HEMT device and preparation method thereof

By implanting ions on the back of the stacked structure of the HEMT device to form an isolation layer, the problems of difficulty in forming the isolation layer and damage to the interlayer dielectric layer are solved, the reliability and breakdown resistance of the device are improved, and the process process is simplified.

CN119008407APending Publication Date: 2024-11-22SHANGHAI XINWEI SEMICON CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411301643.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-18
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

During the preparation of HEMT devices, it is difficult to form an isolation layer and is prone to damage the interlayer dielectric layer, resulting in poor device reliability.

Method used

By performing ion implantation on the back of the stacked structure of the semiconductor structure, an isolation layer is formed, which avoids high-energy ions from damaging the interlayer dielectric layer, and thins the substrate or forms trenches when necessary to reduce the depth of ion implantation.

Benefits of technology

The quality of the interlayer dielectric layer is improved, the breakdown resistance of the device is enhanced, the reliability is improved, and the process difficulty of the isolation layer is reduced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008407A_ABST
    Figure CN119008407A_ABST
Patent Text Reader

Abstract

The invention provides an HEMT device and a preparation method thereof, the preparation method of the HEMT device comprises the following steps: a semiconductor structure is provided, the semiconductor structure comprises a laminated structure, a source / drain electrode, a cap layer and a grid electrode electrically connected with the cap layer, the laminated structure comprises a channel layer, a barrier layer and an interlayer dielectric layer which are laminated, the source electrode penetrates through the interlayer dielectric layer and is electrically connected with the barrier layer, the drain electrode penetrates through the interlayer dielectric layer and is electrically connected with the barrier layer, the cap layer is located on the upper surface of the barrier layer between the source electrode and the drain electrode, the interlayer dielectric layer covers the cap layer, and the grid electrode penetrates through the interlayer dielectric layer above the cap layer; and performing ion implantation on the laminated structure from one surface, deviating from the interlayer dielectric layer, of the channel layer to form an isolation layer located in the barrier layer and the channel layer, wherein the isolation layer is located at the periphery of an area between the source electrode and the drain electrode. According to the invention, the ions for forming the isolation layer are injected from the back surface of the laminated structure, so that the process difficulty is reduced, the damage to the interlayer dielectric layer is avoided, and the performance of the device is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the field of semiconductor integrated circuit manufacturing and relates to a HEMT device and a preparation method thereof. Background Art

[0002] The third-generation semiconductor material gallium nitride (GaN) has become an ideal candidate material for high-voltage and high-frequency applications due to its wide bandgap and high electron saturation velocity. It is often used to make high electron mobility transistors (HEMT).

[0003] At present, in the process of manufacturing HEMT devices, after epitaxially forming the stacked GaN channel layer, AlGaN barrier layer, P-type GaN gate and interlayer dielectric layer, ions are usually injected into the GaN channel layer and AlGaN barrier layer from the front side of the interlayer dielectric layer to form a high-resistance isolation layer that blocks the electron gas layer at the interface between the GaN channel layer and the AlGaN barrier layer, and then the source, gate and drain of the HEMT device are manufactured. However, when the high-energy ions that form the isolation layer pass through the interlayer dielectric layer and enter the AlGaN barrier layer and the GaN channel layer, the structure of the interlayer dielectric layer will be destroyed, causing damage to the interlayer dielectric layer, and the dielectric properties of the interlayer dielectric layer will be reduced, resulting in a high risk of front breakdown of the interlayer dielectric layer, affecting the reliability of the device. At the same time, due to the thickness of the interlayer dielectric layer, the energy of ion implantation is relatively large, which greatly increases the difficulty of the process.

[0004] Therefore, there is an urgent need to find a method for preparing a HEMT device that reduces the difficulty of making an isolation layer while improving the reliability of the device. Summary of the invention

[0005] In view of the above-mentioned shortcomings of the prior art, an object of the present invention is to provide a HEMT device and a method for preparing the same, so as to solve the problems in the prior art that it is difficult to form an isolation layer for the HEMT device and that the interlayer dielectric layer is damaged when forming the isolation layer, resulting in poor reliability of the device.

