Conductivity testing structure for buffer layer in semiconductor wafer and preparation method of conductivity testing structure

By setting up partitions in semiconductor wafers to remove two-dimensional electronic gas and conduct conductivity testing, the problem of the inability to accurately monitor the conductivity of the buffer layer in the prior art is solved, the accuracy and efficiency of detection are improved, and the quality of the device is improved and yield.

CN119050099APending Publication Date: 2024-11-29RUISI MICROSYSTEMS (YANTAI) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411237026.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

The prior art cannot promptly and accurately monitor the conductivity of the III-V nitride semiconductor wafer buffer layer during the process, affecting the trap effect and radio frequency loss of the device.

Method used

A conductivity test structure for buffer layer in semiconductor wafers was designed. By setting a partition area in the test area, two-dimensional electronic gas is removed to avoid interference with conductivity testing. The two-dimensional electronic gas is removed by etching and ion implantation processes, and the During the preparation process, a test electrode is set up for detection.

Benefits of technology

It improves the accuracy and detection efficiency of buffer layer conductivity testing, ensuring the product quality and yield of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119050099A_ABST
    Figure CN119050099A_ABST
Patent Text Reader

Abstract

The invention discloses a conductivity test structure of a buffer layer in a semiconductor wafer and a preparation method thereof, which are applied to the field of semiconductors, and the conductivity test structure of the buffer layer in the semiconductor wafer comprises a substrate, and a buffer layer, a channel layer and a barrier layer which are sequentially grown along a direction far away from the substrate, two-dimensional electron gas separated by a partition region is formed at a heterojunction interface formed by the channel layer and the barrier layer; the partition area is arranged corresponding to a test area of the buffer layer conductivity test structure; and test electrodes are respectively arranged on one side, back to the substrate, of the buffer layer conductivity test structure and on the table surfaces on the two sides of the test area. According to the method, the two-dimensional electron gas corresponding to the test area in the semiconductor prefabricated member is removed, so that the two-dimensional electron gas corresponding to the test area is prevented from interfering with the conductivity test of the buffer layer when the conductivity of the buffer layer is tested, the accuracy of testing the conductivity of the buffer layer is improved, and the detection efficiency is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductors, and in particular to a buffer layer conductivity test structure in a semiconductor wafer and a preparation method thereof. Background Art

[0002] Devices based on III-V nitride semiconductors have the advantages of high frequency, high power, and low noise, and are widely used in base stations, radars, satellite communications and other fields. III-V semiconductor wafers are usually processed and prepared by epitaxially growing multiple semiconductor layers on a substrate. The multiple semiconductor layers generally include a nucleation layer, a buffer layer, a channel layer, a barrier layer, and a top cap protection layer. The channel layer and the barrier layer form a heterojunction and generate a layer of two-dimensional electron gas (2DEG) with good conductivity at the heterojunction interface to provide the required current for the prepared device. In order to increase the mobility of 2DEG and reduce the trap effect, a thicker buffer layer needs to be grown to improve product quality. The conductivity of the buffer layer has a great influence on the trap effect and RF loss of the device, but it is currently impossible to accurately monitor the conductivity of the buffer layer in a timely manner during the process.

[0003] Therefore, how to provide a test structure for accurately and efficiently testing the conductivity of the buffer layer is a technical problem that those skilled in the art need to solve urgently. Summary of the invention

[0004] In view of this, the purpose of the present invention is to provide a conductivity test structure of the buffer layer in a semiconductor wafer and a preparation method thereof, which solves the problem that the conductivity of the buffer layer in the prior art has a great influence on the trap effect and radio frequency loss of the device, but the conductivity of the buffer layer cannot be accurately monitored in time during the process.

[0005] In order to solve the above technical problems, the present invention provides a buffer layer conductivity test structure in a semiconductor wafer, comprising:

[0006] A substrate, and a buffer layer, a channel layer, and a barrier layer sequentially grown in a direction away from the substrate;

[0007] A two-dimensional electron gas separated by a partition region is formed at the heterojunction interface formed by the channel layer and the barrier layer; the partition region is arranged corresponding to the test region of the buffer layer conductivity test structure;

[0008] The side of the buffer layer conductivity test structure facing away from the substrate and the mesas located on both sides of the test area are respectively provided with test electrodes.

[0009] Optionally, the isolation area is a surface area of ​​the buffer layer conductivity test structure away from the substrate, corresponding to the test area, and has a recessed structure formed inwardly where the barrier layer and a portion of the channel layer are removed by an etching process to remove the two-dimensional electron gas corresponding to the test area.

[0010] Optionally, the isolation area is a surface area of ​​the buffer layer conductivity test structure away from the substrate, corresponding to the test area, and is formed inwardly by injecting ions into the barrier layer and a partial thickness of the channel layer through a doping process to remove a high-resistance area of ​​the two-dimensional electron gas corresponding to the test area.

[0011] Optionally, a test area is provided at the edge of the semiconductor wafer, and the buffer layer conductivity test structure is provided in the test area.

[0012] The present invention also provides a method for preparing a buffer layer conductivity test structure in a semiconductor wafer, comprising:

[0013] Providing a semiconductor preform; the semiconductor preform at least comprises a substrate, and a buffer layer, a channel layer and a barrier layer sequentially grown in a direction away from the substrate, wherein a two-dimensional electron gas is formed at a heterojunction interface formed by the channel layer and the barrier layer;

[0014] Removing the two-dimensional electron gas corresponding to the test area in the semiconductor preform to obtain a preprocessed semiconductor wafer;

[0015] In the surface of the pre-processed semiconductor wafer away from the substrate, test electrodes are respectively prepared on the mesas located on both sides of the test area to obtain a buffer layer conductivity test structure.

