PVD Molybdenum Gradient Oxidation And Etching For Bottom On Bottom Gap Filling

Through gradient oxidation and etching technology, the problems of seams and voids during metal gap filling in manufacturing in microelectronics are solved, and seamless bottom-up gap filling is achieved, reducing manufacturing costs and defect risks.

CN119054068APending Publication Date: 2024-11-29APPLIED MATERIALS INC
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202380034945.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-04-25
Filing Date
2023-03-30
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

In microelectronic device manufacturing, there is a barrier during metal gap filling process that the fill material closes the gap before the bottom is completely filled, and traditional removal methods may cause the seed layer at the bottom of the gap to be removed, increasing manufacturing costs and the risk of defects.

Method used

The bottom surface of the substrate is preferentially oxidized by gradient oxidation, followed by etching back and isotropic etching to remove unnecessary seed layers, retain the bottom metal seed layer, and fill or partially fill features through metal gap filling treatment, using inductively coupled plasma The bulk technology enables selective oxidation and etching, ensuring seamless bottom-up gap filling.

Benefits of technology

It effectively solves the problems of seams and voids during metal gap filling, reduces manufacturing time and defect risks, improves filling quality and efficiency, and achieves seamless bottom-up gap filling.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119054068A_ABST
    Figure CN119054068A_ABST
Patent Text Reader

Abstract

A method and apparatus for gap filling in a semiconductor device are provided. The method includes forming a metal seed layer on an exposed top surface of a substrate, where the substrate has a feature in the form of a trench or via formed in the top surface of the substrate, the feature having sidewalls and a bottom surface extending between the sidewalls. A gradient oxidation treatment is performed to oxidize the exposed portion of the metal seed layer to form a metal oxide, wherein the gradient oxidation treatment preferentially oxidizes a field region of the substrate above the bottom surface of the feature. And removing the oxidized part of the seed crystal layer through etching-back treatment. The second etching process removes other portions of the seed layer. The metal gap filling process fills or partially fills the feature with a gap filling material.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] Embodiments of the present invention relate to a method and apparatus for forming a thin film. More specifically, the present disclosure relates to a method and apparatus for metal gap filling in semiconductor devices.

[0002] background

[0003] The manufacture of microelectronic devices typically involves complex processing sequences that require hundreds of individual processes to be performed on semiconductor, dielectric, and conductive substrates. Examples of these processes include oxidation, diffusion, ion implantation, thin film deposition, cleaning, etching, photolithography, and other operations. Each operation is time-consuming and expensive.

[0004] As the critical dimensions of microelectronic devices continue to decrease, the design and manufacture of these devices on substrates are becoming or have become increasingly complex. Control of critical dimensions and process uniformity is becoming increasingly important. Complex multilayer stacks used to manufacture microelectronic devices involve precise process monitoring of critical dimensions such as thickness, roughness, stress, density, and potential defects. The process recipe used to form the device has multiple incremental processes to ensure that the critical dimensions are maintained. Typically, each incremental process may utilize one or more process chambers, which adds additional time for forming the device and also increases the chance of defects. Therefore, each process increases the overall manufacturing cost and the risk of defects in the completed microelectronic device.

[0005] Furthermore, as the critical dimensions of these devices shrink, past manufacturing techniques encounter new obstacles. For example, when preparing a liner and / or seed layer to grow a metal gap fill, the liner and / or seed layer may still be present at the sides of the gap, potentially causing the gap to close before the fill material is completely filled at the bottom. Conventional methods for removing the seed layer from the sides and top surface of the gap may additionally result in the removal of the seed layer at the bottom of the gap used to seed the fill material.

[0006] For at least the foregoing reasons, there is a continuing need for improved gap fill manufacturing methods.

[0007] Overview

[0008] The present disclosure relates to a method and apparatus for forming a thin film. More particularly, the present disclosure relates to a method and apparatus for filling features on a substrate.

[0009] In one example, a method of filling a feature on a substrate is provided. The method includes forming a metal seed layer on an exposed top surface of a substrate, wherein the substrate has a feature in the form of a trench or via formed in the top surface of the substrate, the feature having sidewalls and a bottom surface extending between the sidewalls. A gradient oxidation process is performed to oxidize an exposed portion of the metal seed layer to form a metal oxide, wherein the gradient oxidation process preferentially oxidizes a field region of the substrate above the bottom surface of the feature. An etch back process removes an oxidized portion of the seed layer. A second etching process removes other portions of the seed layer. A metal gap fill process fills or partially fills the feature with a gap fill material.

[0010] In another example, another method for filling features on a substrate is provided. The method includes depositing a molybdenum-containing layer on an exposed surface of a substrate, wherein the substrate includes a plurality of features formed in a top surface of the substrate, each of the plurality of features having a sidewall surface and a bottom surface, and the deposited molybdenum-containing layer is formed on the top surface of the substrate and the sidewall surface and bottom surface of the plurality of features. The exposed surface of the substrate is exposed to a gradient oxidation process, wherein the gradient oxidation process forms an oxidized region of the molybdenum-containing layer. The oxidized region is preferentially etched, wherein after the preferential etching of the oxidized region, a first portion of the deposited molybdenum-containing layer remains on the bottom surface of each of the plurality of features. An isotropic etching process removes a portion of the molybdenum-containing layer. Filling the features with a second molybdenum layer, wherein filling the features with the second molybdenum layer includes growing the second molybdenum layer from a second portion of the molybdenum-containing layer deposited on the sidewall surface and a first portion of the deposited molybdenum-containing layer on the bottom surface of each feature.

