Collimation device of physical vapor deposition equipment and physical vapor deposition equipment
By designing a collimator with adjustable cross-sectional area of the hollow part in a physical vapor deposition device, the problem of limited application scope of existing collimators is solved, and the optimal coverage of holes and grooves with multiple aspect ratio characteristics is achieved. improves production efficiency and machine utilization.
Patent Information
- Application Number
- CN202310595436.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-24
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2043-05-24
AI Technical Summary
The existing collimator can only be used for holes and grooves with a single aspect ratio feature, and cannot adapt to wafers with a variety of different aspect ratio features, resulting in poor bottom coverage and time-consuming replacement of collimator, which affects the impact of Production efficiency and machine utilization.
Design a collimating device for a physical vapor deposition device, including a first collimator and a second collimator, to adjust the transverse of the overlapping portion of the hollow part by stacking it in a process chamber and allowing it to move in a plane The cross-sectional area is adapted to holes and grooves with different depth and aspect ratio characteristics, and achieves the matching of multiple depth and aspect ratios.
The optimal bottom coverage of holes and groove wafers with various aspect ratio features is achieved without changing collimators, improving production efficiency and machine utilization.
Smart Images

Figure CN119020736A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor manufacturing, and in particular to an alignment device of a physical vapor deposition device and a physical vapor deposition device. Background Art
[0002] With the development of integrated circuits, the scale of the semiconductor devices they contain is still expanding, and the circuit density continues to increase, while the size of the devices needs to be continuously reduced, resulting in the width of interconnects (such as through holes, trenches, contacts and gates, etc.) being reduced and the aspect ratio being increased, which in turn poses increasing challenges to the manufacture of these structures.
[0003] Physical vapor deposition (PVD) is a widely used technology for wafer metal film deposition, with high deposition efficiency and good film density. However, due to the completely random sputtering direction of its particles, it is difficult to ensure that a film of uniform thickness is produced everywhere on the wafer, and it is easy to produce overhangs at the corners of high aspect ratio features, further reducing the feature width, and even causing premature blockage and defects such as pores, affecting the conductivity of the area.
[0004] A collimator is a device that can significantly improve the collimation of particles and the ability of PVD thin film deposition to fill high aspect ratio features. The device is usually a thin wall with equal thickness and includes some through holes that can pass through the thin wall. It can filter out particles with a large angle between the target and the wafer. Only particles that are close to vertical can reach the wafer surface, thereby improving the step coverage of the groove.
[0005] However, existing collimators only have a single aperture and aspect ratio, and cannot be applied to wafers with holes and grooves with different aspect ratios to achieve optimal bottom coverage. If a collimator with another aperture needs to be replaced, the chamber will have a long maintenance time, seriously affecting production efficiency and machine utilization. Summary of the invention
[0006] The present invention aims to solve at least one of the technical problems existing in the prior art, and proposes an alignment device for a physical vapor deposition device and a physical vapor deposition device, which can be applicable to wafers with various holes and grooves with different aspect ratios, so as to achieve the optimal bottom coverage, and there is no need to replace the collimator, thereby improving production efficiency and machine utilization.
[0007] To achieve the purpose of the present invention, a collimation device of a physical vapor deposition device is provided, comprising a first collimator and a second collimator, wherein the first collimator and the second collimator are both arranged in a process chamber of the physical vapor deposition device and are stacked between a target material and a base in the process chamber;
[0008] The first collimator has a plurality of first hollow parts, the second collimator has a plurality of second hollow parts, and each of the first hollow parts and each of the second hollow parts are arranged correspondingly;
[0009] The first collimator and / or the second collimator can move within the plane where the first collimator is located, so as to adjust the cross-sectional area of the overlapping portion between each of the first hollow portions and the corresponding each of the second hollow portions.
[0010] Optionally, the first collimator is fixedly connected to a shielding member in the process chamber, and the second collimator is movably connected to the shielding member along a radial direction of the process chamber.
[0011] Optionally, the first collimator includes a first annular sidewall and a first grid structure, wherein the first grid structure is located in a space defined by the first annular sidewall and connected to the first annular sidewall; grids in the first grid structure constitute the first hollow portion;
[0012] The first annular side wall is fixedly connected to the shielding component, and the outer circumferential surface of the first annular side wall is in contact with the inner circumferential surface of the shielding component.
[0013] Optionally, the second collimator includes a second annular sidewall and a second grid structure, the second grid structure is located in the space defined by the second annular sidewall and connected to the second annular sidewall; the grids in the second grid structure constitute the second hollow portion;
[0014] The second annular side wall is connected to the shielding member so as to be movable along a radial direction of the process chamber.
[0015] Optionally, the radial thickness of the second annular side wall is smaller than the radial thickness of the first annular side wall, and when the cross-sectional area of the overlapping portion of each first hollow portion and the corresponding second hollow portion is the largest, the orthographic projection of the second annular side wall on the radial cross section of the process chamber completely falls into the orthographic projection of the first annular side wall on the radial cross section of the process chamber.
