Low-accident-rate steel billet continuous casting casting method and device, medium and equipment
Patent Information
- Application Number
- CN202411201926.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-29
- Publication Date
- 2024-12-03
AI Technical Summary
During the continuous casting and pouring of existing steel billets, there are high accident rates, high training costs, unstable operation, inconsistent operation, and unification of production. The existing automatic pouring system has radiation problems, high maintenance costs and poor control stability.
The pouring process is divided into three stages, setting the casting speed and time of the steel casting, and automatic control is achieved through computer programs to ensure the slow rise and stability of the liquid level, and combining with the existing automatic casting system to improve the success rate.
A low accident rate pouring process was achieved, with a success rate of 99%, reducing production and equipment damage losses, simplifying operations, reducing training costs, and improving the molten steel collection rate and pouring success rate.
Smart Images

Figure CN119057032A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of steelmaking, and in particular to a method for continuous casting of steel billets with a low accident rate and a device, medium and equipment thereof. Background Art
[0002] The continuous casting process is the process of continuously injecting molten steel into a crystallizer to form the structural steel billet required by the steel rolling mill.
[0003] Start pouring: cold material is loaded into the crystallizer ( Figure 1 a), the molten steel is injected into the crystallizer, and the molten steel rapidly cools and solidifies to form a billet head after encountering the cold material ( Figure 1 b), the molten steel gradually rises to form a billet shell, and the dummy rod pulls the billet out of the crystallizer to form a billet under the action of the straightening machine.
[0004] At present, most of the continuous casting billet pouring in China is mainly done manually, and the pouring worker starts the continuous casting according to the size of the steel flow, the liquid level, and the casting speed. The manual operation has the following defects:
[0005] 1. The process of continuous casting start-up is learned by experienced steel casters in the process of master teaching, helping and guiding. The training time of steel casters is long, the operation accident rate is high during the training process, and the success rate of steel casting during the training period is low. Continuous casting production is a continuous production mode. Once the start-up failure occurs, it will affect the smooth operation of the converter blowing process. It takes at least 2 to 3 years to train a good steel caster from scratch to be able to start casting smoothly. There are many accident losses during the training process, and the cost of personnel training is high;
[0006] 2. The pouring process cannot be unified. The pouring process is operated according to personal habits. The operating habits need to match the crystallizer. After replacing the crystallizer, it is easy to cause accidents such as steel leakage and steel overflow during the initial pouring;
[0007] 3. The operation time of the initial pouring process is long, and the water inlet can only be opened after the pouring liquid surface is stable, resulting in too long waste billet head, wasting molten steel and increasing the cost of pouring;
[0008] 4. After the failure of continuous casting, the economic loss is large, the processing time is long, and it has a significant impact on safety, equipment, production plan, etc. The failure of continuous casting single stream and single pouring will also cause molten steel loss, increased refractory cost, equipment burnout, single stream, etc. The loss of a single pouring failure is close to 500 yuan. The number of production times per month is 96 to 120 times. After multiple failures, the loss is huge after the loss is superimposed. One leakage will lose 2 to 5 tons of molten steel, and the leaked molten steel will become scrap steel. The price difference between scrap steel and qualified billet is 850 yuan. Calculation: 850*2=1700 yuan. The production process uses 85 yuan of nozzles, 320 yuan of casings, asbestos cloth fillers, ingot guide rods, cold materials, etc. The production cost is nearly 1,000 yuan. After the leakage, the spray equipment of the secondary cooling system will be damaged, and the nozzles, spray pipes, guide rollers and other equipment will be damaged, increasing the cost.
[0009] 5. During the manual pouring operation, personnel need to operate at close range, which is very dangerous and can easily cause serious safety accidents;
[0010] The automatic billet pouring system automates the pouring process, reduces pouring accidents and improves the success rate of pouring. The main manufacturers of current products on the market are Radium Molybdenum Corporation and Haineng Corporation. The working principle is: using a cesium source to illuminate the depth of the environment inside the crystallizer and track the changes in the height of the molten steel level in the crystallizer, and realizing automatic pouring by controlling the molten steel flow rate according to the changes in the molten steel level.