[0006] To achieve the above object and other related objects, the present invention provides a method for preparing a HEMT device, comprising the following steps:

[0007] A semiconductor structure is provided, the semiconductor structure comprising a stacked structure, a source, a drain, a cap layer and a gate electrically connected to the cap layer, the stacked structure at least comprising a channel layer, a barrier layer and an interlayer dielectric layer stacked in sequence, the source electrode penetrates the interlayer dielectric layer and is electrically connected to the barrier layer, the drain electrode penetrates the interlayer dielectric layer and is electrically connected to the barrier layer, the cap layer is located on the upper surface of the barrier layer between the source electrode and the drain electrode, the interlayer dielectric layer covers the cap layer, and the gate penetrates the interlayer dielectric layer above the cap layer;

[0008] Ions are implanted into the stacked structure from a side of the channel layer away from the interlayer dielectric layer to form an isolation layer located in the barrier layer and the channel layer, wherein the isolation layer is located at the periphery of the region between the source and the drain.

[0009] Optionally, a plurality of cap layers are disposed on the upper surface of the barrier layer, and the source electrode, the cap layer, the drain electrode and the cap layer are alternately arranged in sequence.

[0010] Optionally, a connection portion is further provided on the upper surface of the barrier layer. In the arrangement direction of the cap layers, the connection portion is spaced apart from the source electrode by a preset distance and is connected to the cap layers on both sides of the source electrode.

[0011] Optionally, a substrate is further provided in the stacked structure, and the channel layer is stacked on an upper surface of the substrate.

[0012] Optionally, before ion implantation is performed on the stacked structure, a step of thinning the substrate from the back side of the substrate is also included.

[0013] Optionally, the method of thinning the substrate includes dry etching, wet etching, and chemical mechanical polishing.

[0014] Optionally, forming the isolation layer comprises the following steps:

[0015] forming a patterned shielding layer on the back side of the laminated structure;

[0016] Ion implantation is performed on the stacked structure based on the patterned shielding layer to obtain the isolation layer.

[0017] Optionally, after forming the shielding layer and before performing ion implantation on the stacked structure, a step of forming a groove located on the lower surface layer of the stacked structure based on the patterned shielding layer is further included.

[0018] Optionally, after forming the isolation layer, the method further includes forming a protective layer on a side of the channel layer away from the interlayer dielectric layer.

[0019] The present invention also provides a HEMT device, which is manufactured by using the above-mentioned method for manufacturing the HEMT device.

[0020] As described above, the HEMT device and the preparation method thereof of the present invention improve the process of manufacturing the device. After forming the front structure of the device, ions forming the isolation layer are injected into the channel layer and the barrier layer from the back of the stacked structure, thereby avoiding the high-energy ions forming the isolation layer from damaging the interlayer dielectric layer above the barrier layer, ensuring the quality of the interlayer dielectric layer, and then ensuring the breakdown resistance of the device, thereby improving the reliability of the device. In addition, since the isolation layer is ion-implanted from the back of the stacked structure, the stacked structure can be thinned from the back of the stacked structure based on process requirements, or after the stacked structure is thinned and a groove is formed in the substrate to expose the channel layer on the bottom surface, ion implantation can be performed to reduce the depth of ion implantation, thereby reducing the process difficulty of forming the isolation layer, and has a high industrial utilization value. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 The process flow chart of the HEMT device manufacturing method of the present invention is shown.

[0022] Figure 2 The cross-sectional structure schematic diagram shows the semiconductor structure of the method for preparing the HEMT device of the present invention.

[0023] Figure 3 A distribution diagram showing various components on the upper surface of the barrier layer in the method for manufacturing the HEMT device of the present invention.

[0024] Figure 4 It is a schematic diagram showing the cross-sectional structure after thinning the substrate in the method for preparing the HEMT device of the present invention.

[0025] Figure 5 It is a schematic diagram showing the cross-sectional structure after forming a patterned shielding layer in the method for preparing a HEMT device of the present invention.

[0026] Figure 6 It is a schematic diagram showing the cross-sectional structure of the HEMT device manufacturing method of the present invention after forming an isolation layer.

[0027] Figure 7 It is a schematic diagram showing the cross-sectional structure of the HEMT device preparation method of the present invention after removing the shielding layer.

[0028] Description of Figure Numbers

[0029] 1 Semiconductor structure

[0030] 11. Laminated structure

[0031] 12 Channel layer

[0032] 13 Barrier layer

[0033] 14 Interlayer dielectric layer

[0034] 15 Substrate

[0035] 16 Cap layer

[0036] 161 Connection

[0037] 17 Source

[0038] 18 Drain

[0039] 19 Gate

[0040] 2 Shielding layer

[0041] 3 Isolation layer DETAILED DESCRIPTION

[0042] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0043] See also Figures 1 to 7 It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner, and the drawings only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.

