Bridge production process of electric double-beam crane
By using diamond steel and rebar design in bridges of electric double beam cranes, combined with high-strength materials and multi-layer spraying technology, the weight increase and erosion caused by industrial steel is solved, achieving higher structural strength and longer Service life.
Patent Information
- Application Number
- CN202411170892.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-23
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-08-23
AI Technical Summary
The existing electric double-beam cranes have a large overall weight when using industrial steel, and are susceptible to dust and sea breeze erosion for a long time when working on construction sites or ports, resulting in a reduced service life.
Designed with diamond steel and rebar inside the hollow cavity, optimize the bridge structure to reduce the light by sandblasting, laser cutting, multi-layer spray paint and high-strength welding processes, combined with Q460 or S690 high-strength steel and carbon fiber reinforced plastic materials. Weight and increase strength and corrosion resistance.
It effectively reduces the overall weight of the bridge, while improving structural strength and corrosion resistance, extending the service life of the crane, and reducing maintenance costs and failure rates.
Smart Images

Figure CN119017018A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of cranes, and in particular to a bridge production process for an electric double-beam crane. Background Art
[0002] Electric double-girder bridge crane is a large lifting equipment, commonly used in industrial and warehousing fields. It consists of two main beams to form a bridge structure that can move laterally on the track. The electric double-girder crane has relatively high requirements for process during production. It not only requires precise engineering design and calculation to ensure that the crane can withstand the design load, but also requires high-strength and wear-resistant materials to ensure the long-term stable operation of the crane, and then cooperates with sophisticated manufacturing and assembly processes to ensure the quality and accuracy of each component. Finally, regular maintenance and overhaul are carried out to maintain the long-term safety and efficiency of the crane.
[0003] Most of the traditional crane bridges use I-shaped steel to increase the overall load-bearing effect. However, I-shaped steel is relatively heavy. If used in a bridge, the overall weight of the crane may be higher. If other steel materials are used, the overall load-bearing capacity may be reduced. At the same time, some cranes may work at construction sites or ports, which may cause the exterior to be eroded by dust or sea breeze for a long time, which will reduce the service life of the crane to a certain extent. Therefore, a bridge production process for an electric double-beam crane is proposed. Summary of the invention
[0004] 1. Technical issues to be solved
[0005] In view of the deficiencies in the prior art, the present invention provides a bridge production process for an electric double-beam crane, which solves the problems that the existing use of I-shaped steel will increase the overall weight of the crane beam to a certain extent, and the long-term operation of the crane at a construction site or port may cause the crane to be corroded by dust and salt contained in the sea breeze, thereby reducing its service life.
[0006] (II) Technical solution
[0007] To achieve the above objectives, the present invention is implemented through the following technical solutions:
[0008] A bridge production process for an electric double-beam crane, comprising a bridge assembly, wherein the bridge assembly comprises a bridge frame, wherein a hollow cavity is provided inside the bridge frame, wherein four corners inside the hollow cavity are fixedly connected with triangular steels, wherein diamond steels are arranged inside the hollow cavity, wherein four outer walls of the diamond steels are fixedly connected with threaded steels, wherein one end of the threaded steels away from the diamond rods is fixedly connected with the inner wall of the hollow cavity;
[0009] Through the above technical solution, the design of using diamond steel and threaded steel inside the hollow cavity helps to effectively disperse the load and enhance the overall structural strength and stability of the bridge. This design can improve the performance of the bridge under high load conditions and ensure its safety and reliability.
