Oil and gas well crack leaking stoppage method
By employing a step-by-step construction and high-temperature hydrolysis method, and utilizing a combination of polyacrylamide water-absorbing resin and sodium hydroxide solution, the problem of crack sealing in old shale gas wells has been solved, achieving a highly efficient and controllable plugging effect, which is suitable for casing cementing operations.
Patent Information
- Application Number
- CN202410995870.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-24
- Publication Date
- 2024-11-22
AI Technical Summary
Existing technologies are insufficient to effectively seal multiple fractures in old shale gas wells after initial fracturing. Traditional plugging materials are ineffective in environments lacking drilling fluid and have limited expansion ratios, making it difficult to meet the plugging requirements of casing cementing.
The method of step-by-step construction is adopted. First, a plugging fluid containing polyacrylamide water-absorbing resin is pumped to initially seal the leak. Then, a sodium hydroxide solution is pumped to hydrolyze it into polyacrylic acid water-absorbing resin, forming a sealing layer with a high expansion ratio. The expansion reaction is controlled by utilizing the high temperature environment of the formation to enhance the sealing effect.
It achieves reliable plugging in a drilling fluid-free environment, significantly improves the expansion ratio, and significantly improves the sealing effect of fractures, ensuring the safety and success rate of cementing operations.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of oil and gas wells, and in particular to a method for plugging cracks in oil and gas wells. Background Art
[0002] Shale gas reservoirs have the characteristics of low porosity, low permeability, and no natural production capacity. Its efficient development requires the use of large-scale hydraulic fracturing to form artificial fractures to provide seepage channels for production, but there are problems such as rapid production decline and short stable production period after the initial transformation. It is necessary to run a small casing into the original wellbore, cement the small casing, and then perform repeated fracturing to increase the production capacity of shale gas wells again.
[0003] The technology of cementing old shale gas wells by inserting small casing is called casing-in-casing technology. Since there are original cracks from the initial fracturing in old shale gas wells, the original cracks need to be sealed before the casing-in-casing cementing operation to prevent cement slurry from leaking into the cracks during the cementing process, affecting cementing safety. The original cracks formed by the initial fracturing are numerous, deep, and have low pressure inside the cracks, making the plugging operation difficult. It is difficult to form a tight plugging layer in the cracks using traditional bridging plugging materials, and the plugging effect is difficult to meet the requirements.
[0004] Regarding the method of plugging cracks, CN 108048055 A discloses a novel delayed expansion plugging agent and its preparation method, which is prepared by the reaction of the following raw materials, and the raw material ratio is calculated by the following weight parts: 1-4 parts of 2-acrylamide-2-methylpropane sulfonate, 14-20 parts of acrylate, 1-4 parts of acrylic acid, 1-2 parts of cross-linking agent, 1-2 parts of initiator and 60-80 parts of solvent, and the solvent is a mixture of isopropanol and distilled water. The plugging agent has the effect of delayed expansion, and almost no water absorption and expansion occurs in clear water. Under alkaline conditions, the water absorption and expansion at 80°C reaches more than 10 times; it utilizes the introduction of esterification groups, which are hydrolyzed by temperature and alkalinity, thereby exposing the water-absorbing groups, and then water absorption and expansion occur again. However, there are the following problems: (1) Limited application scenarios: The plugging agent is only applicable to the process of