Method for improving excessive accumulation of carbon-containing polymer in etching warm-up process

By generating and breaking silicon-hydrogen bonds in the etching chamber, the problem of excessive accumulation of carbon-containing polymers was solved, thereby improving the stability of the etching chamber and the quality of the products.

CN119008372APending Publication Date: 2024-11-22CHONGQING XINLIAN MICROELECTRONICS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411090731.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-09
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

During the warm-up process of semiconductor etching, carbon-containing polymers can easily accumulate in excess, leading to instability on the surface of the upper electrode, affecting product quality and potentially causing defects.

Method used

A carbon-hydrogen-fluorine gas is introduced into the etching chamber to generate a film containing silicon-hydrogen bonds. The silicon-hydrogen bonds are broken by introducing carbon tetrafluoride gas to generate volatile hydrogen fluoride and hydrofluorocarbons, thereby controlling the carbon content of the film.

Benefits of technology

This process enables a long-lasting warm-up process, stabilizes etching chamber conditions, reduces the accumulation of carbon-containing polymers, and improves product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008372A_ABST
    Figure CN119008372A_ABST
Patent Text Reader

Abstract

According to the method for improving excessive accumulation of the carbon-containing polymer in the etching warm-up process, a stable condition can be formed for the etching cavity by introducing the hydrocarbon and fluorine gas into the etching cavity, and the hydrocarbon and fluorine gas easily generates a steady-state film layer containing silicon-hydrogen bonds for the upper electrode, so that the stability of the etching cavity is facilitated, and the yield of the etching cavity is improved. And after carbon tetrafluoride gas is introduced into the etching cavity, fluorine ions with strong oxidizing ability can be provided through the carbon tetrafluoride gas to capture hydrogen ions in the film layer, so that silicon-hydrogen bonds are broken to form volatile hydrogen fluoride and / or generate hydrofluorocarbon compounds, the film layer on the surface of the upper electrode can be regulated and controlled, and the performance of the device is improved. The long-acting warming-up process is achieved, the problem that carbon-containing polymers with long carbon chains are accumulated on the surface of the upper electrode is solved, and the product quality is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of semiconductor manufacturing, and relates to a method for improving excessive accumulation of carbon-containing polymers in an etching warm-up process. Background Art

[0002] In the production process of semiconductor etching technology, a warm-up (Seasoning) step is generally required before etching the wafer, especially for a brand new etching chamber that has never been used, an etching chamber that has undergone periodic maintenance (PM), and an etching chamber that has been idle for too long. The warm-up step refers to placing a warm-up wafer (i.e. a wafer with a layer of silicon dioxide film or bare silicon on the surface) in the etching chamber, etching the warm-up wafer, and making the etching reaction product cover the entire inner wall of the etching chamber, so that the etching chamber reaches the working state required by the etching process, thereby improving the etching rate stability and wafer-to-wafer uniformity of the etching chamber.

[0003] In existing semiconductor etching equipment, the upper electrode is a crucial component. The upper electrode has multiple air inlet holes inside. The reaction gas is redistributed and introduced through the air inlet holes of the upper electrode, and the reaction gas forms plasma in the etching chamber through a radio frequency power supply. The plasma is used to etch the wafer adsorbed on the lower electrode to pattern the wafer. The upper electrode can control the range and uniformity of the plasma, so that the etching rates in the middle and edge of the wafer are the same, so as to prepare high-quality products.

[0004] In the conventional warm-up process, a gas containing carbon dioxide and fluorine (CHF) is usually used as a reaction gas. That is, the CHF gas is dissociated to allow H ions to combine with the upper electrode containing silicon (Si) to form silicon hydrogen (Si) on the surface of the upper electrode. x H y ) film layer, so that the upper electrode is not easy to directly absorb the products in the etching process, so as to facilitate the dynamic stability of the upper electrode surface, and then stabilize the production status of the etching chamber, so that the subsequent product wafers can be etched under appropriate production conditions to ensure product quality. However, the silicon hydrogen film layer is easy to absorb carbon-containing products, and then accumulate into carbon-containing polymers with long carbon chains. When the accumulation of the polymer reaches a certain amount, the polymer is easy to fall off during the production process, causing defects.

