Efficient titanizing device and using method thereof

Through the rotating device and electromagnetic induction heating device, the liquid magnesium is uniformly coated in the argon environment, which solves the problems of uneven coating and oxidation of the inner wall of the reactor, and achieves efficient titanium permeability, prevents the iron value of the sponge titanium product from exceeding the standard, and improves production Efficiency and product quality.

CN118996324APending Publication Date: 2024-11-22LUOYANG SUNRUI WANJI TITANIUM CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411131975.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-19
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In the prior art, the titanium coating on the inner wall of the reactor is uneven and easy to oxidize, resulting in poor titanium permeability effect and causing the problem of excessive iron value of sponge titanium products.

Method used

Using a rotating device and an electromagnetic induction heating device, the liquid magnesium is driven to uniformly coat the inner wall of the reactor through an argon environment, and the temperature is controlled to avoid titanium oxidation and achieve uniform generation of titanium ferroalloy.

Benefits of technology

It improves the titanium seepage effect, prevents the iron value of sponge titanium products from exceeding the standard, significantly shortens the titanium seepage cycle, and improves production efficiency and product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118996324A_ABST
    Figure CN118996324A_ABST
Patent Text Reader

Abstract

The invention provides an efficient titanizing device and a using method thereof.The efficient titanizing device is used for assisting a reactor in titanizing, and a heating device is arranged on a base and used for heating the reactor; the rotating device is arranged on the upper surface of the base, penetrates through the heating device, is connected with the reactor and is used for rotating the reactor; the inflating pipe, the evacuating pipe and the pressure measuring pipe are arranged on a large cover of the reactor and are used for controlling the gas pressure in the reactor; the charging pipe is arranged on a large cover of the reactor and is used for charging the reactor; by arranging the rotating device, the reactor can rotate, liquid magnesium liquid in the reactor is driven to flow in the reactor, the magnesium liquid is uniformly smeared on the inner wall of the reactor, the reaction contact area of the liquid magnesium and titanium tetrachloride is enlarged, and the inner wall of the reactor is uniformly covered with generated titanium; the non-uniform phenomenon caused by manual titanium powder smearing is avoided, the titanizing effect is effectively improved, and the iron value of a sponge titanium product is prevented from exceeding the standard.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of magnesium thermal method titanium sponge production, and in particular to a high-efficiency titanium infiltration device and a use method thereof. Background Art

[0002] At present, the main method for producing sponge titanium is the Kroll process, which is a vacuum distillation method of reducing titanium tetrachloride with magnesium. A steel reactor is used. In order to avoid the introduction of impurity elements such as Cr and Ni into the sponge titanium, the reactor is generally made of carbon steel. During the production of sponge titanium, the temperature inside the reactor is as high as 1000°C. The iron in carbon steel can be easily introduced into the sponge titanium. Therefore, the inner wall of the new reactor needs to be titaniumized to reduce the introduction of iron. The conventional titaniumization method is to first apply a layer of titanium powder on the inner wall of the reactor, and then heat the reactor to form a layer of titanium-iron alloy on the inner wall of the reactor, thereby avoiding the introduction of iron on the reactor wall during the production process.

[0003] The biggest problem with this method at present is that the titanium powder is not evenly applied and is easily oxidized. The oxidized titanium powder during the titanium infiltration process is difficult to generate titanium-iron alloy on the reactor wall, making it difficult to achieve an effective titanium infiltration effect. During use, it is easy to cause the iron value of the sponge titanium product to exceed the standard.

[0004] Patent No.: CN104004987B discloses a titanium diffusion method for a reactor for sponge titanium production, wherein the magnesium used can be liquid magnesium, and the amount of liquid magnesium and titanium tetrachloride added is such that the generated titanium forms a titanium diffusion layer with the new reactor wall. However, in this method, the magnesium liquid is at the bottom of the reactor, and only the surface layer of the magnesium liquid reacts with the gaseous titanium tetrachloride, resulting in low reduction reaction efficiency and uneven titanium adhesion to the reactor wall.

