Maintenance optimization method for highway major and medium repair asphalt pavement

By assessing road conditions through PCI and SSI indexes and applying targeted maintenance measures, the method optimizes asphalt pavement maintenance, extending service life and reducing costs.

CN119067253APending Publication Date: 2024-12-03ANHUI STAR CONSTR ENG CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411101630.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-12
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

Traditional asphalt pavement maintenance methods lack comprehensive understanding of road conditions and targeted maintenance measures, leading to inefficiencies in extending the service life and increasing maintenance costs.

Method used

Conduct road disease surveys to assess PCI and SSI indexes, segment roads based on these indexes, and apply targeted maintenance measures such as daily, medium, or major repairs to improve load-bearing capacity, and include quality inspections to ensure effectiveness.

Benefits of technology

Enhances the service life of asphalt pavements, reduces maintenance costs, and improves economic and social benefits by ensuring targeted and effective maintenance strategies.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119067253A_ABST
    Figure CN119067253A_ABST
Patent Text Reader

Abstract

The invention discloses a highway major and medium repair asphalt pavement maintenance optimization method, which comprises the following steps: carrying out disease investigation on a highway, and evaluating a PCI (Peripheral Component Interconnect) index; detecting the pavement strength, and calculating a pavement strength index SSI; according to the evaluation results of the PCI index and the SSI index, the damage condition and the bearing capacity of the pavement are determined; reasonably segmenting the old road according to an evaluation result; dividing the road surface into different paragraphs according to the PCI index and the SSI index; daily maintenance measures are taken for the paragraph with the high PCI index and the high SSI index; for the paragraphs with low PCI indexes and SSI indexes, targeted major and medium repair and maintenance measures are taken; the method has the beneficial effects that the service life of the pavement is effectively prolonged by comprehensively knowing the damage condition and the bearing capacity of the pavement and taking targeted maintenance measures; meanwhile, maintenance cost is reduced, and economic and social benefits are improved; the method is simple and convenient to operate, and can be widely applied to major and medium repair asphalt pavement maintenance projects of various highways.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of asphalt pavement maintenance, and in particular relates to an optimization method for asphalt pavement maintenance during major or medium-sized highway repairs. Background Art

[0002] In the specific process of highway pavement construction, asphalt roads have extremely significant practical advantages. They have a high degree of continuity during use and are a type of seamless pavement. In the process of its construction, it has relatively solid and flat practical characteristics, and its own driving comfort is relatively strong. However, in the long-term operation of the highway, the components of the retrograde pavement are simply subject to a certain degree of practical damage. Therefore, the construction unit needs to have a more scientific maintenance awareness and extremely excellent maintenance plans during the progress process, and reasonably apply the construction technology effectively, and then carry out comprehensive repair and maintenance of the project pavement, thereby greatly reducing the degree of damage to the asphalt pavement.

[0003] In highway construction, asphalt pavement is widely used because of its good wear resistance, anti-skid, noise reduction and other properties; as time goes by, various diseases will appear on the asphalt pavement, such as cracks, rutting, looseness, etc., which affect the use function and safety of the road; in order to keep the road surface in good condition, major and medium repairs are required; however, traditional maintenance methods have certain limitations, such as lack of comprehensive understanding of road conditions and lack of targeted maintenance measures. Summary of the invention

[0004] The purpose of the present invention is to provide a method for optimizing the maintenance of asphalt pavement during major and medium-sized highway repairs, so as to improve the road use function, extend the service life of the pavement, reduce the maintenance cost, and improve the economic and social benefits.

[0005] To achieve the above-mentioned purpose, the present invention provides the following technical solution: a method for optimizing the maintenance of asphalt pavement during major and medium-sized highway repairs, the optimization method being as follows:

[0006] Conduct road disease surveys and assess PCI indexes;

[0007] Test the pavement strength and calculate the pavement strength index (SSI); determine the pavement damage and bearing capacity based on the evaluation results of the PCI and SSI indexes;

[0008] According to the evaluation results, the old road is reasonably segmented; the road surface is divided into different sections according to the size of the PCI index and SSI index; for sections with higher PCI and SSI indexes, daily maintenance measures are taken; for sections with lower PCI and SSI indexes, targeted major and medium maintenance measures are taken;

[0009] For expressways and first-class highways with PCI ratings of excellent or good, routine maintenance is the main method, with minor repairs to local damage.

