Sampling branch circuit board and welding quality confirmation method
By designing the three-layer FPC structure and welding area characteristics of the sampling branch circuit board, the welding quality is confirmed by using the tin crawling state, the problems of false welding and safety risks during the welding process of the new energy FFC sampling line are solved, and efficient welding quality confirmation and Improved welding reliability.
Patent Information
- Application Number
- CN202411388803.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-30
- Publication Date
- 2024-12-03
AI Technical Summary
New energy FFC sampling lines are prone to false welding problems during welding, and the welding quality is difficult to confirm through appearance, which poses a high safety risk.
Design a sampling branch circuit board, adopting a three-layer FPC structure, including a sten zone, a stencil zone and a soldering zone, and form multiple sampling branch pad groups through the window opening process, and set tin-enameled holes and semicircular holes in the soldering zone. , use the tin crawling state to confirm the welding quality, combine the S-shaped structure buffer and the fuse to ensure welding reliability.
Through visual inspection of the tin crawling state, the occurrence of dummy welding is significantly reduced, the safety risks caused by poor welding quality during energy storage batteries are reduced, and the welding success rate and reliability are improved.
Smart Images

Figure CN119069967A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of new energy FFC sampling line manufacturing, and in particular to a sampling branch circuit board and a welding quality confirmation method. Background Art
[0002] In the new energy FFC sampling line, when the sampling branch is connected to the FFC sampling body by soldering, due to the characteristics of the welding process, the problem of cold soldering will occur, and the branch is soldered at the bottom, and the welding quality is difficult to confirm from the appearance, which poses a high safety risk. Therefore, a product that can confirm the welding quality by the solder creeping state is invented. Summary of the invention
[0003] The present invention aims to provide a sampling branch circuit board and a welding quality confirmation method, which can conveniently and effectively confirm the welding quality when the sampling branch circuit board is welded and connected with an FFC sampling body.
[0004] Based on the first aspect of the present invention, the following technical solution is provided:
[0005] A sampling branch circuit board adopts a three-layer FPC structure consisting of an upper insulating layer, a circuit layer and a lower insulating layer, including an FPC sampling body welding area and a battery busbar welding area located at both ends of the sampling branch circuit board; a plurality of sampling branch pad groups are formed in the FPC sampling body welding area through a window opening process, and the position of each sampling branch pad group corresponds to a branch connection pad of the FPC sampling body; each group of the sampling branch pad groups includes a tin-adding area located in the middle of the front side of the sampling branch circuit board and tin-climbing areas on both sides of the front side, and a welding area located on the back side of the sampling branch circuit board; the welding area extends to the edges of both sides of the FPC sampling body welding area, and the tin-adding area is provided with at least one tin-enameling hole penetrating to the welding area; each of the tin-climbing areas is provided with a semicircular hole penetrating to the welding area at the edge of the FPC sampling body welding area.
[0006] Furthermore, the sampling branch pad group is distributed in parallel in the FPC sampling body welding area; in the sampling branch pad group, the widths of the tin adding area, the tin creeping area and the welding area are equal.
[0007] Furthermore, the widths of the sampling branch pad groups are equal, and the center distances between adjacent sampling branch pad groups are equal.
[0008] Furthermore, the length of the welding zone is 3 mm to 15 mm, and the width is 0.5 mm to 1.5 mm; the center distance between adjacent welding zones is 1 mm to 2 mm.
[0009] Furthermore, the distance between the tin creeping area and the tin adding area is not less than 0.3 mm.
[0010] Furthermore, the sampling branch circuit board also includes a fool-proof positioning area in the middle, and the fool-proof positioning area is arranged adjacent to the battery busbar welding area and is used for welding alignment of the sampling branch circuit board and the battery pack busbar.
[0011] Furthermore, the fool-proof positioning structure of the fool-proof positioning area is a positioning hole.
