Electrostatic force microscope probe and preparation method and application thereof

The preparation of electrostatic force microscope probes in KOH electrolyte solution solved the problem that the existing technology is difficult to measure the large fluctuating microstructure, improved the measurement accuracy and sensitivity, and formed a sharp and accurate probe.

CN119020846APending Publication Date: 2024-11-26XIAN AEROSPACE MEASUREMENT & TESTING RES INST
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411113967.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-14
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

The existing electrostatic force microscope probes are difficult to measure microstructures with fluctuations of more than 10 μm, and the cone angle of the probe tip greatly affects the measurement accuracy.

Method used

The tungsten wire probe was prepared by using electrochemical polishing method in KOH electrolyte to form an electrostatic force microscope probe with a sharp tip, and the control circuit monitors the polishing current to ensure the sharpness of the probe tip.

Benefits of technology

The sensitivity of detecting electrostatic force gradients is improved, the accuracy of EFM measuring the surface profile of the microscopic large undulating workpiece is improved, and a smooth surface and a symmetrical conical probe tip is formed.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119020846A_ABST
    Figure CN119020846A_ABST
Patent Text Reader

Abstract

The invention discloses an electrostatic force microscope probe and a preparation method and application thereof. The method comprises the following steps: putting a platinum ring into a container filled with KOH electrolyte; a tungsten filament is selected, and the lower end of the tungsten filament penetrates through the platinum ring to be placed in the KOH electrolyte; the anode of a control circuit is connected with the tungsten filament, the cathode of the control circuit is connected with the platinum ring, and the control circuit is started to electrochemically polish the tungsten filament; when the upper end and the lower end of the tungsten filament are separated, the control circuit is closed, and the tungsten filament is taken out to obtain the electrostatic force microscope probe. The prepared electrostatic force microscope probe is applied to an electrostatic force microscope. The probe prepared by the invention can be used for measuring a large-fluctuation microstructure workpiece with an abrupt slope.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of measurement and testing, and in particular relates to an electrostatic force microscope probe. The present invention also relates to a preparation method and application of the probe. Background Art

[0002] Electrostatic force microscopy (EFM) is a scanning probe microscope that measures the electrostatic interaction between the probe and the workpiece surface and characterizes the surface profile of the workpiece being measured. As a measuring instrument for research, production process and equipment operation, EFM can be used for surface observation, dimension determination, surface roughness measurement, particle size analysis, surface defect analysis, etc., and has a very wide range of applications.

[0003] Its working principle is similar to that of atomic force microscopy (AFM), but unlike AFM, which measures the van der Waals force between the probe and the workpiece surface, EFM achieves workpiece surface profile imaging by measuring the Coulomb interaction between the two. When working, a working voltage is applied between the probe and the sample, and the probe oscillates on the workpiece surface under the action of electrostatic force, but does not contact the workpiece surface. The performance index of the EFM probe is the most critical factor in determining the resolution of the microscope. The advantage of this measurement method is that it does not damage the surface of the workpiece to be measured due to the use of non-contact measurement, and at the same time, it has a certain measurement accuracy in measuring the surface profile of the workpiece. The disadvantage is that due to the length of the probe tip and the structure of the cantilever probe, this EFM is difficult to measure microstructures with fluctuations greater than 10μm. In addition, the cone angle of the currently commonly used EFM probe tip is greater than 40°, and the large cone angle of the probe tip also directly affects the profile of the measured microstructure. Summary of the invention

[0004] The purpose of the present invention is to provide a method for preparing an electrostatic force microscope probe, by which the prepared probe can measure a workpiece with a steep slope and a large undulating microstructure.

[0005] The second object of the present invention is to provide an electrostatic force microscope probe prepared by the above preparation method.

[0006] The third object of the present invention is to provide an application of an electrostatic force microscope probe.

[0007] The first technical solution adopted by the present invention is a method for preparing an electrostatic force microscope probe, which is specifically implemented according to the following steps:

[0008] Step 1, placing a platinum ring into a container filled with KOH electrolyte;

[0009] Step 2, select a tungsten wire, pass the lower end of the tungsten wire through a platinum ring and place it in a KOH electrolyte;

[0010] Step 3, connecting the anode of the control circuit to the tungsten wire, connecting the cathode to the platinum ring, and starting the control circuit to electrochemically polish the tungsten wire;

[0011] Step 4: When the upper end and the lower end of the tungsten wire are separated, the control circuit is turned off, and the tungsten wire is taken out to obtain an electrostatic force microscope probe.

