Method for etching SiC groove with smooth side wall
Through chemical mechanical polishing processing, ultrasonic cleaning and intelligent process parameter optimization, the accuracy and efficiency problems in traditional SiC trench etching process are solved, and the smoothness of SiC trench sidewalls is improved and the production efficiency is improved, ensuring semiconductors High performance and consistency of devices.
Patent Information
- Application Number
- CN202411091874.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-22
AI Technical Summary
Traditional SiC trench etching processes are difficult to meet the requirements of high precision and high efficiency at the same time, and improper process parameters control leads to an increase in sidewall roughness, affecting device performance, and poor product consistency and stability.
Chemical mechanical polishing treatment, ultrasonic cleaning, automatic pipette and intelligent stirrer configuration etching solution, scanning electron microscope detection and analysis database combined with machine learning algorithms are used to optimize process parameters to achieve the improvement of the smoothness of the etching side wall.
It significantly improves the smoothness and dimensional accuracy of the SiC trench side walls, reduces human errors, improves production efficiency, and ensures high performance and product consistency of semiconductor devices.
Smart Images

Figure CN119008391A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of semiconductor processing, and in particular to a method for etching a SiC groove with smooth sidewalls. Background Art
[0002] In the field of semiconductor and micro-nano processing, SiC (silicon carbide) is a material with excellent physical and chemical properties. Due to its high hardness, high thermal conductivity, high electron saturation rate and radiation resistance, it is widely used in the manufacture of high-voltage, high-frequency, high-temperature and high-reliability devices. However, the high hardness and chemical stability of SiC materials also bring challenges to its processing. In particular, when preparing SiC grooves with smooth sidewalls, traditional processes often find it difficult to meet the requirements of high precision and high efficiency at the same time. Traditional SiC groove etching processes usually include sample preparation, cleaning, etching, surface treatment and final smoothing. Although these steps can prepare SiC grooves that meet the requirements to a certain extent, they still face many problems in practical applications. For example, the sidewall roughness may increase due to improper control of process parameters during the etching process, thereby affecting the performance of the device. At the same time, traditional processes often rely on a large amount of manual operation and empirical judgment, and it is difficult to achieve precise control and standardization of process parameters, resulting in poor product consistency and stability. To this end, we propose a method for etching SiC grooves with smooth sidewalls. Summary of the invention
[0003] The object of the present invention is to provide a method for etching a SiC trench with smooth side walls.
[0004] In order to solve the problems raised in the above background technology, the present invention provides the following technical solution: a method for etching a SiC groove with smooth sidewalls, comprising the following steps:
[0005] Step 1: Sample preparation and pretreatment: prepare high-quality SiC substrate samples with clean surfaces, and perform chemical mechanical polishing on the SiC substrate samples;
[0006] Step 2: Cleaning and drying the sample: Place the pretreated SiC substrate sample in an ultrasonic cleaning tank with a cleaning agent added. After cleaning, place the substrate in a clean oven for drying.
[0007] Step 3: Prepare the etching solution, use an automatic pipette to accurately weigh the required chemical reagents, and use an intelligent stirrer to stir the prepared chemical reagents evenly;
[0008] Step 4: Etching the dried SiC substrate sample;
[0009] Step 5: Surface treatment: removing the photoresist on the surface of the etched SiC substrate sample, and then cleaning and drying again;
[0010] Step 6: Smoothing: using chemical mechanical polishing technology to smooth the SiC substrate sample to further optimize the smoothness of the groove;
[0011] Step 7: Analyze the results: Use a scanning electron microscope to analyze the etching results and establish an analysis database.
[0012] As a further solution of the present invention: in the step 1, the high-quality, surface-cleaned SiC substrate sample is a SiC substrate sample with no obvious defects, cracks or impurities on the surface. The process of chemical mechanical polishing is as follows: using a scanning electron microscope to detect the size and thickness of the SiC substrate, fixing the SiC substrate on a polyurethane polishing pad of a chemical mechanical polisher, using an alumina polishing agent, and controlling the pressure and rotation speed of the polishing head and the flow rate of the polishing liquid according to the results of the scanning electron microscope detection. Under the synergistic effect of mechanical grinding and chemical corrosion, the tiny protrusions and damaged layers on the surface of the substrate are removed. After cleaning, the SiC substrate is taken out from the cleaning tank, rinsed with deionized water to remove the cleaning agent residue, and then the substrate is placed in a pre-cleaned and dried oven, and the drying temperature is set to 100° C. and the drying time is set to 45 minutes.
