Single-wire or double-wire narrow-gap welding gun capable of improving welding quality

By introducing high-frequency induction preheating and tungsten argon arc welding arc into the narrow gap welding torch, combined with mechanical insulating block tracking technology, the problem of conductive nozzle installation and welding sidewall fusion of the narrow gap welding torch is solved, and the welding quality and efficiency are improved.

CN119057185APending Publication Date: 2024-12-03NANJING DONGSIDA ELECTROMECHANICAL TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411102173.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-12
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

The narrow gap welding gun lacks a conductive nozzle, which causes the welding wire to be easily "sticked" or "arced" at the outlet of the gun rod, and the entire gun rod needs to be replaced frequently, and the structure is complex and difficult to process, which cannot effectively ensure the fusion of the welding side walls.

Method used

A narrow gap welding torch including a high-frequency induction preheater and a tungsten argon arc welding arc was designed. The high-frequency induction heating coil and a tungsten argon arc welding torch rod were used for local high-temperature preheating, and passed through a whole or split insulation block. Realize mechanical weld tracking and simplify the installation and replacement of conductive nozzles.

Benefits of technology

It improves the fusion rate of the welding side wall, shortens the preheating time and cost, ensures the welding quality, and solves the weld tracking and splashing problems through mechanical tracking, extending the service life of the conductive nozzle.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119057185A_ABST
    Figure CN119057185A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of welding, high-frequency induction heating and machinery, in particular to the technology of a single-wire or double-wire narrow-gap welding gun capable of improving the welding quality, preheating while welding, tracking an insulating block and the like. The two narrow-gap welding gun rods are symmetrically arranged, the air supply pipe and the inclined air supply pipe are arranged between the two welding guns, and the preheater is an electric arc of a high-frequency induction preheater or an argon arc welding machine. The method plays an important role in ensuring the reliable fusion of the side wall and the tracking of the welding seam.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the fields of welding, high-frequency induction heating and mechanical technology, and in particular to a welding-while-preheating technology and a weld tracking technology for a single-wire or double-wire narrow-gap welding gun capable of improving welding quality. Background Art

[0002] Patent: A new type of twin-wire narrow gap welding gun 202010220373.5 and an improved twin-wire narrow gap welding gun 2020215782-144.0, both of which involve the preheating function of narrow gap welding. An improved twin-wire narrow gap welding gun 2020215782-144.0, the preheating function is achieved by flame heating, and subsequent tests show that the flame heating temperature does not meet practical requirements. A new type of twin-wire narrow gap welding gun 202010220373.5 The heating electrode is a tungsten rod or a carbon rod. It is not practical to say that the heating electrode is a tungsten rod or a carbon rod.

[0003] Narrow gap welding is a relatively new welding method. It uses an "I" type groove, which can greatly reduce the amount of welding wire to be filled, thereby doubling the welding production efficiency. However, the lack of fusion of the welding side wall is the most common welding defect. Moreover, once the welding side wall does not fuse, it is difficult to repair. Therefore, how to ensure the fusion of the welding side wall as much as possible from the equipment is the common goal of all welding equipment related personnel. At present, there is another shortcoming of the narrow gap original welding equipment: most of the narrow gap welding guns do not have a conductive nozzle. The reason is that the gap between the two welded parts is very narrow, and the gun rod needs to be cooled by water. Due to the limitation of the narrow space, it is not convenient to install a conductive nozzle on the gun rod. The outlet of the gun rod is equivalent to a conductive nozzle. However, the conductive nozzle is a consumable part. The welders in the factory have to replace a conductive nozzle every two or three days or three or four days. Therefore, if the welding wire "sticks" or "arces" at the outlet of the welding gun gun rod, the entire gun rod must be replaced. The narrow gap welding gun has a complex structure and cannot be processed by conventional processing methods. At present, most of them are made by 3D printing methods. Therefore, how to install the conductive tip on the narrow gap welding gun is also a technical problem that this application strives to solve. Summary of the invention

[0004] In order to solve the above problems, the present invention provides a single-wire or double-wire narrow gap welding method which can improve welding quality, realize local high-temperature preheating, shorten preheating time and cost, and facilitate the installation of conductive nozzles.

