Calculation method for aluminum yield and aluminum output of aluminum electrolysis cell

By obtaining the design parameters and health data of the aluminum electrolytic cell, a mathematical model was established, and the aluminum production and output of the aluminum electrolytic cell were calculated, which solved the problem of measurement difficulties in the existing technology and realized the aluminum electrolytic production management Intelligent and digital upgrades.

CN119004848APending Publication Date: 2024-11-22SHENYANG ALUMINIUM MAGNESIUM INSTITUTE
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411233927.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The existing aluminum electrolytic cells have difficulty in measuring aluminum production, low measurement frequency and certain delays and errors in the results, making it difficult to meet the needs of intelligent and digital upgrades.

Method used

By obtaining the electrolytic cell design parameters, cathode type, anode information and health, a mathematical model is established, and the actual aluminum production and aluminum output are calculated to improve the rapid and accurate calculations.

Benefits of technology

It realizes rapid and accurate calculation of aluminum production and aluminum output in aluminum electrolytic cells, and improves the intelligence and digitalization level of electrolytic production management.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119004848A_ABST
    Figure CN119004848A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of aluminum electrolysis, in particular to a method for calculating the aluminum yield and the aluminum output of an aluminum electrolysis cell, and the method for calculating the aluminum yield comprises the following steps: S1, obtaining the design parameters of the electrolysis cell, the furnace wall thickness L and the aluminum level height AL, and calculating to obtain the theoretical aluminum yield M0; s2, the cathode type, the anode information and the cell electrolysis life D of the electrolytic cell are obtained, and the erosion pit volume V1 and the erosion correction aluminum amount M1 are obtained through calculation; s3, the health degree condition of the electrolytic cell is obtained, and the precipitation correction aluminum amount M2 is obtained according to the health degree condition; and S4, calculating according to the formula M = M0 + M1 + M2 to obtain the actual in-process aluminum yield M. The actual aluminum discharge amount can be obtained by calculating the in-process aluminum production amount according to the aluminum level height before and after aluminum discharge. A mathematical model is formed by designing a calculation method for data such as electrolytic cell design parameters, the aluminum production amount and the aluminum output amount can be rapidly and accurately calculated, and the intelligent and digital level of electrolytic production management is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of aluminum electrolysis, and in particular to a method for calculating the aluminum production and output of an aluminum electrolysis cell. Background Art

[0002] The aluminum production of an aluminum reduction cell refers to the amount of liquid aluminum contained in the aluminum reduction cell during the production process. It is one of the most critical production process parameters in the production management of aluminum reduction cells and is directly related to the thermal balance management and magnetic fluid stability management of aluminum reduction cells. However, the current aluminum electrolysis production still does not pay enough attention to the parameter of aluminum production, mainly because it is difficult to measure.

[0003] At present, in the measurement of aluminum production, domestic and foreign electrolytic enterprises often use the time-consuming and labor-intensive inert metal inventory method, which has a very low measurement frequency and the results have certain delays and errors. With the increasing demand for intelligent and digital upgrades in my country's aluminum electrolysis industry in recent years, there is an urgent need for a method to quickly and accurately obtain the aluminum production of the electrolytic cell and introduce this parameter into the daily management of electrolytic production. Summary of the invention

[0004] In view of the above-mentioned shortcomings and deficiencies of the prior art, the present invention provides a method for calculating the aluminum production and output of an aluminum electrolytic cell. By designing a calculation method for data such as electrolytic cell design parameters, a mathematical model is formed, which can quickly and accurately calculate the aluminum production and output, thereby improving the intelligence and digitization level of electrolytic production management.

[0005] In order to achieve the above object, the main technical solutions adopted by the present invention include:

[0006] A method for calculating the aluminum production of an aluminum reduction cell comprises the following steps:

[0007] S1, obtain the design parameters of the electrolytic cell, the thickness of the furnace wall L and the aluminum level AL, and calculate the theoretical aluminum production M0 in the electrolytic cell;

[0008] S2, obtaining the cathode type, anode information and electrolytic life D of the electrolytic cell, and calculating the erosion pit volume V1 and the erosion corrected aluminum amount M1;

[0009] S3, obtaining the health status of the electrolytic cell, and obtaining the precipitated corrected aluminum amount M2 according to the health status;

[0010] S4. Calculate the actual aluminum production M by the following formula:

[0011] M=M0+M1+M2.

