A two-color molding die for the transmission components of the door lock of a new energy vehicle
By designing a two-color molding mold for door lock transmission members of new energy vehicles, continuous production is achieved using a rotary table and multi-mold structure, and the anti-detachment effect of soft rubber parts is improved through the design of skateboard seats and plug rods, solving the traditional low production efficiency and anti-prevention The problem of poor removal effect has achieved efficient and continuous production process and good molding quality.
Patent Information
- Application Number
- CN202411649609.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-11-19
- Publication Date
- 2025-02-18
- Estimated Expiration
- 2044-11-19
AI Technical Summary
In the prior art, when producing automobile door lock transmission members, the first injection molded product needs to be transferred to the second injection mold, resulting in low production efficiency and poor anti-detachment effect of the soft rubber part.
Design a new energy vehicle door lock transmission member two-color molding mold, including a rotary table, two lower molds, one-shot upper mold and two-shot upper mold. By setting up a slider and a plug rod, the circular hole mold core rod can be followed by one. When the mold is opened, it moves downward when the mold is opened, and when the mold is closed, the soft rubber part can be clamped onto the hard rubber part through a convex shaped boss to improve the anti-detachment effect.
It realizes that the two injections are directly carried out without transferring the one-injection molded product. The two lower molds can be continuously and uninterruptedly produced, with high production efficiency. The anti-detachment effect of the soft rubber part is improved through the improved mold structure, and the product molding quality is good.
Smart Images

Figure CN119141792B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of injection molds, and in particular to a two-color molding mold for a door lock transmission component of a new energy vehicle. Background Art
[0002] like Figure 2-Figure 4 As shown, this product is a small component in the car door lock, which plays a transmission role. Figure 3 The structure shown is the hard plastic part. Figure 4 The structure shown is the soft rubber part. The hard rubber and soft rubber have different structures and colors. The soft rubber part plays a sealing role to prevent dust from entering the structure and causing abnormal noise. In order to ensure the integrity of the structure, it is generally produced by injection molding. Since two injection molding processes are required, the traditional method requires the first injection molded product to be transferred to the second injection mold, resulting in inability to produce continuously and low production efficiency. At the same time, during the second injection molding process, the soft rubber part is directly injected on the hard rubber part, and two columns are provided at the bottom of the soft rubber part to be inserted into the round holes of the hard rubber. This structure results in poor anti-slip effect of the soft rubber part. Summary of the invention
[0003] The present invention aims to solve the deficiencies of the prior art and provides a two-color molding die for a door lock transmission component of a new energy vehicle.
[0004] In order to achieve the above-mentioned purpose, the present invention adopts the following technical scheme: a two-color molding mold for a transmission component of a door lock of a new energy vehicle, comprising two lower molds, a one-shot upper mold, and a two-shot upper mold. A turntable is rotatably connected to the worktable of an injection molding machine, and the two lower molds are fixedly installed at the two ends of the top of the turntable by bolts, and the one-shot upper mold and the two-shot upper mold are respectively installed on the movable crossbeam of the injection molding machine, and correspond to the two lower molds one by one; the lower mold comprises a lower mold base, a slide plate base, and a lower mold core mounting plate, the one-shot upper mold comprises a one-shot upper mold base, a one-shot hot glue template, and a one-shot upper mold core mounting plate connected in sequence from top to bottom, and the two-shot upper mold comprises a two-shot upper mold base, a two-shot hot glue template, a two-shot cooling template, and a two-shot upper mold core mounting plate connected in sequence from top to bottom;
[0005] A first-shot glue feeding cup is provided at the top center of the first-shot upper mold base, and two first-shot glue injection cups are symmetrically arranged on both sides of the first-shot glue feeding cup, and a first cooling pipeline is provided at the inner edge of the first-shot upper mold base; a second-shot glue feeding cup is provided at the top center of the second-shot upper mold base, and four second-shot glue injection cups are evenly distributed around the second-shot glue feeding cup are provided inside, and a second cooling pipeline is provided at the inner edge of the second-shot upper mold base; an air inlet pipe and an air outlet pipe for adjusting the pressure are respectively provided on the first-shot glue injection cup and the second-shot glue injection cup;
