Method and system for predicting cracking and pulverization of polycrystalline NCM electrode particles

By constructing an anisotropic polycrystalline fracture phase field model and combining with finite element simulation, the problem of insufficient accuracy of cracking and powder prediction of polycrystalline NCM electrode particles is solved, and more accurate microscopic scale analysis and anisotropic impact consideration is achieved, improving the Prediction accuracy and applicability reduce battery design and inspection costs.

CN119089732AActive Publication Date: 2024-12-06HUAZHONG UNIV OF SCI & TECH
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411057370.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-02
Publication Date
2024-12-06
Estimated Expiration
2044-08-02

AI Technical Summary

Technical Problem

In the process of predicting the cracking and powderization of polycrystalline NCM electrode particles, the prediction accuracy is insufficient, and the microscopic scale analysis and anisotropic impact considerations are lacking, resulting in inaccurate prediction results.

Method used

The anisotropic polycrystalline fracture phase field model is constructed, including grain boundary phase field equations, solid mechanics equations and Li+ diffusion equations. Numerical solution is performed through finite element simulation software to obtain the cracking and powdering distribution of polycrystalline NCM electrode particles, and consider Li+ diffusion Bidirectional coupling with mechanical stress.

Benefits of technology

Improves the accuracy of cracking powder prediction, can analyze stress and Li+ concentration distribution on microscopic scale, dynamically displays the cracking process, is suitable for different geometric and material conditions, provides a strategy to suppress cracking, and reduces the design and inspection of lithium-ion batteries. cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119089732A_ABST
    Figure CN119089732A_ABST
Patent Text Reader

Abstract

The invention belongs to but is not limited to the technical field of electronic core industry, and discloses a polycrystalline NCM electrode particle cracking pulverization prediction method and system, and the method comprises the steps: constructing an anisotropic polycrystalline fracture phase field model which comprises a grain boundary phase field equation, a solid mechanical equation, a Li < + > diffusion equation and a fracture phase field equation; constructing a polycrystalline NCM electrode particle two-dimensional geometry, setting parameters required by a physical place, carrying out grid division, and setting initial conditions and boundary conditions; finite element simulation software is used for numerical solution, and the cracking and pulverization distribution of the polycrystalline NCM electrode particles is obtained. According to the method, bidirectional coupling of Li < + > diffusion and mechanical stress as well as cracking pulverization and mechanical stress is considered, and the critical energy release rate is calculated and corrected by using the grain boundary phase field, so that the mechanism of cracking pulverization of the polycrystalline NCM electrode particles can be accurately reflected, and the accuracy of cracking pulverization prediction is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to but is not limited to the technical field of the core electronic industry, and in particular relates to a method and system for predicting cracking and pulverization of polycrystalline NCM electrode particles. Background Art

[0002] Lithium-ion batteries (LIBs) are widely used in electric vehicles (EVs) due to their high energy density, long cycle life, and low manufacturing cost. Although LIB technology has made great progress, the energy density is still difficult to meet the requirements of electric vehicles for power batteries. Extending the limited driving range of current EVs requires the development of high-energy-density LIBs, among which nickel-rich layered LiNi 1-x-y Co x Mn y O 2 The Ni-containing cathode (NCM) is considered to be the most promising cathode candidate. The energy density of NCM electrodes can be further improved by increasing the Ni content, but the performance enhancement obtained using this approach comes at the expense of cycling performance and mechanical stability. During the cycling process, cracking and pulverization occur in the NCM electrode particles, allowing the electrolyte to penetrate the interior of the particles. This process brings two serious consequences: first, it accelerates the surface degradation of the electrolyte and NCM active materials, seriously compromising the available capacity and service life of the NCM electrode. Second, it reduces the electrochemical performance of the NCM particles.

[0003] At present, the experimental and simulation studies on polycrystalline NCM electrode particles are incomplete. Most experimental observations are conducted in a non-in-situ manner, and the observation of cracking and pulverization ignores the generation and expansion of cracks during the charging and discharging process, and lacks research on the crack formation mechanism and influencing mechanism. The methods used in simulation studies are too backward, and often only analyze the cracking process from the perspective of stress, which cannot accurately simulate the generation and expansion of cracks.

[0004] Through the above analysis, the problems and defects of the existing technology are as follows: the methods used in the existing simulation research are too backward, and often only analyze the cracking process from the perspective of stress, and cannot accurately simulate the generation and expansion of cracks.

[0005] 1) Insufficient prediction accuracy: Traditional prediction methods for electrode particle cracking and pulverization are often based on empirical formulas or simplified physical models, which are difficult to accurately reflect the complex behavior of polycrystalline NCM electrode particles during the charging and discharging process, resulting in inaccurate prediction results.

