Preparation method of potassium hydrogen persulfate composite salt
By combining hydrogen peroxide with potassium persulfate and fumed sulfuric acid under low temperature conditions, the consumption of alkaline potassium salts in water generation and neutralization reactions is solved, and the problems of high energy consumption and high risk in the prior art are achieved. The efficient preparation of potassium bisulfate composite salt and the recycling of mother liquor water reduce production costs and environmental impact.
Patent Information
- Application Number
- CN202411570393.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-11-06
- Publication Date
- 2024-12-03
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The method for preparing potassium persulfate composite salt in the prior art has problems such as high energy consumption, high risk, high equipment cost, complex operation and large amount of mother liquor water treatment. Especially in the smoke-induced sulfuric acid method, vacuum concentration treatment is required. This leads to waste of resources and a great impact on the environment.
By mixing 70% hydrogen peroxide with potassium persulfate, slowly adding fume sulfuric acid, controlling the reaction temperature to 5-15°C, cooling after adding potassium carbonate, suction filtration and centrifugation, obtaining potassium persulfate composite salt-wet product, and By drying, the final product can be obtained. This method can reduce the consumption of alkaline potassium salt in water generation and neutralization reaction, realize the recycling of mother liquor water, and reduce energy consumption and cost.
This method reduces water generation and heat release under low temperature conditions, reduces reaction risks, realizes recycling of mother liquor water, reduces wastewater discharge, improves the conversion rate of hydrogen peroxide, and reduces production costs and environmental impact.
Smart Images

Figure CN119059494A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of inorganic peroxide preparation, and more specifically to a method for preparing potassium persulfate composite salt. Background Art
[0002] Chlorosulfonic acid method, anodic oxidation method and oleum method are the methods for preparing potassium persulfate composite salt at present, wherein, the process of chlorosulfonic acid method requires reaction temperature of -15 ° C, and energy consumption is large; it is also necessary to extract byproduct hydrogen chloride gas from the container, hydrogen chloride is highly corrosive, so it has high requirements on pipeline material; anodic oxidation method is to generate peroxydisulfuric acid by electrolysis of sulfuric acid in platinum electrode electrolyzer, and then hydrolyze to generate peroxymonosulfuric acid, but the process uses expensive platinum electrolyzer, equipment investment cost is high, energy consumption is high, and operation is complicated. And oleum method is to add stabilizer with hydrogen peroxide as primer, and then drip oleum to form a mixture of peroxymonosulfuric acid, sulfuric acid and hydrogen peroxide, although this method reacts violently and releases heat; but because of its simple operation and strong practicality, it has become the main choice of industrial production. However, when the concentration of oleum in oleum method is 65%, hydrogen peroxide and oleum can be fully reacted, and the degree of danger is high.
[0003] The Chinese patent with the patent number CN2018107632585 announced on March 26, 2021 discloses a continuous production equipment and preparation method of potassium persulfate composite salt; this preparation method prepares potassium persulfate composite salt by reacting hydrogen peroxide with sulfuric acid. Although this method can be carried out continuously, the primary mother liquor separated after the potassium persulfate composite salt cannot be directly used for recycling, but must be concentrated by vacuum heating to form secondary mother liquor water; secondary mother liquor water can be used for recycling, which is cumbersome and consumes a lot; and during the reaction process, hydrogen peroxide and sulfuric acid react and neutralize to generate water, thereby diluting the solution, so that the final product is directly cooled and crystallized to obtain the final product potassium persulfate composite salt, and then a lower concentration of primary mother liquor water is obtained. If the primary mother liquor water is directly discharged, it will damage the environment. If it is necessary to reduce the impact of the discharge on the environment, the primary mother liquor needs to be vacuum concentrated to increase the concentration of the primary mother liquor so that it can enter the circulation, and the generated condensed water can be discharged. However, such operation takes a long time, requires a large amount of mother liquor to be processed, wastes too much resources, consumes a lot of resources, and is costly.