[0013] As a further solution of the present invention: in the step 2, the sample is cleaned and dried by adding a water-based cleaning agent into an ultrasonic cleaning tank, placing the pretreated SiC substrate into the cleaning tank, starting an ultrasonic generator, and utilizing the cavitation effect of ultrasonic waves in the cleaning liquid to generate tiny bubbles and quickly burst them, thereby generating a strong impact force and microjets to remove the polishing liquid, tiny particles and organic pollutants remaining on the surface of the substrate.
[0014] As a further solution of the present invention: In the step three, the etching solution is configured by using an automatic pipette, setting an accurate aspiration volume, aspirating a corresponding amount of chemical reagent from a reagent bottle, and stirring the configured chemical reagent evenly through an intelligent stirrer. During the stirring process, a pH meter is used to monitor the changes in the physical and chemical properties of the solution in real time.
[0015] As a further solution of the present invention: In the step four, the etching is performed by placing the dried SiC substrate in the reaction chamber of the etcher, ensuring that the substrate is placed stably and can fully contact with the etching gas or solution, and starting the etcher according to pre-set etching parameters, such as temperature, pressure, etching time and flow rate of the gas or solution, so that the etchant reacts chemically with the SiC substrate to gradually form a groove structure.
[0016] As a further solution of the present invention: in the step five, the surface treatment method is to use a photoresist remover to remove the photoresist on the surface of the etched SiC substrate sample, then rinse the substrate with deionized water to remove the residual remover and photoresist fragments, and clean the SiC substrate after removing the photoresist again to remove possible residual chemicals and impurities, and then put the substrate into an oven for drying.
[0017] As a further solution of the present invention: In step six, the smoothing treatment method is to fix the SiC substrate on the polyurethane polishing pad of a chemical mechanical polishing machine, use an aluminum oxide polishing agent, and control the pressure, rotation speed and flow rate of the polishing head according to the results of scanning electron microscopy detection. Under the synergistic effect of mechanical grinding and chemical corrosion, the slight roughness of the groove sidewall and bottom is removed to make the groove surface smoother and flatter.
[0018] As a further solution of the present invention: in the step seven, the method for analyzing the results is to place the smoothed SiC substrate sample into the sample chamber of a scanning electron microscope, perform high-resolution imaging of the grooves formed by etching, and evaluate the etching effect by observing the shape, depth, side wall smoothness and dimensional accuracy parameters of the grooves. At the same time, the obtained images and related data are recorded and organized, and compared with the data in the analysis database to determine the etching effect.
[0019] As a further solution of the present invention: the analysis database of step seven stores the result data of multiple etching experiments, including the shape, depth, side wall smoothness, dimensional accuracy parameters of the groove and the corresponding etching parameters and pretreatment, cleaning and polishing process conditions. A machine learning algorithm is used to deeply mine and analyze the data in the database, and a correlation model between the etching effect and various process parameters is established. Before each etching experiment, the correlation model is used to intelligently predict and optimize the preset etching parameters to predict the etching effect to be achieved. At the same time, a recommended process parameter combination can be provided for the current etching task based on the best practice cases in the historical data.
