Pressure sensing and storage integrated device and preparation method thereof

By wrapping the pressure sensing and storage integrated device of the pressure sensing layer and the storage auxiliary layer on the porous elastic matrix, the problems of easy loss of signals of traditional pressure sensors and low processing speed are solved, and more efficient pressure signal processing and storage are achieved, reducing pressure signal processing and storage Energy consumption is suitable for applications in multiple fields.

CN118999854APending Publication Date: 2024-11-22XIAMEN UNIV
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411076548.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-07
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

Traditional pressure sensors quickly return to the initial state after the external pressure is removed, resulting in signal loss, and the integration of separate perception with storage hardware leads to problems such as reduced processing speed, increased energy consumption and data redundancy.

Method used

Design a pressure sensing and storage integrated device, by wrapping the pressure sensing layer and the pressure storage auxiliary layer on the porous elastic matrix, using conductive materials and polymer shear thickening liquid for impregnation, combined with a flexible packaging layer, the device is realized Preparation, prolonging the recovery time of the pressure sensing layer to store the pressure signal.

Benefits of technology

It significantly improves the processing capacity and speed of pressure sensing systems, reduces data redundancy and energy consumption, provides greater flexibility and application potential, and promotes the development of pressure sensing systems toward efficient, safe and intelligent directions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118999854A_ABST
    Figure CN118999854A_ABST
Patent Text Reader

Abstract

The invention relates to a pressure sensing and storage integrated device and a preparation method thereof, the pressure sensing and storage integrated device comprises a device body, the device body comprises a porous elastic matrix, the periphery of the porous elastic matrix is wrapped with a pressure sensing layer, the periphery of the pressure sensing layer is wrapped with a pressure storage auxiliary layer, or the periphery of the porous elastic matrix is wrapped with the pressure storage auxiliary layer. The periphery of the pressure storage auxiliary layer is wrapped by a pressure sensing layer. The pressure sensing layer obtains external pressure signals, the pressure auxiliary storage layer prolongs the recovery time of the pressure sensing layer after the pressure sensing layer is pressed, and the recovery stage is a storage stage, so that a single device has dual capabilities of sensing and storing the pressure signals, the processing capability and speed of the pressure sensing system on the pressure signals are remarkably improved, and the reliability of the pressure sensing system is improved. The problems of low speed, data redundancy, high energy consumption and the like caused by a separated integrated device are solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of pressure sensors, and in particular to a pressure sensing and storage integrated device and a preparation method thereof. Background Art

[0002] The pressure sensing system can sense external pressure signals and convert them into usable electrical signal outputs. It is often used in wearable devices, smart homes, bionic prostheses, intelligent robots, etc. The pressure signal of a traditional pressure sensor is volatile, that is, when the external pressure is removed, the pressure sensor quickly returns to its initial state and the previous pressure signal is lost, so the pressure sensor signal needs to be stored for subsequent signal processing.

[0003] In the prior art, pressure sensing elements are usually integrated with devices with storage functions such as memristors or memories to form an integrated pressure sensing system. The pressure sensing unit is responsible for sensing external pressure information, and the storage device completes the time-series recording and storage of the signal. However, the integration of this separate perception and storage hardware will inevitably lead to a decrease in processing speed. In addition, the integrated design will also introduce redundancy in data processing, consume a large amount of computing resources and storage space, and increase the energy consumption of the system in application scenarios that frequently respond to external changes. Summary of the invention

[0004] In view of the shortcomings of the background technology, the object of the present invention is to provide a pressure sensing and storage integrated device and a preparation method thereof.

[0005] To achieve the above object, the present invention provides the following technical solutions:

[0006] A pressure sensing and storage integrated device comprises a device body, wherein the device body comprises a porous elastic matrix, a pressure sensing layer is wrapped around the porous elastic matrix, a pressure storage auxiliary layer is wrapped around the pressure sensing layer, or the porous elastic matrix is ​​wrapped around the pressure storage auxiliary layer, and the pressure storage auxiliary layer is wrapped around the pressure sensing layer.

[0007] Furthermore, the porous elastic substrate is wrapped with a pressure sensing layer, and the pressure sensing layer is wrapped with a pressure storage auxiliary layer.

[0008] Furthermore, it also includes a flexible packaging layer, which is respectively attached to the top surface and the bottom surface of the device body.

