Method for catalytically synthesizing bio-based furfuryl carbamate

Preparation of lead-nickel oxides through heterogeneous catalysts solves the problems of high resource consumption and high reaction temperature in traditional urethane synthesis, and achieves high efficiency and low temperature synthesis of bio-based furfuryamide methylformate with good catalysis Stability and environmental protection advantages.

CN119056460AInactive Publication Date: 2024-12-03LISHUI UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411185740.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-27
Publication Date
2024-12-03
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

In the prior art, the synthesis of carbamates mainly relies on organic amine compounds and homogeneous catalytic systems produced by traditional petrochemicals, resulting in high resource consumption, difficult catalyst recovery and separation, and high reaction temperature, which is not suitable for bio-based reactions. Substrate.

Method used

Using heterogeneous catalysts, the lead-nickel oxide catalyst is prepared by precipitating soluble lead salt and nickel salt with precipitant agent, and used to methoxycarbonylation reaction of bio-based furfuryamine and dimethyl carbonate to achieve carbamic acid Green synthesis of esters.

Benefits of technology

It has achieved efficient synthesis of bio-based furfurylamide formate at normal pressure and lower temperatures. The catalyst has good activity and stability, is easy to recover and separate, reduces its dependence on traditional fossil resources, and is in line with the green and sustainable development goals. .

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119056460A_ABST
    Figure CN119056460A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of organic chemical industry, in particular to a method for catalytically synthesizing bio-based furfuryl carbamate. According to the method, furfuryl amine is used as a raw material, dimethyl carbonate is used as a carbonylation reagent and a reaction solvent, a heterogeneous lead-nickel composite metal oxide is used as a catalyst, a methoxycarbonylation reaction is carried out, and the bio-based furfuryl carbamate is prepared. The preparation method of the heterogeneous catalyst comprises the following steps: adding soluble lead salt and soluble nickel salt into water to prepare a metal salt solution; meanwhile, adding the metal salt solution and a precipitant to carry out precipitation reaction, aging, drying the obtained solid precipitate, and calcining to obtain the heterogeneous catalyst. According to the method for catalytically synthesizing the bio-based furfuryl amino formate, the methoxycarbonylation reaction of furfuryl amine and DMC at normal pressure and lower temperature can be realized, the reaction conditions are mild, and the reaction process is green and environment-friendly.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of organic chemical industry, and in particular to a method for catalytically synthesizing bio-based furfuryl carbamate. Background Art

[0002] Carbamates are important intermediate compounds in the field of organic synthesis and fine chemicals, and are mainly used in the synthesis and manufacture of agricultural chemicals, medicines, dyes, etc. In addition, carbamates can be directly pyrolyzed into isocyanates, so they are also important raw materials for the synthesis of isocyanates. At present, the phosgene method is mainly used for the synthesis of isocyanates in industry. In contrast, the pyrolysis method of carbamates has significant advantages in environmental protection and safe production. Therefore, the efficient synthesis of carbamates is of great significance, especially for the non-phosgene synthesis of isocyanates. According to the type of carbonyl source, the synthesis method of carbamates mainly includes oxidative carbonylation of amines, reductive carbonylation of nitro compounds, methoxycarbonylation of amines, alcoholysis of urea, etc. Among them, the methoxycarbonylation of amines, that is, the reaction of organic amines with dimethyl carbonate (DMC), is considered to be one of the most promising green synthesis processes for carbamates because dimethyl carbonate is a non-toxic chemical derived from carbonic acid, and the reaction conditions are mild and the reaction process has high atomic economy.