[0011] In yet another example, a cluster tool for filling features on a substrate is provided. The cluster tool includes an oxygen source fluidly coupled to a processing region of a first processing chamber, wherein the oxygen source is configured to deliver an oxygen-containing gas to the processing region. The cluster tool has a first flow control valve and a first inductively coupled plasma source, the first flow control valve being configured to control the flow of an oxygen-containing gas provided from the oxygen source to the processing region, and the first inductively coupled plasma source being configured to generate plasma in the processing region, wherein the plasma includes an oxygen-containing gas and a controller. The cluster tool includes a second processing chamber having a first etching gas source fluidly coupled to a processing region of a second processing chamber, a second flow control valve configured to control the flow of a first etching gas provided by the first etching gas source to the processing region, and a second etching gas source fluidly coupled to the processing region of the second processing chamber, wherein the second etching gas source is configured to deliver a second etching gas to the processing region, wherein a third flow control valve is configured to control the flow of a second etching gas provided from the second etching gas source to the processing region. The controller is configured to form a metal seed layer on an exposed top surface of a substrate, wherein the substrate has a feature in the form of a trench or via formed in the top surface of the substrate, the feature having sidewalls and a bottom surface extending in the sidewalls. The controller is also configured to perform a gradient oxidation process to oxidize the exposed portion of the metal seed layer to form a metal oxide, wherein the gradient oxidation process preferentially oxidizes a field region of the substrate above the bottom surface of the feature. The controller performs an etch back process to remove an oxidized portion of the seed layer. The controller performs a second etching process to remove a portion of the seed layer and performs a molybdenum gap fill process to fill or partially fill the feature with a gap fill material.

[0012] BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Thus, the manner in which the above-described features of the present disclosure may be understood in detail may be that the present disclosure, briefly summarized above, may be more particularly described with reference to embodiments, some of which are illustrated in the accompanying drawings. It should be noted, however, that the drawings illustrate only typical embodiments of the present disclosure and are therefore not to be considered limiting of its scope, as the present disclosure may admit to other equally effective embodiments.

[0014] Figure 1 A schematic top view illustrating one example of a multi-chamber processing tool according to one or more embodiments of the present disclosure.

[0015] Figures 2A-2F Illustrated are views of a semiconductor device during different stages of fabrication in accordance with one or more embodiments of the present disclosure.

[0016] Figure 3A flow chart of a method for filling features on a substrate according to one or more embodiments of the present disclosure is illustrated.

[0017] To facilitate understanding, identical reference numerals have been used, where possible, to designate identical elements that are common to the figures. It is contemplated that elements and features of one embodiment may be beneficially incorporated in other embodiments without further recitation.

[0018] Specific description

[0019] In the above overview, the following detailed description, the claims and the drawings, reference is made to specific features (including method operations) of the present disclosure. It should be understood that the disclosure in this specification includes all possible combinations of these specific features. For example, where a specific feature is disclosed in the context of a specific aspect or embodiment of the present disclosure or a specific claim, the feature may also be used in combination with other features and / or in the context of other features in the specific aspects and embodiments of the present disclosure, as well as in the general case of the disclosed invention, to the extent possible.

[0020] As used herein, the term "comprising" and its grammatical equivalents refer to the optional presence of other components, ingredients, operations, etc. For example, an article "comprising" (or "including") components A, B, and C may consist of (i.e., only include) components A, B, and C, or may include not only components A, B, and C but also one or more other components.

[0021] When this document refers to a method that includes two or more defined operations, the defined operations may be performed in any order or simultaneously (unless the context excludes such a possibility), and the method may include one or more other operations performed before any defined operation, between two defined operations, or after all defined operations (unless the context excludes such a possibility).

[0022] Embodiments of the present disclosure relate to a method and apparatus for filling features on a substrate. For example, the method can perform highly selective gradient oxidation and etching of physical vapor deposited (PVD) metals as a bottom seed layer in a bottom-up gap fill. The metal gap fill process can be used to deposit different metals, such as tungsten (W), molybdenum (Mo), ruthenium (Ru), and other metals. The present disclosure includes separate process sequences that include metal oxidation (e.g., WO x 、MoO x ) treatment and for the selective removal of metal oxides.

[0023] PVD metal deposition typically results in a thicker film on the area around the via (or trench) and a thinner film at the bottom of the via. The oxidation and etching gradient process selectively removes the field metal. The metal placed in the area around the via is "selectively" oxidized seven times faster than the metal placed at the bottom of the via. Selective oxidation allows the subsequent etching process to remove the field metal oxide while leaving a small bottom metal layer as a seed for the metal fill. The selectivity of etching to remove the oxidized metal in the field relative to the bottom (unoxidized) metal is very high, resulting in a thin metal seed layer remaining at the bottom of the via. The oxidation process uses an inductively coupled (ICP) oxygen (O2) plasma with low power, low O2 flow and high temperature reaction to produce a high ion ratio at low ion energy, which enhances the selectivity of preferentially oxidizing the metal in the field rather than the metal at the bottom of the via. Using this method, the field metal can be completely removed while leaving a good quality metal seed layer at the bottom of the structure, achieving seamless bottom-up gap fill.

[0024] Examples of processing systems that may be suitably modified according to the teachings provided herein include integrated processing systems or other suitable processing systems commercially available from Applied Materials, Inc. located in Santa Clara, Calif. It is contemplated that other processing systems, including those from other manufacturers, may be adapted to benefit from the aspects described herein.