[0006] A first shot glue liquid box connected to a first shot glue feed cup and a first shot glue injection cup is provided at the inner center of the first shot hot glue template, a third cooling pipeline is provided at the inner edge, and a first shot glue injection tube corresponding to the first shot glue injection cup is provided at the bottom of the first shot glue liquid box; a second shot glue liquid box connected to a second shot glue feed cup and a second shot glue injection cup is provided at the inner center of the second shot hot glue template, a fourth cooling pipeline is provided at the inner edge, and a second shot glue injection tube corresponding to the second shot glue injection cup is provided at the bottom of the second shot glue liquid box; electric heating tubes are provided inside the inner walls of the first shot glue liquid box and the second shot glue liquid box, and inside the inner walls of the first shot glue injection tube and the second shot glue injection tube;
[0007] A glue injection positioning plate is provided at the bottom of the one-shot hot glue template, two one-shot glue injection guide sleeves are provided on the top of the glue injection positioning plate, and the one-shot glue injection tube extends into the one-shot glue injection guide sleeve. Two sets of one-shot upper mold cores are provided on the glue injection positioning plate, which are left and right parts of each other; a plurality of two-shot glue injection guide sleeves are provided at the bottom of the two-shot hot glue template, and the two-shot glue injection tube extends into the two-shot glue injection guide sleeve. The bottom of the two-shot glue injection guide sleeve extends into the two-shot cooling template, and a fifth cooling pipeline is provided on the inner edge and middle of the two-shot cooling template;
[0008] A pair of plug rods are fixed by bolts on the front side of the one-shot upper mold core mounting plate, and two one-shot upper mold core boxes with bottom openings are arranged on the top. The bottom of a group of one-shot upper mold cores passes through a one-shot upper mold core box, and a sixth cooling pipeline is arranged on the inner edge of the one-shot upper mold core box; four two-shot glue liquid diverter plates corresponding to the two-shot glue injection guide sleeves are embedded in the top of the two-shot upper mold core mounting plate, and a two-shot glue channel is arranged on the diverter plate, and a two-shot glue injection branch pipe is arranged at the bottom of the two-shot glue channel, and two two-shot upper mold core boxes with bottom openings are arranged inside the two-shot upper mold core mounting plate, and four two-shot upper mold cores are arranged on the two-shot upper mold core box, and a seventh cooling pipeline is arranged in the two-shot upper mold core box;
[0009] Two lower mold core seats are arranged on the top of the lower mold core mounting plate, and the lower mold core seats are butted with the corresponding one-shot upper mold core box and the two-shot upper mold core box. Four lower mold core cavities distributed in a rectangular shape are arranged on the top of the lower mold core seat, and an I-shaped one-shot glue path is arranged between the four lower mold core cavities. The bottom outlet of the one-shot glue guide sleeve is butted with the center point of the one-shot glue path. An eighth cooling pipeline is arranged on the inner edge of the lower mold core seat. Two pairs of connecting plates corresponding to the lower mold core seats are arranged at the bottom of the lower mold core mounting plate, and a round hole mold core rod is inserted through the top of each connecting plate. A first spring is sleeved on the round hole mold core rod. A plurality of first spring grooves corresponding to the first springs are arranged at the bottom of the lower mold core mounting plate, and the top of the first spring abuts against the first spring groove.
[0010] A slide groove is provided on the top of the skateboard seat, and a skateboard is slidably provided in the slide groove. Slide rods are provided at both ends of one side of the skateboard. Two sockets corresponding to the insertion rods are provided on the top of the skateboard seat, and the sockets are connected with the slide groove. The bottom of the insertion rod facing the slide rod and the end of the slide rod are provided with inclined surfaces. A pair of second spring grooves connected with the slide groove are provided on the side of the top of the skateboard seat away from the sockets, and a second spring connected with the skateboard is installed in the second spring groove. A plurality of wave grooves corresponding to the round hole mold core rod are provided on the top of the skateboard.
[0011] In particular, upper positioning blocks in the shape of an inverted convex letter are provided in the middle of the bottom of the four sides of the first-shot upper mold core mounting plate and the second-shot upper mold core mounting plate, and lower positioning blocks in the shape of a concave letter are provided in the middle of the top of the four sides of the lower mold core mounting plate. When the mold is closed, the upper positioning blocks are plugged into the lower positioning blocks.
[0012] In particular, an ejector plate that slides up and down is provided in the lower mold base, and a plurality of ejector pins corresponding to the product cavity are provided on the ejector plate. The ejector pins penetrate the slide plate, the connecting plate, the slide plate base, and the lower mold core base, and an ejector hole corresponding to the ejector plate is provided at the bottom of the lower mold base.
[0013] Particularly, a plurality of positioning columns are arranged at the bottom of the lower die base, and positioning grooves corresponding to the positioning columns are arranged at the top of the rotary table, and the positioning columns are inserted into the positioning grooves.
