Cleaning method for improving after-tack defect of silicon surface oxide and manufacturing method of semiconductor device
The sacrificial oxide layer on the wafer surface is removed through a two-step cleaning method, which reduces the risk of oxide re-adhesion, solves the problem of oxide re-adhesion defects on the wafer surface in the prior art, and improves the performance and yield of semiconductor devices.
Patent Information
- Application Number
- CN202411148843.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-20
- Publication Date
- 2024-11-29
AI Technical Summary
In the existing wafer manufacturing process, there are still serious oxide back-tight defects on the surface of the cleaned wafer, which is difficult to meet the requirements of semiconductor processes for electrical stability, consistency and yield.
Two-step cleaning method is adopted: the first step is to remove the partial thickness of the sacrificial oxide layer using SPM solution and the first HF solution, and the second step is to remove the remaining sacrificial oxide layer using the second HF solution, SC1 solution and SC2 solution to reduce the oxide back Risk of stickiness.
It effectively reduces the occurrence of silicon surface oxide back-touch defects and improves the performance and yield of semiconductor devices.
Smart Images

Figure CN119049959A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of semiconductor technology, and in particular to a cleaning method for improving oxide back-adhesion defects on a silicon surface and a method for manufacturing a semiconductor device. Background Art
[0002] During the wafer manufacturing process, especially before the gate oxide layer grows, the cleanliness of the wafer surface is extremely high, because any tiny surface defect may continue to grow and be difficult to remove during the subsequent oxide layer growth and polysilicon deposition process, becoming a more complex defect source that affects device performance. These defects not only affect the quality of the gate oxide layer, but also have a destructive effect on the electrical performance of the device.
[0003] In order to improve the cleanliness of the wafer surface, the existing wafer manufacturing process usually adopts a wet cleaning process, generally using one or more cleaning solutions such as sulfuric acid hydrogen peroxide solution (SPM solution), hydrofluoric acid solution (HF solution), ammonia hydrogen peroxide solution (SC1 solution), and hydrochloric acid hydrogen peroxide solution (SC2 solution) to clean the wafer. However, actual applications have found that there are still serious defects on the surface of the wafer after cleaning with the existing cleaning method, which makes it difficult to meet the increasingly high development needs of semiconductor processes for the electrical stability, consistency and yield of wafers.
[0004] Therefore, there is an urgent need in the art to develop a new wafer surface cleaning method to minimize the generation of defects. Summary of the invention
[0005] The purpose of the present invention is to provide a cleaning method for improving oxide back-sticking defects on the silicon surface. The cleaning method first removes a sacrificial oxide layer of a certain thickness by a first cleaning to avoid oxide back-sticking defects caused by exposure of the silicon substrate; and then removes the remaining sacrificial oxide layer by a second cleaning. During the second cleaning, the oxide content in the second HF solution is significantly reduced, and the risk of oxide back-sticking on the exposed silicon substrate surface is also reduced. The cleaning method of the present invention effectively improves the generation of oxide back-sticking defects on the silicon surface.
[0006] In order to achieve the above object, the present invention provides a cleaning method for improving the oxide back-adhesion defect on the silicon surface, comprising the following steps:
[0007] Step S1, providing a wafer and placing it in a cleaning tank, wherein the wafer comprises: a silicon substrate and a sacrificial oxide layer covering a surface of the silicon substrate;
[0008] Step S2, using the SPM solution and the first HF solution in sequence to perform a first cleaning on the wafer to remove a portion of the sacrificial oxide layer;
[0009] Step S3, using a second HF solution, an SC1 solution, and an SC2 solution in sequence to perform a second cleaning on the first cleaned wafer to remove the remaining sacrificial oxide layer on the surface of the wafer.
[0010] Optionally, the concentration of the first HF solution is greater than the concentration of the second HF solution.
[0011] Optionally, in the first HF solution and the second HF solution, the volume ratio of the hydrofluoric acid original solution to water is 1:50-200, and the concentration of the hydrofluoric acid original solution is 40w / w%-50w / w%.