[0044] Embodiment 1

[0045] This embodiment provides a method for preparing a HEMT device, such as Figures 1 to 7 As shown, Figure 1 The method for preparing the HEMT device comprises the following steps:

[0046] S1: Provide a semiconductor structure, the semiconductor structure comprising a stacked structure, a source, a drain, a cap layer and a gate electrically connected to the cap layer, the stacked structure at least comprising a channel layer, a barrier layer and an interlayer dielectric layer stacked in sequence, the source electrode penetrates the interlayer dielectric layer and is electrically connected to the barrier layer, the drain electrode penetrates the interlayer dielectric layer and is electrically connected to the barrier layer, the cap layer is located on the upper surface of the barrier layer between the source and the drain, the interlayer dielectric layer covers the cap layer, and the gate penetrates the interlayer dielectric layer above the cap layer;

[0047] S2: performing ion implantation from a side of the channel layer away from the interlayer dielectric layer into the stacked structure to form an isolation layer located between the barrier layer and the channel layer, wherein the isolation layer is located at the periphery of a region between the source and the drain.

[0048] See also Figures 2 to 4 , perform the step 1: provide a semiconductor structure 1, the semiconductor structure 1 includes a stacked structure 11, a source 17, a drain 18, a cap layer 16 and a gate 19 electrically connected to the cap layer 16, the stacked structure 11 at least includes a channel layer 12, a barrier layer 13 and an interlayer dielectric layer 14 stacked in sequence, the source 17 penetrates the interlayer dielectric layer 14 and is electrically connected to the barrier layer 13, the drain 18 penetrates the interlayer dielectric layer 14 and is electrically connected to the barrier layer 13, the cap layer 15 is located on the upper surface of the barrier layer 13 between the source 17 and the drain 18, the interlayer dielectric layer 14 covers the cap layer 16, and the gate 19 penetrates the interlayer dielectric layer 14 above the cap layer 16.

[0049] Specifically, Figure 2 , which is a schematic cross-sectional view of the semiconductor structure 1 , wherein the channel layer 12 is made of GaN, AlGaN, InGaN or other suitable semiconductor materials. In this embodiment, a GaN layer is used as the channel layer 12 .

[0050] Specifically, the material of the barrier layer 13 includes In x Al y Ga 1-x-y N、Al x Ga 1-x N、In x Al 1-x N or other suitable materials. In this embodiment, Al x Ga 1-x N serves as the barrier layer 13 .

[0051] Specifically, the material of the interlayer dielectric layer 14 includes aluminum nitride, silicon nitride, silicon oxide or other suitable dielectric materials.

[0052] Specifically, the material of the source electrode 17 includes titanium, titanium nitride, silver, gold, copper, aluminum, nickel, tungsten, platinum or other suitable conductive materials; the material of the drain electrode 18 includes titanium, titanium nitride, silver, gold, copper, aluminum, nickel, tungsten, platinum or other suitable conductive materials; the material of the gate electrode 19 includes titanium, titanium nitride, silver, gold, copper, aluminum, nickel, tungsten, platinum or other suitable conductive materials.

[0053] As an example, the source electrode 17 is embedded in the barrier layer 13 and the contact type between the source electrode 17 and the barrier layer 13 is an ohmic contact, and the drain electrode 18 is embedded in the barrier layer 13 and the contact type between the drain electrode 18 and the barrier layer 13 is an ohmic contact.

[0054] Specifically, the source electrode 17 forms an ohmic contact with the barrier layer 13, so that the two-dimensional electron gas layer (conductive channel) formed between the barrier layer 13 and the channel layer 12 is connected to the source electrode 17; the drain electrode 18 forms an ohmic contact with the barrier layer 13, so that the two-dimensional electron gas layer (conductive channel) formed between the barrier layer 13 and the channel layer 12 is connected to the drain electrode 18.

[0055] Specifically, under the condition that the source electrode 17 is connected to the two-dimensional electron gas layer (conductive channel) between the barrier layer 13 and the channel layer 12 , the source electrode 17 may also penetrate the barrier layer 13 .

[0056] Specifically, under the condition that the drain electrode 18 is connected to the two-dimensional electron gas layer (conductive channel) between the barrier layer 13 and the channel layer 12 , the drain electrode 18 may also penetrate the barrier layer 13 .

[0057] As an example, the cap layer 16 is made of P-type GaN, P-type AlGaN or other semiconductor materials that can completely deplete the two-dimensional electron gas at the interface between the barrier layer 13 and the channel layer 12 below the cap layer 16 .