[0014] Particularly, a guide mechanism is provided between the first-shot upper mold, the second-shot upper mold and the corresponding lower mold.
[0015] The beneficial effects of the present invention are:
[0016] The present invention provides a rotary table, two lower molds, a first-shot upper mold, and a second-shot upper mold. It is not necessary to demould and transfer the first-shot molded product, and the second-shot can be directly performed. At the same time, the two lower molds can be produced continuously and uninterruptedly, and the production efficiency is high.
[0017] The present invention provides a slide plate seat and an insert rod, so that the core rod of the round hole mold can move down when the upper mold is opened and move up when the mold is closed, so that the soft rubber part can be clamped on the hard rubber part through a convex boss, which further plays an anti-slip effect and has good product molding quality.
[0018] The present invention can prevent the glue liquid from condensing in advance by setting a first shot hot glue template and a second shot hot glue template, and the injection molding quality is good;
[0019] The present invention provides a first cooling pipeline, a second cooling pipeline, a third cooling pipeline, a fourth cooling pipeline, a fifth cooling pipeline, a sixth cooling pipeline, a seventh cooling pipeline, and an eighth cooling pipeline, so that the mold and the product cavity can be cooled quickly, thereby improving production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 It is a structural schematic diagram of the present invention;
[0021] Figure 2 This is a schematic diagram of the product structure;
[0022] Figure 3 This is a schematic diagram of the hard plastic structure of the product in one shot molding;
[0023] Figure 4 This is a schematic diagram of the soft rubber structure of the product's two-shot molding;
[0024] Figure 5 It is a schematic diagram of the internal structure of the first-shot upper mold base and the second-shot upper mold base of the present invention;
[0025] Figure 6 It is a schematic diagram of the internal structure of the one-shot thermal glue template and the two-shot thermal glue template of the present invention;
[0026] Figure 7 It is a schematic diagram of the structure of the glue injection positioning plate and the two-shot cooling template of the present invention;
[0027] Figure 8 It is a schematic diagram of the structure of the upper positioning block and the lower positioning block of the present invention;
[0028] Fig. 9 It is a schematic diagram of the structure of the first shot upper mold core mounting plate and the second shot upper mold core mounting plate of the present invention;
[0029] Fig.10 It is a schematic diagram of the structure of the first shot upper mold core box and the second shot upper mold core box of the present invention;
[0030] Fig.11 It is a schematic diagram of the structure of the lower mold core mounting plate of the present invention;
[0031] Fig.12 It is a schematic diagram of the structure of the lower mold core seat of the present invention;
[0032] Fig.13 It is a schematic diagram of the structure of the skateboard seat of the present invention;
[0033] Fig.14 for Fig.13 a rear view of the structure shown;
[0034] Fig.15 for Fig.14 Middle AA section view;
[0035] Fig.16 It is a schematic diagram of the structure of the skateboard of the present invention;
[0036] Fig.17 It is a schematic diagram of the positions of the insertion rod, the slide plate and the second spring of the present invention;
[0037] Fig.18 It is a schematic diagram of the ejector plate structure of the present invention;
[0038] Fig.19 It is a schematic diagram of the positioning column structure of the present invention;
[0039] Fig. 20 It is a schematic diagram of the positions of the circular hole mold core rod and the wave groove of the present invention;
[0040] In the figure:
[0041] 1-lower die;
[0042] 11-lower die base; 1101-ejector plate; 1102-ejector pin; 1103-positioning column;
[0043] 12-slide plate seat; 1201-slide groove; 1202-slide plate; 1203-slide bar; 1204-jack; 1205-second spring groove; 1206-second spring; 1207-wave groove;
[0044] 13-lower mold core mounting plate; 1301-lower mold core seat; 1302-lower mold core cavity; 1303-a shot-jet channel; 1304-eighth cooling pipeline; 1305-connecting plate; 1306-circular hole mold core rod; 1307-first spring; 1308-lower positioning block;
[0045] 2-One shot on the mold;
[0046] 21-first shot upper mold base; 2101-first shot glue cup; 2102-first shot glue cup; 2103-first cooling pipeline;
[0047] 22-first shot hot glue template; 2201-first shot glue liquid box; 2202-third cooling pipeline; 2203-first shot glue injection tube; 2204-glue injection positioning plate; 2205-first shot glue injection guide sleeve; 2206-first shot upper mold core;
[0048] 23-first shot upper mold core mounting plate; 2301-insertion rod; 2302-first shot upper mold core box; 2303-sixth cooling pipeline; 2304-upper positioning block;
[0049] 3-Two-shot upper mold;
[0050] 31-second shot upper mold base; 3101-second shot glue inlet cup; 3102-second shot glue injection cup; 3103-second cooling pipeline;
[0051] 32-two shot hot glue template; 3201-two shot glue liquid box; 3202-fourth cooling pipeline; 3203-two shot glue injection tube; 3204-two shot glue injection guide sleeve;