[0004] Therefore, it is necessary to provide a method for preparing a potassium persulfate composite salt which is simple to operate, has a low risk, does not require vacuum concentration, and can reduce the amount of mother liquor water to be treated. Summary of the invention
[0005] In view of the problems existing in the prior art, the object of the present invention is to provide a method for preparing a potassium persulfate composite salt, which can reduce the water generated in the reaction process through the joint action of hydrogen peroxide, potassium persulfate and oleum, and at the same time reduce the consumption of alkaline potassium salt in the neutralization reaction, thereby reducing the treatment amount of mother liquor water generated by the reaction, reducing energy consumption and reducing cost.
[0006] To solve the above problems, the present invention adopts the following technical solutions.
[0007] A method for preparing potassium persulfate composite salt, the specific steps are as follows: Oxidation reaction: mixing hydrogen peroxide with a mass concentration of 70%, a hydrogen peroxide stabilizer and potassium persulfate uniformly to form a first mixed system; Slowly drop fuming sulfuric acid into the first mixed system, stirring while dropping, and controlling the dropwise reaction temperature to be 5-15° C. to form an oxidizing solution; Mixing reaction: After the mother liquid water and the oxidizing solution are evenly mixed, potassium carbonate is added and stirred. After the reaction is completed, the mixture is cooled to 0-1°C and kept warm for 30 min. After suction filtration and centrifugation, a wet product of potassium persulfate composite salt and mother liquid water are obtained; Drying: After drying the wet product of potassium persulfate composite salt, an anti-caking agent is added to obtain the final product of potassium persulfate composite salt.
[0008] Furthermore, the mass concentration of the oleum is 20-65%.
[0009] Furthermore, the mass concentration of the oleum is 20%.
[0010] Furthermore, the mass ratio of the hydrogen peroxide to potassium persulfate is 1:1.06-1.73.
[0011] Furthermore, the reaction temperature of the mixed reaction is 10-30°C.
[0012] Furthermore, the anti-caking agent is one of magnesium oxide, magnesium carbonate or magnesium sulfate.
[0013] Furthermore, the anti-caking agent is added in an amount of 0.5-2.0% of the dry product of potassium persulfate composite salt.
[0014] Furthermore, the drying temperature of the wet product of potassium persulfate composite salt is 55-65°C.
[0015] Furthermore, the molar ratio of the hydrogen peroxide to oleum is 1:0.38-0.62.
[0016] Furthermore, the hydrogen peroxide stabilizer is one of potassium pyrophosphate, salicylic acid, 8-hydroxyquinoline, sodium hexametaphosphate or ethylenediaminetetraacetic acid.
[0017] Furthermore, the hydrogen peroxide stabilizer is potassium pyrophosphate.
[0018] Compared with the prior art, the advantages of the present invention are: 1. The present invention allows potassium persulfate and oleum to coexist in an oxidation reaction, so that potassium persulfate reacts with water under acidic conditions and hydrolyzes to generate hydrogen peroxide. While reducing the generation of water, the reaction between hydrogen peroxide and oleum is further promoted, the conversion rate of hydrogen peroxide is improved, and the excess water in the reaction system is reduced, thereby reducing the amount of mother liquid water separated during the reaction. In addition, the entire reaction is carried out at a low temperature, so that the spontaneous hydrolysis of hydrogen peroxide and potassium persulfate is not likely to occur, and the heat released by oleum in contact with water is reduced, so that the reaction between hydrogen peroxide and oleum is slowed down, thereby reducing the danger during the reaction.
[0019] 2. The mother liquor water of this scheme contains H2O2, KHSO5, KHSO4 or K2SO4 and other substances after centrifugation; while obtaining the target product potassium persulfate composite salt, the mother liquor water can be directly used in the "mixed reaction of mother liquor water and oxidizing liquid" of the present invention to achieve the recycling of mother liquor water. Moreover, in the recycling process of mother liquor water, it is possible to achieve normal recycling without adding additional vacuum concentration equipment, so that no additional wastewater is generated in the reaction process, thereby reducing the impact of the discharge of acidic wastewater on the environment.