[0012] Optionally, the ratio of the hydrofluoric acid original solution to water in the first HF solution is 1:100, the cleaning temperature is 20° C.-25° C., and the cleaning time is 3 min-4 min.
[0013] Optionally, the ratio of the hydrofluoric acid original solution to water in the second HF solution is 1:200, the cleaning temperature is 20° C.-25° C., and the cleaning time is 1 min-2 min.
[0014] Optionally, in the SPM solution, the volume ratio of sulfuric acid to hydrogen peroxide is 1:3-8, and the cleaning temperature is 100°C-150°C;
[0015] In the SC1 solution, the volume ratio of ammonia water, hydrogen peroxide and deionized water is 1:2:50, and the cleaning temperature is 65°C-85°C;
[0016] In the SC2 solution, the volume ratio of hydrochloric acid, hydrogen peroxide and deionized water is 1:1:50, and the cleaning temperature is 65°C-85°C.
[0017] Optionally, the thickness of the portion is 50%-90% of the total thickness of the sacrificial oxide layer.
[0018] Optionally, the total thickness of the sacrificial oxide layer is 6nm-10nm.
[0019] Optionally, the sacrificial oxide layer includes a silicon dioxide layer.
[0020] Optionally, the number of wafers in the cleaning tank is at least two, and the distance between adjacent wafers is greater than 2 cm.
[0021] Optionally, the method further comprises: in steps S2 and S3, before cleaning with any one of the SPM solution, the first HF solution, the second HF solution, the SC1 solution and the SC2 solution, rinsing the wafer with deionized water; and,
[0022] Step S4, rinsing the wafer with deionized water and completing drying.
[0023] Optionally, the first cleaning tank carries the SPM solution, the second cleaning tank carries the first HF solution, and the first cleaning of the wafer includes: placing the wafer in the first cleaning tank and the second cleaning tank in sequence for cleaning.
[0024] Optionally, the third cleaning tank carries the second HF solution, the fourth cleaning tank carries the SC1 solution, and the fifth cleaning tank carries the SC2 solution. The second cleaning of the wafer includes: placing the wafer in the third cleaning tank, the fourth cleaning tank and the fifth cleaning tank in sequence for cleaning.
[0025] Another aspect of the present invention provides a method for manufacturing a semiconductor device, comprising:
[0026] A wafer is provided, the wafer comprising: a silicon substrate and a sacrificial oxide layer covering a surface of the silicon substrate;
[0027] Cleaning the etched wafer using the aforementioned cleaning method for improving the oxide back-sticking defect on the silicon surface;
[0028] A gate oxide layer is grown on the cleaned wafer surface.
[0029] Compared with the prior art, the beneficial effects of the technical solution of the present invention include at least:
[0030] The invention provides a cleaning method for improving oxide back-adhesion defects on the silicon surface. Different from the prior art which completely removes the sacrificial oxide layer on the substrate surface by one cleaning, the invention adopts a first cleaning and a second cleaning two-step removal method: firstly, a first HF solution is used to remove at least half of the thickness of the sacrificial oxide layer, and the remaining sacrificial oxide layer is reserved to cover the surface of the silicon substrate to avoid exposing the silicon substrate and preventing the oxide dissolved in the first HF solution after cleaning from back-adhering to the silicon substrate surface to form surface defects; then, a second HF solution is used to remove the remaining sacrificial oxide layer, and the oxide content in the second HF solution is significantly reduced, so that the risk of oxide back-adhering to the exposed silicon substrate surface during the second cleaning is greatly reduced, and the defects caused by oxide back-adhering on the silicon surface in the cleaning process are effectively improved, and the performance and yield of semiconductor devices are improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] Figure 1 A flow chart of a cleaning method for improving oxide sticking defects on the silicon surface provided by one embodiment of the present invention.
[0032] Figure 2 AC is a schematic diagram of a wafer cross section during a cleaning process according to an embodiment of the present invention.
[0033] Figure 3 A flow chart of a method for manufacturing a semiconductor device provided by an embodiment of the present invention.
[0034] Figure 4 It is a comparison diagram of surface defects of wafers cleaned by Example 1 of the present invention and the comparative example.