[0005] Therefore, the existing technology cannot solve the problem of uneven titanium coating on the inner wall of the reactor, easy oxidation of titanium, resulting in poor titanium infiltration effect and excessive iron value of sponge titanium products. Summary of the invention

[0006] In view of this, the present invention aims to propose an efficient titanium diffusion device and its use method to solve the problem in the prior art that the titanium coating on the inner wall of the reactor is uneven and easily oxidized, resulting in poor titanium diffusion effect and excessive iron value of the sponge titanium product.

[0007] In order to improve the uniformity of titanium coating on the inner wall of the reactor and avoid titanium oxidation, the present invention utilizes magnesium and titanium tetrachloride to undergo a reduction reaction to generate titanium. An argon environment is created through the titanium infiltration device of the present invention, and the reactor is driven to rotate, so that liquid magnesium can be evenly coated on the inner wall of the reactor, thereby avoiding the situation where titanium cannot evenly cover the inner wall of the reactor during artificial coating or direct reduction reaction, reducing titanium oxidation, achieving a better titanium infiltration effect, and improving the quality of sponge titanium products.

[0008] At the same time, the present invention adopts induction coil heating, which can better control the temperature, ensure the stable progress of the reduction reaction and the titanium diffusion process, and significantly improve the production efficiency of the titanium diffusion reaction.

[0009] The technical solution of the present invention is achieved as follows: a high-efficiency titanium infiltration device is used to assist a reactor in titanium infiltration operations, comprising an air filling tube, an evacuation tube, a feeding tube, a pressure measuring tube, a rotating device, a heating device and a base; the heating device is arranged on the base, and is used to heat the reactor; the rotating device is arranged on the base, and the rotating device is connected to the reactor through the heating device, and is used to rotate the reactor; the air filling tube, the evacuation tube and the pressure measuring tube are arranged on the large cover of the reactor, and are used to control the gas pressure in the reactor; the feeding tube is arranged on the large cover of the reactor, and is used to add materials to the reactor.

[0010] Furthermore, the rotating device includes a motor, a transmission device, a roller bracket, a driving wheel and a driven wheel, the driving wheel and the driven wheel are arranged in sequence along the axis direction of the reactor, the driving wheel and the driven wheel are respectively connected to the roller bracket, and the driving wheel is connected to the motor via the transmission device.

[0011] Furthermore, the roller bracket includes a fixing portion and two connecting portions, the two connecting portions are fixedly connected to the fixing portion at an angle, and are used to connect the driving wheel or the driven wheel; the fixing portion is provided with a connecting hole, and is used to connect to the base.

[0012] Furthermore, the rotating device includes two groups of driving wheels and two groups of driven wheels, and the driving wheels and the driven wheels are respectively arranged symmetrically with the axis of the reactor as an axis.

[0013] Furthermore, the driving wheel includes two first rollers for driving the reactor to rotate.

[0014] Furthermore, the heating device is a bow-shaped electromagnetic induction heating coil.

[0015] A method for using a high-efficiency titanium infiltration device, based on any of the above-mentioned high-efficiency titanium infiltration devices, comprises the following specific steps:

[0016] S1: Preparation before production; firstly, a preset amount of solid magnesium is placed in the reactor, and after the reactor is assembled, pressure testing is performed to detect leaks. After the pressure testing is completed, the reactor is evacuated and then filled with argon gas;

[0017] S2: Installing the reactor: placing the assembled reactor to be titaniumized flat on the rotating device;

[0018] S3: melting solid magnesium; starting the heating device to heat the reactor until all the solid magnesium is melted into a liquid state, starting the rotating device to drive the reactor to rotate, and ensuring that the liquid magnesium in the reactor is evenly coated on the inner wall of the reactor;

[0019] S4: Open the feeding pipe valve and add titanium tetrachloride at a rate of 450-550 kg / h for 1-2 hours;

[0020] S5: After the addition is completed, the reactor is further heated to 900° C. to 1100° C. by the heating device and kept warm for 1 to 3 hours, so that the titanium on the inner wall of the reactor reacts with the inner wall of the reactor to form a titanium-iron alloy;

[0021] S6: After the titanium infiltration is completed, the heating device and the rotating device are turned off in turn, and the titanium infiltration reactor is cooled by air cooling;

[0022] S7: depressurizing the reactor after titanium infiltration, cleaning the low-cost materials in the reactor after opening the lid and checking the titanium infiltration effect;

[0023] S8: Reactors that pass the titanium infiltration test can be used as cold ends.