[0052] 33-second shot cooling template; 3301-fifth cooling pipeline;
[0053] 34-Second shot upper mold core mounting plate; 3401-Second shot glue liquid diverter plate; 3402-Second shot glue channel; 3403-Second shot glue injection branch pipe; 3404-Second shot upper mold core box; 3405-Second shot upper mold core; 3406-Seventh cooling pipeline;
[0054] 4-Turntable;
[0055] The following is a detailed description of the embodiments of the present invention with reference to the accompanying drawings. DETAILED DESCRIPTION
[0056] The present invention will be further described below in conjunction with embodiments:
[0057] like Figure 1 As shown, a two-color molding mold for a door lock transmission component of a new energy vehicle includes two lower molds 1, a one-shot upper mold 2, and a two-shot upper mold 3. A turntable 4 is rotatably connected to the workbench of the injection molding machine. The two lower molds 1 are fixedly installed at both ends of the top of the turntable 4 by bolts. The one-shot upper mold 2 and the two-shot upper mold 3 are respectively installed on the movable crossbeam of the injection molding machine, and correspond to the two lower molds 1 one by one; the lower mold 1 includes a lower mold base 11, a slide plate base 12, and a lower mold core mounting plate 13. The one-shot upper mold 2 includes a one-shot upper mold base 2 connected in sequence from top to bottom. 1. A first-shot hot glue template 22, a first-shot upper mold core mounting plate 23, and a second-shot upper mold 3 include a second-shot upper mold base 31, a second-shot hot glue template 32, a second-shot cooling template 33, and a second-shot upper mold core mounting plate 34 connected in sequence from top to bottom; a guide mechanism is provided between the first-shot upper mold 2, the second-shot upper mold 3 and the corresponding lower mold 1; by arranging a turntable 4, two lower molds 1, a first-shot upper mold 2, and a second-shot upper mold 3, there is no need to demold and transfer the first-shot molded product, and the second-shot can be directly performed, and at the same time, the two lower molds 1 can be continuously and uninterruptedly produced, and the production efficiency is high.
[0058] like Figure 5 As shown, a first-shot glue feeding cup 2101 is provided at the top center of the first-shot upper mold base 21, and two first-shot glue injection cups 2102 are symmetrically arranged on both sides of the first-shot glue feeding cup 2101 are provided inside, and a first cooling pipeline 2103 is provided at the inner edge of the first-shot upper mold base 21; a second-shot glue feeding cup 3101 is provided at the top center of the second-shot upper mold base 31, and four second-shot glue injection cups 3102 are evenly distributed around the second-shot glue feeding cup 3101 are provided inside, and a second cooling pipeline 3103 is provided at the inner edge of the second-shot upper mold base 31; an air inlet pipe and an air outlet pipe for adjusting the pressure are respectively provided on the first-shot glue injection cup 2102 and the second-shot glue injection cup 3102.
[0059] like Figure 6 As shown, a first-shot glue liquid box 2201 connected to a first-shot glue feeding cup 2101 and a first-shot glue injection cup 2102 is provided at the inner center of the first-shot hot glue template 22, a third cooling pipeline 2202 is provided at the inner edge, and a first-shot glue injection tube 2203 corresponding to the first-shot glue injection cup 2102 is provided at the bottom of the first-shot glue liquid box 2201; a second-shot glue liquid box 3201 connected to a second-shot glue feeding cup 3101 and a second-shot glue injection cup 3102 is provided at the inner center of the second-shot hot glue template 32, a fourth cooling pipeline 3202 is provided at the inner edge, and a second-shot glue injection tube 3203 corresponding to the second-shot glue injection cup 3102 is provided at the bottom of the second-shot glue liquid box 3201; electric heating tubes are provided inside the inner walls of the first-shot glue liquid box 2201 and the second-shot glue liquid box 3201, and inside the inner walls of the first-shot glue injection tube 2203 and the second-shot glue injection tube 3203. By providing the first shot hot glue template 22 and the second shot hot glue template 32, the glue liquid can be prevented from condensing in advance, and the injection molding quality is improved;
[0060] like Figure 7 As shown, a glue injection positioning plate 2204 is provided at the bottom of the one-shot hot glue template 22, two one-shot glue injection guide sleeves 2205 are sleeved on the top of the glue injection positioning plate 2204, a one-shot glue injection tube 2203 extends into the one-shot glue injection guide sleeve 2205, and two groups of one-shot upper mold cores 2206 which are left and right parts of each other are provided on the glue injection positioning plate 2204; a plurality of two-shot glue injection guide sleeves 3204 are provided at the bottom of the two-shot hot glue template 32, the two-shot glue injection tubes 3203 extend into the two-shot glue injection guide sleeves 3204, and the bottom of the two-shot glue injection guide sleeves 3204 extends into the two-shot cooling template 33, and a fifth cooling pipeline 3301 is provided on the inner edge and middle of the two-shot cooling template 33.