[0006] 2) Lack of micro-scale analysis: The cracking and pulverization of polycrystalline NCM electrode particles is a process involving the micro-scale, and traditional methods are often difficult to analyze and predict at the micro-scale.

[0007] 3) Failure to consider the effect of anisotropy: Polycrystalline materials are anisotropic, that is, the physical properties in different directions may be different. Traditional methods often ignore the impact of this property on cracking and powdering. Summary of the invention

[0008] In view of the problems existing in the prior art, the present invention provides a method and system for predicting cracking and pulverization of polycrystalline NCM electrode particles, which aims to improve the accuracy of prediction of cracking and pulverization of polycrystalline NCM electrode particles.

[0009] The present invention is implemented as follows: a method for predicting cracking and pulverization of polycrystalline NCM electrode particles, comprising:

[0010] S1, construct anisotropic polycrystalline fracture phase field model, including grain boundary phase field equation, solid mechanics equation, Li + Diffusion equations and fracture phase field equations;

[0011] S2, construct the two-dimensional geometry of polycrystalline NCM electrode particles, set the parameters required for the physical field, perform meshing and set initial conditions and boundary conditions;

[0012] S3, using finite element simulation software to perform numerical solution, the cracking and pulverization distribution of polycrystalline NCM electrode particles was obtained.

[0013] Further, in step S1, the grain boundary phase field equation is used to calculate the modified critical energy release rate inside the polycrystalline NCM electrode particles, and the solid mechanics equation is used to calculate the stress and elastic strain energy density distribution. + The diffusion equation is used to calculate Li + Concentration distribution, fracture phase field equation is used to calculate cracking and powdering distribution.

[0014] Further, in step S2, the two-dimensional geometry of the polycrystalline NCM electrode particles is drawn by the Voronoi diagram algorithm; the set physical parameters include Young's modulus, Poisson's ratio, density, temperature, Li + Diffusion rate, maximum Li + Concentration, reference Li + concentration, grain boundary phase field length parameter, fracture phase field length parameter, grain boundary critical energy release rate, primary particle energy release rate, unit concentration volume change, partial molar volume, all primary particle crystal directions; the mesh is divided into triangular meshes, and the maximum mesh size is set to 0.02μm; the initial conditions include the initial value of the grain boundary phase field, Li + Initial concentration of diffusion, initial displacement of solid mechanics, initial value of fracture phase field; boundary conditions, Dirichlet boundary conditions of grain boundary phase field, Li + Diffusion flux, free boundary conditions in solid mechanics.

[0015] Furthermore, in step S2, an independent spatial coordinate system is constructed for each primary particle in the polycrystalline NCM electrode particles, and the orientation of the coordinate system is the crystal orientation of the primary particle.

[0016] Furthermore, in step S3, two solving steps are used to numerically solve the model. The first step is to solve the grain boundary phase field equation in a steady state, obtain the modified critical energy release rate distribution and store it. The second step is to solve the solid mechanics equation, the Li+ diffusion equation and the fracture phase field equation in a transient state, and transfer the solution stored in the first step to the second step as the value of the critical energy release rate.

[0017] The grain boundary phase field equation constructed in S1 is:

[0018]

[0019] Where p is the grain boundary phase field order parameter, l p is the grain boundary phase field length parameter, represents the Hamiltonian operator. Modified critical energy release rate G p It can be written as

[0020] G p =g(p)G c_G ++((1-g(p))G c_GB

[0021] Where g(p) = (1-p) 2 , G c_G is the critical energy release rate of the grain, G c_GB is the critical energy release rate at the grain boundary.

[0022] Specifically, the solid mechanics equation constructed in S1 is:

[0023]

[0024] in, is the Hamiltonian operator, C(d) represents the modified elastic stiffness tensor;

[0025] ε e Represent the elastic strain tensor:

[0026] ε e =ε-ε c ,

[0027] ε is the total strain tensor;

[0028] ε c is the chemical strain tensor:

[0029] ε c =(cc ref )β ij,

[0030] β ij is the anisotropic change in volume per unit concentration;

[0031] c represents Li + Concentration, c ref Indicates reference Li + concentration.

[0032] In the formula, the expression of the modified elastic stiffness tensor C(d) is:

[0033]

[0034] Among them, C 0 is the elastic stiffness tensor of the normal material, k 0 is the bulk modulus, I is the unit matrix, sign - is the sign function, ε e is the elastic strain tensor, tr(ε e ) is ε e traces;

[0035] g(d) is the phase field degenerate function:

[0036] g(d)=(1-d) 2 +k,

[0037] k is a numerical stability parameter.

[0038] Li constructed in S1 + The diffusion equation is:

[0039]

[0040] Where J is the Li per unit area per unit time + Molar flux, D represents Li + The diffusion rate, represents the Hamiltonian operator, Ω ij represents partial molar volume, R represents ideal gas constant, T represents Kelvin temperature, and c represents Li + Concentration, c max Indicates the maximum Li that the material can accommodate + Concentration, σ h represents hydrostatic stress.

