Integrated equal-material manufacturing device and method of three-dimensional structure
By using superimposed beam and temperature control technology in manufacturing devices, the speed and efficiency problems in complex three-dimensional structure manufacturing are solved, and the efficient molding of unsupported structures is achieved, the surface finish and structural integrity are improved, and suitable for personalized and small Mass production.
Patent Information
- Application Number
- CN202411478544.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-22
- Publication Date
- 2024-12-03
AI Technical Summary
The prior art has problems such as slow manufacturing speed, layered traces, waste of materials and difficulty in handling support structures when manufacturing complex three-dimensional structures, especially in additive manufacturing and reduced material manufacturing, which lacks design flexibility and high efficiency.
Six loading plates distributed around the barrel are adopted, and each loading plate is equipped with an array-distributed projection laser. Three-dimensional forming without support structure is achieved in the barrel by superimposing the light beam, and the light intensity is accurately controlled using transparent barrels and temperature control components. and temperature to ensure uniform curing.
It improves manufacturing speed and efficiency, reduces stratification traces, significantly improves the surface finish and structural integrity of the finished product, adapts to personalized and small batch production needs, and meets high performance requirements.
Smart Images

Figure CN119058087A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of advanced manufacturing technology, and in particular to an integrated equal-material manufacturing device and method for a three-dimensional structure. Background Art
[0002] With the development of modern industry, the demand for manufacturing complex three-dimensional structures is growing, driving the development of various manufacturing technologies, including additive manufacturing (AM), subtractive manufacturing (SDM), and formative manufacturing (FM). Although these technologies have achieved significant progress in specific areas, they each face a series of challenges and limitations when manufacturing complex products. AM technologies, such as selective laser sintering (SLS), fused deposition modeling (FDM), and stereolithography (SLA), offer advantages in design flexibility and material utilization. However, their layer-by-layer manufacturing approach limits fabrication speed and easily produces delamination marks, which affects the overall mechanical properties and surface finish of the finished product. Furthermore, the fabrication of overhangs or complex internal structures requires additional support structures, which not only increases manufacturing costs but also presents challenges in post-processing. Subtractive manufacturing technologies, such as computer numerical control (CNC) machining, while offering excellent performance in terms of manufacturing accuracy and surface quality, often result in significant material waste and significantly increase the difficulty and cost of machining complex parts or those with complex internal structures. Furthermore, subtractive manufacturing often requires specialized operating skills and expensive equipment investment. Although isocratic manufacturing technologies, such as forging and casting, can produce parts with good mechanical properties, these technologies often lack design flexibility and are not sufficiently responsive to the needs of personalized and small-batch production.
[0003] A Chinese patent (publication number CN 110834410 A) discloses a method for forming complex three-dimensional structures using PDMS based on 3D printing. The method involves pre-preparing PDMS silicone and a supporting gel for printing. The initial three-dimensional structure model is then printed layer by layer in the gel medium, and then solidified after forming. However, this method still falls under the category of additive manufacturing, requiring the configuration of supporting structures. While the supporting structures can be recycled, they still require processing before and after forming, impacting printing efficiency. Furthermore, the connection between the supporting structure and the printed structure suffers from poor surface quality and structural integrity. Summary of the Invention
[0004] The purpose of the present invention is to address the defects of the prior art and provide an integrated equal-material manufacturing device and method for three-dimensional structures. Six loading plates are arranged around the barrel, and an array of distributed projection lasers are arranged on each loading plate to slice the target structure. A translucent printing substrate is arranged in the barrel, so that each forming point of the target structure is solidified and formed by a superimposed light beam. The superimposed light beam comes from the light beams emitted by multiple projection lasers on the six loading plates, so that the target structure can be integrated and formed in the barrel without a supporting structure, realizing equal-material manufacturing, improving printing efficiency and meeting the needs of personalized and small-batch production.
[0005] The first object of the present invention is to provide an integrated equal-material manufacturing device for a three-dimensional structure, which adopts the following scheme:
[0006] It includes a loading plate and a projection laser. Multiple projection laser arrays are arranged on the loading plate. Six loading plates correspond to the six faces of the cube distributed inside to form a working chamber. The barrel is placed in the working chamber, and the projection laser is facing the barrel. Each forming point in the barrel is superimposed by the light beams output by the projection lasers on at least two different loading plates, so that the light intensity at the forming point is greater than the curing light intensity threshold.