[0005] The technical solution of the present invention is: a single-wire or double-wire narrow gap welding gun capable of improving welding quality comprises a preheater placed in sequence, two symmetrically placed narrow gap welding gun rods, an air supply pipe between the two welding guns and an inclined air supply pipe, wherein the preheater is a high-frequency induction preheater.

[0006] Furthermore, the preheater is a high-frequency induction preheater; the high-frequency heating coil of the high-frequency induction preheater is placed in front of the narrow gap welding gun rod along the welding direction, and is also placed in the narrow gap between the first weldment and the second weldment, close to the weld; and the surfaces of the first weldment, the second weldment and the weld adjacent to the high-frequency heating coil are heated at the same time.

[0007] Furthermore, the high-frequency heating coil is a hollow water-cooled copper tube, which is covered with an outer insulation layer and has a single turn.

[0008] Furthermore, the preheater is an arc for tungsten inert gas arc welding, comprising two tungsten inert gas arc welding gun rods, wherein the tungsten inert gas arc welding gun rods are placed in front of the narrow gap welding gun rod along the welding direction from front to back, the gas supply pipe is placed in the middle of the two tungsten inert gas arc welding gun rods, and the inclined gas supply pipe is placed below the tungsten inert gas arc welding gun rods. The tungsten inert gas arc welding gun rods are placed in the narrow gap between the first weldment and the second weldment, close to the weld. The lower ends of the two gun rods have inclined holes, and tungsten electrodes are inserted into the inclined holes and locked with screws (2-8). The tungsten electrodes are tilted to point to the intersection of the two side walls of the weldment and the weld, and the distance between the two tungsten electrode tips is 7-20 mm. The first weldment and the second weldment and the weld can be heated simultaneously, and the tips of the two tungsten electrodes are respectively aligned with the adjacent lines of the first weldment and the weld or the adjacent lines of the second weldment and the weld.

[0009] Furthermore, the narrow gap welding gun rod, argon arc welding gun rod and high-frequency heating coil connecting rod all include a slider A or a slider B, a guide rail A or a guide rail B, the upper ends of the narrow gap welding gun rod, the argon arc welding gun rod and the high-frequency heating coil connecting rod are connected to the slider A or the slider B, the slider A or the slider B slides in the guide rail A or the guide rail B respectively, the guide rail A or the guide rail B is arranged on the first weldment and the second weldment through a bracket, and a plurality of insulating blocks are placed on the narrow gap welding gun rod, the argon arc preheating gun rod and the high-frequency heating coil connecting rod and the lower part of the conductive nozzle, and the insulating blocks are mounted on the narrow gap welding gun rod, the argon arc welding gun rod, the high-frequency heating coil connecting rod and the conductive nozzle and abut against the gas supply pipe.

[0010] Furthermore, several insulating blocks are placed at the narrow gap welding gun rod, argon arc welding gun rod, high-frequency heating coil connecting rod and the lower end of the conductive nozzle. Several threaded holes are arranged on each gun rod or conductive nozzle below the insulating block. Screws are screwed into each threaded hole to prevent the insulating blocks at the above-mentioned locations from slipping off. A blind hole is arranged at both ends of the insulating block, and a compression spring is arranged in the blind hole. The two ends of the insulating block and the side wall abutment surface are arc-shaped. When the welding gun rod moves in the narrow gap, the arc surface at the end of the insulating block is easy to slide over the side wall of the weldment.

[0011] Furthermore, the insulating block is an integral insulating block or a split insulating block; a compression spring is arranged between the integral insulating block and the weldment on one side, and the assembled integral insulating block always abuts against one side wall of the weldment on the other side under the action of the spring force; the split insulating block includes two symmetrically arranged insulating blocks, a compression spring is arranged between the symmetrically arranged insulating blocks, and the assembled split insulating block always abuts against the two side walls of the weldment respectively under the action of the spring force.

[0012] Furthermore, the two symmetrically placed arc-shaped narrow gap welding gun rods include U-shaped water cooling holes and wire feeding holes, the lower ends of the U-shaped water cooling holes are close to the conductive nozzles, and the upper ends of the U-shaped water cooling holes are connected to flexible water inlet pipes and water outlet pipes.

