Method for treating electroplating waste liquid of cable metal conductor

By detecting the composition of the electroplating waste liquid and calibrating the reactor, combining precipitant and ozone disinfection treatment, the problems of low quality and high cost of electroplating waste liquid treatment are solved, ensuring the safe emission and environmental protection of the waste liquid.

CN119080330AInactive Publication Date: 2024-12-06CHANGZHOU HENGFENG SPECIAL CONDUCTOR CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411406743.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-10
Publication Date
2024-12-06
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing electroplating waste liquid treatment method cannot be targeted chemical treatment based on the main elements in the waste liquid, resulting in low treatment quality, untimely adjustment of the temperature and pressure data of the reactor, resulting in increased costs, and it is impossible to ensure whether the waste liquid contains viruses, and direct emissions may be Pollution of the environment.

Method used

The waste liquid components are detected by a liquid chromatography-mass spectrometer and an atomic absorption spectrometer, calibrate the reactor and set up an alarm, adjust the pH value, and disinfect the waste liquid with precipitants, activated carbon and ozone to ensure the quality and safety of the chemical reaction.

Benefits of technology

It improves the quality and efficiency of electroplating waste liquid treatment, reduces costs, ensures safe emission of waste liquid, and prevents environmental pollution.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119080330A_ABST
    Figure CN119080330A_ABST
Patent Text Reader

Abstract

The invention discloses a treatment method of cable metal conductor electroplating waste liquid. The treatment method comprises the following steps of S1, pretreatment, S2, reaction kettle calibration, S3, pH value adjustment, S4, chemical treatment, S5, neutralization reaction and S6, final discharge. Before a worker treats the electroplating waste liquid, a small amount of samples are extracted by a working test tube, then pollutants in the electroplating waste liquid are analyzed through a liquid chromatograph-mass spectrometer, inorganic element pollutants such as heavy metals in the electroplating waste liquid are analyzed through an atomic absorption spectrometer, and the content of the pollutants in the electroplating waste liquid is determined through detection of the two instruments. Main elements in the electroplating waste liquid can be determined, then a reactant is added according to the main elements, so that the reaction speed of the electroplating waste liquid is increased, the electroplating waste liquid is detected in advance, a chemical reaction can be performed according to main components of the electroplating waste liquid, and the chemical reaction quality of the electroplating waste liquid is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of electroplating waste liquid treatment, in particular to a method for treating cable metal conductor electroplating waste liquid. Background Art

[0002] Electroplating waste liquid refers to the waste liquid in the electroplating process, which usually contains heavy metal ions, chemicals and other pollutants, and has potential hazards to the environment and human health. The treatment and reuse of electroplating waste liquid is very important because it can reduce the emission of pollutants and save resources at the same time. When treating electroplating waste liquid, it is normal to directly treat the electroplating waste liquid chemically, and it cannot be treated chemically according to the main elements contained in the electroplating waste liquid, resulting in low treatment quality of electroplating waste liquid. The electroplating liquid needs to be treated repeatedly, which increases the cost of electroplating waste liquid treatment and reduces the work efficiency of electroplating waste liquid treatment. Therefore, "the original treatment of electroplating waste liquid is troublesome, and the treatment quality of electroplating waste liquid is low, which affects the normal discharge of electroplating fees", which is specifically manifested in the following aspects:

[0003] (1) When treating electroplating waste liquid, it is normally directly subjected to chemical treatment, and chemical treatment cannot be carried out according to the main elements contained in the electroplating waste liquid, resulting in low treatment quality of the electroplating waste liquid; (2) When the electroplating waste liquid is chemically treated by a reactor, the reaction parameters of the reactor need to be adjusted. When the temperature and pressure data on the reactor do not meet the settings, an alarm is not issued in time, which affects the treatment of the electroplating waste liquid, and the excess heat generated by the reactor is directly volatilized, thereby increasing the cost of treating the electroplating waste liquid; (3) After the electroplating waste liquid is chemically treated, it is normally discharged directly, resulting in the inability to determine whether the electroplating waste liquid contains viruses. Direct discharge will pollute the environment, thereby reducing the safety of waste liquid discharge. Summary of the invention