[0025] Figure 1 A schematic top view of an example multi-chamber processing system 100 or cluster tool is shown, which can be used to perform gradient oxidation and etching of PVD metals according to embodiments of the present disclosure. The processing system 100 includes a plurality of processing chambers 102 coupled to a first transfer chamber 104. The first transfer chamber 104 is also connected to a first pair of pass-through chambers 106. The first transfer chamber 104 has a centrally disposed transfer robot (not shown) for transferring substrates between the pass-through chamber 106 and the processing chamber 102. The pass-through chamber 106 is coupled to a second transfer chamber 110, which is coupled to a processing chamber 114 configured to perform a pre-cleaning process and a processing chamber 116 or an atomic deposition chamber configured to perform a PVD deposition process (or alternatively, an epitaxial growth process). The second transfer chamber 110 has a centrally disposed transfer robot (not shown) for transferring substrates between a set of load lock chambers 112 and the processing chambers 114 or the processing chambers 116. The factory interface 120 is connected to the second transfer chamber 110 through the load lock chamber 112. The factory interface 120 is coupled to one or more pods 130 on the opposite side of the load lock chamber 112. The pods 130 may be front opening unit pods (FOUP) or similar devices for storing and transporting substrates.

[0026] Prior to various operations, the substrate may first be transferred from one of the wafer transfer boxes 130 to the processing chamber 114 where a pre-cleaning process is performed to remove contaminants, such as carbon or oxide contaminants, from exposed surfaces of source / drain regions of transistors formed on the substrate.

[0027] The substrate is then transferred to one or more processing chambers 102. In some embodiments, the processing chamber 102 can etch a via or trench in a dielectric material layer of the substrate. In some embodiments, the substrate is provided to an etching chamber that is not part of the processing system 100 to perform a trench formation process. In other operations, the substrate has a trench formed therein. Once the trench is formed in the dielectric material, the substrate is transferred to the processing chamber 114 for cleaning.

[0028] The substrate is then transferred to at least one of the processing chambers 116 and / or the processing chambers 102, where one or more operations are performed. For example, the substrate is transferred to one of the processing chambers 102, where a metal deposition operation is performed to form a seed layer. The metal can be deposited in any suitable chamber, such as a PVD chamber, an atomic layer deposition (ALD) chamber, an epitaxy (EPI) chamber, or other suitable chamber.

[0029] After the deposition of the seed layer, the substrate can be transferred to one of the processing chambers 102 where a gradient oxidation operation can be performed. The gradient oxidation can be performed in an inductively coupled plasma (ICP) reactor or other suitable plasma processing chamber. The gradient oxidation operation is configured to oxidize unwanted portions of a metal layer formed on the substrate. For example, a metal formed in the bottom and sidewalls of a trench or via can be oxidized together with a metal disposed in a field region (i.e., the top side of the substrate).

[0030] The substrate is transferred to one of the processing chambers 102, where an etching operation is performed to selectively remove the oxidized portion of the deposited metal layer. For example, the etching operation can be performed in an etching chamber. Alternatively, the etching operation can be performed in an ICP reactor that performs gradient oxidation.

[0031] After the etching operation, a portion of the deposited metal layer (e.g., seed material) will remain thicker along the bottom surface of the via or trench and remain thinner in the field region. In some embodiments, the seed material may additionally be present along the sidewalls of the feature. An isotropic etching process may be performed to target the seed layer. The isotropic etching process may be performed in the same or a second processing chamber to remove a portion of the seed material. The isotropic etching process removes the seed material in the field region while thinning the thicker seed material along the bottom surface of the via or trench. The isotropic etching process results in only the seed material remaining primarily in the via, in preparation for the gap fill operation.

[0032] The substrate may then be transferred to one of the processing chambers 102 or 116 where a gap fill operation is performed. The gap fill operation may be performed in a CVD chamber, an ALD chamber, or other suitable chamber. For example, the processing chamber 102 or 116 may deposit a metal (e.g., tungsten (W), molybdenum (Mo), ruthenium (Ru), or other suitable material grown on a seed layer disposed at the bottom of a trench or on a feature) to form a portion of a microelectronic device.

[0033] The system controller 180 is coupled to the processing system 100 for controlling the processing system 100 or components thereof. For example, the system controller 180 may control the operation of the processing system 100 using direct control of the chambers 102, 104, 106, 110, 112, 114, 116, 120, 130 of the processing system 100 or by controlling controllers associated with the chambers 102, 104, 106, 110, 112, 114, 116, 120, 130. In operation, the system controller 180 enables data and feedback to be collected from the various chambers to coordinate the execution of the processing system 100.

[0034] The system controller 180 generally includes a central processing unit (CPU) 182, a memory 184, and support circuits 186. The CPU 182 may be one of any form of general purpose processor that may be used in an industrial environment. The memory 184, a non-transitory computer readable medium or a machine readable storage device, may be accessed by the CPU 182 and may be one or more disks in a memory such as a random access memory (RAM), a read-only memory (ROM), a floppy disk, a hard disk, or any other form of local or remote digital storage. The support circuits 186 are coupled to the CPU 182 and may include caches, clock circuits, input / output subsystems, power supplies, etc. Various implementations disclosed in the present disclosure may generally be implemented under the control of the CPU 182 by executing computer instruction codes stored in the memory 184 (or in the memory of a particular processing chamber), such as a computer program product or software routine. That is, the computer program product is tangibly embodied on the memory 184 (or a non-transitory computer readable medium or a machine readable storage device). When the CPU 182 executes the computer instruction codes, the CPU 182 controls the chamber to perform operations according to various embodiments.

