Vibration reduction rubber material and preparation method thereof

Through the synergistic effect of composite cell and modified glass flakes, the problem of mechanical properties degradation of rubber materials when improving vibration damping performance is solved, and a good vibration damping effect and mechanical properties balance is achieved, and the dynamic-static stiffness ratio reaches 1.04.

CN119060419AActive Publication Date: 2024-12-03ZHEJIANG YOUJU NEW MATERIAL TECHNOLOGY CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411037290.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-31
Publication Date
2024-12-03
Estimated Expiration
2044-07-31

AI Technical Summary

Technical Problem

While improving vibration damping performance, existing rubber vibration damping materials are prone to affect their mechanical properties, and simple micron-scale bubble cells are prone to form through holes, resulting in poor vibration damping effect.

Method used

Compound cell combined with modified glass flakes, nano- and micro-scale cell cells are prepared through ultrafine sodium bicarbonate particles and foaming agent H. The modified glass flakes are adsorbed with the surface energy of natural rubber to increase damping performance, and through modification The grafted polymer of the flakes makes it compatible with natural rubber, forming an overall network effect.

Benefits of technology

It achieves that the vibration damping effect is significantly improved without affecting the mechanical properties, and the dynamic and static stiffness ratio can be as low as 1.04, with good mechanical properties and vibration damping effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004971440170000041
    Figure BDA0004971440170000041
Patent Text Reader

Abstract

The invention provides a damping rubber material and a preparation method thereof. The preparation method comprises the following steps: starting an internal mixer, adding natural rubber, plastifying, adding a softening agent and a composite foaming agent, and mixing; adding a filling agent, continuously mixing after the torque is stable, and discharging rubber to obtain a section of rubber compound; after standing for 12 hours, starting the open mill, adding the rubber compound, after a covered roller is smooth, adding a vulcanization accelerator and sulfur, performing left and right cutting for three times, discharging sheets to obtain second-section rubber compound, and standing; and vulcanizing and foaming the second-stage rubber compound to obtain the product. The composite foam holes are combined with the modified glass flakes, so that the synergistic vibration reduction effect is achieved; the composite foam holes are formed by combining nano-scale foam holes and micron-scale foam holes and are prepared from superfine sodium bicarbonate particles and a foaming agent H, the micron-scale foam holes and the nano-scale foam holes are mixed, through holes are not prone to being formed, meanwhile, borne external force can be effectively diffused from the micron-scale foam holes to the nano-scale foam holes for digestion, and therefore the vibration reduction effect becomes good.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field The invention relates to the field of functional rubber, and in particular to a vibration-damping rubber material and a preparation method thereof. Background Art When an object is in a dynamic condition, as long as there is an unbalanced mass, it will inevitably vibrate, and vibration will inevitably generate noise. With the rapid development of modern industry, vibration and noise have become serious problems in various fields: it will reduce operating accuracy and affect product quality; shorten product life, make high-precision instruments unable to work properly; endanger safety, cause early damage to equipment or structures; pollute the environment and affect personal health; vibrations such as earthquakes even cause great damage to human life and property. Therefore, studying and mastering vibration control technology has become a major issue facing industrial development in various countries. The most fundamental and best way to eliminate vibration and noise is to reduce or eliminate the vibration of the vibration source. But in reality, it is impossible to completely eliminate the vibration of the vibration source. Therefore, other methods of controlling vibration must be adopted. The most widely used and effective method in practical application is to use various vibration reduction products, especially rubber vibration reduction products. It can effectively isolate vibration from the excitation source, and can also alleviate the vibration of the vibration rest. Therefore, it is widely used in the vibration isolation of power machinery and auxiliary equipment and instruments such as fans and water pumps in aircraft, vehicles, ships, etc. The characteristics of rubber are that it has both high elasticity and high viscosity, which makes it incomparable in terms of cushioning, vibration reduction and dynamic sealing. Rubber foam materials are conducive to impact deformation and have good vibration reduction effects. However, due to the foaming of the material, it is also easy to cause a decrease in its mechanical properties, thus limiting its application. Therefore, how to improve the vibration reduction performance of rubber materials without affecting its mechanical properties, or even improve its mechanical properties, is the key to current research. Summary of the invention