[0016] Optionally, the second collimator further includes a first fixing portion and a second fixing portion, and the first fixing portion and the second fixing portion are arranged opposite to each other along any diameter direction of the second annular side wall;
[0017] One end of the first fixing portion is fixedly connected to the outer circumferential surface of the second annular side wall, and the other end is used to pass through the first through hole of the shielding member along the diameter direction and extend outside the shielding member, and is used to be connected to a driving member; the driving member is used to drive the first fixing portion to move along the diameter direction;
[0018] One end of the second fixing portion is fixedly connected to the outer circumferential surface of the second annular side wall, and the other end is used to be movably inserted into the second through hole of the shielding member along the diameter direction.
[0019] Optionally, the driving member includes a transmission shaft and a driving source, wherein one end of the transmission shaft is connected to the other end of the first fixed part, the other end of the transmission shaft passes through the chamber wall of the process chamber and extends outside the process chamber, and is connected to the driving source; the driving source is used to drive the first fixed part to move along the diameter direction through the transmission shaft.
[0020] Optionally, the first collimator is located between the second collimator and the target material; and the thickness of the first collimator at different positions is consistent.
[0021] Optionally, the first collimator is located between the second collimator and the target; the thickness of the second collimator at different positions is consistent; or,
[0022] The thickness of the second collimator increases from the outer edge to the center according to a preset rule.
[0023] Optionally, the preset rules include:
[0024] The thickness of the second collimator increases from the outer edge to the center first and then remains unchanged; or, the thickness of the second collimator increases linearly from the outer edge to the center; or, the thickness of the second collimator increases segmentally from the outer edge to the center.
[0025] Optionally, the mesh wall of at least one of the first mesh structure and the second mesh structure is set to have the same thickness, or the thickness increases gradually along the axial direction of the process chamber toward the base; or,
[0026] A tapered portion is provided at one end of the grid wall of at least one of the first grid structure and the second grid structure away from the base, and an axial cross-section of the tapered portion has an arc shape, a triangle, or a trapezoid.
[0027] Optionally, when the cross-sectional area of the overlapping portion of each of the first hollow portions and the corresponding each of the second hollow portions is the largest, the orthographic projections of each of the first hollow portions and the corresponding each of the second hollow portions on the radial cross section of the process chamber completely overlap.
[0028] Optionally, the aspect ratio of the first hollow portion is greater than or equal to 1:2 and less than or equal to 1:1.
[0029] Optionally, the aspect ratio of the second hollow portion distributed in the central area of the second collimator is greater than or equal to 3:1 and less than or equal to 1:1; the aspect ratio of the second hollow portion distributed in the edge area of the second collimator is greater than or equal to 1:2 and less than or equal to 1:1.
[0030] Optionally, the first collimator and the second collimator are arranged at intervals along the axial direction of the process chamber.
[0031] As another technical solution, the present invention further provides a physical vapor deposition device, including a process chamber, in which a target material and a base arranged below the target material are arranged, and also includes the above-mentioned alignment device provided by the present invention.
[0032] The present invention has the following beneficial effects:
[0033] The collimation device of the physical vapor deposition equipment provided by the present invention can adjust the cross-sectional area of the overlapping part of each first hollow part and the corresponding second hollow part by stacking a first collimator and a second collimator between a target material and a base in a process chamber, and enable the first collimator and / or the second collimator to move within the plane where the first collimator and / or the second collimator are located, so as to adjust the aspect ratio of the overlapping part, so as to match with a variety of wafers with holes and grooves having different aspect ratio characteristics by adjusting the aspect ratio, so as to achieve the optimal bottom coverage, and there is no need to replace the collimator, thereby improving the production efficiency and machine utilization.
[0034] The physical vapor deposition equipment provided by the present invention can be applied to wafers with various holes and grooves with different aspect ratios by adopting the above-mentioned collimation device provided by the present invention, so as to achieve the optimal bottom coverage, and there is no need to replace the collimator, thereby improving production efficiency and machine utilization. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] Figure 1 A cross-sectional view of a physical vapor deposition apparatus provided by an embodiment of the present invention;
[0036] Figure 2 A radial cross-sectional view of a first collimator used in an embodiment of the present invention;
[0037] Figure 3 A radial cross-sectional view of a second collimator used in an embodiment of the present invention;
[0038] Figure 4 An axial cross-sectional view of a first collimator used in an embodiment of the present invention;
[0039] Figure 5 Four structural diagrams of the first grid structure used in the embodiments of the present invention;
[0040] Figure 6 An axial cross-sectional view of a second collimator used in an embodiment of the present invention;
[0041] Figure 7 Four structural diagrams of the second collimator used in the embodiments of the present invention;
[0042] Figure 8 A partial enlarged view of a driving member used in an embodiment of the present invention;
[0043] Fig. 9 A diagram of a process of relative movement of a first collimator and a second collimator used in an embodiment of the present invention;
[0044] Fig.10 Another process diagram of relative movement of a first collimator and a second collimator used in an embodiment of the present invention;
[0045] Fig.11 This is another process diagram of relative movement of a first collimator and a second collimator adopted in an embodiment of the present invention. DETAILED DESCRIPTION
[0046] In order to enable those skilled in the art to better understand the technical solution of the present invention, the alignment device of the physical vapor deposition device and the physical vapor deposition device provided by the present invention are described in detail below with reference to the accompanying drawings.