[0041] The fracture phase field equation constructed in S1 is:

[0042]

[0043] Among them, G pis the modified critical energy release rate of the polycrystalline NCM electrode particle material; d is the fracture phase field order parameter, where d = 1 indicates that the material is completely damaged, d = 0 indicates that the material is intact (i.e., no failure), and 0 < d < 1 indicates a transitional state; l d represents the length parameter of the fracture phase field, represents the Hamiltonian operator, and H is defined as the historical maximum tensile strain energy density:

[0044] H = max Ψ e (t)

[0045] where Ψ e (t) represents the tensile elastic strain energy density, and its expression is:

[0046]

[0047] where g(d) is the phase field degradation function, ε e is the elastic strain tensor, C 0 is the elastic stiffness tensor of the normal material, ε vol is the volumetric component of the elastic strain, ε dev is the deviatoric component of the elastic strain, tr(ε e ) is the trace of ε e .

[0048] The two-dimensional geometry of the polycrystalline NCM electrode particles constructed in S2 is generated using the Voronoi diagram algorithm. The generated two-dimensional polycrystalline geometry is circular with a radius of 5 μm. The internal primary particles are irregular hexagons with an average particle size of 0.57 μm, and their sizes and shapes are random.

[0049] The two-dimensional geometric mesh of the polycrystalline NCM electrode particles constructed in S2 is divided using triangular meshes. The maximum mesh size is set to 0.02 μm. The constructed mesh contains a total of 508,636 triangular regions, and the degrees of freedom during simulation are 5.1 million.

[0050] The physical parameters set in S2 are: Young's modulus E = 120 GPa, Poisson's ratio ν = 0.3, density ρ = 4.14 g / cm 3 , temperature T = 300 K, Li + diffusion rate D = 7×10 -15 m 2 / s, maximum Li + concentration c max = 35,164 mol / m 3 , reference Li + concentration c max = 31,648 mol / m 3 , grain boundary phase field length parameter l p = 0.05 μm, fracture phase field length parameter ld =0.05μm, grain boundary critical energy release rate G c_GB =2N / m, primary particle energy release rate G c_G =10N / m. The volume change per unit concentration and the partial molar volume are anisotropic, where the volume change per unit concentration is set to: β a =β b =0.597cm 3 / mol, β c =1.052cm 3 / mol. The partial molar volume is set to: Ω a =Ω b =1.79cm 3 / mol,Ω c =3.16cm 3 / mol. All primary particle orientations are randomly generated and set using scripts;

[0051] The initial conditions set in S2 are: the initial value of the grain boundary phase field is set to 0, Li + The initial diffusion concentration is set to 31648 mol / m 3 , the initial displacement of solid mechanics is set to no displacement, and the initial value of the fracture phase field is set to 0; the boundary conditions set in S2 are: the Dirichlet boundary condition is set at the grain boundary of the polycrystalline NCM electrode particles in the grain boundary phase field, and the value is set to 1; Li + The flux size of the polycrystalline NCM electrode particles in the diffusion equation is set to 7.33×10 -5 mol / (m 2 ·s); free boundary conditions are used for polycrystalline NCM electrode particles in solid mechanics.

[0052] Furthermore, in step S3, the cracking and pulverization distribution of the polycrystalline NCM electrode particles is the distribution of the fracture phase field order parameter.

[0053] Another object of the present invention is to provide a polycrystalline NCM electrode particle cracking and pulverization prediction system for realizing the polycrystalline NCM electrode particle cracking and pulverization prediction method, comprising:

[0054] Model building module, used to construct anisotropic polycrystalline fracture phase field model, including grain boundary phase field equation, solid mechanics equation, Li + Diffusion equations and fracture phase field equations;

[0055] 2D geometry construction module, used to construct the 2D geometry of polycrystalline NCM electrode particles, set the parameters required for the physical field, perform meshing and set initial conditions and boundary conditions;

[0056] The numerical solution module is used to perform numerical solution using finite element simulation software to obtain the cracking and pulverization distribution of polycrystalline NCM electrode particles.

[0057] Another object of the present invention is to provide a computer device, the computer device includes a memory and a processor, the memory stores a computer program, when the computer program is executed by the processor, the processor executes the steps of the polycrystalline NCM electrode particle cracking and pulverization prediction method.

[0058] Another object of the present invention is to provide a computer-readable storage medium storing a computer program, which, when executed by a processor, enables the processor to execute the steps of the method for predicting cracking and pulverization of polycrystalline NCM electrode particles.

[0059] Another object of the present invention is to provide an information data processing terminal, which is used to implement the polycrystalline NCM electrode particle cracking and pulverization prediction system.