[0007] Furthermore, a spatial light modulator, a Fourier transform lens, and a high-pass beam block are provided in the projection laser along the optical path, and the light beam is output to the forming point in the barrel after passing through the high-pass beam block.
[0008] Furthermore, the barrel is made of a transparent material, and the light beams output by the projection laser can pass through the barrel wall and act on the material in the barrel. The barrel is equipped with a temperature control component for adjusting the temperature of the material.
[0009] Furthermore, the barrel is a cylindrical structure, with a cavity for accommodating materials formed inside.
[0010] Furthermore, adjacent loading plates among the six loading plates are connected to form a closed working chamber.
[0011] Furthermore, each forming point in the barrel is formed by superimposing the light beams output by the projection lasers on six loading plates, and at least one light beam output by the projection laser on each loading plate is transmitted to the forming point.
[0012] A second object of the present invention is to provide a method for manufacturing an integrated three-dimensional structure as described in the first object, comprising:
[0013] The barrel is placed in the working chamber surrounded by the loading plate, and the material is stored in the barrel;
[0014] All forming points in the barrel are configured based on the target structure slice, each forming point corresponds to at least two projection lasers, and the projection lasers are located on different loading plates;
[0015] The projection laser works so that each forming point receives the superposition of multiple beams from different projection lasers. All forming points are solidified together, and the target structure is formed in one piece inside the barrel.
[0016] Furthermore, when the projection laser output light beam passes through a plurality of forming points, the light intensity of the projection laser output light beam is made smaller than the curing light intensity threshold of all the passing forming points.
[0017] Furthermore, after the molding point receives the superposition of multiple light beams, the light intensity at the molding point is greater than the light intensity threshold for curing the material at the molding point, and adjacent molding points are connected.
[0018] Furthermore, the barrel controls the temperature of the material it carries so that the material at non-forming point positions remains in a liquid state.
[0019] Compared with the prior art, the present invention has the following advantages and positive effects:
[0020] (1) In order to solve the problem that the additive manufacturing of complex workpieces still needs to establish a support structure, which affects the printing efficiency, six loading plates are arranged around the barrel. An array of projection lasers is arranged on each loading plate to slice the target structure. A translucent printing substrate is arranged in the barrel so that each forming point of the target structure is solidified by a superimposed light beam. The superimposed light beam comes from the light beams emitted by multiple projection lasers on the six loading plates, which can solidify the entire three-dimensional structure in the barrel at one time, avoiding the problems of inter-layer seams and support structures in traditional additive manufacturing, thereby improving the manufacturing speed and efficiency of parts, reducing delamination marks, and significantly improving the surface finish and structural integrity of the finished product. It overcomes the common surface roughness and internal defects in traditional additive manufacturing, can process a variety of materials, and adapt to different manufacturing needs. Especially in the applications of aerospace, medical and automotive industries, it can meet the requirements of high performance and personalization.
[0021] (2) The transparent barrel allows the light beam output by the projection laser to directly pass through the barrel wall and act on the material inside the barrel, making the entire curing process more efficient. The light beam can evenly irradiate the molding point of the material, accelerating the curing process. The barrel is equipped with a temperature control component that can accurately adjust the temperature of the material and control the speed and quality of the curing reaction. Precise temperature control helps to optimize the physical properties of the molded parts and reduce molding defects. The design of the closed working chamber also helps to reduce the interference of the external environment on the molding process, thereby improving the structural integrity and surface quality of the molded parts.
[0022] (3) By superimposing the beams of light from multiple projection lasers on the forming points from different directions, it is possible to ensure that the light intensity of the material at each forming point in the barrel is uniform, thereby achieving a more uniform curing process. Uniform curing helps to improve the mechanical properties and surface quality of the molded parts. When the output beam of the projection laser passes through multiple forming points, by controlling the light intensity to be less than the curing light intensity threshold of all the passing forming points, the molding error caused by overexposure of the passing points before reaching the target molding point can be avoided, which helps to improve the molding accuracy and detail resolution. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] The accompanying drawings, which constitute a part of the present invention, are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute improper limitations on the present invention.