[0024] Furthermore, in step S3, the solid magnesium heating temperature ranges from 640°C to 770°C.

[0025] Furthermore, in step S4, the excess magnesium on the inner wall of the reactor reacts with titanium tetrachloride to generate titanium.

[0026] Furthermore, it also includes a control system, which includes an explosion-proof control box, a frequency converter and a remote controller for one-button start, stop, frequency increase and frequency decrease operations.

[0027] Furthermore, in step S6, argon is used to maintain a positive pressure in the reactor during the cooling process, and the pressure is controlled at 0.01-0.05 MPa.

[0028] Compared with the prior art, the high-efficiency titanium infiltration device and the use method thereof of the present invention have the following advantages:

[0029] 1. The present invention can make the reactor rotate by arranging a rotating device, so as to drive the liquid magnesium in the reactor to flow inside the reactor, and the magnesium liquid is evenly applied to the inner wall of the reactor, thereby expanding the reaction contact area between the liquid magnesium and titanium tetrachloride, so that the generated titanium evenly covers the inner wall of the reactor, thereby improving the reaction efficiency and speed, avoiding the uneven phenomenon caused by artificial application of titanium powder, reducing the oxidation of titanium powder, effectively improving the titanium infiltration effect, and preventing the iron value of the sponge titanium product from exceeding the standard.

[0030] 2. The present invention combines electromagnetic induction heating and a roller frame by providing a high-efficiency titanium diffusion device, and uses the roller frame to rotate the reactor to ensure that the liquid magnesium on the inner wall of the reactor is evenly coated, and then titanium tetrachloride is added through the feeding system to achieve the formation of a titanium layer on the inner wall of the reactor, and the temperature is further adjusted to ensure the formation of a titanium diffusion layer on the reactor wall, thereby improving the titanium diffusion efficiency and effect.

[0031] 3. The present invention utilizes an electromagnetic induction heating coil to heat the reactor, and quickly adjusts the temperature through an induction heating device, so that the pure titanium layer can be combined with the inner wall of the reactor to produce a titanium-iron alloy, completing the titanium infiltration process, greatly improving the titanium infiltration efficiency and effect, and significantly shortening the titanium infiltration cycle. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] The accompanying drawings constituting a part of the present invention are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the accompanying drawings:

[0033] Figure 1 A schematic diagram of the structure of the device in the present invention;

[0034] Figure 2 A front view of the device of the present invention;

[0035] Figure 3 A right side view of the device of the present invention;

[0036] Description of reference numerals:

[0037] 1. Reactor; 2. Inflation tube; 3. Evacuation tube; 4. Feeding tube; 5. Pressure measuring tube; 6. Rotating device; 601. Motor; 602. Transmission device; 603. Roller bracket; 6031. Fixing part; 60311. Connecting hole; 6032. Connecting part; 604. Driving wheel; 6041. First roller; 605. Driven wheel; 6051. Second roller; 8. Heating device; 9. Temperature sensor; 10. Base. DETAILED DESCRIPTION

[0038] In order to make the technical means, objectives and effects of the present invention easy to understand, the embodiments of the present invention are described in detail below with reference to specific drawings.

[0039] It should be noted that all the terms used in the present invention to indicate directionality and position, such as "upper", "lower", "left", "right", "front", "back", "vertical", "horizontal", "inside", "outside", "top", "lower", "lateral", "longitudinal", "center", etc., are only used to explain the relative positional relationship and connection status between the components in a certain state, and are only for the convenience of describing the present invention, rather than requiring the present invention to be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the descriptions of "first", "second", etc. in the present invention are only used for descriptive purposes, and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features.

