Systems and methods for using colloidal silica to resist corrosion of wellhead components in square wells
By forming a colloidal silicone barrier between the wellhead components and the square well of the oil-producing wells, the problem of corrosion is solved, the corrosion prevention effect is achieved, the repair and replacement costs are reduced, and productivity and environmental safety are improved.
Patent Information
- Application Number
- CN202380030506.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-31
- Filing Date
- 2023-03-29
- Publication Date
- 2024-12-06
AI Technical Summary
The prior art is difficult to effectively prevent corrosion caused by water and dissolved oxygen in the square wells of the wellhead components of the oil-producing wells, resulting in high repair and replacement costs, and may involve safety and environmental issues.
Using colloidal silicone, a barrier is formed to resist corrosion by forming a precipitation layer between the surface of the wellhead component and the base and side walls of the square well, covering the wellhead component and extending to the base and side walls of the square well, forming a barrier to resist corrosion of water and dissolved oxygen, combined The substances include colloidal silica, water, activators, oxygen deoxygenators and corrosion inhibitors.
Effectively prevent corrosion of wellhead components, reduce or eliminate the need for repair and replacement, reduce related costs and safety risks, improve productivity, and reduce environmental impact.
Smart Images

Figure CN119096033A_ABST
Abstract
Description
[0001] Priority declaration
[0002] This application claims priority to U.S. patent application No. 17 / 709,819, filed on March 31, 2022, the entire contents of which are incorporated herein by reference. Technical Field
[0003] The present disclosure generally relates to systems and methods for resisting corrosion of wellhead components in square wells using colloidal silica. Background Art
[0004] Typically, an oil production well has an above-ground wellhead component and an underground wellhead component. Some of the underground wellhead components are present in the well. Examples of such wellhead components include surface casing and casing head chassis. Typically, the wellhead components in the well are covered with sand. In some cases, the above-ground wellhead components (such as water injection pipeline flanges) may leak and cause the sand in the well to become wet. In some cases, rainwater causes the sand in the well to become wet. Other water sources may also make the sand in the well wet. The water in the sand in the well may cause corrosion of one or more of the wellhead components present in the well (such as casing head chassis and / or surface casing). In addition to the water itself, corrosion may also be caused by oxygen dissolved in the water. Summary of the invention
[0005] The present disclosure generally relates to a system and method for resisting corrosion of wellhead components in a square well using colloidal silica. For example, the well of the system can be an oil well, a gas well or a water well. In general, the present disclosure provides a colloidal silica that occupies a volume extending from the surface of the wellhead component to the base and sidewalls of the square well. As an example, in some embodiments, the colloidal silica covers a portion of the surface of the wellhead surface casing and extends to the base and sidewalls of the square well, so that the colloidal silica occupies the spatial volume between the square well and the covering surface of the surface casing. As another example, in certain embodiments, the colloidal silica completely covers the surface of the casing head chassis and extends to the base and sidewalls of the square well, so that the colloidal silica occupies the spatial volume between the square well and the covering surface of the casing head chassis. As another example, in some embodiments, the colloidal silica covers a portion of the surface of the wellhead surface casing and a portion of the surface of the casing head chassis, and extends to the base and sidewalls of the square well, so that the colloidal silica occupies the spatial volume between the square well and the covering surface of the wellhead surface casing and the covering surface of the casing head chassis.
[0006] Typically, colloidal silica is formed by precipitation from a composition containing colloidal silicon dioxide, water, and an activator. In some embodiments, the composition further comprises an oxygen scavenger and / or a corrosion inhibitor. The oxygen scavenger and / or the corrosion inhibitor can be used to reduce (e.g., avoid) corrosion caused by water contained in the composition and / or substances present in the water (e.g., dissolved oxygen).
[0007] Typically, after preparation, the composition is arranged in the square well relatively quickly (e.g., immediately). After mixing the components of the composition, the formation of gel due to precipitation can occur quickly (e.g., immediately). In some embodiments, relatively quickly (e.g., immediately) after mixing, the composition is usually poured into the square well at a close distance (e.g., poured on the top of the bottom of the square well or arranged on the top of the sand layer on the bottom of the square well) to evenly distribute the composition. The gel is arranged in the space between the square well and the wellhead component, rather than simply as a coating on the wellhead component.