[0010] For expressways and first-class highways where the PCI is rated as medium or below, medium repair and overlay measures should be adopted;

[0011] For roads at or below the second level, where the road condition index is rated as inferior or below, if the strength requirements are not met, major repair measures should be taken to improve the load-bearing capacity;

[0012] Carry out quality inspection and acceptance on maintained roads to ensure that the maintenance results achieve the expected goals.

[0013] As a preferred technical solution of the present invention, the evaluation results are divided into five standards: "excellent, good, medium, poor, and bad".

[0014] As a preferred technical solution of the present invention, for expressways and first-class highways with a pavement condition index PCI evaluation of excellent or good, daily maintenance is mainly carried out, and minor repairs are performed on local damage. Specific measures include clearing debris on the road surface and repairing small areas of damage.

[0015] As a preferred technical solution of the present invention, medium repair and overlay measures are adopted, and specific measures include milling the damaged road surface and laying a new asphalt concrete layer.

[0016] As a preferred technical solution of the present invention, major repair and strengthening measures are taken to improve its bearing capacity. Specific measures include rebuilding seriously damaged sections and strengthening the base structure.

[0017] As a preferred technical solution of the present invention, the specific method for conducting a road disease survey and evaluating the PCI index is as follows:

[0018] Inspect the road surface to see if there are cracks, potholes, or rutting problems;

[0019] Use distance meter and ruler tools to measure the length, width and depth of cracks, as well as the depth and extent of potholes and rutting;

[0020] Assess the degree of pavement damage, record the type and degree of damage, and score it according to the PCI index standards;

[0021] According to the scoring results, the PCI index is divided into different levels;

[0022] Analyze the results of PCI index assessment to determine the main causes of road damage;

[0023] According to the analysis results, formulate corresponding maintenance measures;

[0024] Re-inspect the road surface regularly, observe the effectiveness of maintenance measures, and make necessary adjustments and improvements.

[0025] As a preferred technical solution of the present invention, the main reasons for road damage are determined to include material aging, excessive traffic flow, and heavy-loaded vehicles.

[0026] As a preferred technical solution of the present invention, the specific method for quality inspection and acceptance of the maintained highway is as follows:

[0027] Appearance inspection: Observe whether the road surface is flat, without cracks or obvious damage;

[0028] Thickness detection: Use a thickness gauge to detect the pavement thickness to ensure that the pavement thickness after maintenance meets the design requirements;

[0029] Compactness test: Through the compaction test, check whether the compaction of the road surface meets the standard requirements;

[0030] Friction coefficient test: Use a friction coefficient tester to test the friction coefficient of the road surface to ensure that the road surface has sufficient friction;

[0031] Drainage performance test: Check whether the drainage performance of the road surface is good to ensure that there is no water accumulation on the road surface;

[0032] Traffic carrying capacity test: Through heavy-load vehicle tests, test whether the road surface can withstand the expected traffic load;

[0033] Structural strength test: Through the structural strength test, check whether the structural strength of the road surface meets the design requirements;

[0034] Acceptance review: Based on the above test results, an acceptance review will be conducted on the maintained highway to assess whether it has achieved the expected maintenance effect.