[0013] Furthermore, a piece of the gun barrel at the lower end of the narrow gap welding gun barrel is cut off to make the thickness of the gun barrel thinner, and an arc-shaped semicircular groove wire-feeding hole is arranged on the cut surface, and a piece of the upper part of the conductive nozzle is cut off to make the thickness of the upper part of the conductive nozzle thinner, and an arc-shaped semicircular groove wire-feeding hole is arranged on the cut surface, and the semicircular groove wire-feeding hole and the semicircular groove wire-feeding hole are combined to form a circular wire-feeding hole, and a circular wire-feeding hole is arranged at the lower end of the semicircular groove wire-feeding hole of the conductive nozzle, and the welding wire is sent out from the circular wire-feeding hole; the thickness of the lower end of the narrow gap welding gun barrel becomes thinner, and at the thinned part of the gun barrel, through holes and countersunk holes are arranged around the semicircular groove wire-feeding hole, and at the thinned part of the upper end of the conductive nozzle, threaded holes are arranged around the arc-shaped semicircular groove wire-feeding hole, screws are passed through the through holes and the threaded holes, and the screws lock the gun barrel and the conductive nozzle.

[0014] Furthermore, the air supply pipe and the inclined air supply pipe can be rectangular pipes or circular pipes, and are preferably rectangular thin-walled 304 stainless steel pipes with a wall thickness of 1.0-2.0 mm.

[0015] The beneficial effects of the present invention are:

[0016] 1) The difficulty in fusing the side wall is a major problem in narrow gap welding. Experiments have found that the higher the preheating temperature, the easier it is for the side wall to fuse, so preheating is very important. A few years ago, the applicant had a patent that proposed preheating with a flame heating gun, but the flame temperature was low and the preheating temperature was not high. Compared with preheating with flame, the present invention uses high-frequency induction method for preheating or arc preheating with argon arc welding, which has no tempering problem and is safer. Moreover, the preheating range can be controlled by the shape of the heating coil or the position of the tungsten electrode of the argon arc welding machine, which is convenient for achieving local high temperature. Compared with preheating with flame over a large area, it shortens the preheating time and cost and ensures reliable fusion of the side wall.

[0017] 2) Weld seam tracking is another major problem in narrow gap welding. The present invention proposes to use integral insulating blocks and split insulating blocks for mechanical tracking, which is not subject to arc or electromagnetic interference and is stable and reliable. The present invention installs several insulating blocks on the narrow gap welding gun rod, the argon arc preheating gun rod, the high-frequency heating coil connecting rod and the lower end of the conductive nozzle, and makes the insulating blocks abut the side wall, further ensuring the reliable fusion of the side wall;

[0018] The upper ends of the narrow gap welding gun rod, the argon arc preheating gun rod and the high frequency heating coil connecting rod are all connected to the slider, which can slide in the guide rail. The spring can keep the distance between the gun rod and the side wall unchanged, with good tracking effect, which is conducive to the reliable fusion of the side wall. The slider and the guide rail can be sliders and guide rails with rolling balls, so that the gun rod moves more flexibly, and a smaller spring force can make the insulating block close to the side wall of the weldment, so that the distance between the welding wire and the side wall of the weldment remains unchanged.

[0019] 3) Welding spatter adheres to and sticks to the side wall of the weldment, which hinders the movement of the mechanical tracking block. This is a chronic problem of the mechanical tracker. The present invention installs several insulating blocks on the narrow gap welding gun rod, the argon arc preheating gun rod, the high-frequency heating coil connecting rod and the lower end of the conductive nozzle. The spring makes the insulating block abut the side wall, and the insulating blocks on both sides abut against the air supply pipe, which completely blocks the spatter from crossing the insulating block and sticking to the upper side wall. When welding the next weld, the welding gun is raised and the insulating block is also raised. The insulating block is always running in the non-splash area, which better overcomes the chronic problem of spatter hindering the operation of the mechanical tracker.

[0020] 4) The gun barrel of a general narrow gap welding gun is specially made, and the outlet of the gun barrel is equivalent to a conductive tip. Once "wire sticking" or "arcing" occurs at the outlet of the gun barrel, the entire gun barrel needs to be replaced. This application can install a special conductive tip for easy replacement. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] The present invention will be further described below in conjunction with the accompanying drawings and embodiments.