[0012] The first technical solution of the present invention is also characterized in that:

[0013] In step 1, the concentration of KOH electrolyte is 1 mol / L.

[0014] In step 2, the diameter of the tungsten wire is 0.1 mm to 0.2 mm, the purity is 99.93% to 99.97%, and the length is 30 mm to 40 mm.

[0015] The control circuit in step 3 includes:

[0016] A collection circuit for converting the current of the KOH electrolyte into an output voltage;

[0017] A drive inversion circuit for inverting the output voltage of the acquisition circuit;

[0018] A comparator circuit for comparing the output voltage of the driving inversion circuit; a driving circuit for causing a current to be generated in the tungsten filament and producing an on-off effect as the current changes;

[0019] The acquisition circuit, the driving inversion circuit, the comparison circuit and the driving circuit are connected in sequence.

[0020] The acquisition circuit includes a first resistor and a first power operational amplifier. The reverse input terminal of the first power operational amplifier is connected to the platinum ring, and the same-direction input terminal of the first power operational amplifier is grounded; the first resistor is connected across the reverse input terminal and output terminal resistor of the first power operational amplifier.

[0021] The driving inversion circuit includes a second resistor, a third resistor and a second power operational amplifier, one end of the second resistor is connected to the output end of the acquisition circuit, the other end of the second resistor is connected to the reverse input end of the second power operational amplifier, the third resistor is connected across the reverse input end and the output end of the second power operational amplifier, and the same-direction input end of the second power operational amplifier is grounded.

[0022] The comparison circuit includes a fourth resistor, a fifth resistor, a sixth resistor, a seventh resistor, an eighth resistor, a third power operational amplifier and a comparison power supply;

[0023] One end of the fourth resistor is connected to the output end of the driving inversion circuit, the other end of the fourth resistor is connected to one end of the fifth resistor, the other end of the fifth resistor is connected to the output end of the third power operational amplifier, the same-direction input end of the third power operational amplifier is connected to one end of the sixth resistor, one end of the sixth resistor is respectively connected to the seventh resistor and the eighth resistor, the other end of the seventh resistor is connected to the comparison power supply, and the other ends of the comparison power supply and the eighth resistor are both grounded.

[0024] The driving circuit includes a micro relay, a control switch, a diode and a driving power supply; one end of the diode is connected to the output end of the comparison circuit, and the other end is connected to the micro relay, the driving power supply and the control switch in sequence. The output end of the micro relay is also grounded through a line, and the other end of the control switch is connected to the tungsten filament.

[0025] The second technical solution adopted by the present invention is that the electrostatic force microscope probe,

[0026] The third technical solution adopted by the present invention is the application of an electrostatic force microscope probe.

[0027] The beneficial effects of the present invention are:

[0028] (1) The preparation method of the electrostatic force microscope probe of the present invention comprises the following steps: placing a tungsten wire inside a platinum ring, and under the action of the surface tension of a KOH electrolyte, an electrochemical reaction occurs around the tungsten wire near the surface of the KOH electrolyte to form a meniscus; as the electropolishing continues, the diameter of the tungsten wire near the surface of the KOH electrolyte gradually decreases, and when the tungsten wire immersed in the KOH electrolyte falls, the upper tungsten wire is taken out to form an electrostatic force microscope probe with a sharp measuring tip at the upper part, and the formed probe has a smooth surface and a symmetrical cone, which improves the sensitivity of detecting the electrostatic force gradient, thereby greatly improving the accuracy of EFM measurement of the surface profile of a microscopic large undulation workpiece.