[0035] Compared with the prior art, the present invention has the following beneficial effects:

[0036] By fully understanding the damage and bearing capacity of the road surface, targeted maintenance measures can be taken to effectively extend the service life of the road surface; at the same time, maintenance costs can be reduced and economic and social benefits can be improved;

[0037] The method is easy to operate and can be widely used in major and medium-sized asphalt pavement maintenance projects of various types of highways. BRIEF DESCRIPTION OF THE DRAWINGS

[0038] Figure 1 It is a flow chart of the maintenance optimization method of the present invention. DETAILED DESCRIPTION

[0039] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0040] Example 1

[0041] See also Figure 1 , which is the first embodiment of the present invention, provides a method for optimizing the maintenance of asphalt pavement during major or medium-sized highway repairs, comprising the following steps:

[0042] Conduct road disease surveys and assess PCI indexes;

[0043] Test the pavement strength and calculate the pavement strength index (SSI); determine the pavement damage and bearing capacity based on the evaluation results of the PCI and SSI indexes;

[0044] According to the evaluation results, the old road is reasonably segmented; the road surface is divided into different sections according to the size of the PCI index and SSI index; for sections with higher PCI and SSI indexes, daily maintenance measures are taken; for sections with lower PCI and SSI indexes, targeted major and medium maintenance measures are taken;

[0045] For expressways and first-class highways with PCI ratings of excellent or good, routine maintenance is the main method, with minor repairs to local damage.

[0046] For expressways and first-class highways where the PCI is rated as medium or below, medium repair and overlay measures should be adopted;

[0047] For roads at or below the second level, where the road condition index is rated as inferior or below, if the strength requirements are not met, major repair measures should be taken to improve the load-bearing capacity;

[0048] Carry out quality inspection and acceptance on maintained roads to ensure that the maintenance results achieve the expected goals.

[0049] Example 2

[0050] See also Figure 1 , which is the second embodiment of the present invention, provides a method for optimizing the maintenance of asphalt pavement during major or medium-sized highway repairs, comprising the following steps:

[0051] Conduct road disease surveys and assess PCI indexes;

[0052] Test the pavement strength and calculate the pavement strength index (SSI); determine the pavement damage and bearing capacity based on the evaluation results of the PCI and SSI indexes;

[0053] According to the evaluation results, the old road is reasonably segmented; the road surface is divided into different sections according to the size of the PCI index and SSI index; for sections with higher PCI and SSI indexes, daily maintenance measures are taken; for sections with lower PCI and SSI indexes, targeted major and medium maintenance measures are taken;

[0054] For expressways and first-class highways with PCI ratings of excellent or good, routine maintenance is the main method, with minor repairs to local damage.

[0055] For expressways and first-class highways where the PCI is rated as medium or below, medium repair and overlay measures should be adopted;

[0056] For roads at or below the second level, where the road condition index is rated as inferior or below, if the strength requirements are not met, major repair measures should be taken to improve the load-bearing capacity;

[0057] Carry out quality inspection and acceptance on maintained roads to ensure that the maintenance results achieve the expected goals.

[0058] In this embodiment, preferably, the evaluation results are divided into five standards: "excellent, good, fair, poor, and bad".

[0059] In this embodiment, preferably, for expressways and first-class highways with a pavement condition index PCI evaluation of excellent or good, daily maintenance is mainly carried out, and minor repairs are performed on local damage. Specific measures include clearing debris from the road surface and repairing small areas of damage.

[0060] In this embodiment, preferably, medium repair and overlay measures are taken, and specific measures include milling the damaged road surface and laying a new asphalt concrete layer.

[0061] In this embodiment, preferably, major repair measures are taken to improve its bearing capacity. Specific measures include rebuilding severely damaged sections and strengthening the base structure.

[0062] In this embodiment, preferably, the specific method of conducting a road disease survey and evaluating the PCI index is as follows:

[0063] Inspect the road surface to see if there are cracks, potholes, or rutting problems;

[0064] Use distance meter and ruler tools to measure the length, width and depth of cracks, as well as the depth and extent of potholes and rutting;

[0065] Assess the degree of pavement damage, record the type and degree of damage, and score it according to the PCI index standards;

[0066] According to the scoring results, the PCI index is divided into different levels;

[0067] Analyze the results of PCI index assessment to determine the main causes of road damage;

[0068] According to the analysis results, formulate corresponding maintenance measures;

[0069] Re-inspect the road surface regularly, observe the effectiveness of maintenance measures, and make necessary adjustments and improvements.