[0004] The object of the present invention is to provide a method for treating electroplating waste liquid of cable metal conductors, so as to solve the problems of the current electroplating waste liquid treatment method proposed in the above background technology: 1) when treating the electroplating waste liquid, the electroplating waste liquid is normally directly subjected to chemical treatment, and cannot be subjected to targeted chemical treatment according to the main elements contained in the electroplating waste liquid, thereby resulting in low treatment quality of the electroplating waste liquid; (2) when the electroplating waste liquid is chemically treated by a reactor, because the reaction parameters of the reactor need to be adjusted, when the temperature and pressure data on the reactor do not meet the settings, an alarm is not issued in time, affecting the treatment of the electroplating waste liquid, and the excess heat generated on the reactor is directly volatilized, thereby increasing the cost of treating the electroplating waste liquid; (3) after the electroplating waste liquid is chemically treated, it is normally discharged directly, resulting in the inability to determine whether the electroplating waste liquid contains viruses, and direct discharge will pollute the environment, thereby reducing the safety of waste liquid discharge.

[0005] To achieve the above object, the present invention provides the following technical solution: a method for treating cable metal conductor electroplating waste liquid, the method comprising the following steps:

[0006] S1. Preprocessing

[0007] 1. Extract samples, 2. Detect components, ① Liquid chromatography-mass spectrometry (LC-MS), ② Atomic absorption spectrometer (AAS), 3. Primary filtration, ① Connect to the reaction kettle, ② Filter through the filter;

[0008] S2. Calibration Reactor

[0009] 1. Testing equipment, ① calibrate the instrument, ② clean the instrument, 2. Set parameters, set temperature and pressure, 3. Set alarms, ① set alarm values, ② collect emergency treatment, 4. Residual heat recovery, use circulating cooling water system;

[0010] S3. Adjust pH value

[0011] 1. Detect pH value, ① waste liquid is acidic, ② waste liquid is alkaline, 2. Add neutralizer, ① sodium hydroxide when acidity is too high, ② sulfuric acid when acidity is too low, 3. Confirm that pH value meets the standard;

[0012] S4. Chemical treatment

[0013] 1. Chemical reaction, ① adding precipitant, ② using activated carbon and silica gel resin for adsorption, ③ oxidation-reduction method, adding potassium permanganate, 2. Resource recovery, recycling rare metals by electrolysis, 3. Solid-liquid separation, ① filtering the precipitate, ② discharging the waste liquid after the reaction;

[0014] S5. Neutralization reaction

[0015] 1. Neutralization of waste liquid, 2. Disinfection of waste liquid, ①Connecting ozone generator, ②Ozone disinfection, 3. Testing waste liquid, ①pH meter to test pH value, ②COD meter to test organic matter content, ③BOD meter to test the amount of oxygen required for biodegradation of organic matter, ④Ion chromatograph to test the ion content in waste liquid, such as cyanide and chromium ion;

[0016] S6. Final emission

[0017] 1. Waste liquid collection, ① storage of treated waste liquid, ② waste liquid transportation, 2. waste liquid discharge, 3. environmental testing, regular monitoring of the ecological environment through environmental testing instruments.

[0018] Preferably, the calculation formula for the amount of water pollutants discharged after the treatment of the electroplating waste liquid is Q=C*A, where Q is the wastewater discharge amount, measured in cubic meters (m3) / day, C is the wastewater concentration, measured in milligrams / liter (mg / L), and A is the discharge area, measured in square meters (m2).

[0019] Preferably, the formula for calculating chemical oxygen demand in the treatment of electroplating waste liquid is CODcr=C1×V1+C2×V2 / (V1+V2).

[0020] Preferably, in the chemical oxygen demand calculation formula, CODcr is the chemical oxygen demand, the unit is milligrams per liter (mg / L), C1 and C2 are the concentrations of potassium permanganate consumed in the test solution, the unit is milligram equivalents per liter (mgEq / L), V1 and V2 are the volumes of potassium permanganate consumed in the test solution, the unit is milliliters (mL).

[0021] Preferably, the calculation formula for the heavy metal concentration in the electroplating waste liquid is C=m / V, where C is the heavy metal concentration, m is the mass of the heavy metal, and V is the wastewater volume.

[0022] Preferably, in the heavy metal concentration calculation formula, the unit of C is milligram / liter (mg / L), the unit of m is milligram (mg), and the unit of V is liter (L).

[0023] Preferably, the heat demand (Q) of the reactor during operation is calculated by a formula Q=mcΔT, wherein Q is the heat demand, m is the material mass, c is the specific heat capacity, and ΔT is the temperature change.

[0024] Preferably, the process gas consumption calculation formula when the reactor is working is Cgas=0.038×P×S, wherein Cgas is the gas consumption, P is the pressure, and S is the diameter of the reactor.

