano-silicon dioxide and 2% diphenylmethane diisocyanate by weight of the starch mixture, mixing at high speed, heating the starch mixture to 55° C., adding 0.1% catalyst by weight of the starch mixture, keeping the mixture warm for 4 hours, dehydrating and drying, and re-powdering until the powder passes a 100-mesh sieve to obtain the modified starch, which can enhance the performance of the modified starch.

[0009] Preferably, the modified epoxidized soybean oil includes epoxidized soybean oil, bisphenol A, ethylene glycol, adipic acid and an acid catalyst. The weight ratio of epoxidized soybean oil, bisphenol A, ethylene glycol, adipic acid and the acid catalyst in the modified epoxidized soybean oil is 93:3:1:1:2, which is conducive to modifying the epoxidized soybean oil.

[0010] Preferably, the preparation method of the modified epoxidized soybean oil is as follows: epoxy soybean oil, bisphenol A and ethylene glycol are obtained in proportion, the epoxy soybean oil, bisphenol A and ethylene glycol are added to a reactor to carry out an addition reaction, adipic acid is added to the reactor, a mixing reaction is continued, and finally an acid catalyst is added to the reactor and a catalytic reaction is carried out at 180° C., and then vacuum dehydration is carried out to prepare the modified epoxidized soybean oil, so as to facilitate the modification of the epoxy soybean oil.

[0011] Preferably, the preparation method of the protective film is as follows: modified starch, xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil are obtained in proportion, the modified starch and distilled water are added into an ultrasonic treatment tank in a ratio of 1:10, ultrasonic treatment is performed for 15 minutes, dehydration treatment is performed, ethanol with a concentration of 85%-95% is added, ultrasonic treatment is performed again, and after treatment for 20 minutes, ethanol is recovered to a concentration of 55% by a reduced pressure distillation method to obtain a modified starch emulsion; Xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil were added into a reactor, mixed at high speed for reaction, heated to 65°C during the mixing reaction, and then kept warm for 20 minutes. After the reaction was completed, the temperature was slowly lowered and cooled, and after cooling to room temperature, the modified starch emulsion was added, mixed thoroughly and evenly, and filtered to obtain a film-forming liquid. The film-forming liquid is poured into a homogenizing container, and dispersed homogenously at a speed of 3500rpm / min-4000rpm / min for 15 minutes. The homogenized liquid is coated on a glass plate, and dried at a temperature of 45°C for 12 hours. After drying, the film is peeled off to obtain a protective film. A protective film can be prepared.

[0012] A method for manufacturing an indicator-integrated deoxidizer packaging material comprises the following steps: S1: Obtain two protective films and a substrate, adhere the two protective films to the two sides of the substrate respectively, roll and flatten them, and then cut them to make deoxidizer packaging bags; S2: Obtain the protective film, cut it according to the size of the indicator bag, make the indicator bag, and fill it with the indicator to obtain the finished indicator bag; S3: The finished indicator bag is adhered to the deoxidizer packaging bag to obtain an indicator-integrated deoxidizer packaging material.

[0013] Preferably, in S1, the protective film is adhered to the substrate by environmentally friendly glue and is ironed by a roller to ensure the flatness of the deoxidizer packaging bag.

[0014] Preferably, in S3, an indicator pattern of a long strip of oxygen detection line is printed on the surface of the finished indicator bag for indication.

[0015] Beneficial effects of the present invention: The packaging bag is made of a base and a protective film. The paper material of the base itself has strong air permeability. At the same time, the material properties of the protective film allow a large number of gaps to exist inside it, so there is no need to punch holes, and it is not easy for the internal powder to leak. At the same time, the protective film is made of modified starch, xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil. It uses environmentally friendly materials and can be naturally degraded. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 The working flow chart proposed by the present invention. DETAILED DESCRIPTION

[0017] The present invention will be further explained below in conjunction with specific embodiments.