[0003] Technical problem to be solved: In view of the current technical problem of poor vibration damping of rubber, the present invention adopts composite pores in combination with modified glass flakes to achieve the vibration damping effect; the composite pores are a combination of nano-scale pores and micro-scale pores, which are prepared with ultrafine sodium bicarbonate particles and foaming agent H respectively. Simple micro-scale pores are easy to connect to form through holes, and the external force cannot be transmitted, resulting in poor vibration damping effect and affecting the mechanical properties. However, when composite pores are used, micro-pores and nano-pores are interspersed, and through holes are not easily formed. At the same time, the external force can be effectively diffused from the micro-pores to the nano-pores to be eliminated, thereby improving the vibration damping effect.

[0004] Technical solution: A vibration-damping rubber material, comprising the following components, by weight: 100 parts of natural rubber, 8-10 parts of filler, 5 parts of softener, 3-7 parts of composite foaming agent, 2 parts of sulfur and 1 part of vulcanization accelerator; The filler is modified glass flake. Furthermore, the preparation method of the modified glass flakes is: Step 1: Take ethyl acrylate and vinyl acetate, mix them thoroughly, and obtain a mixed monomer; Step 2: Add ammonium persulfate solution and stir for 5 minutes; Step 3: Add glass flakes, mix by ultrasonic for 5-10 minutes, place in a sealed container, heat to 65-75°C and react for 3 hours; Step 4: After the reaction is completed, centrifuge and dry in a vacuum drying oven to constant weight to obtain modified glass flakes. Furthermore, the mass ratio of ethyl acrylate to vinyl acetate is 4:5. Furthermore, the concentration of the ammonium persulfate solution is 9.0×10 -3 mol / L. Furthermore, the glass flakes have a size of 5-50 μm and a thickness of <400 nm. Furthermore, the mass ratio of the mixed monomer to the glass flakes is (1-4):50. Furthermore, the composite foaming agent is ultrafine sodium bicarbonate particles and foaming agent H in a mass ratio of (1-2):1. Furthermore, the ultrafine sodium bicarbonate particles have a particle size of 110-150 nm. Furthermore, the preparation method of the ultrafine sodium bicarbonate particles is, by weight: Step 1: Take 10 parts of sodium bicarbonate and 90 parts of water, stir to dissolve, add 0.5 parts of sodium dodecyl sulfate, stir to obtain a sodium bicarbonate solution; Step 2: Place 1000 parts of anhydrous ethanol in a stirrer, and add the sodium hydrogen carbonate solution into the anhydrous ethanol at a rate of 1 mL / min at a stirring speed of 1100-1200 rpm and a temperature of -5°C; Step 3: Vacuum filtration to separate the precipitate from the liquid and wash with anhydrous ethanol 2-3 times; Step 4: Dry the precipitate under vacuum at 40°C, take it out and grind it to obtain ultrafine sodium bicarbonate particles. The preparation method of the above-mentioned vibration-damping rubber material comprises the following steps: (1) Start the internal mixer, add natural rubber, plasticize for 1 min, add softener and composite foaming agent, and mix for 1 min; (2) Add filler, continue mixing for 5 minutes after the torque stabilizes, and discharge the rubber to obtain a mixed rubber; (3) After standing for 12 hours, start the mixing mill, add the mixed rubber, wait for the roller to be smooth, add the vulcanization accelerator and sulfur, cut the left and right knives 3 times, remove the sheet, obtain the second-stage mixed rubber, and stand for 2 hours; (4) The second-stage mixed rubber is vulcanized and foamed at 150°C for 10-15 minutes using a flat vulcanizer. Beneficial effects: 1. The present invention adopts composite pores combined with modified glass flakes to achieve a synergistic vibration reduction effect. 2. The composite pores in the present invention are a combination of nano-scale pores and micro-scale pores, which are prepared with ultrafine sodium bicarbonate particles and foaming agent H respectively. Simple micro-scale pores are easy to connect to form through holes, and the external force cannot be transmitted, so the vibration reduction effect is poor, and at the same time, it will also affect the mechanical properties. However, when composite pores are used, micro-pores and nano-pores are intermixed, and it is not easy to form through holes. At the same time, the external force can be effectively diffused from the micro-pores to the nano-pores to be digested, so that the vibration reduction effect is improved. 