[0035] System controller 180 is configured to execute methods such as method 300 stored in memory 184 (described further below).

[0036] In some embodiments, the first processing chamber 102 includes an oxygen source 132 fluidly coupled to a processing region 140 of the first processing chamber 102, wherein the oxygen source 132 is configured to deliver an oxygen-containing gas to the processing region 140. The first processing chamber 102 may further include a first flow control valve 133 configured to control a flow rate of the oxygen-containing gas provided from the oxygen source 132 to the processing region 140. The first processing chamber 102 may further include an etching gas source 136 fluidly coupled to the processing region 140 of the first processing chamber 102, wherein the etching gas source 136 is configured to deliver an etching gas to the processing region 140. The first processing chamber 102 may also include a second flow control valve 137 configured to control a flow rate of the etching gas provided from the etching gas source 136 to the processing region 140. The first processing chamber 102 may further include an inductively coupled plasma source 138 configured to generate a plasma in the processing region 140, wherein the plasma includes a hydrogen-containing gas and an oxygen-containing gas.

[0037] In some embodiments, the system controller 180 is configured to control the first flow control valve 133 so that a certain amount of oxygen-containing gas is provided to the surface of the substrate disposed in the processing area 140 of the first processing chamber 102. The oxygen-containing gas preferentially oxidizes the sidewalls of one or more metal-containing layers disposed on the field area and the features formed in the substrate. The system controller 180 is also configured to control the second flow control valve 137 so that a certain amount of etching gas provided to the surface of the substrate preferentially etches the oxidized portions of one or more metal-containing layers disposed on the field area and the sidewalls of the features formed in the substrate. After the oxidized portions of the one or more metal-containing layers are etched, the system controller 180 may optionally control another or the same flow control valve in the same processing chamber so that the amount of the second etching gas provided to the surface of the substrate preferentially etches the one or more metal-containing layers disposed on the field area and the features formed in the substrate.

[0038] Alternatively, after etching the oxidized portion of the one or more metal-containing layers, the substrate can be moved to a second processing chamber in the cluster tool. The second processing chamber has a first etching gas source fluidly coupled to a processing region of the second processing chamber, a second flow control valve configured to control a flow of the first etching gas provided from the first etching gas source to the processing region, and a second etching gas source fluidly coupled to the processing region of the second processing chamber, wherein the second etching gas source is configured to deliver the second etching gas to the processing region, wherein the third flow control valve is configured to control the flow of the second etching gas provided by the second etching gas source to the processing region. The system controller 180 is also configured to control the third flow control valve so that a certain amount of etching gas provided to the surface of the substrate preferentially etches one or more metal-containing layers disposed on the field region and features formed in the substrate.

[0039] Figures 2A-2F and Figure 3 Will discuss together. Figures 2A-2F Shown for illustration Figure 3 The method 300 is provided for providing cross-sectional views of some embodiments of device structures of semiconductor devices at different stages of fabrication. The method 300 can be used to fill various features, such as trenches or vias with gap-fill metal. Figures 2A-2F The method 300 is described, but it should be understood that Figures 2A-2F The structure disclosed in is not limited to the method 300, but can exist independently as a structure independent of the method 300. Similarly, although Figures 2A-2F The method 300 is described, it should be understood that the method 300 is not limited to Figures 2A-2F The structure disclosed in the Figures 2A-2F The structure disclosed in .

[0040] For the sake of clarity, some reference numerals in later figures illustrating subsequent stages have been omitted. When discussing features that are called out in later figures, reference numerals may be gleaned from earlier figures. For example, Figure 2B The reference numerals in the Figure 2A Some features disclosed in are omitted.

[0041] The method 300 begins at operation 310, where a substrate having a trench or a via formed in a top surface is provided. The substrate may be a device substrate or a semiconductor substrate as described herein. Figure 2A Illustrated is a cross-sectional view of a semiconductor device structure 200 during an intermediate stage of fabrication corresponding to operation 310, in accordance with some embodiments. The semiconductor device structure 200 includes a body 210 having a dielectric layer 220 formed thereon.

[0042] The body 210 of the semiconductor device structure 200 can be or include a bulk semiconductor substrate, a semiconductor on insulator (SOI) substrate, etc., which can be doped (e.g., with a p-type dopant or an n-type dopant) or undoped. In some embodiments, the semiconductor material of the body 210 can include a single element semiconductor, such as silicon (Si) or germanium (Ge); a compound semiconductor, including, for example, silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, and / or indium antimonide; an alloy semiconductor including, for example, SiGe, GaAsP, AlInAs, GaInAs, GaInP, and / or GaInAsP; combinations thereof, etc. The body 210 can include additional materials, such as a silicide layer, a metal silicide layer, a metal layer, a dielectric layer, or a combination thereof.

[0043] The dielectric layer 220 may include multiple layers. The dielectric layer 220 includes a top surface 229. In some embodiments, the dielectric layer 220 is silicon oxide, silicon oxynitride, silicon nitride, or a combination thereof. In some embodiments, the dielectric layer 220 is mainly composed of silicon oxide. It should be noted that the foregoing descriptors (e.g., silicon oxide) should not be interpreted as disclosing any specific stoichiometric ratio. Therefore, "silicon oxide" and the like will be understood by those skilled in the art as a material consisting essentially of silicon and oxygen without disclosing any specific stoichiometric ratio.