[0020] 3. The reaction process of this scheme can be carried out in a conventional reactor equipment, and there are no other special and strict requirements on the reaction equipment and materials; therefore, this reaction can be widely operated in industry.
[0021] Fourth, in the preparation method provided by this scheme, due to the co-existence of hydrogen peroxide, oleum and potassium persulfate, oleum with a concentration of less than 65% can also fully react with hydrogen peroxide. This method not only ensures a high conversion rate of hydrogen peroxide, but also significantly reduces the risk of the reaction, making the entire reaction safe and reliable. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 It is the reaction flow chart of the present invention. DETAILED DESCRIPTION
[0023] Embodiment 1:
[0024] Oxidation reaction: add 48.60 g of 70% hydrogen peroxide into a 1000 ml four-necked flask, add 0.48 g of potassium pyrophosphate, then add 51.40 g of potassium persulfate, stir for 10 minutes, then slowly add 58.10 g of 20% fuming sulfuric acid, control the temperature of the dropwise addition reaction to be 5-15°C, and obtain an oxidized solution after completion. The hydrogen peroxide content in the oxidized solution was measured to be 4.34%, and the hydrogen peroxide conversion rate was calculated to be 79.90%.
[0025] Mixing reaction: After 316.20 g of mother liquor water and the above-mentioned oxidizing liquid are mixed, 59.80 g of potassium carbonate is added and neutralization reaction is carried out at a temperature of 10-30°C. After the addition is completed, it is cooled to 0-1°C and kept warm for 30 minutes. After suction filtration and centrifugation, 179.10 g of potassium persulfate composite salt wet product and 335.90 g of mother liquor water are obtained. The potassium persulfate composite salt wet product is dried and magnesium oxide is added to obtain the final product potassium persulfate composite salt, and the product yield is 86.0%.
[0026] Embodiment 2:
[0027] Oxidation reaction: add 48.60 g of 70% hydrogen peroxide into a 1000 ml four-necked flask, add 0.48 g of potassium pyrophosphate, then add 67.60 g of potassium persulfate, stir for 10 minutes, then slowly add 46.90 g of 20% fuming sulfuric acid, control the temperature of the dropwise addition reaction to be 5-15°C, and obtain an oxidized solution after completion. The hydrogen peroxide content in the oxidized solution was measured to be 3.14%, and the hydrogen peroxide conversion rate was calculated to be 85.00%.
[0028] Mixing reaction: After 326.20 g of mother liquor water and the above-mentioned oxidizing liquid are mixed, 52.00 g of potassium carbonate is added to carry out neutralization reaction at a temperature of 10-30°C. After the addition is completed, it is cooled to 0-1°C and kept warm for 30 minutes. After suction filtration and centrifugation, 198.50 g of potassium persulfate composite salt wet product and 326.20 g of mother liquor water are obtained. The potassium persulfate composite salt wet product is dried and magnesium oxide is added to obtain the final product potassium persulfate composite salt, and the product yield is 95.00%.
[0029] Embodiment 3:
[0030] Oxidation reaction: add 48.60 g of 70% hydrogen peroxide into a 1000 ml four-necked flask, add 0.48 g of potassium pyrophosphate, then add 84.20 g of potassium persulfate, stir for 10 minutes, then slowly add 35.60 g of 20% fuming sulfuric acid, control the temperature of the dropwise addition reaction to be 5-15°C, and obtain an oxidized solution after completion. The hydrogen peroxide content in the oxidized solution was measured to be 3.65%, and the hydrogen peroxide conversion rate was calculated to be 82.00%.
[0031] Mixing reaction: After 336.80 g of mother liquor water and the above-mentioned oxidizing solution are mixed, 43.50 g of potassium carbonate is added to carry out neutralization reaction at a temperature of 10-30°C. After the addition is completed, it is cooled to 0-1°C and kept warm for 30 minutes. After suction filtration and centrifugation, 183.90 g of potassium persulfate composite salt wet product and 350.90 g of mother liquor water are obtained. The potassium persulfate composite salt wet product is dried and magnesium oxide is added to obtain the final product potassium persulfate composite salt, and the product yield is 88.00%.