[0003] Generally speaking, metal salts such as zinc, lead, sodium, potassium, sodium methoxide and ionic liquids have good catalytic performance in the reaction of organic amines with dimethyl carbonate. However, this type of homogeneous catalytic system brings challenges to catalyst recovery, product separation and environmental protection. Therefore, it is of great significance to develop efficient heterogeneous catalysts with simple preparation methods for the synthesis of carbamates. At present, a small number of heterogeneous catalysts with good catalytic performance in the synthesis of carbamates by dimethyl carbonate have been reported. For example, Li et al. prepared Al / SBA-15 catalyst for the reaction of 1,6-hexanediamine and DMC by isovolumetric impregnation method. However, the catalyst activity was low and it was necessary to react at 70°C for 35h. The HDC yield of dicarbamate reached 84.2% (Ind. Eng. Chem. Res. 2014, 53, 2, 626–634). Puértolas et al. prepared CeO by precipitation method. 2 Catalyst for the methoxycarbonylation of 2,4-diaminotoluene (2,4-TDA) with DMC. After 7.5 h at 140 °C, 83% dicarbamate can be obtained. However, CeO 2After repetition, both activity and selectivity decreased significantly (ACS Catal. 2019, 9, 7708-7720). Kang et al. synthesized mixed metal oxide catalysts such as Zn / Al / Ce and Zn / Al / Pb by coprecipitation method, which were used for the methoxycarbonylation reaction of aniline and DMC. After reacting at 200°C for 7 hours, the yields of methyl phenylcarbamate (MPC) reached 78.2% and 94.0%, respectively, and the activity and selectivity of the catalyst did not decrease significantly after repeated use. Unfortunately, the reaction temperature required for this catalytic system is too high, and the catalytic effect is not ideal for reaction substrates that are unstable at high temperatures (RSCAdv., 2019, 9, 42474–42480; ACS Omega 20205(35), 22529-22535).

[0004] Based on the existing research reports on the synthesis of carbamates by dimethyl carbonate, the method currently generally uses organic amine compounds produced by traditional petrochemical industry and the reaction process mostly adopts a homogeneous catalytic system. Using expensive and non-renewable petroleum-based amines as raw materials and using homogeneous catalytic systems that are difficult to recycle and separate will greatly restrict the development of the carbamate industry and its related industries. However, there are no reports on the synthesis of carbamates using bio-based amine compounds as raw materials and heterogeneous catalytic systems with good catalytic performance for the methoxycarbonylation reaction of bio-based amine compounds. Furfurylamine is a bio-based primary amine obtained by reductive amination of furfural, the only biomass platform molecule currently produced on a large scale industrially. It is a good petrochemical raw material substitute for the synthesis of carbamates by dimethyl carbonate. The development of heterogeneous catalysts with good catalytic performance and stability for the reaction of bio-based furfurylamine with DMC to synthesize carbamates has significant economic benefits and environmental advantages. It is a process route that meets the national "dual carbon" strategic goals and is of great significance to the green and sustainable development of the carbamate industry and its related industries. Summary of the invention

[0005] Based on the above content, the present invention provides a method for catalytically synthesizing bio-based furfuryl carbamate. In the present invention, methyl carbamate is generated by reacting bio-based primary amine with dimethyl carbonate under the action of a heterogeneous catalyst. The raw materials of the process are cheap and easy to obtain, the reaction process is green and environmentally friendly, the catalyst preparation method is simple, and the catalyst has excellent reusability.

[0006] To achieve the above object, the present invention provides the following solutions:

[0007] One of the technical solutions of the present invention is a method for preparing a heterogeneous catalyst, comprising the following steps:

[0008] Adding soluble lead salt and soluble nickel salt into water to prepare a metal salt solution;

[0009] The metal salt solution and the precipitant are added at the same time to carry out precipitation reaction, and then aged. The obtained solid precipitate is dried and then calcined to obtain the heterogeneous catalyst.

[0010] The second technical solution of the present invention is a heterogeneous catalyst prepared by the above-mentioned preparation method.

[0011] The third technical solution of the present invention is the use of the above-mentioned heterogeneous catalyst in the catalytic synthesis of bio-based furfurylaminocarbamate.

[0012] A fourth technical solution of the present invention is a method for catalytically synthesizing bio-based furfural carbamate, which uses furfural amine as a raw material, dimethyl carbonate as a carbonylation reagent and a reaction solvent, and the above-mentioned heterogeneous catalyst as a catalyst to carry out a methoxycarbonylation reaction to obtain bio-based furfural carbamate.

[0013] The present invention discloses the following technical effects:

[0014] The heterogeneous catalyst (lead nickel oxide catalyst) of the present invention has good catalytic reaction activity and excellent catalytic stability, low catalyst cost, easy separation from the product and convenient recovery and application.

[0015] The present invention provides a new green catalytic synthesis method of bio-based carbamate. The present invention uses biomass-based furfural amine as a raw material, opens up the raw material source of carbamate and related downstream industries, and reduces the dependence on traditional fossil resources.