[0024] Figure 1 Schematic diagram of the principle of the projection laser in Examples 1 and 2 of the present invention.
[0025] Figure 2 Schematic diagram of the arrangement of the projection laser on the loading plate in Examples 1 and 2 of the present invention.
[0026] Figure 3 Schematic diagram of the barrel in Examples 1 and 2 of the present invention.
[0027] Figure 4 Schematic diagram of the integrated equal-material manufacturing device for the three-dimensional structure in Examples 1 and 2 of the present invention.
[0028] Among them, 1. projection laser; 2. loading plate; 3. laser source; 4. beam expander; 5. first lens; 6. pinhole spatial filter; 7. second lens; 8. reflector; 9. refractive beam shaper; 10. spatial light modulator; 11. Fourier transform lens; 12. high-pass beam block; 13. projection surface; 14. barrel. DETAILED DESCRIPTION
[0029] Example 1
[0030] In a typical embodiment of the present invention, Figure 1-Figure 4 As shown, a three-dimensional structure integrated equal material manufacturing device is provided.
[0031] The current isotropic manufacturing technology lacks design flexibility, is insufficiently responsive to the needs of small-batch production, and has limited adaptability to the needs of lightweight design, the application of high-performance materials, and personalized customization. Additive manufacturing technology has the problem of slow manufacturing speed. For the manufacture of overhangs or complex internal structures, additional support structures are required, which increases manufacturing costs and post-processing difficulties. Based on this, the present embodiment provides an integrated isotropic manufacturing device with a three-dimensional structure, which is provided with six loading plates 2 distributed around a barrel 14, and each loading plate 2 is provided with an array of projection lasers 1 to slice the target structure. A light-transmitting printing substrate is provided in the barrel 14, so that each forming point of the target structure is solidified and formed by superimposed light beams. The superimposed light beams come from the light beams emitted by multiple projection lasers 1 on the six loading plates 2, so that the target structure can be integrated and formed in the barrel 14 without a support structure, thereby realizing isotropic manufacturing, improving printing efficiency, and meeting the needs of personalized and small-batch production.
[0032] like Figure 4 As shown, the integrated equal-material manufacturing device for three-dimensional structure includes a loading plate 2, a projection laser 1 and a barrel 14. Multiple projection lasers 1 are arranged in an array on the loading plate 2. Six loading plates 2 corresponding to the six faces of the cube are distributed inside to form a working cavity. The barrel 14 is placed in the working cavity, and the projection laser 1 is facing the barrel 14. Each forming point in the barrel 14 is superimposed by the light beams output by the projection lasers 1 on at least two different loading plates 2, so that the light intensity at the forming point is greater than the curing light intensity threshold.
[0033] By arranging projection lasers 1 on six loading plates 2, light beams are output from the six faces of the cube, so that the forming points can receive light beams from multiple directions and perform light curing on demand. Since each forming point is cured by the superposition of light beams from projection lasers 1 on at least two different loading plates 2, three-dimensional, all-round forming can be achieved in the barrel 14, thereby producing complex three-dimensional structures.
[0034] In addition, the coordinated operation of multiple lasers can simultaneously cure multiple points, significantly increasing the speed of the manufacturing process, especially when manufacturing large or complex structures. Curing from multiple directions can reduce the interlayer delamination problem common in traditional additive manufacturing, thereby improving the structural integrity and mechanical properties of the molded part.
[0035] In traditional additive manufacturing, complex or overhanging structures often require additional support structures. The integrated three-dimensional structure manufacturing device provided in this embodiment can reduce this need, and multi-directional curing can naturally support the formation of the structure. The device can precisely control the light intensity at each forming point, ensuring that only the points requiring curing reach the curing light intensity threshold, which helps improve forming accuracy and reduce material waste.
[0036] like Figure 1As shown, a spatial light modulator 10 , a Fourier transform lens 11 , and a high-pass beam block 12 are provided along the optical path in the projection laser 1 . The light beam passes through the high-pass beam block 12 and is output to the forming point in the barrel 14 .