[0020] By adopting the above technical solution, compared with the prior art, the beneficial effects of the present invention are:
[0021] 1. The present invention constructs a comprehensive etching effect analysis database, and uses a machine learning algorithm to deeply mine and analyze the data in the database, thereby mining the complex relationship and potential rules between the etching effect and the process parameters, thereby realizing the intelligent prediction and optimization of the etching process parameters, improving the accuracy and efficiency of the etching experiment, and reducing the experimental cost and time consumption, providing strong support for the process development in the field of semiconductor devices and micro-nano processing;
[0022] 2. The present invention uses chemical mechanical polishing technology in the smoothing step and combines the detection results of scanning electron microscopy to accurately control the polishing parameters. This high-precision control method significantly improves the sidewall smoothness of the SiC groove, meets the strict requirements of the micro-nano processing field for high-quality groove structures, and provides an important guarantee for the manufacture of high-performance semiconductor devices. At the same time, the setting of ultrasonic cleaning ensures the smoothness and cleanliness of the SiC substrate surface;
[0023] 3. The present invention uses intelligent chemical reagent configuration and etching process parameter settings, combined with real-time monitoring technology, to ensure that each link of the etching process can be carried out under optimal conditions. This high-precision parameter control can significantly improve the side wall smoothness and dimensional accuracy of the groove. At the same time, it effectively reduces human errors and comprehensively improves overall production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 Schematic diagram of the method flow in an embodiment of the present invention. DETAILED DESCRIPTION
[0025] The specific embodiments of the present invention will be further described below in conjunction with the accompanying drawings. It should be noted that the description of these embodiments is used to help understand the present invention, but does not constitute a limitation of the present invention.
[0026] In addition, the technical features involved in the various embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.
[0027] Please see attached Figure 1 The present invention provides a method for etching a SiC groove with smooth sidewalls, comprising the following steps:
[0028] Step 1: Sample preparation and pretreatment: prepare high-quality, surface-cleaned SiC substrate samples, and perform chemical mechanical polishing on the SiC substrate samples;
[0029] Step 2: Cleaning and drying the sample: Place the pretreated SiC substrate sample in an ultrasonic cleaning tank with a cleaning agent added. After cleaning, place the substrate in a clean oven for drying.
[0030] Step 3: Prepare the etching solution, use an automatic pipette to accurately weigh the required chemical reagents, and use an intelligent stirrer to stir the prepared chemical reagents evenly;
[0031] Step 4: Etching the dried SiC substrate sample;
[0032] Step 5: Surface treatment: removing the photoresist on the surface of the etched SiC substrate sample, and then cleaning and drying again;
[0033] Step 6: Smoothing: using chemical mechanical polishing technology to smooth the SiC substrate sample to further optimize the smoothness of the groove;
[0034] Step 7: Analyze the results: Use a scanning electron microscope to analyze the etching results and establish an analysis database.
[0035] In one embodiment of the present invention: in the step 1, the high-quality, surface-cleaned SiC substrate sample is a SiC substrate sample with no obvious defects, cracks or impurities on the surface. The process of chemical mechanical polishing is as follows: using a scanning electron microscope to detect the size and thickness of the SiC substrate, fixing the SiC substrate on a polyurethane polishing pad of a chemical mechanical polisher, using an alumina polishing agent, controlling the pressure and rotation speed of the polishing head and the flow rate of the polishing liquid according to the results of the scanning electron microscope detection, removing the tiny protrusions and damaged layer on the surface of the substrate under the synergistic effect of mechanical grinding and chemical corrosion, and after cleaning, taking out the SiC substrate from the cleaning tank, rinsing it with deionized water to remove the cleaning agent residue, and then placing the substrate in a pre-cleaned and dried oven, setting the drying temperature to 100°C and the drying time to 45 minutes.
[0036] In one embodiment of the present invention: in the step 2, the sample is cleaned and dried by adding a water-based cleaning agent into an ultrasonic cleaning tank, placing the pretreated SiC substrate into the cleaning tank, starting an ultrasonic generator, and utilizing the cavitation effect of ultrasonic waves in the cleaning liquid to generate tiny bubbles and quickly burst them, thereby generating a strong impact force and microjets to remove the polishing liquid, tiny particles and organic pollutants remaining on the surface of the substrate.
[0037] In one embodiment of the present invention: in step three, the etching solution is configured by using an automatic pipette, setting an accurate aspiration volume, aspirating a corresponding amount of chemical reagent from a reagent bottle, and stirring the configured chemical reagent evenly with an intelligent stirrer. During the stirring process, a pH meter is used to monitor the changes in the physical and chemical properties of the solution in real time.
[0038] In one embodiment of the present invention: in the step four, the etching is performed by placing the dried SiC substrate in the reaction chamber of the etcher, ensuring that the substrate is placed stably and can be fully in contact with the etching gas or solution, and starting the etcher according to pre-set etching parameters, such as temperature, pressure, etching time and flow rate of the gas or solution, so that the etchant reacts chemically with the SiC substrate to gradually form a groove structure.
