Wormlike micelle with pH response and preparation method thereof

By using dynamic ion pair self-assembly method of raw material A and acid in pH-responsive worm-like micelles, the preparation process is simplified, the complex covalent method problems in the prior art are solved, and significant under stimulation of slight pH is achieved The change in rheological properties has expanded the application potential.

CN118995240APending Publication Date: 2024-11-22GREATER BAY AREA INST FOR INNOVATION HUNAN UNIV
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411487503.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-24
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The preparation process of existing pH-responsive worm-like micelles involves covalent methods for introducing stimulus-responsive groups and building ultra-long hydrophobic chains, resulting in complex synthesis and purification processes.

Method used

The raw material A and acid are mixed at a specific mass ratio, and a dynamic ion pair is formed by van der Waals force and ion pair electrostatic force to prepare a worm-like micelle with pH response, which simplifies the preparation process and uses -COOH and -NH2, - NCH3 serves as a good pH stimulation response group to achieve efficient self-assembly of worm-like micelles.

Benefits of technology

简化了制备过程,降低了复杂性,扩大了应用潜能,实现了在微小pH刺激下显著转变流变性质的能力,适用于石油工业和其他技术应用。

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118995240A_ABST
    Figure CN118995240A_ABST
Patent Text Reader

Abstract

The invention discloses a wormlike micelle with pH response and a preparation method thereof, and relates to the technical field of colloid and surface and interface chemistry, the preparation method comprises the following steps: at 25-90 DEG C, adding a raw material A and acid into water, and mixing to obtain the wormlike micelle with pH response. A raw material A and acid form a dynamic ion pair through protonation / deprotonation action and classical acting force, and the dynamic ion pair not only can be efficiently self-assembled into wormlike micelles, but also has good adjustability, so that a system quickly responds under tiny stimulation, a response window is narrow, and good adjustability is shown.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of colloid and surface interface chemistry, and in particular to a worm-like micelle with pH response and a preparation method thereof. Background Art

[0002] Smart, responsive wormlike micelles constructed based on surfactant self-assembly have attracted considerable attention due to their combined self-assembly, dynamic response, and controllable properties. These smart, responsive wormlike micelles can respond to one or more stimuli, including temperature, light, pH, redox, CO2, and magnetism. pH-responsive smart wormlike micelles are the most widely studied of all smart responsive materials due to their rapid response, low cost, and ease of industrial production. They have shown broad application prospects in a variety of fields, including oil color enhancement and daily chemical care.

[0003] The construction of pH-responsive wormlike micelle systems typically involves covalently introducing responsive groups to impart intelligent responsiveness to the wormlike micelles. Alternatively, ultralong hydrophobic chains are constructed based on this covalent approach to promote the efficient self-assembly of surfactant molecules into wormlike micelles. However, both the covalent introduction of stimulatory groups and the construction of ultralong hydrophobic carbon chains involve complex organic synthesis and purification, complicating the preparation process. Summary of the Invention

[0004] In order to solve the complexity problem of the synthesis and purification process involved in the construction of worm-like micelles in the prior art, the present invention provides a pH-responsive worm-like micelle and a preparation method thereof.

[0005] To achieve the above objectives, the specific technical solutions of the present invention are as follows.

[0006] The first aspect of the present invention provides a method for preparing pH-responsive worm-like micelles, comprising the following steps: Raw material A and acid are added to water at a mass ratio of 1.4-3.92:0.29-1.14 at 25-90°C to obtain pH-responsive worm-like micelles; The mass ratio of the sum of the raw material A and the acid to water is 2-5:95-196; The raw material A is hexadecylamine, octadecylamine, N,N -Dimethylhexadecyl tertiary amine, N,N -dimethyloctadecyl tertiary amine, N,N- Any one of dihydroxyethyl octadecyl tertiary amine and oleylamine; The acid is any one of formic acid, acetic acid, propionic acid, hexanoic acid and salicylic acid.

