Lower cover plate with flow uniformizing function, preparation method thereof and probe card
By designing multiple through holes on the lower cover of the probe card and setting a second plating layer, the electrical connection between the probe and the first plating layer is achieved, and the problem of probe ablation due to excessive current is solved, and the probe is improved The stability of the needle card and reduces production costs.
Patent Information
- Application Number
- CN202411084144.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-11-22
AI Technical Summary
During the testing process of existing vertical probe cards, the probe is ablated due to excessive current, which causes the probe cards to need to be repaired or scrapped, which increases production costs.
A lower cover plate with uniform flow function is designed, and a plurality of through holes is formed by depositing and electroplating on the substrate, and a second plating layer is provided on the inner wall of the through hole, through which the probe passes through the through hole and the first plating layer is electrically compatible. Connect to achieve shunt and uniform current, avoiding ablation of a single probe due to excessive current.
It improves the test stability of the probe card, reduces production costs, and avoids the ablation of the probe due to excessive current.
Smart Images

Figure CN119001168A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of probe cards, and in particular to a lower cover plate with a flow-uniforming function, a preparation method thereof, and a probe card. Background Art
[0002] Before chip packaging, it is usually necessary to use a probe card to test its performance to reduce the defective rate of chip products. Currently, the common types of probe cards on the market include: cantilever probe cards, MEMS probe cards (2D / 3D) and vertical probe cards.
[0003] A common vertical probe card includes a test head and a PCB (Printed Circuit Board). The test head includes an upper cover, a lower cover and a plurality of probes. The upper cover and the lower cover are connected to the PCB through fasteners. The upper cover is located on the side of the lower cover close to the PCB. The probes are inserted into the upper cover and the lower cover. The needle tails of the probes penetrate the upper cover so as to contact the PAD (pad) on the PCB. The lower cover is roughly located at the needle rod of the probe to prevent the probe from jumping too much during the test. During the test, the needle head and needle tail of the probe contact the chip PAD and the PCB PAD respectively, thereby achieving signal conduction. However, during the test process, some probes are burned due to excessive current, so the probe card needs to be repaired. In severe cases, the probe card may even be scrapped, increasing production costs. Summary of the invention
[0004] In order to overcome the defects in the prior art, the embodiments of the present invention provide a lower cover plate with a flow-uniforming function, a preparation method thereof, and a probe card, which are used to solve the above-mentioned problems.
[0005] The embodiment of the present application discloses: a method for preparing a lower cover plate with a flow-uniform function, comprising the following steps:
[0006] Providing a substrate, the substrate comprising a first surface and a second surface arranged opposite to each other, and depositing a first seed layer on the first surface and / or the second surface of the substrate;
[0007] Performing photolithography and development on the first seed layer to form a plating area and a non-plating area on the substrate, and then electroplating a first plating layer in the plating area;
[0008] Performing degumming corrosion on the electroplated substrate to remove the first seed layer in the non-electroplating area on the substrate;
[0009] Disposing a film layer on the first surface and the second surface of the substrate, wherein the film layer covers the substrate and the first coating layer thereon;
[0010] Punching holes on the substrate after the film layer is provided, so that a plurality of through holes are formed on the substrate, and the through holes penetrate the film layer, the first plating layer and the substrate at the same time;
[0011] Depositing a second seed layer on the film layer, and then electroplating the substrate to form a second plating layer on the surface of the film layer and the inner wall of the through hole;
[0012] The second seed layer and the second plating layer are removed from the surface of the film layer.
[0013] Specifically, the substrate includes a plurality of electroplating regions that are arranged at intervals, so that the first plating layers in the plurality of electroplating regions are arranged at intervals.
[0014] Specifically, the substrate is one of sapphire, ceramic, silicon carbide or silicon nitride.
[0015] Specifically, the film layer is made of dry film or PI film, and the thickness of the film layer is between 10 and 20 μm.
[0016] Specifically, the first seed layer and / or the second seed layer is made of copper-titanium alloy, copper-chromium alloy or copper.
[0017] Specifically, the first plating layer and / or the second plating layer is metal copper.
[0018] Specifically, holes are punched on the substrate by laser.