[0032] Embodiment 4:
[0033] Oxidation reaction: add 48.60 g of 70% hydrogen peroxide into a 1000 ml four-necked flask, add 0.48 g of potassium pyrophosphate, then add 51.40 g of potassium persulfate, stir for 10 minutes, then slowly add 53.00 g of 65% fuming sulfuric acid, control the temperature of the dropwise addition reaction to be 5-15°C, and obtain an oxidized solution after completion. The hydrogen peroxide content in the oxidized solution was measured to be 4.17%, and the hydrogen peroxide conversion rate was calculated to be 81.30%.
[0034] Mixing reaction: After 306.00 g of mother liquor water and the above-mentioned oxidizing solution are mixed, 59.80 g of potassium carbonate is added and neutralization reaction is carried out at a temperature of 10-30°C. After the addition is completed, it is cooled to 0-1°C and kept warm for 30 minutes. After suction filtration and centrifugation, 177.60 g of potassium persulfate composite salt wet product and 322.10 g of mother liquor water are obtained. The potassium persulfate composite salt wet product is dried and magnesium oxide is added to obtain the final product potassium persulfate composite salt, and the product yield is 85.7%.
[0035] Embodiment 5:
[0036] Oxidation reaction: add 48.60 g of 70% hydrogen peroxide into a 1000 ml four-necked flask, add 0.48 g of potassium pyrophosphate, then add 67.60 g of potassium persulfate, stir for 10 minutes, then slowly add 46.90 g of 35% fuming sulfuric acid, control the temperature of the dropwise addition reaction to be 5-15°C, and obtain an oxidized solution after completion. The hydrogen peroxide content in the oxidized solution was measured to be 3.41%, and the hydrogen peroxide conversion rate was calculated to be 83.70%.
[0037] Mixing reaction: After 326.20 g of mother liquor water and the above-mentioned oxidizing liquid are mixed, 52.00 g of potassium carbonate is added and neutralization reaction is carried out at a temperature of 10-30°C. After the addition is completed, it is cooled to 0-1°C and kept warm for 30 minutes. After suction filtration and centrifugation, 186.3 g of potassium persulfate composite salt wet product and 338.4 g of mother liquor water are obtained. The potassium persulfate composite salt wet product is dried and magnesium oxide is added to obtain the final product potassium persulfate composite salt, and the product yield is 89.1%.
[0038] Embodiment 6:
[0039] Oxidation reaction: add 48.60 g of 70% hydrogen peroxide into a 1000 ml four-necked flask, add 0.48 g of potassium pyrophosphate, then add 67.60 g of potassium persulfate, stir for 10 minutes, then slowly add 40.60 g of 45% fuming sulfuric acid, control the temperature of the dropwise addition reaction to be 5-15°C, and obtain an oxidized solution after completion. The hydrogen peroxide content in the oxidized solution was measured to be 4.46%, and the hydrogen peroxide conversion rate was calculated to be 78.65%.
[0040] Mixing reaction: After 326.20 g of mother liquor water and the above-mentioned oxidizing liquid are mixed, 52.00 g of potassium carbonate is added and neutralization reaction is carried out at a temperature of 10-30°C. After the addition is completed, it is cooled to 0-1°C and kept warm for 30 minutes. After suction filtration and centrifugation, 181.7 g of potassium persulfate composite salt wet product and 343.0 g of mother liquor water are obtained. The potassium persulfate composite salt wet product is dried and magnesium oxide is added to obtain the final product potassium persulfate composite salt, and the product yield is 86.9%.