[0008] Typically, sand is placed on top of the colloidal silica and completely covers the upper surface of the gel. Therefore, typically, the colloidal silica is not directly exposed to the surface. When colloidal silica is precipitated from the composition, an aqueous phase is formed on top of the colloidal silica. The sand can absorb the aqueous phase of the composition left after the colloidal silica is precipitated. The sand also helps to reduce (e.g., avoid) the erosion of the colloidal silica by external factors (e.g., weather).
[0009] Over a considerable period of time, little if any water in the sand covering the colloidal silica gel is able to penetrate through the colloidal silica gel to reach the gel-covered wellhead components. Thus, the colloidal silica gel helps resist or even completely prevent corrosion of the gel-covered well components. More generally, it is believed that the gel can behave as a barrier to water and optionally other liquids. Typically, the colloidal silica gel is non-corrosive and will not corrode, for example, under acidic conditions.
[0010] These systems and related methods can be relatively cheap and easy to produce and implement. In addition, these systems and methods can alleviate safety issues and environmental impacts associated with corrosion of wellhead components. In addition, these systems and methods can reduce or eliminate the need to repair and / or replace corroded wellhead components, which may be expensive and difficult to repair and / or replace corroded wellhead components. In addition, the system and method according to the present disclosure can reduce the time and cost associated with monitoring and inspecting the corrosion of wellhead components. As an example, the casing head chassis is a wellhead component located in a square well. Usually, the casing head chassis cannot be replaced at will. As a result, the loss of use time of the well and / or the cost associated with repairing or replacing the casing head chassis may be considerable. As another example, a portion of the wellhead surface casing in a square well may be severely corroded by moisture. Repairing such corroded surface casing may involve deep excavation of the wellhead, and replacing such corroded surface casing may involve workover. Therefore, using colloidal silica to reduce or eliminate the corrosion of the casing head chassis and / or the wellhead surface casing can obtain a large amount of savings and improved productivity.
[0011] In a first aspect, the present disclosure provides a system comprising a square well, the square well comprising a base and sidewalls extending from the base. The system also comprises a wellhead, the wellhead comprising an above-ground region extending above the square well and an underground region in the square well. The underground region of the wellhead comprises a wellhead component having an outer surface. The system further comprises colloidal silica occupying a volume extending from the base and sidewalls of the square well to the outer surface of the wellhead component. The colloidal silica covers the outer surface of the wellhead component.
[0012] In some embodiments, the colloidal silica substantially prevents water from passing through the colloidal silica to the outer surface of the wellhead member.
[0013] In some embodiments, the system further comprises a solid covering the upper surface of the polyacrylamide gel.
[0014] In some embodiments, the system further includes sand covering the upper surface of the colloidal silica gel.
[0015] In some embodiments, the wellhead component includes a casing head chassis.
[0016] In some embodiments, the wellhead component includes a surface casing. In some embodiments, the colloidal silicone covers the outer surface of the additional wellhead component. In some embodiments, the additional wellhead component includes a casing head chassis.
[0017] In some embodiments, the system includes a well selected from the group consisting of an oil well, a gas well, and a water well.
[0018] In some embodiments, the base of the square well has an opening, and the wellhead includes a plurality of casings extending through and below the base of the square well.
[0019] In some embodiments, the plurality of sleeves includes a surface sleeve that receives the other sleeves.
[0020] In some embodiments, the volume occupied by the gel is at least one cubic foot.
[0021] In some embodiments, the colloidal silica comprises at least 6.5 wt. % colloidal silicon dioxide.
[0022] In a second aspect, the present disclosure provides a method for reducing corrosion of an outer surface of a wellhead component in a square well. The method includes: placing a composition in the square well, the composition comprising colloidal silica, water, an activator, an oxygen scavenger, and a corrosion inhibitor; and allowing the colloidal silica to precipitate from the composition to provide colloidal silica gel. The colloidal silica gel covers the outer surface of the wellhead component and extends to the base and sidewalls of the square well.
[0023] In some embodiments, the activating agent is NaCl or 1,6-hexanediol diglycidyl ether.
[0024] In some embodiments, the method further comprises covering the colloidal silica with sand.
[0025] In some embodiments, the wellhead component is a casing head chassis and / or a surface casing.