[0047] Please also read Figures 1 to 11 The collimation device 109 of the physical vapor deposition equipment 100 provided in an embodiment of the present invention includes a first collimator 1 and a second collimator 2. The first collimator 1 and the second collimator 2 are both arranged in the process chamber 101 of the physical vapor deposition equipment 100, and are stacked between the target 102 and the base 103 in the process chamber 101, for example, they can be located near the target 102. It should be noted that the above-mentioned "stacked" means that there is an overlapping area between the orthographic projections of the first collimator 1 and the second collimator 2 on the radial cross-section of the process chamber. The first collimator 1 and the second collimator 2 can be spaced apart in the axial direction of the process chamber, so that relative movement between the two can be achieved. However, the first collimator 1 and the second collimator 2 can also be stacked so as to be relatively movable.
[0048] The first collimator 1 has a plurality of first hollow portions 13, and the second collimator 2 has a plurality of second hollow portions 23. Each first hollow portion 13 and each second hollow portion 23 are arranged correspondingly, and the first collimator 1 and / or the second collimator 2 can move in its own plane, which is, for example, perpendicular to the axial direction of the process chamber 101 (i.e., parallel to the axial direction of the process chamber 101). Figure 1 The vertical direction) is used to adjust the cross-sectional area of the overlapping portion of each first hollow portion 13 and the corresponding second hollow portion 23, so that the aspect ratio of the overlapping portion can be adjusted.
[0049] Specifically, each first hollow portion 13 and each second hollow portion 23 are used to filter particles that are sputtered from the target 102 and move toward the base 103, and the moving direction is outside the specified angle range, so that the particles sputtered from the target 102 can be screened twice, that is, only the particles that pass through the first hollow portion 13 and the second hollow portion 23 can fall smoothly on the surface of the wafer W, that is, the particles fall on the surface of the wafer W through the overlapping parts of each first hollow portion 13 and the corresponding second hollow portion 23. Since the sputtering direction of the particles sputtered from the target 102 is completely random, it is necessary to use the collimator 109 to filter out the particles with a large angle between the target 102 and the wafer, and only particles that are close to vertical can reach the surface of the wafer W to improve the step coverage of the groove. The above-mentioned first hollow portion 13 and second hollow portion 23 are both used to allow particles within a specified angle range to pass through, and the specified angle range is related to the aspect ratio of the overlapping parts of each first hollow portion 13 and the corresponding second hollow portion 23. The larger the aspect ratio, the larger the specified angle range, which is suitable for wafers with holes and grooves with relatively small aspect ratio features; conversely, the smaller the aspect ratio, the smaller the specified angle range, which is suitable for wafers with holes and grooves with relatively large aspect ratio features.
[0050] In some optional embodiments, when the cross-sectional area of the overlapping portion of each first hollow portion 13 and each second hollow portion 23 is the largest, the orthographic projections of each first hollow portion 13 and the corresponding second hollow portion 23 on the radial cross section of the process chamber 101 completely overlap. In other words, the orthographic projections of each first hollow portion 13 and the corresponding second hollow portion 23 on the radial cross section of the process chamber 101 have the same shape and size, so that each first hollow portion 13 and the corresponding second hollow portion 23 can completely overlap, so as to maximize the aspect ratio of the overlapping portion.
[0051] In some optional embodiments, the shape of the orthographic projection of the first hollow portion 13 and the second hollow portion 23 on the radial cross section of the process chamber 101 includes, for example, a circle, a polygon, or any other shape. Further optionally, the polygon may be a triangle, a quadrilateral (such as a square, a rectangle), a hexagon, etc. Taking the shape of the orthographic projection of the first hollow portion 13 and the second hollow portion 23 on the radial cross section of the process chamber 101 as a square as an example, Fig. 9 The left figure in the figure shows that the relative positions of each first hollow portion 13 and each second hollow portion 23 are located at a position where the cross-sectional area of the overlapping portion is the largest (i.e., position 1). At this position 1, each first hollow portion 13 and the corresponding second hollow portion 23 can completely overlap, and the cross-sectional area of the overlapping portion is A; Fig. 9 The right figure in the figure shows that the first collimator 1 and / or the second collimator 2 is located at the position 1 with the largest cross-sectional area, along the specified diameter direction in the plane where the first collimator 1 and / or the second collimator 2 are located (for example Fig. 9When the first hollow portions 13 and the corresponding second hollow portions 23 move a certain distance in a direction parallel to the diagonal O of the square, each first hollow portion 13 and the corresponding second hollow portions 23 do not completely overlap, and for each first hollow portion 13, it will be further divided into a plurality of smaller sub-hollow portions by the side walls that constitute the incompletely overlapping second hollow portions 23. These sub-hollow portions constitute new overlapping portions of each first hollow portion 13 and the corresponding second hollow portions 23, and the cross-sectional area A1 of the new overlapping portion is significantly reduced (for example, reduced to about 1 / 4 of the original cross-sectional area A), thereby realizing the adjustment of the depth-to-width ratio of the overlapping portion.