[0058] Specifically, while ensuring the performance of the device, the size, thickness and shape of the cap layer 16 can be selected according to actual conditions and are not limited here.

[0059] As an example, a plurality of cap layers 16 are provided on the upper surface of the barrier layer 13, and the source 17, the cap layer 16, the drain 18 and the cap layer 16 are alternately arranged in sequence, that is, the source 17, the cap layer 16, the drain 18 and the cap layer 16 in the device are arranged at intervals and constitute a repeating unit.

[0060] Specifically, while ensuring device performance, the distance between the source 17 and the cap layer 16 can be selected according to actual conditions and is no longer restricted here; the distance between the drain 18 and the cap layer 16 can be selected according to actual conditions and is no longer restricted here; the distance between the source 17 and the drain 18 can be selected according to actual conditions and is no longer restricted here.

[0061] As an example, Figure 3 As shown, it is a distribution diagram of various components on the upper surface of the barrier layer 13. A connecting portion 161 is also provided on the upper surface of the barrier layer 13. In the arrangement direction of the cap layer 16, the connecting portion 161 is spaced a preset distance from the source 17 and is connected to the cap layer 16 on both sides of the source 17.

[0062] Specifically, when the connection portion 161 is connected to the cap layers 16 on both sides of the source 17 along the arrangement direction, the same gate 19 can control the turning off and on of the two-dimensional electron gas under the two cap layers 16 .

[0063] Specifically, the connection portion 161 may be connected to one end of the cap layer 16 perpendicular to the arrangement direction of the cap layer 16, or may be connected to one end of the cap layer 16 perpendicular to the arrangement direction of the cap layer 16, so as to achieve the connection of the cap layer 16 on both sides of the source electrode 17 along the arrangement direction of the cap layer 16. In this embodiment, the connection portion 161 connects one end of the cap layer 161 perpendicular to the arrangement direction of the cap layer 16, and the connection portion 161 is located on the same side of the source electrode 17 perpendicular to the arrangement direction of the cap layer 16.

[0064] Specifically, while ensuring the performance of the device, the size and shape of the connecting portion 161 can be selected according to actual conditions and are not limited here.

[0065] Specifically, the interlayer dielectric layer 14 is provided with a source contact hole, a drain contact hole and a gate contact hole, the source contact hole penetrates the interlayer dielectric layer 14 and at least the barrier layer 13 is exposed at the bottom, the drain contact hole penetrates the interlayer dielectric layer 14 and at least the barrier layer 13 is exposed at the bottom, the gate contact hole penetrates the interlayer dielectric layer 14 above the cap layer 16 and the cap layer 16 is exposed on the bottom, the source 17 fills the source contact hole to achieve electrical connection with the barrier layer 13, the drain 18 fills the drain contact hole to achieve electrical connection with the barrier layer 13, and the gate 19 fills the gate contact hole to achieve electrical connection with the cap layer 16.

[0066] Specifically, while ensuring device performance, the opening size and opening shape of the source contact hole can be selected according to actual conditions and are no longer restricted here; the opening size and opening shape of the drain contact hole can be selected according to actual conditions and are no longer restricted here; the opening size and opening shape of the gate contact hole can be selected according to actual conditions and are no longer restricted here.

[0067] As an example, a substrate is further provided in the stacked structure 11, and the channel layer 12 is stacked on the upper surface of the substrate.

[0068] Specifically, the substrate 15 is usually a process platform for forming the channel layer 12. Under the condition of ensuring device performance, the size, thickness and shape of the substrate 15 can be selected according to actual conditions and are not limited here.

[0069] Specifically, the substrate 15 is made of silicon, silicon germanium, glass, silicon carbide, sapphire, diamond, gallium nitride or other suitable materials.

[0070] Specifically, in order to ensure the quality of the formed channel layer 12, when the lattice mismatch between the substrate 15 and the channel layer 12 is large, a buffer layer needs to be formed between the substrate 15 and the channel layer 12 to reduce the lattice mismatch between the substrate 15 and the channel layer 12, and the lattice mismatch between the buffer layer and the channel layer 12 is small. Under the condition of ensuring the quality of the formed channel layer 12, the material of the buffer layer can be selected according to actual conditions. For example, an aluminum nitride layer can be set between the silicon substrate and the gallium nitride channel layer as a buffer layer to ensure the quality of the formed gallium nitride channel layer.

[0071] Specifically, the lattice mismatch between the substrate 15 and the channel layer 12 is relatively large. Under the condition of ensuring the quality of the formed channel layer 12, the thickness of the buffer layer can be selected according to actual conditions and is not limited here.

