Alloy low-cost control method and system for converter tapping of aluminum killed steel
Through improved linear planning solution methods and real-time data acquisition, the problem of alloy cost control during steelmaking is solved, the rapid and accurate alloy batching is achieved, the cost of steelmaking alloy is reduced, and the production efficiency is improved.
Patent Information
- Application Number
- CN202411496696.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-25
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-10-25
AI Technical Summary
The prior art is difficult to effectively control the alloy cost during the steelmaking process, resulting in high alloy cost, low production efficiency, and inaccurate alloy batching, which affects the steel smelting cost and production efficiency.
The improved linear programming solution method is used to combine real-time data acquisition and database establishment. By determining the alloy element yield calculation formula and optimizing the batching model, the rapid and accurate calculation of the alloy addition amount is achieved and the alloy cost is reduced.
It has achieved rapid and precise optimization of alloy ingredients, reduced steelmaking alloy costs, improved production efficiency, and ensured the scientificity and accuracy of alloy types and added amounts under the premise of meeting the requirements of liquid steel composition.
Smart Images

Figure CN119028475A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a low-cost control method and system for aluminum killed steel converter steel alloy tapping, belonging to the technical field of steelmaking. Background Art
[0002] In order to meet the physical and chemical performance requirements of different steel grades during the steelmaking process, various alloys are added to the molten steel for deoxidation and alloying, and the composition of each element is adjusted to the specified range of the process. The alloy cost accounts for a large proportion of the steel smelting cost. If the alloy type and the amount added can be reasonably selected and the alloy cost can be reduced to the lowest level under the premise of meeting production needs, it is very important to control production costs and improve efficiency.
[0003] The converter steelmaking process has good dynamic conditions due to the impact of steel flow. Adding alloys in this process is conducive to the rapid melting of alloys, and it is a good time to add alloys. At present, the type of alloy and the weight of alloy addition are selected according to the converter endpoint conditions and the target control composition in the steelmaking production process, which are relatively fixed. The disadvantage of this alloy addition is that it is not conducive to cost control. However, in the smelting process, it is difficult to achieve accurate batching according to the conditions of molten steel, mainly because: the time from the composition detection results to steelmaking is short, and considering the alloy type, price, composition, deoxidation and alloying effect and other factors at the same time, manual experience calculation is almost impossible to achieve. Therefore, if a low-cost control method for aluminum-killed steel steelmaking alloys can be developed to guide operators to quickly read relevant information within a few minutes before the converter steelmaking, and complete the optimal batching calculation that meets the process requirements, it will be of great significance to reduce the cost of steelmaking alloys and improve production efficiency.
[0004] Chinese invention patent CN114611844B discloses a method and system for determining the amount of alloy added in the converter steelmaking process. The patent application calculates the alloy element yield rate through a neural network and uses integer linear programming to solve the alloy addition amount. The invention uses a neural network to predict the alloy yield rate, but the neural network calculation is complex, and when the setting is improper, the data will not converge, resulting in the problem of being unable to calculate.
[0005] Chinese invention patent application CN116665791A discloses a method for calculating low-cost converter alloys applicable to all types of steel. The patent application first calculates the alloy corresponding to a single component based on the alloy composition and price, and continues to calculate other alloys with the remaining unmet components of the molten steel brought by the alloy until all alloy calculations are completed. The alloy types and alloy weights calculated by this method may not be optimal.