[0061] like Fig. 9 , Fig.10 As shown, a pair of plug rods 2301 are fixed to the front side of the one-shot upper mold core mounting plate 23 by bolts, and two one-shot upper mold core boxes 2302 with bottom openings are arranged on the top, and the bottom of a group of one-shot upper mold cores 2206 is inserted into one of the one-shot upper mold core boxes 2302, and a sixth cooling pipeline 2303 is arranged on the inner edge of the one-shot upper mold core box 2302; four two-shot glue liquid diverter plates 3401 corresponding to the two-shot glue injection guide sleeves 3204 are embedded in the top of the two-shot upper mold core mounting plate 34, and two-shot glue channels 3402 are arranged on the diverter plates 3401, and two-shot glue injection branch pipes 3403 are arranged at the bottom of the two-shot glue channels 3402, and two two-shot upper mold core boxes 3404 with bottom openings are arranged inside the two-shot upper mold core mounting plate 34, four two-shot upper mold cores 3405 are arranged on the two-shot upper mold core box 3404, and a seventh cooling pipeline 3406 is arranged in the two-shot upper mold core box 3404.
[0062] Fig.11 , Fig.12 As shown, two lower mold core seats 1301 are provided on the top of the lower mold core mounting plate 13, and the lower mold core seats 1301 are connected with the corresponding first-shot upper mold core box 2302 and second-shot upper mold core box 3404. Four lower mold core cavities 1302 distributed in a rectangular shape are provided on the top of the lower mold core seat 1301, and an I-shaped injection glue channel 1303 is provided between the four lower mold core cavities 1302. The bottom outlet of the first-shot glue guide sleeve 2205 is connected with the center point of the injection glue channel 1303. The lower mold core seat 13 An eighth cooling pipeline 1304 is provided on the inner edge of 01, and two pairs of connecting plates 1305 corresponding to the lower mold core seat 1301 are provided at the bottom of the lower mold core mounting plate 13, and a round hole mold core rod 1306 is inserted through the top of each connecting plate 1305, and a first spring 1307 is sleeved on the round hole mold core rod 1306. A plurality of first spring grooves corresponding to the first spring 1307 are provided at the bottom of the lower mold core mounting plate 13, and the top of the first spring 1307 abuts against the first spring groove.
[0063] Figure 13-Figure 17 , Fig. 20As shown, a slide groove 1201 is provided on the top of the slide seat 12, and a slide plate 1202 is slidably provided in the slide groove 1201, and slide rods 1203 are provided at both ends of one side of the slide plate 1202. Two insertion holes 1204 corresponding to the insertion rod 2301 are provided on the top of the slide seat 12, and the insertion holes 1204 are connected with the slide groove 1201, and the bottom of the insertion rod 2301 facing the side of the slide rod 1203 and the end of the slide rod 1203 are provided with inclined surfaces, and a pair of second spring grooves 1205 connected with the slide groove 1201 are provided on the side of the top of the slide seat 12 away from the insertion holes 1204, and a second spring 1206 connected with the slide plate 1202 is installed in the second spring groove 1205, and a plurality of wave grooves 1207 corresponding to the round hole mold core rod 1306 are provided on the top of the slide plate 1202.
[0064] The present invention provides a slide plate seat 12 and an insert rod 2301, so that the circular hole mold core rod 1306 can move downward when the first shot upper mold 2 is opened and move upward when the mold is closed, so that the soft rubber part can be clamped on the hard rubber part through a convex boss, further playing an anti-slip effect, and the product molding quality is good;
[0065] like Figure 8 As shown, an upper positioning block 2304 in the shape of an inverted convex U is provided in the middle of the bottom of the four sides of the first-shot upper mold core mounting plate 23 and the second-shot upper mold core mounting plate 34, and a lower positioning block 1308 in the shape of a concave U is provided in the middle of the top of the four sides of the lower mold core mounting plate 13. When the mold is closed, the upper positioning block 2304 is plugged into the lower positioning block 1308.