[0029] (2) The preparation method of the electrostatic force microscope probe of the present invention monitors the polishing current by setting a control circuit, and immediately turns off the polishing current after the lower and upper parts of the tungsten wire separate and settle, thereby ensuring that the formed probe tip is sharp. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Figure 1 It is a schematic structural diagram of an electrostatic force microscope in the method for preparing an electrostatic force microscope probe of the present invention;

[0031] Figure 2 It is a schematic diagram of electrochemical polishing in the method for preparing an electrostatic force microscope probe of the present invention;

[0032] Figure 3 It is a schematic diagram of a control circuit in the method for preparing an electrostatic force microscope probe of the present invention;

[0033] Figure 4 is a SEM image of a probe tip prepared by the method for preparing an electrostatic force microscope probe of the present invention;

[0034] Figure 5 It is a schematic diagram of the change of current over time during the electrochemical polishing process of the present invention;

[0035] Figure 6It is a schematic diagram of the result of measuring the displacement in the up and down directions using the EFM probe prepared in Example 3 of the present invention.

[0036] In the figure, 1. cantilever, 2. probe tip, 3. electrostatic force, 4. sample to be tested, 5. power supply, 6. control circuit, 7. tungsten filament, 8. meniscus, 9. platinum ring, 10. KOH electrolyte, 11. first resistor, 12. first power operational amplifier, 13. second resistor, 14. second power operational amplifier, 15. third resistor, 16. fourth resistor, 17. fifth resistor, 18. third power operational amplifier, 19. sixth resistor, 20. seventh resistor, 21. eighth resistor, 22. micro relay, 23. control switch, 24. diode, 25. comparison power supply, 26. driving power supply. DETAILED DESCRIPTION

[0037] The present invention is described in detail below with reference to the accompanying drawings and specific embodiments.

[0038] Electrostatic force microscopy (EFM) is a measuring instrument used in research, production processes and equipment operation. It is used in areas where the distance between the two is relatively long, such as the manufacture of electronic components and high-voltage technology. Figure 1 As shown, it includes a cantilever 1, a probe tip 2 is fixedly arranged at the lower part of the cantilever 1, and a sample 4 to be measured is placed below the probe tip 2. The measurement is achieved by the electrostatic force 3 between the probe tip 2 and the sample 4 to be measured. The EFM tip is placed at a height b (b≥5nm) above the sample surface. The charge Q1 on the top of the tip interacts with the charge Q2 on the sample surface. The electrostatic interaction force of the charge at the top of the tip is determined by Coulomb's law. The electrostatic force 3F E The calculation formula is as follows:

[0039]

[0040] Where ε is the dielectric constant of the medium (such as air), Q1 and Q2 are charges, and b is the distance between the charges.

[0041] At the same time, there is a capacitor C between the tip of the electrostatic force microscope and the sample. The polarization of this capacitor is related to the voltage V p This means that the charge: Q = C ip V p The capacitor is then polarized to the "tip sample" voltage, with the opposite polarization charges +Q and -Q attracting each other.

[0042] Example 1

[0043] The preparation method of the electrostatic force microscope probe of the present invention is specifically implemented according to the following steps:

[0044] Step 1, placing a platinum ring 9 into a container filled with a KOH electrolyte 10 with a concentration of 1 mol / L;

[0045] Step 2, such as Figure 2 As shown, a tungsten wire 7 is selected, and the lower end of the tungsten wire 7 is passed through a platinum ring 9 and placed in a KOH electrolyte 10;

[0046] Furthermore, in order to facilitate operation, the tungsten wire 7 is bent into an L shape; and the lower portion of the L-shaped tungsten wire 7 is placed in a KOH electrolyte 10 with a concentration of 1 mol / L.

[0047] Furthermore, in order to facilitate the L-shaped tungsten wire 7 to pass through the platinum ring 9, the diameter of the tungsten wire 7 is 0.1 mm to 0.2 mm; the purity is 99.93% to 99.97%, and the length is 30 mm to 40 mm; and the diameter of the platinum ring 9 is 10 mm.

[0048] Step 3, connecting the anode of the control circuit 6 to the tungsten wire 7, connecting the cathode to the platinum ring 9, and starting the control circuit 6 to perform electrochemical polishing on the tungsten wire 7;

[0049] Due to the surface tension of the KOH electrolyte 10, a meniscus 8 will be formed around the tungsten wire 7 near the surface of the KOH electrolyte 10. Once a voltage is applied between the tungsten wire 7 and the platinum ring 9, an electrochemical reaction will occur from the top of the meniscus 8 to the lower end of the tungsten wire 7 immersed in the KOH electrolyte 10.