[0016] The method for catalytically synthesizing bio-based furfuryl carbamate of the present invention can realize the methoxycarbonylation reaction of furfurylamine and DMC at normal pressure and relatively low temperature, with mild reaction conditions and green and environmentally friendly reaction process. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0018] Figure 1 This is the MS chart of bio-based furfurylaminocarbamate prepared in Example 1 of the present invention.

[0019] Figure 2 The XRD spectra of NiO, PbO and lead-nickel composite oxide catalyst (PbO-NiO, lead:nickel molar ratio is 0.1) in the examples and comparative examples of the present invention are shown. DETAILED DESCRIPTION

[0020] Various exemplary embodiments of the present invention will now be described in detail. This detailed description should not be considered as limiting the present invention, but should be understood as a more detailed description of certain aspects, features, and embodiments of the present invention.

[0021] It should be understood that the terms described in the present invention are only for describing a particular embodiment and are not intended to limit the present invention. In addition, for the numerical range in the present invention, it should be understood that each intermediate value between the upper and lower limits of the scope is also specifically disclosed. The intermediate value in any stated value or stated range, and each smaller range between any other stated value or intermediate value in the described range is also included in the present invention. The upper and lower limits of these smaller ranges can be independently included or excluded in the scope.

[0022] Unless otherwise indicated, all technical and scientific terms used herein have the same meanings as those generally understood by those skilled in the art. Although the present invention describes only preferred methods and materials, any methods and materials similar or equivalent to those described herein may also be used in the implementation or testing of the present invention. All documents mentioned in this specification are incorporated by reference to disclose and describe the methods and / or materials associated with the documents. In the event of a conflict with any incorporated document, the content of this specification shall prevail.

[0023] It will be apparent to those skilled in the art that various modifications and variations may be made to the specific embodiments of the present invention description without departing from the scope or spirit of the present invention. Other embodiments derived from the present invention description will be apparent to the skilled artisan. The present invention description and examples are exemplary only.

[0024] The words “include,” “including,” “have,” “contain,” etc. used in this document are open-ended terms, meaning including but not limited to.

[0025] The first aspect of the present invention provides a method for preparing a heterogeneous catalyst, comprising the following steps:

[0026] Adding soluble lead salt and soluble nickel salt into water to prepare a metal salt solution;

[0027] The metal salt solution and the precipitant are added at the same time to carry out precipitation reaction, and then aged. The obtained solid precipitate is dried and then calcined to obtain the heterogeneous catalyst.

[0028] The method of the present invention is to load lead oxide onto nickel oxide in a chemical bond manner to prepare a heterogeneous catalyst, so the heterogeneous catalyst exhibits excellent catalytic stability after multiple cycles of use, and has no tendency of activity reduction.

[0029] In some embodiments of the present invention, the molar ratio of lead to nickel in the metal salt solution is 0.05 to 10:1; and the concentration of the metal salt solution is 0.1 to 2 mol / L.

[0030] In the present invention, the molar ratio of lead to nickel is limited to the above parameter range to ensure a high conversion rate and selectivity of the target product carbamate. Too low or too high a lead content will lead to a decrease in product yield. In addition, since lead is a toxic heavy metal, a lower lead-nickel ratio is preferably used in practical applications.

[0031] In some embodiments of the present invention, the soluble lead salt is lead nitrate and / or lead acetate; the soluble nickel salt is at least one of nickel nitrate, nickel acetate or nickel chloride. Further preferably, the soluble lead salt is lead acetate; the soluble nickel salt is nickel acetate.

[0032] In some embodiments of the present invention, the precipitant is prepared by adding sodium hydroxide and sodium carbonate into water; the concentration of the precipitant is 0.1 to 2 mol / L; and the molar ratio of the sodium hydroxide to the sodium carbonate is 1 to 10:1.

[0033] In some embodiments of the present invention, the pH of the precipitation reaction is 4 to 12;

[0034] In the present invention, within the above-mentioned precipitation reaction pH range, the lead and nickel ions are precipitated more completely, and the formed precipitate is more stable. If the pH of the precipitation reaction is too high or too low, the lead / nickel ion precipitation will be incomplete, thereby affecting the lead-nickel molar ratio in the prepared catalyst, and further resulting in poor catalytic performance.

[0035] In the present invention, the adding method is dropwise addition.

[0036] The pH value of the precipitation reaction is controlled to be constant by controlling the dropping speed of the metal solution and the precipitant.