[0018] Reference Figure 1 , Embodiment 1 In this embodiment, an indicator-integrated deoxidizer packaging material is proposed, the deoxidizer packaging material comprises a packaging bag and an indicator bag bonded to the surface of the packaging bag, the packaging bag is made of a base and a protective film, the indicator bag is made of the protective film, and the indicator bag is filled with an indicator; The raw material composition and content of the protective film include 85 parts of modified starch, 0.85 parts of xylitol, 0.85 parts of polyvinyl alcohol, 3 parts of borax powder, 0.30 parts of sodium trimetaphosphate and 10 parts of modified epoxidized soybean oil by weight, and the modified starch includes corn starch, cassava starch and potato starch; The base is mainly made of log pulp, the packaging bag is bonded to the indicator bag by environmentally friendly glue, the weight ratio of corn starch, tapioca starch and potato starch in the modified starch is 1:1:1, and the corn starch, tapioca starch and potato starch are all sieved through a 100-mesh sieve; Preparation method of modified starch: corn starch, cassava starch and potato starch are obtained, deionized water of 10 times the total amount thereof is added, mixed evenly to obtain a starch mixture, hydrochloric acid is added to adjust the pH value of the starch mixture, after stirring and emulsifying, 1% of acrylic acid, 2% of nano silicon dioxide and 2% of diphenylmethane diisocyanate are added to the starch mixture by weight, mixed at high speed, and the temperature of the starch mixture is heated to 55° C., a catalyst of 0.1% by weight of the starch mixture is added, the mixture is kept warm for reaction for 4 hours, dehydrated and dried, and re-powdered until the powder passes through a 100-mesh sieve to obtain modified starch; The modified epoxidized soybean oil comprises epoxidized soybean oil, bisphenol A, ethylene glycol, adipic acid and an acid catalyst, wherein the weight ratio of the epoxidized soybean oil, bisphenol A, ethylene glycol, adipic acid and the acid catalyst in the modified epoxidized soybean oil is 93:3:1:1:2; The preparation method of modified epoxy soybean oil comprises: obtaining epoxy soybean oil, bisphenol A and ethylene glycol according to a proportion, adding the epoxy soybean oil, bisphenol A and ethylene glycol into a reaction kettle, carrying out an addition reaction, adding adipic acid into the reaction kettle, continuing to carry out a mixing reaction, and finally adding an acid catalyst into the reaction kettle, carrying out a catalytic reaction at 180° C., and then carrying out vacuum dehydration to prepare modified epoxy soybean oil; Preparation method of protective film: modified starch, xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil are obtained in proportion, and the modified starch and distilled water are added into an ultrasonic treatment tank in a ratio of 1:10, and ultrasonic treatment is performed for 15 minutes, followed by dehydration treatment, and ethanol with a concentration of 85%-95% is added, and ultrasonic treatment is performed again. After treatment for 20 minutes, the ethanol is recovered by a reduced pressure distillation method to a concentration of 55%, and a modified starch emulsion is obtained; Xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil were added into a reactor, mixed at high speed for reaction, heated to 65°C during the mixing reaction, and then kept warm for 20 minutes. After the reaction was completed, the temperature was slowly lowered and cooled, and after cooling to room temperature, the modified starch emulsion was added, mixed thoroughly and evenly, and filtered to obtain a film-forming liquid. Pour the film-forming liquid into a homogenizing container, homogenize and disperse it at a speed of 3500rpm / min-4000rpm / min for 15 minutes, apply the homogenized liquid on a glass plate, dry it at a temperature of 45°C for 12 hours, and peel off the film after drying to obtain a protective film; The packaging bag is made of a base and a protective film. The paper material of the base itself has strong air permeability. At the same time, the material properties of the protective film allow a large number of gaps to exist inside it, so there is no need to punch holes, and it is not easy for the internal powder to leak. At the same time, the protective film is made of modified starch, xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil. It uses environmentally friendly materials and can be naturally degraded.

[0019] A method for manufacturing an indicator-integrated deoxidizer packaging material comprises the following steps: S1: Obtain two protective films and a substrate, adhere the two protective films to the two sides of the substrate respectively, roll flat and then cut, adhere the protective films to the substrate with environmentally friendly glue, use roller ironing treatment, and finally make deoxidizer packaging bags; S2: Obtain the protective film, cut it according to the size of the indicator bag, make the indicator bag, and fill it with the indicator to obtain the finished indicator bag; S3: The finished indicator bag is adhered to the deoxidizer packaging bag to obtain an indicator-integrated deoxidizer packaging material, and a surface of the finished indicator bag is printed with an indicator pattern of a long strip of oxygen detection line.