[0025] Preferably, the reaction rate calculation formula when the reactor is working is R=-(d[A]) / dt, where R is the reaction rate, [A] is the concentration of the reactant A, and t is time.

[0026] Compared with the prior art, the present invention has the following beneficial effects:

[0027] The present invention allows a staff member to extract a small amount of sample from a working test tube before processing the electroplating waste liquid, and then use a liquid chromatography-mass spectrometer to analyze pollutants in the electroplating waste liquid, and then use an atomic absorption spectrometer to analyze inorganic element pollutants such as heavy metals in the electroplating waste liquid. Through the detection of the two instruments, the main elements in the electroplating waste liquid can be determined, and then reactants are added according to the main elements, thereby improving the reaction speed of the electroplating waste liquid. By detecting the electroplating waste liquid in advance, chemical reactions can be carried out according to the main components of the electroplating waste liquid, thereby improving the quality of the chemical reaction of the electroplating waste liquid.

[0028] Before the present invention uses a reactor to chemically treat the electroplating waste liquid, the staff needs to calibrate the reactor to prevent instrument failure from affecting the normal operation of the reactor, and then clean the reactor to reduce the impact on the chemical treatment of the electroplating waste liquid. Then, the working temperature of the reactor is set to 40 degrees Celsius, and then the pressure of the reactor is set to 15 bar, which can increase the speed of the electroplating reaction. When the sensor finds that the temperature and pressure are higher than the set value, the alarm is sounded through the alarm, so that the staff can adjust the equipment parameters in time to avoid affecting the treatment of the electroplating waste liquid. Then, the excess heat of the reactor is recovered through the circulating cooling water system, so that when the electroplating waste liquid is treated, the normal operation of the reactor is guaranteed while the waste heat is recovered, thereby reducing the use cost of the reactor.

[0029] The present invention neutralizes the pH value of the waste liquid to reduce the impact on the environment during subsequent discharge, connects the waste liquid to an ozone generator, disinfects the waste liquid with ozone through the ozone generator, eliminates viruses in the waste liquid, detects the pH value of the electroplating waste liquid through a pH meter, detects the organic matter content in the waste liquid through a COD meter, then detects the oxygen required for biodegradation of the organic matter in the waste liquid through a BOD meter, and finally detects the ion content in the waste liquid, such as cyanide and chromium ion, through an ion chromatograph, thereby ensuring that the discharged waste liquid does not have elements that may affect the environment due to viruses and cyanide, reducing pollution to the environment and improving the safety of direct discharge. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Figure 1 A flow chart of the electroplating waste liquid treatment of the present invention;

[0031] Figure 2 It is the debugging and running logic code of the reactor in the electroplating waste liquid treatment of the present invention;

[0032] Figure 3It is the working logic code of the reactor in the electroplating waste liquid treatment of the present invention. DETAILED DESCRIPTION

[0033] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0034] Embodiment 1:

[0035] Please refer to the figure, a method for treating cable metal conductor electroplating waste liquid, the treatment method comprises the following steps:

[0036] S1. Preprocessing

[0037] 1. Extracting samples, 2. Detecting components, ① Liquid chromatography-mass spectrometry (LC-MS), ② Atomic absorption spectrometer (AAS), 3. Primary filtration, ① Connecting to a reactor, ② Filtering through a filter. Before treating the electroplating waste liquid, the staff extracts a small amount of sample from a working test tube for detection, and then uses a liquid chromatography-mass spectrometry to analyze pollutants in the electroplating waste liquid, and then uses an atomic absorption spectrometer (AAS) to analyze inorganic element pollutants such as heavy metals in the electroplating waste liquid. Through the detection of the two instruments, the main elements in the electroplating waste liquid can be determined, and then reactants are added according to the main elements. Then, the electroplating waste liquid is connected to the reactor through a connecting pipe. During the addition process, the electroplating waste liquid is primary filtered, and large particle impurities in the waste liquid are filtered, thereby improving the reaction speed of the electroplating waste liquid. By detecting the electroplating waste liquid in advance, a chemical reaction can be carried out according to the main components of the electroplating waste liquid, thereby improving the quality of the chemical reaction of the electroplating waste liquid;