[0039] In one embodiment of the present invention: in the step five, the surface treatment method is to use a photoresist remover to remove the photoresist on the surface of the etched SiC substrate sample, then rinse the substrate with deionized water to remove the residual remover and photoresist fragments, and clean the SiC substrate after removing the photoresist again to remove possible residual chemicals and impurities, and then put the substrate into an oven for drying.
[0040] In one embodiment of the present invention: in step six, the smoothing treatment method is to fix the SiC substrate on the polyurethane polishing pad of a chemical mechanical polishing machine, use an aluminum oxide polishing agent, control the pressure and rotation speed of the polishing head and the flow rate of the polishing liquid according to the results of the scanning electron microscope detection, and remove the slight roughness of the groove sidewall and bottom under the synergistic effect of mechanical grinding and chemical corrosion, so that the groove surface is smoother and flatter.
[0041] In one embodiment of the present invention: in the step seven, the method for analyzing the results is to place the smoothed SiC substrate sample into the sample chamber of a scanning electron microscope, perform high-resolution imaging of the grooves formed by etching, and evaluate the etching effect by observing the shape, depth, side wall smoothness and dimensional accuracy parameters of the grooves. At the same time, the obtained images and related data are recorded and organized, and compared with the data in the analysis database to determine the etching effect.
[0042] In one embodiment of the present invention: the analysis database of step seven stores the result data of multiple etching experiments, including the shape, depth, side wall smoothness, dimensional accuracy parameters of the groove and the corresponding etching parameters and pretreatment, cleaning and polishing process conditions. A machine learning algorithm is used to deeply mine and analyze the data in the database, and a correlation model between the etching effect and various process parameters is established. Before each etching experiment, the association model is used to intelligently predict and optimize the preset etching parameters to predict the etching effect to be achieved. At the same time, a recommended process parameter combination can be provided for the current etching task based on the best practice cases in the historical data.
[0043] Example 1, please refer to the attached Figure 1 We collected the result data of multiple etching experiments, including the shape, depth, sidewall smoothness, dimensional accuracy parameters of the grooves, and the corresponding etching parameters and pretreatment, cleaning, and polishing process conditions. Subsequently, we used machine learning algorithms to deeply mine and analyze the data in the database, and established a correlation model between the etching effect and various process parameters. Before the actual etching experiment, we used this correlation model to intelligently predict and optimize the preset etching parameters to predict the etching effect to be achieved.
[0044] Example 2, please refer to the attached Figure 1The SiC substrate is fixed on the polyurethane polishing pad of the chemical mechanical polisher and polished with an alumina polishing agent. During the polishing process, a scanning electron microscope is used to monitor the surface morphology of the groove sidewall and bottom in real time, and the pressure, rotation speed and flow rate of the polishing liquid are dynamically adjusted according to the detection results. This high-precision control method enables us to effectively remove the tiny roughness of the groove sidewall and bottom without damaging the SiC material, thereby improving the sidewall smoothness.
[0045] Example 3, please refer to the attached Figure 1 , demonstrated how to improve the etching quality and production efficiency of SiC grooves through intelligent chemical reagent configuration and etching process parameter setting. We use an automatic pipette to accurately weigh the required chemical reagents and use an intelligent stirrer to mix the configured chemical reagents evenly. During the etching process, we use a pH meter to monitor the physical and chemical properties of the etching solution and dynamically adjust the etching parameters based on the feedback results. This intelligent control method not only ensures the stability and repeatability of the etching process, but also significantly improves the sidewall smoothness and dimensional accuracy of the groove. At the same time, by reducing human intervention, we effectively reduce the risk of operational errors and further improve the overall production efficiency.
[0046] Specifically, by constructing a comprehensive etching effect analysis database and using machine learning algorithms to deeply mine and analyze the data in the database, the complex relationship and potential rules between etching effects and process parameters are discovered, thereby realizing intelligent prediction and optimization of etching process parameters, improving the accuracy and efficiency of etching experiments, and reducing experimental costs and time consumption, providing strong support for process development in the field of semiconductor devices and micro-nano processing.