[0035] Figure ID:
[0036] Silicon substrate 1, sacrificial oxide layer 2. DETAILED DESCRIPTION
[0037] The technical solution of the present invention will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0038] It should be noted that all directional indications in the embodiments of the present invention (such as up, down, left, right, front, back, etc.) are only used to explain the relative position relationship, movement status, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.
[0039] Terminology
[0040] In the present invention, "oxides in the cleaning solution" refer to: sacrificial oxide layers and other oxidized pollutants dissolved into the cleaning solution after the wafer surface is cleaned with the cleaning solution (such as the first HF solution).
[0041] As described in the background technology, currently, one or more cleaning solutions such as SPM solution, HF solution, SC1 solution, and SC2 solution are usually used to clean wafers. However, after actual application, it is found that the surface cleanliness of the wafers after cleaning by the existing cleaning methods is not good, and there are still serious defects. The inventors of this application have conducted a lot of research and experimental analysis on this, and finally found that the reasons for the poor cleaning effect of the existing cleaning process include at least the following points:
[0042] (1) When removing the sacrificial oxide layer on the surface of the wafer, the prior art will choose to completely remove the sacrificial oxide layer in the cleaning solution at one time or as completely as possible, exposing the surface of the wafer substrate. As a result, the oxide washed from the wafer surface into the cleaning solution is easily adhered to the substrate surface after the wafer leaves the cleaning solution, forming oxide defects.
[0043] More importantly, the present application discovered that when a silicon substrate has STI (Shallow Trench Isolation), compared to an STI (with filler) surface, since silicon has higher chemical affinity, surface energy, and more surface dangling bonds, the silicon surface is more likely to adsorb oxides in the residual liquid, forming aggregated oxide defects on the silicon surface.
[0044] (2) Conventionally, several wafers are placed face to face in a cleaning tank in a batch cleaning machine for cleaning, and the cleaning liquid flows into the cleaning tank from the bottom until it overflows from the top. However, the present application found that the content of oxides in the cleaning liquid at the overflow position (i.e., oxides washed from the wafer surface into the cleaning liquid) is relatively high, resulting in the wafer facing the liquid flow being more likely to re-adhere oxides near the overflow position, resulting in oxide defects.
[0045] In summary, the present application has found that the wafers cleaned by the existing cleaning method have serious oxide back-sticking defects. To solve this problem, the present application attempts to improve the wafer cleaning method, and finally provides a cleaning method for improving the oxide back-sticking defect on the silicon surface, so as to minimize the generation of wafer surface defects and improve the electrical stability, wafer consistency and yield of the wafer.
[0046] like Figure 1 to Figure 2 As shown, an embodiment of the present invention provides a cleaning method for improving oxide back-adhesion defects on the silicon surface, comprising:
[0047] Step S101 , providing a wafer and placing it in a cleaning tank, wherein the wafer comprises: a silicon substrate 1 and a sacrificial oxide layer 2 covering a surface of the silicon substrate 1 .
[0048] The wafer provided in this step is a wafer before the gate oxide layer is formed. In some embodiments, the structure of the wafer is as shown in FIG. Figure 2 As shown in A, the wafer includes: a silicon substrate 1 and a sacrificial oxide layer 2 covering the surface of the silicon substrate 1; in some other embodiments, the wafer includes: a silicon substrate 1 and a sacrificial oxide layer 2, at least one shallow trench isolation, i.e., STI, is formed in the silicon substrate 1, and the STI is filled with oxide and other materials, and the sacrificial oxide layer 2 is formed to cover the surface of the entire silicon substrate 1 including the STI.
[0049] In some embodiments, the sacrificial oxide layer 2 has a thickness of 6 nm-10 nm, and the sacrificial oxide layer 2 is made of silicon dioxide.
[0050] The silicon substrate 1, the sacrificial oxide layer 2, and the shallow trench isolation can all be prepared by methods known in the art, which will not be elaborated here.
[0051] Step S102 , using the SPM solution and the first HF solution in sequence to perform a first cleaning on the wafer to remove a portion of the sacrificial oxide layer 2 .
