Sputtering detection method

By calculating the expansion amount of the welded part during the resistance spot welding process and performing sputtering detection based on the determination threshold of different intervals, the problem of insufficient sputtering detection accuracy under a single threshold is solved, and high-precision sputtering judgment is achieved.

CN119077209APending Publication Date: 2024-12-06TOYOTA JIDOSHA KK
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410685299.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-06-05
Filing Date
2024-05-30
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

During the resistance spot welding process, it is difficult to accurately distinguish characteristic changes caused by sputtering and other factors during a single determination threshold, resulting in a decrease in sputtering detection accuracy.

Method used

The expansion amount of the welded portion is calculated by applying pressure and stroke between electrodes, and the slope of the waveform with time-changing expansion amount is lower than a preset determination threshold, and the determined target period is divided into two For each interval, different determination thresholds are used to compare the expansion waveform slope of each interval.

Benefits of technology

It realizes the high-precision determination of the sputtering occurrence during the resistance spot welding process, avoids misjudgment, and improves the accuracy of sputtering detection.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119077209A_ABST
    Figure CN119077209A_ABST
Patent Text Reader

Abstract

Provided is a sputter detection method for determining, with high precision, whether or not sputter has occurred during resistance spot welding. A sputter detection method for detecting sputter generated when resistance spot welding is performed on a plurality of overlapped plate-shaped welding materials, the sputter detection method comprising: a welding step of welding a plurality of welding materials by pressing a pair of electrodes while sandwiching a welding portion of the welding material between the pair of electrodes and energizing the pair of electrodes; in this way, a plurality of plate-shaped welding materials are welded. A calculation step for calculating the swell amount of the welded portion on the basis of the stroke and the pressure applied between the pair of electrodes; and a determination step for determining that a sputter has occurred when the magnitude of the slope of the swell amount waveform indicating the time change of the swell amount is lower than a predetermined determination threshold value, in the determination step, applying different determination threshold values to each of the sections obtained by dividing the period to be determined into at least two sections, and determining that the sputter has occurred. The determination threshold value corresponding to each section is compared with the magnitude of the slope of the swell waveform.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a spatter detection method, and more particularly to a spatter detection method for detecting spatter generated when resistance spot welding is performed on a plurality of overlapping plate-shaped welding materials. Background Art

[0002] In resistance spot welding, the welding part of a plurality of overlapping plate-shaped welding materials is sandwiched between a pair of electrodes and pressurized, while the pair of electrodes is energized, thereby performing resistance welding. If the heat generated by the resistance welding is too large, sputtering of a part of the welding part sometimes occurs. If sputtering occurs, it is possible that a poor weld occurs at the welding part or around it. Therefore, in Japanese Patent Publication No. 2008-105041, a method for detecting the generation of sputtering by detecting changes in electrode displacement, inter-electrode voltage or inter-electrode resistance in resistance spot welding is disclosed.

[0003] Japanese Patent Gazette No. 2008-105041 discloses a resistance welding method in which a welding current is passed through the contact portions of the joined parts to perform resistance heating and to apply pressure to melt the contact portions. In this resistance welding method, when the generation of sputtering is detected during power-on, a current (Iw+Iα) obtained by adding a predetermined amount of current Iα to a predetermined welding current Iw is reset as the welding current, and the current (Iw+Iα) is passed through the welded parts until a predetermined power-on time T is reached. Summary of the invention

[0004] As a method for detecting the occurrence of sputtering, it is conceivable that, for example, when the change in characteristics such as electrode displacement, inter-electrode voltage, or inter-electrode resistance is lower than (or higher than) a determination threshold (predetermined value), it is determined that sputtering has occurred. However, sometimes the change in characteristics caused by the occurrence of sputtering overlaps with the change in characteristics caused by factors other than the occurrence of sputtering. In this case, if a single determination threshold is used to determine whether sputtering has occurred, there is a problem that it may be erroneously determined whether sputtering has occurred due to the increase in the amount of change.