[0041] Embodiment 7:
[0042] Oxidation reaction: add 48.6 g of 70% hydrogen peroxide into a 1000 ml four-necked flask, add 0.48 g of potassium pyrophosphate, then add 67.6 g of potassium persulfate, stir for 10 minutes, then slowly add 46.9 g of 4.5% fuming sulfuric acid, control the temperature of the dropwise addition reaction to be 5-15°C, and obtain an oxidized solution after completion. The hydrogen peroxide content in the oxidized solution was measured to be 8.93%, and the hydrogen peroxide conversion rate was calculated to be 57.21%.
[0043] Mixing reaction: After 326.2 g of mother liquor water and the above-mentioned oxidizing liquid are mixed, 52.0 g of potassium carbonate is added and neutralization reaction is carried out at a temperature of 10-30°C. After the addition is completed, it is cooled to 0-1°C and kept warm for 30 minutes. After suction filtration and centrifugation, 153.1 g of potassium persulfate composite salt wet product and 371.6 g of mother liquor water are obtained. The potassium persulfate composite salt wet product is dried and magnesium oxide is added to obtain the final product potassium persulfate composite salt, and the product yield is 73.3%.
[0044] Comparative Example 1: Oxidation reaction: add 48.60 g of 70% hydrogen peroxide into a 1000 ml four-necked flask, add 0.48 g of potassium pyrophosphate, and slowly drop 93.80 g of 20% mass fraction fuming sulfuric acid, control the drop reaction temperature to 5-15°C, and obtain an oxidation solution after completion. The hydrogen peroxide content in the oxidation solution was measured to be 7.65%, and the hydrogen peroxide conversion rate was calculated to be 68.00%.
[0045] Mixing reaction: After mixing 284.80 g of mother liquor water with the above-mentioned oxidizing solution, 86.00 g of potassium carbonate is added to carry out neutralization reaction at a temperature of 10-30°C. After the addition is completed, cool to 0-1°C and keep warm for 30 minutes. After suction filtration and centrifugation, 146.2 g of potassium persulfate composite salt wet product and 339.6 g of mother liquor water are obtained. The potassium persulfate composite salt wet product is dried and magnesium oxide is added to obtain the final product potassium persulfate composite salt, and the product yield is 70.0%.
[0046] Comparative Example 2: (1) Add 0.68 g of potassium pyrophosphate to 68.00 g of a 50% hydrogen peroxide solution, stir and mix well to obtain a hydrogen peroxide mixed solution.
[0047] (2) Then, 86.00 g of 65% fuming sulfuric acid was slowly added dropwise, and the reaction temperature was controlled to be 5-15°C. The conversion rate of hydrogen peroxide was 57.0%.
[0048] (3) After 225.00 g of mother liquor water and the above-mentioned oxidizing solution are mixed, 152.00 g of potassium hydroxide solution with a mass concentration of 48% is added to carry out neutralization reaction at a temperature of 10-30°C. After the addition is completed, it is cooled to 0°C and kept warm for 30 minutes. After suction filtration and centrifugation, 130.83 g of potassium persulfate composite salt wet product and 400.17 g of mother liquor water are obtained. The potassium persulfate composite salt wet product is dried and magnesium oxide is added to obtain the final product potassium persulfate composite salt, and the product yield is 63%.
[0049] Table 1 Raw materials used in the preparation of products of Examples and Comparative Examples and the wastewater discharge rate generated
[0050] It can be seen from Comparative Example 1, Comparative Example 2, Example 1 and Example 2 that the added potassium persulfate reacts with water under the action of low temperature environment and acidic environment to generate potassium sulfate, sulfuric acid and hydrogen peroxide, effectively reducing the excess water in the reaction system and improving the conversion rate of hydrogen peroxide. This method reduces the consumption of alkaline potassium salts during the reaction process and reduces production costs; and the mother liquor water obtained after centrifugation contains a solution of substances such as H2O2, KHSO5, KHSO4 and K2SO4 and no excess water is produced. The mother liquor water obtained after centrifugation does not need to be evaporated and can be directly put into the oxidation liquid for production recycling, further reducing production costs and reducing the generation of wastewater, reducing the negative impact on the environment.