[0016] Optionally, removing the two-dimensional electron gas corresponding to the test area in the semiconductor preform to obtain a preprocessed semiconductor wafer includes:

[0017] A surface area of ​​the semiconductor preform away from the substrate corresponding to the test area is etched using a dry etching process until the barrier layer corresponding to the test area is etched away, and a partial thickness of the channel layer corresponding to the test area is etched away, so as to remove the two-dimensional electron gas in the semiconductor preform corresponding to the test area, thereby obtaining the preprocessed semiconductor wafer.

[0018] Optionally, after the surface area of ​​the semiconductor preform away from the substrate corresponding to the test area is etched by a dry etching process until the barrier layer corresponding to the test area is etched away, and a portion of the channel layer corresponding to the test area is etched away to remove the two-dimensional electron gas in the semiconductor preform corresponding to the test area to obtain the preprocessed semiconductor wafer, the method further includes:

[0019] The etching damage in the pre-treated semiconductor wafer is repaired by a high temperature thermal annealing treatment or an alkaline solution cleaning treatment.

[0020] Optionally, removing the two-dimensional electron gas corresponding to the test area in the semiconductor preform to obtain a preprocessed semiconductor wafer includes:

[0021] An ion implantation process is used to implant ions into a surface area of ​​the semiconductor preform away from the substrate, corresponding to the test area, until the channel layer having a partial thickness corresponding to the test area is doped, so as to remove the two-dimensional electron gas corresponding to the test area in the semiconductor preform, and obtain the preprocessed semiconductor wafer; the implanted ions are ions that can form high-resistance areas in the doped areas of the channel layer and the barrier layer.

[0022] Optionally, when ions are implanted into a surface area of ​​the semiconductor preform away from the substrate corresponding to the test area by an ion implantation process, the method further includes:

[0023] An ion implantation process is used to implant ions into a surface area of ​​the semiconductor preform that is away from the substrate and corresponds to the isolation region until the channel layer having a partial thickness corresponding to the isolation region is doped, so as to remove the two-dimensional electron gas in the semiconductor preform that corresponds to the isolation region.

[0024] Optionally, when test electrodes are prepared respectively on the mesas located on both sides of the test area in the surface of the pre-processed semiconductor wafer away from the substrate, the method further includes:

[0025] In the surface of the pre-processed semiconductor wafer away from the substrate, a mesa outside the test area and between two adjacent isolation areas is deposited to prepare source metal and drain metal.

[0026] Optionally, removing the two-dimensional electron gas corresponding to the test area in the semiconductor preform to obtain a preprocessed semiconductor wafer includes:

[0027] preparing a photoresist on a surface of the semiconductor preform away from the substrate;

[0028] Performing patterning on the photoresist to expose a surface area of ​​the semiconductor preform away from the substrate corresponding to the test area, thereby obtaining a patterned photoresist;

[0029] An etching process or a doping process is performed on the surface area exposed by the patterned photoresist to remove the two-dimensional electron gas corresponding to the test area in the semiconductor preform to obtain the preprocessed semiconductor wafer.

[0030] It can be seen that the buffer layer conductivity test structure in the semiconductor wafer provided by the present invention includes a substrate, and a buffer layer, a channel layer and a barrier layer sequentially grown in a direction away from the substrate, a two-dimensional electron gas separated by a partition area is formed at the heterojunction interface formed by the channel layer and the barrier layer, the partition area is arranged corresponding to the test area of ​​the buffer layer conductivity test structure, and the table surfaces on both sides of the test area of ​​the buffer layer conductivity test structure facing away from the substrate are respectively provided with test electrodes. The present invention sets a partition area for separating the two-dimensional electron gas in the test area corresponding to the buffer layer conductivity test structure, removes the two-dimensional electron gas at the partition area, so as to avoid the two-dimensional electron gas corresponding to the test area from interfering with the conductivity test of the buffer layer when the conductivity of the buffer layer is tested, thereby improving the accuracy of testing the conductivity of the buffer layer and improving the detection efficiency.

[0031] In addition, the present invention also provides a method for preparing a buffer layer conductivity test structure in a semiconductor wafer, which also has the above-mentioned beneficial effects. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the provided drawings without paying creative work.

[0033] Figure 1 A schematic structural diagram of a conductivity testing structure of a buffer layer in a semiconductor wafer provided by an embodiment of the present invention;

[0034] Figure 2 A schematic structural diagram of another semiconductor wafer buffer layer conductivity test structure provided by an embodiment of the present invention;

[0035] Figure 3 A flow chart of a method for preparing a buffer layer conductivity test structure in a semiconductor wafer provided by an embodiment of the present invention;

[0036] Figures 4 to 9 A schematic flow chart of a method for preparing a conductivity test structure of a buffer layer in a semiconductor wafer provided by an embodiment of the present invention;

[0037] Figures 10 to 12 A schematic flow chart of another method for preparing a conductivity test structure of a buffer layer in a semiconductor wafer provided by an embodiment of the present invention;

[0038] 10-substrate, 11-buffer layer and channel layer, 12-barrier layer, 13-patterned photoresist, 14-test electrode, 15-source metal, 16-drain metal, 17-high resistance region, 18-isolation region, 20-two-dimensional electron gas, 30-isolation region. DETAILED DESCRIPTION

[0039] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0040] Transistors based on III-V nitride semiconductors have the advantages of high frequency, high power, and low noise, and are widely used in base stations, radars, satellite communications and other fields. III-V semiconductor wafers are usually prepared by processing multiple semiconductor layers epitaxially grown on substrate materials. Usually, the multiple semiconductor layers include a nucleation layer, a buffer layer, a channel layer, a barrier layer, and a top cap protection layer. The channel layer and the barrier layer can form a heterojunction, and a layer of two-dimensional electron gas with good conductivity can be generated at the heterojunction interface to provide the required current for the transistor. However, in order to improve the mobility of the two-dimensional electron gas and reduce the trap effect, a thicker buffer layer needs to be grown to improve the material quality. However, the conductivity of the buffer layer has a great influence on the trap effect and RF loss of the transistor, and it is difficult to monitor in time during the process preparation. Therefore, accurate and efficient testing of the conductivity of the buffer layer is of great value to the preparation of III-V nitride semiconductor transistors. However, the conventional buffer layer conductivity test structure has a relatively large buffer layer conductivity due to the influence of the two-dimensional electron gas. Therefore, how to provide a test structure for accurately and efficiently testing the buffer layer conductivity is a technical problem that needs to be solved urgently by those skilled in the art.