[0010] Further, the following steps are included:
[0011] S1. Design stage: Design drawings according to customer needs and mark detailed dimensions, materials and specifications on the drawings;
[0012] S2. Material selection: Select appropriate raw materials according to the design drawings, then measure and inspect them and mark them according to the size and specifications of the design drawings. If the raw material sheet is not flat enough, it needs to be leveled by a leveler and finally put into storage for standby;
[0013] S3. Rust removal of materials: First, use a sandblaster to preliminarily remove the rust on the surface of the raw material plate. The sandblasting process can quickly remove large areas of rust and old coatings, and then use ultrasonic rust removal technology to treat small parts and complex shapes;
[0014] S4. Cutting pretreatment: Select water jet cutting machine or laser cutting machine for cutting according to the thickness of the plate in the design drawing. After cutting, remove the residues in the welding part, grind the welding groove, and drill holes at the corresponding positions according to the drawing;
[0015] S5. Spraying paint layer: Before spraying, the dust on the surface of the raw materials needs to be blown away, and the ambient temperature and humidity need to be controlled. Then use a high-pressure airless spray gun to spray a layer of epoxy zinc-rich primer with a thickness of 30μm. After the epoxy zinc-rich primer is air-dried, spray two layers of epoxy micaceous iron thick paste intermediate paint with a single layer thickness of 80μm. It is best to spray two layers of polyurethane topcoat with a single layer thickness of 27μm. When spraying the paint layer, a paint spraying robot is used for automatic spraying, and the spraying error is ±5μm;
[0016] S6. Welding assembly: In the assembly workshop or production line, the rebars are welded to the four outer walls of the diamond steel respectively, and then the rebars on the two sides of the diamond steel are welded to one of the plates. Then the cut and processed materials are positioned and pre-assembled according to the design drawings, and fixtures and positioning devices are used to ensure the precise alignment of each part, and other structural parts are welded to connect the various parts. The welding process includes arc welding, gas shielded welding, etc. During the welding process, the heat input needs to be controlled to avoid deformation and stress concentration. Finally, a self-propelled welding robot is used to enter the bridge frame welded by four plates to weld the rebars on the remaining two sides of the diamond steel;
[0017] S7. Quality inspection: After welding is completed, the weld is inspected, including visual inspection and non-destructive testing, to ensure that the welding quality meets the standards;
[0018] Through the above technical scheme, in step S5, each coat of paint should be sprayed after the upper coat of paint is dry, and can be detected by touch method or drying instrument to avoid the problem of paint peeling due to spraying the next coat of paint when the upper coat is not completely dry, and non-destructive testing can use ultrasonic testing and X-ray testing.
[0019] Furthermore, the diamond steel is Q460 or S690 high-strength steel, and the diamond steel contains carbon fiber reinforced plastic;
[0020] Through the above technical solution, by using Q460 or S690 high-strength steel as the diamond steel, it is possible to reduce weight while maintaining the same or higher strength. Furthermore, by containing carbon fiber reinforced plastic in the composition of the diamond steel, it is possible to improve strength and rigidity without significantly increasing weight.
[0021] Furthermore, the sandblasting machine in step S3 should use hard and angular corundum, quartz sand, or siliceous river sand, the water content of which should not be greater than 1%, and the use of sea sand is strictly prohibited;
[0022] According to the above technical solution, the sandblasting machine in step S3 should use hard and angular corundum, quartz sand, and siliceous river sand, and the water content should not be greater than 1%, thereby avoiding excessive wear of the raw material plate due to sand problems.
[0023] Further, in step S5, the ambient temperature is 10° C. to 38° C., and the maximum relative humidity is 85%;
[0024] Through the above technical solution, the ambient temperature in step S5 is 10° C. to 38° C. and the maximum relative humidity is 85%, thereby avoiding problems with paint surface quality caused by environmental problems.
[0025] Further, in step S5, the pressure of the high-pressure airless spray gun is between 7-15 MPa, and the distance between the high-pressure airless spray gun and the surface of the workpiece is between 15-30 cm;
[0026] Through the above technical solution, the pressure of the high-pressure airless spray gun in step S5 is between 7-15MPa, so as to provide a more uniform coating. The distance between the high-pressure airless spray gun and the surface of the workpiece is between 15-30cm, which avoids uneven coating thickness caused by too close distance and serious atomization of the paint caused by too far distance, thereby affecting the coating quality.
[0027] (III) Beneficial effects
[0028] The present invention provides a bridge production process for an electric double-beam crane, which has the following beneficial effects:
[0029] 1. The present invention provides a bridge production process for an electric double-beam crane, in which I-shaped steel is replaced with diamond steel. Since the weight of the diamond steel after material optimization is usually lighter and the strength remains unchanged, and the weight of the I-shaped steel depends on its cross-sectional size and thickness, the diamond steel can significantly reduce the overall weight of the bridge. Then, a plurality of threaded steel bars are fixed to each outer wall of the diamond steel, so that each inner wall of the hollow cavity forms a triangle with the diamond steel, thereby reducing the overall weight while improving the supporting strength.
[0030] 2. The present invention provides a bridge production process for an electric double-beam crane. The process is simple and reasonable, and greatly improves the rigidity of the crane bridge. Through arc welding and gas shielded welding, the welding deformation is small, the weld strength is high, and the residual stress is small, thereby improving the load-bearing capacity of the crane, extending the service life, reducing the manufacturing cost, and improving the economic benefits of the enterprise.
[0031] 3. The present invention provides a bridge production process for an electric double-beam crane. Through a multi-layer spraying process, the corrosion resistance of the bridge components is significantly improved, which can effectively extend the service life of the crane and reduce the maintenance cost of later use. Moreover, this production process can effectively improve the overall quality and performance of the bridge components of the electric double-beam crane and reduce the failure rate. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 It is a partial axial section view of the present invention;
[0033] Figure 2 It is a front view of the present invention.
