Method for repairing crystallizer copper plate
Repairing the crystallizer copper plate through laser cladding and supersonic spraying technology solves the problem that traditional electroplating repair is difficult to deal with the upper and lower ports simultaneously, and efficient repair of the copper plate is achieved, which improves the over-steel volume and production efficiency, reduces costs, and makes repairs The process is more environmentally friendly and intelligent.
Patent Information
- Application Number
- CN202411239947.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-05
- Publication Date
- 2024-11-29
AI Technical Summary
Traditional restoration processes of crystallizer copper plates such as electroplating are difficult to synchronize the life of the upper and lower ports, which can easily cause electroplating pollution, affecting the quality of the casting blank, production efficiency and cost of continuous casting machines.
Laser cladding and supersonic spraying technology are used to spray the bottom layer and surface layer on the damaged surface of the copper plate, combining sandblasting and heat treatment to achieve the repair of the copper plate, avoid electroplating pollution, and improve the repair efficiency through automatic control throughout the process.
The oversteerage volume of copper plates is increased, the frequency of shutdowns of continuous casting production lines is reduced, the production cost is reduced, and the repair process is more environmentally friendly, green, efficient, and the operation is more intelligent.
Smart Images

Figure CN119035967A_ABST
Abstract
Description
Technical Field
[0001] The present application belongs to the technical field of crystallizer maintenance, and specifically relates to a method for repairing a crystallizer copper plate. Background Art
[0002] The crystallizer is the most critical component in the continuous casting production line. It receives the molten steel injected from the intermediate tank and solidifies it into a solid billet shell according to the specified cross-sectional shape. Its structure, material and performance parameters play a decisive role in the quality of the ingot and the production capacity of the casting machine. The crystallizer copper plate is an important heat-conducting component that solidifies the liquid molten steel into a solid billet shell. The molten steel flows through the crystallizer copper plate and crystallizes into a billet under the action of external cooling water. During the production process of the continuous casting machine, the dummy rod continuously pulls the billet from the crystallizer, which will cause wear on the copper plate surface and needs to be taken offline for remanufacturing and repair. For this reason, the quality of the crystallizer copper plate directly affects the continuous casting machine pulling speed and billet quality, and the amount of steel overload affects the production efficiency and production cost of the continuous casting machine.
[0003] The main failure forms of the crystallizer copper plate are the shedding of the upper coating and the wear of the lower coating. The traditional repair process of the copper plate is electroplating. Due to the limitations of process conditions, it is difficult to achieve a synchronous life of the upper and lower coatings. Most domestic peer manufacturers use electroplating technology to repair and remanufacture the crystallizer copper plate, which is prone to electroplating pollution. Summary of the invention
[0004] The purpose of the present application is to provide a method for repairing a crystallizer copper plate, aiming to solve the technical problem of the difficulty in repairing the crystallizer copper plate to at least a certain extent.
[0005] In order to solve the above technical problems, this application adopts the following technical solutions:
[0006] A first aspect of an embodiment of the present application provides a method for repairing a crystallizer copper plate, the method comprising the following steps:
[0007] Clean the surface of the copper plate to be repaired;
[0008] According to the damage condition of the copper plate, the coating structure for repair is designed using drawing software;
[0009] Perform milling on the damaged surface of the copper plate to be repaired to obtain a first processed surface;
[0010] Using a sandblasting device to sandblast the first processed surface to obtain a second processed surface;
[0011] Using laser cladding equipment to spray a molten base layer on the second processed surface to obtain a first repaired copper plate;
[0012] Using supersonic spraying equipment to spray a molten coating surface layer on the first repaired copper plate molten coating bottom layer to obtain a second repaired copper plate;
[0013] performing heat treatment on the second repaired copper plate to obtain a third repaired copper plate;
[0014] The third repaired copper plate is corrected to obtain a target copper plate.