[0007] The present invention uses raw material A and acid to form worm-like micelles with dynamic ion pairs under the action of van der Waals forces and ion-pair electrostatic forces. The entire preparation process does not involve the introduction of covalent bonds or the construction of ultra-long hydrophobic carbon chains. The mixture is mixed at a mass ratio of 2-5:95-196 of the total mass of raw material A and acid to water to produce pH-responsive worm-like micelles, thereby simplifying the preparation process. Because both -COOH and -NR1R2 are well-characterized groups that respond to pH stimulation, the system is endowed with the ability to undergo significant changes in rheological properties under slight pH stimulation. R1 and R2 are H or CH3 in raw material A. Furthermore, when raw material A and acid are mixed at a mass ratio of 1.4-3.92:0.29-1.14, they can synergistically and efficiently self-assemble into worm-like micelles, demonstrating superior self-assembly capabilities comparable to those of polyacid synergistic systems. This significantly reduces the complexity of preparing pH-responsive worm-like micelles and expands their application potential.

[0008] In another preferred embodiment, when raw material A is hexadecylamine, the corresponding acid is butyric acid; when raw material A is octadecylamine, the corresponding acid is any one of formic acid, acetic acid, propionic acid, and butyric acid; when raw material A is N,N - When the raw material A is N,N - Dihydroxyethyl octadecyl tertiary amine, the corresponding acid is salicylic acid; when raw material A is oleylamine, the corresponding acid is any one of formic acid, propionic acid, and butyric acid.

[0009] In another preferred embodiment, the mixing is performed by stirring.

[0010] In another preferred embodiment, the stirring time is 2 hours to 12 hours, and the stirring speed is 1000 rpm to 1200 rpm.

[0011] The second aspect of the present invention provides a pH-responsive worm-like micelle, which is prepared by the preparation method provided by the first aspect of the present invention.

[0012] In another preferred embodiment, the zero shear viscosity of the pH-responsive worm-like micelles is 500 mPa·S to 200,000 mPa·S.

[0013] In another preferred embodiment, the pH response means that when the pH value of the worm-like micelles is changed to less than 3 or greater than 6, the viscosity thereof decreases to below 20 mPa·S.

[0014] Compared with the prior art, the present invention has the following beneficial effects: (1) The raw materials A and acid used in the present invention are simple in structure and low in price. The entire reaction process is mild, does not require high temperature reaction, and does not involve complex purification of organic synthesis agents, which effectively simplifies the preparation process. During the preparation process, the raw materials A and acid only need to be mixed in water at a mass ratio of 1.4~3.92:0.29~1.14. In the absence of external reagents, the raw materials A and acid form dynamic ion pairs through protonation / deprotonation, van der Waals force and ion pair electrostatic force. The dynamic ion pairs can not only efficiently self-assemble into worm-like micelles, but also have good controllability. In addition, the dynamic ion pair worm-like micelles based on raw materials A / acid have good pH stimulus response groups, which endow the system with the ability to undergo significant changes in rheological properties under slight pH stimulation.

[0015] (2) The present invention uses a simple and economical raw material A and an acid in a mass ratio of 1.4-3.92:0.29-1.14 to synergistically self-assemble into worm-like micelles, showing a superior self-assembly ability comparable to that of a polyacid synergistic system, greatly reducing the complexity of preparing pH-responsive worm-like micelles and expanding their application potential. When tens of microliters of 0.5 mol / L NaOH solution are added to ten milliliters of the worm-like micelle system, a rapid response occurs, and the response window is narrow, especially when the pH value changes by less than 3, a response can occur, showing good controllability. It has great potential in the petroleum industry and other technical applications, including molecular devices and sensors, drug delivery, cleaning processes, drag reduction, textile printing and dyeing, etc.

[0016] (3) Based on the molecular stacking theory and intermolecular interactions, the present invention proposes a more concise and efficient strategy, namely, based on the raw material A, a bulk chemical with a mature production process and simple structure, and based on ionizable dynamic ion pairs and their construction methods. By taking advantage of the low-cost, easily available raw material A and the property of the acid as potential dynamic ion pairs, through the design and screening of the molecular structure, and comprehensively utilizing the van der Waals force and ion pair electrostatic force in the classical interaction force, the chain length matching effect, and the protonation / deprotonation of amines / acids, the system is endowed with the ability to undergo significant changes in its rheological properties under slight pH stimulation. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 1 is a graph showing the relationship between shear viscosity and shear rate of the pH-responsive worm-like micelles at different pH values ​​in Example 1 of the present invention.

[0018] Figure 2 1 is a graph showing the relationship between shear viscosity and shear rate of the pH-responsive worm-like micelles at different pH values ​​in Example 2 of the present invention.