3. The present invention uses modified glass flakes, which are layered and can produce physical and chemical adsorption with natural rubber on their surface. When impacted by external force, the modified glass flakes can constrain the movement of the chain segments of natural rubber, change the conformation and orientation of nearby molecular chains, and widen the conformation distribution, thereby achieving a vibration reduction effect. In places where the natural rubber and the modified glass flake surface are not firmly adsorbed, relative slippage will occur between the polymer chain and the modified glass flake, which can increase the damping performance of the system. 4. The present invention modifies the glass flakes and grafts polymers to make their surface properties compatible with natural rubber, thereby improving their dispersibility in natural rubber and further improving the effect of their direct addition on the mechanical properties of natural rubber; at the same time, by modifying the glass flakes, the natural rubber can form an "overall network effect", which enables the vibration-damping rubber to have better mechanical properties. 5. The dynamic-static stiffness ratio of the vibration-damping rubber roller material of the present invention can be as low as 1.04, with good vibration-damping effect and good mechanical properties. DETAILED DESCRIPTION Example 1 The preparation method of modified glass flakes is: Step 1: Take 4 g of ethyl acrylate and 5 g of vinyl acetate, mix them thoroughly, and obtain a mixed monomer; Step 2: Add excess concentration of 9.0×10 -3 mol / L ammonium persulfate solution, stirring for 5 min; Step 3: Add 450g of glass flakes, mix ultrasonically for 5-10min, place in a sealed container, heat to 65-75℃ and react for 3h; the size of the glass flakes is 5-50μm and the thickness is <400nm; Step 4: After the reaction is completed, centrifuge and dry in a vacuum drying oven to constant weight to obtain modified glass flakes. Example 2 Step 1: Take 4 g of ethyl acrylate and 5 g of vinyl acetate, mix them thoroughly, and obtain a mixed monomer; Step 2: Add excess concentration of 9.0×10 -3 mol / L ammonium persulfate solution, stirring for 5 min; Step 3: Add 225g of glass flakes, mix ultrasonically for 5-10min, place in a sealed container, heat to 65-75℃ and react for 3h; the size of the glass flakes is 5-50μm and the thickness is <400nm; Step 4: After the reaction is completed, centrifuge and dry in a vacuum drying oven to constant weight to obtain modified glass flakes. Example 3 Step 1: Take 4 g of ethyl acrylate and 5 g of vinyl acetate, mix them thoroughly, and obtain a mixed monomer; Step 2: Add excess concentration of 9.0×10 -3 mol / L ammonium persulfate solution, stirring for 5 min; Step 3: Add 115g of glass flakes, mix ultrasonically for 5-10min, place in a sealed container, heat to 65-75℃ and react for 3h; the size of the glass flakes is 5-50μm and the thickness is <400nm; Step 4: After the reaction is completed, centrifuge and dry in a vacuum drying oven to constant weight to obtain modified glass flakes. The grafting rate was determined by the following calculation formula: Grafting rate (%) Example 1 80.4 Example 2 85.7 Example 3 86.3 Considering the grafting rate and the avoidance of resource waste, the modified glass flakes prepared in Example 2 were selected. Example 4 The preparation method of ultrafine sodium bicarbonate particles is as follows, by weight: Step 1: Take 10g of sodium bicarbonate and 90g of water, stir to dissolve, add 0.5g of sodium dodecyl sulfate, stir to obtain a sodium bicarbonate solution; Step 2: Place 1000 g of anhydrous ethanol in a stirrer, and add the sodium bicarbonate solution into the anhydrous ethanol at a rate of 1 mL / min at a stirring speed of 1100-1200 rpm and a temperature of -5°C; Step 3: Vacuum filtration to separate the precipitate from the liquid and wash with anhydrous ethanol three times; Step 4: The precipitate is placed in a vacuum dryer at 40°C, taken out, ground, and screened to obtain ultrafine sodium bicarbonate particles with a particle size of 110-150nm. Example 5 A method for preparing a vibration-damping rubber material comprises the following steps: (1) starting an internal mixer, adding 100 parts of natural rubber, plasticating for 1 minute, adding 5 parts of a softener and 3 parts of a composite foaming agent, wherein the composite foaming agent is ultrafine sodium bicarbonate particles and a foaming agent H in a mass ratio of 1.5:1, and mixing for 1 minute; (2) adding 9 parts of the modified glass flakes prepared in Example 2, and continuing to mix for 5 minutes after the torque stabilizes, and draining the rubber to obtain a mixed rubber; (3) After standing for 12 hours, start the mixing mill, add the mixed rubber, wait for the roller to be smooth, add 1 part of vulcanization accelerator M and 2 parts of sulfur, cut the left and right knives 3 times, remove the sheet, obtain the second-stage mixed rubber, and stand for 2 hours; (4) The second-stage mixed rubber is vulcanized and foamed at 150° C. for 13 minutes using a flat vulcanizer. Example 6 A method for preparing a vibration-damping rubber material comprises the following steps: (1) starting an internal mixer, adding 100 parts of natural rubber, plasticating for 1 minute, adding 5 parts of a softener and 5 parts of a composite foaming agent, wherein the composite foaming agent is ultrafine sodium bicarbonate particles and a foaming agent H in a mass ratio of 1.5:1, and mixing for 1 minute; (2) adding 9 parts of the modified glass flakes prepared in Example 2, and continuing to mix for 5 minutes after the torque stabilizes, and draining the rubber to obtain a mixed rubber; (3) After standing for 12 hours, start the mixing mill, add the mixed rubber, wait for the roller to be smooth, add 1 part of vulcanization accelerator M and 2 parts of sulfur, cut the left and right knives 3 times, remove the sheet, obtain the second-stage mixed rubber, and stand for 2 hours; (4) The second-stage mixed rubber is vulcanized and foamed at 150° C. for 13 minutes using a flat vulcanizer. Example 7 A method for preparing a vibration-damping rubber material comprises the following steps: (1) starting an internal mixer, adding 100 parts of natural rubber, plasticating for 1 minute, adding 5 parts of a softener and 7 parts of a composite foaming agent, wherein the composite foaming agent is ultrafine sodium bicarbonate particles and a foaming agent H in a mass ratio of 1.5:1, and mixing for 1 minute; (2) adding 9 parts of the modified glass flakes prepared in Example 2, and continuing to mix for 5 minutes after the torque stabilizes, and draining the rubber to obtain a mixed rubber; (3) After standing for 12 hours, start the mixing mill, add the mixed rubber, wait for the roller to be smooth, add 1 part of vulcanization accelerator M and 2 parts of sulfur, cut the left and right knives 3 times, remove the sheet, obtain the second-stage mixed rubber, and stand for 2 hours; (4) The second-stage mixed rubber is vulcanized and foamed at 150° C. for 13 minutes using a flat vulcanizer. Example 8 A method for preparing a vibration-damping rubber material comprises the following steps: (1) starting an internal mixer, adding 100 parts of natural rubber, plasticating for 1 minute, adding 5 parts of a softener and 5 parts of a composite foaming agent, wherein the composite foaming agent is ultrafine sodium bicarbonate particles and a foaming agent H in a mass ratio of 1:1, and mixing for 1 minute; (2) adding 9 parts of the modified glass flakes prepared in Example 2, and continuing to mix for 5 minutes after the torque stabilizes, and draining the rubber to obtain a mixed rubber; (3) After standing for 12 hours, start the mixing mill, add the mixed rubber, wait for the roller to be smooth, add 1 part of vulcanization accelerator M and 2 parts of sulfur, cut the left and right knives 3 times, remove the sheet, obtain the second-stage mixed rubber, and stand for 2 hours; (4) The second-stage mixed rubber is vulcanized and foamed at 150° C. for 13 minutes using a flat vulcanizer. Example 9 A method for preparing a vibration-damping rubber material comprises the following steps: (1) starting an internal mixer, adding 100 parts of natural rubber, plasticating for 1 minute, adding 5 parts of a softener and 5 parts of a composite foaming agent, wherein the composite foaming agent is ultrafine sodium bicarbonate particles and a foaming agent H in a mass ratio of 2:1, and mixing for 1 minute; (2) adding 9 parts of the modified glass flakes prepared in Example 2, and continuing to mix