[0022] Figure 1 Front view of the heating coil of the high-frequency induction preheater;

[0023] Figure 2 Figure 1 Top view;

[0024] Figure 3 Overall structure diagram of high frequency induction preheater;

[0025] Figure 4 Front view of the argon arc preheating gun tip;

[0026] Figure 5 Figure 4 Top view;

[0027] Figure 6 The overall structure diagram of the argon arc preheating gun;

[0028] Figure 7 Front view of the insulation block;

[0029] Figure 8 Top view of the overall insulation block;

[0030] Fig. 9Top view of split insulation block;

[0031] Fig.10 Front view of the gun barrel conductive nozzle assembly;

[0032] Fig.11 Fig.10 Side view;

[0033] Fig.12 Top view of the overall insulation block assembly;

[0034] Fig.13 Top view of split insulation block assembly;

[0035] Fig.14 Front view of the lower end of the gun barrel;

[0036] Fig.15 Fig.14 Side view;

[0037] Fig.16 Fig.14 Top view;

[0038] Fig.17 Front view of the contact nozzle;

[0039] Fig.18 Fig.17 Side view;

[0040] Fig.19 Fig.17 Top view.

[0041] In the figure: 1 high-frequency induction preheater, 1-1 high-frequency heating coil, 2 narrow gap welding gun rod, 2-1 conductive tip, 2-3 semicircular groove wire hole below the gun rod, 2-4 semicircular groove wire hole above the conductive tip, 2-5 wire hole, 2-6 through hole, 2-7 threaded hole, 2-8 screw, 2-9 tungsten electrode, 2-10 countersunk hole,

[0042] 2-11 Slider A, 2-12 Guide rail A, 2-13 Slider B, 2-14 Guide rail B, 3 Air supply pipe, 4 First weldment, 5 Second weldment, 6 Narrow gap, 7 Welding seam, 8 Inclined air supply pipe, 10 Welding wire,

[0043] 11 argon arc preheating gun rod or high frequency heating coil connecting rod, 12 insulating block (including integral insulating block and split insulating block), 12-1 blind hole, 12-2 spring, 13 water cooling hole, 14 wire feeding hole, 15 screw hole. DETAILED DESCRIPTION

[0044] The technical solution of the present invention will be clearly and completely described below through specific implementation methods.

[0045] Example 1

[0046] like Figure 1-3 As shown, a single-wire or double-wire narrow gap welding gun of this embodiment that can improve welding quality includes a preheater placed in sequence, two symmetrically placed narrow gap welding gun rods 2, and an air supply pipe 3 and an inclined air supply pipe 8 between the two welding guns, wherein the preheater is a high-frequency induction preheater.

[0047] In this embodiment, the high-frequency heating coil 1-1 of the high-frequency induction heater is placed in front of the narrow gap welding gun rod 2 along the welding direction, and is placed in the narrow gap 6 between the first weldment 4 and the second weldment 5, close to the weld 7, so that the surfaces adjacent to the first weldment 4, the second weldment 5 and the weld 7 and the high-frequency heating coil 1-1 can be heated simultaneously. The high-frequency heating coil 1-1 is a hollow water-cooled copper tube, with an outer flange layer, and a single turn.

[0048] As a mechanical tracking measure, the upper ends of the narrow gap welding gun rod 2, the argon arc preheating gun rod 11, and the high-frequency heating coil connecting rod 11 are connected to the slider A2-11 or the slider B2-13, and the slider A2-11 or the slider B2-13 can slide in the guide rail A2-12 or the guide rail B2-14. The guide rail A2-12 or the guide rail B2-14 is arranged on the first weldment 4 and the second weldment 5 through the bracket. A plurality of integral insulating blocks 12 are placed on the narrow gap welding gun rod 2, the argon arc preheating gun rod 11, the high-frequency heating coil connecting rod, and the lower part of the conductive nozzle 2-1. The insulating blocks 12 are mounted on the narrow gap welding gun rod 2, the argon arc preheating gun rod 11, the high-frequency heating coil connecting rod, and the conductive nozzle 2-1 and abut against the gas supply pipe 3. (As shown in FIG. Figure 7 , 8, 10, 11, 13) at the lower ends of the narrow gap welding gun rod 2, the argon arc preheating gun rod 11, the high-frequency heating coil connecting rod and the conductive nozzle 2-1, there are screw holes 15, screws can be screwed into the screw holes 15 to prevent the insulating block 12 from slipping, and a blind hole 12-1 is arranged at both ends of the integral insulating block. A compression spring 12-2 is arranged in the blind hole. The assembled integral insulating block 12 always abuts against a side wall of the weldment under the action of the spring force. The two ends of the abutting surface of the integral insulating block and the side wall are arc-shaped. When the welding gun rod moves in the narrow gap 6, the arc-shaped surface at the end of the integral insulating block is easy to slide over the side wall of the weldment.