[0034] Among them, 1. bridge component; 101. bridge frame; 102. hollow cavity; 103. diamond steel; 104. triangle plate; 105. threaded steel. DETAILED DESCRIPTION
[0035] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0036] Example:
[0037] A bridge production process for an electric double-beam crane includes a bridge component 1, wherein the bridge component 1 includes a bridge frame 101, wherein a hollow cavity 102 is provided inside the bridge frame 101, wherein four corners inside the hollow cavity 102 are fixedly connected with triangular steels 104, wherein a diamond steel 103 is provided inside the hollow cavity 102, wherein four outer walls of the diamond steel 103 are fixedly connected with threaded steels 105, wherein one end of the threaded steel 105 away from the diamond rod 103 is fixedly connected with the inner wall of the hollow cavity 102;
[0038] The design of using diamond steel 103 and threaded steel 105 inside the hollow cavity 102 helps to effectively disperse the load and enhance the overall structural strength and stability of the bridge. This design can improve the performance of the bridge under high load conditions and ensure its safety and reliability.
[0039] The following steps are involved:
[0040] S1. Design stage: Design drawings according to customer needs and mark detailed dimensions, materials and specifications on the drawings;
[0041] S2. Material selection: Select appropriate raw materials according to the design drawings, then measure and inspect them and mark them according to the size and specifications of the design drawings. If the raw material sheet is not flat enough, it needs to be leveled by a leveler and finally put into storage for standby;
[0042] S3. Rust removal of materials: First, use a sandblaster to preliminarily remove the rust on the surface of the raw material plate. The sandblasting process can quickly remove large areas of rust and old coatings, and then use ultrasonic rust removal technology to treat small parts and complex shapes;
[0043] S4. Cutting pretreatment: Select water jet cutting machine or laser cutting machine for cutting according to the thickness of the plate in the design drawing. After cutting, remove the residues in the welding part, grind the welding groove, and drill holes at the corresponding positions according to the drawing;
[0044] S5. Spraying paint layer: Before spraying, the dust on the surface of the raw materials needs to be blown away, and the ambient temperature and humidity need to be controlled. Then use a high-pressure airless spray gun to spray a layer of epoxy zinc-rich primer with a thickness of 30μm. After the epoxy zinc-rich primer is air-dried, spray two layers of epoxy micaceous iron thick paste intermediate paint with a single layer thickness of 80μm. It is best to spray two layers of polyurethane topcoat with a single layer thickness of 27μm. When spraying the paint layer, a paint spraying robot is used for automatic spraying, and the spraying error is ±5μm;
[0045] S6. Welding assembly: In the assembly workshop or production line, the rebar 105 is welded to the four outer walls of the diamond steel 103 respectively, and then the rebar 105 on two sides of the diamond steel 103 is welded to one of the plates, and then the cut and processed materials are positioned and pre-assembled according to the design drawings, and the clamps and positioning devices are used to ensure the precise alignment of each part, and other structural parts are welded to connect the various parts. The welding process includes arc welding, gas shielded welding, etc. During the welding process, the heat input needs to be controlled to avoid deformation and stress concentration. Finally, a self-propelled welding robot is used to enter the bridge frame 101 welded by four plates to weld the rebar 105 on the remaining two sides of the diamond steel 103;
[0046] S7. Quality inspection: After welding is completed, the weld is inspected, including visual inspection and non-destructive testing, to ensure that the welding quality meets the standards;
[0047] In step S5, each coat of paint should be sprayed after the upper coat of paint is dry. The touch method or drying instrument can be used for detection to avoid the problem of paint peeling due to the spraying of the next coat of paint when the upper coat is not completely dry. In addition, ultrasonic detection and X-ray detection can be used for non-destructive testing.
[0048] The diamond steel 103 is Q460 or S690 high-strength steel, and the diamond steel 103 contains carbon fiber reinforced plastic. By using Q460 or S690 high-strength steel, the weight can be reduced while maintaining the same or higher strength. By containing carbon fiber reinforced plastic in the composition of the diamond steel 103, the strength and rigidity can be improved without significantly increasing the weight.
[0049] In step S3, the sandblasting machine should use hard and angular corundum, quartz sand, and siliceous river sand, and the water content thereof should not be greater than 1%. It is strictly forbidden to use sea sand. In step S3, the sandblasting machine should use hard and angular corundum, quartz sand, and siliceous river sand, and the water content thereof should not be greater than 1%, thereby avoiding excessive wear of the raw material plate due to sand problems.
[0050] In step S5, the ambient temperature is 10° C. to 38° C., and the maximum relative humidity is 85%. By setting the ambient temperature in step S5 to 10° C. to 38° C., and the maximum relative humidity is 85%, problems with paint surface quality caused by environmental problems are avoided.