[0015] In some embodiments, the specific steps of the laser cladding equipment spraying a molten base layer on the second processing surface are: using the laser cladding equipment to perform laser cladding priming on the second processing surface using the first powder, and the thickness of the cladding layer is 0.1mm~0.2mm; the working parameters of the laser cladding equipment are: power 2800W~3000W, moving speed 15mm / s~20mm / s, step distance 1.0mm~1.5mm.
[0016] In some embodiments, the first powder is a Ni-based alloy powder, and the proportions by weight are as follows: C: 0.06% to 0.08%; Cr: 0.30% to 0.40%; Si: 3.80% to 3.90%; Fe: 0.10% to 0.14%; B: 1.00% to 1.10%; Mo: 0.09% to 0.11%; Ni: balance.
[0017] In some embodiments, the specific steps of using supersonic spraying equipment to spray a molten surface layer on the first repaired copper plate molten coating bottom layer are: preheating the second powder to 50°C to 60°C; using supersonic spraying equipment to spray the second powder onto the surface of the molten coating bottom layer; the working parameters of the supersonic spraying equipment are: gun distance 500mm; powder feeding rate 100g / min, oxygen input 2000scfh; kerosene input 6gal / hr.
[0018] In some embodiments, the second powder is a Ni-based alloy powder, and the proportions by weight are as follows: C: 0.70% to 0.80%; Cr: 19% to 20%; Si: 4% to 5%; Fe: 3.0% to 3.2%; B: 2.6% to 2.8%; Mo: 1.8% to 1.9%; Ni: balance.
[0019] In some embodiments, the specific steps of using sandblasting equipment to sandblast the first processing surface are: using fully automatic sandblasting equipment, the spray gun is perpendicular to the first processing surface for sandblasting until the surface smoothness of the first processing surface reaches Ra15 or above; the working parameters of the fully automatic sandblasting equipment are: air pressure: 5kg / cm2; gun distance: 500mm.
[0020] In some embodiments, the sandblasting material of the fully automatic sandblasting equipment is cast steel sand GH40.
[0021] In some embodiments, the specific steps of heat treating the second repaired copper plate are: placing the second repaired copper plate in a heating furnace, filling it with argon for 1 hour to expel all the oxygen in the heating furnace; heating the temperature in the heating furnace to 900°C and keeping it warm for 30 minutes; stopping the argon gas flushing, and continuing to fill it with nitrogen to cool it to below 500°C; maintaining the temperature in the furnace at 450-480°C, keeping it warm for 3 hours, and then slowly cooling it with the furnace to below 150°C and taking it out of the furnace.
[0022] In some embodiments, the specific steps of performing milling on the damaged surface of the copper plate to be repaired are: according to the designed coating structure, using a CNC gantry milling machine to completely remove the coating on the surface of the copper plate to be repaired, and processing the first processing surface.
[0023] In some embodiments, the specific steps of cleaning the surface of the copper plate to be repaired are: cleaning the surface of the copper plate, grinding off the hardened layer on the surface of the copper plate using an angle grinder, and grinding off the dirt on the side of the copper plate.
[0024] It can be seen from the above technical solution that the present application has at least the following advantages and positive effects:
[0025] A method for repairing a crystallizer copper plate in the present application comprises the following steps: pre-treating the damaged surface of the copper plate, spraying a molten base layer on the damaged surface of the copper plate using a laser cladding device, and then using a supersonic spraying device to spray a molten surface layer on the first repaired copper plate molten base layer, thereby avoiding electroplating pollution. Compared with the original repair technology, the robot molten coating technology is more environmentally friendly, green, and efficient, the entire production process is automatically controlled, and the operation is more digital and intelligent. At the same time, by setting a molten base layer to connect the copper plate and the molten surface layer, the bonding strength of the molten coating layer is improved. After the copper plate is repaired by the method, the amount of steel passing through the crystallizer copper plate is increased, which greatly reduces the shutdown frequency of the continuous casting production line, improves the continuous casting operation rate, and reduces the production cost per ton of steel. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative work.
[0027] Figure 1 is a process flow chart of a method for repairing a crystallizer copper plate in an embodiment of the present application;
[0028] Figure 2 It is a structural schematic diagram of a melt-coating structure in a method for repairing a crystallizer copper plate in an embodiment of the present application.