[0019] Figure 3 3 is a graph showing the relationship between shear viscosity and shear rate of the pH-responsive worm-like micelles at different pH values ​​in Example 3 of the present invention.

[0020] Figure 4 4 is a graph showing the relationship between shear viscosity and shear rate of the pH-responsive worm-like micelles at different pH values ​​in Example 4 of the present invention.

[0021] Figure 5 1 is a graph showing the relationship between shear viscosity and shear rate of the pH-responsive worm-like micelles at different pH values ​​in Example 5 of the present invention.

[0022] Figure 6 1 is a graph showing the relationship between shear viscosity and shear rate of the pH-responsive worm-like micelles at different pH values ​​in Example 6 of the present invention.

[0023] Figure 7 1 is a graph showing the relationship between shear viscosity and shear rate of the pH-responsive worm-like micelles at different pH values ​​in Example 7 of the present invention. DETAILED DESCRIPTION

[0024] In order to more clearly understand the above-mentioned objects, features and advantages of the present invention, the present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. It should be noted that, in the absence of conflict, the embodiments of the present application and the features therein can be combined with each other.

[0025] In the following description, many specific details are set forth to facilitate a full understanding of the present invention. However, the present invention may also be implemented in other ways different from those described herein. Therefore, the scope of protection of the present invention is not limited to the specific embodiments disclosed below.

[0026] Example 1 A method for preparing pH-responsive worm-like micelles comprises the following steps: 1.44 g of N,N-dimethyloctadecyl tertiary amine and 0.56 g of hexanoic acid were added to 98 g of distilled water, the water bath temperature was maintained at 90 ° C, and the mixture was stirred at 1200 rpm for 2 h to obtain the N,N-dimethyloctadecyl tertiary amine / hexanoic acid system, i.e., pH-responsive worm-like micelles; wherein, N,N - The dimethyloctadecylamine / hexanoic acid system exhibits a clear and transparent high-viscosity viscoelastic fluid.

[0027] Rheological testing of the N,N-dimethyloctadecylamine / hexanoic acid system at 25°C revealed steady-state rheological results demonstrating a Newtonian fluid at low shear rates and a shear-thinning fluid at high shear rates, exhibiting the classic characteristics of worm-like micelles. Extrapolating the shear plateau to zero shear rate revealed a zero-shear viscosity of 34,000 mPa·s, corresponding to a pH of 5.70.

[0028] The pH of the N,N-dimethyloctadecylamine / n-hexanoic acid system was regulated using 2 mol / L HCl and 0.5 mol / L NaOH. When the pH was 6.24, the solution viscosity was 1 mPa·S; when the pH was 2.67, the solution viscosity was 13 mPa·S. The results are as follows: Figure 1 shown.

[0029] Example 2 A method for preparing pH-responsive worm-like micelles comprises the following steps: Take 2.89g of N,N - Dihydroxyethyl octadecyl tertiary amine and 1.14 g of salicylic acid were added to 196 g of distilled water, the water bath temperature was maintained at 90 ° C, and the mixture was stirred at 1200 rpm for 12 h to obtain N,N - The dihydroxyethyl octadecyl tertiary amine / salicylic acid system is a pH-responsive worm-like micelle; wherein the N,N-dihydroxyethyl octadecyl tertiary amine / salicylic acid system behaves as a clear and transparent high-viscosity viscoelastic fluid.

[0030] Rheological testing of the N,N-dihydroxyethyloctadecylamine / salicylic acid system at 25°C revealed steady-state rheological behavior, demonstrating a Newtonian fluid at low shear rates and a shear-thinning fluid at high shear rates, exhibiting the classic characteristics of worm-like micelles. Extrapolating the shear plateau to zero shear rate revealed a zero-shear viscosity of 24,000 mPa·s, corresponding to a pH of 3.88.

[0031] 0.5 mol / L NaOH was used to analyze N, N - The pH of the dihydroxyethyl octadecyl tertiary amine / salicylic acid system was regulated. When the pH was 7.30, the solution viscosity was 15 mPa·S. The results were as follows: Figure 2 shown.