[0060] In combination with the above technical solutions and the technical problems solved, the advantages and positive effects of the technical solutions to be protected by the present invention are as follows:

[0061] (1) The present invention proposes a method for predicting the cracking and pulverization of polycrystalline NCM electrode particles, taking into account the Li + The bidirectional coupling of diffusion and mechanical stress, cracking and pulverization and mechanical stress, and the use of grain boundary phase field calculation to correct the critical energy release rate enable the present invention to accurately reflect the mechanism of cracking and pulverization of polycrystalline NCM electrode particles, thereby improving the accuracy of cracking and pulverization prediction.

[0062] (2) The method for predicting the cracking and pulverization of polycrystalline NCM electrode particles constructed by the present invention is more vivid and specific. The results of cracking and pulverization can be displayed through a two-dimensional cloud map, and the cracking and pulverization process can be displayed dynamically. At the same time, the stress distribution inside the polycrystalline NCM electrode particles during the cracking and pulverization process, Li + The concentration distribution can also be displayed dynamically.

[0063] (3) The method for predicting the cracking and pulverization of polycrystalline NCM electrode particles constructed by the present invention is universal and suitable for accurately predicting the cracking and pulverization of polycrystalline NCM electrode particles under different geometries, different materials and different working conditions.

[0064] (4) The method for predicting the cracking and pulverization of polycrystalline NCM electrode particles constructed by the present invention can be used to explore inhibition strategies. The effect of inhibiting cracking and pulverization can be achieved by changing the geometric size and shape distribution of the primary and secondary particles, or by structural regulation.

[0065] (5) The geometric model used in the method for predicting the cracking and pulverization of polycrystalline NCM electrode particles constructed by the present invention can be a SEM image of real particles. Therefore, the present invention can be used for the inspection and detection of real polycrystalline NCM electrode particles.

[0066] A method for predicting cracking and pulverization of polycrystalline NCM electrode particles constructed by the present invention can accurately predict the cracking and pulverization of polycrystalline NCM electrode particles during the charging and discharging process. The method has the advantage of using a more accurate physical model to improve the accuracy of the prediction.

[0067] (1) The expected benefits and commercial value of the technical solution of the present invention after transformation are:

[0068] The technical solution of the present invention can be used for the design and inspection of positive electrode materials for lithium-ion batteries, which can greatly reduce the consumption of real experiments, or serve as an auxiliary means for real experiments. Ultimately, it reduces the cost of design and inspection of positive electrode materials for lithium-ion batteries.

[0069] (2) The technical solution of the present invention fills the technical gap in the industry at home and abroad:

[0070] The method for predicting the cracking and pulverization of polycrystalline NCM electrode particles constructed by the present invention is the first of its kind in the industry. It combines previous technical solutions at home and abroad, and on this basis constructs a more accurate and complex physical model, which greatly improves the accuracy of the prediction.

[0071] (3) The technical solution of the present invention solves the technical problems that people have been eager to solve but have never been able to solve successfully:

[0072] The method for predicting the cracking and pulverization of polycrystalline NCM electrode particles constructed by the present invention solves a technical problem, namely, accurately predicting the cracking and pulverization of polycrystalline NCM electrode particles. The prediction models before this are mostly simple stress models, and the prediction accuracy does not meet the actual requirements at all. The prediction accuracy of the present invention is greatly improved.

[0073] Third, the present invention constructs a method for predicting the cracking and pulverization of polycrystalline NCM (nickel cobalt manganese oxide) electrode particles by integrating phase field model, solid mechanics, Li + The diffusion and other physical equations provide a powerful tool for accurately predicting the cracking and pulverization of polycrystalline NCM electrode particles. The following are the technical problems existing in the industrial application of the existing technology and the significant technical progress achieved by this method:

[0074] 1) Improve prediction accuracy: By constructing an anisotropic polycrystalline fracture phase field model, the present invention can comprehensively consider grain boundaries, solid mechanics, Li + The influence of multiple factors such as diffusion on the cracking and pulverization of electrode particles is considered, thereby improving the accuracy of the prediction.

[0075] 2) Realize micro-scale analysis: By numerically solving the two-dimensional geometric model of polycrystalline NCM electrode particles, the present invention can analyze the stress, strain and Li of electrode particles during the charge and discharge process at a micro scale. + Parameters such as concentration distribution provide more detailed and in-depth information for cracking and powdering prediction.

[0076] 3) Considering the influence of anisotropy: By introducing concepts such as modified elastic stiffness tensor and phase field degradation function, the present invention can fully consider the influence of anisotropy of polycrystalline materials on cracking and powdering, so that the prediction results are more in line with the actual situation.

[0077] 4) Optimizing industrial applications: The prediction method of the present invention can provide battery manufacturers with important information about the cracking and pulverization of electrode particles, thereby helping them optimize battery design and manufacturing processes and improve the cycle life and safety of batteries.

