Flexible printed circuit (FPC) expansion and contraction control method
By controlling various processes in the production process of flexible circuit boards, the problem of increase and contraction is solved, the stability and production efficiency of the product are improved, and higher yield and reliability are achieved.
Patent Information
- Application Number
- CN202411054988.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-02
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-08-02
AI Technical Summary
The expansion and shrinkage of flexible circuit boards lead to unstable electrical performance, poor assembly and connection, reduced product reliability and reduced production efficiency, and effective control measures are needed to reduce the occurrence of expansion and shrinkage.
Control of the copper foil substrate by baking, laser, plasma treatment, copper plating, etching, pressing, punching, grinding, ink coating, baking, gold-melting and PI pressing processes, combined with material selection and process to ensure the stability and uniformity of each process parameters, avoid dimensional changes and stress concentration.
It effectively reduces the increase and shrinkage of the flexible circuit board, improves the stability and production efficiency of the product, avoids rework and repair, and improves the yield and reliability of FPC.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of flexible circuit boards, and in particular to a method for controlling the expansion and contraction of FPCs. Background Art
[0002] Flexible printed circuit board (FPC), as one of the important branches of printed circuit board (PCB), is a highly reliable and extremely flexible printed circuit board made of polyimide or polyester film as insulating substrate. Flexible printed circuit board (FPC) has the advantages of high wiring density, ultra-thin, ultra-light, foldable, high assembly flexibility, etc. It can be moved and stretched arbitrarily in the main space, and it is easy to realize the integration of component assembly and wire connection. At present, the application of FPC involves almost all electronic information products, including consumer electronics, communication equipment, automotive products and other wide fields.
[0003] The expansion and contraction of flexible printed circuits (FPCs) may bring the following hazards: In terms of electrical performance, expansion and contraction may cause changes in line spacing, and slight line changes may cause signal transmission interruption or errors; changes in line length and width will affect the resistance value, thereby affecting the performance and stability of the circuit. In terms of assembly and connection, the expansion and contraction of FPCs will prevent them from accurately aligning with the pins of the installed electronic components, affecting the efficiency and quality of assembly. For example, the connector cannot be tightly connected to the FPC, resulting in poor contact; during the welding process, expansion and contraction will cause uneven bonding between the pad and the solder, resulting in problems such as cold welding and false welding, reducing the reliability of welding. In terms of product reliability, the internal stress caused by expansion and contraction may be concentrated in certain parts, which will cause fatigue damage to the circuit board under long-term action and shorten the service life of the product; expansion and contraction may damage the insulation layer of the circuit board, reduce insulation performance, and increase the risk of leakage and short circuit. In addition, due to quality problems caused by expansion and contraction, the generation of scrap will increase, and production costs will increase. FPCs with expansion and contraction problems also need to be reworked or repaired, which will consume a lot of time and manpower and reduce overall production efficiency. In short, the expansion and contraction of flexible circuit boards will have an adverse effect on the product's electrical performance, assembly connections, reliability, and production process. Therefore, effective measures must be taken to control and reduce the occurrence of expansion and contraction during the design, production, and use process.
[0004] In view of this, the present invention is developed by deeply considering the many defects and inconveniences caused by the expansion and contraction of the flexible circuit board, and actively researching, improving and testing to develop the present invention. Summary of the invention
[0005] The purpose of the present invention is to overcome the deficiencies of the prior art and provide a method for controlling the expansion and contraction of an FPC that can improve the expansion and contraction of an FPC.