[0020] Reference Figure 1 , Embodiment 2 In this embodiment, an indicator-integrated deoxidizer packaging material is proposed, the deoxidizer packaging material comprises a packaging bag and an indicator bag bonded to the surface of the packaging bag, the packaging bag is made of a base and a protective film, the indicator bag is made of the protective film, and the indicator bag is filled with an indicator; The raw material composition and content of the protective film include 83 parts of modified starch, 0.80 parts of xylitol, 0.80 parts of polyvinyl alcohol, 3 parts of borax powder, 0.40 parts of sodium trimetaphosphate and 12 parts of modified epoxidized soybean oil by weight, and the modified starch includes corn starch, cassava starch and potato starch; The base is mainly made of log pulp, the packaging bag is bonded to the indicator bag by environmentally friendly glue, the weight ratio of corn starch, tapioca starch and potato starch in the modified starch is 1:1:1, and the corn starch, tapioca starch and potato starch are all sieved through a 100-mesh sieve; Preparation method of modified starch: corn starch, cassava starch and potato starch are obtained, deionized water of 10 times the total amount thereof is added, mixed evenly to obtain a starch mixture, hydrochloric acid is added to adjust the pH value of the starch mixture, after stirring and emulsifying, 1% of acrylic acid, 2% of nano silicon dioxide and 2% of diphenylmethane diisocyanate are added to the starch mixture by weight, mixed at high speed, and the temperature of the starch mixture is heated to 55° C., a catalyst of 0.1% by weight of the starch mixture is added, the mixture is kept warm for reaction for 4 hours, dehydrated and dried, and re-powdered until the powder passes through a 100-mesh sieve to obtain modified starch; The modified epoxidized soybean oil comprises epoxidized soybean oil, bisphenol A, ethylene glycol, adipic acid and an acid catalyst, wherein the weight ratio of the epoxidized soybean oil, bisphenol A, ethylene glycol, adipic acid and the acid catalyst in the modified epoxidized soybean oil is 93:3:1:1:2; The preparation method of modified epoxy soybean oil comprises: obtaining epoxy soybean oil, bisphenol A and ethylene glycol according to a proportion, adding the epoxy soybean oil, bisphenol A and ethylene glycol into a reaction kettle, carrying out an addition reaction, adding adipic acid into the reaction kettle, continuing to carry out a mixing reaction, and finally adding an acid catalyst into the reaction kettle, carrying out a catalytic reaction at 180° C., and then carrying out vacuum dehydration to prepare modified epoxy soybean oil; Preparation method of protective film: modified starch, xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil are obtained in proportion, and the modified starch and distilled water are added into an ultrasonic treatment tank in a ratio of 1:10, and ultrasonic treatment is performed for 15 minutes, followed by dehydration treatment, and ethanol with a concentration of 85%-95% is added, and ultrasonic treatment is performed again. After treatment for 20 minutes, the ethanol is recovered by a reduced pressure distillation method to a concentration of 55%, and a modified starch emulsion is obtained; Xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil were added into a reactor, mixed at high speed for reaction, heated to 65°C during the mixing reaction, and then kept warm for 20 minutes. After the reaction was completed, the temperature was slowly lowered and cooled, and after cooling to room temperature, the modified starch emulsion was added, mixed thoroughly and evenly, and filtered to obtain a film-forming liquid. Pour the film-forming liquid into a homogenizing container, homogenize and disperse it at a speed of 3500rpm / min-4000rpm / min for 15 minutes, apply the homogenized liquid on a glass plate, dry it at a temperature of 45°C for 12 hours, and peel off the film after drying to obtain a protective film; The packaging bag is made of a base and a protective film. The paper material of the base itself has strong air permeability. At the same time, the material properties of the protective film allow a large number of gaps to exist inside it, so there is no need to punch holes, and it is not easy for the internal powder to leak. At the same time, the protective film is made of modified starch, xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil. It uses environmentally friendly materials and can be naturally degraded.