drilling construction. Taking advantage of the characteristics of the drilling fluid having an alkaline environment, the plugging fluid is added to the downhole drilling fluid to achieve the effect of delayed expansion. For cementing technology of inserting small casing into old shale gas wells, there is no drilling construction operation, so there is no drilling fluid, so the application scenarios of the above technology are greatly limited; (2) The plugging time and effect are uncontrollable: the plugging agent mainly contains ester materials, which basically do not absorb water and swell in clean water, but will gradually hydrolyze in an alkaline environment and absorb water and swell. The hydrolysis rate of esters is related to temperature and alkali concentration. The alkali concentration of drilling fluid will change continuously during the drilling process due to the interference of the formation, and the drilling well temperature is also constantly changing. Therefore, the hydrolysis rate of ester materials is difficult to control and the plugging effect is difficult to guarantee. In addition, after the plugging fluid enters the formation cracks, it will be diluted by the formation water, further increasing the uncertainty of the hydrolysis degree of the ester material. The uncertainty of the hydrolysis rate of the ester material caused by the above situation may cause the ester plugging material to swell prematurely and fail to enter the cracks to achieve the purpose of plugging, or it may enter the cracks. Due to low alkali concentration or low temperature, the ester material will not hydrolyze and swell for a long time, resulting in plugging failure. (3) The water absorption expansion ratio is limited: the esterification group is hydrolyzed by temperature and alkalinity and then absorbs water and expands. Under alkaline conditions, the water absorption expansion at 80°C is only more than 10 times, and in the examples, it is up to 30 times, which still needs to be further improved. Summary of the invention
[0005] The purpose of the present invention is to solve the above technical problems and provide a method which is extremely simple, low-cost, controllable plugging time and expansion coefficient, and good plugging effect, and is very suitable for casing plugging construction in shale gas well casing.
[0006] The oil and gas well crack plugging method of the present invention comprises the following steps:
[0007] 1) Prepare the plugging liquid. The components and weight ratios are as follows:
[0008] Water: 100 parts, xanthan gum: 2-4 parts, polyacrylamide water-absorbing resin: 1-5 parts, polypropylene fiber: 0.1-0.6 parts, defoaming agent: 1-4 parts;
[0009] 2) pumping the plugging liquid obtained in step 1) to the bottom of the well, and continuing to squeeze the plugging liquid into the formation cracks after the well is shut down;
[0010] 3) Pump the sodium hydroxide solution into the cracks. Under the high temperature of the formation exceeding 50°C, the polyacrylamide absorbent resin is hydrolyzed into polyacrylic acid absorbent resin, thus completing the crack sealing.
[0011] In the step 1), the polyacrylamide water-absorbing resin is prepared by uniformly mixing 100 parts of water, 20 parts of acrylamide monomer, 0.06 parts of N,N-methylenebisacrylamide and 0.2 parts of ammonium persulfate, curing at 60° C. for 4 hours, drying and crushing.
[0012] In the step 1), the particle size of the polyacrylamide water-absorbing resin is 100 mesh to 200 mesh.
[0013] In the step 1), the fiber length of the polypropylene fiber is 6 mm to 10 mm.
[0014] In the step 2), the concentration of the sodium hydroxide solution is 2-4%wt.
[0015] In the step 2), the plugging liquid obtained in the step 1) is pumped to the bottom of the well and pumped into the well to 200-500m above the leaking layer.
[0016] In the step 2), after the well is shut in, the plugging fluid is continuously squeezed into the cracks until the pump pressure reaches 5-6 MPa.
[0017] In step 3), the sodium hydroxide solution is squeezed into the cracks at a volume of 10-15 m 3 , and retain at least 5-6m in the wellbore 3 .