[0072] As an example, Figure 4 , which is a schematic diagram of the cross-sectional structure after the substrate 15 is thinned, includes a step of thinning the substrate 15 from the back side of the substrate 15 before ion implantation of the stacked structure 11. The back side here refers to the side of the substrate 15 away from the channel layer 12.

[0073] Specifically, the thickness of the substrate 15 is usually relatively thick, and it is difficult to use ion implantation to implant ions through the substrate 15 into the interface region between the channel layer 12 and the barrier layer 13, resulting in process difficulties. By thinning the thickness of the substrate 15 and then performing ion implantation, the difficulty of ion implantation can be reduced, thereby reducing the process difficulty.

[0074] As an example, the method of thinning the substrate 15 includes dry etching, wet etching, chemical mechanical polishing or other suitable methods. Preferably, the substrate 15 is thinned from the side of the substrate 15 away from the channel layer 12 by chemical mechanical polishing.

[0075] Specifically, while ensuring the quality of the isolation layer 3 formed, the thickness of the thinned substrate 15 can be selected according to actual conditions. For example, the substrate 15 of a preset thickness can be retained as a protective layer for protecting the channel layer 12, or the substrate 15 can be completely removed to facilitate the formation of the isolation layer 3.

[0076] Specifically, while ensuring device performance, after completely removing the substrate 15, the channel layer 12 can also be thinned from the side of the channel layer 12 away from the barrier layer 13, and the channel layer 12 can be thinned by dry etching, wet etching, chemical mechanical polishing or other suitable methods.

[0077] Please see again Figures 5 to 7 , perform step S2: perform ion implantation from the side of the channel layer 12 away from the interlayer dielectric layer 14 to the stacked structure 11 to form an isolation layer 3 located in the barrier layer 13 and the channel layer 12, and the isolation layer 3 is located at the periphery of the area between the source 17 and the drain 18.

[0078] As an example, Figure 5 and Figure 6 As shown, they are respectively a schematic diagram of the cross-sectional structure after forming the shielding layer 2 and a schematic diagram of the cross-sectional structure after forming the isolation layer 3. The formation of the isolation layer 3 includes the following steps: forming a patterned shielding layer 2 on the back side of the stacked structure 11; and performing ion implantation on the stacked structure 11 based on the patterned shielding layer 2 to obtain the isolation layer 3.

[0079] Specifically, during the process of ion implantation to form the isolation layer 3, the shielding layer 2 is usually used to protect the non-ion implantation area and block ions from entering the non-doped area to ensure the performance of the device. Based on the ion blocking function of the shielding layer 2, its material can be a composite film layer composed of a hard mask layer and a photoresist layer, can be only a hard mask layer, or can be only a photoresist layer. In this embodiment, the shielding layer 2 covers the side of the laminated structure 11 that is away from the cap layer 16 (i.e., the bottom surface of the laminated structure 11).

[0080] Specifically, the method for forming the patterned shielding layer 2 is a common photolithography process, which will not be described in detail here.

[0081] As an example, after forming the shielding layer 2 and before performing ion implantation on the stacked structure 11 , a step of forming a groove located at the lower surface layer of the stacked structure 11 based on the patterned shielding layer 2 is also included.

[0082] Specifically, when the groove is formed in the lower surface layer of the stacked structure 11, when the substrate 15 is provided in the stacked structure 11, the groove is usually formed in the substrate 15 or penetrates the substrate 15 to reduce the depth of ion implantation, thereby reducing the difficulty of the ion implantation process; when the substrate 15 is not provided in the stacked structure 11, the groove can also be formed in the channel layer 12 of the lower surface layer of the stacked structure 11 while ensuring the device performance.

[0083] Specifically, the isolation layer 3 is usually located in the boundary area between the barrier layer 13 and the channel layer 12, and is used to block the two-dimensional electron gas layer formed between the channel layer 12 and the barrier layer 13. It is generally achieved by destroying the internal lattice structure of the channel layer 12 and the barrier layer 13 outside the area between the source 17 and the drain 18 through high-energy ion implantation, so that it becomes a high-resistance state, thereby isolating the two-dimensional electron gas layer in the area between the source 17 and the drain 18 from the two-dimensional electron gas layer outside the area between the source 17 and the drain 18.

[0084] Specifically, under the condition of ensuring the isolation performance of the isolation layer 3 formed, the dose of ion implantation and the energy of ion implantation for forming the isolation layer 3 can be selected according to actual conditions, and are not limited here.