[0005] The present disclosure has been made to solve such a problem, and an object of the present disclosure is to provide a spatter detection method for accurately determining whether spatter has occurred during resistance spot welding.

[0006] A spatter detection method for resistance spot welding involved in one embodiment is a spatter detection method for detecting spatter generated when resistance spot welding is performed on multiple overlapping plate-shaped welding materials, and the spatter detection method has the following steps: a welding step, while clamping the welding part of the welding material between a pair of electrodes and pressurizing it, energizing the pair of electrodes, thereby welding multiple plate-shaped welding materials; a calculation step, calculating the expansion amount of the welding part based on the pressure and stroke between the pair of electrodes; and a judgment step, when the slope of the expansion amount waveform representing the time change of the expansion amount is lower than a predetermined judgment threshold, it is judged that spattering has occurred, in which a different judgment threshold is applied to each interval obtained by dividing the object period of judgment into at least two, and the judgment threshold corresponding to each interval is compared with the slope of the expansion amount waveform.

[0007] According to the present disclosure, it is possible to provide a spatter detection method for determining with high accuracy whether spatter has occurred during resistance spot welding.

[0008] The above and other objects, features and advantages of the present disclosure will become more fully understood from the detailed description given below and the accompanying drawings which are given by way of example only, but which should not be construed as limiting the present disclosure thereto. BRIEF DESCRIPTION OF THE DRAWINGS

[0009] Figure 1 It is a schematic diagram of a resistance spot welding system.

[0010] Figure 2 It is a graph showing the time change of the expansion amount and the time change of the slope of the expansion amount waveform.

[0011] Figure 3 It is a diagram showing a time change of an expansion amount and a time change of a slope of an expansion amount waveform for explaining a splash detection method according to an embodiment.

[0012] Figure 4 1 is a diagram showing a time change in the expansion amount and a time change in the slope of the expansion amount waveform for explaining the splash detection method of Comparative Example 1.

[0013] Figure 5 1 and 2 are graphs showing time changes in the amount of expansion and time changes in the slope of the expansion amount waveform for explaining the splash detection method of Comparative Example 2. DETAILED DESCRIPTION

[0014] Implementation Method 1

[0015] Hereinafter, the embodiments of the present disclosure will be described with reference to the accompanying drawings. However, the present disclosure is not limited to the following embodiments. In addition, for the purpose of clear description, the following description and the accompanying drawings are appropriately simplified. In the following description, the same or equivalent elements are marked with the same reference numerals, and repeated descriptions are omitted.

[0016] Figure 1 is a schematic diagram of a resistance spot welding system. Figure 1 The resistance spot welding system 100 will be described. Figure 1 The resistance spot welding system 100 shown in the figure has an upper movable electrode 101 and a lower fixed electrode 103 as a pair of electrodes. A welding portion 109 of a metal plate 105 and a metal plate 107 to be welded is arranged to overlap between the upper movable electrode 101 and the lower fixed electrode 103. In addition, the movable electrode and the fixed electrode may be turned upside down. The metal plates 105 and 107 are a plurality of plate-shaped welding materials, which are stacked up and down.

[0017] The upper movable electrode 101 moves up and down as indicated by the arrow, thereby applying pressure to the weld 109. The upper movable electrode 101 and the lower fixed electrode 103 sandwich the weld 109 from the direction in which the metal plates 105 and 107 overlap. The upper movable electrode 101 and the lower fixed electrode 103 allow current to flow while applying pressure to the weld 109. The metal plates 105 and 107 are welded by the resistance heat generated in the weld 109 sandwiched by the upper movable electrode 101 and the lower fixed electrode 103. The weld 109 is melted by the resistance heat and then solidified to form a nugget. Figure 1 In the figure, two metal plates are depicted, but there may be three or more metal plates.