[0037] Specifically, the projection laser 1 comprises a laser source 3, a spatial light modulator 10 (SLM), a beam expander 4, a lens, a pinhole spatial filter 6, a reflector 8, a refractive beam shaper 9, a Fourier transform lens 11, a high-pass beam block 12, and a beam splitter. Along the optical path, the laser source 3, beam expander 4, first lens 5, pinhole spatial filter 6, second lens 7, reflector 8, refractive beam shaper 9, lens, spatial light modulator 10, Fourier transform lens 11, and high-pass beam block 12 are arranged in sequence. After being output from the high-pass beam block 12, the light beam forms a projection surface 13 at the forming point, thereby solidifying the material in the barrel 14.
[0038] The light source uses a diode laser as the pump laser source 3, a device that generates laser light through a solid gain medium. Diode lasers are widely used due to their high efficiency, compact size, and variety of wavelength options.
[0039] The spatial light modulator 10 (SLM) is composed of thousands of tiny controllable units, which are light modulating materials such as liquid crystals and micromirrors. By changing the voltage or light signal applied to the unit, the phase and amplitude of the light wave passing through each unit can be precisely controlled. Using a liquid crystal SLM (LCoS SLM), the electro-optical effect of liquid crystal is used to modulate the phase and amplitude of the light wave. The arrangement and orientation of the liquid crystal unit can be controlled by an electric field, thereby changing the propagation characteristics of the light wave. The beam expander 4 is used to improve the quality of the light beam so that it maintains good focus during transmission. The lens is used to focus and transmit light to achieve efficient and precise light control.
[0040] Pinhole spatial filter 6 physically filters out light waves generated by aberrations or other non-ideal factors in the optical system, thereby reducing aberrations and improving imaging contrast and resolution. Reflector 8 reflects light, redirecting the optical path. Refractive beam shaper 9 is an optical element that modifies the shape, size, or angle of a beam based on the principle of light refraction. The shaper is composed of multiple lenses, and effective beam shaping can be achieved through precise design of the lens shape and arrangement.
[0041] The Fourier transform lens 11 is used to generate an object hologram. The high-pass beam block 12 is used to suppress low-frequency contamination or noise in the light wave. A beam splitter can also be provided to split the incident light beam into two or more parts.
[0042] The temperature control assembly integrated within barrel 14 precisely controls the material temperature, which is crucial for controlling the speed and quality of the curing reaction. Specifically, the temperature control assembly can be mounted on a combined heating and cooling module. The heating and cooling module utilizes semiconductors for heating and cooling, while a temperature sensor monitors the temperature within barrel 14 in real time, ensuring that the heating and cooling modules can precisely control the temperature within barrel 14.
[0043] A controller may also be provided for receiving signals from the temperature sensor and regulating the operation of the heating-cooling module according to preset temperature parameters to maintain constant temperature conditions.
[0044] like Figure 3 As shown, the barrel 14 is made of a transparent material. This allows the light beam to pass through unimpeded and act on the material, which helps achieve a more uniform curing effect. In this embodiment, the barrel 14 is cylindrical in structure, forming a cavity inside to hold the material. The cylindrical structure can be a circular or rectangular cylindrical structure.
[0045] like Figure 2 and Figure 4 As shown, the enclosed working chamber formed by six loading plates 2 provides better environmental control, reducing the impact of external factors such as dust and humidity on the molding process. Due to the high precision and uniform curing during the molding process, the need for post-processing (such as grinding and polishing) is greatly reduced, thereby reducing manufacturing costs and time.
[0046] As can be understood, the material is a resin material that cures only at a certain exposure level. The required light intensity for curing, or the curing threshold, is then calculated based on whether each point is cured or not. For a single point, six beams of light can be superimposed in space. Because the spatial light modulator 10 can adjust both light intensity and phase, the light intensity at any point in space can be controlled to be above or below the curing threshold.
[0047] The wavelengths of the DPSS lasers used were 532 nm, 266 nm, and 355 nm.
[0048] In some embodiments, the resin material used is polyethylene glycol diacrylate, and the material concentration ranges from 5 wt % to 15 wt %. The photoinitiator used is Irgacure 784, and the photoinitiator concentration ranges from 0.5 to 1.5 wt %.
[0049] In some embodiments, the resin material used is 1,6-hexanediol diacrylate (HDDA) with a concentration range of 10wt%-20wt%, the aluminum oxide powder concentration range is 40wt%-60wt%, and the photoinitiator used is diphenyl (2,4,6-trimethylbenzoyl) phosphine oxide (TPO) with a photoinitiator concentration of 0.1-1.5wt%.