[0052] In this step, the surface of the wafer is first cleaned with an SPM solution to remove metal and organic matter on the surface of the wafer. Otherwise, the organic matter on the surface of the wafer will cause the surface to be hydrophobic, affecting the cleaning effect of the subsequent cleaning solution.
[0053] In some embodiments, the SPM solution is a mixed solution of sulfuric acid and hydrogen peroxide, the volume ratio of sulfuric acid to hydrogen peroxide is 1:3-8, and the cleaning temperature is 100°C-150°C.
[0054] Next, the wafer is first cleaned using a first HF solution to remove a portion of the thickness of the sacrificial oxide layer 2 on the wafer surface. In some embodiments, the volume ratio of the hydrofluoric acid original solution to water in the first HF solution is 1:(50-200), and the concentration of the hydrofluoric acid original solution is 40w / w%-50w / w%.
[0055] Note, contrast Figure 2 As can be seen from the AB diagram, in this step, only a partial thickness of the sacrificial oxide layer 2 is required to be removed, rather than completely or as completely as possible removing the sacrificial oxide layer 2, the purpose of which is to retain the remaining thickness of the sacrificial oxide layer 2 to cover the surface of the silicon substrate 1, avoid exposing the silicon substrate 1, and prevent the oxide dissolved in the first HF solution after cleaning from sticking back to the surface of the silicon substrate 1 to form surface defects.
[0056] Step S103 , using a second HF solution, an SC1 solution, and an SC2 solution in sequence to perform a second cleaning on the first cleaned wafer to remove the remaining sacrificial oxide layer 2 on the surface of the wafer.
[0057] like Figure 2 As shown in Figure C, in this step, the second HF solution is first used to clean the wafer after the first cleaning treatment to remove the remaining sacrificial oxide layer 2 on the surface of the wafer and improve the surface cleanliness of the wafer. In some embodiments, in the second HF solution, the volume ratio of the hydrofluoric acid original solution and water is 1: (50-200), and the concentration of the hydrofluoric acid original solution is 40w / w%-50w / w%. It can be understood that since a portion of the thickness of the sacrificial oxide layer 2 has been removed during the first cleaning, the content of oxides in the cleaning solution when the entire sacrificial oxide layer 2 is removed by one cleaning in the prior art is compared. The content of oxides washed into the second HF solution during the second cleaning of the present invention is significantly reduced, thereby reducing the risk of surface defects formed by oxides sticking back to the surface of the silicon substrate 1 exposed during the second cleaning.
[0058] Therefore, more critically, in some embodiments, the thickness of the sacrificial oxide layer 2 removed by the first cleaning of the present invention accounts for at least half of the total thickness, and the remaining small portion of the thickness of the sacrificial oxide layer 2 is left for the second cleaning step. As an example, the partial thickness is 50%-90% of the total thickness of the sacrificial oxide layer. It can be understood that since the exposure of the surface of the silicon substrate 1 is avoided during the first cleaning, the greater the thickness of the sacrificial oxide layer 2 removed by the first cleaning, the lower the thickness of the sacrificial oxide layer 2 required to be removed by the subsequent second cleaning without forming oxide back-adhesion defects, and the lower the oxide content in the second HF solution, then the risk of the exposed silicon substrate 1 surface during the second cleaning forming surface defects by back-adhesion oxide will also be lower.
[0059] Furthermore, in some embodiments, the concentration of the first HF solution is greater than that of the second HF solution, so as to ensure the cleaning effect while taking into account the cleaning efficiency, cost and safety. Specifically, a first HF solution with a higher concentration is used to quickly remove most of the thickness (50%-90% of the total thickness) of the sacrificial oxide layer 2 to improve the cleaning efficiency; and then a second HF solution with a lower concentration is used to gently remove the remaining small thickness of the sacrificial oxide layer 2 to reduce possible damage to the surface of the silicon substrate 1. As an example, the ratio of the hydrofluoric acid original solution to water in the first HF solution is 1:100, the cleaning temperature is 20℃-25℃, and the cleaning time is 3min-4min; the ratio of the hydrofluoric acid original solution to water in the second HF solution is 1:200, the cleaning temperature is 20℃-25℃, and the cleaning time is 1min-2min.