[0011] The existing automatic billet pouring system has problems: increasing the amount of cesium source (increasing the radiation), and the need to establish an independent PLC control system, which requires a large capital investment and high maintenance costs; in actual production and use, it needs to be debugged according to the specific pouring equipment. After debugging, the equipment is difficult to adapt to different molten steel flows, resulting in poor stability in molten steel flow rate control, and the inability to control the rising speed of the molten steel level in the crystallizer, affecting the low success rate of pouring. In addition, the existing automatic billet pouring system is particularly unable to accurately control the flow rate and injection volume of molten steel during the initial pouring process, which seriously affects the normal subsequent molten steel injection.
[0012] The information disclosed in the background technology section is only intended to enhance the understanding of the overall background of the invention and should not be regarded as an admission or any form of suggestion that the information constitutes the prior art already known to a person skilled in the art. Summary of the invention
[0013] In view of the above-mentioned technical problems, the present application provides a method for continuous casting of steel billets with a low accident rate and its device, medium, and equipment. The method can realize the pouring process and complete the control of the time and pulling speed of the four stages: billet head formation, billet demolding, billet liquid level lifting, and crystallizer liquid level stabilization. Each stage of the pouring process runs according to the set time and pulling speed, thereby controlling the molten steel level to rise slowly, achieving the control of a stable liquid level and realizing automatic pouring.
[0014] The present application provides a method for continuous casting of steel billets with a low accident rate, comprising the following steps:
[0015] Step S1: After the cold material is loaded in the crystallizer, molten steel is injected into the copper tube cavity of the crystallizer until the cold material is submerged and a billet head is formed in the crystallizer, which is the first stage of molten steel pouring; the molten steel drawing speed in the first stage is V1, and the casting time is T1; the molten steel drawing speed is the liquid level rising speed of the molten steel in the crystallizer;
[0016] Step S2: After the vibration billet head is demoulded from the end of the first stage, molten steel is continuously poured into the copper tube of the crystallizer, and the pouring time T2 is set at the molten steel drawing speed V2 to complete the second stage;
[0017] Step S3: From the end of the second stage, continue to cast molten steel into the copper tube of the crystallizer at the set molten steel pulling speed V3 for time T3, until the molten steel level in the crystallizer stabilizes at 55-65% of the total volume of the copper tube of the crystallizer, completing the third stage, and then transfer to the second casting system to continue the subsequent molten steel casting operation.
[0018] Preferably, when the first stage is completed, the liquid level in the crystallizer satisfies H1: H1 = [D1 + D2 + L2*0.7 + V1*1000 / 60*T1] - V 1*T 1;
[0019] Wherein: D1 is the depth of the ingot inserting into the crystallizer (mm); D2 is the thickness of the gap filler between the outer wall of the ingot head and the inner cavity of the copper tube (mm); L2 is the length of the cold material (mm); V1 is the set first-stage molten steel pulling speed (m / min); T1 is the set first-stage casting time (s); V1 is set to 0.3-0.5m / min; T1 is set to 2-10s.
[0020] Preferably, the liquid level in the crystallizer is
[0021] H2=[H1+V2*1000 / 60*T2]-V2*T2;
[0022] Among them, H1 is the liquid level height in the crystallizer after the first stage is completed (mm); V2 is the molten steel pulling speed set in the second stage (m / min); T2 is the set duration of molten steel casting in the second stage (s); V2 is set to 0.5-1.5 m / min; T2 is set to 8-20s.
[0023] Preferably, the liquid level H3 when the third stage is completed is:
[0024] H3=[H2+V3*1000 / 60*T3)]-V3*T3; T3 is the setting time of casting molten steel in the third stage in s; V3 is the setting speed of molten steel in the third stage in m / min; V3 is 1.5~1.9m / min; T3 is 10~20s; and 650mm <H3<710mm。
[0025] Preferably, the V3 set in the third stage satisfies: V3<V water inlet-0.2m / min; the T3 set satisfies T3<V water inlet corresponding to the emergence time;
[0026] Preferably, the demoulding time of the vibrating blank head is set to 3 to 5 seconds.
[0027] Preferably, when the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 14.5mm, the V nozzle is 1.6 meters / minute; when the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 15mm, the V nozzle is 1.9 meters / minute; when the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 15.5mm, the V nozzle is 2.1 meters / minute; when the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 16mm, the V nozzle is 2.3 meters / minute; when the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 16.5mm, the V nozzle is 2.4 meters / minute; when the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 17mm, the V nozzle is 2.5 meters / minute;
[0028] Preferably, when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 14.5mm, the V-nozzle is 1.4 m / min; when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 15mm, the V-nozzle is 1.6 m / min; when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 15.5mm, the V-nozzle is 1.7 m / min; when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 16mm, the V-nozzle is 1.9 m / min; when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 16.5mm, the V-nozzle is 2.1 m / min; when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 17mm, the V-nozzle is 2.3 m / min.