[0050] In some embodiments, the resin material used is 1,6-hexanediol diacrylate (HDDA) at a concentration range of 10 wt%-20 wt%, the titanium powder concentration is 30 wt%-50 wt%, and the photoinitiator used is diphenyl (2,4,6-trimethylbenzoyl) phosphine oxide (TPO) at a concentration of 1-3 wt%.
[0051] Each forming point in the barrel 14 is superimposed by the light beams output by the projection lasers 1 on the six loading plates 2, and the light beam output by at least one projection laser 1 on each loading plate 2 is transmitted to the forming point. Specifically, polyethylene glycol diacrylate (PEGDA) with a photoinitiator is configured, and then the material is loaded into the barrel 14, the temperature control module is started, and the manufacturing operation is started after the temperature stabilizes. The three-dimensional model after slicing of the target structure is imported, and the light intensity and phase required for each projection laser 1 are calculated. The projection lasers 1 on the six loading plates 2 are debugged and manufacturing is started. After manufacturing is completed, the manufactured three-dimensional structure is cleaned with PBS.
[0052] Example 2
[0053] In another typical embodiment of the present invention, Figure 1-Figure 4 As shown, a working method of a three-dimensional structure integrated equal material manufacturing device is provided, using the three-dimensional structure integrated equal material manufacturing device as in Example 1.
[0054] A working method of an integrated equal-material manufacturing device for a three-dimensional structure, comprising:
[0055] The barrel 14 is placed in the working chamber surrounded by the loading plate 2, and the barrel 14 contains material;
[0056] All forming points in the barrel 14 are configured based on the target structure slice, each forming point corresponds to at least two projection lasers 1, and the projection lasers 1 are located on different loading plates 2;
[0057] The projection laser 1 works so that each forming point receives the superposition of multiple beams from different projection lasers 1 , and all the forming points are solidified together, and the target structure is integrally formed in the barrel 14 .
[0058] When the output light beam of the projection laser 1 passes through multiple forming points, the light intensity of the output light beam of the projection laser 1 is made smaller than the curing light intensity threshold of all the passing forming points.
[0059] After the molding point receives the superposition of multiple light beams, the light intensity at the molding point is greater than the light intensity threshold for material solidification at the molding point, and adjacent molding points are connected.
[0060] The barrel 14 controls the temperature of the material it carries so that the material at non-forming points remains in a liquid state.
[0061] Specifically, the working method of the integrated equal-material manufacturing device for a three-dimensional structure in this embodiment includes:
[0062] Step 1: Assemble the barrel 14.
[0063] Place the barrel 14 in a predetermined working position and ensure that it is stable.
[0064] Temperature control components, including but not limited to heaters and temperature sensors, are installed at predetermined locations within barrel 14 to precisely control the temperature of the material within barrel 14. The temperature control components are connected to the control system via electrical wiring to ensure accurate and reliable signal transmission. During assembly, the temperature measurement system is tested to verify its sensitivity and stability. This testing can be accomplished by varying the temperature within barrel 14 and monitoring the sensor readings.
[0065] Step 2: Assemble the projection part.
[0066] Reference Figure 1 , assemble a single projection laser 1, and install the assembled single projection laser 1 on six predetermined loading plates 2, ensuring the correct positioning and fixation of each unit.
[0067] Step 3: Assemble the entire manufacturing equipment.
[0068] Combine the barrel 14 assembled in step 1 with the projection part assembled in step 2, ensuring that the connection between the barrel 14 and the projection part is correct and that all electrical and mechanical connections are secure and correct.
[0069] Step 4: Prepare the light-curing resin material.
[0070] PEGDA powder was dissolved in RO water at 30° C. and 500 rpm to prepare a mixed solution, and then photoinitiator Irgacure 784 was added. The prepared material was 10 wt % polyethylene glycol diacrylate and 1 wt % photoinitiator.
[0071] Step 5: Start manufacturing.
[0072] A mixed solution of a photoinitiator and a photocurable resin material is loaded into the barrel 14. The resulting 3D model is then sliced and introduced into the device. The projection section is turned on for fabrication, with six beams irradiating the material for 8 seconds.
[0073] Step 6, cleaning.