[0060] Next, the wafer is cleaned with SC1 solution to remove particles, metal ions and organic matter on the surface of the wafer. The SC1 solution is an alkaline solution containing ammonia water, hydrogen peroxide and deionized water. In some embodiments, the volume ratio of ammonia water, hydrogen peroxide and deionized water in the SC1 solution is 1:2:50, and the cleaning temperature is 65°C-85°C.
[0061] Next, the wafer is cleaned with SC2 solution to further remove the remaining metal ions and ensure the cleanliness of the wafer surface. The SC2 solution is an acidic solution, comprising hydrochloric acid, hydrogen peroxide and deionized water. In some embodiments, the volume ratio of hydrochloric acid, hydrogen peroxide and deionized water in the SC2 solution is 1:1:50, and the cleaning temperature is 65°C-85°C.
[0062] In some embodiments, before using any one of the SPM solution, the first HF solution, the second HF solution, the SC1 solution and the SC2 solution for cleaning, the wafer is rinsed with deionized water to remove the residual cleaning solution on the surface of the wafer, so as to facilitate the subsequent cleaning steps and avoid introducing new contaminants in the subsequent cleaning steps.
[0063] In some embodiments of the present invention, the cleaning tank used is a cleaning tank in a single wafer cleaning machine. The single wafer cleaning machine processes each wafer individually. Although it can reduce the risk of cross contamination and easily control the cleaning quality, it has low cleaning efficiency and high time cost.
[0064] In order to improve the cleaning efficiency, in other embodiments, the cleaning tank is a cleaning tank in a batch cleaning machine, and the batch cleaning machine can simultaneously place several wafers into the cleaning tank for batch processing. The prior art usually places at least 50 wafers face to face into the cleaning tank in the batch cleaning machine for cleaning. However, the present application finds that processing too many wafers at one time will not only lead to too high oxide content in the cleaning liquid, but also increase the risk of oxides sticking back to the surface of the silicon substrate 1, especially near the surface of the liquid overflow outlet. At the same time, the distance between two adjacent wafers in the cleaning tank is too close (less than 1 cm), and they are placed face to face, which increases the risk of oxides cleaned from one wafer surface sticking back to its own surface or the surface of the wafer facing the surface.
[0065] To solve the above technical problems, the present application has experimentally verified that when the spacing between adjacent wafers in the cleaning tank is greater than 2 cm, it can effectively prevent oxides from sticking back to the wafer surface; however, the spacing should not be too large, which will not only make it difficult to better reduce the oxide sticking rate, but will also lead to a decrease in wafer cleaning efficiency. Optionally, the spacing between adjacent wafers is 2 cm-10 cm.
[0066] In some embodiments, the number of the cleaning tank is one, and the SPM solution, the first HF solution, the second HF solution, the SC1 solution and the SC2 solution flow into the tank in sequence according to the cleaning requirements and sequence, and are discharged after use. Although this can save equipment costs, using the same tank from beginning to end for a multi-step cleaning process will result in a loss in cleaning effect and process flexibility; therefore, in other embodiments, the number of the cleaning tanks is multiple. As an example, the number of the cleaning tanks is 5, the first cleaning tank carries the SPM solution, the second cleaning tank carries the first HF solution, and the first cleaning of the wafer includes: placing the wafer in the first cleaning tank and the second cleaning tank in sequence for cleaning, the third cleaning tank carries the second HF solution, the fourth cleaning tank carries the SC1 solution, and the fifth cleaning tank carries the SC2 solution, and the second cleaning of the wafer includes: placing the wafer in the third cleaning tank, the fourth cleaning tank and the fifth cleaning tank in sequence for cleaning.
[0067] like Figure 3 As shown, an embodiment of the present invention provides a method for manufacturing a semiconductor device, comprising:
[0068] Step S201 , providing a wafer, wherein the wafer comprises: a silicon substrate and a sacrificial oxide layer covering a surface of the silicon substrate.
[0069] Step S202 , cleaning the etched wafer using the cleaning method for improving the silicon surface oxide sticking defect described above in the present invention.