[0009] A method for preparing a pressure sensing and storage integrated device comprises the following steps:

[0010] Step 1: Disperse the conductive material in deionized water, stir at room temperature, add 0.05wt% to 1wt% of an aqueous dispersant, dissolve and stir at room temperature to obtain a conductive modified solution with a conductive material concentration of 0.5wt% to 5wt% by mass, and then immerse the porous elastic matrix in the conductive modified solution for 1 to 3 hours, take it out and dry it at 50°C to 80°C, repeat the above immersion operation several times, and prepare a conductive porous elastic matrix wrapped by the pressure sensing layer;

[0011] Step 2: The conductive porous elastic matrix obtained in step 1 is immersed in a polymer shear thickening liquid with a concentration of 1wt% to 10wt% for 5 to 30 minutes, and dried at 70 to 90°C for 3 to 6 hours to obtain a porous elastic matrix wrapped by a pressure sensing and storage auxiliary layer;

[0012] Step 3: Attach a flexible packaging layer to the top and bottom surfaces of the porous elastic matrix obtained in step 2 to prepare an integrated pressure sensing and storage device.

[0013] Furthermore, in step 1, the porous elastic matrix needs to be cleaned before the immersion treatment, which specifically includes the following steps: adding the porous elastic matrix to anhydrous ethanol, ultrasonically treating it, rinsing it in deionized water for 5-10 minutes to remove surface oil and impurities, and finally drying it at room temperature.

[0014] Furthermore, in step 1, the conductive material is any one or more of carbon nanotubes, carbon black, graphite, graphene, graphene oxide, reduced graphene oxide, and polypyrrole nanoparticles.

[0015] Furthermore, in step 1, the aqueous dispersant is any one of polyvinyl alcohol, polyacrylic acid, polyvinyl pyrrolidone, sodium carboxymethyl cellulose, and hydroxyethyl cellulose.

[0016] Furthermore, in step 1, the porous elastic matrix is ​​made of one of polyvinyl chloride, polyethylene, polypropylene, polyurethane, and thermoplastic polyurethane.

[0017] Furthermore, in step 2, the polymer shear thickening liquid is any one of polyborosiloxane shear thickening liquid, silica shear thickening liquid, and polystyrene shear thickening liquid.

[0018] Furthermore, in step 3, the material used for the flexible packaging layer is any one of polyester film, polycarbonate, polysiloxane, polyvinyl alcohol, and epoxy resin.

[0019] The beneficial effects of the present invention are:

[0020] 1. The present invention proposes a pressure sensing and storage integrated device and a preparation method thereof. The pressure sensing layer realizes the acquisition of external pressure signals, and the pressure-assisted storage layer prolongs the recovery time of the pressure sensing layer after being compressed. The recovery stage is the storage stage, which enables a single device to have the dual capabilities of pressure signal sensing and storage, significantly improving the pressure sensing system's processing capability and speed for pressure signals, solving the problems of low speed, data redundancy and high energy consumption caused by separate integrated devices, providing greater flexibility and application potential for system design, and promoting the pressure sensing system to develop in a more efficient, safe and intelligent direction, and better meeting the application needs of multiple fields such as industry, medical care and consumer electronics. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] In order to more clearly illustrate the embodiments of the invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0022] Figure 1 is a schematic diagram of the present invention;

[0023] Figure 2 An exploded view of the present invention;

[0024] Figure 3 for Figure 1 AA section view;

[0025] Figure 4 for Figure 3 An enlarged schematic diagram of point B;

[0026] Figure 5 One of the current and time variation curves when the present invention senses and stores pressure signals;

[0027] Figure 6 The second graph of the current and time variation when the present invention senses and stores the pressure signal;

[0028] In the figure, 10, device body; 101, porous elastic matrix; 102, pressure sensing layer; 103, pressure storage auxiliary layer; 20, flexible packaging layer. DETAILED DESCRIPTION

[0029] Combine the following Figure 1-6 The present invention is described in detail.

[0030] A pressure sensing and storage integrated device includes a device body 10, wherein the device body 10 includes a porous elastic matrix 101, wherein the porous elastic matrix 101 is wrapped with a pressure sensing layer 102, wherein the pressure sensing layer 102 is wrapped with a pressure storage auxiliary layer 103, or wherein the porous elastic matrix 101 is wrapped with a pressure storage auxiliary layer 103, wherein the pressure storage auxiliary layer 103 is wrapped with the pressure sensing layer 102.

[0031] In this embodiment, the porous elastic matrix 101 is wrapped with a pressure sensing layer 102 , and the pressure sensing layer 102 is wrapped with a pressure storage auxiliary layer 103 .

[0032] In this embodiment, a flexible packaging layer 20 is further included, which is attached to the top surface and the bottom surface of the device body 10 respectively.