[0044] The dielectric layer 220 is patterned with one or more features 222. In some embodiments, the features 222 can be selected from trenches, vias, holes, or combinations thereof. In a particular embodiment, the features 222 are vias.

[0045] At operation 320, a liner layer 225 is formed on the surface of one or more features. The liner layer 225 may be formed by a PVD process, an ALD process, an EPI process, or other suitable deposition process. The liner layer 225 may be formed of titanium silicon (nitride) or other suitable material. The liner layer 225 may be formed on the exposed surface of the substrate. Figure 2A As shown, liner layer 225 is disposed in feature 222 and along top surface 229 of dielectric layer 220. When feature 222 is a trench structure, liner layer 225 can be disposed within feature 222. Alternatively, when feature 222 is a via, liner layer 225 can be optional. Liner layer 225 can be disposed on top surface 229 of dielectric layer 220, including upper surface or field region 227. In the following discussion, when liner layer 225 is not present, field region 227 corresponds to top surface 229 of dielectric layer 220.

[0046] The initial thickness of liner layer 225 can be in the range of about 0 angstroms to about 100 angstroms, for example, in the range of about 20 angstroms to about 50 angstroms. In some embodiments, liner layer 225 can be discontinuous along, for example, sidewall surface 223 and / or bottom surface 224 of feature 222. Any suitable metal deposition process can be used to deposit liner layer 225. In one example, a PVD process is used to deposit liner layer 225.

[0047] Feature 222 has a first depth measured from field region 227 to bottom surface 224 and a width defined between two sidewall surfaces 223. In some embodiments, the depth is in a range of about 2nm to 200nm, 3nm to 200nm, 5nm to 100nm, 2nm to 100nm, or 50nm to 100nm. In some embodiments, the width is in a range of about 2nm to 100nm, 4nm to 20nm, 10nm to 50nm, or 50nm to 100nm. In some embodiments, feature 222 has an aspect ratio (depth / width) in a range of about 1 to 20, 1 to 4, 1 to 2, or 3 to 4.

[0048] In some embodiments, feature 222 extends downward from field region 227 into body 210. Feature 222 includes sidewall surfaces 223 and a bottom surface 224 extending between sidewall surfaces 223. Sidewall surfaces 223 and bottom surface 224 are formed by exposed liner layer 225 when a liner is present, and are formed on dielectric layer 220 when liner layer 225 is not present. In some embodiments, sidewall surfaces 223 are tapered.

[0049] In operation 330 , a seed layer 230 is formed over the surface of one or more features, for example, over the surface of the liner layer 225 . Figure 2B A cross-sectional view of semiconductor device structure 200 is illustrated during an intermediate stage of fabrication corresponding to operation 330 in accordance with some embodiments. Seed layer 230 may be formed on exposed surfaces of the substrate, namely, over sidewall surfaces 223 and bottom surface 224 of feature 222 and on field region 227.

[0050] The seed layer 230 is a metal material suitable for use as a seed layer for subsequent deposition of a metal gap filling material. The seed layer 230 may be molybdenum (Mo) or a molybdenum-containing layer, tungsten (W) or a tungsten-containing layer, or ruthenium (Ru) or a ruthenium-containing layer. In one example, the seed layer 230 is a molybdenum (Mo) or a molybdenum-containing layer. The seed layer 230 may be formed on the sidewall surface 223 and the bottom surface 224 of one or more features 222 and on the field region 227. The seed layer 230 may be a conformal layer. The seed layer 230 may be deposited using any suitable deposition process 232. In one example, the seed layer 230 is deposited using a physical vapor deposition (PVD) process. Alternatively, the seed layer 230 may be formed using a low temperature, low pressure CVD or ALD process. The seed layer 230 may be used to repair any damage or discontinuity in the liner layer. In one example, the deposition process 232 may be cycled and repeated for 3 to 7 cycles or at least even as little as 1-2 cycles.

[0051] Seed layer 230 may create an overhang in field region 227 that obstructs or blocks a top opening of one or more features 222. The overhang reduces the width of the top opening at the top of feature 222 from a first, larger width to a second, narrower width.

[0052] At operation 340 , the seed layer 230 is exposed to a gradient oxidation process. Figure 2C A cross-sectional view of the semiconductor device structure 200 is illustrated during an intermediate stage of fabrication corresponding to operation 340 in accordance with some embodiments. The gradient oxidation process oxidizes portions of the seed layer 230 to form an oxide seed layer 240 .

[0053] In some embodiments, the gradient oxidation process includes using an O2 inductively coupled plasma (ICP) that includes a limited gas flow to produce an oxygen-deficient reaction mode on the exposed metal seed layer 230 (e.g., a molybdenum-containing layer). The O2ICP provides a low-power O2 plasma 242 with a high ion / radical ratio that enhances field oxidation and deactivates active species before reaching the molybdenum-containing seed layer 230 above the bottom surface 224. In this mode, the field region 227 and the overhang 234 are oxidized, or more severely oxidized, which allows preferential etching of the oxidized region of the oxidized seed layer 240 while maintaining the seed layer 230 along the bottom surface 224 of the feature 222. In one example, the oxidation of the seed layer 230 is seven times more selective at the field region 227 than at the bottom surface 224. Therefore, the oxidized seed layer 240 is preferentially formed in the field region 227. In one example, the gradient oxidation of the molybdenum-containing seed layer 230 results in MoO x The oxidation seed layer 240 is formed.