[0026] In some embodiments, the composition comprises: 66 wt.% to 91.5 wt.% water; 6.5 wt.% to 32 wt.% colloidal silica; 0.2 wt.% to 4 wt.% NaCl; 0.04 wt.% to 1 wt.% oxygen scavenger; and 1 wt.% to 15 wt.% corrosion inhibitor.
[0027] In some embodiments, the composition comprises: 66 wt.% to 91.5 wt.% water; 6.5 wt.% to 32 wt.% colloidal silica; 2.5 wt.% to 15 wt.% 1,6-hexanediol diglycidyl ether; 0.04 wt.% to 1 wt.% oxygen scavenger; and 1 wt.% to 15 wt.% corrosion inhibitor.
[0028] In some embodiments, the colloidal silica occupies a volume of at least one cubic foot. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Figure 1 is a schematic diagram of the system.
[0030] Figure 2 is a schematic diagram of the system.
[0031] Figure 3 is a schematic diagram of the system.
[0032] Figure 4 is a schematic diagram of the system.
[0033] Figure 5 is a schematic diagram of the system.
[0034] Figure 6 is a photograph of colloidal silica covered by an aqueous phase, which in turn is covered by a low-density gel. DETAILED DESCRIPTION
[0035] Figure 1 Schematically depicted is a system 1000 which may be, for example, part of a well such as an oil well, a gas well, or a water well.
[0036] System 1000 includes a square well 1010 having a bottom 1020 and sidewalls 1030. An uppermost surface 1012 of square well 1010 substantially corresponds to a ground surface 1040, such that square well 1010 is generally located underground.
[0037] System 1000 also includes a wellhead 1050 having an above-ground wellhead region 1060 extending above surface 1040 and a subsurface wellhead region 1070 extending below surface 1040 through wellbore 1010 and through an opening 1025 in bottom 1020 of wellbore 1010. Typically, wellhead regions 1060 and 1070 have a variety of different components. As an example, Figure 1 As shown, the above-ground wellhead area 1060 may include a water injection pipeline flange 1062 and a crown adapter 1064, and the underground wellhead area 1070 may include a casing head chassis 1072 and a tubing head 1074. The wellhead 1050 includes a surface casing 1076, the outer surface of which is exposed in the square well 1010. The surface casing 1076 accommodates a plurality of nested casings, which are exposed below the bottom 1020 of the square well 1010 (see Figures 2 to 4 ).
[0038] Figure 2 The system 2000 is schematically depicted, and includes a wellhead 2050 having an above-ground region 2060 and a subsurface region 2070, respectively. The above-ground region 2060 includes a water injection valve 2062, a crown adapter 2064, an additional valve 2066, and a tubing head 2068. The subsurface region 2070 includes a casing head chassis 2072 and a tubing head 2074, which are arranged above the bottom 2020 of the square well. The subsurface region 2070 also includes a plurality of nested casings, which are housed within surface casings (generally depicted at 2076) and extend below the bottom 2020 of the square well.
[0039] Figure 3The system 3000 is schematically depicted, and includes a wellhead 3050 having an above-ground region 3060 and a subsurface region 3070. The above-ground region 3060 includes a water flow conduit 3061 in fluid communication with an injection valve 3062. In addition, the above-ground region includes a crown adapter 3064 and additional valves 3066 and 3067. The subsurface region 3070 includes a casing head chassis 3072 and a tubing head 3074, which are arranged above the bottom 3020 of the square well. The subsurface region 3070 further includes surface casing and a plurality of nested casings (generally depicted as 3076), which extend through the bottom 3020 of the square well and below the bottom. In some embodiments, the injection line flange between the water flow conduit 3061 and the injection valve 3062 may leak, for example, due to air exposure and continuous water flow. This may cause leaking water to overflow onto the sand covering the wellbore, which may cause corrosion of the surface casing 3076, casing head chassis 3072 and / or tubing head 3074.
[0040] Figure 4 The underground area of the wellhead 4050 is schematically depicted. Above the bottom 4020 of the square well, the wellhead 4050 includes a casing head chassis 4072, a circular ring plate 4073, and a surface casing 4076. The surface casing 4076 extends through the opening 4025 in the bottom 4020 of the square well and enters the conductor 4075. The surface casing 4076 accommodates a plurality of nested casings 4077, 4078, and 4079. In some embodiments, the bottom 4020 of the square well is made of cement. The integrity of cement is sometimes low, and cracks may occur in the cement, which may allow water to penetrate, thereby causing corrosion, for example, at the interface of the surface casing 4076 and the bottom 4020 of the square well. Colloidal silica gel can reduce, for example, prevent such corrosion.