[0047] Specifically, by using chemical mechanical polishing technology in the smoothing step and combining the detection results of scanning electron microscopy to accurately control the polishing parameters, this high-precision control method significantly improves the side wall smoothness of the SiC groove, meets the strict requirements of the micro-nano processing field for high-quality groove structures, and provides an important guarantee for the manufacture of high-performance semiconductor devices. At the same time, the ultrasonic cleaning setting ensures the smoothness and cleanliness of the SiC substrate surface.
[0048] Specifically, through intelligent chemical reagent configuration and etching process parameter setting, combined with real-time monitoring technology, every link of the etching process can be carried out under optimal conditions. This high-precision parameter control can significantly improve the side wall smoothness and dimensional accuracy of the groove. At the same time, it effectively reduces human errors and comprehensively improves overall production efficiency.
[0049] Working principle:
[0050] First, the automatic pipette and intelligent stirrer accurately prepare the etching solution, and real-time monitoring technology is used to ensure the stability and accuracy of the etching process. Then, a comprehensive etching effect analysis database and machine learning algorithm are used to intelligently predict and optimize the etching process parameters to improve the accuracy and efficiency of the etching experiment. After etching is completed, the high-precision sidewall smoothness control stage is entered. Chemical mechanical polishing technology and scanning electron microscopy are used to accurately control the polishing parameters and improve the sidewall smoothness of the SiC groove. At this point, the entire workflow is completed.
[0051] The above-mentioned front, back, left, right, top and bottom are all based on the figures in the specification. Figure 1 As a benchmark, according to the person's observation perspective, the side of the device facing the observer is defined as the front, the left side of the observer is defined as the left, and so on.
[0052] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the scope of protection of the present invention.
[0053] It should be noted that the device structure and the drawings of the present invention mainly describe the principle of the present invention. In terms of the technology of the design principle, the settings of the power mechanism, power supply system and control system of the device are not fully described. On the premise that the technical personnel in this field understand the principle of the above invention, the details of the power mechanism, power supply system and control system can be clearly known. The control method of the application document is automatic control through a controller, and the control circuit of the controller can be realized by simple programming by the technical personnel in this field.
[0054] The standard parts used therein can all be purchased from the market and can be customized according to the instructions and drawings. The specific connection methods of each part adopt conventional means such as mature bolts, rivets, welding, etc. in the prior art. The machinery, parts and equipment all adopt conventional models in the prior art, and the structures and principles of the components known to technical personnel in this field can be known by these technical personnel through technical manuals or through conventional experimental methods.
[0055] The above describes in detail the embodiments of the present invention in conjunction with the accompanying drawings, but the present invention is not limited to the described embodiments. For those skilled in the art, various changes, modifications, substitutions and variations are made to these embodiments without departing from the principle and spirit of the present invention, and they still fall within the protection scope of the present invention.
Claims
1. A method for etching a SiC trench with smooth sidewalls, characterized in that: The following steps are involved: Step 1: Sample preparation and pretreatment: prepare high-quality SiC substrate samples with clean surfaces, and perform chemical mechanical polishing on the SiC substrate samples; Step 2: Cleaning and drying the sample: Place the pretreated SiC substrate sample in an ultrasonic cleaning tank with a cleaning agent added. After cleaning, place the substrate in a clean oven for drying. Step 3: Prepare the etching solution, use an automatic pipette to accurately weigh the required chemical reagents, and use an intelligent stirrer to stir the prepared chemical reagents evenly; Step 4: Etching the dried SiC substrate sample; Step 5: Surface treatment: removing the photoresist on the surface of the etched SiC substrate sample, and then cleaning and drying again; Step 6: Smoothing: using chemical mechanical polishing technology to smooth the SiC substrate sample to further optimize the smoothness of the groove; Step 7: Analyze the results: Use a scanning electron microscope to analyze the etching results and establish an analysis database.