[0066] like Fig.18 As shown, an ejector plate 1101 which slides up and down is provided in the lower mold base 11, and a plurality of groups of ejector pins 1102 corresponding to the product cavity are provided on the ejector plate 1101. The ejector pins 1102 pass through the slide plate 1202, the connecting plate 1305, the slide plate base 12, and the lower mold core base 1301. An ejector hole corresponding to the ejector plate 1101 is provided at the bottom of the lower mold base 11.
[0067] like Fig.19 As shown, a plurality of positioning posts 1103 are provided at the bottom of the lower die base 11, and positioning grooves corresponding to the positioning posts 1103 are provided at the top of the turntable 4, and the positioning posts 1103 are inserted into the positioning grooves.
[0068] The working steps of the present invention are as follows:
[0069] S1. The first shot upper mold 2 and the corresponding lower mold 1 below are molded together. At this time, the insertion rod 2301 is inserted into the insertion hole 1204. During the downward movement of the insertion rod 2301, the slide plate 1203 is pushed to move and the second spring 1206 begins to be compressed. At this time, the circular hole mold core rod 1306 moves upward with the movement of the wave groove 1207 and is inserted into the circular hole of the hard rubber part. Fig. 20 As shown;
[0070] S2, inject glue into the first shot glue cup 2101, the glue liquid enters the first shot glue channel 1303 after passing through the first shot glue cup 2102 and the first shot glue tube 2203, and is divided into four paths through the first shot glue channel 1303 to flow to four first shot product cavities. After the injection molding is completed, cooling water circulates in each cooling pipeline to start cooling;
[0071] S3, after the first shot molding, the first shot upper mold 2 is opened. When the mold is opened, the insert rod 2301 moves upward, and the slide plate 1203 is reset under the action of the second spring 1206. The circular hole mold core rod 1306 moves downward along the wave groove 1207 to flow out of the injection molding cavity for the boss structure at the bottom of the soft rubber part;
[0072] S4, the lower mold 1 is transferred to the bottom of the second-shot upper mold 3 under the action of the turntable 4, the second-shot upper mold 3 and the lower mold 1 are molded together, and then glue is injected into the second-shot glue cup 3101, and the glue enters the second-shot glue channel 3402 through the second-shot glue cup 3102 and the second-shot glue injection tube 3203, and is divided into two paths through the second-shot glue channel 3402 to flow to the two second-shot glue injection branch pipes 3403, and is injected into the second-shot product cavity through the second-shot glue injection branch pipes 3403; at the same time, another lower mold 1 and the first-shot upper mold 2 perform a first-shot injection molding process;
[0073] S5. After the second shot is cooled and molded, the second shot upper mold 3 is opened, and the ejector plate 1101 moves upward under the action of the ejector cylinder of the injection molding machine, thereby driving the ejector pin 1102 to move upward, and the final molded product is ejected. After taking it out, the other lower mold with the first shot molded product is transferred to the bottom of the second shot upper mold 3, and the second shot injection molding process is continued. In this way, the two lower molds 1 can perform the first shot injection molding process and the second shot injection molding process alternately.
[0074] The present invention provides a turntable, two lower molds, a one-shot upper mold and a two-shot upper mold. The one-shot molded product does not need to be transferred, and the two-shot molds can be directly produced. At the same time, the two lower molds can be produced continuously and uninterruptedly, and the production efficiency is high. By providing a slide plate seat and an insertion rod, the circular hole mold core rod can move down when the one-shot upper mold is opened and move up when the mold is closed, so that the soft rubber part can be clamped on the hard rubber part through a convex boss, which further has an anti-slip effect and has good product molding quality.
[0075] The present invention provides a turntable 4, two lower molds 1, a first-shot upper mold 2, and a second-shot upper mold 3, so that the first-shot molded product does not need to be transferred, and the second-shot mold can be directly performed. At the same time, the two lower molds 1 can be continuously and uninterruptedly produced, and the production efficiency is high; the present invention provides a slide plate seat 12 and an insert rod 2301, so that the round hole mold core rod 1306 can move downward when the first-shot upper mold 2 is opened and move upward when the mold is closed, so that the soft rubber part can be moved through a convex boss (such as Figure 4 As shown) is clipped onto the hard rubber part, which further prevents it from falling off and ensures good product molding quality;
[0076] In the description of the present invention, it is to be understood that the terms “center”, “longitudinal”, “lateral”, “length”, “width”, “thickness”, “up”, “down”, “front”, “back”, “left”, “right”, “vertical”, “horizontal”, “top”, “bottom”, “inside”, “outside”, “clockwise”, “counterclockwise”, “axial”, “radial”, “circumferential”, etc., indicating orientations or positional relationships are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.