[0018] In view of the technical problems existing in the background technology, the following improvements have been made: (1) For underground cracks without an alkaline environment, a step-by-step construction method is adopted, firstly, a plugging liquid containing a polyacrylamide absorbent resin with moderate water absorption and swelling properties is squeezed into the formation to initially form a plugging layer; then, an aqueous sodium hydroxide solution is squeezed into the cracks to hydrolyze the polyacrylamide absorbent resin into a polyacrylic acid absorbent resin, which greatly increases the water absorption multiple, so that the deformable polyacrylic acid absorbent resin is tightly filled in the cracks, reducing the leakage space of the cracks, and increasing the extrusion and overlap capacity between the absorbent resins, thereby improving the leak-proof ability of the plugging liquid. Compared with the background technology, the method of the present invention does not require the presence of drilling fluid downhole, and can also achieve the purpose of delayed expansion and plugging cracks, and is particularly suitable for well repair and plugging operations such as casing in casing; (2) The plugging time and effect are controllable: since it does not need to rely on drilling fluid to provide an alkaline environment, the concentration of the sodium hydroxide solution can be controlled according to the actual situation, and the time required for the expansion reaction (i.e., the plugging time) can be adjusted. The hydrolysis reaction can occur at a formation temperature exceeding 50°C, and the plugging effect is controllable. The plugging liquid can be squeezed into the formation and the later expansion activation can be achieved more accurately and reliably, and the construction reliability rate is high and the success rate is large. (3) The polyacrylamide water-absorbing resin is used as the main plugging agent of the plugging liquid. After absorbing water, it will expand, and the expansion multiple is about 22 times; after the formation temperature exceeds 50°C, in the environment of sodium hydroxide alkaline solution, the polyacrylamide water-absorbing resin will hydrolyze into polyacrylic acid water-absorbing resin, and its expansion multiple will increase by hundreds of times. After the water absorption multiple is significantly increased, the water-absorbing resin will seal the crack space tightly, thereby significantly improving the plugging effect. Here, compared with 100 parts of water, the addition amount of the polyacrylamide water-absorbing resin is 1 to 5 parts. Too much will lead to poor fluidity of the plugging liquid, and too little will lead to poor plugging effect. (4) The main function of the xanthan gum in the plugging liquid is to increase viscosity and suspend, preventing the sedimentation of the polyacrylamide resin. The main function of the fiber in the plugging liquid is to stabilize the polyacrylamide water-absorbing resin that enters the crack in the crack, enhance the retention capacity of the water-absorbing resin in the crack, and prevent the water-absorbing resin from entering the deep crack under the effect of density difference and later sodium hydroxide aqueous solution squeezing and other effects to affect the plugging effect.
[0019] The method of the invention is extremely simple, low in cost, and has a good plugging time and plugging effect, and is particularly suitable for casing plugging construction operations in shale gas well casings. DETAILED DESCRIPTION
[0020] In order to more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the embodiments or the prior art will be briefly introduced below. Obviously, the following descriptions are only some embodiments of the present invention. For those of ordinary skill in the art, other embodiments can be obtained based on these embodiments without creative work. The following parts are parts by weight.
[0021] Example 1
[0022] Preparation of plugging liquid: prepare the plugging liquid according to 100 parts of water, 2 parts of xanthan gum, 1 part of polyacrylamide absorbent resin, 0.1 parts of polypropylene fiber and 1 part of defoaming agent.
[0023] Prepare sodium hydroxide solution according to 100 parts of water and 2 parts of sodium hydroxide.
[0024] Experiment: The prepared plugging liquid was cured at 84°C, and the water absorption multiple of the water-absorbing resin was tested regularly. After the water-absorbing resin in the prepared plugging liquid was saturated with water in the plugging liquid, the water absorption multiple was 21 times. The water-absorbing resin saturated with water in the plugging liquid was placed in sodium hydroxide lye and cured at 84°C for 24 hours. The water absorption multiple was tested to be 368 times.
[0025] Operation: In a shale gas well with a depth of 3,200 meters and a bottom hole temperature of 84°C, before the casing-in-casing cementing operation, the plugging liquid was pumped to the bottom of the well using a continuous tubing and pumped to 200m above the leaking layer; after the well was shut down, the plugging liquid was continuously squeezed into the formation cracks until the pump pressure reached 5MPa; then the continuous tubing was used to pump 10m 3 Sodium hydroxide solution is squeezed into the formation cracks and stored in the wellbore for 5m 3 Sodium hydroxide lye, make sure the lye completely soaks the polyacrylamide absorbent resin in the cracks, and wait for 24 hours.