[0040] In the description of the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0041] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "illustrative embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner.

[0042] The present invention discloses a high-efficiency titanium infiltration device, which is used to assist a reactor 1 in titanium infiltration operation, and comprises an air filling pipe 2, an evacuation pipe 3, a feeding pipe 4, a pressure measuring pipe 5, a rotating device 6, a heating device 8 and a base 10; the heating device 8 is arranged on the base 10, and is used to heat the reactor 1; the rotating device 6 is arranged on the base 10, and the rotating device 6 passes through the heating device 8 and is connected to the reactor 1, and is used to rotate the reactor 1; the air filling pipe 2, the evacuation pipe 3 and the pressure measuring pipe 5 are arranged on the large cover of the reactor 1, and are used to control the gas pressure in the reactor 1; the feeding pipe 4 is arranged on the large cover of the reactor 1, and is used to feed the reactor 1.

[0043] The rotating device 6 can make the reactor 1 rotate, driving the liquid magnesium in the reactor 1 to flow inside the reactor 1, and the magnesium liquid is evenly applied to the inner wall of the reactor 1, and then the liquid magnesium on the inner wall of the reactor 1 reacts with the gaseous titanium tetrachloride injected after heating, so that the generated titanium evenly covers the inner wall of the reactor 1, thereby expanding the reaction contact area between the liquid magnesium and the titanium tetrachloride, improving the reaction efficiency and speed, avoiding the uneven phenomenon caused by artificial application of titanium powder, reducing the oxidation of titanium powder, effectively improving the titanium infiltration effect, and preventing the iron value of the sponge titanium product from exceeding the standard.

[0044] Specifically, the rotating device 6 includes a motor 601, a transmission device 602, a roller bracket 603, a driving wheel 604 and a driven wheel 605, the driving wheel 604 and the driven wheel 605 are sequentially arranged along the axis direction of the reactor 1, the driving wheel 604 and the driven wheel 605 are respectively connected to the roller bracket 603, and the driving wheel 604 is connected to the motor 601 through the transmission device 602. The rotating device 6 is provided with power by the motor 601, which is transmitted to the driving wheel 604 through the transmission device 602, thereby driving the driven wheel 605 and the reactor 1 connected thereto to rotate. It is helpful for the liquid magnesium in the reactor to evenly cover the inner wall of the reactor 1 at high temperature, avoid the existence of uncovered areas, and improve the titanium infiltration effect.

[0045] Specifically, the roller bracket 603 includes a fixing portion 6031 and two connecting portions 6032. The two connecting portions 6032 are fixedly connected to the fixing portion 6031 at an angle, and are used to connect the driving wheel 604 or the driven wheel 605. The fixing portion 6031 is provided with a connecting hole 60311, and is used to connect the base 10. This arrangement enables the roller bracket 603 to be connected to multiple driving wheels 604 or driven wheels 605 at the same time, further improving the structural stability and reliability of the rotating device 6.

[0046] Preferably, the angle between the two connecting parts 6032 is in the range of 100°-170°. Within this angle range, the connecting parts 6032 of the same length are lower in height, which can reduce the overall size of the roller bracket 603, expand the contact range between the two fixing parts 6031 and the reactor 1, help reduce the installation height of the reactor 1, and improve the overall structural stability of the device.

[0047] Specifically, the rotating device 6 includes two sets of driving wheels 604 and two sets of driven wheels 605, and the driving wheels 604 and the driven wheels 605 are respectively arranged symmetrically with the axis of the reactor 1 as the axis. The two sets of driving wheels 604 and the two sets of driven wheels 605 are arranged to facilitate the installation of the reactor 1, and the symmetrical arrangement can effectively support the reactor 1, so that the rotation of the reactor 1 is more stable, the force on a single support point is greatly reduced, the deformation caused by uneven force is reduced, and the vibration generated by the reactor 1 during the rolling process is reduced, which helps to improve the overall stability and reliability of the device.

