Vacuum coating film thickness monitoring method and device
By setting up test points and optical data comparison systems in the vacuum coating equipment, the problem of online film thickness monitoring is solved, real-time detection of the film layer and efficient utilization of resources are achieved, and process abnormalities and resource waste are avoided.
Patent Information
- Application Number
- CN202310615746.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-29
- Publication Date
- 2024-11-29
AI Technical Summary
Existing vacuum coating equipment cannot conduct online film thickness monitoring, resulting in difficulty in film layer control, abnormal process or product scrapping, and comprehensive coverage of the substrate is required when measuring film thickness, resulting in waste of resources.
By setting test points in vacuum coating equipment, pre-monitoring the standard optical parameters of the film, collecting optical data using light sources and signal receivers, comparing and feedbacking differences in real time, real-time film thickness abnormality detection and control, including adjusting the evaporation rate or issuing alarm.
Accurate and real-time detection of the film layer is achieved, resource waste is avoided, and the accuracy of the film layer and process stability are ensured.
Smart Images

Figure CN119040837A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of vacuum coating, and in particular to a method and device for monitoring the film thickness of vacuum coating. Background Art
[0002] In the prior art, the film thickness monitoring method for vacuum coating equipment is relatively simple. The evaporation equipment mainly monitors the film thickness through a crystal oscillator. However, the decomposition reaction during the evaporation of organic salt materials (FAI / MAI / PEAI, etc.) leads to inaccurate film thickness monitoring; equipment such as Sputter does not have online film thickness monitoring equipment and can only perform film thickness testing after the process is completed. Since online film thickness monitoring cannot be performed, it is impossible to understand the actual film formation situation in the vacuum chamber, which is not conducive to the control of the film layer, resulting in process abnormalities or product scrapping. When a certain film thickness needs to be measured during an experiment, the substrate needs to be fully covered, resulting in a waste of resources. Summary of the invention
[0003] 1. Technical issues to be resolved
[0004] In view of the above-mentioned shortcomings and deficiencies of the prior art, the present invention provides a method and device for monitoring the thickness of vacuum coating, which solves the problem that the actual film formation situation in the vacuum chamber cannot be understood due to the inability to perform online film thickness monitoring, which is not conducive to the control of the film layer, resulting in process abnormalities or product scrapping; when it is necessary to measure a certain film thickness during an experiment, the substrate needs to be fully covered, resulting in a waste of resources.
[0005] (II) Technical solution
[0006] In order to achieve the above-mentioned object, a first aspect of the present invention provides a method for monitoring the film thickness of a vacuum coating.
[0007] A second aspect of the present invention provides a vacuum coating film thickness monitoring device.
[0008] In view of this, according to a first aspect of an embodiment of the present application, a method for monitoring the thickness of a vacuum coating is proposed, the method comprising:
[0009] Deposit a pre-monitored film at the test point and set a standard optical parameter A of the pre-monitored film;
[0010] The light source selects light of a corresponding wavelength according to the material of the deposited pre-monitored thin film;
[0011] The signal receiver collects the light source information under different film thicknesses and obtains the actual optical parameter B after the light passes through the film;
[0012] The actual optical parameter B is fed back to the information processing unit and converted into a digital signal, which is reflected on the electronic screen and compared with the preset standard optical parameter A;
[0013] When the difference between the standard optical parameter A and the actual optical parameter B exceeds 5%, it is considered as abnormal film thickness and feedback control is performed.
[0014] In one implementation, a pre-monitored thin film is deposited at a test point, and a standard optical parameter A of the pre-monitored thin film is set, including:
[0015] The standard optical parameters A include absorbance, transmittance, and refractive index.
[0016] In one implementation, the light source selects light of a corresponding wavelength according to the material of the deposited pre-monitored thin film, including:
[0017] The material of the thin film will absorb light of a specific wavelength, and the color of a specific film layer structure will change as the thickness changes. The degree of change can be characterized by optical data.
[0018] In one implementation, the signal receiver collects light source information under different film thicknesses to obtain actual optical parameters B after light passes through the film, including:
[0019] The actual optical parameters B include absorbance, transmittance, and refractive index.
[0020] In one implementation, the actual optical parameter B is fed back to the information processing unit and converted into a digital signal, which is reflected on the electronic screen and compared with the preset standard optical parameter A, including:
[0021] The information processing unit can be connected to the outside of the vacuum coating machine chamber by wireless or wired means.