[0006] In order to achieve the above object, the solution of the present invention is: A method for controlling the expansion and contraction of an FPC, comprising the following steps: S1. Bake the copper foil substrate and then return it to the temperature to improve the dimensional stability of the substrate, remove moisture from the copper foil substrate, and reduce dimensional changes caused by moisture evaporation during subsequent processing; S2, laser, select laser energy to avoid excessive energy causing excessive heating of the substrate, control the laser speed to ensure even heat distribution; S3, plasma treatment, to clean and activate the surface of the substrate after laser treatment, remove surface pollutants, oxides and organic impurities, improve surface performance and wettability, and enhance the bonding force between materials; S4, copper plating, control the current density to avoid local overheating and stress concentration caused by excessive current, control the electroplating time to ensure uniform thickness of the copper plating layer, control the composition of the plating solution to ensure stable performance of the plating solution; S5, etching, control the concentration of the etching solution, keep the concentration of the etching solution stable and appropriate, avoid concentration fluctuations leading to uneven etching rate, control the temperature and time of etching, prevent dimensional changes caused by over-etching or under-etching, ensure that the etching solution is evenly stirred during the etching process, so that the etching reaction proceeds evenly; balance the line distribution, so that the lines are evenly distributed on the FPC; S6. Laminating CVL, controlling the laminating temperature to avoid excessive expansion of the substrate and CVL due to high temperature, or loose bonding due to low temperature; adjusting the pressure to ensure that the CVL and the substrate are tightly fitted to reduce gaps and uneven stress; controlling the laminating time to ensure sufficient time for the adhesive to fully cure; S7, Punching, control the punching speed to avoid excessive heat generated by punching too fast, control the punching pressure, apply pressure evenly to prevent material deformation caused by uneven pressure; S8, grinding, reduce grinding pressure, control grinding speed, use multi-stage grinding, gradually adjust grinding volume, control temperature during grinding, and avoid changes in substrate material properties caused by excessive temperature; S9, ink, apply the ink evenly to avoid large differences in ink thickness; S10, baking, using a hot air circulation oven to ensure uniform temperature distribution in the baking chamber; S11, gold plating, control the temperature and concentration of the chemical gold plating solution to avoid excessive temperature fluctuations; control the concentration of each component in the gold plating solution; S12, PI lamination, control the lamination pressure, ensure that the pressure is evenly distributed in the entire lamination area, so that the PI and the substrate fit tightly; control the lamination time, ensure that there is enough lamination time for the PI material to fully solidify and fuse; S13, punching shape, bake the FPC before punching, design the punching path to make it symmetrical; control the punching speed to avoid excessive impact force caused by too fast speed and deformation of the material; control the punching pressure to complete the punching without over-extruding the material; keep the punching temperature stable.
[0007] Further, in step S12, PI uses PI materials with low thermal expansion coefficient and stable performance, and performs incoming material inspection on PI materials to ensure that their thickness is uniform and free of defects; accurately controls the lamination temperature to avoid uneven expansion or contraction caused by excessively high or low temperatures; Furthermore, the steps S1 to S5 are all processed by roll-to-roll processing, the copper foil substrate of step S1 uses a whole roll of copper foil, and the first and last rolls of the substrate of steps S2-S5 are both pulled by guide films, and the front and rear guide films are 8m each.
[0008] Furthermore, there is a black shadow process between step S3 plasma treatment and step S4 copper plating process. Before the black shadow process, the FPC is pre-baked to remove moisture and internal stress; after the black shadow process is completed, slow cooling or annealing is performed to reduce internal stress.
[0009] Furthermore, there is an exposure process between step S4 copper plating and step S5 etching process, using glass film, the front and rear rolls are pulled by guide films, and the front and rear pulling films are 8m each.
[0010] Furthermore, in step S6, the CVL is pre-processed before laminating the CVL, and the arrow in the waste area in the board feeding direction points forward.
[0011] Furthermore, the present invention also includes a shrinkage test step, taking 30 PNL from the first section, middle section and last section of the whole roll product, marking 1-30 as the first section, 31-60 as the middle section, and 61-90 as the last section, collecting and monitoring the data of each PNL and corresponding to its corresponding marking sequence.