[0033] A method for preparing a pressure sensing and storage integrated device comprises the following steps:

[0034] Step 1: Disperse the conductive material in deionized water, stir at room temperature, add 0.05wt% to 1wt% of an aqueous dispersant, dissolve and stir at room temperature to obtain a conductive modified solution with a conductive material concentration of 0.5wt% to 5wt% by mass, and then immerse the porous elastic matrix 101 in the conductive modified solution for 1 to 3 hours, take it out and dry it at 50°C to 80°C, repeat the above immersion operation several times, and prepare a conductive porous elastic matrix 101 wrapped by a pressure sensing layer 102;

[0035] Step 2: The conductive porous elastic substrate 101 obtained in step 1 is immersed in a polymer shear thickening liquid with a concentration of 1wt% to 10wt% for 5 to 30 minutes, and dried at 70 to 90°C for 3 to 6 hours to obtain a porous elastic substrate 101 wrapped by a pressure sensing and storage auxiliary layer;

[0036] Step 3: Attach the flexible packaging layer 20 to the top and bottom surfaces of the porous elastic substrate 101 obtained in step 2 to prepare a pressure sensing and storage integrated device.

[0037] In this embodiment, in step 1, the porous elastic matrix 101 needs to be cleaned before the immersion treatment, which specifically includes the following steps: adding the porous elastic matrix 101 to anhydrous ethanol, ultrasonically treating it, placing it in deionized water for 5-10 minutes to remove surface oil and impurities, and finally drying it at room temperature.

[0038] In this embodiment, in step 1, the conductive material is any one or more of carbon nanotubes, carbon black, graphite, graphene, graphene oxide, reduced graphene oxide, and polypyrrole nanoparticles.

[0039] In this embodiment, in step 1, the aqueous dispersant is any one of polyvinyl alcohol, polyacrylic acid, polyvinyl pyrrolidone, sodium carboxymethyl cellulose, and hydroxyethyl cellulose.

[0040] In this embodiment, in step 1, the porous elastic matrix 101 is made of one of polyvinyl chloride, polyethylene, polypropylene, polyurethane, and thermoplastic polyurethane.

[0041] In this embodiment, in step 2, the polymer shear thickening liquid is any one of polyborosiloxane shear thickening liquid, silica shear thickening liquid, and polystyrene shear thickening liquid.

[0042] In this embodiment, in step 3, the material used for the flexible packaging layer 20 is any one of polyester film, polycarbonate, polysiloxane, polyvinyl alcohol, and epoxy resin.

[0043] Specifically, in step 1, graphite is dispersed in deionized water, stirred at room temperature, 0.05wt% polyvinyl alcohol is added, dissolved and stirred at room temperature, and a conductive modified solution with a graphite concentration of 0.5wt% by mass is obtained, and then the porous elastic matrix 101 is immersed in the conductive modified solution for 1 hour, taken out and dried at 50°C, and the above immersion operation is repeated several times; in step 2, the conductive porous elastic matrix 101 obtained in step 1 is immersed in a 10wt% polyborosiloxane shear thickening solution for 5 minutes, and dried at 70°C for 3 hours; in step 3, a flexible encapsulation layer 20 made of polyester film is attached to the top and bottom surfaces of the porous elastic matrix 101 obtained in step 2. The porous elastic matrix 101 is irregularly distributed at any position of the elastic matrix.

[0044] The present invention proposes a pressure sensing and storage integrated device and a preparation method thereof, and its working principle is as follows:

[0045] When subjected to pressure, the device as a whole undergoes compression deformation, and the pressure sensing layer 102 and the pressure storage auxiliary layer 103 have a consistent deformation trend. The deformation caused by the device compression causes the conductive materials in the pressure sensing layer 102 to quickly contact. The contact area between the conductive materials depends on the applied pressure and directly affects the tightness of the conductive network, thereby causing the device resistance signal to change. This is the process of the pressure sensing layer 102 sensing the signal. For more specific processes and principles, please refer to the prior art and common knowledge in this field.