[0026] When the pump pressure was increased to the possible bottom hole pressure of 11 MPa during cementing, the wellbore leakage was measured to be 0.5 L / min, and the leakage was significantly reduced, which can effectively prevent the occurrence of well leakage during cementing construction.
[0027] Example 2
[0028] Preparation of plugging liquid: prepare the plugging liquid according to 100 parts of water, 3 parts of xanthan gum, 3 parts of polyacrylamide absorbent resin, 0.3 parts of polypropylene fiber and 2 parts of defoaming agent.
[0029] Prepare sodium hydroxide solution according to 100 parts of water and 3 parts of sodium hydroxide.
[0030] In a shale gas well, the well depth is 3700 meters and the bottom temperature is 90℃. Before the casing-in-casing cementing operation, the plugging liquid is first pumped to the bottom of the well using a continuous tubing and pumped into the 500m above the leaking layer. After the well is shut down, the plugging liquid is continuously squeezed into the formation cracks until the pump pressure reaches 6MPa. Then the 15m 3 Sodium hydroxide solution is squeezed into the formation cracks and stored in the wellbore for 6m 3 Sodium hydroxide lye, make sure the lye completely soaks the polyacrylamide absorbent resin in the cracks, and wait for 24 hours.
[0031] When the pump pressure was increased to the possible bottom hole pressure of 11 MPa during cementing, the wellbore leakage was measured to be 0.4 L / min, and the leakage was significantly reduced, which can effectively prevent the occurrence of well leakage during cementing construction.
[0032] Example 3
[0033] Preparation of plugging liquid: prepare the plugging liquid according to 100 parts of water, 4 parts of xanthan gum, 5 parts of polyacrylamide absorbent resin, 0.6 parts of polypropylene fiber and 4 parts of defoaming agent.
[0034] Prepare sodium hydroxide lye according to 100 parts of water and 4 parts of sodium hydroxide.
[0035] A shale gas well with a depth of 3,600 meters and a bottom temperature of 88°C was used. Before the casing-in-casing cementing operation, the plugging fluid was pumped to the bottom of the well using a continuous tubing, and then pumped to 300m above the leaking layer and shut down the well. After shutting down the well, the plugging fluid was continuously squeezed into the formation cracks until the pump pressure reached 6MPa. Then, the plugging fluid was pumped to the bottom of the well using a continuous tubing. 3 Sodium hydroxide solution is squeezed into the formation cracks and stored in the wellbore for 5m 3 Sodium hydroxide lye, make sure the lye completely soaks the polyacrylamide absorbent resin in the cracks, and wait for 24 hours.
[0036] When the pump pressure was increased to the possible bottom hole pressure of 11 MPa during cementing, the wellbore leakage was measured to be 0.5 L / min, and the leakage was significantly reduced, which can effectively prevent the occurrence of well leakage during cementing construction.
[0037] Comparative Example 1
[0038] Preparation of plugging liquid: prepare the plugging liquid according to 100 parts of water, 3 parts of xanthan gum, 3 parts of polyacrylamide absorbent resin, 0.3 parts of polypropylene fiber and 2 parts of defoaming agent.
[0039] In a shale gas well with a depth of 3,600 meters and a bottom hole temperature of 88°C, before the casing-in-casing cementing operation, the plugging liquid was first pumped to the bottom of the well using a continuous tubing, and then pumped to 300m above the leaking layer and shut down the well; after shutting down the well, the plugging liquid was continued to be squeezed into the formation cracks until the pump pressure reached 6MPa, and then waited for 24 hours.
[0040] The pump pressure was increased to the possible bottom hole pressure of 11MPa during the cementing process, and the wellbore leakage was measured to be 45L / min. The leakage was large and difficult to meet the construction requirements.