[0005] Therefore, it is necessary to provide a method for improving the excessive accumulation of carbon-containing polymers during the etching warm-up process. Summary of the invention

[0006] In view of the above-mentioned shortcomings of the prior art, an object of the present invention is to provide a method for improving the excessive accumulation of carbon-containing polymers in the etching warm-up process, so as to solve the problem of accumulation of carbon-containing polymers in the etching warm-up process in the prior art.

[0007] To achieve the above-mentioned object and other related objects, the present invention provides a method for improving the excessive accumulation of carbon-containing polymers in the etching warm-up process, comprising the following steps:

[0008] Introducing a carbon, hydrogen and fluorine gas into the etching chamber, and the carbon, hydrogen and fluorine gas combines with the silicon-containing upper electrode to form a film layer containing silicon-hydrogen bonds on the surface of the upper electrode;

[0009] Carbon tetrafluoride gas is introduced into the etching chamber, and the carbon tetrafluoride gas combines with the film layer to break the silicon-hydrogen bonds in the film layer.

[0010] Optionally, the film layer includes one or a combination of a silicon hydrogen film layer and a silicon hydrogen carbon film layer containing silicon-hydrogen-carbon bonds.

[0011] Optionally, when the film layer is the silicon hydrogen film layer, the carbon tetrafluoride gas combines with the silicon hydrogen film layer to generate hydrogen fluoride gas; when the film layer is the silicon hydrogen carbon film layer, the carbon tetrafluoride gas combines with the silicon hydrogen carbon film layer to generate hydrofluorocarbon compounds.

[0012] Optionally, the upper electrode comprises a silicon upper electrode or a quartz upper electrode.

[0013] Optionally, the hydrocarbon-fluorine gas includes CH 2 F 2 Gas and CHF 3 One or a combination of gases.

[0014] Optionally, the process conditions for introducing the carbon tetrafluoride gas into the etching chamber to break the silicon-hydrogen bond include: chamber pressure of 80-100 mT, RF power of 500-700 W, flow rate of the carbon tetrafluoride gas of 200-400 sccm, and etching time of 80-120 s.

[0015] Optionally, before the carbon-hydrogen-fluorine gas is introduced into the etching chamber for the warm-up process, a step of dry cleaning the etching chamber is also included; the cleaning gas used for the dry cleaning includes one or a combination of oxygen and carbon tetrafluoride gas.

[0016] Optionally, after the carbon tetrafluoride gas is introduced into the etching chamber for a warm-up process, a step of inertly purging the etching chamber is further included; the inert gas used for the inert purification includes argon.

[0017] Optionally, the steps are repeated N times, where N≥1.

[0018] Optionally, the method is applicable to a single-frequency plasma etcher or a multi-frequency plasma etcher.

[0019] As described above, the method for improving the excessive accumulation of carbon-containing polymers in the etching warm-up process of the present invention forms a stable condition for the etching chamber by introducing hydrocarbon fluorine gas into the etching chamber. The hydrocarbon fluorine gas can easily generate a stable film layer containing silicon-hydrogen bonds on the upper electrode, which is beneficial to the stability of the etching chamber. After carbon tetrafluoride gas is introduced into the etching chamber, fluorine ions with strong oxidizing ability can be provided by the carbon tetrafluoride gas to capture hydrogen ions in the film layer, so that the silicon-hydrogen bonds are broken to form volatile hydrogen fluoride and / or generate hydrofluorocarbon compounds, so that the film layer on the surface of the upper electrode can be regulated, a long-term warm-up process can be realized, the problem of accumulation of long carbon chain carbon-containing polymers on the surface of the upper electrode can be improved, and product quality can be improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 The process flow chart of the method for improving the excessive accumulation of carbon-containing polymers in the etching warm-up process of the present invention is shown.

[0021] Figure 2 to Figure 5 A schematic diagram showing the mechanism of each step in the warm-up process of the present invention. DETAILED DESCRIPTION

[0022] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0023] For example, when describing the embodiments of the present invention in detail, for the sake of convenience, the cross-sectional view showing the device structure will not be partially enlarged according to the general scale, and the schematic view is only an example, which should not limit the scope of protection of the present invention. In addition, in actual production, the three-dimensional space dimensions of length, width and depth should be included.