[0019] Specifically, the second seed layer and the second coating layer on the surface of the film layer are removed by chemical mechanical polishing.
[0020] The embodiment of the present application also discloses: a lower cover plate with a flow-uniforming function, comprising a substrate, the substrate comprising a first surface and a second surface arranged opposite to each other, a first coating layer being provided on the first surface and / or the second surface of the substrate, a plurality of through holes being provided on the substrate and penetrating the first coating layer and the substrate at the same time, and an inner wall of the through hole being provided with a second coating layer for communicating with the first coating layer.
[0021] The embodiment of the present application also discloses: a probe card, which includes a plurality of probes and a lower cover plate with a flow equalization function as described in the embodiment, wherein the plurality of probes are respectively inserted into through holes of the lower cover plate with a flow equalization function.
[0022] The present invention has at least the following beneficial effects: the lower cover plate with current equalization function in the present scheme has a second plating layer in the through hole for installing the probe of the probe card, and the second plating layers in multiple (probe) through holes in the same network are electrically connected through the first plating layer corresponding to the network. In this way, multiple probes in the same network can be electrically connected through the first plating layer, and the first plating layer can shunt and equalize the current of multiple probes in the same network. When a probe is subjected to excessive current during the test, the current can be divided to other probes in the network through the first plating layer, thereby avoiding the phenomenon of burning of the probe due to excessive current, improving the test stability of the probe card, and reducing production costs.
[0023] In order to make the above and other purposes, features and advantages of the present invention more obvious and easy to understand, preferred embodiments are specifically cited below and described in detail with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0025] Figure 1 is a schematic diagram of the structure after the first seed layer is deposited on both sides of the substrate in an embodiment of the present invention;
[0026] Figure 2 is a schematic diagram of the structure of the first seed layer after photolithography and development in an embodiment of the present invention;
[0027] Figure 3 2 is a schematic diagram of a structure in which a first electroplating layer is electroplated on both sides of a substrate in an embodiment of the present invention;
[0028] Figure 4 Schematic diagram of the structure after the non-electroplating area on the substrate is stripped and etched in an embodiment of the present invention;
[0029] Figure 5 is a schematic diagram of the structure after film layers are provided on both sides of the substrate in an embodiment of the present invention;
[0030] Figure 6 It is a schematic diagram of the structure of punching holes in a substrate and forming a second plating layer in a through hole after a film layer is provided in an embodiment of the present invention;
[0031] Figure 7 yes Figure 6 A partial enlarged view of the middle A;
[0032] Figure 8is a schematic structural diagram of removing the second seed layer and the second coating layer from the surface of the film layer in an embodiment of the present invention;
[0033] Fig. 9 1 is a top view of a lower cover plate having a flow-uniforming function in an embodiment of the present invention.
[0034] The figure numbers of the above drawings are: 1, substrate; 11, through hole; 2, first seed layer; 3, photoresist; 4, first coating layer; 5, film layer; 6, second coating layer. DETAILED DESCRIPTION
[0035] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0036] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", "fixed", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium, and it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood by specific circumstances.
[0037] In the present invention, unless otherwise clearly specified and limited, a first feature being “above” or “below” a second feature may include the first feature and the second feature being in direct contact, or may include the first feature and the second feature being in contact not directly but through another feature between them. Moreover, a first feature being “above”, “below”, and “above” a second feature includes the first feature being directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being “below”, “below”, and “below” a second feature includes the first feature being below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0038] In the description of this embodiment, it should be understood that the terms "center", "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating the orientation or position relationship are based on the orientation or position relationship shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the scope of protection of the present application.
[0039] In addition, the terms "first", "second", etc. are only used to distinguish in description and have no special meaning.
[0040] The method for preparing the lower cover plate with flow uniformity function in this embodiment mainly comprises the following steps:
[0041] Step 1: Provide a substrate 1, the substrate 1 comprising a first surface and a second surface arranged opposite to each other, and deposit a first seed layer 2 on the first surface and / or the second surface of the substrate 1. Figure 1 As shown, in this embodiment, the first seed layer 2 is deposited on the first surface and the second surface of the substrate 1 respectively.