[0052] Taking the shape of the orthographic projection of the first hollow portion 13 and the second hollow portion 23 on the radial cross section of the process chamber 101 as an example, Fig.10 The left figure shows that the relative positions of each first hollow portion 13 and each second hollow portion 23 are located at the position where the cross-sectional area of the overlapping portion is the largest (i.e., position 1). At this position 1, each first hollow portion 13 and the corresponding second hollow portion 23 can completely overlap, and the cross-sectional shape of the overlapping portion is a hexagon, and the cross-sectional area of the overlapping portion is A; Fig.10 The right figure shows that when the first collimator 1 and / or the second collimator 2 moves a certain distance from the position 1 with the largest cross-sectional area mentioned above, along the specified diameter direction in the plane where the first collimator 1 and / or the second collimator 2 are located (for example, along the diameter direction O inclined 45° to the left in the plane parallel to the paper surface), each first hollow portion 13 and the corresponding second hollow portion 23 do not completely overlap, and for each first hollow portion 13, it will be further divided into a plurality of smaller sub-hollow portions by the side walls that constitute the incompletely overlapping second hollow portions 23. These sub-hollow portions constitute new overlapping portions of each first hollow portion 13 and each corresponding second hollow portion 23. The cross-sectional shape of the new overlapping portion is mainly a parallelogram or a rhombus (there are also a small number of special shapes), and the cross-sectional area A1 is significantly reduced (for example, reduced to about 1 / 3 of the original cross-sectional area A), thereby realizing the adjustment of the depth-to-width ratio of the overlapping portion.
[0053] For example, the shape of the orthographic projection of the first hollow portion 13 and the second hollow portion 23 on the radial cross section of the process chamber 101 is a triangle. Fig.11 The left figure shows that the relative positions of each first hollow portion 13 and each second hollow portion 23 are located at a position where the cross-sectional area of the overlapping portion is the largest (i.e., position 1). At this position 1, each first hollow portion 13 and the corresponding second hollow portion 23 can completely overlap, and the cross-sectional shape of the overlapping portion is a triangle, and the cross-sectional area of the overlapping portion is A; Figure 2When the first collimator 1 and / or the second collimator 2 moves a certain distance from the above-mentioned position with the largest cross-sectional area along the specified diameter direction in its own plane (for example, along the diameter direction O inclined 45° to the left in the plane parallel to the paper surface), each first hollow portion 13 and the corresponding second hollow portion 23 do not completely overlap, and for each first hollow portion 13, it will be further divided into a plurality of smaller sub-hollow portions by the incompletely overlapping side walls constituting the second hollow portion 23. These sub-hollow portions constitute new overlapping portions of each first hollow portion 13 and each corresponding second hollow portion 23. The cross-sectional shape of the new overlapping portion is mainly a triangle, a parallelogram or a rhombus (there are also a small number of special shapes), and the cross-sectional area A1 is significantly reduced (for example, reduced to about 1 / 3 of the original cross-sectional area A), thereby realizing the adjustment of the depth-to-width ratio of the overlapping portion.
[0054] The embodiment of the present invention stacks the first collimator 1 and the second collimator 2 between the target 102 and the base 103 in the process chamber 101, and enables the first collimator 1 and / or the second collimator 2 to move within the plane where the first collimator 1 and / or the second collimator 2 are located, thereby adjusting the cross-sectional area of the overlapping portion of each first hollow portion 13 and the corresponding second hollow portion 23 to adjust the aspect ratio of the overlapping portion, so that the aspect ratio can be adjusted to match a variety of wafers with holes and grooves with different aspect ratio characteristics, so as to achieve the optimal bottom coverage, and there is no need to replace the collimator, thereby improving production efficiency and machine utilization.
[0055] In some optional embodiments, such as Figure 2 As shown, the first collimator 1 is fixedly connected to the shielding member 104 in the process chamber 101, and the second collimator 2 is connected to the shielding member 104 so as to be movable along the radial direction of the process chamber 101. In this case, the first collimator 1 is fixed relative to the process chamber 101, and the cross-sectional area of the overlapping portion of each first hollow portion 13 and the corresponding second hollow portion 23 can be adjusted by only moving the second collimator 2 along the radial direction of the process chamber 101.
[0056] In some optional embodiments, such as Figure 2As shown, the first collimator 1 includes a first annular sidewall 11 and a first grid structure 12, wherein the first grid structure 12 is located in the space defined by the first annular sidewall 11 and connected to the first annular sidewall 11. The grid in the first grid structure 12 constitutes a first hollow portion 13 (i.e., a through hole); the first annular sidewall 11 is used to be fixedly connected to the shielding member 104 in the process chamber 101, and the outer peripheral surface of the first annular sidewall 11 is in contact with the inner peripheral surface of the shielding member 104. The above-mentioned first grid structure 12 is a grid-like structure composed of multiple thin walls. Taking the shape of the positive projection of the first hollow portion 13 and the second hollow portion 23 on the radial section of the process chamber 101 as a square as an example, four thin walls can be enclosed into a square grid, i.e., the first hollow portion 13. Each thin wall has a certain height. When the particles move downward, the particles with too large an angle will collide with the thin wall and adhere to it, i.e., the particle filtering effect is achieved. The first annular side wall 11 is used to fix all the thin walls. Optionally, the first annular side wall 11 is integrally formed with the first grid structure 12. In addition, by fixing the first annular side wall 11 to the shielding member 104 in the process chamber 101, the first collimator 1 can be fixed in the process chamber 101, and the first collimator 1 can be fixed. At the same time, by making the outer circumference of the first annular side wall 11 fit the inner circumference of the shielding member 104, the gap between the outer circumference of the first annular side wall 11 and the inner circumference of the shielding member 104 can be blocked to prevent particles from passing directly through this position. It is easy to understand that if the first collimator 1 is fixed, the second collimator 2 needs to move in its own plane relative to the first collimator 1. Optionally, the first annular side wall 11 can be integrally formed or welded with the shielding member 104.