[0046] If there is no pressure storage auxiliary layer 103, the porous elastic matrix 101 will rebound quickly and return to its original state after being compressed, so that the pressure signal disappears quickly, and there is no time to convert it into a current signal output and read the pressure value. The present invention specifically sets a pressure storage auxiliary layer 103. After being compressed, the polymer material in the pressure storage auxiliary layer 103 will fuse due to the pressure, and the intermolecular force makes it tightly bonded, thereby generating resistance to the pressure sensing layer 102 and the porous elastic matrix 101, and the bonding contact area is positively correlated with the magnitude of the applied pressure. The greater the pressure, the greater the contact area of ​​the polymer bonding, resulting in greater resistance generated by the adhesion of the polymer material. When the pressure is removed, due to the existence of this resistance, the rebound of the porous elastic matrix 101 is hindered, and then the electrical contact state of the conductive material in the pressure sensing layer 102 is regulated, and the conductive network formed cannot be quickly restored to the initial state, resulting in the resistance change of the pressure sensing layer 102 caused by the compression deformation showing a gradual recovery trend over a period of time, rather than a step response, and it is precisely because of the non-step response that there is time to output the signal and read the pressure value. In other words, the pressure storage auxiliary layer 103 provides resistance so that the entire device can only slowly return to its original state. During the process of returning to its original state, the pressure signal is converted into a current signal, and the current signal can exist for a certain period of time, which is equivalent to the pressure signal existing in another form after the pressure is removed and not disappearing immediately, so that the current resistance signal can always keep the memory of the initial pressure information during this slow recovery process. The process of slowly returning to its original state is the pressure information "storage" stage.

[0047] The degree of resistance signal recovery is positively correlated with the slow recovery time after the pressure is removed. The longer the resistance recovery time is, the greater the degree of resistance signal recovery is. Therefore, in the entire resistance recovery process, there are corresponding resistance recovery time points and resistance recovery sizes corresponding to the initial pressure. The initial pressure information can be accurately obtained through the corresponding relationship.

[0048] like Figure 5As shown in the figure, when the pressure sensing and storage integrated device is not subjected to pressure, the state of the pressure sensing and storage integrated device is defined as stage I, indicating that the pressure sensing and storage integrated device is in the initial state; when the pressure sensing and storage integrated device is subjected to pressure, the state of the pressure sensing and storage integrated device is defined as stage II, indicating that the pressure sensing and storage integrated device is in the pressure sensing process; when the pressure sensing and storage integrated device removes the applied pressure, the state of the pressure sensing and storage integrated device is defined as stage III, indicating that the pressure sensing and storage integrated device is in the pressure storage process. In stage III, i.e., each time period Δt in the slow recovery process has a corresponding current change ΔI corresponding to it, and this corresponding relationship refers to the nonlinear relationship between Δt and ΔI. In order to obtain this nonlinear relationship, it is necessary to do multiple groups of experiments before formally using the device: apply pressure of the same pressure value multiple times (know the pressure value applied when applying), and then observe the numerical relationship between Δt and ΔI in the current and time change curve, so as to obtain the nonlinear relationship, so as to infer the pressure value applied when formally using it.

[0049] For initial pressures of different magnitudes, the greater the initial pressure, the greater the resistance generated by the adhesion of the polymer material in the pressure sensing layer 102, and the longer the resistance recovery time. By comparing the relative recovery rate of the resistance signal at the same resistance recovery time, that is, the greater the initial pressure, the slower the relative recovery of the resistance signal at the same resistance recovery time, pressures of different magnitudes can be identified. Regarding how to compare the relative recovery rate of the resistance signal: for two pressures of different magnitudes at the same resistance recovery time, the change value of each current I is divided by the peak value of each current I to obtain values ​​a and b respectively. Compare the values ​​a and b. The smaller the value, the greater the initial pressure. For details, please refer to Figure 6 , I1 / I 10 >I2 / I 20 >I3 / I 30 , so curve 1( Figure 6 The initial pressure of curve 3 (the curve at the bottom) is the smallest. Figure 6 The initial pressure of the curve at the top is the highest.

[0050] In short, after the pressure applied to the device is removed, the resistance generated by the viscoelastic polymer of the pressure storage auxiliary layer 103 can regulate the resistance recovery process of the pressure sensing layer 102. During this whole process, the initial pressure can be obtained through the corresponding relationship between the degree of resistance signal recovery and the slow recovery time after the pressure is removed. In addition, by adjusting the viscosity of the polymer material and the contact area of ​​mutual adhesion, the adhesion resistance can be changed to achieve the regulation of the storage time. The more sticky it is, the longer the recovery time and the longer the storage time.

[0051] The signal output and reading process refer to the prior art, and the external ammeter is always connected to the device to output and read the data of the pressure sensing layer 102. The pressure storage auxiliary layer 103 prolongs the time required for the resistance change recovery of the pressure sensing layer 102, so that the external ammeter has sufficient time to output and read the data. If there is no pressure storage auxiliary layer 103, the external ammeter will not have time to output and read the data, and can only set up a special memory like the prior art.