[0051] In step S5, the pressure of the high-pressure airless spray gun is between 7-15MPa, and the distance between the high-pressure airless spray gun and the surface of the workpiece is between 15-30cm. By setting the pressure of the high-pressure airless spray gun between 7-15MPa in step S5, a more uniform coating is provided. By setting the distance between the high-pressure airless spray gun and the surface of the workpiece between 15-30cm, it is avoided that the coating thickness may be uneven due to a close distance, and the coating may be seriously atomized due to a long distance, thereby affecting the coating quality.
[0052] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A bridge production process for an electric double-beam crane, comprising a bridge assembly (1), characterized in that: The bridge assembly (1) comprises a bridge frame (101), a hollow cavity (102) is provided inside the bridge frame (101), four corners inside the hollow cavity (102) are fixedly connected with triangular steels (104), a diamond steel (103) is arranged inside the hollow cavity (102), four outer walls of the diamond steel (103) are fixedly connected with threaded steels (105), and one end of the threaded steel (105) away from the diamond rod (103) is fixedly connected to the inner wall of the hollow cavity (102).
2. The bridge production process of an electric double-beam crane according to claim 1 is characterized in that: The following steps are involved: S1. Design stage: Design drawings according to customer needs and mark detailed dimensions, materials and specifications on the drawings; S2. Material selection: Select appropriate raw materials according to the design drawings, then measure and inspect them and mark them according to the size and specifications of the design drawings. If the raw material sheet is not flat enough, it needs to be leveled by a leveler and finally put into storage for standby; S3. Rust removal of materials: First, use a sandblaster to preliminarily remove the rust on the surface of the raw material plate. The sandblasting process can quickly remove large areas of rust and old coatings, and then use ultrasonic rust removal technology to treat small parts and complex shapes; S4. Cutting pretreatment: Select water jet cutting machine or laser cutting machine for cutting according to the thickness of the plate in the design drawing. After cutting, remove the residues in the welding part, grind the welding groove, and drill holes at the corresponding positions according to the drawing; S5. Spraying paint layer: Before spraying, the dust on the surface of the raw materials needs to be blown away, and the ambient temperature and humidity need to be controlled. Then use a high-pressure airless spray gun to spray a layer of epoxy zinc-rich primer with a thickness of 30μm. After the epoxy zinc-rich primer is air-dried, spray two layers of epoxy micaceous iron thick paste intermediate paint with a single layer thickness of 80μm. It is best to spray two layers of polyurethane topcoat with a single layer thickness of 27μm. When spraying the paint layer, a paint spraying robot is used for automatic spraying, and the spraying error is ±5μm; S6. Welding assembly: In an assembly workshop or production line, the threaded steel (105) is welded to the four outer walls of the diamond steel (103) respectively, and then the threaded steel (105) on two sides of the diamond steel (103) is welded to one of the plates, and then the cut and processed materials are positioned and pre-assembled according to the design drawings, and fixtures and positioning devices are used to ensure that each part is accurately aligned, and other structural parts are welded to connect the various parts. The welding process includes arc welding, gas shielded welding, etc. During the welding process, it is necessary to control the heat input to avoid deformation and stress concentration. Finally, a self-propelled welding robot is used to enter the bridge frame (101) welded by four plates to weld the threaded steel (105) on the remaining two sides of the diamond steel (103); S7. Quality inspection: After welding is completed, weld inspection is carried out, including visual inspection and non-destructive testing, to ensure that the welding quality meets the standards.
3. The bridge production process of an electric double-beam crane according to claim 1 is characterized in that: The diamond steel (103) is Q460 or S690 high-strength steel, and the diamond steel (103) contains carbon fiber reinforced plastic.
4. The bridge production process of an electric double-beam crane according to claim 2 is characterized in that: In step S3, the sandblasting machine should use hard and angular corundum, quartz sand, or siliceous river sand, the water content of which should not be greater than 1%, and it is strictly forbidden to use sea sand.
5. The bridge production process of an electric double-beam crane according to claim 2 is characterized in that: In step S5, the ambient temperature is 10° C. to 38° C., and the maximum relative humidity is 85%.
6. The bridge production process of an electric double-beam crane according to claim 2, characterized in that: In step S5, the pressure of the high-pressure airless spray gun is between 7-15 MPa, and the distance between the high-pressure airless spray gun and the surface of the workpiece is between 15-30 cm.
Citation Information
Patent Citations
Steel structure bridge and processing technology thereof
CN111549650A
Processing technology of prefabricated bridge structure
CN116277470A
Method for manufacturing steel-made internal mould of hollow beam for bridge
CN1775398A
Bridge girder, bridge girder part and process for constructing bridge girder
EP0841434A1
Long span bridge building structure and the method of manufacturing long span bridge building
KR101857275B1