[0057] In some optional embodiments, such as Figure 3As shown, the second collimator 2 includes a second annular side wall 21 and a second grid structure 22, wherein the second grid structure 22 is located in the space defined by the second annular side wall 21 and is connected to the second annular side wall 21; the grid in the second grid structure 22 constitutes a second hollow portion 23 (i.e., a through hole); the second annular side wall 21 is connected to the shielding member 104 so as to be movable along the radial direction of the process chamber 101. Similar to the first grid structure 12, the second grid structure 22 is a grid-like structure composed of a plurality of thin walls. For example, the shape of the orthographic projection of the first hollow portion 13 and the second hollow portion 23 on the radial cross section of the process chamber 101 is a square, and four thin walls can be combined to form a square grid, i.e., the second hollow portion 23. The second annular side wall 21 is used to fix all the thin walls. Optionally, the second annular side wall 21 and the second grid structure 22 are integrally formed. In addition, by connecting the second annular side wall 21 and the shielding member 104 so as to be movable along the radial direction of the process chamber 101 , the second collimator 2 can be fixed in the process chamber 101 through the shielding member 104 and can also be moved relative to the first collimator 1 in the process chamber 101 .
[0058] Further optionally, the radial thickness of the second annular side wall 21 is smaller than the radial thickness of the first annular side wall 11, and the cross-sectional area of the overlapping portion of each first hollow portion 13 and each second hollow portion 23 is the largest (for example, at Figures 9 to 11 When the shield 104 is at position 1 in the left figure, the orthographic projection of the second annular side wall 21 on the radial cross section of the process chamber 101 completely falls into the orthographic projection of the first annular side wall 11 on the radial cross section of the process chamber 101. In this way, the gap between the outer circumference of the second annular side wall 21 and the inner circumference of the shield 104 can be blocked by the first annular side wall 11 to prevent particles from directly passing through the gap between the second annular side wall 21 and the shield 104.
[0059] There are many ways to connect the second annular side wall 21 and the shielding member 104 so that they can move along the radial direction of the process chamber 101. In some optional embodiments, for example Figure 3 As shown, the second collimator 2 further includes a first fixing portion 3 and a second fixing portion 4, both of which are arranged along any diameter direction (for example Figure 3 Taking the shape of the positive projection of the first hollow portion 13 and the second hollow portion 23 on the radial cross section of the process chamber 101 as a square as an example, the diameter direction O is, for example, a direction parallel to the diagonal of the square. Figure 1 and Figure 8As shown, one end of the first fixing portion 3 is fixedly connected to the outer circumferential surface of the second annular side wall 21, and the other end is used to pass through the first through hole of the shielding member 104 along the above-mentioned diameter direction O, and extend to the outside of the shielding member 104, and is used to connect with the driving member. Optionally, the shielding member 104 includes, for example, an upper shielding member 104a and a lower shielding member 104b, which are overlapped in the axial direction of the process chamber 101, and the above-mentioned first through hole is formed between the upper shielding member 104a and the lower shielding member 104b.
[0060] The driving member 6 is used to drive the first fixed part 3 to move along the diameter direction O; one end of the second fixed part 4 is fixedly connected to the outer peripheral surface of the second annular side wall 21, and the other end is used to be movably arranged in the second through hole of the shielding member 104 along the diameter direction O, and the second through hole can be formed between the upper shielding member 104a and the lower shielding member 104b. The driving member can be a manual driving member. Alternatively, it can also be a driver, for example, including a transmission shaft 5 and a driving source 6, wherein one end of the transmission shaft 5 is connected to the other end of the first fixed part 3, and the other end of the transmission shaft 5 passes through the chamber wall of the process chamber 101 and extends to the outside of the process chamber 101, and is connected to the driving source 6; the driving source 6 is used to drive the first fixed part 3 to move along the diameter direction O through the transmission shaft 5. Specifically, the driving source 6 is, for example, a rotating motor, and the transmission shaft 5 is, for example, a screw. The driving shaft of the rotating motor 6 cooperates with the screw thread through a rotating nut. Under the drive of the rotating motor, the nut drives the screw to move linearly during rotation, thereby driving the first fixed part 3 and the second annular side wall 21 to move synchronously.