[0041] The present invention sets a partition area for separating two-dimensional electron gas in a test area corresponding to a test structure of a buffer layer conductivity, and removes the two-dimensional electron gas in the partition area, so as to avoid interference of the two-dimensional electron gas corresponding to the test area with the conductivity test of the buffer layer when the conductivity of the buffer layer is tested, thereby improving the accuracy of testing the conductivity of the buffer layer and improving the detection efficiency.

[0042] Please refer to Figure 1 , Figure 1 A schematic diagram of a structure for testing conductivity of a buffer layer in a semiconductor wafer provided by an embodiment of the present invention. The testing structure may include:

[0043] A substrate 10, and a buffer layer, a channel layer and a barrier layer 12 sequentially grown in a direction away from the substrate 10;

[0044] A two-dimensional electron gas 20 separated by a partition region 30 is formed at the heterojunction interface formed by the channel layer and the barrier layer 12; the partition region 30 is arranged corresponding to the test region of the buffer layer conductivity test structure;

[0045] On one side of the buffer layer conductivity test structure facing away from the substrate 10 , test electrodes 14 are respectively disposed on the mesas located on both sides of the test area.

[0046] It should be noted that, in this embodiment, the substrate 10 may be a gallium nitride substrate, an aluminum gallium nitride substrate, an aluminum indium gallium nitride substrate, a silicon substrate, an aluminum oxide substrate, a gallium arsenide substrate, a silicon carbide substrate, a diamond substrate, a germanium substrate, or any other substrate 10 capable of growing III-V semiconductor materials. In this embodiment, when preparing the semiconductor wafer, the above-mentioned buffer layer, channel layer and barrier layer 12 may be prepared in sequence on the upper surface of the substrate 10, and may also include a nucleation layer located between the substrate 10 and the buffer layer, and a top cap protection layer located on the side of the barrier layer 12 facing away from the substrate 10. The nucleation layer plays a role in assisting the growth of the upper semiconductor material on the substrate 10, which affects the defect density, surface morphology and electrical properties of 2DEG of the upper material. The buffer layer can regulate crystal stress, reduce defect density, and improve the material quality of the channel layer. The channel layer and the barrier layer 12 form a heterojunction, and a layer of two-dimensional electron gas 20 (2DEG) with good conductivity can be generated at the heterojunction interface. The top cap protection layer can reduce the oxidation and surface state density of the barrier layer 12, and reduce the impact of the process on the 2DEG. Figure 1 As shown, the channel layer is located on the side facing away from the substrate 10 , and the buffer layer is located on the side facing the substrate 10 .

[0047] In this embodiment, in the test area corresponding to the buffer layer conductivity test structure, a partition area 30 is set to separate the two-dimensional electron gas 20 existing at the heterojunction interface between the channel layer and the barrier layer 12, and the two-dimensional electron gas 20 located in the partition area 30 is removed. Therefore, when the conductivity of the buffer layer is tested, since there is no two-dimensional electron gas 20 gathering in the test area, the accuracy of the test of the conductivity of the buffer layer can be improved. Further, in this embodiment, the partition area 30 can be consistent with the test area, that is, the partition area 30 with the electron gas removed is the test area of ​​the above-mentioned buffer layer conductivity test structure.

[0048] In addition, on the side of the buffer layer conductivity test structure facing away from the substrate 10 in this embodiment, the mesas on both sides of the test area are respectively provided with test electrodes 14, and the test electrodes 14 are two electrodes for testing the conductivity of the buffer layer. The specific test method can refer to the existing conductivity test method, for example, high and low voltages can be applied to the two test electrodes 14 respectively, and then the current value between the two test electrodes 14 can be read to calculate the conductivity of the buffer layer. The mesas on both sides of the test area in this embodiment are the surfaces of the unprocessed area on both sides of the partition area 30 where the two-dimensional electron gas 20 is removed in the buffer layer conductivity test structure, and the test area and the mesas on both sides of the test area are both located in an active area between two adjacent isolation areas 18, that is, the semiconductor wafer can include multiple independent active processing areas, and the adjacent active processing areas are separated by the isolation area 18. Therefore, the buffer layer conductivity test structure in this embodiment can be prepared together with other functional structures in the semiconductor wafer, that is, the conductivity of the buffer layer can be detected in real time during the preparation process, which improves the flexibility and accuracy of the detection, thereby improving the product yield.

[0049] The present embodiment does not limit the specific structure of the isolation area 30 or the test area, as long as the two-dimensional electron gas 20 corresponding to the isolation area 30 and the test area is removed to avoid the two-dimensional electron gas 20 at the heterojunction interface between the channel layer and the barrier layer 12 affecting the accuracy of the conductivity detection of the buffer layer.

[0050] Furthermore, in order to ensure that the two-dimensional electron gas 20 corresponding to the test area is removed, a partition region 30 is formed at the heterojunction interface between the channel layer and the barrier layer 12 to separate the two-dimensional electron gas 20. The partition region 30 can be set as a surface of the buffer layer conductivity test structure away from the substrate 10, corresponding to the surface area of ​​the test area, and a channel layer with a partial thickness removed by an etching process is formed inwardly to remove a recessed structure of the two-dimensional electron gas 20 corresponding to the test area.