[0041] Reference again Figure 1 , the system 1000 also includes a colloidal silica gel 1080 that completely covers a portion of the outer surface of the surface casing 1076 and the casing head chassis 1072 and extends to the bottom 1020 and the sidewalls 1030 of the square well 1010. Therefore, the colloidal silica gel 1080 occupies the spatial volume between the square well 1010 and the gel-covered outer surface of the surface casing 1076 and the casing head chassis 1072. The sand layer 1090 is arranged on top of the colloidal silica gel 1080. With this arrangement, the colloidal silica gel 1080 acts as a barrier that prevents water present in the sand 1090 from reaching the gel-covered outer surface of the surface casing 1076 and the casing head chassis 1072 for a considerable period of time, thereby maintaining a substantially dry condition around the gel-covered outer surface of the surface casing 1076 and the casing head chassis 1072. As a result, the colloidal silicone helps resist, or even completely prevent, corrosion of the gel-covered outer surfaces of the skin sleeve 1076 and the sleeve head chassis 1072 during these time periods.
[0042] Figure 5 Schematically depicted is a system 5000 that includes a square well 5010 having a bottom 5020 and sidewalls 5030. The system 5000 also includes a wellhead 5050 having a subsurface region 5070 extending through the square well 5010 and through an opening 5025 in the bottom 5020 of the square well 5010. The system 5000 also includes a colloidal silicone 5080 that completely covers a portion of the outer surface of the subsurface wellhead region 5070 and extends to the bottom 5020 and sidewalls 5030 of the square well 5010. In some embodiments, the portion of the outer surface of the subsurface wellhead region 5070 covered by the colloidal silicone comprises a casing head chassis. In some embodiments, the portion of the outer surface of the subsurface wellhead region 5070 covered by the colloidal silicone comprises a surface casing. A sand layer 5090 is disposed on top of the colloidal silicone 5080. In some embodiments, the bottom 5020 layer below the colloidal silicone 5080 comprises cement. In some embodiments, the bottom 5020 layer below the colloidal silica gel 5080 includes sand.
[0043] In some embodiments, the square well 5010 (or 1010) has a diameter of at least 1.25 (e.g., 1.36, at least 1.4, at least 1.5, at least 1.6, at least 1.7, at least 1.8, at least 1.9, at least 2.0) meters (m) and at most 5 (e.g., at most 4, at most 3) m.
[0044] In some embodiments, the square well 5010 (or 1010) has a depth of at least 4.5 (e.g., 4.54, at least 5, at least 6, at least 7, at least 8, at least 9) feet (ft) and at most 10 (e.g., at most 9, at most 8, at most 7, at most 6, at most 5) ft.
[0045] Typically, the height of the colloidal silica gel is sufficient to at least partially (e.g., completely) cover the casing head chassis. In some embodiments, the distance between the bottom of the square well and the highest part of the casing head chassis is 10 feet. In certain embodiments, the height of the colloidal silica gel 5080 (or 1080) in the well is at least 1 (e.g., at least 2, at least 3, at least 4, at least 5, at least 6, at least 7, at least 8, at least 9) ft and at most 10 (e.g., at most 9, at most 8, at most 7, at most 6, at most 5, at most 4, at most 3, at most 2) ft.
[0046] In some embodiments, the volume occupied by colloidal silica 5080 (or 1080) is at least 1 (eg, at least 5, at least 10) cubic feet (ft 3 ) and up to 30 (e.g. up to 25, up to 20) ft 3 .
[0047] Typically, the density of colloidal silica gel 5080 (or 1080) is greater than the density of water. In certain embodiments, the colloidal silica gel has a density of at least 1.13 (eg, 1.14, 1.15, 1.3) g / ml and at most 2.5 g / mL.
[0048] Typically, colloidal silica 5080 (or 1080) is formed by precipitation from a composition comprising colloidal silica, water, and an activator. As used herein, an "activator" is a substance that promotes the precipitation of colloidal silica from a composition. Examples of activators include NaCl and 1,6-hexanediol diglycidyl ether ( D7109). In some embodiments, the composition further comprises a corrosion inhibitor (e.g., O-3670R) and / or an oxygen scavenger (e.g., sodium sulfite (Na2SO3), OXYGON TM Typically, corrosion inhibitors and / or oxygen scavengers protect the composition from corrosion caused by water and / or dissolved oxygen.
