Etching compensation method

By obtaining the attenuation coefficient and associated parameters of the etching rate of the medicine liquid, compensating the etching time, the problems of waste and inconsistent morphology of traditional Chinese medicine liquid by wet etching are solved, and more efficient etching time management and wafers are achieved Surface morphology consistency.

CN119092426APending Publication Date: 2024-12-06BAODING DRY CORE INTEGRATED CIRCUIT (HANGZHOU) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411238854.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

The existing wet etching process has severe waste of medicine and low etching time compensation accuracy, resulting in inconsistent wafer surface morphology.

Method used

By obtaining the attenuation coefficient and associated parameters of the etching rate decay of the drug liquid, the compensation etching time is calculated and the etching time of the wafer to be etched is adjusted to reduce the etching amount reduction problem caused by the etching rate decay during the use of the drug liquid. , improve the consistency of the shape.

Benefits of technology

Effectively reduce waste of medicine liquid, improve the compensation accuracy of etching time, ensure the consistency of etching morphology of each batch of wafers, and there is no need to frequently change the medicine liquid.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119092426A_ABST
    Figure CN119092426A_ABST
Patent Text Reader

Abstract

The etching compensation method comprises the following steps: acquiring initial etching time required for etching a to-be-etched layer with a preset thickness on the surface of a first batch of wafers by liquid medicine; acquiring an attenuation coefficient of etching rate attenuation of the liquid medicine in the etching process; acquiring associated parameters causing the etching rate of the liquid medicine to be attenuated; and adding the product result of the attenuation coefficient and the correlation parameter and the initial etching time to serve as the actual etching time of the wafer to be etched. The compensation etching time of the wafer to be etched is calculated by obtaining the attenuation coefficient of the etching rate attenuation of the liquid medicine in the etching process and the associated parameters causing the etching rate attenuation of the liquid medicine, so that the problem that the etching amount is reduced due to the etching rate attenuation when the liquid medicine is used is solved. According to the technical scheme, the liquid medicine does not need to be replaced in the whole using period of the liquid medicine, liquid medicine waste can be effectively reduced, targeted etching time compensation can be carried out according to different correlation parameters of each batch of wafers, and each batch of wafers can obtain finer compensation etching time.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of semiconductor manufacturing, and in particular to an etching compensation method. Background Art

[0002] The semiconductor etching process is to use physical, chemical or both methods to purposefully remove the part of the thin film layer that is not covered by the resist, so that the same pattern as that on the resist film can be obtained on the thin film. The etching process can be divided into dry etching process and wet etching process. Wet etching is a traditional etching method. The specific principle is to immerse the wafer in a certain chemical reagent or reagent solution, so that the part of the thin film surface that is not covered by the resist reacts chemically with the reagent and is removed. Its advantages are mainly simple operation, low equipment requirements, easy mass production, and good etching selectivity.

[0003] However, there are still many problems in the wet etching process in the prior art. Summary of the invention

[0004] The technical problem solved by the invention is to provide an etching compensation method to reduce the waste of chemical solution and improve the accuracy of etching time compensation.

[0005] To solve the above problems, the present invention provides an etching compensation method, including: obtaining the initial etching time required for a chemical solution to etch a layer to be etched with a preset thickness on the surface of a first batch of wafers; obtaining the attenuation coefficient of the etching rate of the chemical solution during the etching process; obtaining the associated parameters that cause the etching rate of the chemical solution to attenuate before etching the wafer to be etched; taking the product of the attenuation coefficient and the associated parameters as the compensation etching time of the wafer to be etched; and taking the sum of the compensation etching time and the initial etching time as the actual etching time of the wafer to be etched.

[0006] Optionally, the method for obtaining the initial etching time includes: providing a first tank solution; forming the etched layer of the preset thickness on the surface of a first batch of wafers; detecting the initial etching rate of the first tank solution in etching the etched layer; and taking the ratio of the preset thickness to the initial etching rate as the initial etching time.

[0007] Optionally, the attenuation coefficient includes: a first attenuation coefficient in which the etching rate of the chemical solution decays with time; and a second attenuation coefficient in which the etching rate of the chemical solution decays with an increase in the number of wafers processed.