[0006] It can be seen that there are no relatively stable paths and methods to control alloy costs in the market. This field is still in a relatively blank stage. The industry still uses experience in production, which is not conducive to cost management and control, and is not conducive to the rational, scientific and quantitative use of additives. Summary of the invention
[0007] In view of the shortcomings of the above technical methods, in order to solve the above problems, the purpose of the present invention is to provide a low-cost control method and system for aluminum killed steel converter alloy tapping, which overcomes the situation that the neural network may not converge when calculating the alloy yield, and can quickly and accurately optimize the batching according to the current composition of the molten steel. The specific technical scheme is as follows: A low-cost control method for aluminum killed steel converter steel alloy, comprising the following steps: Step (1) collecting real-time data of the converter production process and establishing a database; Step (2) limits the range of molten iron loading and scrap steel loading to stabilize the output of the converter; Step (3) according to the steel type to be smelted and the target carbon content of the steel type, the parameters of the oxygen content at the converter end point and the number of times the tapping hole is used are read to determine the calculation formula for the alloy element yield; Step (4) limiting the tapping angle to between -104°C and -100°C, controlling the amount of slag in the converter, and reducing the influence of fluctuations in the amount of slag in the converter on the alloy yield; Step (5) uses an improved linear programming solution method to establish an alloy addition solution model, and the alloy addition solution model takes the lowest total alloy addition cost Z as the objective function: , Where: is the price of alloy j, is the amount of alloy j added, n is the type of alloy; The constraints are as follows: ; in, is the lower limit of the composition of element i, %; Represents the content of element i in alloy j, %; is the weight of alloy j added, kg; is the weight of element i in the molten steel when tapping from the converter, kg; is the upper limit of the composition of element i, %; i is an alloying element; is the weight of element i reduced in the converter slag, kg; The amount of alloy added is less than the maximum amount of alloy that can be added: , in, is the maximum amount of the jth alloy added to the steel grade in actual production. The maximum amount of different alloys added to different steel grades is determined according to the process production requirements and stored in the database; Step (6) After the steel is tapped from the converter, the furnace number and the alloy addition amount are stored in the real-time database.
[0008] Furthermore, the real-time data of the converter production process in step (1) includes: furnace number, steel type, molten iron charge, scrap steel addition, number of times the tapping port is used, tapping time, converter end point composition, converter end point temperature, converter end point oxygen content, tapping amount, converter slag amount, converter end point slag composition, amount of each alloy added during the tapping process, ladle steel liquid composition after alloying, alloy composition, alloy price, steel liquid target composition and alloy element recovery rate.
[0009] Furthermore, the calculation process of the converter steel output in step (2) is as follows: the converter molten iron loading is controlled within a range of 159-162 t, and the molten iron recovery rate is calculated according to an empirical value of 0.89; the converter scrap steel loading is controlled within a range of 46-48 t, and the scrap steel recovery rate is calculated according to an empirical value of 0.80.
[0010] Furthermore, the alloy element yields in step (3) are as follows: Aluminum yield The calculation process is: When the tapping hole is used less than or equal to 100 times, the calculation formula is: , When the tapping hole is used more than 100 times, the calculation formula is: , in, is the amount of aluminum added, kg; is the oxygen content at the converter end point, ppm; The number of times the tapping hole is used; Manganese recovery rate The calculation formula is: , in, is the amount of manganese added, kg; The calculation process of silicon yield is: When the tapping hole is used less than or equal to 100 times, the calculation formula is: , When the tapping hole is used more than 100 times, the calculation formula is: , in, is the amount of silicon added, kg; The recovery rate of P element introduced into the alloy is calculated as 100%.
[0011] Furthermore, the effect of the amount of slag from the converter on the content of Si and Mn elements in the alloy batching process in the step (4) is that when the converter produces aluminum-killed steel, the aluminum blocks are added during the steel-tapping process to strongly deoxidize the molten steel, so that the Si and Mn elements in the slag are reduced to the molten steel, resulting in the amount of slag from the converter affecting the alloy batching; , in, is any one of the element components of Si and Mn in the molten steel, %; The amount of liquid steel in the converter when tapping steel i Element weight, kg; For the alloy i Element weight, kg; for i Element alloy yield, %; is the weight of molten steel, kg; , , in, is the weight of Si in the converter slag, kg; is the mass content of SiO2 in converter slag, %; is the weight of Mn in the converter slag, kg; is the mass content of MnO in converter slag, %; is the amount of slag in the converter, kg; The calculation formula of converter slag amount is as follows: , in, For converter slag Mass content, %; The amount of phosphorus brought into the converter slag is calculated as follows: , in, For the converter slag Weight, kg; is the oxygen content at the converter end point, ppm; is the slag discharging time, s.
[0012] Furthermore, the alloy composition and alloy price in the real-time database are updated according to the alloy storage batches.