[0074] The solidified three-dimensional model was taken out and washed with PBS.
[0075] In other optional embodiments, the working method of the integrated isotropic material manufacturing device for three-dimensional structures includes:
[0076] The equipment of Example 1 is used to manufacture integrated materials of complex three-dimensional structures. The specific steps are as follows:
[0077] Step 1: Assemble the barrel 14.
[0078] Place the barrel 14 in a predetermined working position and ensure that it is stable.
[0079] Temperature control components, including but not limited to heaters and temperature sensors, are installed at predetermined locations within barrel 14 to precisely control the temperature of the material within barrel 14. The temperature control components are connected to the control system via electrical wiring to ensure accurate and reliable signal transmission. During assembly, the temperature measurement system is tested to verify its sensitivity and stability. This testing can be accomplished by varying the temperature within barrel 14 and monitoring the sensor readings.
[0080] Step 2: Assemble the projection part.
[0081] Reference Figure 1 , assemble a single projection laser 1, and install the assembled single projection laser 1 on six predetermined loading plates 2, ensuring the correct positioning and fixation of each unit.
[0082] Step 3: Assemble the entire manufacturing equipment.
[0083] Combine the barrel 14 assembled in step 1 with the projection part assembled in step 2, ensuring that the connection between the barrel 14 and the projection part is correct and that all electrical and mechanical connections are secure and correct.
[0084] Step 4: preparing a light-curing resin material containing ceramic powder.
[0085] HDDA powder was dissolved in RO water and a mixed solution was prepared at 40°C and 500 rpm. Then, a photoinitiator, diphenyl (2,4,6-trimethylbenzoyl) phosphine oxide (TPO), and alumina ceramic powder were added. The prepared material was 10 wt% polyethylene glycol diacrylate, 1.5 wt% TPO, and 40 wt% alumina powder.
[0086] Step 5: Start manufacturing.
[0087] A mixed solution of a photoinitiator, ceramic powder, and a photocurable resin material is loaded into the barrel 14. The resulting 3D model is then sliced and introduced into the device. The projection unit is turned on for fabrication, with six beams irradiating the material for 5 seconds.
[0088] Step 6, cleaning.
[0089] The solidified three-dimensional model was taken out and washed with PBS.
[0090] Step 7: degreasing and sintering.
[0091] The sintering process was carried out in a muffle furnace under a helium-protected atmosphere, with the temperature rising to 300°C, and then sintered at 1500°C to enhance the mechanical properties of the material.
[0092] In other optional embodiments, the working method of the integrated isotropic material manufacturing device for three-dimensional structures includes:
[0093] The equipment of Example 1 is used to manufacture integrated materials of complex three-dimensional structures. The specific steps are as follows:
[0094] Step 1: Assemble the barrel 14.
[0095] Place the barrel 14 in a predetermined working position and ensure that it is stable.
[0096] Temperature control components, including but not limited to heaters and temperature sensors, are installed at predetermined locations within barrel 14 to precisely control the temperature of the material within barrel 14. The temperature control components are connected to the control system via electrical wiring to ensure accurate and reliable signal transmission. During assembly, the temperature measurement system is tested to verify its sensitivity and stability. This testing can be accomplished by varying the temperature within barrel 14 and monitoring the sensor readings.
[0097] Step 2: Assemble the projection part.
[0098] Reference Figure 1 , assemble a single projection laser 1, and install the assembled single projection laser 1 on six predetermined loading plates 2, ensuring the correct positioning and fixation of each unit.
[0099] Step 3: Assemble the entire manufacturing equipment.
[0100] Combine the barrel 14 assembled in step 1 with the projection part assembled in step 2, ensuring that the connection between the barrel 14 and the projection part is correct and that all electrical and mechanical connections are secure and correct.
[0101] Step 4: preparing a light-curing resin material containing ceramic powder.
[0102] HDDA powder was dissolved in RO water and a mixed solution was prepared at 55°C and 500 rpm. Then, a photoinitiator, diphenyl (2,4,6-trimethylbenzoyl) phosphine oxide (TPO), and metal titanium powder were added. The prepared material was 15 wt% polyethylene glycol diacrylate, 3 wt% TPO, and 35 wt% metal titanium powder.
[0103] Step 5: Start manufacturing.