[0029] Preferably, when the V water inlet is 1.50m / min, the emergence time is 28.64s; when the V water inlet is 1.60m / min, the emergence time is 26.85s; when the V water inlet is 1.70m / min, the emergence time is 25.27s; when the V water inlet is 1.80m / min, the emergence time is 23.87s; when the V water inlet is 1.90m / min, the emergence time is 22.61s; when the V water inlet is 2.0 ... in, the seedling emergence time is 21.48s; when the V water inlet is 2.10m / min, the seedling emergence time is 20.46s; when the V water inlet is 2.20m / min, the seedling emergence time is 19.53s; when the V water inlet is 2.30m / min, the seedling emergence time is 18.68s; when the V water inlet is 2.40m / min, the seedling emergence time is 17.90s; when the V water inlet is 2.50m / min, the seedling emergence time is 17.18s.
[0030] Another aspect of the present application further provides a billet continuous casting device with a low accident rate, comprising:
[0031] The first stage control module is used for injecting molten steel into the copper tube cavity of the crystallizer until the cold material is filled in the crystallizer, and then forming a billet head in the crystallizer, which is the first stage of molten steel pouring; the molten steel pulling speed in the first stage is V1, and the casting time is T1; the molten steel pulling speed is the speed at which the liquid level of the molten steel in the crystallizer rises.
[0032] The second stage control module is used to continue pouring molten steel into the copper tube of the crystallizer after the vibrating billet head is demoulded from the end of the first stage, and to set the pouring time T2 under the molten steel drawing speed V2 to complete the second stage;
[0033] The third stage control module is used to continue pouring molten steel into the copper tube of the crystallizer at the set molten steel pulling speed V3 for time T3 from the end of the second stage, until the molten steel level in the crystallizer stabilizes at 55-65% of the total volume of the copper tube of the crystallizer, completing the third stage, and then transferring to the second casting system to continue the subsequent molten steel casting operation.
[0034] Another aspect of the present application provides a computer-readable storage medium having a computer program stored thereon, which, when executed, implements the steps of the above-mentioned method for continuous casting of steel billets with a low accident rate.
[0035] Another aspect of the present application provides a computer device, including a processor, a memory, and a computer program stored in the memory, wherein the processor implements the steps of the above-mentioned billet continuous casting method when executing the computer program.
[0036] The beneficial effects of this application include:
[0037] 1) The low-accident-rate steel billet continuous casting method and its device, medium, and equipment provided in this application have been used continuously on 4 continuous casting machines of our company, with a pouring success rate of up to 99%, effectively reducing the pouring accident rate and avoiding production and equipment damage losses caused by pouring accidents; starting pouring directly from the water inlet can effectively reduce the length of the billet head and improve the molten steel recovery rate of the casting machine; this method simplifies the operation, realizes one-button starting, and reduces the technical labor intensity of steel pouring workers.
[0038] 2) The present application provides a method for continuous casting of steel billets with a low accident rate and its device, medium, and equipment. The method divides the pouring process into three stages and sets parameters according to the characteristics of each stage, thereby achieving control over the flow stability of molten steel in the process, improving the flow stability of molten steel, and reducing the occurrence of overflow. It can also be used in conjunction with the existing automatic casting control system to make up for the shortcomings of existing equipment and increase the success rate of billet casting. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] Figure 1 This is a physical picture of the existing continuous casting process, where a) is the inner cavity of the crystallizer filled with cold material; b) is the head of the solidified billet after pouring;
[0040] Figure 2 A schematic diagram of the continuous casting process provided in the embodiment of the present application; a) is the first stage of pouring molten steel to bury the cold material; b) is the second stage of continuing to pour molten steel; c) is the state of pouring molten steel to the transfer system;
[0041] Figure 3 A photo of the system user interface in at least one embodiment provided in this application;
[0042] Figure 4 A photo of a system parameter setting interface in at least one embodiment provided in this application;
[0043] Figure 5 A photo of the interface for setting various parameters of the system at each stage in at least one embodiment provided in this application;
[0044] Figure 6 A schematic flow chart of a method for continuous casting of steel billets with low accident rate in at least one embodiment provided in the present application;
[0045] Figure 7 A schematic diagram of a module of a billet continuous casting device with low accident rate in at least one embodiment provided in the present application. DETAILED DESCRIPTION
[0046] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Generally, the components of the embodiments of the present invention described and shown in the drawings here can be arranged and designed in various different configurations.