[0052] The above embodiments are only for illustrating the technical concept and features of the present invention, and their purpose is to enable those skilled in the art to understand the content of the present invention and implement it, and they cannot be used to limit the protection scope of the present invention. Any equivalent changes or modifications made according to the spirit of the present invention should be included in the protection scope of the present invention.

Claims

1. A pressure sensing and storage integrated device, characterized in that: The device body includes a porous elastic matrix, the porous elastic matrix is ​​wrapped with a pressure sensing layer on the periphery, the pressure sensing layer is wrapped with a pressure storage auxiliary layer on the periphery, or the porous elastic matrix is ​​wrapped with a pressure storage auxiliary layer on the periphery, the pressure storage auxiliary layer is wrapped with a pressure sensing layer on the periphery.

2. The integrated pressure sensing and storage device according to claim 1, characterized in that: The porous elastic substrate is wrapped with a pressure sensing layer, and the pressure sensing layer is wrapped with a pressure storage auxiliary layer.

3. A pressure sensing and storage integrated device according to any one of claims 1-2, characterized in that: It also includes flexible packaging layers, which are respectively attached to the top surface and the bottom surface of the device body.

4. A method for preparing a pressure sensing and storage integrated device, characterized in that: The following steps are involved: Step 1: Dispersing a conductive material in deionized water, stirring at room temperature, adding 0.05 wt% to 1 wt% of an aqueous dispersant, dissolving and stirring at room temperature to prepare a conductive modification solution having a conductive material concentration of 0.5 wt% to 5 wt% by mass, and then immersing a porous elastic substrate in the conductive modification solution for 1 to 3 hours, removing the porous elastic substrate and drying it at 50°C to 80°C. Repeating the above immersion operation several times to prepare a conductive porous elastic substrate wrapped by the pressure sensing layer; Step 2: immersing the conductive porous elastic matrix obtained in step 1 in a polymer shear thickening solution having a concentration of 1 wt% to 10 wt% for 5 to 30 minutes, and drying at 70 to 90° C. for 3 to 6 hours to obtain a porous elastic matrix wrapped by a pressure sensing and storage auxiliary layer; Step 3: Attach flexible packaging layers to the top and bottom surfaces of the porous elastic matrix obtained in step 2 to prepare an integrated pressure sensing and storage device.

5. The method for preparing a pressure sensing and storage integrated device according to claim 4, characterized in that: In step 1, the porous elastic matrix needs to be cleaned before the dipping treatment, which specifically includes the following steps: adding the porous elastic matrix to anhydrous ethanol, ultrasonically treating it, rinsing it in deionized water for 5-10 minutes to remove surface oil and impurities, and finally drying it at room temperature.

6. A method for preparing a pressure sensing and storage integrated device according to claim 4 or 5, characterized in that: In step 1, the conductive material is any one or more of carbon nanotubes, carbon black, graphite, graphene, graphene oxide, reduced graphene oxide, and polypyrrole nanoparticles.

7. The method for preparing a pressure sensing and storage integrated device according to claim 4 or 5, characterized in that: In step 1, the aqueous dispersant is any one of polyvinyl alcohol, polyacrylic acid, polyvinyl pyrrolidone, sodium carboxymethyl cellulose, and hydroxyethyl cellulose.

8. The method for preparing a pressure sensing and storage integrated device according to claim 4 or 5, characterized in that: In step 1, the porous elastic matrix is ​​made of one of polyvinyl chloride, polyethylene, polypropylene, polyurethane, and thermoplastic polyurethane.

9. The method for preparing a pressure sensing and storage integrated device according to claim 4 or 5, characterized in that: In step 2, the polymer shear thickening liquid is any one of polyborosiloxane shear thickening liquid, silica shear thickening liquid, and polystyrene shear thickening liquid.

10. The method for preparing a pressure sensing and storage integrated device according to claim 4 or 5, characterized in that: In step 3, the material used for the flexible packaging layer is any one of polyester film, polycarbonate, polysiloxane, polyvinyl alcohol, and epoxy resin.

Citation Information

Patent Citations

  • Press bar sensing in-hole pressure distribution states

    CN111119860A

  • Perception and storage integrated bionic tactile fiber and preparation method thereof

    CN112816528A

  • Pressure sensor module

    JP1998185734A

  • Highly-Sensitive Capacitive-Type Pressure Sensor for Detection of Motion Embedded into Automatic Safety Shutdown System of Cutting Process Equipment

    KR102242936B1

  • Flexible embedded interconnects

    US20140170919A1