[0012] Furthermore, the length of the welding area is 3mm to 15mm; the width is 0.5mm to 1.5mm; the center distance between adjacent welding areas is 1mm to 2mm; and the distance between the tin creeping area and the tin adding area is not less than 0.3mm.
[0013] Furthermore, the sampling branch circuit board also includes an S-shaped structural buffer in the middle for flexibly connecting the FPC sampling body welding area and the battery busbar welding area; in the S-shaped structural buffer, gaps are arranged between the two side edges of its circuit layer and the two side edges of the upper insulating layer and the lower insulating layer; micro-connection points are arranged at both turning areas of the S-shaped structural buffer, and there is no circuit layer at the micro-connection points. The S-shaped structural buffer forms a double-point connection with the FPC sampling body welding area and the battery busbar welding area through its end points and the micro-connection points; when the micro-connection point is disconnected, the sampling branch circuit board adapts to the distance change between the FPC sampling body welding area and the battery busbar welding area through the stretching of the S-shaped structural buffer.
[0014] Furthermore, a fuse is provided in the circuit layer between the two turning areas of the S-shaped structure buffer zone.
[0015] Furthermore, the blown fuse adopts a serpentine structure.
[0016] Furthermore, the line width of the blown fuse is 0.05 mm to 0.2 mm.
[0017] Furthermore, the sampling branch circuit board also includes a fool-proof positioning area in the middle, and the fool-proof positioning area is arranged adjacent to the battery busbar welding area, and is provided with a fool-proof positioning structure for welding and aligning the sampling branch circuit board and the battery pack busbar.
[0018] Furthermore, the fool-proof positioning structure is a positioning hole.
[0019] Furthermore, the battery busbar welding area is a double-sided welding pad or a single-sided welding pad, and the single-sided welding pad is formed by removing the lower insulating layer of the battery busbar welding area.
[0020] Based on the second aspect of the present invention, the following technical solution is provided:
[0021] A method for confirming the welding quality of a sampling branch circuit board uses the sampling branch circuit board as described above; and comprises the following steps:
[0022] Adjust the relative positions of the sampling branch circuit board and the FPC sampling body so that a group of front pads on the sampling branch circuit board and a branch connection pad on the FPC sampling body are aligned;
[0023] Adding tin to the tin adding area of the front solder pad by a printing process or a tinning process;
[0024] Performing a soldering operation, heating and melting the tin, allowing the tin to fully flow, flowing through the tinning holes on the tinning area to the soldering area on the back of the tinning area, and then flowing through the gap between the soldering area and the branch connection pad to the soldering area of the front pad;
[0025] When the tin is observed to flow to the tin creeping areas on both sides, the welding quality is considered qualified and heating is stopped to complete the welding.
[0026] By adopting the sampling branch circuit board of the present invention, the welding quality can be conveniently confirmed through the tin creeping state, which can greatly reduce the occurrence of cold solder joints and greatly reduce the safety risks caused by cold solder joints when the energy storage battery is working. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 It is a side view of a schematic diagram of the structure of a flexible circuit board of a sampling branch circuit board of the present invention;
[0028] Figure 2 It is a schematic diagram of the circuit layer structure of the sampling branch circuit board of the present invention;
[0029] Figure 3 is a front view of the sampling branch circuit board of the present invention;
[0030] Figure 4 is a back view of the sampling branch circuit board of the present invention;
[0031] Figure 5 It is a structural diagram of the FPC sampling body;
[0032] Figure 6 It is a schematic diagram of welding of the sampling branch circuit board and the FPC sampling body of the present invention. DETAILED DESCRIPTION
[0033] To further illustrate the various embodiments, the present invention provides drawings. These drawings are part of the disclosure of the present invention, which are mainly used to illustrate the embodiments and can be used in conjunction with the relevant descriptions in the specification to explain the operating principles of the embodiments. With reference to these contents, a person of ordinary skill in the art should be able to understand other possible implementations and advantages of the present invention. The components in the figures are not drawn to scale, and similar component symbols are generally used to represent similar components.