[0022] In one implementation, when the difference between the standard optical parameter A and the actual optical parameter B exceeds 5%, it is considered as abnormal film thickness and feedback control is performed, including:
[0023] Feedback control can control the evaporation rate by adjusting the temperature of the heating wire or issue an alarm to notify staff to handle the matter.
[0024] According to a second aspect of the embodiment of the present application, a vacuum coating film thickness monitoring device suitable for a vacuum coating film thickness monitoring method is provided, comprising: a frame, a signal receiver, a substrate, a light source transmitter, a light source protection box, and a test point;
[0025] The frame is arranged inside the vacuum coating equipment, and a tray is provided under the frame; a signal receiver is provided on the inner side of the frame close to the substrate; a test point is provided at the position of the substrate corresponding to the signal receiver; a light source transmitter is provided under the substrate; and a light source protection box is provided outside the light source transmitter.
[0026] In one implementation, the signal receiver, the test point, and the light source transmitter are in a straight line.
[0027] In one implementation, an opening is provided above the light source protection box.
[0028] In one implementation, the light source emitter can be angle-adjustable.
[0029] In one implementation, the frame is a movable fixing device in a vacuum coating machine.
[0030] According to a third aspect of an embodiment of the present application, an electronic device is proposed, comprising a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein when the processor executes the program, the steps of a vacuum coating film thickness monitoring method as described in any one of claims 1 to 6 are implemented.
[0031] (III) Beneficial effects
[0032] The beneficial effects of the present invention are:
[0033] The present invention provides a vacuum coating film thickness monitoring method and device. By setting measurement points, specific positions in continuous multi-process sections are exposed only in specific process sections, so that there are only one or several film layer structures at specific positions in a large-area substrate, which is convenient for film layer detection and ensures the accuracy and real-time performance of single film layer measurement. Measurement is fixed near the measurement point to avoid waste of resources. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings in the following description are only embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the provided drawings without paying any creative work.
[0035] Figure 1 A flow chart of a vacuum coating film thickness monitoring method provided in this application;
[0036] Figure 2 A schematic diagram of a vacuum coating film thickness monitoring device for a rotary vacuum coating machine of a vacuum coating film thickness monitoring device provided in the present application;
[0037] Figure 3 A schematic diagram of a vacuum coating film thickness monitoring device for an Inline vacuum coating machine provided by the present application;
[0038] Figure 4A schematic diagram of a support opening of a vacuum coating film thickness monitoring device of an Inline vacuum coating machine of a vacuum coating film thickness monitoring device provided in the present application;
[0039] Figure 5 A schematic diagram of a vacuum coating film thickness refractive index monitoring method of a rotary vacuum coating machine of a vacuum coating film thickness monitoring device provided in the present application.
[0040] Illustration: 1: frame; 2: signal receiver; 3: substrate; 4: light source transmitter; 5: light source protection box; 6: test point; 7: evaporation source or other coating source; 101: hanging beam; 102: tray; 103: roller; 104: bracket; 105: support plate opening; 501: opening. DETAILED DESCRIPTION
[0041] It should be understood that the specific embodiments described herein are only used to explain the present invention, and are not used to limit the present invention.
[0042] The method and system of the present invention are further described below in conjunction with specific embodiments.
[0043] First, as Figure 1 As shown, the present application provides a method for monitoring the thickness of a vacuum coating film, the method comprising:
[0044] S100 deposits a pre-monitored thin film at the test point and sets the standard optical parameter A of the pre-monitored thin film.
[0045] In this embodiment, the standard optical parameter A includes absorbance, transmittance, and refractive index.
[0046] In this embodiment, the preset value is calculated as follows:
[0047] The evaporation rate is v1, the detection interval is t, the evaporation thickness in each cycle is s (s = v1 * t), and the optical coefficient of a material is a. The optical parameters can be calculated. For example, according to Beer's law, the absorbance A = evaporation thickness s × absorption cell optical path length b × absorption coefficient a.
[0048] In this embodiment, the test point is a TEG point. The TEG point is a technical method adopted by the OLED industry, and is now innovatively introduced into the photovoltaic industry, taking the perovskite industry as an example; the OLED industry TEG uses a mask (metal mask) to expose at a specific position, and in a continuous multi-process segment, a specific position is only exposed in a specific process segment, so that there is only one or several film layer structures at a specific position in a large-area substrate, which is convenient for film layer detection. Masks are not used in industries such as the perovskite industry, but a certain distance (5 to 10 mm) can be extended at a fixed position on the edge of the tray or bracket, and holes can be opened in the fixed position area, so as to realize the thin film deposition at a specific position in a specific process segment, and then realize online film thickness monitoring.