[0012] After adopting the above scheme, the FPC expansion and shrinkage control method of the present invention can effectively improve the expansion and shrinkage in the FPC production process by controlling each process in the FPC production process, including material selection, material processing, and parameter control in each process, avoid FPC defects caused by expansion and shrinkage, ensure product stability, avoid rework or repair due to FPC expansion and shrinkage, and improve FPC production efficiency. DETAILED DESCRIPTION
[0013] In order to further explain the technical solution of the present invention, the present invention is described in detail below through specific embodiments.
[0014] The present invention discloses a method for controlling the expansion and contraction of an FPC, which comprises the following steps: S1. Bake the copper foil substrate in an oven at 120°C for 4 hours and return to the temperature for 3 hours. Baking the copper foil substrate can reduce the risk of expansion and shrinkage. In addition, baking can also improve dimensional stability and remove moisture from the copper foil substrate, thereby improving the precision and accuracy of laser processing.
[0015] S2. Laser: select appropriate laser energy to avoid excessive energy causing excessive heating of the substrate and resulting in large expansion and contraction; control the laser speed and reasonably control the laser scanning speed to ensure even heat distribution and reduce expansion and contraction caused by local thermal stress.
[0016] S3, plasma treatment, cleans and activates the surface of the substrate after laser treatment, removes surface pollutants, oxides and organic impurities, etc., improves surface energy, and enhances the bonding force between materials. After plasma treatment, the properties of the FPC surface are improved, which helps to better control the expansion and contraction of the material in subsequent processes.
[0017] S4, copper plating, control the current density, select the appropriate current density to avoid excessive current causing local overheating and stress concentration, causing expansion and contraction; control the electroplating time to ensure that the thickness of the copper plating layer is uniform, not too thick or too thin; control the composition of the plating solution, test and supplement the main salt, additives and other components in the plating solution before copper plating to ensure the stability of the plating solution performance.
[0018] S5, Etching, control the concentration of the etching solution, keep the concentration of the etching solution stable and appropriate, avoid concentration fluctuations leading to uneven etching rate and causing expansion and contraction; control the temperature and time of etching to prevent dimensional changes caused by over-etching or insufficient etching, ensure that the etching solution is evenly stirred during the etching process, so that the etching reaction proceeds evenly; balance the line distribution, so that the lines are evenly distributed on the FPC, and avoid expansion and contraction caused by local stress concentration.
[0019] S6. Laminating CVL, control the laminating temperature, select the appropriate temperature range, avoid excessive expansion of the substrate and CVL due to too high temperature, or loose bonding due to too low temperature; adjust the pressure, apply appropriate pressure evenly, ensure that CVL and the substrate are tightly fitted, reduce gaps and uneven stress; control the laminating time, ensure enough time for the adhesive to fully cure, but not too long to avoid affecting production efficiency and causing unnecessary dimensional changes.
[0020] S7. Punching: Control the punching speed to avoid excessive heat generated by punching too fast; control the punching pressure and apply appropriate pressure evenly to prevent material deformation caused by uneven pressure.
[0021] S8, grinding plate, reduce grinding plate pressure, control grinding plate speed, use multi-stage grinding plate, gradually adjust the grinding amount, control the temperature during grinding plate, and avoid changes in substrate material properties caused by excessive temperature.
[0022] S9. Ink: Apply the ink evenly to avoid large differences in ink thickness, because inks of different thicknesses may shrink to different degrees during baking.
[0023] S10. Baking: Use a hot air circulation oven to ensure that the temperature in the baking chamber is evenly distributed to avoid excessive expansion of the substrate and ink due to excessively high temperature, or incomplete curing of the ink due to excessively low temperature.
[0024] S11, gold plating, control the temperature and concentration of the chemical gold plating solution to stabilize the temperature within an appropriate range to avoid excessive temperature fluctuations; at the same time, control the concentration of each component in the gold plating solution to ensure the uniformity and stability of the reaction. During the gold plating process, the dimensional changes of the FPC are detected in real time. Once the expansion or contraction is found to be beyond the allowable range, the process parameters are adjusted in time.