[0037] During the catalyst preparation process, the pH value of the precipitation reaction solution is maintained at 4-12 until the metal salt solution is completely precipitated.

[0038] The aging temperature is 20-100°C and the time is 1-24 hours. After the aging is completed, the steps of filtering and washing to neutrality are also included.

[0039] On the one hand, the aging process completes the precipitation reaction and forms a stable and uniform precipitate. At the same time, during this period, the precipitate undergoes processes such as grain growth, improvement, and particle enlargement.

[0040] The aging temperature and time are limited to the above parameter ranges mainly to ensure that the precipitation reaction is complete and the formed precipitate grains are uniform and stable, while at the same time, the impurities adsorbed on the crystal surface are transferred into the solution.

[0041] In some embodiments of the present invention, the drying temperature is 80-120°C for 8-24 hours, the calcination temperature is 300-800°C for 2-6 hours, and the step of grinding the dried solid precipitate is also included before calcination.

[0042] The drying process removes most of the free water in the precipitate to form stable precipitated crystals. Too high a temperature will cause the crystals to further lose some of their crystalline water, affecting the pore structure, specific surface area and other properties of the catalyst precursor. If the drying step is omitted and the catalyst is directly calcined at high temperature, splashing may occur due to the high water content. On the other hand, it will also affect the process of the precipitated crystals turning into catalysts, resulting in different catalyst surface properties and stability differences.

[0043] The calcination process causes the precipitated crystals containing crystal water to form the corresponding metal / composite metal oxides through thermal decomposition. The decomposition may be incomplete at a lower calcination temperature, while too high a temperature may affect the physical (pores, specific surface area) and chemical (surface acidity and alkalinity) properties of the catalyst surface. Therefore, the present invention limits the calcination temperature to the above parameter range.

[0044] The present invention adopts a constant pH coprecipitation method to prepare a heterogeneous catalyst, and the heterogeneous catalyst can be a single-component metal oxide or a composite oxide; in some specific embodiments of the present invention, the preparation method of the heterogeneous catalyst comprises the following steps:

[0045] (1) Dissolve a soluble metal salt in deionized water in a certain proportion to prepare a metal salt solution with a total concentration of 0.1 to 2 mol / L, wherein the metal ion in the metal salt solution is Zr 4+ 、Ce 4+ , Nb 5+ 、Ni 2+ 、Al 3+ , Cu 2+ 、Co 2+ 、Ti 2+ , Pb 2+ Mg 2+ , Mn 2+ 、Zn 2+ One or more of the following: dissolving sodium hydroxide and sodium carbonate in deionized water in a certain ratio to prepare a precipitant with a total concentration of 0.1 to 2 mol / L;

[0046] (2) at room temperature, dropwise adding a metal salt solution and a precipitant simultaneously under vigorous stirring to carry out a precipitation reaction, determining the pH required for the co-precipitation according to the selected metal type, and controlling the precipitation reaction pH value to be constant by the dropwise addition speed of the metal solution and the precipitant;

[0047] (3) After the precipitation reaction is completed, the obtained suspension is aged at 20-100° C. for 1-24 h, filtered, and washed until neutral. The obtained solid precipitate is dried at 80-120° C. for 8-24 h. After the solid is fully ground, it is calcined at 300-800° C. for 2-6 h to prepare the heterogeneous catalyst.

[0048] In the catalyst preparation process, the soluble metal salt is at least one of nitrate, acetate or metal chloride.

[0049] The single-component metal oxide or composite oxide includes ZrO 2 、CeO 2 , Nb 2 O 5 、NiO、Al 2 O 3 ,CuO,Co 3 O 4 、TiO 2 , one or more composite oxides of PbO, MgO, MnO, ZnO, and NiO.

[0050] The second aspect of the present invention provides a heterogeneous catalyst prepared by the above-mentioned preparation method.

[0051] The third aspect of the present invention provides a use of the above-mentioned heterogeneous catalyst in the catalytic synthesis of bio-based furfurylcarbamate.

[0052] The fourth aspect of the present invention provides a method for catalytically synthesizing bio-based furfural carbamate, using furfural amine as a raw material, dimethyl carbonate as a carbonylation reagent and a reaction solvent, and carrying out a methoxycarbonylation reaction under the action of the above-mentioned heterogeneous catalyst to obtain bio-based furfural carbamate.