[0038] S2. Calibration Reactor

[0039] 1. Testing equipment, ① calibrate the instrument, ② clean the instrument, 2. Set parameters, set temperature and pressure, 3. Set the alarm, ① set the alarm value, ② collect emergency treatment, 4. Residual heat recovery, using a circulating cooling water system, before the reactor chemically treats the electroplating waste liquid, the staff needs to calibrate the reactor to prevent instrument failure from affecting the normal operation of the reactor, and then clean the reactor to reduce the impact on the chemical treatment of the electroplating waste liquid. Then set the working temperature of the reactor to 40 degrees Celsius, and then set the pressure of the reactor to 15bar, which can increase the speed of the electroplating reaction. When the sensor finds that the temperature and pressure are higher than the set value, the alarm is sounded through the alarm, so that the staff can adjust the equipment parameters in time to avoid affecting the treatment of the electroplating waste liquid. Then, the excess heat of the reactor is recovered through the circulating cooling water system, so that when the electroplating waste liquid is treated, the normal operation of the reactor is guaranteed, and the residual heat is recovered to reduce the use cost of the reactor;

[0040] S3. Adjust pH value

[0041] 1. Detect pH value, ① waste liquid is acidic, ② waste liquid is alkaline, 2. Add neutralizer, ① add sodium hydroxide when acidity is too high, ② add sulfuric acid when acidity is too low, 3. Confirm that pH value meets the standard. Before chemical treatment of electroplating waste liquid, use pH meter to detect pH value. When waste liquid is acidic, add sodium hydroxide for neutralization, and when waste liquid is alkaline, add sulfuric acid for neutralization, so as to facilitate the chemical treatment of electroplating waste liquid;

[0042] S4. Chemical treatment

[0043] 1. Chemical reaction, ① adding precipitant, ② using activated carbon and silica gel resin for adsorption, ③ oxidation-reduction method, adding potassium permanganate, 2. Resource recovery, recovering rare metals by electrolysis, 3. Solid-liquid separation, ① filtering the precipitate, ② discharging the waste liquid after the reaction, adding precipitant to the reactor to convert harmful substances in the waste liquid into precipitate, and then removing the precipitate from the waste liquid by gravity sedimentation or centrifugal separation, and then using activated carbon and resin adsorbents to adsorb heavy metal ion harmful substances in the waste liquid, and then adding potassium permanganate to oxidize and reduce the waste liquid to remove heavy metal ions in the waste liquid;

[0044] S5. Neutralization reaction

[0045] 1. Neutralization of waste liquid, 2. Disinfection of waste liquid, ①Connecting to ozone generator, ②Ozone disinfection, 3. Testing waste liquid, ①pH meter to test pH value, ②COD meter to test organic matter content, ③BOD meter to test the amount of oxygen required for biodegradation of organic matter, ④Ion chromatograph to test the ion content in waste liquid, such as cyanide and chromium ion. After chemical treatment of waste liquid, neutralize the pH value of waste liquid to reduce the impact on the environment during subsequent discharge, and then connect the waste liquid to the ozone generator. Then, the waste liquid is disinfected with ozone by an ozone generator to eliminate the viruses in the waste liquid. Then, the pH value of the electroplating waste liquid is detected by a pH meter. Then, the organic matter content in the waste liquid is detected by a COD meter. Then, the oxygen required for biodegradation of the organic matter in the waste liquid is detected by a BOD meter. Finally, the ion content in the waste liquid, such as cyanide and chromium ion, is detected by an ion chromatograph, so as to ensure that the discharged waste liquid does not contain elements that may affect the environment such as viruses and cyanide, reduce pollution to the environment, and improve the safety of direct discharge.

[0046] S6. Final emission

[0047] 1. Waste liquid collection, ① storage of treated waste liquid, ② transportation of waste liquid, 2. Waste liquid discharge, 3. Environmental testing, regular monitoring of the ecological environment through environmental testing instruments, unified collection and treatment of treated waste liquid, and then transportation of waste liquid to the discharge site, discharge in batches to reduce the impact of large-scale discharge on the environment, and then regular testing of the environment through testing instruments to ensure that the waste liquid will not have an impact on the environment.

[0048] In this embodiment: the calculation formula for the amount of water pollutants discharged after the treatment of electroplating waste liquid is Q=C*A, Q is the wastewater discharge amount, the unit is cubic meter (m3) / day, C is the wastewater concentration, the unit is milligram / liter (mg / L), and A is the discharge area, the unit is square meter (m2).

[0049] In this embodiment: the chemical oxygen demand calculation formula for electroplating waste liquid treatment is CODcr=C1×V1+C2×V2 / (V1+V2).