[0012] Furthermore, the step S1 includes the following steps:

[0013] S11, obtaining electrolytic cell design parameters including furnace width x, furnace length y and furnace height z, the furnace length y is a function of the furnace height z, i.e., y=f(z), the furnace width x is a function of the furnace height z, i.e., x=g(z);

[0014] S12, obtain the furnace thickness L and the aluminum level AL. The furnace of the electrolytic cell is an inverted frustum structure. The furnace volume V0 of the electrolytic cell is calculated by the following formula:

[0015]

[0016] S13. The theoretical aluminum production M0 is calculated by the following formula:

[0017] M0=V0×ρ

[0018] Here, ρ is the density of liquid aluminum.

[0019] Furthermore, the step S2 comprises the following steps:

[0020] S21, obtaining the cathode type of the electrolytic cell, and obtaining the erosion rate R corresponding to the cathode type;

[0021] S22, obtaining anode information and cell electrolysis life D, wherein the anode information includes anode length L A , anode width W A 、Number of anodes No A ;

[0022] S23. Calculate the erosion pit volume V1 using the following formula:

[0023] V1=L A ×W A ×No A ×R×D

[0024] S24. Calculate the erosion correction aluminum amount M1 using the following formula:

[0025] M1=V1×ρ

[0026] Here, ρ is the density of liquid aluminum.

[0027] Furthermore, step S3 includes the following steps:

[0028] Obtain the health S of the electrolytic cell, and determine the precipitated corrected aluminum amount M2 = h(S) according to the health S of the electrolytic cell; h(S) is a piecewise function, when 90≤S<100, h(S)=-1.5 tons; when 80≤S<90, h(S)=-2.0 tons; when 70≤S<80, h(S)=-2.5 tons; when 60≤S<70, h(S)=-3.0 tons; when S<60, h(S)=-3.5 tons.

[0029] A method for calculating the aluminum output of an aluminum reduction cell adopts the method for calculating the aluminum output of an aluminum reduction cell, comprising step S5, wherein the step S5 is to respectively obtain the aluminum level before and after the aluminum output, and calculate the actual aluminum output m of the electrolytic cell.

[0030] Furthermore, the step S5 comprises the following steps:

[0031] S51, obtain the aluminum level AL before aluminum output B , the aluminum level AL before aluminum discharge B As the aluminum level AL in step S1, the actual aluminum production M is calculated according to steps S1-S4, and the actual aluminum production M is used as the aluminum production M before aluminum tapping. B ;

[0032] S52, obtain the aluminum level AL after aluminum is discharged A , the aluminum level AL after aluminum is discharged A As the aluminum level AL in step S1, the actual aluminum production M is calculated according to steps S1-S4, and the actual aluminum production M is used as the aluminum production M after aluminum is tapped. A ;

[0033] S53, according to the aluminum production before and after aluminum discharge, the actual aluminum discharge amount m is calculated by the following formula;

[0034] m=M B -M A .

[0035] The beneficial effects of the present invention are:

[0036] The present invention provides a method for calculating the aluminum production and output of an aluminum electrolytic cell. By designing a calculation method for data such as electrolytic cell design parameters, a mathematical model is formed, which can quickly and accurately calculate the aluminum production and output. The calculation parameters and the obtained data can be introduced into the daily management of electrolytic production, thereby improving the intelligence and digitization level of electrolytic production management. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Figure 1 The present invention is a flow chart of a method for calculating the aluminum production of an aluminum electrolytic cell. DETAILED DESCRIPTION

[0038] In order to better explain the present invention and facilitate understanding, the present invention is described in detail below through specific implementation modes in conjunction with the accompanying drawings.

[0039] like Figure 1 As shown, a method for calculating the aluminum production of an aluminum reduction cell comprises the following steps:

[0040] S1, obtain the design parameters of the electrolytic cell, the thickness of the furnace wall L and the aluminum level AL, and calculate the theoretical aluminum production M0 in the electrolytic cell;

[0041] S2, obtaining the cathode type, anode information and electrolytic life D of the electrolytic cell, and calculating the erosion pit volume V1 and the erosion corrected aluminum amount M1;

[0042] S3, obtaining the health status of the electrolytic cell, and obtaining the precipitated corrected aluminum amount M2 according to the health status;

[0043] S4. Calculate the actual aluminum production M by the following formula:

[0044] M=M0+M1+M2.

[0045] Specifically, the step S1 includes the following steps:

[0046] S11, obtaining electrolytic cell design parameters including furnace width x, furnace length y and furnace height z, the furnace length y is a function of the furnace height z, i.e., y=f(z), the furnace width x is a function of the furnace height z, i.e., x=g(z);

[0047] S12, obtain the furnace thickness L and the aluminum level AL. The furnace of the electrolytic cell is an inverted frustum structure. The furnace volume V0 of the electrolytic cell is calculated by the following formula:

[0048]

[0049] S13. The theoretical aluminum production M0 is calculated by the following formula:

[0050] M0=V0×ρ

[0051] Here, ρ is the density of liquid aluminum.