for 5 minutes after the torque stabilizes, and draining the rubber to obtain a mixed rubber; (3) After standing for 12 hours, start the mixing mill, add the mixed rubber, wait for the roller to be smooth, add 1 part of vulcanization accelerator M and 2 parts of sulfur, cut the left and right knives 3 times, remove the sheet, obtain the second-stage mixed rubber, and stand for 2 hours; (4) The second-stage mixed rubber is vulcanized and foamed at 150° C. for 13 minutes using a flat vulcanizer. Example 10 A method for preparing a vibration-damping rubber material comprises the following steps: (1) starting an internal mixer, adding 100 parts of natural rubber, plasticating for 1 minute, adding 5 parts of a softener and 5 parts of a composite foaming agent, wherein the composite foaming agent is ultrafine sodium bicarbonate particles and a foaming agent H in a mass ratio of 1.5:1, and mixing for 1 minute; (2) adding 8 parts of the modified glass flakes prepared in Example 2, and continuing to mix for 5 minutes after the torque stabilizes, and draining the rubber to obtain a mixed rubber; (3) After standing for 12 hours, start the mixing mill, add the mixed rubber, wait for the roller to be smooth, add 1 part of vulcanization accelerator M and 2 parts of sulfur, cut the left and right knives 3 times, remove the sheet, obtain the second-stage mixed rubber, and stand for 2 hours; (4) The second-stage mixed rubber is vulcanized and foamed at 150° C. for 13 minutes using a flat vulcanizer. Embodiment 11 A method for preparing a vibration-damping rubber material comprises the following steps: (1) starting an internal mixer, adding 100 parts of natural rubber, plasticating for 1 minute, adding 5 parts of a softener and 5 parts of a composite foaming agent, wherein the composite foaming agent is ultrafine sodium bicarbonate particles and a foaming agent H in a mass ratio of 1.5:1, and mixing for 1 minute; (2) adding 10 parts of the modified glass flakes prepared in Example 2, and continuing to mix for 5 minutes after the torque stabilizes, and draining the rubber to obtain a mixed rubber; (3) After standing for 12 hours, start the mixing mill, add the mixed rubber, wait for the roller to be smooth, add 1 part of vulcanization accelerator M and 2 parts of sulfur, cut the left and right knives 3 times, remove the sheet, obtain the second-stage mixed rubber, and stand for 2 hours; (4) The second-stage mixed rubber is vulcanized and foamed at 150° C. for 13 minutes using a flat vulcanizer. Example 12 A method for preparing a vibration-damping rubber material comprises the following steps: (1) starting an internal mixer, adding 100 parts of natural rubber, plasticating for 1 minute, adding 5 parts of a softener and 5 parts of a composite foaming agent, wherein the composite foaming agent is ultrafine sodium bicarbonate particles and a foaming agent H in a mass ratio of 1.5:1, and mixing for 1 minute; (2) adding 9 parts of the modified glass flakes prepared in Example 2, and continuing to mix for 5 minutes after the torque stabilizes, and draining the rubber to obtain a mixed rubber; (3) After standing for 12 hours, start the mixing mill, add the mixed rubber, wait for the roller to be smooth, add 1 part of vulcanization accelerator M and 2 parts of sulfur, cut the left and right knives 3 times, remove the sheet, obtain the second-stage mixed rubber, and stand for 2 hours; (4) The second-stage mixed rubber is vulcanized and foamed at 150°C for 10 minutes using a flat vulcanizer. Embodiment 13 A method for preparing a vibration-damping rubber material comprises the following steps: (1) starting an internal mixer, adding 100 parts of natural rubber, plasticating for 1 minute, adding 5 parts of a softener and 5 parts of a composite foaming agent, wherein the composite foaming agent is ultrafine sodium bicarbonate particles and a foaming agent H in a mass ratio of 1.5:1, and mixing for 1 minute; (2) adding 9 parts of the modified glass flakes prepared in Example 2, and continuing to mix for 5 minutes after the torque stabilizes, and draining the rubber to obtain a mixed rubber; (3) After standing for 12 hours, start the mixing mill, add the mixed rubber, wait for the roller to be smooth, add 1 part of vulcanization accelerator M and 2 parts of sulfur, cut the left and right knives 3 times, remove the sheet, obtain the second-stage mixed rubber, and stand for 2 hours; (4) The