[0018] The amount by which the upper movable electrode 101 is pressed after contacting the metal plate 105 is called a stroke. The stroke is measured at the upper movable electrode 101. The applied force is measured at the lower fixed electrode 103. A processing device such as a computer (not shown) uses these measured values ​​to calculate the expansion amount of the welded portion 109. Based on the calculated expansion amount, the processing device generates an expansion amount waveform indicating the time change of the expansion amount.

[0019] Figure 2 It is a graph showing the time change of the expansion amount and the time change of the slope of the expansion amount waveform. Figure 2 The left side of is a graph showing the time change of the expansion amount and the time change of the slope of the expansion amount waveform for the case where sputtering occurs and the case where sputtering does not occur in the first half of the power-on time, respectively. Figure 2 The right side of is a graph showing the time change of the expansion amount and the time change of the slope of the expansion amount waveform for the case where sputtering occurs and the case where sputtering does not occur when the power-on time is about to end. Figure 2, the tendency of the expansion amount and the expansion amount waveform are respectively described for the case where sputtering occurs and the case where sputtering does not occur.

[0020] exist Figure 2 In each graph of . The time change of the expansion amount when splashing occurs and the time change of the slope of the expansion amount waveform are shown by the black solid line. Figure 2 In each graph of , the time change of the expansion amount when no splash occurs and the time change of the slope of the expansion amount waveform are represented by gray solid lines.

[0021] Figure 2 The vertical axis of each graph shown above represents the expansion amount of the welded portion 109 calculated from the measured value of the stroke and the measured value of the pressure. The expansion amount of the welded portion 109 is calculated by the following formula (1).

[0022]

[0023] Here, E is the expansion amount, S is the stroke, a is the strain amount conversion coefficient, and F is the pressure. The strain amount conversion coefficient a is a coefficient for converting the pressure into the strain amount, and can be set to an arbitrary constant.

[0024] Thus, by using the stroke measured at the upper movable electrode 101 and the pressure measured at the lower fixed electrode 103, the expansion amount can be calculated with higher accuracy than when either of them is used independently. In addition, the slope of the expansion amount waveform indicating the time change of the expansion amount is the change amount of the expansion amount per unit time.

[0025] Time point t0 indicates the start time point of the power-on time. Time point t1 indicates the end time point of the power-on time. Time point t1 also indicates the start time point of the holding time for holding the upper movable electrode 101 and the lower fixed electrode 103 until they are opened. Time point t2 indicates the end time point of the holding time for holding the upper movable electrode 101 and the lower fixed electrode 103 until they are opened.

[0026] like Figure 2 As shown on the left side of , if power is turned on, sputtering may occur in the interval from time point t0 to time point t1. The expansion amount changes sharply (decreases) when sputtering occurs. Therefore, it is possible to detect splashing based on the slope of the expansion amount waveform. In order to detect splashing, a method can be conceived, for example, when the slope of the expansion amount waveform is lower than a predetermined judgment threshold, to determine that splashing has occurred.

[0027] like Figure 2As shown on the right side of , with the end of the power-on, the welded portion 109 of the welding material shrinks, thereby causing a change (decrease) in the amount of expansion caused by the shrinkage of the welding material immediately after the power-on time ends. Therefore, the amount of expansion and the slope of the expansion amount waveform, as shown by the gray solid line, begin to decrease from around time point t1. Here, in the case where sputtering occurs when the power-on time is about to end, the change in the amount of expansion caused by the shrinkage of the welding material overlaps with the change in the amount of expansion caused by the generation of sputtering. If these two changes in the amount of expansion overlap, the amount of expansion and the slope of the expansion amount waveform change (decrease) sharply from time point t1 as shown by the black solid line. In addition, the minimum value of the slope of the expansion amount waveform in the interval from time point t1 to time point t2 is significantly smaller than the minimum value of the slope of the expansion amount waveform in the interval from time point t0 to time point t1.