[0021] A method for manufacturing an indicator-integrated deoxidizer packaging material comprises the following steps: S1: Obtain two protective films and a substrate, adhere the two protective films to the two sides of the substrate respectively, roll flat and then cut, adhere the protective films to the substrate with environmentally friendly glue, use roller ironing treatment, and finally make deoxidizer packaging bags; S2: Obtain the protective film, cut it according to the size of the indicator bag, make the indicator bag, and fill it with the indicator to obtain the finished indicator bag; S3: The finished indicator bag is adhered to the deoxidizer packaging bag to obtain an indicator-integrated deoxidizer packaging material, and a surface of the finished indicator bag is printed with an indicator pattern of a long strip of oxygen detection line.

[0022] Reference Figure 1 , Embodiment 3 In this embodiment, an indicator-integrated deoxidizer packaging material is proposed, the deoxidizer packaging material comprises a packaging bag and an indicator bag bonded to the surface of the packaging bag, the packaging bag is made of a base and a protective film, the indicator bag is made of the protective film, and the indicator bag is filled with an indicator; The raw material composition and content of the protective film include 84 parts of modified starch, 0.90 parts of xylitol, 0.80 parts of polyvinyl alcohol, 3 parts of borax powder, 0.30 parts of sodium trimetaphosphate and 11 parts of modified epoxidized soybean oil by weight, and the modified starch includes corn starch, cassava starch and potato starch; The base is mainly made of log pulp, the packaging bag is bonded to the indicator bag by environmentally friendly glue, the weight ratio of corn starch, tapioca starch and potato starch in the modified starch is 1:1:1, and the corn starch, tapioca starch and potato starch are all sieved through a 100-mesh sieve; Preparation method of modified starch: corn starch, cassava starch and potato starch are obtained, deionized water of 10 times the total amount thereof is added, mixed evenly to obtain a starch mixture, hydrochloric acid is added to adjust the pH value of the starch mixture, after stirring and emulsifying, 1% of acrylic acid, 2% of nano silicon dioxide and 2% of diphenylmethane diisocyanate are added to the starch mixture by weight, mixed at high speed, and the temperature of the starch mixture is heated to 55° C., a catalyst of 0.1% by weight of the starch mixture is added, the mixture is kept warm for reaction for 4 hours, dehydrated and dried, and re-powdered until the powder passes through a 100-mesh sieve to obtain modified starch; The modified epoxidized soybean oil comprises epoxidized soybean oil, bisphenol A, ethylene glycol, adipic acid and an acid catalyst, wherein the weight ratio of the epoxidized soybean oil, bisphenol A, ethylene glycol, adipic acid and the acid catalyst in the modified epoxidized soybean oil is 93:3:1:1:2; The preparation method of modified epoxy soybean oil comprises: obtaining epoxy soybean oil, bisphenol A and ethylene glycol according to a proportion, adding the epoxy soybean oil, bisphenol A and ethylene glycol into a reaction kettle, carrying out an addition reaction, adding adipic acid into the reaction kettle, continuing to carry out a mixing reaction, and finally adding an acid catalyst into the reaction kettle, carrying out a catalytic reaction at 180° C., and then carrying out vacuum dehydration to prepare modified epoxy soybean oil; Preparation method of protective film: modified starch, xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil are obtained in proportion, and the modified starch and distilled water are added into an ultrasonic treatment tank in a ratio of 1:10, and ultrasonic treatment is performed for 15 minutes, followed by dehydration treatment, and ethanol with a concentration of 85%-95% is added, and ultrasonic treatment is performed again. After treatment for 20 minutes, the ethanol is recovered by a reduced pressure distillation method to a concentration of 55%, and a modified starch emulsion is obtained; Xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil were added into a reactor, mixed at high speed for reaction, heated to 65°C during the mixing reaction, and then kept warm for 20 minutes. After the reaction was completed, the temperature was slowly lowered and cooled, and after cooling to room temperature, the modified starch emulsion was added, mixed thoroughly and evenly, and filtered to obtain a film-forming liquid. Pour the film-forming liquid into a homogenizing container, homogenize and disperse it at a speed of 3500rpm / min-4000rpm / min for 15 minutes, apply the homogenized liquid on a glass plate, dry it at a temperature of 45°C for 12 hours, and peel off the film after drying to obtain a protective film; The packaging bag is made of a base and a protective film. The paper material of the base itself has strong air permeability. At the same time, the material properties of the protective film allow a large number of gaps to exist inside it, so there is no need to punch holes, and it is not easy for the internal powder to leak. At the same time, the protective film is made of modified starch, xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil. It uses environmentally friendly materials and can be naturally degraded.