[0048] Specifically, the driving wheel 604 includes two first rollers 6041, which are used to drive the reactor 1 to rotate. This arrangement can better support the reactor 1 and improve the stability of the rotation of the reactor 1.

[0049] Specifically, the driven wheel 605 includes two temperature sensors 9 for supporting the reactor 1. This arrangement can better support the reactor 1 and improve the stability of the rotation of the reactor 1.

[0050] Specifically, the heating device 8 is an electromagnetic induction heating coil. This device changes the existing heating method of the pit-type resistance furnace and uses electromagnetic induction heating. The device is easy to install, has high control accuracy, does not require pre-furnace preparation, has fast heating speed and high efficiency, and helps to shorten the titanium infiltration cycle and improve production efficiency.

[0051] Specifically, the heating device 8 is in an arc shape. This arrangement enables the heating coil to cover the surface of the reactor 1 more evenly, ensuring that each part of the reactor 1 is heated evenly, helping to avoid deformation or quality problems of the reactor 1 caused by uneven heating; shortening the heating time, reducing energy loss, and improving energy efficiency.

[0052] Specifically, the motor 601 and the heating device 8 are connected to the control center to adjust the speed and direction of the reactor 1. This setting can adjust the speed and direction of the reactor 1 according to actual processing needs, adjust the internal heating temperature and heating speed of the reactor 1, help improve the reaction efficiency and titanium production cycle, improve the automated processing capability, and improve production efficiency.

[0053] Specifically, a temperature sensor 9 is also included to detect the temperature of the outer wall of the reactor 1. This arrangement helps to facilitate the control of the heating temperature, improve the control accuracy of the titanium infiltration process, and further improve the titanium infiltration effect.

[0054] Preferably, the temperature sensor 9 is a temperature measuring thermocouple.

[0055] Specifically, the gas filling tube 2 is connected to the gas source and is used to fill argon gas into the reactor 1 and perform pressure leak detection. This arrangement facilitates filling air into the reactor 1 during pressure leak detection, and after the leak detection is completed, the argon gas source is switched to fill argon gas into the reactor 1, which reduces the number of gas pipes, facilitates installation, and reduces the risk of gas leakage.

[0056] Specifically, the evacuation pipe 3 is connected to the vacuum machine and is used to evacuate the reactor 1. The evacuation pipe 3 is provided to facilitate the vacuum machine to evacuate the gas inside the reactor 1, thereby preventing impurity gas from being retained inside the reactor 1 and affecting the solid magnesium heating effect.

[0057] Specifically, the feed pipe 4 is connected to the titanium tetrachloride material. This arrangement facilitates the opening of the large cover of the reactor 1 during the titanium infiltration process, reduces the infiltration of external air, and affects the titanium reaction effect and the titanium infiltration quality.

[0058] A method for using a high-efficiency titanium-infiltrating device comprises the following specific steps:

[0059] S1: Preparation before production; first, a preset amount of solid magnesium is placed in the reactor 1, and after the reactor 1 is assembled, pressure testing is performed to detect leaks. After the pressure testing is completed, the reactor 1 is evacuated and then filled with argon gas;

[0060] S2: Installing the reactor 1: placing the assembled reactor 1 to be titaniumized flat on the rotating device 6;

[0061] S3: melting of solid magnesium; starting the heating device 8 to heat the reactor 1 until the solid magnesium is completely melted into a liquid state, starting the rotating device 6 to drive the reactor 1 to rotate, ensuring that the liquid magnesium in the reactor is evenly applied to the inner wall of the reactor 1;

[0062] S4: Open the valve of the feeding pipe 4 and add titanium tetrachloride at a rate of 450-550 kg / h for 1-2 hours;

[0063] S5: After the addition is completed, the reactor 1 is further heated to 900° C. to 1100° C. by the heating device 8 and kept warm for 1 to 3 hours, and the titanium on the inner wall of the reactor 1 reacts with the inner wall of the reactor 1 to form a titanium-iron alloy;

[0064] S6: After the titanium infiltration is completed, the heating device 8 and the rotating device 6 are turned off successively, and the titanium infiltration reactor 1 is cooled by air cooling;

[0065] S7: Depressurize the reactor 1 after titanium infiltration, clean the low-priced materials in the reactor 1 after opening the cover, and check the titanium infiltration effect;

[0066] S8: Reactors that pass the titanium infiltration test can be used as cold ends.