[0070] Step S203, growing a gate oxide layer on the cleaned wafer surface.
[0071] Example 1
[0072] This embodiment provides a cleaning method for improving oxide back-sticking defects on the silicon surface, comprising:
[0073] (1) Prepare SPM solution, first HF solution, second HF solution, SC1 solution and SC2 solution for later use.
[0074] SPM solution composition: the volume ratio of sulfuric acid to hydrogen peroxide is 1:5;
[0075] The first HF solution component: the ratio of hydrofluoric acid original solution (concentration of 40w / w%-50w / w%) and water is 1:100;
[0076] The second HF solution composition: the ratio of hydrofluoric acid original solution (concentration of 40w / w%-50w / w%) and water is 1:200;
[0077] SC1 solution composition: ammonia water, hydrogen peroxide and deionized water in a volume ratio of 1:2:50;
[0078] SC2 solution components: the volume ratio of hydrochloric acid, hydrogen peroxide and deionized water is 1:1:50.
[0079] (2) A wafer is provided and placed in a first cleaning tank. The wafer includes a silicon substrate 1 and a sacrificial oxide layer 2 covering the surface of the silicon substrate 1. The wafer is rinsed with an SPM solution at a cleaning temperature of 100° C.-150° C. for a cleaning time of 1 min-4 min.
[0080] (3) After rinsing the wafer with deionized water, place the wafer in a second cleaning tank and rinse the wafer with the first HF solution at a cleaning temperature of 20° C.-25° C. for 3 min.-4 min. to remove a portion of the sacrificial oxide layer.
[0081] (4) After rinsing the wafer with deionized water, place the wafer in a third cleaning tank and rinse the wafer with a second HF solution at a cleaning temperature of 20° C.-25° C. for 1 min.-2 min. to remove the remaining sacrificial oxide layer.
[0082] (5) After rinsing the wafer with deionized water, place the wafer in the fourth cleaning tank and rinse the wafer with the SC1 solution at a cleaning temperature of 65° C.-85° C. for a cleaning time of 0.5 min-2 min.
[0083] (6) After rinsing the wafer with deionized water, place the wafer in the fifth cleaning tank and rinse the wafer with the SC2 solution at a cleaning temperature of 65°C-85°C and a cleaning time of 0.5min-2min.
[0084] Comparative Example
[0085] Compared with Example 1, the comparative example adopts the existing cleaning process, deletes step (4), removes the entire thickness of the sacrificial oxide layer at one time in step (3), and the cleaning time of step (3) is 4 minutes to 5 minutes.
[0086] The cleaned wafers in Example 1 and the comparative example were rinsed with deionized water, and after drying, the defects on the wafer surface were statistically analyzed by electrical testing and other means to generate a Defect MAP. Figure 4 As shown, compared with the comparative cleaning method, the number of surface defects of the wafers cleaned by the cleaning method of the present application is significantly reduced.
[0087] In summary, the present invention first removes a portion of the sacrificial oxide layer by the first cleaning to avoid exposure of the silicon substrate and the generation of oxide back-adhesion defects; then removes the remaining sacrificial oxide layer by the second cleaning, and the oxide content in the second HF solution is significantly reduced during the second cleaning, and the risk of oxide back-adhesion on the exposed silicon substrate surface is also reduced. The cleaning method of the present invention can effectively improve the generation of oxide back-adhesion defects on the silicon surface and improve the performance and yield of semiconductor devices.
[0088] Although the content of the present invention has been described in detail through the above preferred embodiments, it should be appreciated that the above description should not be considered as a limitation of the present invention. After reading the above content, it will be apparent to those skilled in the art that various modifications and substitutions of the present invention will occur. Therefore, the protection scope of the present invention should be limited by the appended claims.
Claims
1. A cleaning method for improving oxide back-adhesion defects on silicon surface, characterized in that: The following steps are involved: Step S1, providing a wafer and placing it in a cleaning tank, wherein the wafer comprises: a silicon substrate and a sacrificial oxide layer covering a surface of the silicon substrate; Step S2, using the SPM solution and the first HF solution in sequence to perform a first cleaning on the wafer to remove a portion of the sacrificial oxide layer; Step S3, using a second HF solution, an SC1 solution, and an SC2 solution in sequence to perform a second cleaning on the first cleaned wafer to remove the remaining sacrificial oxide layer on the surface of the wafer.