[0077] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0078] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral one; it can be a mechanical connection, an electrical connection, or communication with each other; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0079] The above is an exemplary description of the present invention. Obviously, the specific implementation of the present invention is not limited to the above-mentioned method. As long as various improvements are made using the method concept and technical solution of the present invention, or they are directly applied to other occasions without improvement, they are all within the protection scope of the present invention.
Claims
1. A two-color molding die for a new energy vehicle door lock transmission component, comprising two lower dies (1), a one-shot upper die (2), and a two-shot upper die (3), characterized in that: The worktable of the injection molding machine is rotatably connected to a turntable (4), two lower molds (1) are respectively fixedly mounted on the two ends of the top of the turntable (4) by bolts, and the first-shot upper mold (2) and the second-shot upper mold (3) are respectively mounted on the movable crossbeam of the injection molding machine and correspond to the two lower molds (1) one by one; the lower mold (1) comprises a lower mold base (11), a slide plate base (12), and a lower mold core mounting plate (13); the first-shot upper mold (2) comprises a first-shot upper mold base (21), a first-shot hot glue template (22), and a first-shot upper mold core mounting plate (23) which are connected in sequence from top to bottom; the second-shot upper mold (3) comprises a second-shot upper mold base (31), a second-shot hot glue template (32), a second-shot cooling template (33), and a second-shot upper mold core mounting plate (34) which are connected in sequence from top to bottom; A first-shot glue feeding cup (2101) is provided at the top center of the first-shot upper mold base (21), and two first-shot glue injection cups (2102) are symmetrically arranged on both sides of the first-shot glue feeding cup (2101) are provided inside, and a first cooling pipeline (2103) is provided at the inner edge of the first-shot upper mold base (21); a second-shot glue feeding cup (3101) is provided at the top center of the second-shot upper mold base (31), and four second-shot glue injection cups (3102) are evenly distributed around the second-shot glue feeding cup (3101) are provided inside, and a second cooling pipeline (3103) is provided at the inner edge of the second-shot upper mold base (31); an air inlet pipe and an air outlet pipe for adjusting pressure are respectively provided on the first-shot glue injection cup (2102) and the second-shot glue injection cup (3102); The first-shot hot glue template (22) has a first-shot glue liquid box (2201) connected to the first-shot glue feeding cup (2101) and the first-shot glue injection cup (2102) at its inner center, a third cooling pipeline (2202) is provided at its inner edge, and a first-shot glue injection tube (2203) corresponding to the first-shot glue injection cup (2102) is provided at the bottom of the first-shot glue liquid box (2201); the second-shot hot glue template (32) has a first-shot glue liquid box (2201) connected to the second-shot glue feeding cup (3101) and the second-shot glue injection cup (2102) at its inner center. A second-shot glue liquid box (3201) connected to the glue injection cup (3102) is provided with a fourth cooling pipeline (3202) at the inner edge, and a second-shot glue injection tube (3203) corresponding to the second-shot glue injection cup (3102) is provided at the bottom of the second-shot glue liquid box (3201); electric heating tubes are provided inside the inner walls of the first-shot glue liquid box (2201) and the second-shot glue liquid box (3201), and inside the inner walls of the first-shot glue injection tube (2203) and the second-shot glue injection tube (3203); A glue injection positioning plate (2204) is provided at the bottom of the first-shot hot glue template (22), two first-shot glue injection guide sleeves (2205) are sleeved on the top of the glue injection positioning plate (2204), a first-shot glue injection tube (2203) extends into the first-shot glue injection guide sleeve (2205), and two groups of first-shot upper mold cores (2206) that are left and right parts of each other are provided on the glue injection positioning plate (2204); a plurality of second-shot glue injection guide sleeves (3204) are provided at the bottom of the second-shot hot glue template (32), a second-shot glue injection tube (3203) extends into the second-shot glue injection guide sleeve (3204), and the bottom of the second-shot glue injection guide sleeve (3204) extends into the second-shot cooling template (33), and a fifth cooling pipeline (3301) is provided on the inner edge and middle of the second-shot cooling template (33); A pair of plug rods (2301) are fixed to the front side of the one-shot upper mold core mounting plate (23) by bolts, and two one-shot upper mold core boxes (2302) with bottom openings are arranged on the top, and a group of one-shot upper mold cores (2206) are