[0052] Specifically, step S2 includes the following steps:

[0053] S21, obtaining the cathode type of the electrolytic cell, and obtaining the erosion rate R corresponding to the cathode type;

[0054] S22, obtaining anode information and cell electrolysis life D, wherein the anode information includes anode length L A , anode width W A 、Number of anodes No A ;

[0055] S23. Calculate the erosion pit volume V1 using the following formula:

[0056] V1=L A ×W A ×No A ×R×D

[0057] S24. Calculate the erosion correction aluminum amount M1 by the following formula:

[0058] M1=V1×ρ

[0059] Here, ρ is the density of liquid aluminum.

[0060] Specifically, step S3 includes the following steps:

[0061] Obtain the health S of the electrolytic cell, and determine the amount of precipitated corrected aluminum M2=h(S) according to the health S of the electrolytic cell;

[0062] h(S) is a piecewise function:

[0063] When 90≤S<100, h(S)=-1.5 tons;

[0064] When 80≤S<90, h(S)=-2.0 tons;

[0065] When 70≤S<80, h(S)=-2.5 tons;

[0066] When 60≤S<70, h(S)=-3.0 tons;

[0067] When S<60, h(S)=-3.5 tons.

[0068] The health degree calculation method may adopt the online digital electrolytic cell health degree evaluation calculation method provided in Chinese Patent Publication No. CN110093632A.

[0069] A method for calculating the aluminum output of an aluminum reduction cell adopts the method for calculating the aluminum output of an aluminum reduction cell, comprising step S5, wherein the step S5 is to respectively obtain the aluminum level before and after the aluminum output, and calculate the actual aluminum output m of the electrolytic cell.

[0070] Specifically, step S5 includes the following steps:

[0071] S51, obtain the aluminum level AL before aluminum output B , the aluminum level AL before aluminum discharge B As the aluminum level AL in step S1, the actual aluminum production M is calculated according to steps S1-S4, and the actual aluminum production M is used as the aluminum production M before aluminum tapping. B ;

[0072] S52, obtain the aluminum level AL after aluminum is discharged A , the aluminum level AL after aluminum is discharged A As the aluminum level AL in step S1, the actual aluminum production M is calculated according to steps S1-S4, and the actual aluminum production M is used as the aluminum production M after aluminum is tapped. A ;

[0073] S53, according to the aluminum production before and after aluminum discharge, the actual aluminum discharge amount m is calculated by the following formula;

[0074] m=M B -M A .

[0075] The following will illustrate embodiments according to specific circumstances, and it should be understood that the present invention can be implemented in various forms and should not be limited by the embodiments described herein. On the contrary, the embodiments are provided to enable a clearer and more thorough understanding of the present invention and to fully convey the scope of the present invention to those skilled in the art.

[0076] Example 1

[0077] In this embodiment, the aluminum electrolytic cell is a 500kA electrolytic cell, and the corresponding furnace design parameters are obtained. The furnace wall thickness L is manually measured to be 0.15 meters, and the aluminum level AL is measured to be 0.265 meters. The aluminum level is measured using a device and method for measuring process parameters of molten salt electrolysis equipment disclosed in Chinese Patent Publication No. CN115786993A. The above data are substituted into steps S11-S12 to obtain the furnace volume V0, and the density ρ of liquid aluminum is 2300kg / m 3 , and then substitute the above data into step S13, and calculate that the theoretical aluminum production M0 in the electrolytic cell is 43.65 tons.

[0078] In this embodiment, the cathode type is a graphitized cathode. The erosion rate of the graphitized cathode is 2-3 cm / year. Taking the median, the erosion rate R is 2.5 cm / year. The anode length L is measured. A is 1.66m, anode width W A 0.65m, number of anodes No A is 48. In this embodiment, the life of the electrolytic cell is 314 days, i.e., 0.86 years. Substituting the above data into steps S21-S23, the erosion pit volume V1 is obtained. The density ρ of liquid aluminum is 2300 kg / m 3 , and then substitute the above data into step S24, and calculate that the erosion corrected aluminum amount M1 is 3.15 tons.

[0079] In this embodiment, the health S of the electrolytic cell of this embodiment is calculated to be 92 points according to the online digital electrolytic cell health evaluation calculation method provided in Chinese Patent Publication No. CN110093632A, and the precipitated corrected aluminum amount M2 is -1.5 tons when substituted into the piecewise function h(S);

[0080] Substituting the theoretical aluminum production M0, the erosion-corrected aluminum production M1 and the precipitation-corrected aluminum production M2 into step S4, the actual aluminum production M is calculated to be 45.30 tons.