[0024] For ease of description, spatial relational terms such as “under”, “below”, “below”, “below”, “over”, etc. may be used herein to describe the relationship of one element or feature shown in the drawings to other elements or features. It will be understood that these spatial relational terms are intended to include other orientations of the device in use or operation in addition to the orientation depicted in the drawings, and may include embodiments in which the first and second features are formed in direct contact, and may also include embodiments in which additional features are formed between the first and second features, so that the first and second features may not be in direct contact. In addition, when a layer is referred to as being “between” two layers, it may be the only layer between the two layers, or one or more intervening layers may also be present.

[0025] It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner, and therefore the illustrations only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.

[0026] like Figure 1 The present embodiment provides a method for improving the excessive accumulation of carbon-containing polymers in the etching warm-up process. By introducing a hydrocarbon-hydrogen-fluorine body into the etching chamber, a stable condition can be formed for the etching chamber. The hydrocarbon-hydrogen-fluorine gas can easily generate a stable film layer containing silicon-hydrogen bonds on the upper electrode, which is beneficial to the stability of the etching chamber. After the carbon tetrafluoride gas is introduced into the etching chamber, the carbon tetrafluoride gas can provide fluorine ions with strong oxidizing ability to capture hydrogen ions in the film layer, so that the silicon-hydrogen bonds are broken to form volatile hydrogen fluoride and / or generate hydrofluorocarbon compounds, so that the film layer on the surface of the upper electrode can be regulated, a long-term warm-up process can be realized, the problem of accumulation of long carbon chain carbon-containing polymers on the surface of the upper electrode is improved, and product quality is improved.

[0027] Among them, the method for improving the excessive accumulation of carbon-containing polymers in the etching warm-up process at least includes the following steps:

[0028] S1: introducing a carbon, hydrogen, and fluorine gas into the etching chamber, and the carbon, hydrogen, and fluorine gas is combined with the silicon-containing upper electrode to form a film layer containing silicon-hydrogen bonds on the surface of the upper electrode;

[0029] S2: introducing carbon tetrafluoride gas into the etching chamber, wherein the carbon tetrafluoride gas combines with the film layer to break the silicon-hydrogen bonds in the film layer.

[0030] Specifically, in the semiconductor etching process, before etching the wafer, a warm-up process is required to ensure the quality of the wafer. Figure 2During the warm-up process, when the carbon hydrogen fluorine (CHF) gas is introduced into the etching chamber, the carbon hydrogen fluorine gas will dissociate and provide hydrogen (H) ions, and the H ions will combine with the upper electrode 100 containing silicon (Si) to form a silicon hydrogen (SixHy) film layer containing silicon-hydrogen bonds on the surface of the upper electrode 100. The silicon hydrogen film layer can make it difficult for the upper electrode 100 to directly absorb the product in the etching process, so that the silicon hydrogen film layer has a protective effect on the surface of the upper electrode 100, and further stabilize the production status of the etching chamber, so that the subsequent product wafers can be etched under suitable production conditions to ensure product quality.

[0031] The upper electrode 100 containing silicon may include a silicon upper electrode or a quartz upper electrode, which is not excessively limited here. In this embodiment, the upper electrode is only an example of a silicon upper electrode, but as required, the upper electrode 100 may also be a quartz upper electrode containing silicon.

[0032] However, see Figure 3 However, the silicon hydrogen film layer attached to the surface of the upper electrode 100 is prone to absorb carbon (C)-containing products (such as the photoresist located on the surface of the wafer can produce carbon-containing products after being etched in the etching chamber, etc.), generating a silicon hydrogen carbon film layer containing silicon-hydrogen-carbon (Si-HC) bonds, and as time goes by, the carbon-containing products adsorbed by the silicon hydrogen film layer will accumulate, thereby generating a carbon-containing polymer with a long carbon chain attached to the surface of the upper electrode 100, and when the accumulation of the carbon-containing polymer reaches a certain amount, the carbon-containing polymer is likely to fall off during the production process, causing defects.