[0070] In this embodiment, preferably, the main reasons for determining the road surface damage include material aging, excessive traffic flow, and heavy-loaded vehicles.

[0071] In this embodiment, preferably, the specific method for quality inspection and acceptance of the maintained highway is as follows:

[0072] Appearance inspection: Observe whether the road surface is flat, without cracks or obvious damage;

[0073] Thickness detection: Use a thickness gauge to detect the pavement thickness to ensure that the pavement thickness after maintenance meets the design requirements;

[0074] Compactness test: Through the compaction test, check whether the compaction of the road surface meets the standard requirements;

[0075] Friction coefficient test: Use a friction coefficient tester to test the friction coefficient of the road surface to ensure that the road surface has sufficient friction;

[0076] Drainage performance test: Check whether the drainage performance of the road surface is good to ensure that there is no water accumulation on the road surface;

[0077] Traffic carrying capacity test: Through heavy-load vehicle tests, test whether the road surface can withstand the expected traffic load;

[0078] Structural strength test: Through the structural strength test, check whether the structural strength of the road surface meets the design requirements;

[0079] Acceptance review: Based on the above test results, an acceptance review will be conducted on the maintained highway to assess whether it has achieved the expected maintenance effect.

[0080] The cracks on the road surface can be effectively repaired by means of sealant. During the application process, the sealant is composed of polymer materials with outstanding adhesion. The corresponding materials are improved on the basis of rubber and can fully produce high-quality adhesion with asphalt. Therefore, it is a common practical material in the process of repairing cracks. The equipment used for effective repair by sealant is mainly grooving machine and sealant machine. After the grooving machine is used to open the road surface, it is effectively cleaned, and then the sealant material is preheated, and the material is completely embedded in the cracks, etc. After it is thoroughly dried, vehicles can be allowed to pass; effective grouting work is carried out through the slurry sealing material. After the cracks are cleaned, the slurry sealing material can be fully stirred and filled into the corresponding cracks, and then the overall cracks can be effectively leveled and compacted; after 20 minutes of demulsification, traffic can be opened. For relatively mild cracks, the physical sealing method can be applied. The corresponding method is mostly used for crack prevention projects during the application process; at the same time, maintenance using this method can effectively improve the overall waterproof function of the asphalt pavement, and greatly increase the durability and anti-skid performance of the pavement.

[0081] Different measures should be taken to deal with the aging of asphalt pavements according to the degree of aging in different regions. In areas with serious aging, the maintenance period should be shortened. For most aging problems, the most important thing is to strengthen process technology and engineering technology, and scientifically improve the configuration of asphalt. In the process of secondary utilization of aged asphalt, technology should be strengthened to avoid the re-aging of asphalt. During the construction process, the thickness and density of asphalt paving should be reasonably configured in combination with local road conditions and regional climate. Finally, advanced detection methods and monitoring technologies should be used to detect the entire road condition during the use of asphalt roads, and timely remedies should be made for aging pavements.

[0082] For the repair of oil spills on asphalt pavement, the most fundamental thing is to pay attention to the qualified configuration ratio of asphalt raw materials, so that its adhesion meets the standard and avoids the isolation of aggregate and asphalt; pay attention to the cleanliness of the road surface when paving the road, and pay attention to the flatness and uniformity of the asphalt during the asphalt spraying process to avoid leakage and uneven thickness;

[0083] Optimize the configuration of asphalt and adopt suitable asphalt mixture to enhance its adhesion and adhesion. Add anti-stripping agent in appropriate proportion to the asphalt to reduce the degree of stripping to the maximum extent possible. Finally, pay attention to the ratio of gaps between the asphalt skeletons. Appropriate gaps are more conducive to the smoothness of the asphalt pavement.