[0049] The integral insulating block 12 also has the function of preventing splashing from spraying upward.

[0050] The gun barrel of the narrow gap welding gun cannot be ventilated and heat dissipated in the narrow gap, and must be water-cooled. Therefore, in this embodiment, U-shaped water cooling holes 13 and wire feeding holes 14 are arranged in two symmetrically placed arc-shaped gun barrels 2, the lower end of the U-shaped water cooling hole is close to the conductive nozzle 2-1, and the upper end of the U-shaped water cooling hole is connected to a flexible water inlet pipe and a water outlet pipe.

[0051] To equip the gun barrel 2 with a special conductive tip, the thickness of the gun barrel at the lower end of the gun barrel 2 must be thinned, that is, a piece is cut off, and an arc-shaped semicircular groove wire-moving hole 2-3 is arranged on the cut surface. A piece of the upper part of the conductive tip 2-1 is also cut off to make the thickness of the upper part of the conductive tip thinner, and an arc-shaped semicircular groove wire-moving hole 2-4 is arranged on the cut surface. The semicircular groove wire-moving hole 2-3 and the semicircular groove wire-moving hole 2-4 together form a circular wire-moving hole. A circular wire-moving hole 2-5 is arranged at the lower end of the semicircular groove wire-moving hole 2-4 of the conductive tip 2-1. The wire circular hole 2-5 is the wire outlet hole of the conductive tip, and the welding wire 10 is fed out from the wire circular hole 2-5. At the thinning part of the narrow gap welding gun rod 2, a through hole 2-6 and a countersunk hole 2-10 are arranged around the semicircular groove wire hole 2-3. At the thinning part of the conductive tip 2-1, a threaded hole 2-7 is arranged around the arc-shaped semicircular groove wire hole 2-4. Screws 2-8 are passed through the through holes 2-6 and the threaded holes 2-7. The screws 2-8 lock the gun rod 2 and the conductive tip 2-1, and the screw heads are placed in the countersunk holes 2-10.

[0052] The air supply pipe 3 and the inclined air supply pipe 8 can be rectangular tubes or circular tubes, and are preferably rectangular thin-walled 304 stainless steel tubes with a wall thickness of 1.0-2.0 mm.

[0053] Example 2

[0054] Same as Example 1, except that the preheater is an arc of tungsten inert gas welding, such as Figure 4-6 As shown, it includes two tungsten inert gas arc preheating gun rods 11, which are placed in front of the narrow gap welding gun rod 2 one after the other along the welding direction, and the air supply pipe 3 is placed in the middle of the two tungsten inert gas preheating gun rods 11. The inclined air supply pipe 8 is next to the tungsten inert gas arc preheating gun rods 11. The tungsten inert gas arc preheating gun rods 11 are placed in the narrow gap 6 between the first weldment 4 and the second weldment 5, close to the weld 7. The lower ends of the two gun rods have inclined holes, and tungsten electrodes 2-9 are inserted into the inclined holes. The tungsten electrodes 2-9 are inclined to point to the intersection of the two side walls of the weldment and the weld 7 respectively, and the distance between the two tungsten electrode tips is 7 20 mm, which can heat the first weldment 4 and the second weldment 5 and the weld 7 at the same time. The tips of the two tungsten electrodes 2-9 are respectively aligned with the adjacent lines of the first weldment 4 and the weld 7 or the adjacent lines of the second weldment 5 and the weld 7.

[0055] Several integral insulating blocks 12 are placed on the narrow gap welding gun rod, the argon arc welding gun rod, the high-frequency heating coil connecting rod and the lower part of the conductive nozzle 2-1. The insulating blocks 12 are mounted on each gun rod and abut against the air supply pipe 3.