[0047] Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the invention claimed for protection, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0048] The technical means that are not described in detail in this application and are not used to solve the technical problems of this application are all set according to the common knowledge in the field, and can be implemented in a variety of common knowledge settings.
[0049] See also Figures 1 to 7The invention provides a method for continuous casting of steel billets with low accident rate, comprising the following steps:
[0050] Step S1: After the cold material is loaded into the crystallizer, molten steel is injected into the copper tube cavity of the crystallizer until the cold material is submerged to form a billet head in the crystallizer, which is the first stage of molten steel pouring; the molten steel drawing speed in the first stage is V1, and the casting time is T1; the molten steel drawing speed is the speed at which the liquid level of the molten steel in the crystallizer rises.
[0051] Step S2: After the vibration billet head is demoulded from the end of the first stage, molten steel is continuously poured into the copper tube of the crystallizer, and the pouring time T2 is set at the molten steel drawing speed V2 to complete the second stage;
[0052] Step S3: From the end of the second stage, continue to cast molten steel into the copper tube of the crystallizer at the set molten steel pulling speed V3 for time T3, until the molten steel level in the crystallizer stabilizes at 55-65% of the total volume of the copper tube of the crystallizer, completing the third stage, and then transfer to the second casting system to continue the subsequent molten steel casting operation.
[0053] This method divides the start-up pouring process into three stages, and performs molten steel casting in steps. Different casting speeds and casting times are set in each stage, thereby effectively avoiding the problem that the existing automatic casting system cannot be used due to the unstable molten steel level during the start-up pouring process. In conjunction with the existing pouring system, the success rate of the pouring process can be increased to 99%, avoiding material waste caused by multiple failures, reducing various losses caused by failed pouring, and avoiding damage to the equipment.
[0054] The molten steel is injected into the crystallizer and combined with the cold material to form a billet head. As the molten steel covers the cold material and vibrates the crystallizer to improve the tightness of the combination of the molten steel and the cold material, the billet head demoulding stage is entered to complete the first stage; as the molten steel level in the crystallizer continues to rise in the second stage, the liquid level gradually rises in the crystallizer to complete the second stage; after the second stage, it is the third stage of stable control of the molten steel level. After continuing to add molten steel until the molten steel level reaches the control position, it is switched to the radium molybdenum automatic pouring state. In each stage, the data module calculates the liquid level rising speed and the time required for pouring according to the size of the nozzle used, and automatically simulates human operation to complete the four stages to achieve automatic pouring. Thereby effectively improving the success rate of pouring. In the continuous casting pouring process, while the molten steel is continuously injected into the crystallizer, the molten steel level rises slowly, the pulling speed continues to increase, and finally the pulling speed matches the liquid level and the liquid level is stable.
[0055] In a specific embodiment, the demoulding time of the vibrating blank head is set to 3 to 5 seconds. According to this setting, the demoulding can be completed in time.
[0056] The first stage (from the beginning of molten steel injection to the end of covering the cold material)
[0057] In a specific embodiment, when the first stage is completed, the liquid level in the crystallizer satisfies H1:
[0058] H1=[D1+D2+L2*0.7+V1*1000 / 60*T1]-V 1*T 1; wherein: D1 is the depth of the ingot inserted into the crystallizer (mm); D2 is the thickness of the gap filler between the outer wall of the ingot head and the inner cavity of the copper tube (mm); L2 is the length of the cold material (mm); V1 is the set first-stage molten steel pulling speed (m / min); T1 is the set first-stage casting time (s); V1 is 0.3~0.5m / min; T1 is 2~10s; the pulling speed V1 and time T1 can be modified and adjusted according to the nozzle diameter and casting section used.
[0059] After setting V1 and T1, the liquid level H1 of the first stage is determined to determine the completion position of the first stage: in a specific embodiment, H1 ingot insertion depth 100mm + 5mm asbestos filler + 280mm cold material length. D1 = 100mm; D2 = 5mm; L2 = 280mm; H1 = 385mm.