[0084] Although the embodiments of the present invention have been shown and described, as detailed above, it will be understood by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A method for optimizing maintenance of asphalt pavement during major or medium highway repairs, characterized in that: The optimization method is as follows: Conduct road disease surveys and assess PCI indexes; Test the pavement strength and calculate the pavement strength index (SSI); determine the pavement damage and bearing capacity based on the evaluation results of the PCI and SSI indexes; According to the evaluation results, the old road is divided into reasonable sections; According to the size of the PCI index and the SSI index, the road surface is divided into different sections; for sections with higher PCI and SSI indexes, daily maintenance measures are taken; for sections with lower PCI and SSI indexes, targeted major and medium maintenance measures are taken; For expressways and first-class highways with PCI ratings of excellent or good, routine maintenance is the main method, with minor repairs to local damage. For expressways and first-class highways where the PCI is rated as medium or below, medium repair and overlay measures should be adopted; For roads at or below the second level, where the road condition index is rated as inferior or below, if the strength requirements are not met, major repair measures should be taken to improve the load-bearing capacity; Carry out quality inspection and acceptance on maintained roads to ensure that the maintenance results achieve the expected goals.

2. The method for optimizing maintenance of asphalt pavement during major or medium highway repairs according to claim 1 is characterized by: The evaluation results are divided into five standards: "excellent, good, medium, poor, and poor".

3. The method for optimizing maintenance of asphalt pavement during major or medium highway repairs according to claim 1 is characterized by: For expressways and first-class highways with a PCI rating of excellent or good, daily maintenance is the main approach, with minor repairs to local damage. Specific measures include clearing debris from the road surface and repairing small areas of damage.

4. The method for optimizing maintenance of asphalt pavement during major or medium highway repairs according to claim 1 is characterized by: Take medium-term repair and overlay measures, which include milling the damaged road surface and laying a new asphalt concrete layer.

5. The method for optimizing maintenance of asphalt pavement during major or medium highway repairs according to claim 1 is characterized by: Major repair measures are taken to improve its carrying capacity. Specific measures include rebuilding severely damaged sections and strengthening the basic structure.

6. The method for optimizing maintenance of asphalt pavement during major or medium highway repairs according to claim 1 is characterized by: The specific methods for investigating highway damage and evaluating the PCI index are as follows: Inspect the road surface to see if there are cracks, potholes, or rutting problems; Use distance meter and ruler tools to measure the length, width and depth of cracks, as well as the depth and extent of potholes and rutting; Assess the degree of road damage, record the type and degree of damage, and score it according to the PCI index standards; According to the scoring results, the PCI index is divided into different levels; Analyze the results of PCI index assessment to determine the main causes of road damage; According to the analysis results, formulate corresponding maintenance measures; Re-inspect the road surface regularly, observe the effectiveness of maintenance measures, and make necessary adjustments and improvements.

7. The method for optimizing maintenance of asphalt pavement during major or medium highway repairs according to claim 6 is characterized by: The main reasons for road deterioration were determined to include material aging, heavy traffic flow, and heavy-loaded vehicles.

8. The method for optimizing maintenance of asphalt pavement during major or medium highway repairs according to claim 1 is characterized by: The specific methods for quality inspection and acceptance of maintained roads are as follows: Appearance inspection: Observe whether the road surface is flat, without cracks or obvious damage; Thickness detection: Use a thickness gauge to detect the pavement thickness to ensure that the pavement thickness after maintenance meets the design requirements; Compactness test: Through the compaction test, check whether the compaction of the road surface meets the standard requirements; Friction coefficient test: Use a friction coefficient tester to test the friction coefficient of the road surface to ensure that the road surface has sufficient friction; Drainage performance test: Check whether the drainage performance of the road surface is good to ensure that there is no water accumulation on the road surface; Traffic carrying capacity test: Through heavy-load vehicle tests, test whether the road surface can withstand the expected traffic load; Structural strength test: Through the structural strength test, check whether the structural strength of the road surface meets the design requirements; Acceptance review: Based on the above test results, an acceptance review will be conducted on the maintained highway to assess whether it has achieved the expected maintenance effect.

Citation Information

Cited By

  • Method for selecting segmented maintenance strategy of asphalt pavement

    CN121412808A