[0051] It should be noted that the recessed structure for removing the two-dimensional electron gas 20 corresponding to the test area formed in the present embodiment is the partition area 30 for separating the two-dimensional electron gas 20 mentioned above. In the present embodiment, the recessed structure is etched as the partition area 30, so that the two-dimensional electron gas 20 can be completely removed from the position corresponding to the test area, thereby ensuring the accuracy of the detection.

[0052] Further, in a feasible embodiment, in order to avoid damaging the semiconductor wafer and ensure the preparation of the partition area 30, reference may be made to Figure 2 , Figure 2A schematic diagram of another structure for testing the conductivity of a buffer layer in a semiconductor wafer provided by an embodiment of the present invention. The above-mentioned isolation region 30 can be set as a surface area of ​​the buffer layer conductivity test structure away from the substrate 10, corresponding to the surface area of ​​the test area, inwardly formed with ions implanted into the barrier layer 12 and a portion of the thickness of the channel layer by a doping process to remove the high resistance region 17 of the two-dimensional electron gas 20 corresponding to the test area.

[0053] It should be noted that the high resistance region 17 in this embodiment, that is, the isolation region 30 corresponding to the test region, is doped by injecting ions into the heterojunction interface between the channel layer and the barrier layer 12 to form a high resistance region at a position corresponding to the test region, thereby eliminating the influence of the two-dimensional electron gas 20 on the conductivity test of the buffer layer, thereby ensuring the accuracy of the conductivity detection of the buffer layer.

[0054] Furthermore, in order to prevent the buffer layer conductivity test structure from affecting the functional area of ​​the semiconductor wafer, a test area may be provided at the edge of the semiconductor wafer, and the buffer layer conductivity test structure is provided in the test area.

[0055] It should be noted that in this embodiment, the test area is set at the edge of the semiconductor wafer so that there is no functional area of ​​the semiconductor wafer outside the set test area, so as to avoid the buffer layer conductivity test structure prepared in the above test area affecting the functionality of the adjacent functional area of ​​the semiconductor wafer. In this embodiment, while ensuring that the other functional areas of the semiconductor wafer are not affected, the complexity of preparation is increased, and the test area can also be set in other areas of the semiconductor wafer. The purpose of preparing the above buffer layer conductivity test structure in this embodiment is to monitor the conductivity of the buffer layer formed in the semiconductor production process. Only a limited number of them (for example, 1 or 2) need to be set on the entire wafer. The subsequent processes (such as deposition of source and drain metal electrodes, etc.) can be carried out after the test is qualified.

[0056] It should be further explained that the above-mentioned buffer layer conductivity test structure is prepared in a process embedded in the normal process of the semiconductor wafer. For example, after the barrier layer is grown, the next step of a normal HEMT (high electron mobility transistor) device is to deposit a protective layer or etch the barrier layer to obtain a gate groove or a source-drain groove for depositing a gate metal. The process of preparing the buffer layer conductivity test structure in the present application can be completed together with the above-mentioned step of depositing a protective layer or etching a barrier layer to obtain a gate groove or a source-drain groove for depositing a gate metal, or can be prepared separately before the above-mentioned step. The buffer layer conductivity test structure in the semiconductor wafer provided by the embodiment of the present invention comprises a substrate 10, and a buffer layer, a channel layer and a barrier layer 12 sequentially grown in a direction away from the substrate 10, a two-dimensional electron gas 20 separated by a partition area 30 is formed at the heterojunction interface formed by the channel layer and the barrier layer 12, the partition area 30 is arranged corresponding to the test area of ​​the buffer layer conductivity test structure, and the table surfaces on both sides of the test area of ​​the buffer layer conductivity test structure facing away from the substrate 10 are respectively provided with test electrodes 14. The present invention sets the partition area 30 for separating the two-dimensional electron gas 20 in the test area corresponding to the buffer layer conductivity test structure, removes the two-dimensional electron gas 20 at the partition area 30, so as to avoid the two-dimensional electron gas 20 corresponding to the test area from interfering with the conductivity test of the buffer layer when the conductivity of the buffer layer is tested, thereby improving the accuracy of testing the conductivity of the buffer layer and improving the detection efficiency.

[0057] In addition, the embodiment of the present invention uses the recessed structure formed to remove the two-dimensional electron gas 20 corresponding to the test area as the partition area 30 for separating the two-dimensional electron gas 20, thereby ensuring that the partition area 30 for separating the two-dimensional electron gas 20 completely removes the two-dimensional electron gas 20, thereby improving the accuracy of the buffer layer conductivity detection; uses the high-resistance area formed at the position corresponding to the test area as the partition area 30, thereby eliminating the influence of the two-dimensional electron gas 20 on the buffer layer conductivity test and ensuring the preparation efficiency of the buffer layer conductivity test structure; and sets the test area at the edge of the semiconductor wafer to avoid the influence of the set buffer layer conductivity test structure on the functional area of ​​the semiconductor wafer, thereby improving the product yield.

[0058] A method for preparing a conductivity test structure of a buffer layer in a semiconductor wafer provided in an embodiment of the present invention is introduced below. The method for preparing the conductivity test structure of a buffer layer in a semiconductor wafer described below and the conductivity test structure of a buffer layer in a semiconductor wafer described above can be referred to each other.

[0059] Please refer to Figure 3 , Figure 3 A flow chart of a method for preparing a conductivity test structure of a buffer layer in a semiconductor wafer provided by an embodiment of the present invention may include:

[0060] S101: providing a semiconductor preform; the semiconductor preform at least comprises a substrate, and a buffer layer, a channel layer and a barrier layer sequentially grown in a direction away from the substrate, and a two-dimensional electron gas is formed at a heterojunction interface formed by the channel layer and the barrier layer.