[0029] The reference numerals are explained as follows: 1. melt-coated bottom layer; 2. melt-coated surface layer. DETAILED DESCRIPTION
[0030] In order to make the technical personnel in the technical field to which the present application belongs to understand the present application more clearly, the technical scheme in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without creative work are within the scope of protection of the present application.
[0031] Figure 1 is a process flow chart of a method for repairing a crystallizer copper plate in an embodiment of the present application, Figure 2 is a structural schematic diagram of a melt coating structure in a method for repairing a crystallizer copper plate in an embodiment of the present application, such as Figure 1 and Figure 2 As shown, the repair method includes the following steps:
[0032] S1: Clean the surface of the copper plate to be repaired;
[0033] Specifically, the specific steps for surface cleaning the copper plate to be repaired are: clean the surface of the copper plate, use an angle grinder to grind off the hardened layer on the surface of the copper plate, and grind off the dirt on the side of the copper plate. When grinding, pay attention to apply force evenly and do not grind out low spots locally.
[0034] S2: Based on the damage condition of the copper plate, use drawing software to design the coating structure for repair;
[0035] Specifically, according to the damage condition of the copper plate, a first processing surface is designed using two-dimensional drawing software, the first processing surface is an inclined surface, and a coating structure is designed on the first processing surface.
[0036] like Figure 2 As shown, the molten coating structure is a composite molten coating layer, and the molten coating structure includes a molten coating bottom layer 1 and a molten coating surface layer 2.
[0037] S3: performing milling on the damaged surface of the copper plate to be repaired to obtain a first processed surface;
[0038] Specifically, the specific steps of milling the damaged surface of the copper plate to be repaired are: designing a first processing surface drawing according to the two-dimensional drawing software in S2, inputting the drawing into a CNC gantry milling device, using the CNC gantry milling device to remove all coatings on the surface of the copper plate to be repaired, and processing the first processing surface.
[0039] S4: sandblasting the first processed surface using a sandblasting device to obtain a second processed surface;
[0040] Specifically, the specific steps of using the sandblasting equipment to sandblast the first processing surface are: using the fully automatic sandblasting equipment, the spray gun is perpendicular to the first processing surface to perform sandblasting until the surface smoothness of the first processing surface reaches Ra15 or above; the working parameters of the fully automatic sandblasting equipment are: air pressure: 5kg / cm2; gun distance: 500mm. The purpose of using sandblasting is to make the surface of the second processing surface smoother and convenient for spraying. The sandblasting material of the fully automatic sandblasting equipment is cast steel sand GH40.
[0041] S5: using laser cladding equipment to spray a molten base layer on the second processed surface to obtain a first repaired copper plate;
[0042] Specifically, the second processing surface is laser clad with the first powder by laser cladding equipment, and the thickness of the cladding layer is 0.1mm-0.2mm; the working parameters of the laser cladding equipment are: power 2800W-3000W, moving speed 15mm / s-20mm / s, and step distance 1.0mm-1.5mm.
[0043] The first powder is a Ni-based alloy powder, and the proportions thereof are as follows by weight percentage: C: 0.07%; Cr: 0.35%; Si: 3.85%; Fe: 0.12%; B: 1.04%; Mo: 0.1%; and Ni: the balance.
[0044] S6: using a supersonic spraying device to spray a molten coating surface layer on the first repaired copper plate molten coating bottom layer to obtain a second repaired copper plate;
[0045] Specifically, the specific steps of using supersonic spraying equipment to spray a molten surface layer on the first repaired copper plate molten coating bottom layer are: preheating the second powder to 50°C to 60°C; using supersonic spraying equipment to spray the second powder onto the surface of the molten coating bottom layer; the working parameters of the supersonic spraying equipment are: gun distance 500mm; powder feeding rate 100g / min, oxygen input 2000scfh; kerosene input 6gal / hr.