[0013] The present invention also applies to protect a system for realizing the above-mentioned low-cost control method of aluminum killed steel converter steel alloy, including a client, a batching server and a memory. The client obtains the furnace number, steel type, scrap steel weight, molten iron weight, number of times the steel tapping hole is used, converter end oxygen content, component measurement information, steel type component control target, alloy price and alloy composition. The batching server completes the alloy batching calculation according to the steel type component control target, alloy price and alloy composition, and stores the real-time data of the converter and the calculation results into a database, updates the statistical regression formula of the alloy yield, and reads the P content in the refined steel liquid into the database to verify the calculation of the slag amount under the converter. The database and the calculation formula are stored in the memory.
[0014] The beneficial effects of the present invention are: The present invention can quickly and accurately batch the steel according to the current composition of the molten steel; When the test results of the chemical composition of the converter endpoint molten steel come out, the client loads the furnace number, steel type, molten steel weight, converter endpoint molten steel chemical composition, and the steel type composition control target corresponding to the furnace, clicks the batching calculation button, and starts the batching server to quickly and accurately calculate the addition amount of each alloy, optimize the batching, and improve production efficiency.
[0015] The present invention selects the alloy yield calculation formula according to the converter operating conditions, and the calculation result of the alloy addition amount is more scientific and accurate; The alloy recovery rate calculation formula is selected according to the converter operating conditions. In addition, as the number of times the converter tapping hole is used increases, the slag blocking effect of the slag blocking cone gradually deteriorates. The big data analysis method is used to predict the amount of slag in the converter and store it in the database. Considering the influence of the amount of slag in the converter on the alloy ingredients, it is helpful to improve the accuracy of the recovery rate of Si, Mn, and P elements. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is a control flow diagram of the present invention. DETAILED DESCRIPTION
[0017] The present invention is further illustrated by the following examples: The present invention can be better understood according to the following examples. However, it is easy for those skilled in the art to understand that the specific materials, process conditions and results described in the examples are only used to illustrate the present invention, and should not and will not limit the present invention described in detail in the claims.
[0018] The invention discloses a low-cost control method for aluminum killed steel converter tapping alloy. Figure 1 , including the following steps: Step (1) collects real-time data of the converter production process and establishes a database. The real-time data of the converter production process includes: furnace number, steel type, molten iron charge, scrap steel charge, number of times the tapping port is used, tapping time, converter end point composition, converter end point temperature, converter end point oxygen content, tapping amount, converter slag amount, converter end point slag composition, alloy addition amount during tapping, alloy composition of steel in the ladle after alloying, alloy composition, alloy price, steel target composition and alloy element recovery rate.
[0019] Step (2) limits the range of molten iron loading and scrap steel loading to stabilize the converter tapping. The converter tapping is calculated as follows: the converter molten iron loading is controlled within a range of 159-162 t, and the molten iron recovery rate is calculated according to an empirical value of 0.89; the converter scrap steel loading is controlled within a range of 46-48 t, and the scrap steel recovery rate is calculated according to an empirical value of 0.80.
[0020] Step (3) reads the parameters of the converter end oxygen content and the number of times the tapping hole is used according to the type of steel being smelted and the target carbon content of the steel type, and determines the calculation formula for the alloy element yield.
[0021] The alloy element yields are as follows: Aluminum yield The calculation process is: When the tapping hole is used less than or equal to 100 times, the calculation formula is: , When the tapping hole is used more than 100 times, the calculation formula is: , in, is the amount of aluminum added, kg; is the oxygen content at the converter end point, ppm; The number of times the tapping hole is used; Manganese recovery rate The calculation formula is: , in, is the amount of manganese added, kg; The calculation process of silicon yield is: When the tapping hole is used less than or equal to 100 times, the calculation formula is: , When the tapping hole is used more than 100 times, the calculation formula is: , in, is the amount of silicon added, kg; The recovery rate of P element introduced into the alloy is calculated as 100%.