[0104] A mixed solution of a photoinitiator, ceramic powder, and a photocurable resin material is loaded into the barrel 14. The resulting 3D model is then sliced and introduced into the device. The projection unit is turned on for fabrication, with six beams irradiating the material for 5 seconds.
[0105] Step 6, cleaning.
[0106] The solidified three-dimensional model was taken out and washed with PBS.
[0107] Step 7: degreasing and sintering.
[0108] The sintering process was carried out in a muffle furnace under a helium-protected atmosphere, with the temperature rising to 300°C, and then sintered at 1500°C to enhance the mechanical properties of the material.
[0109] By superimposing the light beams at the forming points from different directions using multiple projection lasers 1, it is possible to ensure that the light intensity of the material at each forming point in the barrel 14 is uniform, thereby achieving a more uniform curing process. Uniform curing helps to improve the mechanical properties and surface quality of the molded part. When the projection laser 1 outputs a light beam passing through multiple forming points, by controlling the light intensity to be less than the curing light intensity threshold of all the passing forming points, molding errors caused by overexposure of the passing points before reaching the target molding point can be avoided, which helps to improve molding accuracy and detail resolution.
[0110] The foregoing description is merely a preferred embodiment of the present invention and is not intended to limit the present invention. Those skilled in the art will readily appreciate that various modifications and variations of the present invention are possible. Any modifications, equivalent substitutions, or improvements made within the spirit and principles of the present invention are intended to be within the scope of protection of the present invention.
Claims
1. A three-dimensional structure integrated equal material manufacturing device, characterized in that: It includes a loading plate and a projection laser. A plurality of projection laser arrays are arranged on the loading plate. Six loading plates correspond to the six faces of a cube distributed inside to form a working cavity. A barrel is placed in the working cavity, and the projection laser faces the barrel. Each forming point in the barrel is superimposed by light beams output by projection lasers on at least two different loading plates, so that the light intensity at the forming point is greater than the curing light intensity threshold.
2. The integrated equal-material manufacturing device for three-dimensional structure according to claim 1, characterized in that: The projection laser is provided with a spatial light modulator, a Fourier transform lens and a high-pass beam block along the optical path direction, and the light beam is output to the forming point in the barrel after passing through the high-pass beam block.
3. The integrated equal-material manufacturing device for three-dimensional structure according to claim 1, characterized in that: The barrel is made of transparent material, and the light beams output by the projection laser can pass through the barrel wall to act on the material in the barrel. The barrel is equipped with a temperature control component for adjusting the temperature of the material.
4. The integrated equal-material manufacturing device for three-dimensional structure according to claim 3, characterized in that: The barrel is a cylindrical structure, and a cavity for accommodating materials is formed inside.
5. The integrated equal-material manufacturing device for three-dimensional structure according to claim 1, characterized in that: Adjacent loading plates among the six loading plates are connected to form a closed working chamber.
6. The integrated equal-material manufacturing device for three-dimensional structure according to claim 5, characterized in that: Each forming point in the barrel is superimposed by the light beams output by the projection lasers on six loading plates, and at least one light beam output by the projection laser on each loading plate is transmitted to the forming point.
7. A working method of a three-dimensional structure integrated equal material manufacturing device, using the three-dimensional structure integrated equal material manufacturing device as claimed in any one of claims 1 to 6, characterized in that: include: The barrel is placed in the working chamber surrounded by the loading plate, and the material is stored in the barrel; All forming points in the barrel are configured based on the target structure slice, each forming point corresponds to at least two projection lasers, and the projection lasers are located on different loading plates; The projection laser works so that each molding point receives the superposition of multiple beams from different projection lasers, all molding points are solidified together, and the target structure is formed in one piece in the barrel.
8. The working method of the integrated equal-material manufacturing device for three-dimensional structure according to claim 7, characterized in that: When the output beam of the projection laser passes through a plurality of forming points, the light intensity of the output beam of the projection laser is made smaller than the curing light intensity threshold of all the passing forming points.
9. The working method of the integrated equal-material manufacturing device for three-dimensional structure according to claim 8, characterized in that: After the molding point receives the superposition effect of multiple light beams, the light intensity at the molding point is greater than the light intensity threshold of the material solidification at the molding point, and adjacent molding points are connected.