[0061] It should be noted that the semiconductor preform in this embodiment includes a substrate, and a buffer layer, a channel layer and a barrier layer that are sequentially grown in a direction away from the substrate, which is a partial structure in an existing semiconductor wafer. At this time, the two-dimensional electron gas formed at the heterojunction interface between the channel layer and the barrier layer is in an uninterrupted state. If the conductivity of the buffer layer in the semiconductor preform is tested at this time, the two-dimensional electron gas at the heterojunction interface between the channel layer and the barrier layer will seriously affect the conductivity of the buffer layer, thereby causing a large deviation between the test result and the actual result, affecting the yield of the semiconductor wafer finally prepared.

[0062] S102: removing the two-dimensional electron gas in the semiconductor preform corresponding to the test area to obtain a pre-processed semiconductor wafer.

[0063] In this embodiment, the two-dimensional electron gas corresponding to the test area in the semiconductor preform is removed so that there is no two-dimensional electron gas gathering in the area where the conductivity of the buffer layer is detected, forming a partition area to avoid affecting the detection of the conductivity of the buffer layer. This embodiment does not limit the specific method of removing the two-dimensional electron gas in the semiconductor preform corresponding to the test area, as long as the two-dimensional electron gas in the specified position can be removed. For example, the two-dimensional electron gas corresponding to the test area in the semiconductor preform can be removed by an etching process or a doping process.

[0064] Further, in order to ensure that the two-dimensional electron gas corresponding to the test area in the semiconductor preform is completely removed and to improve the removal efficiency, the above-mentioned removal of the two-dimensional electron gas corresponding to the test area in the semiconductor preform to obtain the pre-processed semiconductor wafer may include:

[0065] A surface area of ​​the semiconductor preform away from the substrate corresponding to the test area is etched using a dry etching process until the barrier layer corresponding to the test area is etched away, and a partial thickness of the channel layer corresponding to the test area is etched away, so as to remove the two-dimensional electron gas corresponding to the test area in the semiconductor preform, thereby obtaining a preprocessed semiconductor wafer.

[0066] It should be noted that in this embodiment, dry etching is used to etch the surface of the semiconductor preform away from the substrate, corresponding to the surface area of ​​the test area, until the barrier layer corresponding to the test area and a portion of the channel layer are etched away. Since only the two-dimensional electron gas in the test area is removed in this embodiment, and the buffer layer is not affected, dry etching should be performed from the side of the structure facing away from the substrate, from the barrier layer to the channel layer, until the two-dimensional electron gas corresponding to the test area is removed.

[0067] Furthermore, in order to avoid causing processing damage in the removal area of ​​the pre-processed semiconductor wafer after removing the two-dimensional electron gas corresponding to the test area, thereby affecting the test accuracy, after the surface of the semiconductor preform away from the substrate is etched by the dry etching process, the surface area corresponding to the test area is etched away until the barrier layer corresponding to the test area is etched away, and the channel layer corresponding to the test area is etched away with a partial thickness to remove the two-dimensional electron gas in the semiconductor preform corresponding to the test area, and after obtaining the pre-processed semiconductor wafer, the method may further include:

[0068] The etching damage in the pre-treated semiconductor wafer is repaired by a high temperature thermal annealing treatment or an alkaline solution cleaning treatment.

[0069] It should be noted that the preparation of the conductivity test structure of the buffer layer by etching process is very easy to introduce etching damage and form donor defects during the preparation process, resulting in surface leakage, which makes the conductivity of the buffer layer too large. Therefore, in order to ensure the accuracy of the conductivity detection of the buffer layer, this embodiment needs to repair the damage after etching, including the use of high-temperature thermal annealing treatment to provide a high-temperature environment, so that the pre-treated semiconductor wafer can rearrange the atoms of the damaged layer under the high-temperature environment, thereby reducing the defect state density. And the use of alkaline solution cleaning treatment, the alkaline solution is used to remove the damaged layer by corrosiveness to the pre-treated semiconductor wafer, thereby reducing the surface state density at the etching position. It should be further explained that in this embodiment, the pre-treated semiconductor wafer can also be placed in a MOCVD (metal organic chemical vapor deposition reactor) chamber for heat treatment, and ammonia is introduced into the MOCVD chamber during the heat treatment. Ammonia is decomposed in a high-temperature environment to release nitrogen atoms, and nitrogen atoms can fill vacancy defects, thereby repairing the etching damage on the semiconductor surface.

[0070] Further, in a feasible embodiment, in order to avoid etching damage in the etching area after removing the two-dimensional electron gas corresponding to the test area by the etching process as described above, so as to improve the preparation efficiency, the above-mentioned removal of the two-dimensional electron gas corresponding to the test area in the semiconductor preform to obtain the pre-processed semiconductor wafer may include:

[0071] An ion implantation process is used to implant ions into a surface area of ​​a semiconductor preform that is away from a substrate and corresponds to a test area, until a channel layer having a partial thickness corresponding to the test area is doped, so as to remove the two-dimensional electron gas corresponding to the test area in the semiconductor preform and obtain a preprocessed semiconductor wafer; the implanted ions are ions that can form high-resistance areas in the doped areas of the channel layer and the barrier layer.

[0072] It should be noted that in this embodiment, ions are implanted into the surface area corresponding to the test area on the side of the semiconductor preform facing away from the substrate through an ion implantation doping process, so that a high resistance area is formed in the partial area corresponding to the test area in the semiconductor preform, with the purpose of removing the two-dimensional electron gas corresponding to the test area in the semiconductor preform. At the same time, this embodiment will not cause damage to the semiconductor preform, can ensure the preparation efficiency, and avoid the problem of low test accuracy. The ions injected in this embodiment can be boron ions or nitrogen ions, or other ions that can transform the above-mentioned semiconductor structure into a high-resistance state structure can be selected, thereby destroying the formation of the two-dimensional electron gas and removing the influence of the two-dimensional electron gas on the conductivity of the buffer layer.