[0046] The second powder is a Ni-based alloy powder, and the proportions thereof are as follows by weight percentage: C: 0.75%; Cr: 19.5%; Si: 4.5%; Fe: 3.1%; B: 2.7%; Mo: 1.9%; and Ni: the balance.
[0047] S7: heat-treating the second repaired copper plate to obtain a third repaired copper plate;
[0048] Specifically, the specific steps of heat treating the second repaired copper plate are: placing the second repaired copper plate in a heating furnace, filling it with argon for 1 hour to expel all the oxygen in the heating furnace; heating the temperature in the heating furnace to 900°C and keeping it warm for 30 minutes; stopping the argon filling, and continuing to fill it with nitrogen to cool it to below 500°C; maintaining the temperature in the furnace at 450-480°C, keeping it warm for 3 hours, and then slowly cooling it with the furnace to below 150°C and taking it out of the furnace.
[0049] S8: performing correction processing on the third repaired copper plate to obtain a target copper plate.
[0050] Specifically, due to the high temperature, the copper plate will deform after being melted. In order to facilitate subsequent processing, the copper plate is milled and ground on a gantry leveling machine according to the requirements of the drawing to meet the technical requirements. The flatness requirement for the wide copper plate is <0.5mm; the flatness requirement for the narrow copper plate is <0.3mm.
[0051] During the specific implementation of this embodiment, the copper plate repaired by this method is applied to the crystallizer of a medium and low speed casting machine (the ladle capacity is 220t, the slab size is 900-1600mm×230mm, the continuous casting machine radius is 9.5m, the metallurgical length is 34.5m, and the pulling speed is 0.8-1.7m / min). After testing, the copper plate repaired by this method actually has an online steel passing rate of 257,800 tons, which is more than 2.5 times the steel passing rate of the original electroplating process (80,000-100,000 tons). The increase in the steel passing rate of the crystallizer copper plate has greatly reduced the shutdown frequency of the continuous casting production line, improved the continuous casting operation rate, and reduced the production cost per ton of steel.
[0052] It can be seen from the above technical solution that the present application has at least the following advantages and positive effects:
[0053] A method for repairing a crystallizer copper plate in the present application comprises the following steps: pre-treating the damaged surface of the copper plate, spraying a molten base layer on the damaged surface of the copper plate using a laser cladding device, and then using a supersonic spraying device to spray a molten surface layer on the first repaired copper plate molten base layer, thereby avoiding electroplating pollution. Compared with the original repair technology, the robot molten coating technology is more environmentally friendly, green, and efficient, the entire production process is automatically controlled, and the operation is more digital and intelligent. At the same time, by setting a molten base layer to connect the copper plate and the molten surface layer, the bonding strength of the molten coating layer is improved. After the copper plate is repaired by the method, the amount of steel passing through the crystallizer copper plate is increased, which greatly reduces the shutdown frequency of the continuous casting production line, improves the continuous casting operation rate, and reduces the production cost per ton of steel.
[0054] Unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include the first and second features being in direct contact, or may include the first and second features not being in direct contact but being in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes the first feature being directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes the first feature being directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0055] In the description of the present application, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise" and "counterclockwise" indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0056] In this application, unless otherwise clearly specified and limited, the terms "connection", "fixation", etc. should be understood in a broad sense. For example, "fixation" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0057] In addition, the descriptions of "first", "second", etc. in this application are only for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" or "second" may explicitly or implicitly include one or more features. In the description of this application, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0058] Although the embodiments of the present application have been shown and described, those skilled in the art will appreciate that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present application, and that the scope of the present application is defined by the claims and their equivalents.
Claims
1. A method for repairing a crystallizer copper plate, It is characterized in that The repair method comprises the following steps: Clean the surface of the copper plate to be repaired; According to the damage condition of the copper plate, the coating structure for repair is designed using drawing software; Perform milling on the damaged surface of the copper plate to be repaired to obtain a first processed surface; Using a sandblasting device to sandblast the first processed surface to obtain a second processed surface; Using laser cladding equipment to spray a molten base layer on the second processed surface to obtain a first repaired copper plate; Using supersonic spraying equipment to spray a molten coating surface layer on the first repaired copper plate molten coating bottom layer to obtain a second repaired copper plate; heat treating the second repaired copper plate to obtain a third repaired copper plate; The third repaired copper plate is corrected to obtain a target copper plate.