[0053] The present invention utilizes a heterogeneous catalyst (lead-nickel composite oxide) to catalyze the reaction of furfurylamine and dimethyl carbonate to prepare furfurylamine methyl formate. The reaction formula is as follows:

[0054]

[0055] In some embodiments of the present invention, the temperature of the methoxycarbonylation reaction is 90-170° C., and the time is 2-15 hours. More preferably, the temperature of the methoxycarbonylation reaction is 110-150° C., and the time is 4-11 hours.

[0056] In some embodiments of the present invention, the molar ratio of the furfurylamine to the dimethyl carbonate is 1:8-24; and the added amount of the catalyst is 1-10 wt % of the total mass of the furfurylamine and the dimethyl carbonate.

[0057] The present invention discloses a method for catalytic synthesis of bio-based carbamates and a method for preparing an efficient and stable heterogeneous catalyst used in the reaction process thereof. The bio-based carbamate is methyl furfurylamine, which uses bio-based furfurylamine derived from biomass platform molecule furfural as raw material, and undergoes methoxycarbonylation reaction with dimethyl carbonate under the action of a single-component metal oxide or a composite metal oxide catalyst to generate methyl furfurylamine. The single-component metal oxide or composite metal oxide catalyst used in the methoxycarbonylation reaction in the specific embodiment of the present invention is prepared by a constant pH coprecipitation method, and the catalyst can achieve a good bio-based primary amine conversion rate and a high selectivity of carbamate under mild reaction conditions, avoiding the problem of humins easily produced by high-temperature polymerization of bio-based molecules, and also has excellent reusability.

[0058] The present invention is further described below in conjunction with specific embodiments, but the protection scope of the present invention is not limited thereto.

[0059] Example 1

[0060] A mixed metal salt solution of lead acetate and nickel acetate (the concentration of the metal salt solution is 0.1 mol / L) is prepared according to the molar ratio of lead to nickel of 0.05:1. The metal salt solution and the precipitant prepared by sodium hydroxide and sodium bicarbonate (the molar ratio of sodium hydroxide to sodium bicarbonate is 5:1, the solvent of the precipitant is water, and the concentration of the precipitant is 0.1 mol / L) are added dropwise to a beaker under vigorous stirring. The pH value of the reaction solution is controlled at about 10.5 by adjusting the dropping speed of the metal salt solution and the precipitant. The obtained suspension is placed in an oven for aging at 70°C for 12 hours, filtered, and the filter cake is washed with distilled water until neutral and placed in an oven for drying at 100°C for 12 hours. After grinding, it is calcined at 500°C in a muffle furnace for 3 hours to obtain a lead-nickel composite oxide catalyst (i.e., a heterogeneous catalyst, referred to as: catalyst). 0.06g of catalyst, 1mmol of furfurylamine and 8mmol of dimethyl carbonate are added to a high-pressure stirred autoclave, sealed and N 2 The mixture was purged and reacted at 120°C for 5 hours. The product was analyzed by GC, and the conversion rate of furfurylamine was 96.79%, and the yield of carbamate was 66.0%.

[0061] Embodiments 2 to 5

[0062] The catalyst preparation and catalytic reaction are the same as those in Example 1, except that the molar ratios of lead to nickel in the lead acetate and nickel acetate mixed metal salt solutions of Examples 2 to 5 are 0.1:1, 0.2:1, 0.5:1, and 1:1, respectively. After GC analysis, the furfurylamine conversion rates of the obtained products were 98.11%, 95.54%, 84.47%, and 85.47%, respectively, and the carbamate yields were 66.54%, 64.09%, 63.68%, and 63.44%, respectively.