[0042] Step 2: Perform photolithography and development on the first seed layer 2 to form a plating area and a non-plating area on the substrate 1. Figure 2 As shown, a photoresist 3 is coated on the surface of the portion of the first seed layer 2 corresponding to the non-electroplating area of the substrate 1, and then developed, so that the first seed layer 2 corresponding to the non-electroplating area of the substrate 1 is covered by the photoresist 3, and the first seed layer 2 corresponding to the electroplating area of the substrate 1 is exposed. Subsequently, a first plating layer 4 is electroplated on the first seed layer 2 corresponding to the electroplating area of the substrate 1, as shown in FIG. Figure 3 shown.
[0043] Step 3: The substrate 1 after electroplating is subjected to degumming and etching to remove the photoresist 3 and the redundant first seed layer 2 on the surface of the substrate 1. Figure 4 shown.
[0044] Step 4: a film layer 5 is provided on the first surface and the second surface of the substrate 1 obtained in step 3, so that the film layer 5 covers the surface of the substrate 1 and the first coating layer 4 on the substrate 1, such as Figure 5 shown.
[0045] Step 5: drilling holes on the substrate 1 after the film layer 5 is provided, so that a plurality of through holes 11 for the probe to pass through are formed on the substrate 1. These through holes 11 penetrate the film layer 5, the first plating layer 4 and the substrate 1 at the same time, such as Figure 6 shown.
[0046] Step 6: Figure 6 and Figure 7As shown, a second seed layer (not shown in the figure) is deposited on the surface of the film layer 5 of the substrate 1 obtained in step 5, and then the substrate 1 is electroplated to form a second plating layer 6 on the surface of the film layer 5 and the inner wall of the through hole 11. Preferably, the second plating layer 6 on the inner wall of the through hole 11 extends along the axial direction to connect with the second plating layer 6 on the surface of the film layer 5, so as to ensure that the second plating layer 6 on the inner wall of the through hole 11 can be connected with the first plating layer 4 on the substrate 1.
[0047] Step 7: Figure 8 As shown, removing the second seed layer and the second plating layer 6 on the surface of the film layer 5 can prevent the second plating layers 6 on the inner walls of all through holes 11 on the substrate 1 from being electrically connected through the second seed layer and the second plating layer 6 .
[0048] It should be noted that the number of first plating layers 4 can be one or more, and the number of first plating layers 4 is determined by the number of networks in which multiple probes on the probe card are distributed. When the number of first plating layers 4 is multiple, multiple first plating layers 4 are arranged at intervals to avoid connecting two first plating layers 4 corresponding to different networks. Accordingly, in step 2, when preparing the electroplating area on the substrate 1, the multiple electroplating areas should be arranged at intervals to prepare the first plating layers 4 arranged at intervals in the subsequent steps.
[0049] Specifically, if Fig. 9 As shown, multiple probes of the probe card can be distributed in multiple different networks, and multiple probes can be included in the same network, and one first coating layer 4 corresponds to multiple probes in one network. In other words, the area of one first coating layer 4 is slightly larger than the area of the multiple probes in the corresponding network, so that each probe in the network can be connected to the first coating layer 4. If the first coating layer 4 is provided on both the first and second surfaces of the substrate 1, the positions of the first coating layers 4 on the two surfaces are substantially the same.
[0050] The lower cover plate prepared by the above method has a second coating 6 in the through hole 11 for installing the probe of the probe card. The second coating 6 in multiple (probe) through holes 11 in the same network is electrically connected through the first coating 4 corresponding to the network. In this way, multiple probes in the same network can be electrically connected through the first coating 4. The first coating 4 can shunt and equalize the multiple probes in the same network. When a probe is subjected to excessive current during the test, the current can be divided to other probes in the network through the first coating 4, thereby avoiding the phenomenon of burning of the probe due to excessive current, improving the test stability of the probe card, and reducing production costs.
[0051] Specifically, the substrate 1 of this embodiment can be made of sapphire, ceramic, silicon carbide or silicon nitride. Before forming the first seed layer 2 on the surface of the substrate 1, the substrate 1 can be polished to 100-500 μm by chemical mechanical polishing.