[0056] Example 3

[0057] The same as the first embodiment, except that a plurality of split insulating blocks 12 are placed on the narrow gap welding gun rod, the argon arc welding gun rod, the high frequency heating coil connecting rod and the lower part of the conductive tip 2-1. The split insulating blocks 12 are mounted on each gun rod and abut against the gas supply pipe 3. Figure 7 As shown in Figures 9, 10, 12, and 13, a plurality of threaded holes 15 are arranged on each gun barrel or conductive nozzle below the split insulating block 12, and a screw is screwed into each threaded hole 15 to prevent the split insulating blocks 12 at the above-mentioned locations from slipping off. A blind hole 12-1 is arranged at each end of the split insulating block, and a compression spring 12-2 is arranged in the blind hole. The assembled split insulating block 12 always abuts against the two side walls of the weldment under the action of the spring force, and the two ends of the abutting surface between the split insulating block and the side wall are arc-shaped. When the welding gun barrel moves in the narrow gap 6, the arc-shaped surface at the end of the split insulating block is easy to slide over the side wall of the weldment.

[0058] In terms of preventing splashing and spraying upward and reducing the sliding resistance of the insulating block, the split insulating block 12 is better than the integral insulating block.

[0059] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Those skilled in the art may make various modifications or equivalent substitutions to the present invention within the essence and protection scope of the present invention, and such modifications or equivalent substitutions should also be deemed to fall within the protection scope of the technical solution of the present invention.

Claims

1. A single-wire or double-wire narrow gap welding gun capable of improving welding quality, comprising a preheater placed in sequence, two narrow gap welding gun rods (2) placed symmetrically, an air supply pipe (3) between the two welding guns, and an inclined air supply pipe (8), characterized in that: The preheater is a high-frequency induction preheater.

2. A single-wire or double-wire narrow gap welding gun capable of improving welding quality according to claim 1, characterized in that: The high-frequency heating coil (1-1) of the high-frequency induction preheater is placed in front of the narrow gap welding gun rod (2) along the welding direction, and is also placed in the narrow gap (6) between the first weldment (4) and the second weldment (5), close to the weld (7); and the surfaces of the first weldment (4), the second weldment (5) and the weld (7) adjacent to the high-frequency heating coil (1-1) are heated simultaneously.

3. A single-wire or double-wire narrow gap welding gun capable of improving welding quality according to claim 2, characterized in that: The high-frequency heating coil (1-1) is a hollow water-cooled copper tube, which is covered with an outer insulation layer and has a single turn.

4. A single-wire or double-wire narrow gap welding gun capable of improving welding quality according to claim 1, characterized in that: The preheater is an arc for tungsten inert gas welding, comprising two tungsten inert gas welding gun rods (11), the tungsten inert gas welding gun rods (11) are placed in front of a narrow gap welding gun rod (2) along the welding direction from front to back, the gas supply pipe (3) is placed between the two tungsten inert gas welding gun rods (11), the inclined gas supply pipe (8) is below the tungsten inert gas welding gun rods (11), the tungsten inert gas welding gun rods (11) are placed in the narrow gap (6) between the first weldment (4) and the second weldment (5), close to the weld (7), and the two The lower end of the gun barrel is provided with an oblique hole, into which a tungsten electrode (2-9) is inserted and locked with a screw (2-8), the tungsten electrodes (2-9) are tilted to point to the intersections of the two side walls of the weldment and the weld (7), and the distance between the two tungsten electrode tips is 7-20 mm, so that the first weldment (4) and the second weldment (5) and the weld (7) can be heated at the same time, and the tips of the two tungsten electrodes (2-9) are respectively aligned with the adjacent lines between the first weldment (4) and the weld (7) or the adjacent lines between the second weldment (5) and the weld (7).