[0008] Optionally, the method for obtaining the first attenuation coefficient includes: obtaining a first etching time required for the chemical solution to etch the layer to be etched of the preset thickness on the surface of the first batch of wafers; allowing the chemical solution to stand for a static treatment; after the chemical solution has been allowed to stand for a chemical solution usage cycle time, obtaining a second etching time required for the chemical solution to etch the layer to be etched of the preset thickness on the surface of the second batch of wafers; and taking the ratio of the difference between the second etching time and the first etching time to the chemical solution usage cycle time as the first attenuation coefficient.

[0009] Optionally, the method for obtaining the first etching time and the second etching time includes: providing a second tank chemical solution; forming the layer to be etched of the preset thickness on the surface of a first batch of wafers; detecting a first etching rate of the layer to be etched by the chemical solution in the second tank; taking the ratio of the preset thickness to the first etching rate as the first etching time; after the chemical solution is allowed to stand for the chemical solution usage cycle time, detecting a second etching rate of the layer to be etched by the chemical solution in the second tank; taking the ratio of the preset thickness to the second etching rate as the second etching time.

[0010] Optionally, the first tank medicine liquid and the second tank medicine liquid are different tank medicine liquids.

[0011] Optionally, the first tank of medicine liquid and the second tank of medicine liquid are the same tank of medicine liquid.

[0012] Optionally, obtaining the first etching time and obtaining the initial etching time are the same step.

[0013] Optionally, the method for obtaining the second attenuation coefficient includes: obtaining a third etching time required by the chemical solution to etch the layer to be etched of the preset thickness on the surface of the first batch of wafers; processing the wafers with the maximum processing number of the single-tank chemical solution based on the chemical solution; after the chemical solution processes the wafers with the maximum processing number of the single-tank chemical solution, obtaining a fourth etching time required by the chemical solution to etch the layer to be etched of the preset thickness on the surface of an additional batch of wafers; and taking the ratio of the difference between the fourth etching time and the third etching time to the maximum processing number of the single-tank chemical solution as the second attenuation coefficient.

[0014] Optionally, the method for obtaining the third etching time and the fourth etching time includes: providing a third tank chemical solution; forming the layer to be etched of the preset thickness on the surface of a first batch of wafers; detecting a third etching rate at which the third tank chemical solution etches the layer to be etched; using the ratio of the preset thickness to the third etching rate as the third etching time; after the chemical solution processes the wafers with the maximum processing number of the single tank chemical solution, detecting a fourth etching rate at which the third tank chemical solution etches the layer to be etched; using the ratio of the preset thickness to the fourth etching rate as the fourth etching time.

[0015] Optionally, the first tank medicine solution and the third tank medicine solution are different tank medicine solutions.

[0016] Optionally, the first tank medicine solution and the third tank medicine solution are the same tank medicine solution.

[0017] Optionally, obtaining the third etching time and obtaining the initial etching time are the same step.

[0018] Optionally, the associated parameters causing the etching rate of the solution to decay include: the time the solution has been used before etching the wafer to be etched; and the number of wafers processed by the solution before etching the wafer to be etched.

[0019] Optionally, the method for obtaining the compensatory etching time includes: adding the product of the used time and the first attenuation coefficient and the product of the number of processed wafers and the second attenuation coefficient as the compensatory etching time of the wafer to be etched.

[0020] Optionally, the chemical solution includes: aluminum etching solution.

[0021] Optionally, the material of the layer to be etched includes: aluminum, aluminum-silicon-copper or aluminum-silicon.

[0022] Compared with the prior art, the technical solution of the present invention has the following advantages:

[0023] In the etching compensation method of the technical solution of the present invention, by obtaining the attenuation coefficient of the etching rate attenuation of the chemical solution during the etching process, and the associated parameters that cause the etching rate of the chemical solution to attenuate before etching the wafer to be etched, the compensation etching time of the wafer to be etched is calculated, thereby reducing the problem of reduced etching amount caused by the etching rate attenuation during the use of the chemical solution, and improving the consistency of the morphology of the to-be-etched layer of the wafer after etching at different periods during the entire use cycle of the chemical solution. The chemical solution does not need to be replaced during the entire use cycle of the chemical solution, which can effectively reduce the waste of the chemical solution, and according to the different associated parameters of each batch of wafers, targeted etching time compensation can be performed, so that each batch of wafers can obtain a more refined compensation etching time.