[0049] The S200 light source selects light of a corresponding wavelength according to the material of the deposited pre-monitored thin film.
[0050] In this embodiment, the film material will absorb specific wavelengths, and the color of the specific film structure will change as the thickness changes. The degree of change can be characterized by optical data. For example, in the deposition of perovskite layer, metal salts such as PbI2 are deposited to prepare organic salts such as FAI, and their color will change as the thickness of organic salts such as FAI changes.
[0051] On the side wall of the chamber, a light source with a specific wavelength (the specific wavelength can be selected according to the sensitive wavelength of the film material thickness change) is adjusted to adjust the angle of the light source so that the direction of the light source corresponds to the position of the test point.
[0052] The S300 signal receiver collects light source information under different film thicknesses and obtains the actual optical parameter B after the light passes through the film.
[0053] In this embodiment, the actual optical parameter B includes absorbance, transmittance, and refractive index.
[0054] S400 feeds back the actual optical parameter B to the information processing unit, converts it into a digital signal, and displays it on the electronic screen for comparison with the preset standard optical parameter A.
[0055] In this embodiment, the digital signal of the optical data can be fed back to the information processing unit by connecting to the outside of the vacuum coating machine wirelessly or by wire.
[0056] S500 When the difference between the standard optical parameter A and the actual optical parameter B exceeds 5%, it is considered as abnormal film thickness and feedback control is performed.
[0057] In this embodiment, the feedback control can control the evaporation rate by adjusting the temperature of the heating wire or issue an alarm to notify the staff to handle the matter.
[0058] In a second aspect, the present application provides a vacuum coating film thickness monitoring device, comprising: a frame 1, a signal receiver 2, a substrate 3, a light source transmitter 4, a light source protection box 5, and a test point 6;
[0059] A frame 1 is arranged inside the vacuum coating equipment, and a tray 3 is provided under the frame 1; a signal receiver 2 is provided on the inner side of the frame 1 close to the substrate 3, which can collect light information of the light source passing through the substrate; a test point 6 is provided at the position of the substrate 3 corresponding to the signal receiver 2; a light source transmitter 4 is provided under the substrate 3; and a light source protection box 5 is provided outside the light source transmitter 4.
[0060] In this embodiment, the signal receiver 2 , the test point 6 , and the light source transmitter 4 are located in a straight line.
[0061] In this embodiment, an opening 501 is provided above the light source protection box 5 , and the light source protection box 5 plays a role in protecting the light source to prevent the vacuum coating from affecting the light source. The opening 501 of the light source protection box 5 will be opened during testing.
[0062] In this embodiment, the light source transmitter 4 can be angle-adjusted, and different corresponding wavelengths can be selected for different materials. For example, FAI can use about 271nm, and the fixed angle can be adjusted to correspond to the position to be tested so that the light source, test point 6 and signal receiver 2 are in a straight line.
[0063] In this embodiment, the frame 1 is a movable fixing device in the vacuum coating machine.
[0064] Specifically, Figure 2 As shown, in a rotary vacuum coating machine, the frame 1 is a suspended structure, the frame 1 sets the tray 102 in the vacuum coating machine through the hanging beam 101, and the signal receiver 2 is located at the corresponding test point position of the tray 102. Figure 5 As shown, when monitoring the film thickness by refractive index, the signal receiver 2 needs to be set in the vacuum chamber in a direction opposite to the light source 4, so that the light source 4, the test point 6, and the signal receiver 2 form a right triangle.
[0065] During actual use, the tray 102 will rotate at a constant speed (20 to 30 revolutions / min), and the absorption sampling interval is 10 to 500 ms. For qualitative characterization of film thickness changes, 20 to 30 revolutions / min rotation can meet the needs. For quantitative characterization of film thickness changes, the rotation can be stopped at a specified position.