[0081] In this embodiment, the aluminum level AL before the aluminum is automatically measured B = 0.265m, after steps S51 and S1-S4, the aluminum production M is calculated. B = 45.30 tons; Automatically measured aluminum level AL after aluminum is discharged A =0.241m, after calculating the aluminum through steps S52 and S1-S4, the aluminum production M A =41.58 tons. Substituting the above data into step S53, the actual aluminum output m is calculated to be 3.72 tons.

[0082] Although the embodiments of the present invention have been shown and described above, it is to be understood that the above embodiments are exemplary and are not to be construed as limitations of the present invention. A person skilled in the art may alter, modify, replace and modify the above embodiments within the scope of the present invention.

Claims

1. A method for calculating the aluminum production of an aluminum reduction cell, characterized in that: The following steps are involved: S1, obtain the design parameters of the electrolytic cell, the thickness of the furnace wall L and the aluminum level AL, and calculate the theoretical aluminum production M0 in the electrolytic cell; S2, obtaining the cathode type, anode information and electrolytic life D of the electrolytic cell, and calculating the erosion pit volume V1 and the erosion corrected aluminum amount M1; S3, obtaining the health status of the electrolytic cell, and obtaining the precipitated corrected aluminum amount M2 according to the health status; S4. Calculate the actual aluminum production M by the following formula: M=M0+M1+M2.

2. A method for calculating the aluminum production of an aluminum reduction cell according to claim 1, characterized in that: The step S1 comprises the following steps: S11, obtaining electrolytic cell design parameters including furnace width x, furnace length y and furnace height z, the furnace length y is a function of the furnace height z, i.e., y=f(z), the furnace width x is a function of the furnace height z, i.e., x=g(z); S12, obtain the furnace thickness L and the aluminum level AL. The furnace of the electrolytic cell is an inverted frustum structure. The furnace volume V0 of the electrolytic cell is calculated by the following formula: S13. The theoretical aluminum production M0 is calculated by the following formula: M0=V0×ρ Here, ρ is the density of liquid aluminum.

3. The method for calculating the aluminum production of an aluminum reduction cell according to claim 1, characterized in that: The step S2 comprises the following steps: S21, obtaining the cathode type of the electrolytic cell, and obtaining the erosion rate R corresponding to the cathode type; S22, obtaining anode information and cell electrolysis life D, wherein the anode information includes anode length L A , anode width W A 、Number of anodes No A ; S23. Calculate the erosion pit volume V1 using the following formula: V1=L A ×W A ×No A ×R×D S24. Calculate the erosion correction aluminum amount M1 by the following formula: M1=V1×ρ Here, ρ is the density of liquid aluminum.

4. The method for calculating the aluminum production of an aluminum reduction cell according to claim 1, characterized in that: The step S3 comprises the following steps: Obtain the health S of the electrolytic cell, and determine the precipitated corrected aluminum amount M2 = h(S) according to the health S of the electrolytic cell; h(S) is a piecewise function, when 90≤S<100, h(S)=-1.5 tons; when 80≤S<90, h(S)=-2.0 tons; when 70≤S<80, h(S)=-2.5 tons; when 60≤S<70, h(S)=-3.0 tons; when S<60, h(S)=-3.5 tons.

5. A method for calculating the aluminum output of an aluminum reduction cell, using the method for calculating the aluminum output of an aluminum reduction cell as claimed in any one of claims 1 to 4, characterized in that: The method comprises step S5, wherein the step S5 is to respectively obtain the aluminum level before and after aluminum discharge, and calculate the actual aluminum discharge amount m of the electrolytic cell.

6. A method for calculating the amount of aluminum produced by an aluminum reduction cell as claimed in claim 5, characterized in that: The step S5 comprises the following steps: S51, obtain the aluminum level AL before aluminum output B , the aluminum level AL before aluminum discharge B As the aluminum level AL in step S1, the actual aluminum production M is calculated according to steps S1-S4, and the actual aluminum production M is used as the aluminum production M before aluminum tapping. B ; S52, obtain the aluminum level AL after aluminum is discharged A , the aluminum level AL after aluminum is discharged A As the aluminum level AL in step S1, the actual aluminum production M is calculated according to steps S1-S4, and the actual aluminum production M is used as the aluminum production M after aluminum is tapped. A ; S53, according to the aluminum production before and after aluminum discharge, the actual aluminum discharge amount m is calculated by the following formula; m=M B -M A 。