[0078] 5) Promote scientific research progress: The prediction method of the present invention also provides researchers with a new research tool, which helps them to have a deeper understanding of the cracking and pulverization mechanism of polycrystalline NCM electrode particles and promote scientific research progress in related fields. BRIEF DESCRIPTION OF THE DRAWINGS

[0079] Figure 1 It is a schematic diagram of a method for predicting cracking and pulverization of polycrystalline NCM electrode particles provided by an embodiment of the present invention;

[0080] Figure 2 is a flow chart of a method for predicting cracking and pulverization of polycrystalline NCM electrode particles provided by an embodiment of the present invention;

[0081] Figure 3 is a two-dimensional geometric schematic diagram of a polycrystalline NCM electrode particle provided by an embodiment of the present invention;

[0082] Figure 4 Schematic diagram of the evolution of cracking and pulverization distribution of polycrystalline NCM electrode particles provided by an embodiment of the present invention;

[0083] Figure 5 It is a schematic diagram of the cracking and pulverization evolution process of polycrystalline NCM electrode particles at different primary particle sizes provided by an embodiment of the present invention;

[0084] Figure 6 It is a schematic diagram of the cracking and pulverization evolution process of polycrystalline NCM electrode particles under different secondary particle sizes provided by an embodiment of the present invention;

[0085] Figure 7 is a comparison diagram of cracking and pulverization results of polycrystalline NCM electrode particles with different structures provided in an embodiment of the present invention;

[0086] Figure 8It is a structural diagram of a polycrystalline NCM electrode particle cracking and pulverization prediction system provided in an embodiment of the present invention. DETAILED DESCRIPTION

[0087] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0088] In view of the problems existing in the prior art, the present invention provides a method and system for predicting cracking and pulverization of polycrystalline NCM electrode particles. The present invention is described in detail below with reference to the accompanying drawings.

[0089] Two specific industrial application examples of this prediction method involve the design and maintenance of lithium-ion batteries, especially for battery performance optimization in electric vehicles and portable electronic devices:

[0090] Example 1: Electric vehicle battery performance optimization

[0091] 1) Application background:

[0092] The battery performance of electric vehicles directly affects the vehicle's mileage and life. Polycrystalline NCM electrode materials are widely used in electric vehicle batteries because they can provide higher energy density. However, electrode particles are prone to cracking and powdering during the charge and discharge process, affecting the cycle life and safety of the battery.

[0093] 2) Application method:

[0094] Using the prediction method of the present invention, electric vehicle manufacturers can predict the cracking and pulverization behavior of electrodes under different design and use conditions through simulation models. By adjusting the charging strategy and use environment in the battery management system, battery performance can be optimized and its service life can be extended.

[0095] Example 2: Portable electronic device battery maintenance

[0096] 1) Application background:

[0097] Portable electronic devices, such as smartphones and laptops, have extremely high requirements for battery reliability and maintenance. The health of the battery is directly related to the service life of the device and the user experience.

[0098] 2) Application method:

[0099] Using the method of the present invention, equipment manufacturers can simulate the performance of batteries under different usage modes and environmental conditions during the design phase. In addition, by predicting the cracking and pulverization trend, manufacturers can set more appropriate battery maintenance reminders in advance to help users effectively manage battery use and avoid sudden failures caused by battery mechanical failure.

[0100] In the above two embodiments, by accurately predicting the cracking and pulverization trend of polycrystalline NCM electrode particles in actual applications, the performance and safety of lithium-ion batteries can be significantly improved. This prediction capability not only helps optimize battery design, but also provides important information for daily maintenance and performance management of batteries.

[0101] like Figure 1 and Figure 2 As shown, a method for predicting cracking and pulverization of polycrystalline NCM electrode particles constructed by the present invention mainly includes:

[0102] S1, construct anisotropic polycrystalline fracture phase field model, including grain boundary phase field equation, solid mechanics equation, Li + Diffusion equation and fracture phase field equation.

[0103] S2, construct the two-dimensional geometry of polycrystalline NCM electrode particles, set the parameters required for the physical field, perform meshing and set the initial conditions and boundary conditions.

[0104] S3, using finite element simulation software to perform numerical solution, the cracking and pulverization distribution of polycrystalline NCM electrode particles was obtained.

[0105] The grain boundary phase field equation constructed in S1 is:

[0106]

[0107] Where p is the grain boundary phase field order parameter, l p is the grain boundary phase field length parameter, represents the Hamiltonian operator. Modified critical energy release rate G p It can be written as

[0108] G p =g(p)G c_G +(1-g(p))G c_GB

[0109] Where g(p) = (1-p) 2 , G c_G is the critical energy release rate of the grain, G c_GB is the critical energy release rate at the grain boundary.