[0063] Example 6

[0064] A mixed metal salt solution of lead acetate and nickel acetate was prepared in a ratio of 0.1:1 between lead and nickel (the concentration of the metal salt solution was 0.1 mol / L). The metal salt solution and a precipitant prepared from sodium hydroxide and sodium bicarbonate (the molar ratio of sodium hydroxide to sodium bicarbonate was 5:1, the solvent of the precipitant was water, and the concentration of the precipitant was 0.1 mol / L) were added dropwise to a beaker under vigorous stirring. The pH value of the reaction solution was controlled at about 10.5 by adjusting the dropping speed of the metal salt solution and the precipitant. The obtained suspension was placed in an oven for aging at 70°C for 12 hours, filtered, and the filter cake was washed with distilled water until neutral and placed in an oven for drying at 100°C for 12 hours. After grinding, it was calcined in a muffle furnace at 500°C for 3 hours to obtain a lead-nickel composite oxide catalyst. 0.06 g of catalyst, 1 mmol of furfurylamine and 8 mmol of dimethyl carbonate were added to a high-pressure stirred autoclave, sealed and N 2 The mixture was purged and reacted at 110°C for 7 hours. The product was analyzed by GC, and the furfuryl amination rate was 84.68%, and the yield of carbamate was 47.66%.

[0065] The experimental operation in Examples 7 to 10 is the same as that in Example 6, except that the reaction temperatures for catalytic synthesis of bio-based furfuryl carbamate in Examples 7 to 10 are 120° C., 130° C., 140° C., and 150° C., respectively. The GC analysis of the obtained products showed that the furfurylamine conversion rates were 96.73%, 99.18%, 96.91%, and 96.72%, respectively, and the yields of carbamate were 69.69%, 75.28%, 62.92%, and 52.9%, respectively.

[0066] Embodiment 11

[0067] A mixed metal salt solution of lead acetate and nickel acetate was prepared in a ratio of 0.1:1 between lead and nickel (the concentration of the metal salt solution was 0.1 mol / L). The metal salt solution and a precipitant prepared from sodium hydroxide and sodium bicarbonate (the molar ratio of sodium hydroxide to sodium bicarbonate was 5:1, the solvent of the precipitant was water, and the concentration of the precipitant was 0.1 mol / L) were added dropwise to a beaker under vigorous stirring. The pH value of the reaction solution was controlled at about 10.5 by adjusting the dropping speed of the metal salt solution and the precipitant. The obtained suspension was placed in an oven for aging at 70°C for 12 hours, filtered, and the filter cake was washed with distilled water until neutral and placed in an oven for drying at 100°C for 12 hours. After grinding, it was calcined in a muffle furnace at 500°C for 3 hours to obtain a lead-nickel composite oxide catalyst. 0.06 g of catalyst, 1 mmol of furfurylamine and 8 mmol of dimethyl carbonate were added to a high-pressure stirred autoclave, sealed and N 2 The mixture was purged and reacted at 130° C. for 5 h. The product was analyzed by GC, and the conversion rate of furfurylamine was 89.11%, and the yield of carbamate was 65.83%.

[0068] The operations in Examples 12 to 17 are the same as those in Example 11, except that the reaction times in Examples 12 to 17 are 6 h, 7 h, 8 h, 9 h, 10 h, and 11 h, respectively. The conversion rates of furfurylamine analyzed by GC were 98.53%, 99.18%, 98.89%, 98.92%, 91.18%, and 89.55%, respectively, and the yields of carbamate were 72.26%, 75.28%, 74.13%, 74.84%, 75.28%, and 73.52%, respectively.

[0069] Embodiment 18

[0070] A mixed metal salt solution of lead acetate and nickel acetate was prepared in a ratio of 0.1:1 between lead and nickel (the concentration of the metal salt solution was 0.1 mol / L). The metal salt solution and a precipitant prepared from sodium hydroxide and sodium bicarbonate (the molar ratio of sodium hydroxide to sodium bicarbonate was 5:1, the solvent of the precipitant was water, and the concentration of the precipitant was 0.1 mol / L) were added dropwise to a beaker under vigorous stirring. The pH value of the reaction solution was controlled at about 10.5 by adjusting the dropping speed of the metal salt solution and the precipitant. The obtained suspension was placed in an oven for aging at 70°C for 12 hours, filtered, and the filter cake was washed with distilled water until neutral and placed in an oven for drying at 100°C for 12 hours. After grinding, it was calcined in a muffle furnace at 500°C for 3 hours to obtain a lead-nickel composite oxide catalyst. 0.06 g of catalyst, 1 mmol of furfurylamine and 8 mmol of dimethyl carbonate were added to a high-pressure stirred autoclave, sealed and N 2 The mixture was purged and reacted at 130° C. for 7 h. The product was analyzed by GC, and the conversion rate of furfurylamine was 99.20%, and the yield of carbamate was 75.28%.