[0050] In the present embodiment, CODcr in the chemical oxygen demand calculation formula is chemical oxygen demand, in milligrams per liter (mg / L), C1 and C2 are respectively the concentrations of potassium permanganate consumed in the test solution, in milligram equivalents per liter (mgEq / L), and V1 and V2 are respectively the volumes of potassium permanganate consumed in the test solution, in milliliters (mL).

[0051] In this embodiment: the calculation formula for the heavy metal concentration in the electroplating waste liquid is C=m / V, where C is the heavy metal concentration, m is the mass of the heavy metal, and V is the wastewater volume.

[0052] In this embodiment, in the heavy metal concentration calculation formula, the unit of C is milligram / liter (mg / L), the unit of m is milligram (mg), and the unit of V is liter (L).

[0053] In this embodiment: the heat demand (Q) when the reactor is working is calculated by the formula Q=mcΔT, where Q is the heat demand, m is the material mass, c is the specific heat capacity, and ΔT is the temperature change.

[0054] In this embodiment: the process gas consumption calculation formula when the reactor is working is Cgas=0.038×P×S, where Cgas is the gas consumption, P is the pressure, and S is the diameter of the reactor.

[0055] In this embodiment: the calculation formula of the reaction rate when the reactor is working is R=-(d[A]) / dt, where R is the reaction rate, [A] is the concentration of the reactant A, and t is the time.

[0056] Embodiment 2:

[0057] As shown in the figure, different from the first embodiment, the present embodiment is a method for treating cable metal conductor electroplating waste liquid, and its management method includes the following steps:

[0058] S1. Allow the electroplating waste liquid generated during the electroplating process to settle freely to remove suspended matter, and then filter out fine particles larger than 4 microns in the electroplating waste liquid to obtain a pretreated electroplating solution.

[0059] S2. The pretreated electroplating liquid obtained in step (1) is sent to a coagulation sedimentation tank, and a mixed solution of sulfuric acid and hydrogen peroxide is added, and stirred by a stirring device to make it fully mixed, and then ammonia water is added to stir and mix for 10-20 minutes. The mixed liquid in the coagulation sedimentation tank is stratified, and the precipitate is removed by filtering to obtain an upper waste liquid A.

[0060] S3. Add sodium hydroxide solution to the waste liquid A obtained in step (2), stir the mixed solution in the coagulation sedimentation tank for 10-15 minutes by a stirring device, add sodium dithionite after the reaction to react, the mixed solution in the coagulation sedimentation tank is layered, filter and remove the precipitate to obtain the upper waste liquid B.

[0061] S4. Inject the waste liquid B obtained in step (3) into the treatment reaction tank, add acid to adjust the pH to 2.5-4, and transport it to the adsorption tank, and add nanoparticles with Fe3O4 as the core and SiO2 as the shell as the adsorbent to continuously adsorb until the COD of the water in the adsorption tank reaches 150-165 mg / L, and then stop the adsorption. After the adsorption is completed, drain the remaining waste liquid in the adsorption tank.

[0062] S5. Introduce the waste liquid in step (4) into an ion exchange resin system, and then analyze it with sulfuric acid, distilled water and ethanol in turn to obtain a treated solution, and collect the treated solution into a recovery pool for recycling.

[0063] In summary, compared with Example 2, in this Example 1, before treating the electroplating waste liquid, the staff extracts a small amount of sample from the working test tube for detection, and then uses a liquid chromatography-mass spectrometer to analyze the pollutants in the electroplating waste liquid, and then uses an atomic absorption spectrometer (AAS) to analyze the inorganic element pollutants such as heavy metals in the electroplating waste liquid. Through the detection of the two instruments, the main elements in the electroplating waste liquid can be determined, and then reactants are added according to the main elements. The electroplating waste liquid is then connected to the reactor through a connecting pipe. During the addition process, the electroplating waste liquid is primarily filtered, and large particulate impurities in the waste liquid are filtered, thereby increasing the reaction speed of the electroplating waste liquid. By detecting the electroplating waste liquid in advance, a chemical reaction can be carried out according to the main components of the electroplating waste liquid, thereby improving the quality of the chemical reaction of the electroplating waste liquid.

[0064] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.