[0033] Therefore, the staff needs to clean the carbon-containing polymer on the surface of the upper electrode 100 regularly, which will undoubtedly cause loss of manpower and production failure, and it is difficult to achieve a long-term and effective warm-up process.

[0034] See also Figure 4 and Figure 5 In this embodiment, after executing the above step S1, step S2 is executed, that is, carbon tetrafluoride (CF 4 ) gas, the carbon tetrafluoride gas will dissociate and provide fluorine (F) ions, the F ions have strong oxidizing properties and can snatch H ions in the film layer located on the surface of the upper electrode 100, so that the silicon-hydrogen bonds in the film layer are broken. For example, the F ions can combine with the silicon hydrogen film layer to break the silicon-hydrogen bonds and generate hydrogen fluoride (HF) gas, thereby regulating the content of the silicon hydrogen film layer located on the surface of the upper electrode 100, reducing the amount of carbon-containing products adsorbed by the silicon hydrogen film layer, thereby alleviating or avoiding the problem of excessive accumulation of the carbon-containing polymer.

[0035] Similarly, see Figure 4 and Figure 5 When the silicon hydrogen film layer adsorbs a certain amount of carbon-containing products, the F ions provided by the carbon tetrafluoride gas can also snatch the H ions in the silicon hydrogen carbon film layer containing silicon-hydrogen-carbon bonds located on the surface of the upper electrode 100, so that the silicon-hydrogen-carbon bonds in the silicon hydrogen carbon film layer are broken from the silicon-hydrogen bonds, thereby removing the carbon-containing substances bound by the silicon-hydrogen bonds, thereby alleviating or avoiding the problem of excessive accumulation of the carbon-containing polymers.

[0036] Therefore, after the process of step S1 and step S2, the amount of the carbon-containing polymer located on the surface of the upper electrode 100 can be controlled, thereby realizing a long-lasting warm-up process, improving the problem of accumulation of the carbon-containing polymer on the surface of the upper electrode 100, and improving product quality.

[0037] As an example, the process conditions when the carbon tetrafluoride gas is introduced into the etching chamber to break the silicon-hydrogen bond may include: the chamber pressure is 80-100mT, such as 80mT, 90mT, 100mT, etc., the high-frequency power is 500-700W, such as 500W, 600W, 700W, etc., the low-frequency power is 500-700W, such as 500W, 600W, 700W, etc., the flow rate of the carbon tetrafluoride gas is 200-400sccm, such as 200sccm, 300sccm, 400sccm, etc., and the etching time is 80-120s, such as 80s, 100s, 120s, etc.

[0038] As an example, the hydrocarbon-fluorine gas in step S1 may include CH 2 F 2 Gas and CHF 3 One or a combination of gases can be selected according to needs.

[0039] Further, as required, the above step S1 and step S2 may be repeated N times, wherein N≥1, such as N is 1, 2, 3, etc., and the value of N may be selected as required.

[0040] Furthermore, before the hydrocarbon-fluorine gas is introduced into the etching chamber for the warm-up process, that is, before executing step S1, a step of dry cleaning the etching chamber may be included; wherein the cleaning gas used for the dry cleaning may include one or a combination of oxygen and carbon tetrafluoride gas, but is not limited to this.

[0041] Furthermore, after the carbon tetrafluoride gas is introduced into the etching chamber for a warm-up process, that is, after executing step S2, a step of inert purification of the etching chamber may be included; wherein the inert gas used for the inert purification may include argon (Ar), but is not limited to this.

[0042] The method provided in the present application for improving the excessive accumulation of carbon-containing polymers in the etching warm-up process can be applicable to single-frequency plasma etcher or multi-frequency plasma etcher. The specific type of the single-frequency plasma etcher or the multi-frequency plasma etcher is not limited here.

[0043] In this embodiment, only a multi-frequency plasma etcher is used as an example, but the type of etcher is not limited thereto. Referring to the following table, a specific process condition for improving the excessive accumulation of carbon-containing polymers in the etching warm-up process is provided:

[0044] The data ranges in the above table can be adaptively selected within the range including the endpoints as required, and no excessive restrictions are imposed here.