[0071] The operations in Examples 19 to 22 are the same as those in Example 18, except that the molar ratios of furfurylamine to dimethyl carbonate in Examples 19 to 22 are 1:12, 1:16, 1:20, and 1:24, respectively (the amount of furfurylamine added is fixed at 1 mmol). The furfurylamine conversion rates of the obtained products were 98.96%, 98.19%, 97.85%, and 96.96%, respectively, and the yields of carbamate were 76.02%, 77.15%, 76.98%, and 76.79%, respectively.

[0072] Embodiment 23

[0073] A mixed metal salt solution of lead acetate and nickel acetate was prepared in a ratio of 0.1:1 between lead and nickel (the concentration of the metal salt solution was 0.1 mol / L). The metal salt solution and a precipitant prepared from sodium hydroxide and sodium bicarbonate (the molar ratio of sodium hydroxide to sodium bicarbonate was 5:1, the solvent of the precipitant was water, and the concentration of the precipitant was 0.1 mol / L) were added dropwise to a beaker under vigorous stirring. The pH value of the reaction solution was controlled at about 10.5 by adjusting the dropping speed of the metal salt solution and the precipitant. The obtained suspension was placed in an oven for aging at 70°C for 12 hours, filtered, and the filter cake was washed with distilled water until neutral and placed in an oven for drying at 100°C for 12 hours. After grinding, it was calcined at 500°C in a muffle furnace for 3 hours to obtain a lead-nickel composite oxide catalyst. 0.06 g of catalyst, 1 mmol of furfurylamine and 16 mmol of dimethyl carbonate were added to a high-pressure stirred autoclave, sealed and N 2 The mixture was purged and reacted at 130° C. for 7 h. The product was analyzed by GC, and the conversion rate of furfurylamine was 99.74%, and the yield of carbamate was 77.39%.

[0074] The experimental operation of Examples 24 to 27 is the same as that of Example 23, except that the catalyst used is the catalyst recovered after the catalytic synthesis of bio-based furfuryl carbamate in Example 23. After the catalyst is used, it is centrifuged, washed several times with ethanol solution, dried in an oven, and collected for use. After the catalyst is repeatedly used for the second, third, fourth, and fifth times, the obtained products have a furfurylamine conversion rate of 99.97%, 99.88%, 99.93%, and 99.91%, respectively, and the carbamate yields are 78.75%, 80.70%, 80.91%, and 81.06%, respectively. With the repeated use of the catalyst, the furfurylamine conversion rate and the carbamate yield gradually increase. The analysis may be that the surface acidity and alkalinity of the catalyst change to a certain extent after repeated use, resulting in a slight decrease in the amount of by-products generated, thus resulting in a slight increase in product selectivity.

[0075] It can be seen from the repeated application experiments of Examples 23 to 27 that the lead-nickel composite oxide catalyst has almost no change in activity and yield of methyl furfuralcarbamate after being repeatedly used five times in the methoxycarbonylation reaction of furfuralamine and dimethyl carbonate (catalytic synthesis of bio-based furfuralcarbamate), showing strong stability.

[0076] Comparative Examples 1 to 18

[0077] The catalytic reaction conditions were the same as those in Example 1, except that the heterogeneous catalysts prepared in Example 1 were replaced by ZrO 2 、CeO 2 , Nb 2 O 5 、NiO、Al 2 O 3 ,CuO,Co3 O 4 、TiO 2 , PbO, MgO, MnO, ZnO, PbNiAlO x 、PbCuO x 、PbCuAlO x 、PbZnO x 、CuZrAlO x 、PbZrAlO x (The preparation method of each catalyst in the comparative example is the same as the preparation method of the catalyst in Example 1, the only difference is that lead acetate and nickel acetate are replaced by the corresponding metal salts in each comparative example; the value range of x in each catalyst in the comparative example is 1 to 5) The experimental results are listed in Table 1 below.

[0078] Table 1

[0079]

[0080]

[0081] By comparing the embodiments of the present invention with the comparative examples, it can be seen that in the process of synthesizing furfurylamine methyl formate by reacting furfurylamine with dimethyl carbonate, the lead-nickel composite metal oxide exhibits higher activity than single-component lead, nickel and other metal oxides, and the synergistic effect of lead and nickel oxides significantly enhances the activity of the methoxycarbonylation reaction.