[0110] Specifically, the solid mechanics equation constructed in S1 is:

[0111]

[0112] in, is the Hamiltonian operator, C(d) represents the modified elastic stiffness tensor;

[0113] εe Represent the elastic strain tensor:

[0114] ε e =ε-ε c ,

[0115] ε is the total strain tensor;

[0116] ε c is the chemical strain tensor:

[0117] ε c =(cc ref )β ij ,

[0118] β ij is the anisotropic change in volume per unit concentration;

[0119] c represents Li + Concentration, c ref Indicates reference Li + concentration.

[0120] In the formula, the expression of the modified elastic stiffness tensor C(d) is:

[0121]

[0122] Among them, C 0 is the elastic stiffness tensor of the normal material, k 0 is the bulk modulus, I is the unit matrix, sign - is the sign function, ε e is the elastic strain tensor, tr(ε e ) is ε e traces;

[0123] g(d) is the phase field degenerate function:

[0124] g(d)=(1-d) 2 +k,

[0125] k is a numerical stability parameter.

[0126] Li constructed in S1 + The diffusion equation is:

[0127]

[0128] Where J is the Li per unit area per unit time + Molar flux, D represents Li + The diffusion rate, represents the Hamiltonian operator, Ω ij represents partial molar volume, R represents ideal gas constant, T represents Kelvin temperature, and c represents Li+ Concentration, c max Represents the maximum amount of Li that the material can accommodate + Concentration, σ h Represents the hydrostatic stress.

[0129] The fracture phase field equation constructed in S1 is:

[0130]

[0131] Where G p Is the modified critical energy release rate of the polycrystalline NCM electrode particle material; d is the fracture phase field order parameter, d = 1 indicates that the material is completely damaged, d = 0 indicates that the material is intact (i.e., no failure), and 0 < d < 1 indicates a transitional state; l d Represents the length parameter of the fracture phase field, Represents the Hamiltonian operator, and H is defined as the historical maximum tensile strain energy density:

[0132] H = maxΨ e (t)

[0133] Where Ψ e (t) represents the tensile elastic strain energy density, and its expression is:

[0134]

[0135] Where g(d) is the phase field degradation function, ε e Is the elastic strain tensor, C 0 Is the elastic stiffness tensor of the normal material, ε vol Is the volumetric component of the elastic strain, ε dev Is the deviatoric component of the elastic strain, tr(ε e ) is the trace of ε e Trace.

[0136] The two-dimensional geometry of the polycrystalline NCM electrode particles constructed in S2 is generated using the Voronoi diagram algorithm, as Figure 3 Shown. The generated two-dimensional polycrystalline geometry is circular with a radius of 5 μm, and the internal primary particles are irregular hexagons with an average particle size of 0.57 μm, randomly sized and shaped.

[0137] The two-dimensional geometry mesh of the polycrystalline NCM electrode particles constructed in S2 is divided using triangular meshes, and the maximum mesh size is set to 0.02 μm. The constructed mesh contains a total of 508,636 triangular regions, and the degrees of freedom during simulation are 5.1 million.

[0138] The physical parameters set in S2 are: Young's modulus E = 120 GPa, Poisson's ratio ν = 0.3, density ρ = 4.14 g / cm 3、Temperature T=300K、Li + Diffusion rate D = 7 × 10 -15 m 2 / s, maximum Li + Concentration max =35164mol / m 3 , ReferenceLi + Concentration max =31648mol / m 3 , grain boundary phase field length parameter l p =0.05μm, fracture phase field length parameter l d =0.05μm, grain boundary critical energy release rate G c_GB =2N / m, primary particle energy release rate G c_G =10N / m. The volume change per unit concentration and the partial molar volume are anisotropic, where the volume change per unit concentration is set to: β a =β b =0.597cm 3 / mol, β c =1.052cm 3 / mol. The partial molar volume is set to: Ω a =Ω b =1.79cm 3 / mol,Ω c =3.16cm 3 / mol. All primary particle orientations are randomly generated and set using scripts;

[0139] The initial conditions set in S2 are: the initial value of the grain boundary phase field is set to 0, Li + The initial diffusion concentration is set to 31648 mol / m 3 , the initial displacement of solid mechanics is set to no displacement, and the initial value of the fracture phase field is set to 0;

[0140] The boundary conditions set in S2 are: Dirichlet boundary conditions are set at the grain boundaries of polycrystalline NCM electrode particles in the grain boundary phase field, and the value is set to 1; Li + The flux size of the polycrystalline NCM electrode particles in the diffusion equation is set to 7.33×10 -5 mol / (m 2 ·s); free boundary conditions are used for polycrystalline NCM electrode particles in solid mechanics.

[0141] In S2, for each primary particle in the polycrystalline NCM electrode particles, an independent spatial coordinate system is constructed, and the orientation of the coordinate system is the crystal direction of the primary particle.