[0024] Furthermore, the first tank chemical solution and the second tank chemical solution are the same tank chemical solution, and obtaining the first etching time and obtaining the initial etching time are the same step, thereby simplifying the steps of obtaining the initial etching time and the first attenuation coefficient and improving efficiency.

[0025] Furthermore, the first tank solution and the third tank solution are the same tank solution, and obtaining the third etching time and obtaining the initial etching time are the same step, thereby simplifying the steps of obtaining the initial etching time and the second attenuation coefficient and improving efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 It is a schematic diagram showing the changes of etching time and etching rate with the use time of chemical solution and the number of wafers processed;

[0027] Figure 2 It is a schematic diagram of the process of the etching compensation method according to an embodiment of the present invention;

[0028] Figure 3 It is a schematic diagram showing that the etching time and etching rate change with the use time of the chemical solution and the number of wafers processed in an embodiment of the present invention. DETAILED DESCRIPTION

[0029] As described in the background art, however, the wet etching process in the prior art still has many problems, which will be described in detail below.

[0030] Figure 1 It is a schematic diagram showing how etching time and etching rate change with the use time of chemical solution and the number of wafers processed.

[0031] Aluminum etching solution is a chemical solution specially used for wet etching of aluminum film layer on the surface of semiconductor wafers. In the semiconductor manufacturing process, aluminum etching solution will etch the AL / ALSICU / ALSI film layer on the surface of the wafer to obtain the metal layer pattern. However, the aluminum etching solution will slowly decompose or consume as the solution is used and the number of processed wafers increases, and the etching rate will gradually decrease, resulting in large differences in the cross-sectional morphology of the aluminum film layer on the surface of the wafer after wet etching at different times, thus affecting the performance and consistency of semiconductor chips.

[0032] In the semiconductor manufacturing process, wet aluminum etching can control the aluminum etching rate within a relatively stable range by frequently changing the solution, thereby maintaining the consistency of the cross-sectional morphology of the aluminum film layer on the wafer surface after wet etching at different times. However, this method wastes a lot of aluminum etching solution, is not conducive to controlling product production costs, and is generally not used in semiconductor processes.

[0033] Please refer to Figure 1Another method is to simply divide the entire life cycle of the aluminum etching solution into three periods: early, middle, and final. An etching time is set for each period (the longer the solution is used, the longer the set etching time is). Fixed etching times for different periods are used to maintain the consistency of the wet etching profile morphology of the aluminum film layer on the wafer surface at different periods as much as possible.

[0034] The entire life cycle of the aluminum etching solution is simply divided into three periods: the early stage, the middle stage, and the final stage. The processing needs to select the etching time of the corresponding period according to the current period of the aluminum etching solution to ensure the etching consistency as much as possible. At the same time, the etching morphology of the wafer processed in the same period is better than the etching morphology of using one time in the entire liquid replacement cycle. However, only a rough correction of the solution etching rate in different periods was performed, and the effect of completely eliminating the influence of the solution rate change in the entire liquid replacement cycle was not achieved.

[0035] On this basis, the present invention provides an etching compensation method, which obtains the attenuation coefficient of the etching rate attenuation of the chemical solution during the etching process, and the associated parameters that cause the etching rate of the chemical solution to attenuate before etching the wafer to be etched, and then calculates the compensation etching time of the wafer to be etched, thereby reducing the problem of reduced etching amount caused by the etching rate attenuation during the use of the chemical solution, and improving the consistency of the morphology of the to-be-etched layer of the wafer after etching at different periods during the entire use cycle of the chemical solution. The chemical solution does not need to be replaced during the entire use cycle of the chemical solution, which can effectively reduce the waste of the chemical solution, and according to the different associated parameters of each batch of wafers, targeted etching time compensation can be performed, so that each batch of wafers can obtain a more refined compensation etching time.