[0060] In a specific embodiment, H1=[100mm+5mm+280mm*0.7+Vgate*1000 / 60*T(time 1)]-Vsetting1*T(time 1);
[0061] The second stage (after the first stage is completed, the molten steel casting is completed after the molten steel casting time T2 is set and the molten steel pulling speed V2 is set)
[0062] H2=[H1+V2*1000 / 60*T2]-V2*T2;
[0063] Wherein H1 is the height of the liquid level in the crystallizer after the completion of the first stage (mm); V2 is the molten steel pulling speed set in the second stage (m / min); T2 is the time for casting molten steel in the second stage (s); V2 is 0.5-1.5m / min; T2 is 8-20s; pulling speed V2 and time T2 can be modified and adjusted according to the nozzle diameter and casting section used. In a specific embodiment, the second casting system used in the third stage (after the end of the second stage, when the length of the cavity that can accommodate molten steel is L6*55-65%, it is switched to the second casting system) can be seamlessly switched for the automatic casting control system of Radium Molybdenum Company. L6*55-65% is the cesium source irradiation area of Radium Molybdenum Company, that is, 50mm-150mm from the upper mouth of the crystallizer, and it switches between 95mm-105mm from the upper mouth of the crystallizer.
[0064] In a specific embodiment, the total length of the inner cavity of the copper tube in the continuous casting mold is 900 mm (length L1). During the starting of casting, the depth of the dummy bar inserted into the continuous casting mold is 100 mm (depth D1). Asbestos cloth is filled in the gap between the outer wall of the dummy bar head and the inner cavity of the copper tube to achieve sealing and prevent molten steel from leaking. The thickness of the filled asbestos cloth in the axial direction of the copper tube is 5 mm (thickness D2). A dummy bar is installed inside the copper tube. The dummy bar is used to pull the billet and is arranged on the head of the dummy bar. The length of the charged cold material is 280 mm (length L2). After obtaining the above measured data, the remaining cavity length in the inner cavity of the continuous casting mold copper tube that can accommodate molten steel can be calculated as follows: 900 - 100 - 5 - (280 * 70%) (cold material gap space) - 100 (upper opening space of the continuous casting mold) = 499 mm;
[0065] The remaining cavity length L6 in the inner cavity of the continuous casting mold copper tube that can accommodate molten steel = L1 - D1 - D2 - 70% * L2 (in a specific embodiment, the cavity length of molten steel is: 900 (length of the continuous casting mold copper tube) - 100 (insertion depth of the dummy bar) - 5 (thickness of asbestos cloth filler) - (280 * 70%) (cold material gap space) - 100 (upper opening space of the continuous casting mold) = 499 mm);
[0066] In a specific embodiment, the liquid level height H3 at the end of the third stage:
[0067] H3 = [H2 + V3 * 1000 / 60 * T3)] - V3 * T3; where T3 is the set pouring time of molten steel in the third stage in s; V3 is the set drawing speed of molten steel in the third stage in m / min; V3 is 1.5 - 1.9 m / min; T3 is 10 - 20 s;
[0068] Specifically, 650 mm < H3 < 710 mm; the setting of the H3 height is determined as the detection range of the cesium source of the second casting system, laying the foundation for a smooth switch to the radium - molybdenum automatic pouring system;
[0069] Taking the total length of the continuous casting mold copper tube of 900 mm as an example: 710 mm = 900 mm - 100 mm (distance between the upper opening of the continuous casting mold and the molten steel liquid level) - 150 * 0.6 (lower limit of liquid level automatic control); 650 = 900 mm - 100 mm (distance between the upper opening of the continuous casting mold and the molten steel liquid level) - 150 mm
[0070] In a specific embodiment, it is set that V3 < V nozzle - 0.2 m / min; T3 < emergence time corresponding to V nozzle; (V nozzle is shown in Table 1, and the emergence time corresponding to V nozzle is shown in Table 2). The liquid level rises slowly. When it reaches the lower limit of liquid level automatic control, the automatic pouring mode is switched. By setting T3 in this way, it is prevented that the dummy bar is pulled out of the continuous casting mold in advance, causing the phenomenon of molten steel leakage.