[0050] During the specific reaction, the reaction formula of the cathode platinum ring 9 is as follows:

[0051] 6H2O+6e - →3H2+6OH - ;

[0052] The reaction formula of the anode tungsten wire 7 is as follows:

[0053] W+8OH - →WO4 -2 +4H2O+6e - ;

[0054] Step 4: The position with the fastest electrochemical polishing speed is the surface of the KOH electrolyte 10 where the tungsten wire 7 is close to the platinum ring 9. As the polishing process proceeds, the diameter of the tungsten wire 7 decreases. When the diameter is less than a certain value, the weight of the lower part of the tungsten wire 7 will separate it from the upper part. When the upper end of the tungsten wire 7 is separated from the lower end, the control circuit 6 is turned off, the tungsten wire 7 is taken out, and an electrostatic force microscope probe with a sharp measuring tip is obtained.

[0055] At this point, the amplitude of the polishing current suddenly decreases, but it does not return to zero completely. If the upper part of the tungsten wire is not immediately pulled out of the electrolyte, the polishing of the upper part will continue and the upper stylus tip will quickly lose its sharpness. To avoid oxidation of the probe tip, the EFM probe is stored in a desiccator with a relative humidity of ≤20% when not in use.

[0056] Example 2

[0057] On the basis of Example 1, Figure 3 As shown, in the method for preparing the electrostatic force microscope probe of the present invention, the control circuit 6 in step 3 includes an acquisition circuit, a drive inversion circuit, a comparison circuit and a drive circuit which are interconnected.

[0058] The acquisition circuit includes a first resistor 11 and a first power operational amplifier 12. The resistance of the first resistor 11 is 100 kΩ. The reverse input terminal of the first power operational amplifier 12 is connected to the platinum ring 9, and the same-direction input terminal of the first power operational amplifier 12 is grounded; the first resistor 11 is connected across the reverse input terminal and the output terminal of the first power operational amplifier 12.

[0059] That is, the acquisition circuit is used to convert the current i flowing through the electrolyte into an output voltage u1, as shown in the following formula:

[0060] u1=i*R1;

[0061] Wherein, R1 is the resistance value of the first resistor.

[0062] The driving inversion circuit includes a second resistor 13, a third resistor 15 and a second power operational amplifier 14. The resistance values ​​of the second resistor 13 and the third resistor 15 are both 10kΩ. One end of the second resistor 13 is connected to the output end of the acquisition circuit, and the other end of the second resistor 13 is connected to the reverse input end of the second power operational amplifier 14. The third resistor 15 is connected across the reverse input end and the output end of the second power operational amplifier 14, and the same-direction input end of the second power operational amplifier 14 is grounded.

[0063] Furthermore, the first power operational amplifier 12 and the second power operational amplifier 14 are of the OPA554 type.

[0064] The voltage u2 output by the second power operational amplifier 14 is the inverse of the output voltage u1, as shown in the following formula:

[0065] u2=-u1*(R3 / R2);

[0066] Wherein, R2 is the resistance value of the second resistor, and R3 is the resistance value of the third resistor;

[0067] The comparison circuit includes a fourth resistor 16, a fifth resistor 17, a sixth resistor 19, a seventh resistor 20, an eighth resistor 21, a third power operational amplifier 18 and a comparison power supply 25, wherein the sixth resistor 19 does not participate in the circuit operation, but only plays a role in impedance matching. The resistance values ​​of the fourth resistor 16, the fifth resistor 17, the sixth resistor 19 and the eighth resistor 21 are all 10kΩ, the resistance value of the seventh resistor 20 is 50kΩ, the model of the third power operational amplifier 18 is AD712, and the comparison power supply 25 is a 12V DC power supply.

[0068] Specifically, one end of the fourth resistor 16 is connected to the output end of the driving inversion circuit, the other end of the fourth resistor 16 is connected to one end of the fifth resistor 17, one end of the fifth resistor 17 is connected to the output end of the third power operational amplifier 18, the same-direction input end of the third power operational amplifier 18 is connected to one end of the sixth resistor 19, one end of the sixth resistor 19 is respectively connected to the seventh resistor 20 and the eighth resistor 21, the other end of the seventh resistor 20 is connected to the comparison power supply 25, and the other ends of the comparison power supply 25 and the eighth resistor 21 are both grounded.