[0073] Furthermore, in order to simplify the preparation steps of the semiconductor wafer and improve the preparation efficiency, when the ion implantation process is used to implant ions into the surface area of ​​the semiconductor preform away from the substrate corresponding to the test area, the following steps may be further included:

[0074] An ion implantation process is used to implant ions into a surface area of ​​the semiconductor preform away from the substrate, corresponding to the isolation region, until a channel layer having a partial thickness corresponding to the isolation region is doped, so as to remove the two-dimensional electron gas in the semiconductor preform corresponding to the isolation region.

[0075] In this embodiment, when ions are implanted into the semiconductor preform corresponding to the test area by an ion implantation process to form a high resistance area, ions can be implanted into the surface area of ​​the semiconductor preform corresponding to the isolation area simultaneously to complete the preparation of a structure in which different active areas are isolated in the semiconductor wafer, and the preparation is completed in one step, thereby improving the preparation efficiency. In addition, it can be seen that the buffer layer conductivity test structure in this embodiment is prepared together with other active device structures of the semiconductor wafer.

[0076] Further, in order to ensure accurate removal of the two-dimensional electron gas corresponding to the test area, the above-mentioned removal of the two-dimensional electron gas corresponding to the test area in the semiconductor preform to obtain the pre-processed semiconductor wafer may include:

[0077] Step S11: preparing photoresist on the surface of the semiconductor preform away from the substrate;

[0078] Step S12: performing patterning on the photoresist to expose a surface area of ​​the semiconductor preform away from the substrate corresponding to the test area, thereby obtaining a patterned photoresist;

[0079] Step S13: performing an etching process or a doping process on the surface area exposed by the patterned photoresist to remove the two-dimensional electron gas in the corresponding test area in the semiconductor preform to obtain a pre-processed semiconductor wafer.

[0080] In this embodiment, a patterned photoresist is prepared to protect the surface of the semiconductor preform facing away from the substrate, which corresponds to the area outside the test area, so as to improve the accuracy of the preparation. It should be further explained that after removing the two-dimensional electron gas corresponding to the test area of ​​the semiconductor preform to obtain a pre-processed semiconductor wafer, the remaining patterned photoresist needs to be removed for subsequent preparation.

[0081] S103: On the surface of the pre-processed semiconductor wafer away from the substrate, test electrodes are respectively prepared on the mesas located on both sides of the test area to obtain a buffer layer conductivity test structure.

[0082] In this embodiment, the method for testing the conductivity of the buffer layer is to set the two metal electrodes to high and low voltages respectively, and then read the current value between the two electrodes to calculate the conductivity of the buffer layer.

[0083] Further, in order to reduce the complexity of semiconductor wafer preparation, in the above-mentioned pre-processing of the surface of the semiconductor wafer away from the substrate, when preparing the test electrodes on the mesas located on both sides of the test area respectively, it can also include:

[0084] In the surface of the pre-processed semiconductor wafer away from the substrate, the mesa outside the test area and located between two adjacent isolation areas is deposited and prepared accordingly for source metal and drain metal.

[0085] It should be noted that, in this embodiment, the source metal and the drain metal are deposited outside the test area and on the table located between two adjacent isolation areas. It can be seen that other active functional areas in this application are prepared simultaneously with the buffer layer conductivity test structure including the test area, and it should be further noted that, in this embodiment, the table on which the source metal and the drain metal are deposited is isolated from the table on which the test electrode is deposited.

[0086] The method for preparing a buffer layer conductivity test structure in a semiconductor wafer provided by an embodiment of the present invention comprises providing a semiconductor preform, the semiconductor preform comprising at least a substrate, and a buffer layer, a channel layer and a barrier layer sequentially grown in a direction away from the substrate, a two-dimensional electron gas is formed at a heterojunction interface formed by the channel layer and the barrier layer, the two-dimensional electron gas in the semiconductor preform corresponding to the test area is removed to obtain a pre-processed semiconductor wafer, and test electrodes are respectively prepared on the mesas located on both sides of the test area in the surface of the pre-processed semiconductor wafer away from the substrate to obtain a buffer layer conductivity test structure. The present invention sets a partition area for separating the two-dimensional electron gas in the test area corresponding to the buffer layer conductivity test structure, removes the two-dimensional electron gas in the partition area, so as to avoid the two-dimensional electron gas corresponding to the test area from interfering with the conductivity test of the buffer layer when the conductivity of the buffer layer is tested, thereby improving the accuracy of testing the conductivity of the buffer layer and improving the detection efficiency.

[0087] In addition, the embodiment of the present invention uses dry etching to etch the surface area of ​​the semiconductor preform away from the substrate, corresponding to the test area, until the barrier layer corresponding to the test area and the channel layer of part of the thickness are etched away, thereby ensuring that the two-dimensional electron gas corresponding to the test area in the semiconductor preform is completely removed, while improving the preparation efficiency; using a high-temperature thermal annealing treatment method or an alkaline solution cleaning treatment method, the defect state density at the surface of the etching area is reduced, and the etching damage in the pre-treated semiconductor wafer is repaired to avoid affecting the test accuracy; through an ion implantation doping process, ions are implanted into the surface area of ​​the semiconductor preform on the side facing away from the substrate, corresponding to the test area, so that the semiconductor A high resistance area is formed in a partial area of ​​the preform corresponding to the test area, which will not cause damage to the semiconductor preform, can ensure the preparation efficiency and avoid the problem of low test accuracy; ions are injected into the semiconductor preform corresponding to the test area by using an ion implantation process for doping, and when the high resistance area is formed, ions are simultaneously injected into the surface area of ​​the semiconductor preform corresponding to the isolation area, thereby simplifying the preparation steps; by preparing a patterned photoresist, the photoresist is used to protect the surface of the semiconductor preform facing away from the substrate, corresponding to the area outside the test area, thereby improving the preparation accuracy; by preparing the source metal electrode and the drain metal electrode at the same time when preparing the test electrode, the preparation efficiency can be further improved.