[0022] Step (4) limits the tapping angle to between -104 and -100°C, controls the amount of slag in the converter, and reduces the impact of fluctuations in the amount of slag in the converter on the alloy yield. The impact of the amount of slag in the converter on the content of Si and Mn elements in the alloy batching process is that when the converter produces aluminum-killed steel, the aluminum block is added during the tapping process to strongly deoxidize the molten steel, causing the Si and Mn elements in the slag to be reduced to the molten steel, resulting in the amount of slag in the converter affecting the alloy batching; , in, is any one of Si and Mn elements in the molten steel, %; The amount of liquid steel in the converter when tapping steel i Element weight, kg; For the alloy i Element weight, kg; for i Element alloy yield, %; is the weight of molten steel, kg; , , in, is the weight of Si in the converter slag, kg; is the mass content of SiO2 in converter slag, %; is the weight of Mn in the converter slag, kg; is the mass content of MnO in converter slag, %; is the amount of slag in the converter, kg; The calculation formula of converter slag amount is as follows: , in, For converter slag Mass content, %; The amount of phosphorus brought into the converter slag is calculated as follows: , in, For the converter slag Weight, kg; is the oxygen content at the converter end point, ppm; is the slag discharging time, s.
[0023] Step (5) uses an improved linear programming solution method to establish an alloy addition solution model, and the alloy addition solution model takes the lowest total alloy addition cost Z as the objective function: , Where: is the price of alloy j, is the amount of alloy j added, n is the type of alloy; The constraints are as follows: ; in, is the lower limit of the composition of element i, %; Represents the content of element i in alloy j, %; is the weight of alloy j added, kg; is the weight of element i in the molten steel when tapping from the converter, kg; is the upper limit of the composition of element i, %; i is an alloying element; is the weight of element i reduced in the converter slag, kg; The amount of alloy added is less than the maximum amount of alloy that can be added: , in, is the maximum amount of the jth alloy added to the steel grade in actual production. The maximum amount of different alloys added to different steel grades is determined according to the process production requirements and stored in the database; Step (6) After the steel is tapped from the converter, the furnace number and the alloy addition amount are stored in the real-time database.
[0024] Step (6) After the steel is tapped from the converter, the furnace number and the alloy addition amount are stored in the real-time database. The alloy composition and alloy price in the real-time database are updated according to the alloy storage batch.
[0025] The following example shows the application of the present invention in actual production, taking the case where the applicant's steel plant produces X65 series steel and adds metal manganese, ferrosilicon and aluminum block alloys during the converter steel-out process to meet the element content requirements of the finished steel. The X65 series steel plant's controlled composition is shown in the following table. In the actual production process, the amount of alloy added is estimated by the furnace master based on experience, and the type of alloy is relatively fixed. Since the phosphorus content of this steel is <0.0189%, when the phosphorus content of the converter end steel liquid is low, a cheap alloy can be selected to replace the high-priced alloy.
[0026] Table 1 X65 series steel grade factory controlled finished product composition, %
[0027] According to the loading situation of the converter alloy silo, the selectable alloy types, alloy components and prices are shown in Table 2.
[0028] Table 2 Alloy price, yuan / kg
[0029] Table 3 Alloy composition, wt%
[0030] The objective function is to minimize the total cost of alloy addition:
[0031] At the same time, the following constraints are met:
[0032] Among them, the upper and lower limits of chemical composition are shown in Table 1.
[0033] The recovery rates of Si, Mn and Al elements are predicted based on the steel type and the oxygen content of the current furnace. The recovery rates of C, P, S and Cr elements are calculated as 100%.
[0034] Example 1
[0035] The molten iron loading is 165.0t, the scrap loading is 39.3t, the oxygen content at the converter end is 0.0577%, the converter end C: 0.04%, Si: 0.0001%, Mn: 0.084%, P: 0.0122%, S: 0.0051%, Cr: 0.018%, Al: 0.0%, the tapping hole is used 85 times, and the tapping time is 4.43 min, the alloy element recovery rate and the converter slag amount are read from the database, 1227kg silicon manganese, 1510kg metallic manganese, 370kg aluminum block, 800.35kg medium carbon ferromanganese, 273.15kg low carbon ferrochrome are added to the converter, and the composition of the molten steel is C: 0.0677%, Si: 0.145%, Mn: 1.5795%, P: 0.0144%, S: 0.0023%, Cr: 0.122%, Al: 0.0305%. The composition of the molten steel meets the process requirements. Compared with the original process, the cost per ton of steel of the new process is reduced by 7.2 yuan / ton.