[0023] A method for manufacturing an indicator-integrated deoxidizer packaging material comprises the following steps: S1: Obtain two protective films and a substrate, adhere the two protective films to the two sides of the substrate respectively, roll flat and then cut, adhere the protective films to the substrate with environmentally friendly glue, use roller ironing treatment, and finally make deoxidizer packaging bags; S2: Obtain the protective film, cut it according to the size of the indicator bag, make the indicator bag, and fill it with the indicator to obtain the finished indicator bag; S3: The finished indicator bag is adhered to the deoxidizer packaging bag to obtain an indicator-integrated deoxidizer packaging material, and a surface of the finished indicator bag is printed with an indicator pattern of a long strip of oxygen detection line.

[0024] Reference Figure 1 , Embodiment 4 In this embodiment, an indicator-integrated deoxidizer packaging material is proposed, the deoxidizer packaging material comprises a packaging bag and an indicator bag bonded to the surface of the packaging bag, the packaging bag is made of a base and a protective film, the indicator bag is made of the protective film, and the indicator bag is filled with an indicator; The raw material composition and content of the protective film include 86 parts of modified starch, 0.90 parts of xylitol, 0.90 parts of polyvinyl alcohol, 3 parts of borax powder, 0.20 parts of sodium trimetaphosphate and 9 parts of modified epoxidized soybean oil by weight, and the modified starch includes corn starch, cassava starch and potato starch; The base is mainly made of log pulp, the packaging bag is bonded to the indicator bag by environmentally friendly glue, the weight ratio of corn starch, tapioca starch and potato starch in the modified starch is 1:1:1, and the corn starch, tapioca starch and potato starch are all sieved through a 100-mesh sieve; Preparation method of modified starch: corn starch, cassava starch and potato starch are obtained, deionized water of 10 times the total amount thereof is added, mixed evenly to obtain a starch mixture, hydrochloric acid is added to adjust the pH value of the starch mixture, after stirring and emulsifying, 1% of acrylic acid, 2% of nano silicon dioxide and 2% of diphenylmethane diisocyanate are added to the starch mixture by weight, mixed at high speed, and the temperature of the starch mixture is heated to 55° C., a catalyst of 0.1% by weight of the starch mixture is added, the mixture is kept warm for reaction for 4 hours, dehydrated and dried, and re-powdered until the powder passes through a 100-mesh sieve to obtain modified starch; The modified epoxidized soybean oil comprises epoxidized soybean oil, bisphenol A, ethylene glycol, adipic acid and an acid catalyst, wherein the weight ratio of the epoxidized soybean oil, bisphenol A, ethylene glycol, adipic acid and the acid catalyst in the modified epoxidized soybean oil is 93:3:1:1:2; The preparation method of modified epoxy soybean oil comprises: obtaining epoxy soybean oil, bisphenol A and ethylene glycol according to a proportion, adding the epoxy soybean oil, bisphenol A and ethylene glycol into a reaction kettle, carrying out an addition reaction, adding adipic acid into the reaction kettle, continuing to carry out a mixing reaction, and finally adding an acid catalyst into the reaction kettle, carrying out a catalytic reaction at 180° C., and then carrying out vacuum dehydration to prepare modified epoxy soybean oil; Preparation method of protective film: modified starch, xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil are obtained in proportion, and the modified starch and distilled water are added into an ultrasonic treatment tank in a ratio of 1:10, and ultrasonic treatment is performed for 15 minutes, followed by dehydration treatment, and ethanol with a concentration of 85%-95% is added, and ultrasonic treatment is performed again. After treatment for 20 minutes, the ethanol is recovered by a reduced pressure distillation method to a concentration of 55%, and a modified starch emulsion is obtained; Xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil were added into a reactor, mixed at high speed for reaction, heated to 65°C during the mixing reaction, and then kept warm for 20 minutes. After the reaction was completed, the temperature was slowly lowered and cooled, and after cooling to room temperature, the modified starch emulsion was added, mixed thoroughly and evenly, and filtered to obtain a film-forming liquid. Pour the film-forming liquid into a homogenizing container, homogenize and disperse it at a speed of 3500rpm / min-4000rpm / min for 15 minutes, apply the homogenized liquid on a glass plate, dry it at a temperature of 45°C for 12 hours, and peel off the film after drying to obtain a protective film; The packaging bag is made of a base and a protective film. The paper material of the base itself has strong air permeability. At the same time, the material properties of the protective film allow a large number of gaps to exist inside it, so there is no need to punch holes, and it is not easy for the internal powder to leak. At the same time, the protective film is made of modified starch, xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil. It uses environmentally friendly materials and can be naturally degraded.