[0071] According to the rules shown in Table 1, the molten steel drawing speed (V nozzle) is determined according to the inner diameter of the crystallizer copper tube and the inner diameter of the molten steel casting tube, as shown in Table 1 below:
[0072]
[0073] In a specific embodiment, the copper tube of the crystallizer has a square cross-section, an inner diameter of 150 mm, and a length of 150 mm; an inner diameter of 165 mm, and a length of 165 mm.
[0074] Specifically, when the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 14.5mm, the V nozzle is 1.6 meters / minute; when the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 15mm, the V nozzle is 1.9 meters / minute; when the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 15.5mm, the V nozzle is 2.1 meters / minute; when the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 16mm, the V nozzle is 2.3 meters / minute; when the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 16.5mm, the V nozzle is 2.4 meters / minute; when the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 17mm, the V nozzle is 2.5 meters / minute;
[0075] Specifically, when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 14.5mm, the V-nozzle is 1.4 meters / minute; when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 15mm, the V-nozzle is 1.6 meters / minute; when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 15.5mm, the V-nozzle is 1.7 meters / minute; when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 16mm, the V-nozzle is 1.9 meters / minute; when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 16.5mm, the V-nozzle is 2.1 meters / minute; when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 17mm, the V-nozzle is 2.3 meters / minute.
[0076] According to the formula of emergence time T (the time from molten steel entering the crystallizer to the time when molten steel fills the crystallizer): T = [L0-L2*70%] / V0 / 1000*60, where L0 is the effective length of the crystallizer copper tube; L2 is the cold material filling length; V0 is the initial pulling speed; the emergence time (the time for the guide rod to pull out the mold) under each pulling speed is calculated:
[0077] The results are shown in the following table:
[0078] The time required to cast the area within the length range of -100mm of the total length of the copper tube of the crystallizer with the molten steel at the initial drawing speed shown in the following table = V0 / (total length of the copper tube of the crystallizer - 100mm); the time required to cast the cold material filling height (mm) = V0 / cold material filling height; the results are shown in the following table:
[0079]
[0080] Specifically, when the V water inlet is 1.50m / min, the emergence time is 28.64s; when the V water inlet is 1.60m / min, the emergence time is 26.85s; when the V water inlet is 1.70m / min, the emergence time is 25.27s; when the V water inlet is 1.80m / min, the emergence time is 23.87s; when the V water inlet is 1.90m / min, the emergence time is 22.61s; when the V water inlet is 2.00m / min, the emergence time is 23.87 .... in, the seedling emergence time is 21.48s; when the V water inlet is 2.10m / min, the seedling emergence time is 20.46s; when the V water inlet is 2.20m / min, the seedling emergence time is 19.53s; when the V water inlet is 2.30m / min, the seedling emergence time is 18.68s; when the V water inlet is 2.40m / min, the seedling emergence time is 17.90s; when the V water inlet is 2.50m / min, the seedling emergence time is 17.18s.
[0081] In one specific embodiment, see Figure 2 The process from a to c) is as follows: the molten steel is just injected into the crystallizer and overflows the cold material to form a billet head; after the billet head is obtained by vibrating and accelerating the demoulding, the liquid level gradually rises; when the liquid level reaches the liquid level, the automatic control is automatically turned on, and the ingot head just comes out of the crystallizer to ensure the longest emergence time. The changes in the molten steel level in the crystallizer during this control process are as follows: Figure 3 As shown, 2 to 3 are combined into the second stage; the blank head is formed as the first stage; and the rise from the liquid level to the liquid level being stable is the third stage. Figure 3 The automatic pouring speed curve is red;
[0082] By setting the casting time and casting speed of each stage and the liquid level height of each stage, the molten steel level in the crystallizer can be stably increased during the pouring process. This method can accurately simulate the operator's operation and realize automatic pouring.
[0083] In a specific embodiment, during 8 casting operations, the parameters are set as shown in the following table:
[0084]
[0085]
[0086] The data shown in the table above was used for pouring. The operation was repeated 8 times with a success rate of 100% and no overflow or insufficient molten steel was observed. The specific operation interface parameter settings are as follows: Figure 4 shown.
[0087] In a specific embodiment, the specific operation interface parameter settings are as follows: Figure 5 The parameter settings are shown in the following table:
[0088]
[0089] The pouring was carried out using the data shown in the table above, with a success rate of 100%, and no overflow or shortage of molten steel was observed.