[0036] Example 2
[0037] The amount of molten iron charged was 160.0t, the amount of scrap steel charged was 39.5t, the oxygen content at the converter end was 0.0612%, the C at the converter end was 0.021%, Si was 0.0031%, Mn was 0.0971%, P was 0.0121%, S was 0.0076%, Cr was 0.022%, Al was 0.0%, the number of times the tapping hole was used was 162 times, and the tapping time was 3.93 min, the alloy element recovery rate and the converter slag amount are read from the database, 1315kg silicon manganese, 1514kg metallic manganese, 394kg aluminum block, 649.3kg medium carbon ferromanganese, 301.51kg low carbon ferrochrome are added to the converter, and the composition of the molten steel is C: 0.078%, Si: 0.151%, Mn: 1.5784%, P: 0.0154%, S: 0.0016%, Cr: 0.13%, Al: 0.0303%. The composition of the molten steel meets the process requirements. Compared with the original process, the new process reduces the cost of steel by 8.0 yuan / ton.
[0038] Example 3
[0039] The molten iron charge was 165.12t, the scrap steel charge was 40.0t, the oxygen content at the converter end point was 0.0526%, the converter end point C: 0.042%, Si: 0.0001%, Mn: 0.0804%, P: 0.0107%, S: 0.0058%, Cr: 0.019%, Al: 0.0%, the tapping hole was used 172 times, the tapping time was 3.57min, the alloy element recovery rate and the converter slag amount were read from the database, 1023kg of silicon manganese, 1513kg of metallic manganese and 355kg of aluminum blocks were added into the converter tapping, and the composition of the molten steel was C: 0.0786%, Si: 0.142%, Mn: 1.5709%, P: 0.013%, S: 0.0016%, Cr: 0.118%, Al: 0.0287%. The composition of the molten steel meets the process requirements. Compared with the original process, the new process reduces the cost per ton of steel by 11.2 yuan / ton.
[0040] Based on the above ideal embodiments of the present invention, the relevant staff can make various changes and modifications without departing from the technical concept of the present invention through the above description. The technical scope of the present invention is not limited to the contents of the specification, and its technical scope must be determined according to the scope of the claims.
Claims
1. A low-cost control method for aluminum killed steel converter steel alloy, characterized in that: The following steps are involved: Step (1) collecting real-time data of the converter production process and establishing a database; Step (2) limits the range of molten iron loading and scrap steel loading to stabilize the output of the converter; Step (3) according to the steel type to be smelted and the target carbon content of the steel type, the parameters of the oxygen content at the converter end point and the number of times the tapping hole is used are read to determine the calculation formula for the alloy element yield; Step (4) limiting the tapping angle to between -104°C and -100°C, controlling the amount of slag in the converter, and reducing the influence of fluctuations in the amount of slag in the converter on the alloy yield; Step (5) uses an improved linear programming solution method to establish an alloy addition solution model, and the alloy addition solution model takes the lowest total alloy addition cost Z as the objective function: , Where: is the price of alloy j, is the amount of alloy j added, n is the type of alloy; The constraints are as follows: ; in, is the lower limit of the composition of element i, %; Represents the content of element i in alloy j, %; is the weight of alloy j added, kg; is the weight of element i in the molten steel when tapping from the converter, kg; is the upper limit of the composition of element i, %; i is an alloying element; is the weight of element i reduced in the converter slag, kg; The amount of alloy added is less than the maximum amount of alloy that can be added: , in, is the maximum amount of the jth alloy added to the steel grade in actual production. The maximum amount of different alloys added to different steel grades is determined according to the process production requirements and stored in the database; Step (6) After the steel is tapped from the converter, the furnace number and the alloy addition amount are stored in the real-time database.