[0085] Specifically, the types of ions implanted into the channel layer 12 and the barrier layer 13 include H ions, F ions or other suitable ions.

[0086] Specifically, under the condition of ensuring the performance of the device, the size and shape of the isolation layer 3 can be selected according to actual conditions, and are no longer restricted here; the distance between the upper surface of the isolation layer 3 and the upper surface of the barrier layer 13 and the distance between the lower surface of the isolation layer 3 and the lower surface of the channel layer 12 can be selected according to actual conditions. For example, the upper surface of the isolation layer 3 is flush with the upper surface of the barrier layer 13, and the lower surface of the isolation layer 3 is flush with the lower surface of the channel layer 12, or the upper surface and lower surface of the isolation layer 3 are respectively separated by a preset distance from the upper surface of the barrier layer 13 and the lower surface of the channel layer 12.

[0087] Specifically, Figure 7As shown, it is a schematic diagram of the cross-sectional structure after removing the shielding layer 2. After forming the isolation layer 3, it also includes a step of removing the shielding layer 2. The method for removing the shielding layer 2 is the commonly used photoresist stripping and hard mask layer removal process, which will not be repeated here.

[0088] As an example, after forming the isolation layer 3, the step of forming a protective layer on the side of the channel layer 12 facing away from the interlayer dielectric layer 14 is also included, that is, when the substrate 15 is not provided on the side of the channel layer 12 facing away from the interlayer dielectric layer 14 or a groove exposing the channel layer 15 is formed in the substrate 15, after ion implantation from the bottom surface of the channel layer 12, the protective layer for protecting the channel layer 12 needs to be formed on the back side of the channel layer 12.

[0089] Specifically, the protection layer is used to protect the channel layer 12 to prevent the channel layer 12 from being damaged. The material of the protection layer includes aluminum nitride, silicon nitride, silicon oxide or other suitable materials.

[0090] Specifically, the stacked structure 11 is provided with the groove whose bottom surface exposes the channel layer 12 , and the groove is filled with the protection layer to protect the channel layer 12 exposed on the bottom surface of the groove to avoid damage to the channel layer 12 .

[0091] Specifically, after forming the front structure of the device, ion implantation is performed from the back side of the stacked structure 11 to form the isolation layer 3, thereby avoiding damage to the interlayer dielectric layer 14 during the process of forming the isolation layer 3 by ion implantation from the front side of the device, thereby destroying the internal structure of the interlayer dielectric layer 14 and affecting the dielectric properties of the interlayer dielectric layer 14, ensuring the quality of the interlayer dielectric layer 14, avoiding the risk of front side breakdown of the interlayer dielectric layer 14, and improving the reliability of the device.

[0092] Specifically, by injecting ions from the back side of the stacked structure 11 to form the isolation layer 3, there is no need to consider the effect of the thickness of the interlayer dielectric layer 14 on the process. The thickness of the interlayer dielectric layer 14 can be increased as needed to improve the device's breakdown resistance.

[0093] Specifically, by injecting ions to form the isolation layer 3 from the back side of the stacked structure 11, the stacked structure 11 can be thinned from the back side of the stacked structure 11, or a groove exposing the channel layer can be formed in the substrate 15, and then ion implantation is performed, which can reduce the depth of ion implantation and then reduce the energy of ion implantation, thereby reducing the difficulty of the process and having no effect on the performance of the device.

[0094] The preparation method of the HEMT device of the present embodiment improves the process of manufacturing the HEMT device. After forming the front structure of the device, ions are implanted from the back side of the stacked structure 11 to form the isolation layer 3. This eliminates the need to consider the effect of the thickness of the interlayer dielectric layer 14 on the process. At the same time, the depth of ion implantation can be reduced, thereby reducing the difficulty of the process. In addition, damage to the interlayer dielectric layer 14 during the formation of the isolation layer 3 can be avoided, thereby ensuring the quality of the interlayer dielectric layer 14, thereby ensuring the breakdown resistance of the device and improving the reliability of the device.

[0095] Embodiment 2

[0096] This embodiment provides a HEMT device, such as Figure 7 , which is a schematic diagram of the cross-sectional structure of the HEMT device, and the HEMT device is manufactured by using the above-mentioned method for preparing the HEMT device.