[0067] This arrangement utilizes a titanium diffusion device to enable the magnesium liquid to be more evenly coated on the inner wall of the reactor 1, thereby expanding the contact area between the magnesium liquid and the gaseous titanium tetrachloride, helping to increase the reaction rate of magnesium and the gaseous titanium tetrachloride, and avoiding the magnesium liquid from completely covering the inner wall of the reactor 1, thereby achieving a more efficient and rapid titanium diffusion process, and shortening the titanium diffusion time to less than half of the conventional titanium diffusion time, thereby greatly improving production efficiency and reducing the production cost of sponge titanium.

[0068] Specifically, the preset amount of solid magnesium is greater than the amount of magnesium required for the reduction reaction.

[0069] Preferably, in step S1, 200 kg of solid magnesium is added to a 10-ton reactor. This setting ensures that there is sufficient magnesium in the reactor 1, so that the magnesium can completely cover the inner wall of the reactor 1, and avoids insufficient magnesium liquid causing incomplete magnesium coverage of the inner wall of the reactor 1, which affects the subsequent reduction reaction and the titanium infiltration effect.

[0070] Specifically, in step S3, the solid magnesium heating temperature ranges from 640° C. to 770° C. This set temperature range can maintain the stability and uniformity of the magnesium liquid, facilitate the rotation of the magnesium liquid in the reactor 1 and the subsequent reaction to ensure smooth production, shorten the production cycle, and improve production efficiency.

[0071] Preferably, the heating temperature ranges from 690°C to 720°C.

[0072] Specifically, in step S4, it is ensured that the excess magnesium on the inner wall of the reactor 1 reacts with titanium tetrachloride to generate titanium. The setting of the excess magnesium can improve the efficiency and completeness of the reduction reaction, ensure that the titanium tetrachloride is fully reduced to titanium, help ensure the normal progress of the reduction reaction inside the reactor 1, and ensure the generation of titanium.

[0073] Preferably, in step S4, the valve of the feeding pipe 4 is opened, and titanium tetrachloride is added at a rate of 500 kg / h for 1.5 hours.

[0074] Preferably, in step S5, after the feeding is completed, the reactor 1 is further heated to 980°C to 1050°C by the heating device 8 and kept warm for 2 hours, and the titanium on the inner wall of the reactor 1 reacts with the inner wall of the reactor 1 to form titanium-iron alloy.

[0075] Specifically, in step S6, argon is used to maintain a positive pressure in the reactor 1 during the cooling process, and the pressure is controlled at 0.01-0.05MPa. This setting uses argon to effectively isolate oxygen in the air, prevent titanium and titanium alloys from being oxidized by contact with oxygen during the cooling process, and help maintain the quality and purity of the product after titanium infiltration; using air cooling to cool down can maintain a certain temperature gradient, avoid excessive thermal stress caused by rapid cooling, and use the positive pressure of argon to help control the temperature distribution inside the reactor 1, ensuring that the cooling process is uniform and controllable.

[0076] Preferably, the pressure is controlled at 0.01-0.025 MPa.

[0077] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A highly efficient titaniumizing device, used to assist a reactor (1) in titaniumizing operation, characterized in that: The reactor (1) comprises an air filling pipe (2), an evacuation pipe (3), a feeding pipe (4), a pressure measuring pipe (5), a rotating device (6), a heating device (8) and a base (10); the heating device (8) is arranged on the base (10) and is used to heat the reactor (1); the rotating device (6) is arranged on the base (10), and the rotating device (6) passes through the heating device (8) and is connected to the reactor (1) and is used to rotate the reactor (1); the air filling pipe (2), the evacuation pipe (3) and the pressure measuring pipe (5) are arranged on the large cover of the reactor (1) and are used to control the gas pressure in the reactor (1); the feeding pipe (4) is arranged on the large cover of the reactor (1) and is used to feed materials into the reactor (1).