[0028] Therefore, when a cycle of the expansion amount waveform from time point t0 to time point t2 is used as the target period for determination, if a single determination threshold is applied to the target period to determine whether sputtering occurs, there is a problem of reduced detection accuracy of sputtering. As an example of such a problem, the spatter detection methods of Comparative Examples 1 and 2 in which a single determination threshold is applied to the target period are specifically described.

[0029] Figure 4 FIG. 1 is a diagram showing the time change of the expansion amount and the time change of the slope of the expansion amount waveform for explaining the splash detection method of Comparative Example 1. Figure 4 In the spatter detection method of Comparative Example 1 shown, -0.006 mm / ms, which is a pre-set determination threshold, is applied to the target period. The spatter detection method of Comparative Example 1 can determine that spatter has occurred when the slope of the expansion amount waveform is less than -0.006 mm / ms. In addition, -0.006 mm / ms, which is the determination threshold, is a value that is greater by a predetermined ratio than the minimum value of the slope of the expansion amount waveform when the change in expansion amount due to the generation of sputtering overlaps the change in expansion amount due to the contraction of the welding material.

[0030] like Figure 4 As shown by the black solid line on the left side of , when splash detection is performed by the splash detection method of Comparative Example 1, the slope of the expansion amount waveform indicating the change in expansion amount caused by splash generated in the first half of the power-on time in the interval from time point t0 to time point t1 is greater than the determination threshold. Figure 4As shown by the gray solid line on the left side of , the slope of the expansion amount waveform indicating the change in the expansion amount caused by the contraction of the welding material in the interval from time point t1 to time point t2 is also above the determination threshold. Therefore, in the spatter detection method of Comparative Example 1, although the contraction of the welding material generated immediately after the energization time is suppressed from being erroneously determined as spatter, there is a problem that spatter generated in the first half of the energization time cannot be detected.

[0031] On the other hand, Figure 4 As shown by the solid black line on the right side of , the change in expansion amount due to sputtering generated when the power-on time is about to end in the interval from time point t0 to time point t1 overlaps with the change in expansion amount due to contraction of the welding material. Therefore, when spatter is detected by the spatter detection method of Comparative Example 1, the slope of the expansion amount waveform where these two changes in expansion amount overlap in the interval from time point t1 to time point t2 is lower than the determination threshold. Therefore, in the spatter detection method of Comparative Example 1, spatter generated when the power-on time is about to end can be detected.

[0032] then, Figure 5 1 is a graph showing the time change of the expansion amount and the time change of the slope of the expansion amount waveform for explaining the splash detection method of Comparative Example 2. Figure 5 In the splash detection method of Comparative Example 2 shown, -0.002 mm / ms, which is a pre-set determination threshold, is applied to the target period. The splash detection method of Comparative Example 2 can determine that splash has occurred when the slope of the expansion amount waveform is lower than -0.002 mm / ms. In addition, -0.002 mm / ms, which is the determination threshold, is a value that is greater by a predetermined ratio than the minimum value of the slope of the expansion amount waveform when a change in the expansion amount caused by the occurrence of sputtering occurs.

[0033] like Figure 5 As shown by the black solid line on the left side of , when splash detection is performed by the splash detection method of Comparative Example 2, the slope of the expansion amount waveform indicating the change in expansion amount caused by splash generated in the first half of the energization time in the interval from time point t0 to time point t1 is lower than the determination threshold. Figure 5 As shown by the gray solid line on the left side of , the slope of the expansion amount waveform indicating the change in the expansion amount caused by the contraction of the welding material in the interval from time point t1 to time point t2 is also lower than the determination threshold. Therefore, in the spatter detection method of Comparative Example 2, although it is possible to detect spatter generated in the first half of the energization time, there is a problem of misjudging the contraction of the welding material generated immediately after the energization time as spatter.