[0090] Another aspect of the present application further provides a billet continuous casting device with a low accident rate, comprising:
[0091] The first stage control module is used for injecting molten steel into the copper tube cavity of the crystallizer until the cold material is filled in the crystallizer, and then forming a billet head in the crystallizer, which is the first stage of molten steel pouring; the molten steel pulling speed in the first stage is V1, and the casting time is T1; the molten steel pulling speed is the speed at which the liquid level of the molten steel in the crystallizer rises.
[0092] The second stage control module is used to continue pouring molten steel into the copper tube of the crystallizer after the vibrating billet head is demoulded from the end of the first stage, and to set the pouring time T2 under the molten steel drawing speed V2 to complete the second stage;
[0093] The third stage control module is used to continue pouring molten steel into the copper tube of the crystallizer at the set molten steel pulling speed V3 for time T3 from the end of the second stage, until the molten steel level in the crystallizer stabilizes at 55-65% of the total volume of the copper tube of the crystallizer, completing the third stage, and then transferring to the second casting system to continue the subsequent molten steel casting operation.
[0094] Another aspect of the present application provides a computer-readable storage medium having a computer program stored thereon, which, when executed, implements the steps of the above-mentioned method for continuous casting of steel billets with a low accident rate.
[0095] For example, a memory including instructions, which can be executed by a processor to complete the device control method in the above embodiment. For example, the computer readable storage medium can be a read-only memory (ROM), a random access memory (RAM), a compact disc read-only memory (CD-ROM), a magnetic tape, a floppy disk, and an optical data storage device.
[0096] A person skilled in the art will understand that all or part of the steps to implement the above embodiments may be accomplished by hardware or by instructing related hardware through a program, and the program may be stored in a computer-readable storage medium, and the above-mentioned storage medium may be a read-only memory, a disk or an optical disk, etc.
[0097] Another aspect of the present application provides a computer device, including a processor, a memory and a computer program stored in the memory, wherein when the processor executes the computer program, the steps of the above-mentioned method for continuous casting of steel billets with low accident rate are implemented.
[0098] The electronic device may be provided as a server, which may be a cloud server, a host or a personal computer, etc. The server may implement the steps of the above-mentioned wireless station large-area fault priority protection method by a general bus architecture.
[0099] Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments, or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A method for continuous casting of steel billets with low accident rate, It is characterized in that The following steps are involved: Step S1: After the cold material is loaded in the crystallizer, molten steel is injected into the copper tube cavity of the crystallizer until the cold material is submerged and a billet head is formed in the crystallizer, which is the first stage of molten steel pouring; the molten steel drawing speed in the first stage is V1, and the casting time is T1; the molten steel drawing speed is the liquid level rising speed of the molten steel in the crystallizer; Step S2: After the vibration billet head is demoulded from the end of the first stage, molten steel is continuously poured into the copper tube of the crystallizer, and the pouring time T2 is set at the molten steel drawing speed V2 to complete the second stage; Step S3: From the end of the second stage, continue to cast molten steel into the copper tube of the crystallizer at the set molten steel pulling speed V3 for time T3, until the molten steel level in the crystallizer stabilizes at 55-65% of the total volume of the copper tube of the crystallizer, completing the third stage, and then transfer to the second casting system to continue the subsequent molten steel casting operation.
2. The method for continuous casting of steel billets with low accident rate according to claim 1, It is characterized in that When the first stage is completed, the liquid level in the crystallizer satisfies H1: H1 = [D1 + D2 + L2*0.7 + V1*1000 / 60*T1] - V 1*T 1; Wherein: D1 is the depth of the ingot inserting into the crystallizer (mm); D2 is the thickness of the gap filler between the outer wall of the ingot head and the inner cavity of the copper tube (mm); L2 is the length of the cold material (mm); V1 is the set first-stage molten steel pulling speed (m / min); T1 is the set first-stage casting time (s); V1 is set to 0.3-0.5m / min; T1 is set to 2-10s.
3. The method for continuous casting of steel billets with low accident rate according to claim 1, It is characterized in that When the second stage is completed, the liquid level in the crystallizer is H2 = [H1 + V2*1000 / 60*T2] - V2*T2; Among them, H1 is the liquid level height in the crystallizer after the first stage is completed (mm); V2 is the molten steel pulling speed set in the second stage (m / min); T2 is the set duration of molten steel casting in the second stage (s); V2 is set to 0.5-1.5 m / min; T2 is set to 8-20s.