[0034] The present invention will now be further described with reference to the accompanying drawings and specific implementation methods.
[0035] like Figures 1 to 4 As shown, the present invention provides a sampling branch circuit board 100. The sampling branch circuit board 100 adopts a three-layer structure, including a circuit layer 2, and an upper insulating layer 1 and a lower insulating layer 3 attached to the front and back of the circuit layer 2 respectively.
[0036] This sampling branch circuit board 100 is a universal sampling branch circuit board. For each battery pack, an FPC sampling body 200 and multiple identical sampling branch circuit boards 100 are welded to connect each sampling branch circuit board 100 and each sampling line on the FPC sampling body 200, so as to obtain the battery pack busbar voltage and upload it.
[0037] In this embodiment, the sampling branch circuit board 100 is divided by function, including the FPC sampling body welding area 110 and the battery busbar welding area 140 at both ends, and the S-shaped structure buffer area 120 and the foolproof positioning area 130 in the middle. The circuit layer 2 is a copper foil layer, and an irregular electrode sheet is formed by etching and other processes. The electrode sheet extends from the FPC sampling body welding area to the battery busbar welding area 140.
[0038] 1. FFC sampling body welding area 110
[0039] The FFC sampling body welding area 110 is provided with a plurality of sampling branch pad groups 110a, ..., 110n. Each sampling branch pad group 110a, ..., 110n includes a tinning area 111 located in the middle of the front of the sampling branch circuit board 100, tin creeping areas 112, 113 on both sides of the front, and a welding area 114 located on the back of the sampling branch circuit board 100; the welding area 114 extends to the edges of both sides of the FPC sampling body welding area 110, and the tinning area 111 is provided with at least one tinning hole 115 penetrating to the welding area; each tin creeping area 112, 113 is provided with a semicircular hole 116, 117 penetrating to the welding area at the edge of the FPC sampling body welding area.
[0040] Preferably, each sampling branch pad group is distributed in parallel in the FPC sampling body welding area 110, and each sampling branch pad group has equal structural dimensions in all aspects. For each sampling branch pad group 110a, ..., 110n, the width of the tinning area 111, the tin climbing area 112, 113 and the welding area 114 is equal, and the width is 0.5mm to 1.5mm. The length of each group of pads is 3mm to 15mm, and the center spacing of adjacent sampling branch pad groups is 1mm to 2mm and is consistent with the center spacing of the sampling lines of the FFC sampling body. One or more tinning holes are provided on the pad, and the tinning holes are preferably circular or elliptical, with a diameter slightly smaller than the width of the welding area 114.
[0041] 2. S-type structure buffer 120
[0042] In order to meet the installation accuracy requirements, an S-shaped structure buffer 120 is provided. When the battery cell expands and stretches the sampling branch circuit board 100, the S-shaped structure expands and stretches with the battery cell to form a buffer to prevent the product from being stressed and breaking the circuit.
[0043] In the S-shaped buffer zone 120 , a certain gap is provided between the two side edges of the circuit layer and the two side edges of the upper insulating layer and the lower insulating layer.
[0044] Micro-connection points 121 and 122 are arranged at two turning areas of the S-shaped structure buffer 120. There is no circuit layer at the micro-connection points 121 and 122. The S-shaped structure buffer 120 forms a double-point connection with both ends through its two end points and the micro-connection points 121 and 122. When the battery cell expands and stretches the sampling branch circuit board 100, the micro-connection point will be automatically disconnected by force, so that the S-shaped structure will expand and stretch with the battery cell to form a buffer to prevent the product from breaking the circuit due to force.
[0045] A fuse 123 is formed by etching between two turning areas of the S-shaped structure buffer 120. The fuse 123 has a line width of 0.05 to 0.2 mm according to the size of the fuse current, and the shape can be a straight line or a serpentine line. When a large current occurs in an abnormal short circuit, the fuse can be quickly blown to avoid thermal runaway.