[0025] A method for manufacturing an indicator-integrated deoxidizer packaging material comprises the following steps: S1: Obtain two protective films and a substrate, adhere the two protective films to the two sides of the substrate respectively, roll flat and then cut, adhere the protective films to the substrate with environmentally friendly glue, use roller ironing treatment, and finally make deoxidizer packaging bags; S2: Obtain the protective film, cut it according to the size of the indicator bag, make the indicator bag, and fill it with the indicator to obtain the finished indicator bag; S3: The finished indicator bag is adhered to the deoxidizer packaging bag to obtain an indicator-integrated deoxidizer packaging material, and a surface of the finished indicator bag is printed with an indicator pattern of a long strip of oxygen detection line.

[0026] Reference Figure 1 Embodiment 5 In this embodiment, an indicator-integrated deoxidizer packaging material is proposed, the deoxidizer packaging material comprises a packaging bag and an indicator bag bonded to the surface of the packaging bag, the packaging bag is made of a base and a protective film, the indicator bag is made of the protective film, and the indicator bag is filled with an indicator; The raw material composition and content of the protective film include 88 parts of modified starch, 0.95 parts of xylitol, 0.95 parts of polyvinyl alcohol, 2 parts of borax powder, 0.10 parts of sodium trimetaphosphate and 8 parts of modified epoxidized soybean oil by weight, and the modified starch includes corn starch, cassava starch and potato starch; The base is mainly made of log pulp, the packaging bag is bonded to the indicator bag by environmentally friendly glue, the weight ratio of corn starch, tapioca starch and potato starch in the modified starch is 1:1:1, and the corn starch, tapioca starch and potato starch are all sieved through a 100-mesh sieve; Preparation method of modified starch: corn starch, cassava starch and potato starch are obtained, deionized water of 10 times the total amount thereof is added, mixed evenly to obtain a starch mixture, hydrochloric acid is added to adjust the pH value of the starch mixture, after stirring and emulsifying, 1% of acrylic acid, 2% of nano silicon dioxide and 2% of diphenylmethane diisocyanate are added to the starch mixture by weight, mixed at high speed, and the temperature of the starch mixture is heated to 55° C., a catalyst of 0.1% by weight of the starch mixture is added, the mixture is kept warm for reaction for 4 hours, dehydrated and dried, and re-powdered until the powder passes through a 100-mesh sieve to obtain modified starch; The modified epoxidized soybean oil comprises epoxidized soybean oil, bisphenol A, ethylene glycol, adipic acid and an acid catalyst, wherein the weight ratio of the epoxidized soybean oil, bisphenol A, ethylene glycol, adipic acid and the acid catalyst in the modified epoxidized soybean oil is 93:3:1:1:2; The preparation method of modified epoxy soybean oil comprises: obtaining epoxy soybean oil, bisphenol A and ethylene glycol according to a proportion, adding the epoxy soybean oil, bisphenol A and ethylene glycol into a reaction kettle, carrying out an addition reaction, adding adipic acid into the reaction kettle, continuing to carry out a mixing reaction, and finally adding an acid catalyst into the reaction kettle, carrying out a catalytic reaction at 180° C., and then carrying out vacuum dehydration to prepare modified epoxy soybean oil; Preparation method of protective film: modified starch, xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil are obtained in proportion, and the modified starch and distilled water are added into an ultrasonic treatment tank in a ratio of 1:10, and ultrasonic treatment is performed for 15 minutes, followed by dehydration treatment, and ethanol with a concentration of 85%-95% is added, and ultrasonic treatment is performed again. After treatment for 20 minutes, the ethanol is recovered by a reduced pressure distillation method to a concentration of 55%, and a modified starch emulsion is obtained; Xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil were added into a reactor, mixed at high speed for reaction, heated to 65°C during the mixing reaction, and then kept warm for 20 minutes. After the reaction was completed, the temperature was slowly lowered and cooled, and after cooling to room temperature, the modified starch emulsion was added, mixed thoroughly and evenly, and filtered to obtain a film-forming liquid. Pour the film-forming liquid into a homogenizing container, homogenize and disperse it at a speed of 3500rpm / min-4000rpm / min for 15 minutes, apply the homogenized liquid on a glass plate, dry it at a temperature of 45°C for 12 hours, and peel off the film after drying to obtain a protective film; The packaging bag is made of a base and a protective film. The paper material of the base itself has strong air permeability. At the same time, the material properties of the protective film allow a large number of gaps to exist inside it, so there is no need to punch holes, and it is not easy for the internal powder to leak. At the same time, the protective film is made of modified starch, xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil. It uses environmentally friendly materials and can be naturally degraded.