[0036] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.

[0037] Figure 2 is a flow chart of an etching compensation method according to an embodiment of the present invention, comprising:

[0038] Step S101, obtaining the initial etching time required by the chemical solution to etch the first batch of wafer surfaces with a preset thickness of the to-be-etched layer;

[0039] Step S102, obtaining an attenuation coefficient of the etching rate attenuation of the chemical solution during the etching process;

[0040] Step S103, obtaining the associated parameters that cause the etching rate of the chemical solution to decay before etching the wafer to be etched;

[0041] Step S104, taking the product of the attenuation coefficient and the associated parameter as the compensation etching time of the wafer to be etched;

[0042] Step S105 , adding the compensation etching time to the initial etching time is used as the actual etching time of the wafer to be etched.

[0043] The steps of the etching compensation method will be described in detail below with reference to the accompanying drawings.

[0044] Figure 3 It is a schematic diagram showing that the etching time and etching rate change with the use time of the chemical solution and the number of wafers processed in an embodiment of the present invention.

[0045] Please continue to refer to Figure 2 In step S101, the initial etching time T0 required for the chemical solution to etch the first batch of wafer surfaces with a preset thickness Y on the surface of the to-be-etched layer (not shown) is obtained.

[0046] It should be noted that the initial etching time T0 is the time required to etch the layer to be etched with the preset thickness Y when the solution has not been used for a long time and the effective ingredients in the solution have been decomposed, and a large number of wafers have not been processed and the effective ingredients in the solution have been consumed. It can be understood that the first batch of wafers are the wafers that are first put into the solution tank for etching after the solution is changed.

[0047] In this embodiment, the number of wafers in the first batch can be from 1 wafer to the maximum number of wafers allowed to be placed in one batch (such as 25 wafers).

[0048] In this embodiment, the chemical solution is aluminum etching solution; the corresponding material of the layer to be etched can be aluminum, aluminum silicon copper or aluminum silicon.

[0049] In this embodiment, the method for obtaining the initial etching time T0 includes: providing a first tank solution; forming the layer to be etched with the preset thickness Y on the surface of a first batch of wafers; detecting the initial etching rate ER of the first tank solution etching the layer to be etched; and taking the ratio of the preset thickness Y to the initial etching rate ER as the initial etching time T0, that is, T0=Y / ER.

[0050] It should be noted that the etching process of the first batch of wafers needs to be completed within the shortest possible time after changing the liquid (such as within 0.5 hours after the liquid temperature stabilizes) to reduce the impact of the liquid usage time on the initial etching rate ER, and the initial etching rate ER can be collected multiple times and the average value is obtained.

[0051] Please continue to refer to Figure 2 In step S102, the attenuation coefficient of the etching rate attenuation of the chemical solution during the etching process is obtained.

[0052] In actual production, it is found that long-term use will cause the effective ingredients in the solution to decompose. Even if the newly replaced solution is left standing for a long time (during which no wafers are processed), the etching rate will decrease. In addition, as the number of wafers processed by the solution increases, the effective ingredients in the solution are consumed in large quantities, which in turn leads to a decrease in the etching rate.

[0053] Therefore, in this embodiment, the attenuation coefficient includes: a first attenuation coefficient K1 in which the etching rate of the chemical solution decays as time increases; and a second attenuation coefficient K2 in which the etching rate of the chemical solution decays as the number of wafers processed increases.

[0054] In this embodiment, the method for obtaining the first attenuation coefficient K1 includes: obtaining the first etching time T1 required for the chemical solution to etch the layer to be etched with the preset thickness Y on the surface of the first batch of wafers; subjecting the chemical solution to a static treatment (without processing any wafers during this period); after the chemical solution has been static for a chemical solution usage cycle time Tmax (such as 48 hours), obtaining the second etching time T2 required for the chemical solution to etch the layer to be etched with the preset thickness Y on the surface of the second batch of wafers; and taking the ratio of the difference between the second etching time T2 and the first etching time T1 to the chemical solution usage cycle time Tmax as the first attenuation coefficient K1, that is, K1 = (T2-T1) / Tmax.