2. The high-efficiency titaniumizing device according to claim 1, characterized in that: The rotating device (6) comprises a motor (601), a transmission device (602), a roller bracket (603), a driving wheel (604) and a driven wheel (605), wherein the driving wheel (604) and the driven wheel (605) are arranged in sequence along the axis direction of the reactor (1), the driving wheel (604) and the driven wheel (605) are respectively connected to the roller bracket (603), and the driving wheel (604) is connected to the motor (601) via the transmission device (602).

3. The high-efficiency titaniumizing device according to claim 2, characterized in that: The roller bracket (603) comprises a fixing portion (6031) and two connecting portions (6032), wherein the two connecting portions (6032) are fixedly connected to the fixing portion (6031) at an angle and are used to connect the driving wheel (604) or the driven wheel (605); the fixing portion (6031) is provided with a connecting hole (60311) for connecting to the base (10).

4. The high-efficiency titanium-diffusion device according to claim 2, characterized in that: The rotating device (6) comprises two sets of driving wheels (604) and two sets of driven wheels (605), and the driving wheels (604) and the driven wheels (605) are respectively arranged symmetrically with the axis of the reactor (1) as the axis.

5. The high-efficiency titanium-infiltrating device according to claim 2, characterized in that: The driving wheel (604) comprises two first rollers (6041) for driving the reactor (1) to rotate.

6. The high-efficiency titaniumizing device according to claim 1, characterized in that: The heating device (8) is a bow-shaped electromagnetic induction heating coil.

7. A method for using a high-efficiency titanium-infiltrating device, characterized in that: The high-efficiency titanium-infiltrating device according to any one of claims 1 to 6 comprises the following specific steps: S1: Preparation before production; first, a preset amount of solid magnesium is placed in the reactor (1), and after the reactor (1) is assembled, pressure testing is performed to detect leaks. After the pressure testing is completed, the reactor (1) is evacuated and then filled with argon gas; S2: installing the reactor (1): placing the assembled reactor (1) to be titaniumized flat on the rotating device (6); S3: solid magnesium melting; The heating device (8) is started to heat the reactor (1) until the solid magnesium is completely melted into a liquid state, and the rotating device (6) is started to drive the reactor (1) to rotate, so as to ensure that the liquid magnesium in the reactor is evenly coated on the inner wall of the reactor (1); S4: Open the valve of the feeding pipe (4) and add titanium tetrachloride at a rate of 450-550 kg / h for 1-2 hours; S5: After the addition is completed, the reactor (1) is further heated to 900° C. to 1100° C. by the heating device (8) and kept at this temperature for 1 to 3 hours, so that the titanium on the inner wall of the reactor (1) reacts with the inner wall of the reactor (1) to form a titanium-iron alloy; S6: After the titanium infiltration is completed, the heating device (8) and the rotating device (6) are turned off in sequence, and the titanium infiltration reactor (1) is cooled by air cooling; S7: depressurizing the reactor (1) after titanium infiltration is completed, cleaning the low-cost materials in the reactor (1) after opening the cover, and checking the titanium infiltration effect; S8: Reactors that pass the titanium infiltration test can be used as cold ends.

8. The high-efficiency titaniumizing device according to claim 7, characterized in that: In step S3, the solid magnesium heating temperature ranges from 640°C to 770°C.

9. The high-efficiency titaniumizing device according to claim 7, characterized in that: In step S4, the excess magnesium on the inner wall of the reactor (1) reacts with titanium tetrachloride to generate titanium.

10. The high-efficiency titaniumizing device according to claim 7, characterized in that: In step S6, during the cooling process, argon is used to maintain a positive pressure in the reactor (1), and the pressure is controlled at 0.01-0.05 MPa.