[0032] Example 3 A method for preparing pH-responsive worm-like micelles comprises the following steps: 3.92 g of oleylamine and 1.08 g of propionic acid were added to 95 g of distilled water. The water bath temperature was maintained at 25°C and stirred at 1200 rpm for 2 h to obtain an oleylamine / propionic acid system, i.e., pH-responsive worm-like micelles. The oleylamine / propionic acid system behaved as a clear, transparent, high-viscosity viscoelastic fluid.

[0033] Rheological testing of the oleylamine / propionic acid system at 25°C revealed steady-state rheological results demonstrating a Newtonian fluid at low shear rates and a shear-thinning fluid at high shear rates, exhibiting the classic characteristics of worm-like micelles. Extrapolating the shear plateau to zero shear rate revealed a zero-shear viscosity of 200,000 mPa·s, corresponding to a pH of 5.24.

[0034] The pH of the oleylamine / propionic acid system was regulated using a 0.5 mol / L dilute solution of NaOH. When the pH was 6.74, the solution viscosity was 4 mPa·s. The results were as follows: Figure 3 shown.

[0035] Example 4 A method for preparing pH-responsive worm-like micelles comprises the following steps: 1.71 g of octadecylamine and 0.29 g of formic acid were added to 98 g of distilled water. The water bath temperature was maintained at 25°C and stirred at 1200 rpm for 2 hours to obtain an octadecylamine / formic acid system, i.e., pH-responsive worm-like micelles. The octadecylamine / formic acid system behaved as a clear, transparent, high-viscosity viscoelastic fluid.

[0036] Rheological testing of the octadecylamine / formic acid system at 25°C revealed steady-state rheological results demonstrating a Newtonian fluid at low shear rates and a shear-thinning fluid at high shear rates, exhibiting the classic characteristics of worm-like micelles. Extrapolating the shear plateau to zero shear rate revealed a zero-shear viscosity of 33,000 mPa·s, corresponding to a pH of 4.70.

[0037] The pH of the octadecylamine / formic acid system was regulated by 0.5 mol / L NaOH. When the pH was 7.15, the solution viscosity was 10 mPa·S. Figure 4 shown.

[0038] Example 5 A method for preparing pH-responsive worm-like micelles comprises the following steps: 1.64 g of octadecylamine and 0.36 g of acetic acid were added to 98 g of distilled water. The water bath temperature was maintained at 25°C and stirred at 1200 rpm for 2 h to obtain an octadecylamine / acetic acid system, i.e., pH-responsive worm-like micelles. The octadecylamine / acetic acid system behaved as a clear, transparent, high-viscosity viscoelastic fluid.

[0039] Rheological testing of the octadecylamine / acetic acid system at 25°C revealed steady-state rheological results demonstrating a Newtonian fluid at low shear rates and a shear-thinning fluid at high shear rates, exhibiting the classic characteristics of worm-like micelles. Extrapolating the shear plateau to zero shear rate revealed a zero-shear viscosity of 22,000 mPa·s, corresponding to a pH of 5.40.

[0040] The pH of the octadecylamine / acetic acid system was regulated by a 0.5 mol / L NaOH dilute solution. When the pH was 7.28, the solution viscosity was 3 mPa·s. Figure 5 shown.

[0041] Example 6 A method for preparing pH-responsive worm-like micelles comprises the following steps: 1.57 g of octadecylamine and 0.43 g of propionic acid were added to 98 g of distilled water. The water bath temperature was maintained at 25°C and stirred at 1200 rpm for 2 hours to obtain a 2% octadecylamine / propionic acid system, namely, pH-responsive worm-like micelles. The octadecylamine / propionic acid system behaved as a clear, transparent, high-viscosity viscoelastic fluid.

[0042] Rheological testing of the octadecylamine / propionic acid system at 25°C revealed steady-state rheological results demonstrating a Newtonian fluid at low shear rates and a shear-thinning fluid at high shear rates, exhibiting the classic characteristics of worm-like micelles. Extrapolating the shear plateau to zero shear rate revealed a zero-shear viscosity of 32,000 mPa·s, corresponding to a pH of 5.75.

[0043] The pH of the octadecylamine / propionic acid system was regulated using a dilute solution of 2 mol / L HCl and 0.5 mol / L NaOH. When the pH was 7.32, the solution viscosity was 7 mPa·S. Figure 6 shown.