[0054] In some embodiments, the gradient oxidation treatment includes a reduction treatment followed by an oxidation treatment. In some embodiments, the gradient oxidation treatment includes an oxidation treatment without a reduction treatment. The reduction treatment includes exposing the substrate to a reducing gas, such as hydrogen. The oxidation treatment includes exposing the substrate to an oxidizing gas, such as oxygen. In some embodiments, during the reduction treatment, the processing area is maintained at a pressure of less than about 120 mTorr, such as in a range of about 50 mTorr to about 110 mTorr, in a range of about 60 mTorr to about 100 mTorr, or, for example, in a range from about 70 mTorr to about 90 mTorr. Exposing the semiconductor device structure 200 to the reducing gas includes flowing the reducing gas into the processing area at a flow rate of about 200 sccm or less, such as in a range from about 100 sccm to about 170 sccm, or from about 120 sccm to about 80 sccm. Exposing the semiconductor device structure 200 to the reducing agent may also include flowing a carrier gas (e.g., an inert gas such as argon) into the processing region at a flow rate of about 300 sccm or less, such as in a range of about 100 sccm to about 200 sccm, or in a range of about 120 sccm to about 150 sccm. During the reduction process, the semiconductor device structure 200 may be maintained at a temperature of about 450 degrees Celsius or less, such as in a range of about 200 degrees Celsius to about 450 degrees Celsius, in a range of about 250 degrees Celsius to about 400 degrees Celsius, or, for example, in a range of about 300 degrees Celsius to about 350 degrees Celsius. During the reduction process, an ICP plasma power of 2000 watts or less, such as in a range of about 500 watts to 1500 watts, or, for example, in a range of about 850 watts to about 1000 watts, is applied to maintain the plasma. The reduction treatment may be performed for a period of 60 seconds or less, such as in the range of about 10 seconds to about 40 seconds, or such as in the range of about 10 seconds to about 30 seconds.

[0055] In some embodiments, during the oxidation process, the processing region is maintained at a pressure of less than about 10 mTorr, such as in a range of about 1 mTorr to about 5 mTorr, or such as in a range of about 1 mTorr to about 2 mTorr. Exposing the seed layer 230 to the oxidizing gas includes flowing the oxidizing gas into the processing region at a flow rate of about 20 sccm or less, such as in a range of about 1 sccm to about 10 sccm, or in a range of about 1 sccm to about 5 sccm. Exposing the seed layer 230 to the reducing agent may also include flowing a carrier gas (e.g., an inert gas such as argon, neon, or krypton) into the processing region at a flow rate of about 100 sccm or less, such as in a range from about 50 sccm to about 100 sccm, or in a range from about 50 sccm to about 100 sccm. During the oxidation process, the semiconductor device structure 200 may maintain a temperature of about 450 degrees Celsius or less, such as in a range of about 200 degrees Celsius to about 450 degrees Celsius, in a range of about 250 degrees Celsius to about 400 degrees Celsius, or, for example, in a range from about 300 degrees Celsius to about 350 degrees Celsius. During the oxidation process, the ICP plasma power is 300 watts or less, such as in a range of about 100 watts to 300 watts, or, for example, in a range of about 180 watts to about 210 watts. The oxidation process may be performed for a period of 60 seconds or less, such as in a range of about 10 seconds to about 40 seconds, or, for example, in a range of about 12 seconds to about 30 seconds.

[0056] In some embodiments, the oxidation process is performed at a pressure in a range of about 2 mTorr to about 7 mTorr, an ICP power in a range of about 210 Watts to about 350 Watts, an argon flow rate into the process region in a range of about 50 sccm to about 100 sccm, an oxygen flow rate into the process region in a range of about 2 sccm to about 10 sccm, at a temperature in a range of about 300 degrees Celsius to about 400 degrees Celsius, and for a time period of about 90 seconds to about 180 seconds.

[0057] At operation 350 , the oxide seed layer 240 is exposed to an etch-back process. Figure 2D A cross-sectional view of the semiconductor device structure 200 during an intermediate stage of fabrication corresponding to operation 350 according to some embodiments is illustrated. The etch-back process selectively targets the oxidized seed layer 240 above the seed layer 230. That is, the lower etch rate of the metallic molybdenum (seed layer 230) on its oxide (oxidized seed layer 240) results in additional removal of the seed layer 230 in the field region 227 and the sidewalls 223 on the bottom surface 224.

[0058] The etch-back process includes flowing an etching gas and an optional inert gas into the processing area. The etching gas may include a chlorine-containing or fluorine-containing gas or a combination thereof, wherein the etchant is selected to be reactive to the metal oxide (i.e., the oxidized seed layer 240) above the non-oxide metal (i.e., the seed layer 230). In some embodiments, the etch-back process is performed at a pressure of about 5 mTorr to about 20 mTorr, an ICP power of about 300 watts to about 400 watts, an argon gas flow rate flowing into the processing area in the range of about 450 sccm to about 500 sccm, a WF6 gas flow rate flowing into the processing area in the range of about 5 sccm to about 10 sccm, and a temperature in the range of about 300 degrees Celsius to about 470 degrees Celsius for a period of about 15 seconds to about 30 seconds. The oxidized seed layer 240 may be optionally hot-dipped in WF6 or a chlorine-containing gas at a high pressure of about 0.5 torr to about 15.0 torr.