[0027] A method for manufacturing an indicator-integrated deoxidizer packaging material comprises the following steps: S1: Obtain two protective films and a substrate, adhere the two protective films to the two sides of the substrate respectively, roll flat and then cut, adhere the protective films to the substrate with environmentally friendly glue, use roller ironing treatment, and finally make deoxidizer packaging bags; S2: Obtain the protective film, cut it according to the size of the indicator bag, make the indicator bag, and fill it with the indicator to obtain the finished indicator bag; S3: The finished indicator bag is adhered to the deoxidizer packaging bag to obtain an indicator-integrated deoxidizer packaging material, and a surface of the finished indicator bag is printed with an indicator pattern of a long strip of oxygen detection line.

[0028] Comparing the conventional deoxidizer packaging material with the deoxidizer packaging material prepared in Examples 1 to 5, the deoxidizer packaging materials prepared in Examples 1 to 5 are as follows: Comparative Example Embodiment 1 Embodiment 2 Embodiment 3 Embodiment 4 Embodiment 5 Is it degradable? no yes yes yes yes yes Powder leakage prevention Failure qualified qualified qualified qualified qualified The test method for anti-leakage powder performance is as follows: take a package of samples, cut open the sealed edge and pour out the raw materials. Place the packaging material flat on the table and lay two layers of facial tissue under it. Use colored liquid red ink and use a burette to drop 0.1 ml of red ink onto the surface of the packaging material, which is about half of the air permeability area of ​​the unit piece. After standing for 5 minutes, check whether the facial tissue under the product absorbs the colored liquid red ink. If there is no absorption of red ink, it means the product is qualified.

[0029] It can be seen from the above table that the degradability and anti-leakage property of the deoxidizer packaging material prepared by the present invention are significantly improved.

[0030] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. An indicator-integrated deoxidizer packaging material, characterized in that: The deoxidizer packaging material comprises a packaging bag and an indicator bag bonded to the surface of the packaging bag, the packaging bag is made of a substrate and a protective film, the indicator bag is made of the protective film, and the inside of the indicator bag is filled with an indicator; The raw material composition and content of the protective film include 80 to 90 parts of modified starch, 0.50 to 1.00 parts of xylitol, 0.50 to 1.00 parts of polyvinyl alcohol, 1 to 5 parts of borax powder, 0.10 to 0.50 parts of sodium trimetaphosphate and 7 to 15 parts of modified epoxidized soybean oil by mass. The modified starch includes corn starch, cassava starch and potato starch.

2. The indicator-integrated deoxidizer packaging material according to claim 1, characterized in that: The base is mainly made of log pulp, and the packaging bag is bonded to the indicator bag by environmentally friendly glue.

3. The indicator-integrated deoxidizer packaging material according to claim 1, characterized in that: The weight ratio of corn starch, cassava starch and potato starch in the modified starch is 1-2: (1-2): 1-2, and the corn starch, cassava starch and potato starch are all sieved through a 100-mesh sieve.