[0097] Specifically, the HEMT device includes a semiconductor structure 1 and an isolation layer 3. The semiconductor structure 1 includes a stacked structure 11, a source 17, a drain 18, a cap layer 16, and a gate 19 electrically connected to the cap layer 16. The stacked structure 11 at least includes a channel layer 12, a barrier layer 13, and an interlayer dielectric layer 14 stacked in sequence. The source 17 penetrates the interlayer dielectric layer 14 and is electrically connected to the barrier layer 13. The drain 18 penetrates the interlayer dielectric layer 14 and is electrically connected to the barrier layer 13. The cap layer 16 is located on the upper surface of the barrier layer 13 between the source 17 and the drain 18. The interlayer dielectric layer 14 covers the cap layer 16. The gate 19 penetrates the interlayer dielectric layer 14 above the cap layer 16. The isolation layer 3 is located in the barrier layer 13 and the channel layer 12 on the periphery of the region between the source 17 and the drain 18.

[0098] Specifically, in the stacked structure 11 , due to the material properties of the channel layer 12 and the barrier layer 13 , a two-dimensional electron gas layer serving as a conductive channel of the device can be formed at the interface between the channel layer 12 and the barrier layer 13 .

[0099] Specifically, under the condition of ensuring the device performance, the thickness, size and shape of the channel layer 12 can be selected according to actual conditions and are not limited here.

[0100] Specifically, under the condition of ensuring the device performance, the thickness, size and shape of the barrier layer 13 can be selected according to actual conditions and are not limited here.

[0101] Specifically, the interlayer dielectric layer 14 is used to passivate the barrier layer 13, and at the same time has the function of isolating the source 17, the gate 19 and the drain 18 in the device to ensure the breakdown resistance of the device. While ensuring the performance of the device, the thickness of the interlayer dielectric layer 14 can be selected according to actual conditions and is no longer limited here.

[0102] Specifically, the interlayer dielectric layer 14 is provided with a source contact hole, a drain contact hole and a gate contact hole which penetrate the interlayer dielectric layer 14, the bottom of the source contact hole at least exposes the barrier layer 13, the source electrode 17 fills the source contact hole and is at least electrically connected to the barrier layer 13, so as to achieve connectivity with the two-dimensional electron gas layer formed between the channel layer 12 and the barrier layer 13, the drain electrode 18 fills the drain contact hole and is at least electrically connected to the barrier layer 13, so as to achieve connectivity with the two-dimensional electron gas layer formed between the channel layer 12 and the barrier layer 13, the bottom surface of the gate contact hole exposes the cap layer 16, and the gate 19 fills the gate contact hole to achieve electrical connection with the cap layer 16.

[0103] Specifically, the cap layer 16 is used to enhance the threshold voltage of the device and reduce the on-resistance of the device. Under the condition of ensuring the performance of the device, the size, thickness and shape of the cap layer 16 can be selected according to actual conditions and are not limited here.

[0104] Specifically, the isolation layer 3 is a high-resistance region formed by injecting high-energy ions from the back side of the stacked structure 11, and is mainly used to block the connection between the two-dimensional electron gas layer in the area between the source 17 and the drain 18 and the two-dimensional electron gas layer outside the area between the source 17 and the drain 18. The size and shape of the isolation layer 3 can be selected according to actual conditions and are no longer limited here.

[0105] Specifically, a groove is further provided on the lower surface layer of the stacked structure 11 to reduce the ion implantation depth for forming the isolation layer 3 and reduce the process difficulty for forming the isolation layer 3 .

[0106] Specifically, a substrate 15 is further provided in the stacked structure 11 , and the channel layer 12 is stacked on the upper surface of the substrate 15 .

[0107] Specifically, the substrate 15 is usually used to protect the channel layer 12. Under the condition of ensuring the device performance, the thickness of the substrate 15 can be selected according to actual conditions and is not limited here.

[0108] Specifically, when the substrate 15 is provided in the stacked structure 11 and the groove for forming the isolation layer 3 is provided in the substrate 15, the groove in the substrate 15 exposes the channel layer 12, that is, the groove only passes through the substrate 15 or passes through the substrate 15 and the bottom surface extends into the channel layer 12, so as to reduce the difficulty of forming the isolation layer 3; while ensuring the device performance, the bottom surface of the groove may also be located in the substrate 15.

[0109] Specifically, under the condition of ensuring the performance of the device, the depth of the groove can be selected according to the actual situation and is not limited here.

[0110] Specifically, when the lower surface layer of the stacked structure 11 is provided with the groove and the channel layer 12 is exposed at the bottom of the groove, a protection layer filling the groove is further provided in the groove to protect the channel layer 12 exposed at the bottom of the groove.