[0082] Comparative Example 19

[0083] 2 g of PbO and 1 g of NiO were added together with 100 ml of dimethyl carbonate into a 200 ml hydrothermal autoclave, and treated in an oil bath at 190° C. for 10 h. The autoclave was naturally cooled to room temperature, and the solid was filtered after opening the autoclave, washed with dimethyl carbonate, and dried at 60° C. to obtain a heterogeneous catalyst; 0.06 g of the heterogeneous catalyst prepared above, 1 mmol of furfurylamine and 8 mmol of dimethyl carbonate were added into a high-pressure stirred autoclave, and the autoclave was sealed and N 2 The mixture was purged and reacted at 120°C for 5 hours. The product was analyzed by GC, and the conversion rate of furfurylamine was 15.56%, and the yield of carbamate was 6.42%.

[0084] Figure 1 This is the MS graph of bio-based furfurylaminocarbamate prepared in Example 1 of the present invention. The characteristics of the mass spectrum are completely consistent with the structural characteristics of furfurylaminocarbamate.

[0085] Figure 2 The XRD patterns of NiO, PbO and lead-nickel composite oxide catalyst (PbO-NiO, lead-nickel molar ratio is 0.1) in the examples and comparative examples of the present invention are shown in FIG. Figure 2It can be seen that the catalyst prepared by the present invention is a composite component of lead oxide and nickel oxide obtained by precipitating metal ions, and lead is uniformly dispersed on NiO in the form of PbO, rather than a simple physical mixture of NiO-PbO.

[0086] In summary, the lead-nickel composite oxide catalyst in the present invention is a composite oxide formed of lead and nickel, and the synergistic effect of the two components is used to improve the catalytic performance.

[0087] The embodiments described above are only descriptions of the preferred modes of the present invention, and are not intended to limit the scope of the present invention. Without departing from the design spirit of the present invention, various modifications and improvements made to the technical solutions of the present invention by ordinary technicians in this field should all fall within the protection scope determined by the claims of the present invention.

Claims

1. A method for preparing a heterogeneous catalyst, characterized in that: The following steps are involved: Adding soluble lead salt and soluble nickel salt into water to prepare a metal salt solution; The metal salt solution and the precipitant are added at the same time to carry out precipitation reaction, and then aged. The obtained solid precipitate is dried and then calcined to obtain the heterogeneous catalyst.

2. The method for preparing a heterogeneous catalyst according to claim 1, characterized in that: The molar ratio of lead to nickel in the metal salt solution is 0.05-10:1; the concentration of the metal salt solution is 0.1-2 mol / L.

3. The method for preparing a heterogeneous catalyst according to claim 1, characterized in that: The precipitant is prepared by adding sodium hydroxide and sodium carbonate into water; the concentration of the precipitant is 0.1-2 mol / L; and the molar ratio of the sodium hydroxide to the sodium carbonate is 1-10:

1.

4. The method for preparing a heterogeneous catalyst according to claim 1, characterized in that: The pH of the precipitation reaction is 4 to 12; The aging temperature is 20-100° C. and the aging time is 1-24 hours.

5. The method for preparing a heterogeneous catalyst according to claim 1, characterized in that: The drying temperature is 80-120° C., and the time is 8-24 hours; the calcination temperature is 300-800° C., and the time is 2-6 hours.

6. A heterogeneous catalyst prepared by the preparation method according to any one of claims 1 to 5.

7. Use of the heterogeneous catalyst as claimed in claim 6 in the catalytic synthesis of bio-based furfurylcarbamate.

8. A method for catalytic synthesis of bio-based furfuryl carbamate, characterized in that: Using furfurylamine as a raw material, dimethyl carbonate as a carbonylation reagent and a reaction solvent, and the heterogeneous catalyst according to claim 6 as a catalyst, a methoxycarbonylation reaction is carried out to prepare bio-based furfurylamine formate.

9. The method for catalytic synthesis of bio-based furfuryl carbamate according to claim 8, characterized in that: The temperature of the methoxycarbonylation reaction is 90-170° C. and the time is 2-15 hours.

10. The method for catalytic synthesis of bio-based furfuryl carbamate according to claim 8, characterized in that: The molar ratio of the furfurylamine to the dimethyl carbonate is 1:8-24; and the added amount of the catalyst is 1-10 wt % of the total mass of the furfurylamine and the dimethyl carbonate.