[0069] The output voltage u3 of the third power operational amplifier 18 is expressed as follows:

[0070] u3=-u2*(R5 / R4)+u A *(1+R5 / R4)*(R8 / (R7+R8));

[0071] Wherein, R4 is the resistance value of the fourth resistor, R5 is the resistance value of the fifth resistor, R7 is the resistance value of the seventh resistor, R8 is the resistance value of the eighth resistor, and u A is the power supply output voltage value;

[0072] Assume R4=R5=R6=R7=R8=a;R7=R, then the above formula is:

[0073] u3=2u A (1 / (a+1))*-u2;

[0074] When 2u A If (1 / (a+1)) is greater than u2, the output is positive and there is current in the circuit; otherwise, there is no current in the circuit.

[0075] The driving circuit includes a micro relay 22, a control switch 23, a diode 24 and a driving power supply 26; the model of the micro relay 22 is G6A-274P, and the driving power supply 26 is a 3V DC power supply.

[0076] Specifically, one end of the diode 24 is connected to the output end of the comparison circuit, and the other end is connected to the micro relay 22, the driving power supply 26 and the control switch 23 in sequence. The output end of the micro relay 22 is also grounded through a line. The other end of the control switch 23 is connected to the tungsten wire 7.

[0077] The driving circuit is mainly used to make the chemical reaction in the tungsten filament generate a current of corresponding magnitude and produce an on-off effect according to the magnitude of the current.

[0078] In the control circuit, the polishing current is converted into a voltage signal, amplified 100,000 times, and compared with a reference voltage of 2V. Figure 5 As shown, when the polishing current is equal to or less than 0.02 mA, the control switch 23 is triggered to turn off the polishing process. As can be seen from the figure, the polishing current is about 0.09 mA at the beginning of the polishing process. Then, shortly before the upper and lower parts of the tungsten wire 7 separate, the current decreases to about 0.04 mA. When the current reaches 0.02 mA, the current is automatically cut off.

[0079] On the other hand, the present invention also provides an electrostatic force microscope probe, which is prepared by the above-mentioned preparation method of the electrostatic force microscope probe.

[0080] On the other hand, the present invention also provides the use of the electrostatic force microscope probe in an electrostatic force microscope.

[0081] Example 3

[0082] This embodiment is implemented according to the following steps:

[0083] Step 1, placing a platinum ring 9 with a diameter of 10 mm into a container filled with a KOH electrolyte 10 with a concentration of 1 mol / L;

[0084] Step 2, select a tungsten wire 7, the diameter of the tungsten wire 7 is 0.1 mm, the purity is 99.95%, and the length is 30 mm, and the lower end of the tungsten wire 7 is passed through a platinum ring 9 and placed in a KOH electrolyte 10;

[0085] Step 3, connecting the anode of the control circuit 6 to the tungsten wire 7, connecting the cathode to the platinum ring 9, and starting the control circuit 6 to perform electrochemical polishing on the tungsten wire 7;

[0086] Step 4: When the upper end and the lower end of the tungsten wire 7 are separated, the control circuit 6 is turned off, and the tungsten wire 7 is taken out to obtain an electrostatic force microscope probe.

[0087] The prepared electrostatic force microscope probe is scanned to obtain a SEM (scanning electron microscope) image of the electrostatic force microscope probe, such as Figure 4 As shown, through Figure 4It can be seen that the prepared electrostatic force microscope probe has a smooth surface and a symmetrical cone, the tip radius is about 100nm, the cone half angle is less than 10°, and the aspect ratio is greater than 10:1.

[0088] The EFM probe manufactured in Example 3 was used to measure the displacement of the sample 4 in the up and down directions. The measurement results are shown in Figure 6 , the sample is moved vertically by the piezoelectric drive toward the EFM probe tip with a step size of about 10nm. In each step, the probe tip is controlled by the Z drive separately in response to two different frequency shift set points (Δf1: 0.95Hz, Δf2: 0.76Hz). The distance from the tip to the sample is calculated using the equation to evaluate the displacement of the sample surface. The evaluation results are shown in the figure. After calculation, the measured displacement and the applied displacement are in good agreement with each other, and the standard deviation from the linear fit curve is 3.8nm.