[0049] Typically, if desired, the composition is prepared by combining these components using mixing. Typically, the composition is then relatively quickly (e.g., immediately) arranged in the square well 5010 (or 1010). Typically, within a short period of time (e.g., immediately), colloidal silica precipitates from the composition, thereby forming colloidal silica gel 5080 (or 1080) and a water layer on top of the colloidal silica gel 5080 (or 1080). Sand 5090 (or 1090) is arranged on top of the water layer, and the sand absorbs water from the water layer.
[0050] In some embodiments, the composition contains at least 5000 (eg, at least 6000, at least 7000, at least 8000) liters (L) of water and at most 11000 (eg, at most 10000, at most 9000, at most 8000) L of water.
[0051] In certain embodiments, the composition contains at least 5000 (e.g., at least 6000, at least 7000) L of 20 weight percent (wt. %) colloidal silica solution and at most 11000 (e.g., at most 10000, at most 9000, at most 8000) L of 20 wt. % colloidal silica solution.
[0052] In some embodiments, the composition contains at least 100 (e.g., at least 200, at least 500, at least 600, at least 700) kilograms (kg) of NaCl and at most 1000 (e.g., at most 900, at most 800) kg of NaCl.
[0053] In certain embodiments, the composition contains at least 1000 (e.g., at least 1100, at least 1200, at least 1300, at least 1400) L of 1,6-hexanediol diglycidyl ether and at most 2100 (e.g., at most 2000, at most 1900, at most 1800) L of 1,6-hexanediol diglycidyl ether.
[0054] In some embodiments, the composition contains at least 2.2 (e.g., at least 2.5, at least 3.0, at least 3.5, at least 4.0, at least 4.5, at least 4.8) kg of oxygen scavenger and at most 4.85 (e.g., at most 4.8, at most 4.5, at most 4.0, at most 3.5, at most 3.0, at most 2.5) kg of oxygen scavenger.
[0055] In certain embodiments, the composition contains at least 50 (e.g., at least 60, at least 70, at least 80, at least 90, at least 100, at least 105) kg of corrosion inhibitor and at most 110 (e.g., at most 105, at most 100, at most 90, at most 80, at most 70, at most 60) kg of corrosion inhibitor.
[0056] In certain embodiments, the composition contains at least 50 (e.g., at least 60, at least 70, at least 80, at least 90, at least 100, at least 105) L of corrosion inhibitor and at most 110 (e.g., at most 105, at most 100, at most 90, at most 80, at most 70, at most 60) L of corrosion inhibitor.
[0057] In some embodiments, the composition contains at least 6.5 (eg, at least 10, at least 15) weight percent (wt.%) colloidal silica and at most 32 (eg, at most 25, at most 20) wt.% colloidal silica.
[0058] In certain embodiments, the composition contains at least 66 (eg, at least 73, at least 78) wt.% water and at most 91.5 (eg, at most 88, at most 83) wt.% water.
[0059] In some embodiments where the activator is NaCl, the composition contains at least 0.2 (eg, at least 0.5, at least 1, at least 2) wt. % NaCl and at most 4 (eg, at most 3, at most 2) wt. % NaCl.
[0060] In certain embodiments where the activator is 1,6-hexanediol-diglycidyl ether, the composition contains at least 2.5 (e.g., at least 5, at least 7.5, at least 8) wt.% of 1,6-hexanediol-diglycidyl ether and at most 15 (e.g., at most 12.5, at most 10, at most 8) wt.% of 1,6-hexanediol-diglycidyl ether.
[0061] In some embodiments, the composition contains at least 0.04 (eg, at least 0.07, at least 0.1) wt. % oxygen scavenger and at most 1 (eg, at most 0.9, at most 0.8) wt. % oxygen scavenger.
[0062] In certain embodiments, the composition contains at least 1 (eg, at least 5, at least 8, at least 10) wt. % corrosion inhibitor and at most 15 (eg, at most 12) wt. % corrosion inhibitor.
[0063] Table 1 lists two exemplary compositions.