5. A single-wire or double-wire narrow gap welding gun capable of improving welding quality according to claim 1, characterized in that: The narrow gap welding gun rod (2) and the argon arc welding gun rod (11), and the high-frequency heating coil connecting rod (11) all include a slider A (2-11) or a slider B (2-13), a guide rail A (2-12) or a guide rail B (2-14), the upper ends of the narrow gap welding gun rod (2) and the argon arc welding gun rod (11), and the high-frequency heating coil connecting rod (11) are connected to the slider A (2-11) or the slider B (2-13), and the slider A (2-11) or the slider B (2-13) are respectively connected to the guide rail A (2-12) or the guide rail B (2-14). 4), the guide rail A (2-12) or the guide rail B (2-14) is arranged on the first weldment (4) and the second weldment (5) through the bracket, and a plurality of insulating blocks (12) are placed on the narrow gap welding gun rod (2), the argon arc welding gun rod (11), the high-frequency heating coil connecting rod (11) and the lower part of the conductive nozzle (2-1). The insulating blocks (12) are mounted on the narrow gap welding gun rod (2), the argon arc welding gun rod (11), the high-frequency heating coil connecting rod (11) and the conductive nozzle (2-1) and abut against the air supply pipe (3).

6. A single-wire or double-wire narrow gap welding gun capable of improving welding quality according to claim 5, characterized in that: A plurality of insulating blocks (12) are placed at the lower ends of the narrow gap welding gun rod (2), the argon arc welding gun rod (11), the high frequency heating coil connecting rod (11) and the conductive nozzle (2-1). A plurality of threaded holes (15) are arranged on each gun rod or conductive nozzle below the insulating block (12). A screw is screwed into each threaded hole (15) to prevent the insulating blocks (12) at the above-mentioned locations from slipping off. A blind hole (12-1) is arranged at each end of the insulating block. A compression spring (12-2) is arranged in the blind hole. The two ends of the insulating block and the side wall abutment surface are arc-shaped. When the welding gun rod moves in the narrow gap (6), the arc-shaped surface at the end of the insulating block is easy to slide over the side wall of the weldment.

7. A single-wire or double-wire narrow gap welding gun capable of improving welding quality according to claim 6, characterized in that: The insulating block (12) is an integral insulating block or a split insulating block; a compression spring is arranged between the blind hole of the integral insulating block and the weldment on one side, and the assembled integral insulating block always abuts against one side wall of the weldment on the other side under the action of the spring force; the split insulating block includes two symmetrically arranged insulating blocks, and compression springs are arranged in the blind holes of the symmetrically arranged insulating blocks, and the assembled split insulating blocks always abut against the two side walls of the weldment respectively under the action of the spring force.

8. A single-wire or double-wire narrow gap welding gun capable of improving welding quality according to claim 1, characterized in that: The two symmetrically placed arc-shaped narrow gap welding gun rods (2) include a U-shaped water cooling hole (13) and a wire feeding hole (14), the lower end of the U-shaped water cooling hole is close to the conductive nozzle (2-1), and the upper end of the U-shaped water cooling hole is connected to a flexible water inlet pipe and a water outlet pipe.

9. A single-wire or double-wire narrow gap welding gun capable of improving welding quality according to claim 1, characterized in that: A piece of the gun rod at the lower end of the narrow gap welding gun rod (2) is cut off to make the thickness of the narrow gap welding gun rod (2) thinner, and an arcuate semicircular groove wire-feeding hole (2-3) is arranged on the cut surface; a piece of the upper part of the conductive nozzle (2-1) is cut off to make the thickness of the upper part of the conductive nozzle (2-1) thinner, and an arcuate semicircular groove wire-feeding hole (2-4) is arranged on the cut surface; the semicircular groove wire-feeding hole (2-3) and the semicircular groove wire-feeding hole (2-4) are combined to form a circular wire-feeding hole; a circular wire-feeding hole (2-5) is arranged at the lower end of the semicircular groove wire-feeding hole (2-4) of the conductive nozzle (2-1), and the welding wire (10) is fed out from the circular wire-feeding hole (2-5); A through hole (2-6) and a countersunk hole (2-10) are arranged around a semicircular groove wire-feeding hole (2-3) at a thinned portion of a narrow gap welding gun rod, and a threaded hole (2-7) is arranged around an arcuate semicircular groove wire-feeding hole (2-4) at a thinned portion of a conductive tip. Screws (2-8) are passed through the through holes (2-6) and the threaded holes (2-7), and the screws (2-8) lock the gun rod (2) and the conductive tip (2-1).

10. A single-wire or double-wire narrow gap welding gun capable of improving welding quality according to claim 1, characterized in that: The air supply pipe (3) and the inclined air supply pipe (8) can be rectangular pipes or circular pipes, and are preferably rectangular thin-walled 304 stainless steel pipes with a wall thickness of 1.0-2.0 mm.