[0059] The etch-back process exposes the oxidized seed layer 240 to an etchant process to selectively remove the oxidized seed layer 240 while minimizing removal of the underlying seed layer 230. The etch-back process may be sufficient to reduce the thickness of the seed layer 230 from an initial thickness to a target reduced thickness in the field region 227, and in some examples, completely remove the seed layer 230 from the sidewalls, such as Figure 2D . In one example, the bottom portion 235 of the seed layer 230 remains thicker than the field portion 233 of the seed layer 230. Therefore, the seed layer 230 in the field region 227 is thinner than the seed layer 230 formed over the bottom surface 224. That is, the remaining thickness of the molybdenum-containing seed layer 230 formed over the field region 227 is reduced to be greater than the thickness of the molybdenum-containing seed layer 230 formed over the bottom surface 224 of the feature 222.

[0060] In operation 360, one or more features are isotropically etched. Figure 2E A cross-sectional view of the semiconductor device structure 200 during an intermediate stage of fabrication corresponding to operation 360 is illustrated in accordance with some embodiments. The isotropic etch-back process removes the remaining seed layer 230 in the field region 227 and along the bottom surface 224 of the feature 222 at a similar rate. However, due to the increased thickness of the seed layer 230 along the bottom surface 224 compared to the field region 277, the isotropic etching results in only the material of the seed layer 230 remaining along the bottom surface 224 of the feature 222. Removing the seed layer 230 from all surfaces except the bottom surface 224 improves the film quality during subsequent metal bottom-up fill. Removing the seed layer 230 from the sidewall surface 223 and the field region 227 substantially inhibits the formation of seams and voids that exist during conventional processing during subsequent metal gap fill. Retaining the seed layer 230 only along the bottom surface 224 of the feature 222 for metal gap bottom-up fill substantially results in seamless metal gap fill.

[0061] At operation 370 , one or more features are filled with a metallic material. Figure 2F A cross-sectional view of a semiconductor device structure 200 during an intermediate stage of manufacturing corresponding to operation 360 according to some embodiments is illustrated. A metal may be formed on the seed layer 230 to fill the feature 222 to form a gap fill layer 250. The gap fill layer 250 may be deposited using any suitable metal deposition process. The gap fill layer 250 may be deposited by a chemical vapor deposition (CVD) gap fill process. The gap fill layer 250 may partially or completely fill one or more features. The gap fill layer 250 is formed of a metal such as tungsten (W), molybdenum (Mo), or ruthenium (Ru). In an example, the gap fill layer 250 is formed of molybdenum (Mo).

[0062] In some embodiments, the gap-fill layer 250 is formed using a chemical vapor deposition (CVD) process that includes simultaneously flowing (co-flowing) a molybdenum-containing precursor gas and a reducing agent into a processing region and exposing the semiconductor device structure 200 .

[0063] In another embodiment, the gapfill layer 250 is deposited using an atomic layer deposition (ALD) process at operation 360. The molybdenum gapfill ALD process includes repeated cycles of alternatingly exposing the semiconductor device structure 200 to a molybdenum-containing precursor gas and a reducing agent and purging the process region between alternating exposures.

[0064] In other embodiments, the gap-fill layer 250 is deposited using a pulsed CVD method that includes repeated cycles of alternatingly exposing the semiconductor device structure 200 to a molybdenum-containing precursor gas and a reducing gas without purging the process area.

[0065] The previously described embodiments of the present disclosure have many advantages, including a metal oxidation process and a selective metal oxide removal process which can be completed in two process chambers or a single process chamber, thereby reducing manufacturing time and the possibility of process-induced defects. The method utilizes an inductively coupled plasma (ICP) O2 plasma, which includes a diffusion-limited gas flow within a feature (e.g., a trench or via) formed on a substrate to produce an oxygen-deficient reaction. In one embodiment, the use of an ICP O2 plasma (a low, weak energy O2 plasma with a high ion / radical ratio) is created to enhance field oxidation and deplete reactive oxygen species before reaching the bottom of a trench structure or gap. This provides good selectivity (>7) in the trench structure, and the top field metal is thinned compared to the seed material remaining at the bottom of the trench structure or gap. A second isotropic etching operation is performed directly on the metal seed material. Since the material in the top field region is thinner, i.e., there is less material, the top field metal material is completely removed before the bottom of the trench. This leaves only seed material at the bottom of the trench for bottom-up growth of metal fill. The method can achieve high wafer yields with fewer cycles. These methods address the challenges of seams and voids in conventional metal gapfill processes by removing metal from the field regions and sidewalls while retaining seed metal at the bottom of the gap or trench. In this way, a substantially seamless bottom-up metal gapfill can be performed.

[0066] While the foregoing is directed to embodiments of the present disclosure, other and further embodiments of the disclosure may be devised without departing from the basic scope thereof, and the scope of the same is determined by the claims that follow.

Claims

1. A method for filling a feature on a substrate, the method comprising the following steps: forming a metal seed layer on an exposed top surface of the substrate, wherein the substrate has a feature in the form of a trench or via formed in the top surface of the substrate, the feature having sidewalls and a bottom surface extending between the sidewalls; performing a gradient oxidation process to oxidize exposed portions of the metal seed layer to form a metal oxide, wherein the gradient oxidation process preferentially oxidizes a field region of the substrate above the bottom surface of the feature; performing an etch-back process to remove the oxidized portion of the seed layer; performing an isotropic etching process to remove a portion of the seed layer; and A metal gapfill process is performed to fill or partially fill the features with a gapfill material. 2 . The method of claim 1 , wherein the seed layer is a molybdenum-containing layer, the metal oxide is molybdenum oxide, and the metal gap-fill material contains molybdenum.