[0046] 3. Foolproof positioning area 130
[0047] The foolproof positioning area 130 is arranged on a side close to the battery busbar welding area 140 .
[0048] The region is provided with a positioning hole 131 for positioning and foolproofing the sampling branch circuit board 100 , and the aperture of the positioning hole is 1 to 2.5 mm.
[0049] 4. Battery busbar welding area 140
[0050] The sampling branch circuit board 100 and the battery pack busbar 300 are welded and connected through the battery busbar welding area 140. This area is preferably a double-sided pad for easy welding. When the copper thickness is thin, it can also be a single-sided pad (that is, only the lower insulation layer is removed here), and the length and width of the pad are preferably 5mm to 10mm.
[0051] like Figure 5 As shown, the exemplary FPC sampling body 200 is provided with a plurality of sampling lines 201, 202, ... in parallel, and each sampling line 201, 202, ... has a window at a different position of the FPC sampling body 200 to form branch connection pads 201a, 202a, ... of each sampling line.
[0052] like Figure 6 As shown, during welding, the sampling branch circuit board 100 can be aligned through the sampling branch pad group 110b thereon and the branch connection pad 202a of the FPC sampling body 200, and then soldered and connected by adding tin from the front tin adding area 111. During welding, the tin in the front tin adding area 111 can overflow to the welding area 114 on the back through the tinning hole 115, and the sampling branch circuit board 100 and a certain sampling line in the FPC sampling body 200 are soldered and connected. When the tin overflows from the bottom and overflows to the tin creeping areas 112 and 113, it means that the tin has been evenly distributed between the welding area 114 on the back and the branch connection pad 201a of a certain sampling line of the FPC sampling body 200. By visually inspecting the tin creeping state, the welding effect can be well confirmed to ensure the welding reliability of the product.
[0053] And so on, the welding connection of all sampling branch circuit boards 100 and the FPC sampling body 200 is completed.
[0054] like Figure 6 As shown, based on the above-mentioned sampling branch circuit board 100, the present invention also provides a welding quality confirmation method for the sampling branch circuit board, which can intuitively judge the welding quality during welding and ensure the success rate of welding.
[0055] The specific steps are as follows:
[0056] 1. Install each sampling branch circuit board 100 at the corresponding pad position of the FFC according to the design requirements. Align the sampling branch pad groups 110a, 110b, ... on the sampling branch circuit board 100 with the corresponding branch connection pads 201a, 202a, ... on the FPC sampling body 200, so that the sampling branch circuit 100 falls on the FPC sampling body 200.
[0057] 2. Add tin to the tin adding area in the middle of the front side of the sampling branch circuit board 100 by means of a solder paste printer or a tin dispensing machine.
[0058] 3. Heat and melt the tin through soldering processes such as laser and electric soldering iron.
[0059] 4. The tin is melted and heated until it fully flows, and overflows through the tinning holes 115 to the welding area 114 on the back and the branch connection pads of the FPC sampling body, and the circuits of the sampling branch circuit board 100 and the corresponding circuits of the FPC sampling body are welded.
[0060] 5. When the tin overflows to the tin creeping areas 112 and 113 on both sides, the heating is stopped to form welding. By visually inspecting the tin creeping state, the welding effect can be well confirmed to ensure the welding reliability of the product.
[0061] In summary, by using the sampling branch circuit board of the present invention, the welding quality of the sampling branch circuit board and the FPC sampling body can be quickly confirmed by visual inspection, which can greatly reduce circuit abnormalities caused by poor wiring harness welding quality and ensure the safety of batteries and electrical equipment.
[0062] Although the present invention has been specifically shown and described in conjunction with the preferred embodiments, it should be understood by those skilled in the art that various changes may be made to the present invention in form and details without departing from the spirit and scope of the present invention as defined by the appended claims, all of which are within the scope of protection of the present invention.