[0055] In this embodiment, the method for obtaining the first etching time T1 and the second etching time T2 includes: providing a second tank chemical solution; forming the layer to be etched of the preset thickness Y on the surface of a first batch of wafers; detecting a first etching rate ER1 of the second tank chemical solution etching the layer to be etched; taking the ratio of the preset thickness Y to the first etching rate ER1 as the first etching time T1, that is, T1=Y / ER1; after the chemical solution is allowed to stand for the chemical solution usage cycle time Tmax, detecting a second etching rate ER2 of the second tank chemical solution etching the layer to be etched; taking the ratio of the preset thickness Y to the second etching rate ER2 as the second etching time T2, that is, T2=Y / ER2.

[0056] In this embodiment, the first tank chemical solution and the second tank chemical solution are the same tank chemical solution; obtaining the first etching time T1 and obtaining the initial etching time T0 are the same step, thereby simplifying the steps of obtaining the initial etching time T0 and the first attenuation coefficient K1 and improving efficiency.

[0057] In this embodiment, the method for obtaining the second attenuation coefficient K2 includes: obtaining the third etching time T3 required for the chemical solution to etch the layer to be etched with the preset thickness Y on the surface of the first batch of wafers; based on the chemical solution processing the wafers with the maximum processing number Nmax (such as 2000 pieces) of the single-tank chemical solution; after the chemical solution processes the wafers with the maximum processing number Nmax of the single-tank chemical solution, obtaining the fourth etching time T4 required for the chemical solution to etch the layer to be etched with the preset thickness Y on the surface of an additional batch of wafers; taking the ratio of the difference between the fourth etching time T4 and the third etching time T3 to the maximum processing number Nmax of the single-tank chemical solution as the second attenuation coefficient K2, that is, K2 = (T4-T3) / Nmax.

[0058] It should be noted that after completing the processing of the wafers with the maximum processing number Nmax of the single-tank solution, the processing of the additional batch of wafers should be completed in the shortest possible time (such as within 1 hour after maintaining the temperature of the solution stable) to reduce the impact of the solution usage time on the etching rate.

[0059] In this embodiment, the method for obtaining the third etching time T3 and the fourth etching time T4 includes: providing a third tank chemical solution; forming the layer to be etched with the preset thickness Y on the surface of a first batch of wafers; detecting a third etching rate ER3 of the third tank chemical solution etching the layer to be etched; taking the ratio of the preset thickness Y to the third etching rate ER3 as the third etching time T3, that is, T3=Y / ER3; after the chemical solution processes the wafers with the single tank chemical solution maximum processing number Nmax, detecting the fourth etching rate ER4 of the third tank chemical solution etching the layer to be etched; taking the ratio of the preset thickness Y to the fourth etching rate ER4 as the fourth etching time T4, that is, T4=Y / ER4.

[0060] It should be noted that, in this embodiment, the solution in the second tank needs to be left standing for a long time until the solution reaches the solution usage cycle time Tmax, and the wafer needs to be processed in the solution in the third tank all the time, so the solution in the second tank and the solution in the third tank are different tank solutions.

[0061] In this embodiment, since the first tank solution and the second tank solution are the same tank solution, the first tank solution and the third tank solution are different tank solutions. Therefore, two tank solutions are required in the process of obtaining the initial etching time T0, the first attenuation coefficient K1 and the second attenuation coefficient K2.

[0062] In other embodiments, the first tank solution, the second tank solution and the third tank solution may all be different tank solutions, that is, three tank solutions are required in the process of obtaining the initial etching time T0, the first attenuation coefficient K1 and the second attenuation coefficient K2.