2. The method for repairing a crystallizer copper plate according to claim 1, It is characterized in that The specific steps of the laser cladding equipment spraying the cladding bottom layer on the second processing surface are: Using a laser cladding device to perform laser cladding primer on the second processing surface using a first powder, wherein the thickness of the primer layer is 0.1 mm to 0.2 mm; The working parameters of the laser cladding equipment are: power 2800W-3000W, moving speed 15mm / s-20mm / s, and step distance 1.0mm-1.5mm.
3. The method for repairing a crystallizer copper plate according to claim 2, It is characterized in that The first powder is a Ni-based alloy powder, and the proportion by weight percentage is as follows: C: 0.06%~0.08%; Cr: 0.30%~0.40%; Si: 3.80%~3.90%; Fe: 0.10%~0.14%; B: 1.00%~1.10%; Mo: 0.09%~0.11%; Ni: balance 4. The method for repairing a crystallizer copper plate according to claim 1, It is characterized in that The specific steps of using the supersonic spraying equipment to spray the melt-coated surface layer on the first repaired copper plate melt-coated bottom layer are: Preheat the second powder to 50°C to 60°C; The second powder was sprayed onto the surface of the solvent-coated bottom layer using a supersonic spraying device; the working parameters of the supersonic spraying device were: a gun distance of 500 mm; a powder feeding rate of 100 g / min, an oxygen input of 2000 scfh; and a kerosene input of 6 gal / hr.
5. The method for repairing a crystallizer copper plate according to claim 4, It is characterized in that The second powder is a Ni-based alloy powder, and the weight percentage ratio is as follows: C: 0.70% ~ 0.80%; Cr: 19% ~ 20%; Si: 4% ~ 5%; Fe: 3.0% ~ 3.2%; B: 2.6% ~ 2.8%; Mo: 1.8% ~ 1.9%; Ni: balance.
6. The method for repairing a crystallizer copper plate according to claim 1, It is characterized in that The specific steps of using the sandblasting equipment to sandblast the first processed surface are: Using fully automatic sandblasting equipment, with the spray gun perpendicular to the first processing surface, to perform sandblasting until the surface smoothness of the first processing surface reaches Ra15 or above; The working parameters of the fully automatic sandblasting equipment are: air pressure: 5kg / cm2; gun distance: 500mm.
7. The method for repairing a crystallizer copper plate according to claim 6, It is characterized in that The sandblasting material of the fully automatic sandblasting equipment is cast steel sand GH40.
8. The method for repairing a crystallizer copper plate according to claim 1, It is characterized in that The specific steps of heat treating the second repaired copper plate are: The second repaired copper plate is placed in a heating furnace and filled with argon gas for 1 hour to exhaust all the oxygen in the heating furnace; Heat the temperature in the heating furnace to 900°C and keep it warm for 30 minutes; Stop charging argon and continue to charge nitrogen to cool down to below 500℃; Keep the temperature in the furnace at 450-480℃, keep it warm for 3 hours, then slowly cool it down to below 150℃ and take it out of the furnace.
9. The method for repairing a crystallizer copper plate according to claim 1, It is characterized in that The specific steps of performing milling on the damaged surface of the copper plate to be repaired are: According to the designed coating structure, a CNC gantry milling machine is used to remove all coatings on the surface of the copper plate to be repaired, and the first processing surface is processed.
10. The method for repairing a crystallizer copper plate according to claim 1, It is characterized in that The specific steps of surface cleaning the copper plate to be repaired are: Clean the surface of the copper plate, use an angle grinder to grind off the hardened layer on the surface of the copper plate, and grind off the dirt on the side of the copper plate.
Citation Information
Cited By
Processing method applied to flame coating melting crystallizer copper plate coating
CN120941206A