[0041] Comparative Example 2
[0042] In a shale gas well with a depth of 3,700 meters and a bottom hole temperature of 90°C, before the casing-in-casing cementing operation, the plugging liquid was first pumped to the bottom of the well using a continuous tubing and pumped to 500m above the leaking layer; the well was shut down and the plugging liquid was continued to be squeezed into the formation cracks until the pump pressure reached 5MPa, and then waited for 24 hours.
[0043] The pump pressure was increased to the possible bottom hole pressure of 11MPa during the cementing process, and the wellbore leakage was measured to be 30L / min. The leakage was large and difficult to meet the construction requirements.
[0044] According to the field test results of Comparative Examples 1 and 2, it can be seen that after only using a plugging liquid containing polyacrylamide water-absorbing resin, xanthan gum, fiber, etc. to plug the existing hydraulic fractures, the leakage is still very large, and it is difficult to form a good plugging effect on the existing fractures. According to the field test results of Example 1, Example 2 and Example 3, it can be seen that by using a plugging liquid containing polyacrylamide water-absorbing resin, xanthan gum, fiber, etc. to plug the existing hydraulic fractures, and then squeezing sodium hydroxide alkali solution into the fractures, the water-absorbing resin is hydrolyzed into polyacrylic acid water-absorbing resin, and the volume of the water-absorbing resin is continuously increased to make the cracks more densely plugged, which can effectively improve the plugging effect of the cracks and provide reliable protection for the construction of casing-in-casing cementing operations.
Claims
1. A method for plugging leaks in oil and gas well cracks, characterized in that: The following steps are involved: 1) Prepare the plugging liquid. The components and weight ratios are as follows: Water: 100 parts, xanthan gum: 2-4 parts, polyacrylamide water-absorbing resin: 1-5 parts, polypropylene fiber: 0.1-0.6 parts, defoaming agent: 1-4 parts; 2) pumping the plugging liquid obtained in step 1) to the bottom of the well, and continuing to squeeze the plugging liquid into the formation cracks after the well is shut down; 3) Pump the sodium hydroxide solution into the cracks. Under the high temperature of the formation exceeding 50°C, the polyacrylamide absorbent resin is hydrolyzed into polyacrylic acid absorbent resin, thus completing the crack sealing.
2. The method for plugging leaks in oil and gas well cracks according to claim 1, characterized in that: In the step 1), the polyacrylamide water-absorbing resin is prepared by uniformly mixing 100 parts of water, 20 parts of acrylamide monomer, 0.06 parts of N,N-methylenebisacrylamide and 0.2 parts of ammonium persulfate, curing at 60° C. for 4 hours, drying and crushing.
3. The method for plugging leaks in oil and gas well cracks according to claim 1, characterized in that: In the step 1), the particle size of the polyacrylamide water-absorbing resin is 100 mesh to 200 mesh.
4. The method for plugging leaks in oil and gas well cracks according to claim 1, characterized in that: In the step 1), the fiber length of the polypropylene fiber is 6 mm to 10 mm.
5. The method for plugging leaks in oil and gas well cracks according to any one of claims 1 to 4, characterized in that: In the step 2), the concentration of the sodium hydroxide solution is 2-4%wt.
6. The method for plugging leaks in oil and gas well cracks according to any one of claims 1 to 4, characterized in that: In the step 2), the plugging liquid obtained in the step 1) is pumped to the bottom of the well and pumped into the well to 200-500m above the leaking layer.
7. The method for plugging leaks in oil and gas well cracks according to any one of claims 1 to 4, characterized in that: In the step 2), after the well is shut in, the plugging fluid is continuously squeezed into the cracks until the pump pressure reaches 5-6 MPa.
8. The method for plugging leaks in oil and gas well cracks according to any one of claims 1 to 4, characterized in that: In step 3), the sodium hydroxide solution is squeezed into the cracks at a volume of 10-15 m 3 , and retain at least 5-6m in the wellbore 3 .
Citation Information
Patent Citations
Novel delayed-expansion type plugging agent and preparation method thereof
CN108048055A