[0063] In other embodiments, the first tank solution and the third tank solution may be the same tank solution, and the corresponding steps of obtaining the third etching time T3 and obtaining the initial etching time T0 are the same step, thereby simplifying the steps of obtaining the initial etching time T0 and the first attenuation coefficient K1 and improving efficiency. The second tank solution is different from the first tank solution and the third tank solution, that is, two tank solutions are required in the process of obtaining the initial etching time T0, the first attenuation coefficient K1 and the second attenuation coefficient K2.

[0064] It should be noted that, in this embodiment, the liquid use cycle time Tmax and the single tank liquid maximum processing quantity Nmax are constant standards for whether liquid replacement is required. If either of the two is reached first, liquid replacement is required.

[0065] Please continue to refer to Figure 2 In step S103, the associated parameters that cause the etching rate of the chemical solution to attenuate before etching the wafer to be etched are obtained.

[0066] In this embodiment, the associated parameters causing the etching rate of the chemical solution to decay include: the time Tu that the chemical solution has been used before etching the wafer to be etched; and the number Xp of wafers that have been processed by the chemical solution before etching the wafer to be etched.

[0067] Please continue to refer to Figure 2 In step S104, the product of the attenuation coefficient and the associated parameter is used as the compensation etching time Tc of the wafer to be etched.

[0068] In this embodiment, the method for obtaining the compensation etching time Tc includes: adding the product of the used time Tu and the first attenuation coefficient K1 and the product of the processed wafer number Xp and the second attenuation coefficient K2 as the compensation etching time Tc of the wafer to be etched, that is, Tc=K1*Tu+K2*Xp.

[0069] It should be noted that, in this embodiment, by obtaining the product of the used time Tu and the first attenuation coefficient K1, the time when the etching rate is reduced due to the decomposition of the effective components of the solution due to standing still can be compensated; by obtaining the product of the number of processed wafers Xp and the second attenuation coefficient K2, the time when the etching rate is reduced due to the consumption of the effective components of the solution during the wafer processing can be compensated.

[0070] Please continue to refer to Figure 2 In step S105, the compensation etching time Tc is added to the initial etching time T0 to obtain the actual etching time Tr of the wafer to be etched, that is, Tr=T0+Tc.

[0071] Please refer to Figure 3 , by obtaining the attenuation coefficient of the etching rate attenuation of the chemical solution during the etching process, and the associated parameters that cause the etching rate of the chemical solution to attenuate before etching the wafer to be etched, the compensation etching time Tc of the wafer to be etched is calculated, thereby reducing the problem of reduced etching amount caused by the etching rate attenuation during the use of the chemical solution, and improving the consistency of the morphology of the to-be-etched layer of the wafer after etching at different periods during the entire use cycle of the chemical solution. The chemical solution does not need to be replaced during the entire use cycle of the chemical solution, which can effectively reduce the waste of the chemical solution, and according to the different associated parameters of each batch of wafers, targeted etching time compensation can be performed, so that each batch of wafers can obtain a more refined compensation etching time Tc.

[0072] It should be noted that, in this embodiment, the thickness of the layer to be etched on the wafer to be etched needs to be consistent with the preset thickness Y.

[0073] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.

Claims

1. An etching compensation method, It is characterized in that include: Obtaining the initial etching time required for the chemical solution to etch the first batch of wafer surfaces with a preset thickness of the to-be-etched layer; Obtaining an attenuation coefficient of the etching rate attenuation of the chemical solution during the etching process; Obtaining the associated parameters that cause the etching rate of the chemical solution to decay before etching the wafer to be etched; The product of the attenuation coefficient and the associated parameter is used as the compensation etching time of the wafer to be etched; The sum of the compensation etching time and the initial etching time is used as the actual etching time of the wafer to be etched.

2. The etching compensation method according to claim 1, It is characterized in that The method for obtaining the initial etching time includes: providing a first tank solution; forming the etched layer of the preset thickness on the surface of a first batch of wafers; detecting the initial etching rate of the first tank solution etching the etched layer; and taking the ratio of the preset thickness to the initial etching rate as the initial etching time.

3. The etching compensation method according to claim 2, It is characterized in that The attenuation coefficient includes: a first attenuation coefficient in which the etching rate of the chemical solution decays as time increases; and a second attenuation coefficient in which the etching rate of the chemical solution decays as the number of wafers processed increases.