4. The method for continuous casting of steel billets with low accident rate according to claim 1, It is characterized in that The liquid level H3 when the third stage is completed: H3 = [H2 + V3 * 1000 / 60 * T3)] - V3 * T3; where T3 is the time for casting the molten steel in the third stage in s; V3 is the molten steel drawing speed in the third stage in m / min; V3 is 1.5-1.9 m / min; T3 is 10-20 s; and 650 mm <H3<710mm。 5. The method for continuous casting of steel billets with low accident rate according to claim 1, It is characterized in that The V3 set in the third stage satisfies: V3<V water inlet-0.2m / min; the T3 set satisfies T3<V water inlet corresponding to the emergence time; Preferably, the demoulding time of the vibrating blank head is set to 3 to 5 seconds.
6. The method for continuous casting of steel billets with low accident rate according to claim 5, It is characterized in that When the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 14.5mm, the V nozzle is 1.6 meters / minute; when the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 15mm, the V nozzle is 1.9 meters / minute; when the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 15.5mm, the V nozzle is 2.1 meters / minute; when the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 16mm, the V nozzle is 2.3 meters / minute; when the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 16.5mm, the V nozzle is 2.4 meters / minute; when the inner diameter of the copper tube is 150mm and the inner diameter of the molten steel casting nozzle is 17mm, the V nozzle is 2.5 meters / minute; Preferably, when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 14.5mm, the V-nozzle is 1.4 m / min; when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 15mm, the V-nozzle is 1.6 m / min; when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 15.5mm, the V-nozzle is 1.7 m / min; when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 16mm, the V-nozzle is 1.9 m / min; when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 16.5mm, the V-nozzle is 2.1 m / min; when the inner diameter of the copper tube is 165mm and the inner diameter of the molten steel casting nozzle is 17mm, the V-nozzle is 2.3 m / min.
7. The method for continuous casting of steel billets with low accident rate according to claim 5, It is characterized in that When the V water inlet is 1.50m / min, the emergence time is 28.64s; when the V water inlet is 1.60m / min, the emergence time is 26.85s; when the V water inlet is 1.70m / min, the emergence time is 25.27s; when the V water inlet is 1.80m / min, the emergence time is 23.87s; when the V water inlet is 1.90m / min, the emergence time is 22.61s; when the V water inlet is 2.00m / min, the emergence time is 25.27s. The seedling emergence time is 21.48s; when the V-water inlet is 2.10m / min, the seedling emergence time is 20.46s; when the V-water inlet is 2.20m / min, the seedling emergence time is 19.53s; when the V-water inlet is 2.30m / min, the seedling emergence time is 18.68s; when the V-water inlet is 2.40m / min, the seedling emergence time is 17.90s; when the V-water inlet is 2.50m / min, the seedling emergence time is 17.18s.
8. A billet continuous casting device with low accident rate, It is characterized in that include: The first stage control module is used for injecting molten steel into the copper tube cavity of the crystallizer until the cold material is filled in the crystallizer, and then forming a billet head in the crystallizer, which is the first stage of molten steel pouring; the molten steel pulling speed in the first stage is V1, and the casting time is T1; the molten steel pulling speed is the speed at which the liquid level of the molten steel in the crystallizer rises. The second stage control module is used to continue pouring molten steel into the copper tube of the crystallizer after the vibrating billet head is demoulded from the end of the first stage, and to set the pouring time T2 under the molten steel drawing speed V2 to complete the second stage; The third stage control module is used to continue pouring molten steel into the copper tube of the crystallizer at the set molten steel pulling speed V3 for time T3 from the end of the second stage, until the molten steel level in the crystallizer stabilizes at 55-65% of the total volume of the copper tube of the crystallizer, completing the third stage, and then transferring to the second casting system to continue the subsequent molten steel casting operation.
9. A computer-readable storage medium, It is characterized in that A computer program is stored thereon, and when the computer program is executed, the steps of the method for continuous casting of steel billets with low accident rate as described in any one of claims 1 to 7 are implemented.
10. A computer device comprising a processor, a memory and a computer program stored on the memory, It is characterized in that When the processor executes the computer program, the steps of the billet continuous casting method as described in any one of claims 1 to 7 are implemented.