[0045] The process gas selected in the dry cleaning process and the inert purification process is not limited thereto and can be selected according to specific needs. For example, the inert gas is not limited to argon but can also be other inert gases.

[0046] In summary, the method for improving the excessive accumulation of carbon-containing polymers in the etching warm-up process of the present invention can form a stable condition for the etching chamber by introducing hydrocarbon fluorine gas into the etching chamber. The hydrocarbon fluorine gas can easily generate a stable film layer containing silicon-hydrogen bonds on the upper electrode, which is beneficial to the stability of the etching chamber. After carbon tetrafluoride gas is introduced into the etching chamber, fluoride ions with strong oxidizing ability can be provided by the carbon tetrafluoride gas to capture hydrogen ions in the film layer, so that the silicon-hydrogen bonds are broken to form volatile hydrogen fluoride and / or generate hydrofluorocarbon compounds, so that the film layer on the surface of the upper electrode can be regulated, a long-term warm-up process can be realized, the problem of accumulation of long carbon chain carbon-containing polymers on the surface of the upper electrode can be improved, and product quality can be improved.

[0047] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A method for improving the excessive accumulation of carbon-containing polymers in the etching warm-up process, characterized in that: The following steps are involved: Introducing a carbon, hydrogen and fluorine gas into the etching chamber, and the carbon, hydrogen and fluorine gas combines with the silicon-containing upper electrode to form a film layer containing silicon-hydrogen bonds on the surface of the upper electrode; Carbon tetrafluoride gas is introduced into the etching chamber, and the carbon tetrafluoride gas combines with the film layer to break the silicon-hydrogen bonds in the film layer.

2. The method for improving excessive accumulation of carbon-containing polymers in an etching warm-up process according to claim 1, characterized in that: The film layer includes one or a combination of a silicon hydrogen film layer and a silicon hydrogen carbon film layer containing silicon-hydrogen-carbon bonds.

3. The method for improving excessive accumulation of carbon-containing polymers in an etching warm-up process according to claim 2, characterized in that: When the film layer is the silicon hydrogen film layer, the carbon tetrafluoride gas combines with the silicon hydrogen film layer to generate hydrogen fluoride gas; when the film layer is the silicon hydrogen carbon film layer, the carbon tetrafluoride gas combines with the silicon hydrogen carbon film layer to generate hydrofluorocarbon compounds.

4. The method for improving excessive accumulation of carbon-containing polymers in an etching warm-up process according to claim 1, characterized in that: The upper electrode includes a silicon upper electrode or a quartz upper electrode.

5. The method for improving excessive accumulation of carbon-containing polymers in an etching warm-up process according to claim 1, characterized in that: The carbon, hydrogen and fluorine gas includes one or a combination of CH2F2 gas and CHF3 gas.

6. The method for improving excessive accumulation of carbon-containing polymers in an etching warm-up process according to claim 1, characterized in that: The process conditions for introducing the carbon tetrafluoride gas into the etching chamber to break the silicon-hydrogen bond include: chamber pressure of 80-100 mT, RF power of 500-700 W, flow rate of the carbon tetrafluoride gas of 200-400 sccm, and etching time of 80-120 s.

7. The method for improving excessive accumulation of carbon-containing polymers in an etching warm-up process according to claim 1, characterized in that: Before the carbon, hydrogen and fluorine gas is introduced into the etching chamber for the warm-up process, a step of dry cleaning the etching chamber is also included; the cleaning gas used in the dry cleaning includes one or a combination of oxygen and carbon tetrafluoride gas.

8. The method for improving excessive accumulation of carbon-containing polymers in an etching warm-up process according to claim 1, characterized in that: After the carbon tetrafluoride gas is introduced into the etching chamber for a warm-up process, a step of inert purification of the etching chamber is also included; the inert gas used for the inert purification includes argon.

9. The method for improving excessive accumulation of carbon-containing polymers in an etching warm-up process according to claim 1, characterized in that: Repeat the above steps N times, where N≥1.

10. The method for improving excessive accumulation of carbon-containing polymers in an etching warm-up process according to claim 1, characterized in that: The method is applicable to a single-frequency plasma etcher or a multi-frequency plasma etcher.