2. A method for etching a SiC trench with smooth sidewalls according to claim 1, characterized in that: In the step 1, the high-quality, surface-cleaned SiC substrate sample is a SiC substrate sample with no obvious defects, cracks, and impurities on the surface. The process of chemical mechanical polishing treatment is as follows: using a scanning electron microscope to detect the size and thickness of the SiC substrate, fixing the SiC substrate on a polyurethane polishing pad of a chemical mechanical polisher, using an aluminum oxide polishing agent, and controlling the pressure and rotation speed of the polishing head and the flow rate of the polishing liquid according to the results of the scanning electron microscope detection. Under the synergistic effect of mechanical grinding and chemical corrosion, the tiny protrusions and damaged layers on the surface of the substrate are removed. After cleaning, the SiC substrate is taken out from the cleaning tank, rinsed with deionized water to remove the cleaning agent residue, and then the substrate is placed in a pre-cleaned and dried oven, and the drying temperature is set to 100° C. and the drying time is 45 minutes.
3. A method for etching a SiC trench with smooth sidewalls according to claim 1, characterized in that: In the step 2, the sample is cleaned and dried by adding a water-based cleaning agent into an ultrasonic cleaning tank, placing the pretreated SiC substrate into the cleaning tank, starting an ultrasonic generator, and utilizing the cavitation effect of ultrasonic waves in the cleaning liquid to generate tiny bubbles that quickly burst, thereby generating a strong impact force and microjets to remove the polishing liquid, tiny particles and organic pollutants remaining on the surface of the substrate.
4. A method for etching a SiC trench with smooth sidewalls according to claim 1, characterized in that: In step three, the etching solution is prepared by using an automatic pipette, setting an accurate aspiration volume, aspirating a corresponding amount of chemical reagent from a reagent bottle, and stirring the prepared chemical reagent evenly with an intelligent stirrer. During the stirring process, a pH meter is used to monitor the changes in the physical and chemical properties of the solution in real time.
5. The method for etching a SiC trench with smooth sidewalls according to claim 1, characterized in that: In the step 4, the etching is performed by placing the dried SiC substrate in the reaction chamber of the etcher, ensuring that the substrate is placed stably and can be fully in contact with the etching gas or solution, and starting the etcher according to pre-set etching parameters, such as temperature, pressure, etching time and flow rate of the gas or solution, so that the etchant reacts chemically with the SiC substrate to gradually form a groove structure.
6. A method for etching a SiC trench with smooth sidewalls according to claim 1, characterized in that: In the step 5, the surface treatment method is to use a photoresist remover to remove the photoresist on the surface of the etched SiC substrate sample, then rinse the substrate with deionized water to remove the residual remover and photoresist fragments, and clean the SiC substrate after removing the photoresist again to remove possible residual chemicals and impurities, and then put the substrate into an oven for drying.
7. A method for etching a SiC trench with smooth sidewalls according to claim 1, characterized in that: In the step six, the smoothing treatment method is to fix the SiC substrate on the polyurethane polishing pad of the chemical mechanical polishing machine, use aluminum oxide polishing agent, control the pressure, rotation speed and flow rate of the polishing head according to the results of scanning electron microscope detection, and remove the slight roughness of the groove sidewall and bottom under the synergistic effect of mechanical grinding and chemical corrosion, so that the groove surface is smoother and flatter.
8. The method for etching a SiC trench with smooth sidewalls according to claim 1, characterized in that: In the step seven, the method for result analysis is to place the smoothed SiC substrate sample into the sample chamber of a scanning electron microscope, perform high-resolution imaging of the grooves formed by etching, and evaluate the etching effect by observing the shape, depth, side wall smoothness and dimensional accuracy parameters of the grooves. At the same time, the obtained images and related data are recorded and organized, and compared with the data in the analysis database to determine the etching effect.
9. The method for etching a SiC trench with smooth sidewalls according to claim 1, characterized in that: The analysis database of step seven stores the result data of multiple etching experiments, including the shape, depth, side wall smoothness, dimensional accuracy parameters of the grooves and the corresponding etching parameters and pretreatment, cleaning and polishing process conditions. A machine learning algorithm is used to deeply mine and analyze the data in the database, and a correlation model between the etching effect and various process parameters is established. Before each etching experiment, the correlation model is used to intelligently predict and optimize the preset etching parameters to predict the etching effect to be achieved. At the same time, a recommended process parameter combination can be provided for the current etching task based on the best practice cases in the historical data.
Citation Information
Cited By
Intelligent wafer etching process
CN119786396A
An intelligent wafer etching process
CN119786396B