Claims
1. A sampling branch circuit board, characterized in that: A three-layer FPC structure consisting of an upper insulating layer, a circuit layer and a lower insulating layer is adopted, including an FPC sampling body welding area and a battery busbar welding area located at both ends of the sampling branch circuit board; a plurality of sampling branch pad groups are formed in the FPC sampling body welding area through a window opening process, and the position of each sampling branch pad group corresponds to a branch connection pad of the FPC sampling body; each group of the sampling branch pad groups includes a tinning area located in the middle of the front side of the sampling branch circuit board and tin creeping areas on both sides of the front side, and a welding area located on the back side of the sampling branch circuit board; the welding area extends to the edges of both sides of the FPC sampling body welding area, and the tinning area is provided with at least one tinning hole penetrating to the welding area; each of the tin creeping areas is provided with a semicircular hole penetrating to the welding area at the edge of the FPC sampling body welding area.
2. The sampling branch circuit board according to claim 1, characterized in that: The sampling branch pad group is distributed in parallel in the FPC sampling main body welding area; in the sampling branch pad group, the widths of the tin adding area, the tin creeping area and the welding area are equal.
3. The sampling branch circuit board according to claim 2, characterized in that: The widths of the sampling branch pad groups are equal, and the center distances between adjacent sampling branch pad groups are equal.
4. The sampling branch circuit board according to claim 3, characterized in that: The length of the welding area is 3mm to 15mm; the width is 0.5mm to 1.5mm; the center distance between adjacent welding areas is 1mm to 2mm; the distance between the tin creeping area and the tin adding area is not less than 0.3mm.
5. The sampling branch circuit board according to claim 1, characterized in that: The sampling branch circuit board also includes an S-shaped structural buffer in the middle for flexibly connecting the FPC sampling body welding area and the battery busbar welding area; in the S-shaped structural buffer, gaps are arranged between the two side edges of its circuit layer and the two side edges of the upper insulating layer and the lower insulating layer; micro-connection points are arranged at both turning areas of the S-shaped structural buffer, and there is no circuit layer at the micro-connection points. The S-shaped structural buffer forms a double-point connection with the FPC sampling body welding area and the battery busbar welding area through its end points and the micro-connection points; when the micro-connection point is disconnected, the sampling branch circuit board adapts to the distance change between the FPC sampling body welding area and the battery busbar welding area through the stretching of the S-shaped structural buffer.
6. The sampling branch circuit board according to claim 5, characterized in that: A fuse is arranged on the circuit layer between the two turning areas of the S-shaped structure buffer zone.
7. The sampling branch circuit board according to claim 1, characterized in that: The sampling branch circuit board also includes a fool-proof positioning area in the middle, and the fool-proof positioning area is arranged adjacent to the battery busbar welding area, and is provided with a fool-proof positioning structure for welding and aligning the sampling branch circuit board and the battery pack busbar.
8. The sampling branch circuit board according to claim 7, characterized in that: The foolproof positioning structure is a positioning hole.
9. The sampling branch circuit board according to claim 1, characterized in that: The battery busbar welding area is a double-sided welding pad or a single-sided welding pad, and the single-sided welding pad is formed by removing the lower insulating layer of the battery busbar welding area.
10. A method for confirming the welding quality of a sampling branch circuit board, characterized in that: Using the sampling branch circuit board as described in any one of claims 1 to 9; comprising the following steps: Adjust the relative positions of the sampling branch circuit board and the FPC sampling body so that a certain group of sampling branch pads on the sampling branch circuit board and the corresponding branch connection pads on the FPC sampling body are aligned; Select a sampling branch pad group aligned with the branch connection pad, and add tin to the tin adding area of the sampling branch pad group; Perform the soldering operation, heat and melt the tin, make the tin flow fully, overflow through the tinning holes on the tinning area to the soldering area on the back of the tinning area and the branch connection pads of the FPC sampling body, and finally overflow to the tin creeping area; When the molten tin is observed to overflow to the tin creeping areas on both sides, it indicates that the welding quality is qualified and heating is stopped to complete the welding.
Citation Information
Cited By
Battery module sampling structure
CN119833801A