[0088] In a feasible embodiment, the method for preparing the conductivity test structure of the buffer layer in the semiconductor wafer can refer to Figures 4 to 9 , Figures 4 to 9 A schematic flow chart of a method for preparing a buffer layer conductivity test structure in a semiconductor wafer provided by an embodiment of the present invention. Specifically, the following steps may be included:

[0089] Step S21: providing a semiconductor preform; the semiconductor preform at least comprises a substrate 10, and a buffer layer, a channel layer and a barrier layer 12 sequentially grown in a direction away from the substrate 10, and a two-dimensional electron gas 20 is formed at a heterojunction interface formed by the channel layer and the barrier layer 12. Figure 4 .

[0090] Step S22: Spin-coat a photoresist on the multi-layer semiconductor and perform photolithography to form a patterned photoresist 13 to expose the surface of the semiconductor preform corresponding to the test area, and the remaining part is protected by the patterned photoresist 13. Figure 5 .

[0091] Step S23: using dry etching to etch the barrier layer 12 along the exposed surface of the semiconductor preform, and etching away part of the channel layer, so as to remove the two-dimensional electron gas 20 corresponding to the test area in the semiconductor preform. Figure 6 .

[0092] Step S24: removing the remaining patterned photoresist 13. Figure 7 .

[0093] Step S25: Repair the etching damage caused by dry etching. There are three repair methods, namely: 1. Perform heat treatment in the MOCVD chamber and introduce ammonia into the MOCVD chamber. In a high temperature environment, the ammonia decomposes to release nitrogen atoms. The nitrogen atoms can fill vacancy defects, thereby repairing the etching damage on the semiconductor surface. 2. Use a high temperature thermal annealing process to repair the etching damage. In a high temperature environment, the atoms in the damaged layer can be rearranged, thereby reducing the defect state density. 3. Use an alkaline solution cleaning process to repair the etching damage. The alkaline solution may include alkaline solutions such as tetramethylammonium hydroxide, potassium hydroxide, and ammonia water. It has a certain corrosiveness to Group III nitride semiconductor materials, and can remove the damaged layer, thereby reducing the surface state density. You can refer to Figure 8 .

[0094] Step S26: Deposit test electrodes 14 on the mesas on both sides of the etching area. The test electrodes can be selected from one or more combinations of metals such as Ni (nickel), Ti (titanium), Al (aluminum), Au (gold), Pt (platinum), Nb (niobium), etc., and the buffer layer conductivity test structure is prepared. At the same time, the source metal 15 and the drain metal 16 are deposited in other areas of the semiconductor wafer. The buffer layer conductivity test method is to set the two test electrodes 14 to high and low voltages respectively, and then read the current value between the two electrodes to calculate the conductivity of the buffer layer. Since the etching damage repair technology can efficiently remove the donor-type surface state, the buffer layer conductivity test structure designed by the present invention can accurately test the conductivity of the buffer layer. The test electrode 14, the source metal 15 and the drain metal 16 can be annealed at high temperature, or Si (silicon) ion implantation or etching of part of the semiconductor layer. In the subsequent transistor preparation process, the buffer layer conductivity test structure only needs to be protected with photoresist to complete the subsequent process steps. You can refer to Fig. 9 .

[0095] In a feasible embodiment, steps S22 to S26 in this embodiment can be replaced by the following steps, which can be specifically referred to in Figures 10 to 12 , Figures 10 to 12 A schematic flow chart of another method for preparing a conductivity test structure of a buffer layer in a semiconductor wafer provided by an embodiment of the present invention:

[0096] Step S31: Spin-coat a photoresist on the multilayer semiconductor and perform photolithography to form a patterned photoresist 13 to expose the surface of the semiconductor preform corresponding to the test area and the surface of the semiconductor preform corresponding to the isolation area 18, and the remaining part is protected by the patterned photoresist; Fig.10 ;

[0097] Step S32: using an ion implantation process, ions are implanted into the surface of the semiconductor preform away from the substrate 10, the surface area corresponding to the test area, and the surface area corresponding to the isolation area 18, until the channel layer with a partial thickness corresponding to the test area and the channel layer with a partial thickness corresponding to the isolation area 18 are doped, so as to remove the two-dimensional electron gas 20 corresponding to the test area and the isolation area 18 in the semiconductor preform, and obtain a pre-processed semiconductor wafer; the implanted ions are ions that can form a high resistance area 17 in the doped area of ​​the channel layer and the barrier layer 12; reference can be made to Fig.11 ;

[0098] Step S33: In the pre-processed semiconductor wafer surface away from the substrate 10, the test electrode 14, the source metal 15 and the drain metal 16 are prepared accordingly to obtain a buffer layer conductivity test structure. Fig.12 .

[0099] In this specification, each embodiment is described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the embodiments can be referred to each other. For the device disclosed in the embodiment, since it corresponds to the method disclosed in the embodiment, the description is relatively simple, and the relevant parts can be referred to the method part.

[0100] Finally, it should be noted that, in this article, relationships such as first and second, etc. are used only to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprises" or any other variations are intended to cover non-exclusive inclusion, so that a process, method, article or device that includes a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.

[0101] The above is a detailed introduction to a buffer layer conductivity test structure in a semiconductor wafer and a preparation method thereof provided by the present invention. Specific examples are used in this article to illustrate the principles and implementation methods of the present invention. The description of the above embodiments is only used to help understand the method of the present invention and its core idea; at the same time, for general technical personnel in this field, according to the ideas of the present invention, there will be changes in the specific implementation methods and application scopes. In summary, the content of this specification should not be understood as a limitation on the present invention.