inserted into one of the one-shot upper mold core boxes (2302) at the bottom, and a sixth cooling pipeline (2303) is arranged on the inner edge of the one-shot upper mold core box (2302); four two-shot upper mold core mounting plates (34) corresponding to the two-shot injection glue guide sleeves (3204) are embedded in the top A glue injection liquid diverter plate (3401), the diverter plate (3401) is provided with a two-shot glue channel (3402), the bottom of the two-shot glue channel (3402) is provided with a two-shot glue injection branch pipe (3403), the two-shot upper mold core mounting plate (34) is provided with two two-shot upper mold core boxes (3404) with bottom openings, the two-shot upper mold core box (3404) is provided with four two-shot upper mold cores (3405), and the second-shot upper mold core box (3404) is provided with a seventh cooling pipeline (3406); Two lower mold core seats (1301) are provided on the top of the lower mold core mounting plate (13), and the lower mold core seats (1301) are docked with the corresponding first-shot upper mold core box (2302) and the second-shot upper mold core box (3404). Four lower mold core cavities (1302) distributed in a rectangular shape are provided on the top of the lower mold core seat (1301), and an I-shaped first-shot glue channel (1303) is provided between the four lower mold core cavities (1302). The bottom outlet of the first-shot glue guide sleeve (2205) is docked with the center point of the first-shot glue channel (1303). The lower mold core seat (130 1) An eighth cooling pipeline (1304) is provided at the inner edge, two pairs of connecting plates (1305) corresponding to the lower mold core seat (1301) are provided at the bottom of the lower mold core mounting plate (13), a round hole mold core rod (1306) is inserted through the top of each connecting plate (1305), a first spring (1307) is sleeved on the round hole mold core rod (1306), a plurality of first spring grooves corresponding to the first springs (1307) are provided at the bottom of the lower mold core mounting plate (13), and the top of the first spring (1307) is in contact with the first spring groove; A slide groove (1201) is provided at the top of the slide plate seat (12), a slide plate (1202) is slidably provided in the slide groove (1201), slide bars (1203) are provided at both ends of one side of the slide plate (1202), two insertion holes (1204) corresponding to the insertion rod (2301) are provided at the top of the slide plate seat (12), and the insertion holes (1204) are communicated with the slide groove (1201), and the bottom of the insertion rod (2301) facing the side of the slide bar (1203) and the end of the slide bar (1203) are provided with inclined surfaces, and a pair of second spring grooves (1205) communicating with the slide groove (1201) are provided at the top of the slide plate seat (12) away from the insertion holes (1204), and second springs (1206) connected to the slide plate (1202) are installed in the second spring grooves (1205), and a plurality of wave grooves (1207) corresponding to the round hole mold core rod (1306) are provided at the top of the slide plate (1202).
2. A two-color molding die for a new energy vehicle door lock transmission component according to claim 1, characterized in that: An upper positioning block (2304) in the shape of an inverted convex letter is provided in the middle of the bottom of the four sides of the first-shot upper mold core mounting plate (23) and the second-shot upper mold core mounting plate (34), and a lower positioning block (1308) in the shape of a concave letter is provided in the middle of the top of the four sides of the lower mold core mounting plate (13). When the mold is closed, the upper positioning block (2304) is plugged into the lower positioning block (1308).
3. A two-color molding die for a new energy vehicle door lock transmission component according to claim 1, characterized in that: An ejector plate (1101) that slides up and down is provided inside the lower mold base (11), and a plurality of groups of ejector pins (1102) corresponding to the product cavity are provided on the ejector plate (1101). The ejector pins (1102) penetrate the slide plate (1202), the connecting plate (1305), the slide plate base (12), and the lower mold core base (1301), and an ejector hole corresponding to the ejector plate (1101) is provided at the bottom of the lower mold base (11).
4. A two-color molding die for a new energy vehicle door lock transmission component according to claim 1, characterized in that: A plurality of positioning columns (1103) are provided at the bottom of the lower die base (11), and positioning grooves corresponding to the positioning columns (1103) are provided at the top of the turntable (4), and the positioning columns (1103) are inserted into the positioning grooves.
5. A two-color molding die for a door lock transmission component of a new energy vehicle according to claim 1, characterized in that: A guiding mechanism is provided between the first-shot upper mold (2), the second-shot upper mold (3) and the corresponding lower mold (1).
Citation Information
Patent Citations
Double-color injection mold with front mold ejected out