[0051] It can be seen from Examples 1 to 4 and Comparative Example 1 that this solution effectively improves the conversion rate of hydrogen peroxide and reduces waste in production, thereby reducing production costs by optimizing the use and reaction conditions of hydrogen peroxide.
[0052] It can be seen from Examples 1 to 4 and Comparative Example 2 that the potassium persulfate prepared by the present method has the advantages of high yield, low cost and low wastewater discharge rate compared to the preparation method of Comparative Example 2.
[0053] It can be seen from Example 2, Example 4-Example 7 and Comparative Example 1-Comparative Example 2 that: under the same conditions, the concentration of oleum is changed; the mass concentration of oleum is preferably 20%, and increasing or decreasing the concentration of oleum cannot increase the yield, and has no positive effect on reducing the wastewater discharge rate. It is further shown that adding potassium persulfate to the oxidation reaction can significantly reduce the concentration of oleum reacting with hydrogen peroxide, so that oleum with a mass concentration of less than 65% can also fully react with hydrogen peroxide, and the hydrogen peroxide conversion is maintained at more than 75%.
Claims
1. A method for preparing a potassium persulfate composite salt, characterized in that: The preparation method of potassium persulfate composite salt is as follows: Oxidation reaction: mixing hydrogen peroxide with a mass concentration of 70%, a hydrogen peroxide stabilizer and potassium persulfate uniformly to form a first mixed system; Slowly drop fuming sulfuric acid into the first mixed system, stirring while dropping, and controlling the dropwise reaction temperature to be 5-15° C. to form an oxidizing solution; Mixing reaction: After the mother liquid water and the oxidizing solution are evenly mixed, potassium carbonate is added and stirred. After the reaction is completed, the mixture is cooled to 0-1°C and kept warm for 30 min. After suction filtration and centrifugation, a wet product of potassium persulfate composite salt and mother liquid water are obtained; Drying: After the wet product of potassium persulfate composite salt is dried, an anti-caking agent is added to obtain the final product potassium persulfate composite salt.
2. The method for preparing a potassium persulfate composite salt according to claim 1, wherein: The mass concentration of the oleum is 20-65%.
3. A method for preparing a potassium persulfate composite salt according to claim 2, characterized in that: The mass ratio of the hydrogen peroxide to potassium persulfate is 1:1.06-1.
73.
4. The method for preparing a potassium persulfate composite salt according to claim 1, wherein: The reaction temperature of the mixed reaction is 10-30°C.
5. The method for preparing a potassium persulfate composite salt according to claim 1, characterized in that: The anti-caking agent is one of magnesium oxide, magnesium carbonate or magnesium sulfate.
6. The method for preparing a potassium persulfate composite salt according to claim 1, characterized in that: The amount of the anti-caking agent added is 0.5-2.0% of the dry product of potassium persulfate composite salt.
7. The method for preparing a potassium persulfate composite salt according to claim 1, characterized in that: The drying temperature of the wet product of potassium persulfate complex salt is 55-65°C.
8. The method for preparing a potassium persulfate composite salt according to claim 1, characterized in that: The molar ratio of the hydrogen peroxide to oleum is 1:0.38-0.
62.
9. The method for preparing a potassium persulfate composite salt according to claim 1, characterized in that: The hydrogen peroxide stabilizer is one of potassium pyrophosphate, salicylic acid, 8-hydroxyquinoline, sodium hexametaphosphate or ethylenediaminetetraacetic acid.
10. The method for preparing a potassium persulfate composite salt according to claim 1, characterized in that: The hydrogen peroxide stabilizer is potassium pyrophosphate.
Citation Information
Patent Citations
Potassium peroxymonosulfate composite salt continuous production equipment and preparation method
CN108640089A
Application of potassium persulfate in preparing potassium monopersulfate compound salt and preparation method of potassium monopersulfate compound salt
CN108849977A
Sodium hydrogen persulfate composite salt and preparation method thereof
CN115316400A
Class of stable potassium monopersulfate compositions
US5139763A