4. The indicator-integrated deoxidizer packaging material according to claim 1, characterized in that: The preparation method of the modified starch comprises the following steps: obtaining corn starch, cassava starch and potato starch, adding deionized water in an amount of 10 times the total amount thereof, mixing evenly to obtain a starch mixture, adding hydrochloric acid to adjust the pH value of the starch mixture, stirring and emulsifying, adding 1% by weight of acrylic acid, 2% by weight of nano silicon dioxide and 2% by weight of diphenylmethane diisocyanate to the starch mixture, mixing at high speed, heating the starch mixture to 55° C., adding 0.1% by weight of a catalyst to the starch mixture, keeping the temperature for reaction for 4 hours, dehydrating and drying, and re-powdering until the powder passes through a 100-mesh sieve to obtain the modified starch.

5. The indicator-integrated deoxidizer packaging material according to claim 1, characterized in that: The modified epoxidized soybean oil comprises epoxidized soybean oil, bisphenol A, ethylene glycol, adipic acid and an acid catalyst. The weight ratio of the epoxidized soybean oil, bisphenol A, ethylene glycol, adipic acid and the acid catalyst in the modified epoxidized soybean oil is 93:3:1:1:

2.

6. The indicator-integrated deoxidizer packaging material according to claim 5, characterized in that: The preparation method of the modified epoxy soybean oil comprises the following steps: obtaining epoxy soybean oil, bisphenol A and ethylene glycol in proportion, adding the epoxy soybean oil, bisphenol A and ethylene glycol into a reaction kettle for addition reaction, adding adipic acid into the reaction kettle, continuing the mixing reaction, and finally adding an acid catalyst into the reaction kettle for catalytic reaction at 180° C., and then vacuum dehydrating to obtain the modified epoxy soybean oil.

7. The indicator-integrated deoxidizer packaging material according to claim 1, characterized in that: The preparation method of the protective film comprises: obtaining modified starch, xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxy soybean oil in proportion, adding the modified starch and distilled water in a ratio of 1:10 into an ultrasonic treatment tank, performing ultrasonic treatment for 15 minutes, performing dehydration treatment, adding ethanol with a concentration of 85%-95%, performing ultrasonic treatment again, and after treating for 20 minutes, recovering ethanol to a concentration of 55% by a reduced pressure distillation method to obtain a modified starch emulsion; Xylitol, polyvinyl alcohol, borax powder, sodium trimetaphosphate and modified epoxidized soybean oil were added into a reactor, mixed at high speed for reaction, heated to 65°C during the mixing reaction, and then kept warm for 20 minutes. After the reaction was completed, the temperature was slowly lowered and cooled, and after cooling to room temperature, the modified starch emulsion was added, mixed thoroughly and evenly, and filtered to obtain a film-forming liquid. The film-forming liquid was poured into a homogenizing container and dispersed homogenously at a speed of 3500-4000 rpm / min for 15 minutes. The homogenized liquid was coated on a glass plate and dried at 45°C for 12 hours. After drying, the film was peeled off to obtain a protective film.

8. A method for preparing an indicator-integrated deoxidizer packaging material as claimed in claim 1, characterized in that: The following steps are involved: S1: Obtain two protective films and a substrate, adhere the two protective films to the two sides of the substrate respectively, roll and flatten them, and then cut them to make deoxidizer packaging bags; S2: Obtain the protective film, cut it according to the size of the indicator bag, make the indicator bag, and fill it with the indicator to obtain the finished indicator bag; S3: The finished indicator bag is adhered to the deoxidizer packaging bag to obtain an indicator-integrated deoxidizer packaging material.

9. The method for manufacturing an indicator-integrated deoxidizer packaging material according to claim 8, characterized in that: In S1, the protective film is adhered to the substrate by environmentally friendly glue and is processed by roller ironing.

10. The method for manufacturing an indicator-integrated deoxidizer packaging material according to claim 8, characterized in that: In S3, an indicator pattern of a long strip of oxygen detection line is printed on the surface of the finished indicator bag.

Citation Information

Patent Citations

  • Barrier film

    CN101360783A

  • Preparation method for starch-polyvinyl alcohol biologically-cross-linked nano-composite plastic film

    CN103289131A

  • Starch nanocomposite film and preparation method thereof

    CN104356428A

  • PBAT composite modified biodegradable material and preparation method thereof

    CN113429759A

  • Oxygen indication type deoxidizer

    CN209522059U