[0034] On the other hand, Figure 5As shown by the black solid line on the right side of , when the spatter detection method of Comparative Example 2 is used to detect spatter, the slope of the expansion amount waveform formed by the overlap of the change in expansion amount caused by spatter generated at the end of the power-on time in the interval from time point t0 to time point t1 and the change in expansion amount caused by the contraction of the welding material generated in the interval from time point t1 to time point t2 is also lower than the determination threshold. Therefore, in the spatter detection method of Comparative Example 2, spatter generated at the end of the power-on time can be detected.

[0035] On the other hand, the spatter detection method of the present embodiment is a spatter detection method for detecting spatter generated when resistance spot welding is performed on a plurality of overlapping plate-shaped welding materials, and includes the following welding step, calculation step, and determination step.

[0036] In the welding process, a welding portion 109 of the welding material is sandwiched between a pair of electrodes and pressurized while the pair of electrodes are energized, thereby welding a plurality of plate-shaped welding materials. The calculation process calculates the expansion amount of the welding portion 109 based on the pressure and stroke between the pair of electrodes. When the magnitude of the slope of the expansion amount waveform representing the time variation of the expansion amount is lower than a predetermined determination threshold, the determination process determines that sputtering has occurred. In addition, in the determination process, a plurality of different determination thresholds are applied to each interval obtained by dividing the determination target period into at least two, and the determination threshold corresponding to each interval is compared with the magnitude of the slope of the expansion amount waveform.

[0037] First, in the welding process, the welded portion 109 of the metal plate 105 and the metal plate 107 is clamped under pressure between the upper movable electrode 101 and the lower fixed electrode 103 of the resistance spot welding system 100, and the upper movable electrode 101 and the lower fixed electrode 103 are energized, thereby welding the metal plate 105 and the metal plate 107. In the welding process, when the energization starts, the welded portion 109 of the welding material sandwiched between the upper movable electrode 101 and the lower fixed electrode 103 expands. And after the energization ends, while the upper movable electrode 101 and the lower fixed electrode 103 are kept open, the welded portion 109 of the welding material shrinks. In the welding process, the welded portion 109 solidifies, thereby forming a nugget between the metal plate 105 and the metal plate 107, and the metal plate 105 and the metal plate 107 are welded.

[0038] Next, in the calculation step, an expansion waveform indicating the time variation of the expansion of the weld 109 is calculated from the measured values ​​of the stroke and the measured values ​​of the applied force. The expansion of the weld 109 can be calculated by the above formula (1) using the stroke measured at the upper movable electrode 101 and the applied force measured at the lower fixed electrode 103. Figure 3It is a diagram showing a time change of an expansion amount and a time change of a slope of an expansion amount waveform for explaining a splash detection method according to an embodiment.

[0039] Reference Figure 3 The determination process will be described in detail. Figure 3 As shown, in the determination process, the target period can be divided into two intervals: a first interval from the start time point to the end time point of the power-on time and a second interval from the end time point of the power-on time to the end time point of the holding time for holding the upper movable electrode 101 and the lower fixed electrode 103 until they are opened. That is, the target period is the period from time point t0 to time point t2. Furthermore, the first interval can be the interval from time point t0 to time point t1, and the second interval can be the interval from time point t1 to time point t2. Thus, not only can the sputtering generated in the first half of the power-on time be detected with high precision, but also the sputtering generated when the power-on time is about to end can be detected with high precision.

[0040] Furthermore, in the determination step, a first determination threshold and a second determination threshold that are different from each other are applied to the first interval and the second interval as determination thresholds. Specifically, in the determination step, the first determination threshold is applied to the first interval, and a second determination threshold that is smaller than the first determination threshold is applied to the second interval. Figure 3 In the example shown, the first determination threshold is -0.002 mm / ms, and the second determination threshold is -0.006 mm / ms.