Claims

1. A test structure for the conductivity of a buffer layer in a semiconductor wafer, It is characterized in that include: A substrate (10), and a buffer layer, a channel layer, and a barrier layer (12) grown sequentially in a direction away from the substrate (10); A two-dimensional electron gas (20) separated by a partition region (30) is formed at a heterojunction interface formed by the channel layer and the barrier layer (12); the partition region (30) is arranged corresponding to a test region of the buffer layer conductivity test structure; On one side of the buffer layer conductivity test structure facing away from the substrate (10), test electrodes (14) are respectively arranged on the table surfaces located on both sides of the test area.

2. The semiconductor wafer buffer layer conductivity test structure according to claim 1, It is characterized in that The isolation area (30) is a surface area of ​​the buffer layer conductivity test structure that is away from the substrate (10), corresponding to the test area, and has a recessed structure formed inwardly, in which the barrier layer (12) and a portion of the thickness of the channel layer are removed by an etching process to remove the two-dimensional electron gas (20) corresponding to the test area.

3. The semiconductor wafer buffer layer conductivity test structure according to claim 1, It is characterized in that The isolation region (30) is a surface area of ​​the buffer layer conductivity test structure that is away from the substrate (10) and corresponds to the test region, and is formed inwardly with ions implanted into the barrier layer (12) and a portion of the channel layer through a doping process to remove a high resistance region (17) of the two-dimensional electron gas (20) corresponding to the test region.

4. The semiconductor wafer buffer layer conductivity test structure according to any one of claims 1 to 3, It is characterized in that A test area is arranged at the edge of the semiconductor wafer, and the buffer layer conductivity test structure is arranged in the test area.

5. A method for preparing a buffer layer conductivity test structure in a semiconductor wafer, It is characterized in that include: A semiconductor preform is provided; the semiconductor preform comprises at least a substrate (10), and a buffer layer, a channel layer and a barrier layer (12) grown in sequence in a direction away from the substrate (10), wherein a two-dimensional electron gas (20) is formed at a heterojunction interface formed by the channel layer and the barrier layer (12); Removing the two-dimensional electron gas (20) corresponding to the test area in the semiconductor preform to obtain a pre-processed semiconductor wafer; In the surface of the pre-processed semiconductor wafer away from the substrate (10), test electrodes (14) are respectively prepared on the mesas located on both sides of the test area to obtain a buffer layer conductivity test structure.

6. The method for preparing a buffer layer conductivity test structure in a semiconductor wafer according to claim 5, It is characterized in that The removing of the two-dimensional electron gas (20) corresponding to the test area in the semiconductor preform to obtain a pre-processed semiconductor wafer comprises: A surface area of ​​the semiconductor preform that is away from the substrate (10) and corresponds to the test area is etched using a dry etching process until the barrier layer (12) corresponding to the test area is removed by etching, and a portion of the channel layer corresponding to the test area is removed by etching, so as to remove the two-dimensional electron gas (20) in the semiconductor preform that corresponds to the test area, thereby obtaining the pre-processed semiconductor wafer.

7. The method for preparing a conductivity test structure of a buffer layer in a semiconductor wafer according to claim 6, It is characterized in that After the surface area of ​​the semiconductor preform away from the substrate (10) corresponding to the test area is etched by a dry etching process until the barrier layer (12) corresponding to the test area is removed by etching, and a portion of the channel layer corresponding to the test area is removed by etching to remove the two-dimensional electron gas (20) in the semiconductor preform corresponding to the test area, to obtain the pre-processed semiconductor wafer, the method further comprises: The etching damage in the pre-treated semiconductor wafer is repaired by a high temperature thermal annealing treatment or an alkaline solution cleaning treatment.

8. The method for preparing a buffer layer conductivity test structure in a semiconductor wafer according to claim 5, It is characterized in that The removing of the two-dimensional electron gas (20) corresponding to the test area in the semiconductor preform to obtain a pre-processed semiconductor wafer comprises: An ion implantation process is used to implant ions into a surface area of ​​the semiconductor preform that is away from the substrate (10) and corresponds to the test area, until the channel layer having a partial thickness corresponding to the test area is doped, so as to remove the two-dimensional electron gas (20) in the semiconductor preform corresponding to the test area, thereby obtaining the pre-processed semiconductor wafer; the implanted ions are ions that can cause the doped areas of the channel layer and the barrier layer (12) to form a high resistance area (17).

9. The method for preparing a buffer layer conductivity test structure in a semiconductor wafer according to claim 8, It is characterized in that When using an ion implantation process to implant ions into a surface area of ​​the semiconductor preform away from the substrate (10) corresponding to the test area, the method further comprises: An ion implantation process is used to implant ions into a surface area of ​​the semiconductor preform that is away from the substrate (10) and corresponds to the isolation region (18) until the channel layer having a partial thickness corresponding to the isolation region (18) is doped, so as to remove the two-dimensional electron gas (20) in the semiconductor preform that corresponds to the isolation region (18).

10. The method for preparing a buffer layer conductivity test structure in a semiconductor wafer according to claim 5, It is characterized in that When test electrodes (14) are prepared on the mesas located on both sides of the test area in the surface of the pre-processed semiconductor wafer away from the substrate (10), the method further comprises: In the surface of the pre-processed semiconductor wafer away from the substrate (10), a table outside the test area and located between two adjacent isolation areas (18) is deposited to prepare a source metal (15) and a drain metal (16).

11. The method for preparing a conductivity test structure of a buffer layer in a semiconductor wafer according to claim 5, It is characterized in that The removing of the two-dimensional electron gas (20) corresponding to the test area in the semiconductor preform to obtain a pre-processed semiconductor wafer comprises: Preparing a photoresist on a surface of the semiconductor preform away from the substrate (10); Performing patterning on the photoresist to expose a surface area of ​​the semiconductor preform that is away from the substrate (10) and corresponds to the test area, thereby obtaining a patterned photoresist (13); An etching process or a doping process is performed on the surface area exposed by the patterned photoresist (13) to remove the two-dimensional electron gas (20) corresponding to the test area in the semiconductor preform, thereby obtaining the pre-processed semiconductor wafer.