[0044] Example 7 A method for preparing pH-responsive worm-like micelles comprises the following steps: Take 1.40g of N,N - Dimethylhexadecyl tertiary amine and 0.60 g of hexanoic acid were added to 98 g of distilled water, the water bath temperature was maintained at 25°C, and stirring was carried out at 1200 rpm for 2 hours to obtain an N,N-dimethylhexadecyl tertiary amine / hexanoic acid system, i.e., pH-responsive worm-like micelles. The N,N-dimethylhexadecyl tertiary amine / hexanoic acid system behaved as a clear, transparent, high-viscosity viscoelastic fluid.

[0045] Rheological testing of the N,N-dimethylhexadecylamine / hexanoic acid system at 25°C revealed steady-state rheological behavior, demonstrating a Newtonian fluid at low shear rates and a shear-thinning fluid at high shear rates, exhibiting the classic characteristics of worm-like micelles. Extrapolating the shear plateau to zero shear rate revealed a zero-shear viscosity of 700 mPa·s, corresponding to a pH of 5.77.

[0046] The pH of the N,N-dimethylhexadecylamine / hexanoic acid system was regulated using a dilute solution of 2 mol / L HCl and 0.5 mol / L NaOH. When the pH was 6.39, the solution viscosity was 2 mPa·s. The results are as follows: Figure 7 shown.

[0047] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit the scope of protection of the invention. Obviously, the embodiments described are only some embodiments of the present invention, rather than all embodiments. Based on these embodiments, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention. Although the present invention has been described in detail with reference to the above embodiments, ordinary technicians in this field can still combine, add, delete or make other adjustments to the features in the various embodiments of the present invention according to the circumstances without conflict, without making creative work, so as to obtain different other technical solutions that do not deviate from the concept of the present invention in essence, and these technical solutions also fall within the scope of protection of the present invention.

Claims

1. A method for preparing pH-responsive worm-like micelles, It is characterized in that The following steps are involved: At 25° C. to 90° C., raw material A and acid are added to water in a mass ratio of 1.4 to 3.92:0.29 to 1.14 to obtain pH-responsive worm-like micelles; The mass ratio of the sum of the raw material A and the acid to water is 2-5:95-196; The raw material A is hexadecylamine, octadecylamine, N,N -Dimethylhexadecyl tertiary amine, N,N -Dimethyloctadecyl tertiary amine, N, N- Any one of dihydroxyethyl octadecyl tertiary amine and oleylamine; The acid is any one of formic acid, acetic acid, propionic acid, caproic acid and salicylic acid.

2. The method for preparing pH-responsive worm-like micelles according to claim 1, It is characterized in that When raw material A is hexadecylamine, the corresponding acid is butyric acid; When raw material A is octadecylamine, the corresponding acid is any one of formic acid, acetic acid, propionic acid, and butyric acid; When raw material A is N,N - In the case of dimethyl hexadecyl tertiary amine, the corresponding acid is hexanoic acid; When raw material A is N,N - Dihydroxyethyl octadecyl tertiary amine, the corresponding acid is salicylic acid; When the raw material A is oleylamine, the corresponding acid is any one of formic acid, propionic acid and butyric acid.

3. The method for preparing pH-responsive worm-like micelles according to claim 1, It is characterized in that The mixing is carried out by stirring.

4. The method for preparing pH-responsive worm-like micelles according to claim 3, It is characterized in that The stirring time is 2 hours to 12 hours, and the stirring speed is 1000 rpm to 1200 rpm.

5. A pH-responsive worm-like micelle prepared by the method for preparing pH-responsive worm-like micelles according to any one of claims 1 to 4.

6. The pH-responsive worm-like micelle according to claim 5, It is characterized in that The zero shear viscosity of the pH-responsive worm-like micelle is between 500 mPa·S and 200000 mPa·S.

7. The pH-responsive worm-like micelle according to claim 5, It is characterized in that The pH response means that when the pH value of the worm-like micelles is changed to less than 3 or greater than 6, the viscosity value thereof decreases to less than 20 mPa·S.

Citation Information

Patent Citations

  • Cationic gemini surfactant with analogue cloud temperature phenomenon, and construction method thereof

    CN105435707A

  • Cationic viscoelastic surfactant, and construction method thereof

    CN106732166A

  • Dimeric surfactant worm-like micelle system with pH response

    CN108837772A

  • Temperature regulation type temporary plugging agent as well as preparation method and application thereof