[0064] Table 1
[0065]
[0066] In some embodiments, colloidal silica gel 5080 (or 1080) contains only colloidal silica. However, in certain embodiments, colloidal silica gel 5080 (or 1080) contains water, an activator (e.g., NaCl or 1,6-hexanediol-diglycidyl ether), an oxygen scavenger, and / or a corrosion inhibitor. As an example, in some embodiments, colloidal silica gel 5080 (or 1080) contains at least 6.5 (e.g., at least 10, at least 15) weight percent (wt.%) of colloidal silica and at most 32 (e.g., at most 25, at most 20) wt.% of colloidal silica. As another example, in certain embodiments, colloidal silica gel 5080 (or 1080) contains at least 66 (e.g., at least 73, at least 78) wt.% of water and at most 91.5 (e.g., at most 88, at most 83) wt.% of water. As another example, in some embodiments, colloidal silica gel 5080 (or 1080) contains at least 0.2 (e.g., at least 0.5, at least 1, at least 2) wt.% NaCl and at most 4 (e.g., at most 3, at most 2) wt.% NaCl. As an additional example, in certain embodiments, colloidal silica gel 5080 (or 1080) contains at least 2.5 (e.g., at least 5, at least 7.5, at least 8) wt.% 1,6-hexanediol-diglycidyl ether and at most 15 (e.g., at most 12.5, at most 10, at most 8) wt.% 1,6-hexanediol-diglycidyl ether. As another example, in some embodiments, colloidal silica gel 5080 (or 1080) contains at least 0.03 (e.g., at least 0.07, at least 0.1) wt.% deoxidizer and at most 1 (e.g., at most 0.9, at most 0.8) wt.% deoxidizer. As another example, in certain embodiments, colloidal silica gel 5080 (or 1080) contains at least 0.1 (eg, at least 0.5, at least 1) wt. % of a corrosion inhibitor and at most 2 (eg, at most 1.5) wt. % of a corrosion inhibitor.
[0067] In some embodiments, the colloidal silica is free of substances not present in the composition from which the colloidal silica was precipitated. As an example, in some embodiments, the colloidal silica is free of cement and / or non-aqueous based fluids.
[0068] Examples
[0069] Forming colloidal silica
[0070] A composition containing water, 20 wt.% CB17, and 2 wt.% NaCl was prepared in a container, and the colloidal silica was allowed to precipitate at room temperature for 2 minutes. Figure 6 This is a photo of precipitated colloidal silica. From top to bottom, Figure 6 The three layers shown are a low density gel (EXPANCEL WE40), an aqueous layer (2% NaCl saline), and colloidal silica gel. The low density gel was added to aid visualization of the aqueous layer.
[0071] Sample calculation
[0072] A sample calculation was performed to determine the amount of the components of Composition 1 used to cover 10 feet (ft) above the bottom of a square well with Composition 1. The square well has a diameter of 3 m (9.84 ft). The colloidal silica formed by precipitation will only cover a portion of the space originally occupied by the composition. If the composition covers 10 ft, the precipitated colloidal silica layer will cover 2 to 3 ft above the bottom of the square well. The size of the wellhead components was not taken into account in the calculation. The relevant equations are shown below. The results are in
[0073] The results are presented in Table 2.
[0074]
[0075]
[0076]
[0077]
[0078]
[0079] NaCl (mass) = 10732.5 * 0.02 = 214.65 kg
[0080]
[0081] Corrosion inhibitor (volume) = 10732.5 * 0.01 = 107.325 L
[0082] The corresponding sample calculations were performed to determine the amount of the components of Composition 2 used to cover 10 feet (ft) above the bottom of a square well with Composition 2. The square well has a diameter of 3 m (9.84 ft). The colloidal silica formed by precipitation will only cover a portion of the space initially occupied by the composition. If the composition covers 10 ft, the precipitated colloidal silica layer will cover 2 to 3 ft above the bottom of the square well. The size of the wellhead components was not taken into account in the calculations. The results are presented in Table 2.