[0142] In step S3, two solving steps are used to numerically solve the model. The first step is to solve the grain boundary phase field equation in a steady state to obtain and store the modified critical energy release rate distribution. The second step is to solve the solid mechanics equation, Li + The diffusion equation and the fracture phase field equation are solved by transferring the solution stored in the first step to the second step as the value of the modified critical energy release rate.

[0143] In step S3, the cracking and pulverization distribution of the polycrystalline NCM electrode particles is the distribution of the fracture phase field order parameter. The evolution of the cracking and pulverization distribution of the polycrystalline NCM electrode particles obtained by simulation calculation is as follows: Figure 4 As shown in Figure 2, the cracking and pulverization evolution process of polycrystalline NCM electrode particles under different primary particle sizes is as follows: Figure 5 As shown in Figure 2, the cracking and pulverization evolution process of polycrystalline NCM electrode particles under different secondary particle sizes is as follows: Figure 6 As shown in the figure, the cracking and pulverization results of NCM electrode particles with different structures are compared. Figure 7 shown.

[0144] like Figure 8 As shown, the polycrystalline NCM electrode particle cracking and pulverization prediction system provided by the embodiment of the present invention includes:

[0145] Model building module, used to construct anisotropic polycrystalline fracture phase field model, including grain boundary phase field equation, solid mechanics equation, Li + Diffusion equations and fracture phase field equations;

[0146] 2D geometry construction module, used to construct the 2D geometry of polycrystalline NCM electrode particles, set the parameters required for the physical field, perform meshing and set initial conditions and boundary conditions;

[0147] The numerical solution module is used to perform numerical solution using finite element simulation software to obtain the cracking and pulverization distribution of polycrystalline NCM electrode particles.

[0148] An application embodiment of the present invention provides a computer device, which includes a memory and a processor. The memory stores a computer program. When the computer program is executed by the processor, the processor executes the steps of a method for predicting cracking and pulverization of polycrystalline NCM electrode particles.

[0149] The application embodiment of the present invention provides a computer-readable storage medium storing a computer program. When the computer program is executed by a processor, the processor executes the steps of a method for predicting cracking and pulverization of polycrystalline NCM electrode particles.

[0150] The application embodiment of the present invention provides an information data processing terminal, which is used to implement a multi-crystalline NCM electrode particle cracking and pulverization prediction system.

[0151] In addition to the above embodiments, embodiments of the present invention also include: (1) predicting the cracking and pulverization of NCM electrode particles with different primary particle average particle sizes and different secondary particle sizes; (2) predicting the cracking and pulverization of NCM electrode particles with different primary particle shapes and arrangement regularities; (3) predicting the cracking and pulverization of NCM electrode particles with special structures, such as core-shell structures.

[0152] The use of traditional mechanical models to predict the cracking and pulverization of NCM electrode particles is often quite different from experimental observations. Traditional mechanical models cannot accurately reflect the concentration concentration inside the particles, so the predictions are inaccurate: (1) It is impossible to accurately predict whether cracking will occur, and (2) It is impossible to accurately predict the degree of cracking. In contrast, the physical model used in the present invention more realistically reflects the physical processes inside the NCM electrode particles, and the prediction results are more consistent with experimental observations. An intuitive proof is that the present invention can directly prove the mechanical superiority of the core-shell structured NCM electrode particles, which is consistent with mainstream experimental observations, such as Figure 7 shown.

[0153] It should be noted that the embodiments of the present invention can be implemented by hardware, software, or a combination of software and hardware. The hardware part can be implemented using dedicated logic; the software part can be stored in a memory and executed by an appropriate instruction execution system, such as a microprocessor or dedicated design hardware. It can be understood by a person of ordinary skill in the art that the above-mentioned devices and methods can be implemented using computer executable instructions and / or contained in a processor control code, such as a carrier medium such as a disk, CD or DVD-ROM, a programmable memory such as a read-only memory (firmware), or a data carrier such as an optical or electronic signal carrier. Such code is provided on the carrier medium. The device and its modules of the present invention can be implemented by hardware circuits such as very large-scale integrated circuits or gate arrays, semiconductors such as logic chips, transistors, etc., or programmable hardware devices such as field programmable gate arrays, programmable logic devices, etc., can also be implemented by software executed by various types of processors, and can also be implemented by a combination of the above-mentioned hardware circuits and software, such as firmware.

[0154] The above description is only a specific implementation mode of the present invention, but the protection scope of the present invention is not limited thereto. Any modifications, equivalent substitutions and improvements made by any technician familiar with the technical field within the technical scope disclosed by the present invention and within the spirit and principle of the present invention should be covered by the protection scope of the present invention.