second-stage mixed rubber is vulcanized and foamed at 150°C for 15 minutes using a flat vulcanizer. The cell sizes of the above examples were measured, and the results showed that they were composite cells of nano-scale cells and micro-scale cells. The nano-scale cell size was 100-500 nm, and the micro-scale cell size was 30-300 μm. Comparative Example 1 The difference between this embodiment and embodiment 6 is that no composite foaming agent is used, and ultrafine sodium bicarbonate particles are used. Specifically: A method for preparing a vibration-damping rubber material comprises the following steps: (1) Start the internal mixer, add 100 parts of natural rubber, plasticize for 1 minute, add 5 parts of softener and 5 parts of ultrafine sodium bicarbonate particles, and mix for 1 minute; (2) adding 9 parts of the modified glass flakes prepared in Example 2, and continuing to mix for 5 minutes after the torque stabilizes, and draining the rubber to obtain a mixed rubber; (3) After standing for 12 hours, start the mixing mill, add the mixed rubber, wait for the roller to be smooth, add 1 part of vulcanization accelerator M and 2 parts of sulfur, cut the left and right knives 3 times, remove the sheet, obtain the second-stage mixed rubber, and stand for 2 hours; (4) The second-stage mixed rubber is vulcanized and foamed at 150° C. for 13 minutes using a flat vulcanizer. Comparative Example 2 The difference between this embodiment and embodiment 6 is that no composite foaming agent is used, and all foaming agents H are used, specifically: A method for preparing a vibration-damping rubber material comprises the following steps: (1) Start the internal mixer, add 100 parts of natural rubber, plasticize for 1 minute, add 5 parts of softener and 5 parts of foaming agent H, and mix for 1 minute; (2) adding 9 parts of the modified glass flakes prepared in Example 2, and continuing to mix for 5 minutes after the torque stabilizes, and draining the rubber to obtain a mixed rubber; (3) After standing for 12 hours, start the mixing mill, add the mixed rubber, wait for the roller to be smooth, add 1 part of vulcanization accelerator M and 2 parts of sulfur, cut the left and right knives 3 times, remove the sheet, obtain the second-stage mixed rubber, and stand for 2 hours; (4) The second-stage mixed rubber is vulcanized and foamed at 150° C. for 13 minutes using a flat vulcanizer. Comparative Example 3 The difference between this embodiment and embodiment 6 is that no modified glass flakes are added. Specifically: A method for preparing a vibration-damping rubber material comprises the following steps: (1) starting an internal mixer, adding 100 parts of natural rubber, masticating for 1 minute, adding 5 parts of a softener and 5 parts of a composite foaming agent, wherein the composite foaming agent is ultrafine sodium bicarbonate particles and a foaming agent H in a mass ratio of 1.5:1, mixing for 6 minutes, and draining the rubber to obtain a first-stage mixed rubber; (2) After standing for 12 hours, start the mixing mill, add the mixed rubber, wait for the roller to be smooth, add 1 part of vulcanization accelerator M and 2 parts of sulfur, cut the left and right knives 3 times, remove the sheet, obtain the second-stage mixed rubber, and stand for 2 hours; (3) The second-stage mixed rubber is vulcanized and foamed at 150°C for 13 minutes using a flat vulcanizer. Comparative Example 4 The difference between this embodiment and embodiment 6 is that unmodified glass flakes are added, specifically: A method for preparing a vibration-damping rubber material comprises the following steps: (1) starting an internal mixer, adding 100 parts of natural rubber, plasticating for 1 minute, adding 5 parts of a softener and 5 parts of a composite foaming agent, wherein the composite foaming agent is ultrafine sodium bicarbonate particles and a foaming agent H in a mass ratio of 1.5:1, and mixing for 1 minute; (2) Add 9 parts of glass flakes, continue mixing for 5 minutes after the torque stabilizes, and drain the rubber to obtain a mixed rubber; (3) After standing for 12 hours, start the mixing mill, add the mixed rubber, wait for the roller to be smooth, add 1 part of vulcanization accelerator M and 2 parts of sulfur, cut the left and right knives 3 times, remove the sheet, obtain the second-stage mixed rubber, and stand for 2 hours; (4) The second-stage mixed rubber is vulcanized and