[0061] In some optional embodiments, the second collimator 2 is located on the side of the first collimator 1 close to the base 103. That is, the movable collimator is located below the fixed collimator, which is conducive to blocking the gap between the outer circumference of the second annular side wall 21 and the inner circumference of the shielding member 104 with the help of the first annular side wall 11, and preventing particles from directly passing through the gap between the second annular side wall 21 and the shielding member 104. Optionally, there is a gap between the first collimator 1 and the second collimator 2 to ensure that the second collimator 2 can move normally and prevent the friction between the two due to relative movement from causing debris.
[0062] In some optional embodiments, such as Figure 3As shown, the thickness H1 of different positions of the first collimator 1 is consistent. Specifically, the thickness of the first annular sidewall 11 is consistent with the thickness of each grid wall in the first grid structure 12. Optionally, the aspect ratio of the first hollow portion 13 is greater than or equal to 1:2, and less than or equal to 1:1. However, the present invention is not limited to this. In practical applications, the thickness of different positions of the first collimator 1 can be inconsistent according to the specific requirements of the wafers with holes and grooves with different aspect ratio characteristics. Optionally, the thickness H1 of different positions of the first collimator 1 is consistent, and is greater than or equal to 1 mm and less than or equal to 10 mm. The above aspect ratio is the ratio of the thickness of the first collimator 1 to the aperture of the first hollow portion 13.
[0063] In some optional embodiments, the thickness of different positions of the second collimator 2 is consistent. Specifically, the thickness of the second annular side wall 21 is consistent with the thickness of each grid wall in the second grid structure 22. Optionally, the thickness of the second collimator 2 is greater than or equal to the thickness of the first collimator 1. Or, as Figure 6 and Figure 7 As shown, the thickness of the second collimator 2 increases from the outer edge to the center according to a preset rule. The greater the thickness of the second collimator 2, the greater the aspect ratio of the second hollow portion 23, and vice versa. Based on this, by increasing the thickness of the second collimator 2 from the outer edge to the center according to a preset rule, it can be applied to the situation where the number of particles distributed in the middle area of the process chamber is large, and the number of particles distributed in the edge area is small, so as to avoid the deposition process when the collimation device is not set to obtain a "thick in the middle and thin on both sides" film, thereby improving the uniformity of the film thickness. Optionally, the aspect ratio of the second hollow portion 23 distributed in the central area of the second collimator 2 is greater than or equal to 3:1, and less than or equal to 1:1; the aspect ratio of the second hollow portion 23 distributed in the edge area of the second collimator 2 is greater than or equal to 1:2, and less than or equal to 1:1. In practical applications, according to the specific requirements of wafers with holes and grooves with different aspect ratio characteristics, the aspect ratios of different areas of the second collimator 2 can have multiple combinations. The aspect ratio is the ratio of the thickness of the second collimator 2 to the aperture of the second hollow portion 23 .
[0064] Specifically, Figure 7 As shown in FIG. (a), the thickness of the second collimator 2 at different positions is consistent. Alternatively, Figure 7 As shown in Figures (a) to (d), the thickness of the second collimator 2 increases from the peripheral edge to the center according to a preset rule, and the preset rule may include:
[0065] like Figure 7 As shown in FIG. (b), the thickness of the second collimator 2 increases from the outer edge to the center and then remains unchanged; or Figure 7 As shown in FIG. (c), the thickness of the second collimator 2 increases linearly from the outer edge to the center; or, Figure 7 As shown in FIG. 5( d ), the thickness of the second collimator 2 increases in sections from the outer edge to the center. Based on the above rule, the lower surface 24 of the second collimator 2 is, for example, an arched surface (such as Figure 6 As shown), conical surface (as Figure 7 (c)), step surface (as shown in Figure 7 (d)), trapezoidal table (as shown in Figure 7 (b) shows a surface that is “thick in the middle and thin at the edges”.
[0066] In some optional embodiments, the mesh walls of at least one of the first mesh structure 12 and the second mesh structure 22 are set to have equal thickness, or the thickness increases along the axial direction of the process chamber 101 toward the direction close to the base 103. Since particles can easily accumulate on the top of the side wall, by appropriately thinning the wall thickness of the top of the side wall, it is possible to avoid the particles accumulated on the side wall protruding from the side wall and affecting the aspect ratio of the hollow portion. In the case where the mesh wall of at least one of the first mesh structure 12 and the second mesh structure 22 increases along the axial direction of the process chamber 101 toward the direction close to the base 103, the cross-sectional shape of the mesh wall is, for example, a triangle, a trapezoid, etc. Similarly, a tapered portion may be provided at one end of the mesh wall of at least one of the first mesh structure 12 and the second mesh structure 22 away from the base 103, and the contour shape of the axial cross-section of the tapered portion includes an arc, a triangle, or a trapezoid. Taking the first mesh structure 12 as an example, if Figure 5 As shown in FIG. (a), the mesh walls of the first mesh structure 12 are arranged with equal thickness; Figure 5 As shown in FIG. (b), a tapered portion 121 is provided at one end of the first grid structure 12 away from the base 103, and the contour shape of the axial cross section of the tapered portion 121 is a trapezoid; Figure 5 As shown in FIG. (c), a tapered portion 121 is provided at one end of the first grid structure 12 away from the base 103, and the contour shape of the axial cross section of the tapered portion 121 is an arc shape; Figure 5 As shown in FIG. 5( d ), the thickness of the grid wall of the first grid structure 12 increases gradually along the axial direction of the process chamber 101 toward the base 103 .