[0065] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A method for treating cable metal conductor electroplating waste liquid, characterized in that the method comprises the following steps: S1. Preprocessing 1. Extract samples, 2. Detect components, ① Liquid chromatography-mass spectrometry (LC-MS), ② Atomic absorption spectrometer (AAS), 3. Primary filtration, ① Connect to the reaction kettle, ② Filter through the filter; S2. Calibration Reactor 1. Testing equipment, ① calibrate the instrument, ② clean the instrument, 2. Set parameters, set temperature and pressure, 3. Set alarms, ① set alarm values, ② collect emergency treatment, 4. Residual heat recovery, use circulating cooling water system; S3. Adjust pH value 1. Detect pH value, ① waste liquid is acidic, ② waste liquid is alkaline, 2. Add neutralizer, ① sodium hydroxide when acidity is too high, ② sulfuric acid when acidity is too low, 3. Confirm that pH value meets the standard; S4. Chemical treatment 1. Chemical reaction, ① adding precipitant, ② using activated carbon and silica gel resin for adsorption, ③ oxidation-reduction method, adding potassium permanganate, 2. Resource recovery, recycling rare metals by electrolysis, 3. Solid-liquid separation, ① filtering the precipitate, ② discharging the waste liquid after the reaction; S5. Neutralization reaction 1. Neutralization of waste liquid, 2. Disinfection of waste liquid, ①Connecting ozone generator, ②Ozone disinfection, 3. Testing waste liquid, ①pH meter to test pH value, ②COD meter to test organic matter content, ③BOD meter to test the amount of oxygen required for biodegradation of organic matter, ④Ion chromatograph to test the ion content in waste liquid, such as cyanide and chromium ion; S6. Final emission 1. Waste liquid collection, ① storage of treated waste liquid, ② waste liquid transportation, 2. waste liquid discharge, 3. environmental testing, regular monitoring of the ecological environment through environmental testing instruments.

2. The method for treating cable metal conductor electroplating waste liquid according to claim 1, characterized in that: The calculation formula for the amount of water pollutants discharged after the treatment of electroplating waste liquid is Q=C*A, where Q is the wastewater discharge amount, in cubic meters (m3) / day, C is the wastewater concentration, in milligrams / liter (mg / L), and A is the discharge area, in square meters (m2).

3. The method for treating cable metal conductor electroplating waste liquid according to claim 1, characterized in that: The formula for calculating the chemical oxygen demand in the treatment of electroplating waste liquid is CODcr=C1×V1+C2×V2 / (V1+V2).

4. The method for treating cable metal conductor electroplating waste liquid according to claim 3, characterized in that: In the chemical oxygen demand calculation formula, CODcr is chemical oxygen demand, the unit is milligrams per liter (mg / L), C1 and C2 are respectively the concentrations of potassium permanganate consumed in the test solution, the unit is milligram equivalents per liter (mgEq / L), V1 and V2 are respectively the volumes of potassium permanganate consumed in the test solution, the unit is milliliters (mL).

5. The method for treating cable metal conductor electroplating waste liquid according to claim 1, characterized in that: The calculation formula for the heavy metal concentration in the electroplating waste liquid is C=m / V, where C is the heavy metal concentration, m is the mass of the heavy metal, and V is the wastewater volume.

6. The method for treating cable metal conductor electroplating waste liquid according to claim 5, characterized in that: In the heavy metal concentration calculation formula, the unit of C is milligram / liter (mg / L), the unit of m is milligram (mg), and the unit of V is liter (L).

7. The method for treating cable metal conductor electroplating waste liquid according to claim 1, characterized in that: The heat demand (Q) of the reactor during operation is calculated using a formula Q=mcΔT, where Q is the heat demand, m is the material mass, c is the specific heat capacity, and ΔT is the temperature change.

8. The method for treating cable metal conductor electroplating waste liquid according to claim 1, characterized in that: The process gas consumption calculation formula when the reactor is working is Cgas=0.038×P×S, where Cgas is the gas consumption, P is the pressure, and S is the diameter of the reactor.

9. The method for treating cable metal conductor electroplating waste liquid according to claim 1, characterized in that: The calculation formula of the reaction rate when the reactor is working is R=-(d[A]) / dt, where R is the reaction rate, [A] is the concentration of the reactant A, and t is the time.

Citation Information

Patent Citations

  • Electroplating nickel-containing wastewater treatment and reuse process

    CN105110512A

  • Chemical nickel-plating waste liquor treatment method and system

    CN106587455A

  • Treating process and system for electroplating nickel-containing waste water

    CN108249623A

  • Recycling device for electroplating wastewater treatment

    CN112897754A

  • Electroplating wastewater treatment and monitoring integrated control system

    CN209702372U