[0041] In the determination step, when the magnitude of the slope of the expansion amount waveform in the first interval is less than -0.002 mm / ms, it is determined that sputtering has occurred. In addition, -0.002 mm / ms as the first determination threshold is, for example, a value that is greater by a predetermined ratio than the minimum value of the slope of the expansion amount waveform when a change in the expansion amount caused by the occurrence of sputtering occurs.

[0042] In addition, in the determination step, when the magnitude of the slope of the expansion amount waveform in the second interval is less than -0.006 mm / ms, it is determined that sputtering has occurred. In addition, -0.006 mm / ms as the second determination threshold is, for example, a value that is greater by a predetermined ratio than the minimum value of the slope of the expansion amount waveform when the change in expansion amount due to the occurrence of sputtering and the change in expansion amount due to the contraction of the welding material overlap.

[0043] like Figure 3 As shown by the black solid line on the left side of , when splash detection is performed by the splash detection method according to the present embodiment, the slope of the expansion amount waveform indicating the change in expansion amount caused by splash generated in the first half of the energization time in the first interval is lower than the first determination threshold. Figure 3As shown by the gray solid line on the left side of , the slope of the expansion amount waveform indicating the change in the expansion amount caused by the contraction of the welding material generated in the second interval is greater than the second judgment threshold. Therefore, according to the spatter detection method of this embodiment, it is possible to suppress the contraction of the welding material generated immediately after the power-on time from being mistakenly determined as spatter, and it is possible to detect spatter generated in the first half of the power-on time.

[0044] And, if Figure 3 As shown by the black solid line on the right side of , when the spatter detection method according to the present embodiment is used to detect spatter, the slope of the expansion amount waveform formed by the overlap of the change in expansion amount caused by spatter generated at the end of the energization time in the first interval and the change in expansion amount caused by the contraction of the welding material generated in the second interval is lower than the second determination threshold. Therefore, according to the spatter detection method according to the present embodiment, spatter generated at the end of the energization time can also be detected.

[0045] As described above, in the spatter detection method of the present embodiment, whether spatter has occurred is determined based on a comparison between a plurality of determination thresholds set to different values ​​according to the timing of spatter generation and the slope of the expansion amount waveform. Therefore, according to the spatter detection method of the present embodiment, whether spatter has occurred during resistance spot welding can be determined with high accuracy.

[0046] In addition, the present disclosure is not limited to the above-described embodiments, and can be appropriately modified within a scope not departing from the gist.

[0047] From the disclosure thus described, it is obvious that the embodiments of the disclosure may be varied in a variety of ways. Such variations should not be regarded as departing from the spirit and scope of the disclosure, and all such modifications are intended to be included within the scope of the following claims, which will be obvious to those skilled in the art.

Claims

1. A method for detecting sputtering, for detecting sputtering generated when resistance spot welding is performed on a plurality of overlapping plate-shaped welding materials, The sputtering detection method has the following steps: A welding step of welding the plurality of plate-shaped welding materials by applying a current to the pair of electrodes while sandwiching a welding portion of the welding material between the pair of electrodes and applying pressure; a calculation step of calculating an expansion amount of the weld portion based on a pressure applied between the pair of electrodes and a stroke; and a determination step of determining that the sputtering has occurred when the magnitude of the slope of the expansion amount waveform representing the time variation of the expansion amount is lower than a predetermined determination threshold value, In the determination step, a different determination threshold is applied to each section obtained by dividing the determination target period into at least two sections, and the determination threshold corresponding to each section is compared with the slope of the expansion amount waveform.

2. The sputtering detection method according to claim 1, wherein: In the determination step, The target period is divided into two sections: a first section from a start time point to an end time point of a conduction time and a second section from an end time point of the conduction time to an end time point of a holding time in which the pair of electrodes are held open. The decision threshold value, which is smaller than the decision threshold value applied to the first section, is applied to the second section.

3. The splash detection method according to claim 1, wherein: The expansion amount is In the calculation, E is the expansion amount, S is the stroke, a is the strain conversion coefficient, and F is the pressure.