3. The method of claim 2, wherein an overhanging portion of the seed layer extends into an opening of one or more features formed along the field region of the substrate, and the overhanging portion is preferentially oxidized relative to the metal seed layer within the one or more features.

4. The method of claim 2, wherein the gradient oxidation process and the etch-back process are performed in two separate chambers.

5. The method according to claim 2, further comprising the steps of: A liner layer is formed on the top surface of the substrate, wherein the seed layer is formed on the liner layer and the liner layer extends into the feature. The method of claim 3 , wherein the etch-back process and the isotropic etching process are performed in the same chamber.

7. The method of claim 3, wherein the seed layer is removed from the field region and the overhanging portion.

8. A method of filling a feature formed on a substrate, the method comprising the steps of: A molybdenum-containing layer is deposited on the exposed top surface of the substrate, wherein the substrate comprising a plurality of features formed in the top surface of the substrate, Each of the plurality of features has a sidewall surface and a bottom surface, and The deposited molybdenum-containing layer is formed over the top surface of the substrate, and the sidewall surfaces and the bottom surfaces of the plurality of features; exposing the top surface of the substrate to a gradient oxidation process, wherein the gradient oxidation process forms an oxidized region of the molybdenum-containing layer; preferentially etching the oxidized regions of the deposited molybdenum-containing layer, wherein after preferentially etching the oxidized regions, a first portion of the deposited molybdenum-containing layer remains on the bottom surface and in the top surface surrounding each of the plurality of features; performing an isotropic etching process to remove the molybdenum-containing layer along the top surface while retaining the molybdenum-containing layer on the bottom surface in each of the plurality of features; and The features are filled with a second molybdenum layer, wherein the step of filling the features with the second molybdenum layer comprises the step of growing the second molybdenum layer from the first portion of the deposited molybdenum-containing layer on the bottom surface in each of the features.

9. The method of claim 8, wherein an overhanging portion of the molybdenum-containing layer extends into an opening of one or more features formed along the top surface of the substrate, and the overhanging portion is preferentially oxidized relative to the molybdenum-containing layer within the one or more features.

10. The method of claim 8, wherein the gradient oxidation process and the etch-back process are performed in two separate chambers.

11. The method of claim 8, further comprising the steps of: A liner layer is formed on the top surface of the substrate, wherein the molybdenum-containing layer is formed on the liner layer and the liner layer extends into the feature.

12. The method of claim 9, wherein the etch-back process and the isotropic etching process are performed in the same chamber.

13. The method of claim 12, wherein the molybdenum-containing layer is removed from the top surface and the overhanging portion.

14. A cluster tool for filling features on a substrate, the cluster tool comprising: The first processing chamber comprises: an oxygen source fluidly coupled to a processing region of the first processing chamber, wherein the oxygen source is configured to deliver an oxygen-containing gas to the processing region; a first flow control valve configured to control a flow rate of the oxygen-containing gas provided from the oxygen source to the processing region; a first inductively coupled plasma source configured to generate a plasma in the processing region, wherein the plasma comprises the oxygen-containing gas; and a second processing chamber comprising: a first etching gas source fluidly coupled to a processing region of the second processing chamber, wherein the first etching gas source is configured to deliver a first etching gas to the processing region; a second flow control valve, the second flow control valve being used to control the flow rate of the first etching gas provided from the first etching gas source to the processing area; a second etching gas source fluidly coupled to the processing region of the second processing chamber, wherein the second etching gas source is configured to deliver a second etching gas to the processing region; a third flow control valve, the third flow control valve being used to control the flow rate of the second etching gas provided from a second etching gas source to the processing area; and a second inductively coupled plasma source configured to generate a plasma in the processing region, wherein the plasma comprises the first or second etchant gas; and A controller, the controller being configured to: forming a metal seed layer on an exposed top surface of a substrate, wherein the substrate has a feature in the form of a trench or via formed in the top surface of the substrate, the feature having sidewalls and a bottom surface extending between the sidewalls, performing a gradient oxidation process to oxidize exposed portions of the metal seed layer to form a metal oxide, wherein the gradient oxidation process preferentially oxidizes a field region of the substrate above the bottom surface of the feature, performing an etch-back process to remove the oxidized portion of the seed layer; performing an isotropic etching process to remove portions of the seed layer; and A molybdenum gapfill process is performed to fill or partially fill the features with a gapfill material.

15. The cluster tool of claim 14, wherein the seed layer is a molybdenum-containing layer and the metal oxide is molybdenum oxide.

16. The cluster tool of claim 15, wherein an overhanging portion of the molybdenum-containing layer obstructs or blocks a top opening of one or more features formed along the field region of the substrate, and the overhanging portion is preferentially oxidized.

17. The cluster tool of claim 16, wherein the gradient oxidation process and the etch-back process are performed in two separate chambers.

18. The cluster tool of claim 17, wherein the controller is further configured to: A liner layer is formed on the exposed surface of the substrate, wherein the seed layer is formed on the liner layer and the liner layer extends into the feature.

19. The cluster tool of claim 18, wherein the first etch gas targets molybdenum oxide and the second etch gas targets molybdenum.

20. The cluster tool of claim 19, wherein the seed layer is removed from the field region and the overhanging portion.

Citation Information

Cited By

  • Semiconductor structure and manufacturing method thereof

    CN122476903A