2. The cleaning method for improving the oxide back-adhesion defect on the silicon surface according to claim 1, characterized in that: The concentration of the first HF solution is greater than the concentration of the second HF solution.
3. The cleaning method for improving the oxide back-adhesion defect on the silicon surface according to claim 2, characterized in that: In the first HF solution and the second HF solution, the volume ratio of the hydrofluoric acid original solution to water is 1:50-200, and the concentration of the hydrofluoric acid original solution is 40w / w%-50w / w%.
4. The cleaning method for improving the oxide back-adhesion defect on the silicon surface according to claim 3, characterized in that: The ratio of the hydrofluoric acid original solution to water in the first HF solution is 1:100, the cleaning temperature is 20°C-25°C, and the cleaning time is 3min-4min.
5. The cleaning method for improving the oxide back-adhesion defect on the silicon surface according to claim 3, characterized in that: The ratio of the hydrofluoric acid original solution to water in the second HF solution is 1:200, the cleaning temperature is 20°C-25°C, and the cleaning time is 1min-2min.
6. The cleaning method for improving the oxide back-adhesion defect on the silicon surface according to claim 1, characterized in that: In the SPM solution, the volume ratio of sulfuric acid to hydrogen peroxide is 1:3-8, and the cleaning temperature is 100°C-150°C; In the SC1 solution, the volume ratio of ammonia water, hydrogen peroxide and deionized water is 1:2:50, and the cleaning temperature is 65°C-85°C; In the SC2 solution, the volume ratio of hydrochloric acid, hydrogen peroxide and deionized water is 1:1:50, and the cleaning temperature is 65°C-85°C.
7. The cleaning method for improving the oxide back-adhesion defect on the silicon surface according to claim 1, characterized in that: The thickness of the portion is 50%-90% of the total thickness of the sacrificial oxide layer.
8. The cleaning method for improving the oxide back-adhesion defect on the silicon surface according to claim 7, characterized in that: The total thickness of the sacrificial oxide layer is 6nm-10nm.
9. The cleaning method for improving the oxide back-adhesion defect on the silicon surface according to claim 1, characterized in that: The sacrificial oxide layer includes a silicon dioxide layer.
10. The cleaning method for improving the oxide back-adhesion defect on the silicon surface according to claim 1, characterized in that: The number of wafers in the cleaning tank is at least two, and the distance between adjacent wafers is greater than 2 cm.
11. The cleaning method for improving the oxide back-adhesion defect on the silicon surface according to claim 1, characterized in that: Also includes: In steps S2 and S3, the wafer is rinsed with deionized water before being cleaned with any one of the SPM solution, the first HF solution, the second HF solution, the SC1 solution and the SC2 solution; as well as, Step S4, rinsing the wafer with deionized water and completing drying.
12. The cleaning method for improving the oxide back-adhesion defect on the silicon surface according to claim 1, characterized in that: The first cleaning tank carries the SPM solution, the second cleaning tank carries the first HF solution, and the first cleaning of the wafer includes: placing the wafer in the first cleaning tank and the second cleaning tank in sequence for cleaning.
13. The cleaning method for improving the oxide back-adhesion defect on the silicon surface according to claim 1, characterized in that: The third cleaning tank carries the second HF solution, the fourth cleaning tank carries the SC1 solution, and the fifth cleaning tank carries the SC2 solution. The second cleaning of the wafer includes: placing the wafer in the third cleaning tank, the fourth cleaning tank and the fifth cleaning tank in sequence for cleaning.
14. A method for manufacturing a semiconductor device, characterized in that: include: A wafer is provided, the wafer comprising: a silicon substrate and a sacrificial oxide layer covering a surface of the silicon substrate; Cleaning the etched wafer using the cleaning method for improving silicon surface oxide back-sticking defects according to any one of claims 1 to 13; A gate oxide layer is grown on the cleaned wafer surface.