foamed at 150° C. for 13 minutes using a flat vulcanizer. Comparative Example 5 The difference between this embodiment and embodiment 6 is that the vulcanization foaming time is 5 minutes, specifically: A method for preparing a vibration-damping rubber material comprises the following steps: (1) starting an internal mixer, adding 100 parts of natural rubber, plasticating for 1 minute, adding 5 parts of a softener and 5 parts of a composite foaming agent, wherein the composite foaming agent is ultrafine sodium bicarbonate particles and a foaming agent H in a mass ratio of 1.5:1, and mixing for 1 minute; (2) adding 9 parts of the modified glass flakes prepared in Example 2, and continuing to mix for 5 minutes after the torque stabilizes, and draining the rubber to obtain a mixed rubber; (3) After standing for 12 hours, start the mixing mill, add the mixed rubber, wait for the roller to be smooth, add 1 part of vulcanization accelerator M and 2 parts of sulfur, cut the left and right knives 3 times, remove the sheet, obtain the second-stage mixed rubber, and stand for 2 hours; (4) The second-stage mixed rubber is vulcanized and foamed at 150°C for 5 minutes using a flat vulcanizer. Comparative Example 6 The difference between this embodiment and embodiment 6 is that the vulcanization foaming time is 20 minutes, specifically: A method for preparing a vibration-damping rubber material comprises the following steps: (1) starting an internal mixer, adding 100 parts of natural rubber, plasticating for 1 minute, adding 5 parts of a softener and 5 parts of a composite foaming agent, wherein the composite foaming agent is ultrafine sodium bicarbonate particles and a foaming agent H in a mass ratio of 1.5:1, and mixing for 1 minute; (2) adding 9 parts of the modified glass flakes prepared in Example 2, and continuing to mix for 5 minutes after the torque stabilizes, and draining the rubber to obtain a mixed rubber; (3) After standing for 12 hours, start the mixing mill, add the mixed rubber, wait for the roller to be smooth, add 1 part of vulcanization accelerator M and 2 parts of sulfur, cut the left and right knives 3 times, remove the sheet, obtain the second-stage mixed rubber, and stand for 2 hours; (4) The second-stage mixed rubber is vulcanized and foamed at 150°C for 20 minutes using a flat vulcanizer. The materials of each embodiment were prepared into samples of 50 mm × 50 mm × 40 mm, and their static properties were tested on a mechanical properties testing machine using the national standard method. Then, a vibration test was performed to obtain a frequency response function, test the dynamic stiffness and static stiffness of the material, and calculate its dynamic-static stiffness ratio. Table 1 Dynamic and static stiffness ratio of different embodiments Dynamic-static stiffness ratio Example 5 1.11 Example 6 1.04 Example 7 1.06 Example 8 1.06 Example 9 1.07 Example 10 1.10 Embodiment 11 1.08 Example 12 1.16 Example 13 1.06 Comparative Example 1 1.27 Comparative Example 2 1.20 Comparative Example 3 1.37 Comparative Example 4 1.15 Comparative Example 5 1.53 Comparative Example 6 1.11 The dynamic-static stiffness ratio is closely related to vibration transmission and vibration reduction effects. The smaller the dynamic-static stiffness ratio is, the better the resilience is and the better the vibration transmission effect is. The closer the value is to 1, the better the vibration transmission effect is and the better the vibration reduction is. The tensile strength and elongation at break were tested using a German electronic tensile testing machine in accordance with the national standard GB / T528-2009, with a tensile rate of 500 mm / min. The compression set was tested according to the national standard GB / T7759.1-2015, the test conditions were (70±1)°C, 24h, and the compression rate was 25%. Table 2 Mechanical properties of different embodiments Tensile strength(MPa) Elongation at break (%) Compression set (%) Example 5 21.42 530 17.9 Example 6 20.17 549 18.8 Example 7 18.49 525 18.5 Example 8 19.88 541 18.5 Example 9 20.03 536 18.9 Example 10 19.83 524 18.4 Embodiment 11 20.36 528 18.7 Example 12 20.56 537 17.3 Example 13 19.51 529 18.6 Comparative Example 1 20.39 552 18.3 Comparative Example 2 15.19 463 12.8 Comparative Example 3 17.96 501 17.9 Comparative Example 4 19.22 518 18.5 Comparative Example 5 20.56 530 17.0 Comparative Example 6 15.22 419 11.9