4. The etching compensation method according to claim 3, It is characterized in that The method for obtaining the first attenuation coefficient includes: obtaining a first etching time required for the chemical solution to etch the layer to be etched of the preset thickness on the surface of the first batch of wafers; allowing the chemical solution to stand for a static treatment; after the chemical solution has been allowed to stand for a chemical solution usage cycle time, obtaining a second etching time required for the chemical solution to etch the layer to be etched of the preset thickness on the surface of the second batch of wafers; and taking the ratio of the difference between the second etching time and the first etching time to the chemical solution usage cycle time as the first attenuation coefficient.

5. The etching compensation method according to claim 4, It is characterized in that The method for obtaining the first etching time and the second etching time includes: providing a second tank chemical solution; forming the layer to be etched of the preset thickness on the surface of a first batch of wafers; detecting a first etching rate of the layer to be etched by the chemical solution in the second tank; taking the ratio of the preset thickness to the first etching rate as the first etching time; after the chemical solution is left to stand for the chemical solution usage cycle time, detecting a second etching rate of the layer to be etched by the chemical solution in the second tank; taking the ratio of the preset thickness to the second etching rate as the second etching time.

6. The etching compensation method according to claim 5, It is characterized in that The first tank chemical solution and the second tank chemical solution are different tank chemical solutions.

7. The etching compensation method according to claim 5, It is characterized in that The first tank chemical solution and the second tank chemical solution are the same tank chemical solution.

8. The etching compensation method according to claim 7, It is characterized in that Obtaining the first etching time and obtaining the initial etching time are the same step.

9. The etching compensation method according to claim 3, It is characterized in that The method for obtaining the second attenuation coefficient includes: obtaining the third etching time required by the chemical solution to etch the layer to be etched with the preset thickness on the surface of the first batch of wafers; based on the chemical solution processing the wafers with the maximum processing number of the single-tank chemical solution; after the chemical solution processes the wafers with the maximum processing number of the single-tank chemical solution, obtaining the fourth etching time required by the chemical solution to etch the layer to be etched with the preset thickness on the surface of an additional batch of wafers; and taking the ratio of the difference between the fourth etching time and the third etching time and the maximum processing number of the single-tank chemical solution as the second attenuation coefficient.

10. The etching compensation method according to claim 9, It is characterized in that The method for obtaining the third etching time and the fourth etching time includes: providing a third tank chemical solution; forming the layer to be etched of the preset thickness on the surface of a first batch of wafers; detecting a third etching rate of the third tank chemical solution etching the layer to be etched; using the ratio of the preset thickness to the third etching rate as the third etching time; after the chemical solution processes the wafers with the single tank chemical solution processing limit number, detecting a fourth etching rate of the third tank chemical solution etching the layer to be etched; using the ratio of the preset thickness to the fourth etching rate as the fourth etching time.

11. The etching compensation method according to claim 10, It is characterized in that The first tank chemical solution and the third tank chemical solution are different tank chemical solutions.

12. The etching compensation method according to claim 10, It is characterized in that The first tank chemical solution and the third tank chemical solution are the same tank chemical solution.

13. The etching compensation method according to claim 12, It is characterized in that Obtaining the third etching time and obtaining the initial etching time are the same step.

14. The etching compensation method according to claim 3, It is characterized in that The associated parameters causing the etching rate of the chemical solution to decay include: the time the chemical solution has been used before etching the wafer to be etched; and the number of wafers processed by the chemical solution before etching the wafer to be etched.

15. The etching compensation method according to claim 14, It is characterized in that The method for obtaining the compensation etching time includes: adding the product result of the used time and the first attenuation coefficient and the product result of the processed wafer quantity and the second attenuation coefficient as the compensation etching time of the wafer to be etched.

16. The etching compensation method according to claim 1, It is characterized in that The chemical liquid includes: aluminum corrosion liquid.

17. The etching compensation method according to claim 16, It is characterized in that The material of the layer to be etched includes: aluminum, aluminum silicon copper or aluminum silicon.