Claims

1. A method for predicting cracking and pulverization of polycrystalline NCM electrode particles. It is characterized in that include: S1, construct anisotropic polycrystalline fracture phase field model, including grain boundary phase field equation, solid mechanics equation, Li + Diffusion equations and fracture phase field equations; S2, construct the two-dimensional geometry of polycrystalline NCM electrode particles, set the parameters required for the physical field, perform meshing and set initial conditions and boundary conditions; S3, using finite element simulation software to perform numerical solution, the cracking and pulverization distribution of polycrystalline NCM electrode particles was obtained.

2. The method for predicting cracking and pulverization of polycrystalline NCM electrode particles according to claim 1, It is characterized in that In step S1, the grain boundary phase field equation is used to calculate the modified critical energy release rate inside the polycrystalline NCM electrode particles, and the solid mechanics equation is used to calculate the stress and elastic strain energy density distribution. + The diffusion equation is used to calculate Li + Concentration distribution, fracture phase field equation is used to calculate cracking and powdering distribution.

3. The method for predicting cracking and pulverization of polycrystalline NCM electrode particles according to claim 1, It is characterized in that In step S2, the two-dimensional geometry of the polycrystalline NCM electrode particles is drawn by the Voronoi diagram algorithm; the set physical parameters include Young's modulus, Poisson's ratio, density, temperature, Li + Diffusion rate, maximum Li + Concentration, reference Li + concentration, grain boundary phase field length parameter, fracture phase field length parameter, grain boundary critical energy release rate, primary particle energy release rate, unit concentration volume change, partial molar volume, all primary particle crystal directions; the mesh is divided into triangular meshes, and the maximum mesh size is set to 0.02μm; the initial conditions include the initial value of the grain boundary phase field, Li + Initial concentration of diffusion, initial displacement of solid mechanics, initial value of fracture phase field; boundary conditions, Dirichlet boundary conditions of grain boundary phase field, Li + Diffusion flux, free boundary conditions in solid mechanics.

4. The method for predicting cracking and pulverization of polycrystalline NCM electrode particles according to claim 1, It is characterized in that In the step S2, an independent space coordinate system is constructed for each primary particle in the polycrystalline NCM electrode particles, and the orientation of the coordinate system is the crystal orientation of the primary particle.

5. The method for predicting cracking and pulverization of polycrystalline NCM electrode particles according to claim 1, It is characterized in that In step S3, two solving steps are used to numerically solve the model; the first step is to solve the grain boundary phase field equation in a steady state to obtain and store the modified critical energy release rate distribution; the second step is to solve the solid mechanics equation, Li + The diffusion equation and the fracture phase field equation transfer the solution stored in the first step to the second step as the value of the critical energy release rate.

6. The method for predicting cracking and pulverization of polycrystalline NCM electrode particles according to claim 1, It is characterized in that In the step S3, the cracking and pulverization distribution of the polycrystalline NCM electrode particles is the distribution of the fracture phase field order parameter.

7. A system for predicting cracking and pulverization of polycrystalline NCM electrode particles, which implements the method for predicting cracking and pulverization of polycrystalline NCM electrode particles according to any one of claims 1 to 6, It is characterized in that include: Model building module, used to construct anisotropic polycrystalline fracture phase field model, including grain boundary phase field equation, solid mechanics equation, Li + Diffusion equations and fracture phase field equations; 2D geometry construction module, used to construct the 2D geometry of polycrystalline NCM electrode particles, set the parameters required for the physical field, perform meshing and set initial conditions and boundary conditions; The numerical solution module is used to perform numerical solution using finite element simulation software to obtain the cracking and pulverization distribution of polycrystalline NCM electrode particles.

8. A computer device, It is characterized in that The computer device comprises a memory and a processor. The memory stores a computer program. When the computer program is executed by the processor, the processor executes the steps of the method for predicting cracking and pulverization of polycrystalline NCM electrode particles as claimed in any one of claims 1 to 6.

9. A computer-readable storage medium, It is characterized in that A computer program is stored, and when the computer program is executed by a processor, the processor executes the steps of the method for predicting cracking and pulverization of polycrystalline NCM electrode particles as claimed in any one of claims 1 to 6.

10. An information data processing terminal, It is characterized in that The information data processing terminal includes the multi-crystalline NCM electrode particle cracking and pulverization prediction system as described in claim 7.

Citation Information

Patent Citations

  • SOFC numerical simulation method under multi-physical field coupling effect

    CN111625929A

  • Core-shell NCM electrode particle mechanical failure prediction method and system

    CN117574682A

  • Positive electrode material and preparation method thereof, secondary battery and electric equipment

    CN117613257A

  • Lithium ion battery multi-physical field electrochemical-force-phase field coupling model and modeling method

    CN117725798A

  • Positive electrode material and preparation method and use therefor, lithium-ion battery positive electrode pole piece, and lithium-ion battery

    US20230207802A1