[0025] S12, PI lamination, select PI materials with low thermal expansion coefficient and stable performance, and inspect the incoming PI materials to ensure that their thickness is uniform and free of defects; accurately control the lamination temperature to avoid uneven expansion or contraction caused by too high or too low temperature; control the lamination pressure to ensure that the pressure is evenly distributed in the entire lamination area, so that the PI and the substrate fit tightly, reducing gaps and stress concentration; control the lamination time to ensure sufficient lamination time for the PI material to fully solidify and fuse, but not too long to prevent excessive thermal effects.
[0026] S13, punching shape, bake the FPC before punching, design the punching path to make it symmetrical, reduce the expansion and contraction caused by uneven force; control the punching speed to avoid excessive impact force caused by too fast speed and deformation of the material; control the punching pressure to ensure that the pressure is moderate so that the punching can be completed without over-extruding the material; keep the punching temperature stable to reduce the impact of temperature changes on material properties and dimensions.
[0027] The FPC expansion and shrinkage control method of the present invention can effectively improve the expansion and shrinkage in the FPC production process by controlling each process in the FPC production process, including material selection, material processing, and parameter control in each process, avoid FPC defects caused by expansion and shrinkage, ensure product stability, avoid rework or repair due to FPC expansion and shrinkage, and improve FPC production efficiency.
[0028] In order to improve production efficiency, the steps S1 to S5 are all processed by roll-to-roll processing. The copper foil substrate of step S1 uses a whole roll of copper foil. The substrates of steps S2-S5 are both pulled by guide films, and the front and rear guide films are 8m each. If the length of the pulling film is too short, although the MD expansion and contraction data in the middle is stable, the expansion and contraction data in the etching head and end MD (roll transmission direction) direction are poor, the etching head is small and the end is large, and the head and end MD directions are T-shaped, and the end expansion and contraction is obvious.
[0029] Table 1 is a specific implementation table of the expansion and contraction control project of the present invention:
[0030] Monitor and compare the expansion and contraction: Take 30 PNL from the first section, middle section and last section of the whole roll product, mark 1-30 as the first section, 31-60 as the middle section, and 61-90 as the last section, collect and monitor the data of each PNL and correspond to its corresponding marking sequence. After comparing the expansion and contraction of the existing FPC process with the process of the present invention, it can be concluded that the expansion and contraction of the FPC of the present invention is significantly better than that of the FPC made by the existing process, and the yield of the FPC of the present invention is much higher than that of the FPC made by the existing process.
[0031] The above embodiments do not limit the product form and style of the present invention. Any appropriate changes or modifications made by ordinary technicians in the relevant technical field should be deemed to be within the patent scope of the present invention.
Claims
1. A method for controlling the expansion and contraction of FPC, characterized in that: The following steps are involved: S1. Bake the copper foil substrate and then return it to the temperature to improve the dimensional stability of the substrate, remove moisture from the copper foil substrate, and reduce dimensional changes caused by moisture evaporation during subsequent processing; S2, laser, select laser energy to avoid excessive energy causing excessive heating of the substrate, control the laser speed to ensure even heat distribution; S3, plasma treatment, to clean and activate the surface of the substrate after laser treatment, remove surface pollutants, oxides and organic impurities, improve surface properties, and enhance the bonding force between materials; S4, copper plating, control the current density to avoid local overheating and stress concentration caused by excessive current, control the electroplating time to ensure uniform thickness of the copper plating layer, control the composition of the plating solution to ensure stable performance of the plating solution; S5, etching, control the concentration of the etching solution, keep the concentration of the etching solution stable and appropriate, avoid concentration fluctuations leading to uneven etching rate, control the temperature and time of etching, prevent dimensional changes caused by over-etching or under-etching, ensure that the etching solution is evenly stirred during the etching process, so