[0083] Table 2
[0084]
[0085] Water penetration test
[0086] The sand layer is placed in a container. 10 ml of composition 1 is placed on the top of the sand layer, and colloidal silica is allowed to precipitate from the composition for 2 minutes at room temperature, thereby forming colloidal silica gel on this layer of sand, and forming a water layer on the top of the colloidal silica gel. An additional sand layer is placed on the top of the water layer, and the sand absorbs the water in the water layer. The container is then filled with water, and the container is kept at room temperature. In the course of a day, a part of the top layer of water evaporates. The top water layer is replenished every day to replace the evaporated water. By visual inspection, after 7 days, the bottom sand (below the colloidal silica gel) remains dry. Therefore, the water arranged on the topmost sand does not penetrate through the colloidal silica gel. Therefore, the experiment proves that water cannot penetrate through the colloidal silica layer. Therefore, it is believed that colloidal silica gel can be used to reduce (for example, prevent) the corrosion caused by water in the wellhead components present in the square well.
[0087] Other embodiments
[0088] Although certain embodiments have been disclosed, the disclosure is not limited to such embodiments.
[0089] As an example, although embodiments have been disclosed in which a sand layer is disposed on top of a colloidal silica layer, in some embodiments, there is no sand layer above the colloidal silica. As an example, in some embodiments, the colloidal silica can be covered with a different material, such as but not limited to silica, alumina, or small gravel rocks. As another example, in some embodiments, the colloidal silica extends to the upper surface of the square well, i.e., the ground surface.
Claims
1. A system comprising: A square well, the square well comprising a base and side walls extending from the base; a wellhead, the wellhead comprising an above-ground region extending above the square well and a subterranean region within the square well, the subterranean region of the wellhead comprising a wellhead component having an outer surface; as well as A colloidal silica gel occupies a volume extending from the base and sidewalls of the square well to the outer surface of the wellhead member, wherein the colloidal silica gel covers the outer surface of the wellhead member.
2. The system of claim 1, wherein: The colloidal silica substantially prevents water from passing through the colloidal silica to reach the outer surface of the wellhead member.
3. The system of claim 1, further comprising a solid covering the upper surface of the polyacrylamide gel.
4. The system of claim 1, further comprising sand covering an upper surface of the colloidal silica.
5. The system of claim 1, wherein: The wellhead assembly includes a casing head chassis.
6. The system of claim 1, wherein: The wellhead component includes a surface casing.
7. The system of claim 6, wherein: The colloidal silica covers the outer surface of the additional wellhead component.
8. The system of claim 7, wherein: The additional wellhead components include a casing head chassis.
9. The system of claim 1, wherein: The system includes a well selected from the group consisting of an oil well, a gas well, and a water well.
10. The system of claim 1, wherein: The base of the square well has an opening, and the wellhead includes a plurality of casings extending through the base of the square well and below the base of the square well.
11. The system of claim 1, wherein: The plurality of casings include a surface casing that receives the other casings.
12. The system of claim 1, wherein: The volume occupied by the gel is at least 1 ft 3 .
13. The system of claim 1, wherein: The colloidal silica comprises at least 6.5 wt. % of colloidal silicon dioxide.
14. A method for reducing corrosion of an outer surface of a wellhead component in a square well, the method comprising: placing a composition in the square well, the composition comprising colloidal silica, water, an activator, an oxygen scavenger, and a corrosion inhibitor; as well as allowing colloidal silica to precipitate from the composition to provide a colloidal silica gel, wherein The colloidal silica covers the outer surface of the wellhead component and extends to the base and sidewalls of the square well.
15. The method of claim 14, wherein: The activator is selected from the group consisting of NaCl and 1,6-hexanediol diglycidyl ether.
16. The method of claim 14, further comprising: The colloidal silica was covered with sand.
17. The method of claim 14, wherein: The wellhead component is a casing head chassis and / or a surface casing.
18. The method of claim 14, wherein: The composition comprises: 66 wt.% to 91.5 wt.% water; 6.5 wt.% to 32 wt.% of colloidal silicon dioxide; 0.2 wt.% to 4 wt.% NaCl; 0.04 wt.% to 1 wt.% of an oxygen scavenger; and 1 wt.% to 15 wt.% of a corrosion inhibitor.
19. The method of claim 14, wherein: The composition comprises: 66 wt.% to 91.5 wt.% water; 6.5 wt.% to 32 wt.% of colloidal silicon dioxide; 2.5 wt.% to 15 wt.% of 1,6-hexanediol diglycidyl ether; 0.04 wt.% to 1 wt.% of an oxygen scavenger; and 1 wt.% to 15 wt.% of a corrosion inhibitor.
20. The method of claim 14, wherein: The colloidal silica occupies at least 1ft 3 volume.