[0052] The film layer 5 of this embodiment can be made of a dry film or a PI film (Polyimide Film), the thickness of the film layer 5 is between 10 and 20 μm, and the film layer 5 is cured at a temperature of 100 to 300° C. for 12 hours.
[0053] The material of the first seed layer 2 and / or the second seed layer of this embodiment may be a copper-titanium alloy, a copper-chromium alloy or metal copper.
[0054] In this embodiment, the material of the first plating layer 4 and / or the second plating layer 6 may be metallic copper.
[0055] In step 5, laser can be used to drill holes in the substrate 1 and the first coating layer 4 and the film layer 5 on the surface thereof. Between step 4 and step 5, in other words, after the film layer 5 is provided on the substrate 1 and before drilling, the film layer 5 on the surface of the substrate 1 can be chemically mechanically polished.
[0056] In step 7, the second seed layer and the second plating layer 6 on the surface of the film layer 5 may be removed by chemical mechanical polishing.
[0057] The present invention uses specific embodiments to illustrate the principles and implementation methods of the present invention. The description of the above embodiments is only used to help understand the method of the present invention and its core idea. At the same time, for those skilled in the art, according to the idea of the present invention, there will be changes in the specific implementation methods and application scope. In summary, the content of this specification should not be understood as a limitation on the present invention.
Claims
1. A method for preparing a lower cover plate with a flow-uniform function, characterized in that: The following steps are involved: Providing a substrate, the substrate comprising a first surface and a second surface arranged opposite to each other, and depositing a first seed layer on the first surface and / or the second surface of the substrate; Performing photolithography and development on the first seed layer to form a plating area and a non-plating area on the substrate, and then electroplating a first plating layer in the plating area; Performing degumming corrosion on the electroplated substrate to remove the first seed layer in the non-electroplating area on the substrate; Disposing a film layer on the first surface and the second surface of the substrate, wherein the film layer covers the substrate and the first coating layer thereon; Punching holes on the substrate after the film layer is provided, so that a plurality of through holes are formed on the substrate, and the through holes penetrate the film layer, the first plating layer and the substrate at the same time; Depositing a second seed layer on the film layer, and then electroplating the substrate to form a second plating layer on the surface of the film layer and the inner wall of the through hole; The second seed layer and the second plating layer are removed from the surface of the film layer.
2. The method for preparing the lower cover plate with flow uniformity function according to claim 1, characterized in that: The substrate includes a plurality of electroplating regions arranged at intervals, so that the first plating layers in the plurality of electroplating regions are arranged at intervals.
3. The method for preparing the lower cover plate with flow uniformity function according to claim 1, characterized in that: The substrate is one of sapphire, ceramic, silicon carbide or silicon nitride.
4. The method for preparing the lower cover plate with flow uniformity function according to claim 1, characterized in that: The film layer is made of dry film or PI film, and the thickness of the film layer is between 10 and 20 μm.
5. The method for preparing the lower cover plate with flow uniformity function according to claim 1, characterized in that: The first seed layer and / or the second seed layer are made of copper-titanium alloy, copper-chromium alloy or copper.
6. The method for preparing the lower cover plate with flow uniformity function according to claim 1, characterized in that: The first plating layer and / or the second plating layer is metal copper.
7. The method for preparing the lower cover plate with flow uniformity function according to claim 1, characterized in that: Holes are punched on the substrate by laser.
8. The method for preparing the lower cover plate with flow uniformity function according to claim 1, characterized in that: The second seed layer and the second coating layer on the surface of the film layer are removed by chemical mechanical polishing.
9. A lower cover plate with flow equalization function, characterized in that: The invention comprises a substrate, wherein the substrate comprises a first surface and a second surface arranged opposite to each other, a first plating layer is arranged on the first surface and / or the second surface of the substrate, a plurality of through holes penetrating the first plating layer and the substrate at the same time are arranged on the substrate, and a second plating layer for communicating with the first plating layer is arranged on the inner wall of the through hole.
10. A probe card, characterized in that: It comprises a plurality of probes and the lower cover plate with a flow equalization function as claimed in claim 9, wherein the plurality of probes are respectively arranged in through holes of the lower cover plate with a flow equalization function, and the probes are in contact with the second plating layer on the inner wall of the corresponding through hole.