that the etching reaction proceeds evenly; balance the line distribution, so that the lines are evenly distributed on the FPC; S6. Laminating CVL, controlling the laminating temperature to avoid excessive expansion of the substrate and CVL due to high temperature, or loose bonding due to low temperature; adjusting the pressure to ensure that the CVL and the substrate are tightly fitted to reduce gaps and uneven stress; controlling the laminating time to ensure sufficient time for the adhesive to fully cure; S7, Punching, control the punching speed to avoid excessive heat generated by punching too fast, control the punching pressure, apply pressure evenly to prevent material deformation caused by uneven pressure; S8, grinding, reduce grinding pressure, control grinding speed, use multi-stage grinding, gradually adjust grinding volume, control temperature during grinding, and avoid changes in substrate material properties caused by excessive temperature; S9, ink, apply the ink evenly to avoid large differences in ink thickness; S10, baking, using a hot air circulation oven to ensure uniform temperature distribution in the baking chamber; S11, gold plating, control the temperature and concentration of the chemical gold plating solution to avoid excessive temperature fluctuations; control the concentration of each component in the gold plating solution; S12, PI lamination, control the lamination pressure, ensure that the pressure is evenly distributed in the entire lamination area, so that the PI and the substrate fit tightly; control the lamination time, ensure that there is enough lamination time for the PI material to fully solidify and fuse; S13, punching shape, bake the FPC before punching, design the punching path to make it symmetrical; control the punching speed to avoid excessive impact force caused by too fast speed and deformation of the material; control the punching pressure to complete the punching without over-extruding the material; keep the punching temperature stable.
2. A method for controlling the expansion and contraction of an FPC as claimed in claim 1, characterized in that: In step S12, PI uses PI materials with low thermal expansion coefficient and stable performance, and performs incoming material inspection on PI materials to ensure that their thickness is uniform and free of defects; the pressing temperature is accurately controlled to avoid uneven expansion or contraction caused by excessively high or low temperatures.
3. A method for controlling the expansion and contraction of an FPC as claimed in claim 1, characterized in that: The steps S1 to S5 are all processed by roll-to-roll processing. The copper foil substrate of step S1 is a whole roll of copper foil. The first and last rolls of the substrate of steps S2-S5 are both pulled by guide films, and the front and rear guide films are 8m each.
4. A method for controlling the expansion and contraction of an FPC as claimed in claim 1, characterized in that: There is a black shadow process between step S3 plasma treatment and step S4 copper plating process. Before the black shadow process, the FPC is pre-baked to remove moisture and internal stress.
5. A method for controlling the expansion and contraction of an FPC as claimed in claim 1, characterized in that: There is also an exposure process between step S4 copper plating and S5 etching process, using glass film, the front and rear rolls are pulled by guide films, and the front and rear pulling films are 8m each.
6. A method for controlling the expansion and contraction of an FPC as claimed in claim 1, characterized in that: Step S6: pre-process the CVL before laminating and pressing the CVL, with the arrow in the waste area pointing forward in the board feeding direction.
7. A method for controlling the expansion and contraction of an FPC as claimed in claim 1, characterized in that: The present invention also includes a shrinkage test step, taking 30 PNL from the first section, middle section and last section of the whole roll product, marking 1-30 as the first section, 31-60 as the middle section, and 61-90 as the last section, collecting and monitoring the data of each PNL and corresponding to its corresponding marking sequence.
8. The FPC expansion and contraction control method according to claim 1, characterized in that: Step S12 PI pressing: After preheating with a hot press, a layer of thermosetting film is evenly coated on the substrate, and the PI film is precisely aligned and attached to the film. The temperature is set to 180°C, the pressure is 20 MPa, and the time is 45 minutes for pressing. After pressing, it is naturally cooled for 30 minutes.
Citation Information
Patent Citations
Layer deviation improvement method of multi-layer circuit board
CN107613676A
FPC rolled copper manufacturing process capable of controlling expansion and shrinkage
CN110636709A
Processing method of 5G antenna FPC multilayer board made of high-frequency material
CN115426794A
Manufacturing process of flexible circuit board for power battery
CN116847551A