[0067] Optionally, the first collimator 1 and the second collimator 2 can be made of aluminum, stainless steel, copper or other materials. Preferably, the outer surfaces of the first collimator 1 and the second collimator 2 are relatively rough surfaces to better adhere to the sputtering material.
[0068] In summary, the alignment device of the physical vapor deposition equipment provided in the embodiment of the present invention, by stacking the first collimator 1 and the second collimator 2 between the target material 102 and the base 103 in the process chamber 101, and enabling the first collimator 1 and / or the second collimator 2 to move within the plane where they are located, can adjust the cross-sectional area of the overlapping portion of each first hollow portion 13 and the corresponding second hollow portion 23 to adjust the aspect ratio of the overlapping portion, so that the aspect ratio can be adjusted to match with a variety of wafers with holes and grooves with different aspect ratio characteristics, so as to achieve the optimal bottom coverage, and there is no need to replace the collimator, thereby improving production efficiency and machine utilization.
[0069] As another technical solution, Figure 1 As shown, an embodiment of the present invention further provides a physical vapor deposition device 100, including a process chamber 101, in which a target material 102 and a base 103 arranged below the target material 102 are arranged, and also includes the above-mentioned alignment device 109 provided in an embodiment of the present invention.
[0070] Taking the physical vapor deposition device 100 as a magnetron sputtering device as an example, the magnetron sputtering device includes a process chamber 101, a DC power supply 105, a magnetron 106 and its driving device 107 and a radio frequency power supply 110, wherein a target material 102 and a base 103 located below the target material 102 are arranged in the process chamber 101, and the base 103 is used to carry a wafer W. The target material 102 is electrically connected to the DC power supply 105, and is used to excite the reaction gas (such as argon) in the process chamber 101 to form a plasma, and the positive ions in the plasma bombard the surface of the target material 102 to make the particles on the surface of the target material 102 (uncharged target material 102 atoms) escape. Optionally, the material of the target material 102 includes, for example, copper (for example, used to form a seed layer on a wafer), aluminum, tantalum, etc., which can be sputtered by PVD metal or alloy. The base 103 is electrically connected to the radio frequency power supply 110, and is used to generate a bias voltage on the surface of the wafer that can attract particles to move downward.
[0071] The magnetron 106 is placed above the target 102 and supported by a driving device 107 to maintain a fixed distance between the magnetron 106 and the target 102. The driving device 107 is used to drive the magnetron 106 to rotate, so as to generate a magnetic field capable of binding electrons near the lower surface of the target 102, so that a large number of charged particles bombard the target 102, and a large number of target 102 materials are sputtered in the process chamber 101. The rotation of the magnetron 106 ensures that the target 102 material is uniformly sputtered at different positions on the surface of the target 102.
[0072] The base 103 is disposed below the target 102, and an electrostatic chuck (ESC) is mounted on its upper surface for supporting and adsorbing the wafer. The electrostatic chuck may have adsorption or temperature control functions. The wafer W has holes and grooves with high aspect ratio characteristics. The target 102 material sputtered from the target 102 may move downward and deposit on the wafer surface to form a thin film.
[0073] Optionally, a side magnet device 108 is provided at the outer side of the process chamber 101 near the base 103. The side magnet device 108 can be a permanent magnet or various forms of electromagnets, or even any combination of the two. With the help of the side magnet device 108, the magnetic field can be coupled into the chamber to change the magnetic field distribution in the area near the base 103 inside the chamber, increase the retention time of electrons in the area, thereby increasing the ionization rate of the internal gas while controlling the direction of the plasma and improving the uniformity of the thin film deposited on the wafer.
[0074] The collimator 109 is disposed in the process chamber 101 and connected to the shield 104. Specifically, the shield 104 includes an upper shield and a lower shield, which are overlapped in the axial direction of the process chamber 101, and the collimator is connected between the upper shield and the lower shield.
[0075] The physical vapor deposition equipment provided by the embodiment of the present invention, by adopting the above-mentioned collimation device provided by the embodiment of the present invention, can be applicable to wafers with various holes and grooves with different aspect ratio characteristics, so as to achieve the optimal bottom coverage, and there is no need to replace the collimator, thereby improving production efficiency and machine utilization.
[0076] It is to be understood that the above embodiments are merely exemplary embodiments used to illustrate the principles of the present invention, but the present invention is not limited thereto. For those of ordinary skill in the art, various modifications and improvements can be made without departing from the spirit and essence of the present invention, and these modifications and improvements are also considered to be within the scope of protection of the present invention.
Claims
1. A collimation device for a physical vapor deposition device, characterized in that: The device comprises a first collimator and a second collimator, wherein the first collimator and the second collimator are both arranged in a process chamber of the physical vapor deposition device and are stacked between a target material and a base in the process chamber; The first collimator has a plurality of first hollow parts, the second collimator has a plurality of second hollow parts, and each of the first hollow parts and each of the second hollow parts are arranged correspondingly; The first collimator and / or the second collimator can move within the plane where the first collimator is located, so as to adjust the cross-sectional area of the overlapping portion between each of the first hollow portions and the corresponding each of the second hollow portions.