2. The low-cost control method for aluminum killed steel converter steel alloy according to claim 1, characterized in that: The real-time data of the converter production process in step (1) include: furnace number, steel type, molten iron charge, scrap steel addition, number of times the tapping port is used, tapping time, converter end point composition, converter end point temperature, converter end point oxygen content, tapping amount, converter slag amount, converter end point slag composition, addition amount of each alloy in the tapping process, composition of the ladle steel liquid after alloying, alloy composition, alloy price, target composition of the steel liquid and alloy element recovery rate.
3. The low-cost control method for aluminum killed steel converter tapping alloy according to claim 1, characterized in that: The calculation process of the converter steel output in step (2) is as follows: the converter molten iron loading is controlled within a range of 159-162 t, and the molten iron recovery rate is calculated according to an empirical value of 0.89; the converter scrap steel loading is controlled within a range of 46-48 t, and the scrap steel recovery rate is calculated according to an empirical value of 0.
80.
4. The low-cost control method for aluminum killed steel converter tapping alloy according to claim 1, characterized in that: The alloy element yields in step (3) are as follows: Aluminum yield The calculation process is: When the tapping hole is used less than or equal to 100 times, the calculation formula is: , When the tapping hole is used more than 100 times, the calculation formula is: , in, is the amount of aluminum added, kg; is the oxygen content at the converter end point, ppm; The number of times the tapping hole is used; Manganese recovery rate The calculation formula is: , in, is the amount of manganese added, kg; The calculation process of silicon yield is: When the tapping hole is used less than or equal to 100 times, the calculation formula is: , When the tapping hole is used more than 100 times, the calculation formula is: , in, is the amount of silicon added, kg; The recovery rate of P element introduced into the alloy is calculated as 100%.
5. The low-cost control method for aluminum killed steel converter steel alloy according to claim 1, characterized in that: The effect of the amount of slag from the converter on the content of Si and Mn elements in the alloy batching process in step (4) is that when the converter produces aluminum-killed steel, the aluminum blocks are added during the steel-tapping process to strongly deoxidize the molten steel, so that the Si and Mn elements in the slag are reduced to the molten steel, resulting in the amount of slag from the converter affecting the alloy batching; , in, is any one of the element components of Si and Mn in the molten steel, %; The amount of liquid steel in the converter when tapping steel i Element weight, kg; For the alloy i Element weight, kg; for i Element alloy yield, %; is the weight of molten steel, kg; , , in, is the weight of Si in the converter slag, kg; is the mass content of SiO2 in converter slag, %; is the weight of Mn in the converter slag, kg; is the mass content of MnO in converter slag, %; is the amount of slag in the converter, kg; The calculation formula of converter slag amount is as follows: , in, For converter slag Mass content, %; The amount of phosphorus brought into the converter slag is calculated as follows: , in, For the converter slag Weight, kg; is the oxygen content at the converter end point, ppm; is the slag discharging time, s.
6. The low-cost control method for aluminum killed steel converter steel alloy according to claim 1, characterized in that: The alloy composition and alloy price in the real-time database are updated according to the alloy storage batches.
7. A system for realizing the low-cost control method for aluminum killed steel converter alloy tapping according to any one of claims 1 to 6, characterized in that: It includes a client, a batching server and a memory. The client obtains the furnace number, steel type, scrap steel weight, molten iron weight, number of times the steel tapping hole is used, the oxygen content of the converter end point, component measurement information, steel type component control target, alloy price and alloy composition. The batching server completes the alloy batching calculation according to the steel type component control target, alloy price and alloy composition, and stores the real-time data of the converter and the calculation results into the database, updates the statistical regression formula of the alloy yield, and reads the P content in the refined steel liquid into the database to verify the calculation of the slag amount under the converter. The database and the calculation formula are stored in the memory.
Citation Information
Patent Citations
Method for controlling alloy adding amount in converter tapping process
CN114196795A
Method and system for determining alloy adding amount in converter tapping process
CN114611844A
Converter low-cost alloy calculation method suitable for all steel types
CN116665791A
Calculation method of alloy ingredients in converter blowing
CN118626746A
Cited By
Minimum-cost alloy adding method for steelmaking converter
CN120485457A