[0111] Specifically, when the substrate 15 is not provided on the side of the channel layer 12 facing away from the barrier layer 13 , a protective layer is further provided on the surface of the channel layer 12 facing away from the barrier layer 13 to protect the channel layer 12 and passivate the back side of the channel layer 12 .

[0112] Specifically, by adopting the preparation method of the HEMT device described in Example 1, high-energy ions that form the isolation layer 3 are injected from the back side of the stacked structure 11, thereby avoiding damage to the interlayer dielectric layer 14, ensuring the quality of the interlayer dielectric layer 14, reducing the risk of front side breakdown of the interlayer dielectric layer 14, and improving the reliability of the device.

[0113] The HEMT device of this embodiment is manufactured by adopting the preparation method of the HEMT device described in the first embodiment, thereby ensuring the quality of the interlayer dielectric layer 14, improving the problem of easy breakdown of the front side of the interlayer dielectric layer 14, and improving the reliability of the device.

[0114] In summary, the HEMT device and preparation method of the present invention improve the formation process of the isolation layer. After forming the front structure of the device, ions forming the isolation layer are injected from the back of the laminate structure, thereby avoiding high-energy ions from damaging the interlayer dielectric layer above the barrier layer, ensuring the quality of the interlayer dielectric layer, and then ensuring the breakdown resistance of the device, and improving the reliability of the device. At the same time, after the laminate structure is thinned from the back of the laminate structure, or after the laminate structure is thinned, a groove is formed in the substrate to expose the channel layer on the bottom surface, and then ion implantation can be performed to reduce the depth of ion implantation, thereby reducing the process difficulty of forming the isolation layer. Therefore, the present invention effectively overcomes various shortcomings in the prior art and has a high industrial utilization value.

[0115] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A method for preparing a HEMT device, characterized in that: The following steps are involved: A semiconductor structure is provided, the semiconductor structure comprising a stacked structure, a source, a drain, a cap layer and a gate electrically connected to the cap layer, the stacked structure at least comprising a channel layer, a barrier layer and an interlayer dielectric layer stacked in sequence, the source electrode penetrates the interlayer dielectric layer and is electrically connected to the barrier layer, the drain electrode penetrates the interlayer dielectric layer and is electrically connected to the barrier layer, the cap layer is located on the upper surface of the barrier layer between the source and the drain, the interlayer dielectric layer covers the cap layer, and the gate penetrates the interlayer dielectric layer above the cap layer; Ions are implanted into the stacked structure from a side of the channel layer away from the interlayer dielectric layer to form an isolation layer located in the barrier layer and the channel layer, wherein the isolation layer is located at the periphery of the region between the source and the drain.

2. The method for preparing a HEMT device according to claim 1, characterized in that: A plurality of cap layers are disposed on the upper surface of the barrier layer, and the source electrode, the cap layer, the drain electrode and the cap layer are alternately arranged in sequence.

3. The method for preparing a HEMT device according to claim 2, characterized in that: A connection portion is further provided on the upper surface of the barrier layer. In the direction in which the cap layers are arranged, the connection portion is spaced apart from the source electrode by a preset distance and is connected to the cap layers on both sides of the source electrode.

4. The method for preparing a HEMT device according to claim 1, characterized in that: A substrate is also provided in the stacked structure, and the channel layer is stacked on the upper surface of the substrate.

5. The method for preparing a HEMT device according to claim 4, characterized in that: Before ion implantation is performed on the stacked structure, a step of thinning the substrate from the back side of the substrate is also included.

6. The method for preparing a HEMT device according to claim 5, characterized in that: Methods for thinning the substrate include dry etching, wet etching, and chemical mechanical polishing.

7. The method for preparing a HEMT device according to claim 1, characterized in that: Forming the isolation layer comprises the following steps: forming a patterned shielding layer on the back side of the laminated structure; Ion implantation is performed on the stacked structure based on the patterned shielding layer to obtain the isolation layer.

8. The method for preparing a HEMT device according to claim 7, characterized in that: After forming the shielding layer and before performing ion implantation on the stacked structure, the method further includes forming a groove located at the lower surface layer of the stacked structure based on the patterned shielding layer.

9. The method for preparing a HEMT device according to claim 1, characterized in that: After forming the isolation layer, the method further includes forming a protection layer on a side of the channel layer away from the interlayer dielectric layer.

10. A HEMT device, characterized in that: The HEMT device is manufactured by the method for manufacturing a HEMT device according to any one of claims 1 to 9.

Citation Information

Cited By

  • HEMT device and preparation method therefor

    WO2026118561A1