2. The collimation device according to claim 1, characterized in that: The first collimator is fixedly connected to a shielding member in the process chamber, and the second collimator is movably connected to the shielding member along a radial direction of the process chamber.
3. The collimation device according to claim 2, characterized in that: The first collimator includes a first annular sidewall and a first grid structure, wherein the first grid structure is located in a space defined by the first annular sidewall and connected to the first annular sidewall; grids in the first grid structure constitute the first hollow portion; The first annular side wall is fixedly connected to the shielding component, and the outer circumferential surface of the first annular side wall is in contact with the inner circumferential surface of the shielding component.
4. The collimation device according to claim 3, characterized in that: The second collimator comprises a second annular side wall and a second grid structure, wherein the second grid structure is located in a space defined by the second annular side wall and connected to the second annular side wall; grids in the second grid structure constitute the second hollow portion; The second annular side wall is connected to the shielding member so as to be movable along a radial direction of the process chamber.
5. The collimation device according to claim 4, characterized in that: The radial thickness of the second annular side wall is smaller than the radial thickness of the first annular side wall, and when the cross-sectional area of the overlapping portion of each first hollow portion and the corresponding second hollow portion is the largest, the orthographic projection of the second annular side wall on the radial cross section of the process chamber completely falls into the orthographic projection of the first annular side wall on the radial cross section of the process chamber.
6. The collimation device according to claim 4, characterized in that: The second collimator further includes a first fixing portion and a second fixing portion, wherein the first fixing portion and the second fixing portion are arranged opposite to each other along any diameter direction of the second annular side wall; One end of the first fixing portion is fixedly connected to the outer circumferential surface of the second annular side wall, and the other end is used to pass through the first through hole of the shielding member along the diameter direction and extend outside the shielding member, and is used to be connected to a driving member; the driving member is used to drive the first fixing portion to move along the diameter direction; One end of the second fixing portion is fixedly connected to the outer circumferential surface of the second annular side wall, and the other end is used to be movably inserted into the second through hole of the shielding member along the diameter direction.
7. The collimation device according to claim 6, characterized in that: The driving member includes a transmission shaft and a driving source, wherein one end of the transmission shaft is connected to the other end of the first fixed part, the other end of the transmission shaft passes through the chamber wall of the process chamber and extends outside the process chamber, and is connected to the driving source; the driving source is used to drive the first fixed part to move along the diameter direction through the transmission shaft.
8. The collimation device according to claim 1, characterized in that: The first collimator is located between the second collimator and the target material; and the thickness of the first collimator at different positions is consistent.
9. The collimation device according to claim 1, characterized in that: The first collimator is located between the second collimator and the target; the thickness of the second collimator at different positions is consistent; or, The thickness of the second collimator increases from the outer edge to the center according to a preset rule.
10. The collimation device according to claim 9, characterized in that: The preset rules include: The thickness of the second collimator increases from the outer edge to the center first and then remains unchanged; or, the thickness of the second collimator increases linearly from the outer edge to the center; or, the thickness of the second collimator increases segmentally from the outer edge to the center.
11. The collimation device according to claim 4, characterized in that: The mesh wall of at least one of the first mesh structure and the second mesh structure is arranged with equal thickness, or increases gradually along the axial direction of the process chamber toward the base; or, A tapered portion is provided at one end of the grid wall of at least one of the first grid structure and the second grid structure away from the base, and an axial cross-section of the tapered portion has an arc shape, a triangle, or a trapezoid.
12. The collimation device according to claim 1, characterized in that: When the cross-sectional area of the overlapping portion of each of the first hollow portions and the corresponding each of the second hollow portions is the largest, the orthographic projections of each of the first hollow portions and the corresponding each of the second hollow portions on the radial cross section of the process chamber completely overlap.
13. The collimation device according to claim 8, characterized in that: The aspect ratio of the first hollow portion is greater than or equal to 1:2 and less than or equal to 1:
1.
14. The collimation device according to claim 9 or 10, characterized in that: The depth-to-width ratio of the second hollow portion distributed in the central area of the second collimator is greater than or equal to 3:1 and less than or equal to 1:1; the depth-to-width ratio of the second hollow portion distributed in the edge area of the second collimator is greater than or equal to 1:2 and less than or equal to 1:
1.
15. The collimation device according to claim 1, characterized in that: The first collimator and the second collimator are spaced apart from each other along an axial direction of the process chamber.
16. A physical vapor deposition device, comprising a process chamber, wherein a target material and a susceptor disposed below the target material are arranged in the process chamber, characterized in that: It also comprises the collimation device as described in any one of claims 1-15.
Citation Information
Patent Citations
Physical vapor deposition system and physical vapor depositing method using same
CN105887026A
Biasable flux optimizer / collimator for PVD sputter chamber
CN106987815A
Collimator for use in substrate processing chambers
CN107002220A
Processing device and collimator
CN108026633A
Cavity and cavity plate of PVD (Physical Vapor Deposition) equipment, and operation method of PVD equipment with PVD cavity
CN115433908A