Claims

1. A vibration-damping rubber material, characterized in that: The composition comprises the following components in parts by weight: 100 parts of natural rubber, 8-10 parts of filler, 5 parts of softener, 3-7 parts of composite foaming agent, 2 parts of sulfur and 1 part of vulcanization accelerator; The filler is modified glass flake.

2. A vibration-damping rubber material according to claim 1, characterized in that: The preparation method of the modified glass flakes is: Step 1: Take ethyl acrylate and vinyl acetate, mix them thoroughly, and obtain a mixed monomer; Step 2: Add ammonium persulfate solution and stir for 5 minutes; Step 3: Add glass flakes, mix by ultrasonic for 5-10 minutes, place in a sealed container, heat to 65-75°C and react for 3 hours; Step 4: After the reaction is completed, centrifuge and dry in a vacuum drying oven to constant weight to obtain modified glass flakes.

3. A vibration-damping rubber material according to claim 2, characterized in that: The mass ratio of ethyl acrylate to vinyl acetate is 4:

5.

4. The vibration-damping rubber material according to claim 2, characterized in that: The concentration of the ammonium persulfate solution is 9.0×10 -3 mol / L.

5. The vibration-damping rubber material according to claim 2, characterized in that: The glass flakes have a size of 5-50 μm and a thickness of <400 nm.

6. The vibration-damping rubber material according to claim 2, characterized in that: The mass ratio of the mixed monomer to the glass flakes is (1-4):

50.

7. The vibration-damping rubber material according to claim 1, characterized in that: The composite foaming agent is ultrafine sodium bicarbonate particles and foaming agent H in a mass ratio of (1-2):

1.

8. The vibration-damping rubber material according to claim 7, characterized in that: The particle size of the ultrafine sodium bicarbonate particles is 110-150 nm.

9. The vibration-damping rubber material according to claim 7, characterized in that: The preparation method of the ultrafine sodium bicarbonate particles is, by weight: Step 1: Take 10 parts of sodium bicarbonate and 90 parts of water, stir to dissolve, add 0.5 parts of sodium dodecyl sulfate, stir to obtain a sodium bicarbonate solution; Step 2: Place 1000 parts of anhydrous ethanol in a stirrer, and add the sodium hydrogen carbonate solution into the anhydrous ethanol at a rate of 1 mL / min at a stirring speed of 1100-1200 rpm and a temperature of -5°C; Step 3: Vacuum filtration to separate the precipitate from the liquid and wash with anhydrous ethanol 2-3 times; Step 4: Dry the precipitate under vacuum at 40°C, take it out and grind it to obtain ultrafine sodium bicarbonate particles.

10. A method for preparing a vibration-damping rubber material according to any one of claims 1 to 9, characterized in that: The following steps are involved: (1) Start the internal mixer, add natural rubber, plasticize for 1 min, add softener and composite foaming agent, and mix for 1 min; (2) Add filler, continue mixing for 5 minutes after the torque stabilizes, and discharge the rubber to obtain a mixed rubber; (3) After standing for 12 hours, start the mixing mill, add the mixed rubber, wait for the roller to be smooth, add the vulcanization accelerator and sulfur, cut the left and right knives 3 times, remove the sheet, obtain the second-stage mixed rubber, and stand for 2 hours; (4) The second-stage mixed rubber is vulcanized and foamed at 150°C for 10-15 minutes using a flat vulcanizer.

Citation Information

Patent Citations

  • Preparation method for carboxyl-terminated nitrilo butadiene rubber coated and modified glass flakes

    CN105315745A

  • Preparation method of inflation latex

    CN106380642A

  • High-temperature-resistant low-compression permanent deformation hydrogenated butadiene-acrylonitrile rubber

    CN116804097A

  • Rubber composition and vulcanized rubber

    JP2007099942A