[0066] Specifically, Figure 3 As shown, in an Inline vacuum coating machine, the frame 1 is a bracket structure, the frame 1 sets the bracket 104 in the vacuum coating machine through the roller 103, and the signal receiver 2 is located at the position of the bracket 104 corresponding to the test point 6. Figure 4As shown, the length of the support sheet is extended at the position of the test point 6 on the lower side of the substrate 3, and a hole is opened at the corresponding position of the test point 6, so that the light source, the support sheet opening 105, the test point 6, and the signal receiver are in a straight line. In actual use, the bracket will move forward at a uniform speed (10-20 mm / s), and the absorption sampling interval is 10-500ms. If the film thickness change is qualitatively characterized, 10-20 mm / s can meet the needs. If the film thickness change is quantitatively characterized, the film thickness can be measured by stopping the substrate after the process is accepted.
[0067] In a third aspect, the present application provides an electronic device comprising a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the processor implements the steps of a vacuum coating film thickness monitoring device as described in any one of claims 1 to 6 when executing the program.
[0068] Those skilled in the art will readily appreciate other embodiments of the present invention after considering the specification and practicing the invention disclosed herein. This application is intended to cover any variations, uses or adaptations of the present invention, which follow the general principles of the present invention and include common knowledge or customary techniques in the art that are not disclosed by the present invention. The specification and examples are intended to be exemplary only, and the true scope and spirit of the present invention are indicated by the claims of the present application.
Claims
1. A method for monitoring the thickness of a vacuum coating, characterized in that: The method comprises: Deposit a pre-monitored film at the test point and set a standard optical parameter A of the pre-monitored film; The light source selects light of a corresponding wavelength according to the material of the deposited pre-monitored thin film; The signal receiver collects the light source information under different film thicknesses and obtains the actual optical parameter B after the light passes through the film; The actual optical parameter B is fed back to the information processing unit and converted into a digital signal, which is reflected on the electronic screen and compared with the preset standard optical parameter A; When the difference between the standard optical parameter A and the actual optical parameter B exceeds 5%, it is considered as abnormal film thickness and feedback control is performed.
2. A vacuum coating film thickness monitoring method as claimed in claim 1, characterized in that: Deposit the pre-monitored film at the test point and set the standard optical parameters A of the pre-monitored film, including: The standard optical parameters A include absorbance, transmittance, and refractive index.
3. A vacuum coating film thickness monitoring method as claimed in claim 1, characterized in that: The light source selects the corresponding wavelength of light according to the material of the deposited pre-monitored thin film, including: The material of the thin film will absorb light of a specific wavelength, and the color of a specific film layer structure will change as the thickness changes. The degree of change can be characterized by optical data.
4. A vacuum coating film thickness monitoring method as claimed in claim 1, characterized in that: The signal receiver collects light source information under different film thicknesses and obtains the actual optical parameters B after the light passes through the film, including: The actual optical parameters B include absorbance, transmittance, and refractive index.
5. A vacuum coating film thickness monitoring method as claimed in claim 1, characterized in that: The actual optical parameter B is fed back to the information processing unit and converted into a digital signal and displayed on the electronic screen for comparison with the preset standard optical parameter A, including: The information processing unit can be connected to the outside of the vacuum coating machine chamber by wireless or wired means.
6. A vacuum coating film thickness monitoring method as claimed in claim 1, characterized in that: When the difference between the standard optical parameter A and the actual optical parameter B exceeds 5%, it is considered as abnormal film thickness and feedback control is performed, including: Feedback control can control the evaporation rate by adjusting the temperature of the heating wire or issue an alarm to notify staff to handle the matter.
7. A vacuum coating film thickness monitoring device applicable to a vacuum coating film thickness monitoring method as claimed in claims 1 to 6, characterized in that: include: A frame (1), a signal receiver (2), a base plate (3), a light source transmitter (4), a light source protection box (5), and a test point (6); The frame (1) is arranged inside the vacuum coating equipment, and a tray (3) is arranged below the frame (1); a signal receiver (2) is arranged on the inner side of the frame (1) close to the substrate (3); a test point (6) is arranged at a position of the substrate (3) corresponding to the signal receiver (2); a light source transmitter (4) is arranged below the substrate (3); and a light source protection box (5) is arranged outside the light source transmitter (4).
8. A vacuum coating film thickness monitoring device as claimed in claim 5, characterized in that: An opening (501) is provided above the light source protection box (5).
9. A vacuum coating film thickness monitoring device as claimed in claim 5, characterized in that: The light source emitter (4) can be angle-adjusted.
10. An electronic device comprising a memory, a processor, and a computer program stored in the memory and executable on the processor, characterized in that: When the processor executes the program, a vacuum coating film thickness monitoring method as described in claims 1 to 6 is implemented.
Citation Information