Claims

1. A method for preparing an electrostatic force microscope probe, characterized in that: Follow the steps below to implement it: Step 1, placing a platinum ring (9) into a container filled with KOH electrolyte (10); Step 2, select a tungsten wire (7), pass the lower end of the tungsten wire (7) through a platinum ring (9) and place it in a KOH electrolyte (10); Step 3, connecting the anode of the control circuit (6) to the tungsten wire (7), connecting the cathode to the platinum ring (9), and starting the control circuit (6) to perform electrochemical polishing on the tungsten wire (7); Step 4, when the upper end and the lower end of the tungsten wire (7) are separated, the control circuit (6) is turned off, and the tungsten wire (7) is taken out to obtain an electrostatic force microscope probe.

2. The method for preparing an electrostatic force microscope probe according to claim 1, characterized in that: The concentration of the KOH electrolyte (10) in step 1 is 1 mol / L.

3. The method for preparing an electrostatic force microscope probe according to claim 1, characterized in that: The diameter of the tungsten wire (7) in step 2 is 0.1 mm to 0.2 mm, the purity is 99.93% to 99.97%, and the length is 30 mm to 40 mm.

4. The method for preparing an electrostatic force microscope probe according to claim 1, characterized in that: The control circuit (6) in step 3 comprises: A collection circuit for converting the current of the KOH electrolyte (10) into an output voltage; A drive inversion circuit for inverting the output voltage of the acquisition circuit; A comparison circuit for comparing the output voltage of the driving inverter circuit; A driving circuit for generating a current in the tungsten filament and producing an on-off effect as the current changes; The acquisition circuit, the drive inversion circuit, the comparison circuit and the drive circuit are connected in sequence.

5. The method for preparing an electrostatic force microscope probe according to claim 4, characterized in that: The acquisition circuit comprises a first resistor (11) and a first power operational amplifier (12); the reverse input terminal of the first power operational amplifier (12) is connected to the platinum ring (9), and the non-inverting input terminal of the first power operational amplifier (12) is grounded; the first resistor (11) is connected across the reverse input terminal and the output terminal resistor of the first power operational amplifier (12).

6. The method for preparing an electrostatic force microscope probe according to claim 4, characterized in that: The drive inversion circuit comprises a second resistor (13), a third resistor (15) and a second power operational amplifier (14); one end of the second resistor (13) is connected to the output end of the acquisition circuit; the other end of the second resistor (13) is connected to the reverse input end of the second power operational amplifier (14); the third resistor (15) is connected across the reverse input end and the output end of the second power operational amplifier (14); and the non-inverting input end of the second power operational amplifier (14) is grounded.

7. The method for preparing an electrostatic force microscope probe according to claim 4, characterized in that: The comparison circuit comprises a fourth resistor (16), a fifth resistor (17), a sixth resistor (19), a seventh resistor (20), an eighth resistor (21), a third power operational amplifier (18) and a comparison power supply (25); One end of the fourth resistor (16) is connected to the output end of the driving inversion circuit, the other end of the fourth resistor (16) is connected to one end of the fifth resistor (17), the other end of the fifth resistor (17) is connected to the output end of the third power operational amplifier (18), the non-inverting input end of the third power operational amplifier (18) is connected to one end of the sixth resistor (19), one end of the sixth resistor (19) is respectively connected to the seventh resistor (20) and the eighth resistor (21), the other end of the seventh resistor (20) is connected to the comparison power supply (25), and the other ends of the comparison power supply (25) and the eighth resistor (21) are both grounded.

8. The method for preparing an electrostatic force microscope probe according to claim 4, characterized in that: The driving circuit comprises a micro relay (22), a control switch (23), a diode (24) and a driving power supply (26); one end of the diode (24) is connected to the output end of the comparison circuit, and the other end is connected to the micro relay (22), the driving power supply (26) and the control switch (23) in sequence; the output end of the micro relay (22) is also grounded through a line, and the other end of the control switch (23) is connected to the tungsten wire (7).

9. An electrostatic force microscope probe, characterized in that The electrostatic force microscope probe is prepared by the method for preparing an electrostatic force microscope probe according to any one of claims 1 to 8.

10. Use of the electrostatic force microscope probe according to claim 9 in an electrostatic force microscope.